Product Showcase
ASTM A213/A213M Stainless Steel Products
ASTM A213 covers seamless ferritic and austenitic alloy-steel boiler, superheater and heat-exchanger tubes. Common grades include T5, T9, T11, T12, T22, T91, TP304, TP304L, TP316, TP316L, TP321 and TP347. These tubes are intended for elevated-temperature service in power plants, petrochemical and refinery applications. SHH STEEL supplies ASTM A213 tubes as a China mill-direct source with competitive pricing, full mill test certificates and reliable worldwide delivery.
-
ASTM A213 UNS S35045 Stainless Steel Tube
ASTM A213 UNS S35045 (Alloy 803 class — no TP letter; Al–Ti bearing 25–29Cr / 32–37Ni austenitic) seamless boiler, superheater and heat-exchanger tube with C 0.06–0.10%, Ti 0.15–0.60%, Al 0.15–0.60%, Cu ≤0.75%, Table 4 floors of 70/25 ksi, hardness max 192 HBW / 90 HRB, and 2000 °F [1100 °C] solution anneal with still-air cool or faster. SHH STEEL supplies cold-finished and hot-finished seamless tube with EN 10204 3.1 MTCs.View More -
ASTM A213 UNS S31277 Stainless Steel Tube
ASTM A213 UNS S31277 (27-7MO class — Footnote C, no TP letter) seamless boiler, superheater and heat-exchanger tube with C ≤0.020%, Cr 20.5–23.0%, Ni 26.0–28.0%, Mo 6.5–8.0%, N 0.30–0.40%, Cu 0.50–1.50%, Table 4 floors of 112/52 ksi, hardness max 241 HBW / 100 HRB, and 2050 °F [1120 °C] solution anneal. SHH STEEL supplies cold-finished and hot-finished seamless tube with EN 10204 3.1 MTCs.View More -
ASTM A213 UNS S31272 Stainless Steel Tube
ASTM A213 UNS S31272 (Footnote C, no TP letter — Ti–B microalloyed 14–16Cr / 14–16Ni austenitic) seamless boiler, superheater and heat-exchanger tube with C 0.08–0.12%, Mo 1.00–1.40%, Ti 0.30–0.60%, B 0.004–0.008%, Table 4 floors of 65/29 ksi, hardness max 217 HBW / 95 HRB, and 1920 °F [1050 °C] solution anneal. SHH STEEL supplies cold-finished and hot-finished seamless tube with EN 10204 3.1 MTCs.View More -
ASTM A213 UNS S31254 Stainless Steel Tube
ASTM A213 UNS S31254 (6Mo / 254 SMO class — Footnote C, no TP letter) seamless boiler, superheater and heat-exchanger tube with C ≤0.020%, Cr 19.5–20.5%, Ni 17.5–18.5%, Mo 6.0–6.5%, N 0.18–0.22%, Cu 0.50–1.00%, wall-split Table 4 floors of 98/45 or 95/45 ksi, hardness max 220 HBW / 96 HRB, and 2100 °F [1150 °C] solution anneal. SHH STEEL supplies cold-finished and hot-finished seamless tube with EN 10204 3.1 MTCs.View More -
ASTM A213 UNS S31002 Stainless Steel Tube
ASTM A213 UNS S31002 (no TP letter — low-C low-Si 25Cr–20Ni austenitic) seamless boiler, superheater and heat-exchanger tube with C ≤0.02%, Si ≤0.15%, Cr 24.0–26.0%, Ni 19.0–22.0%, Mo ≤0.10%, N ≤0.10%, Table 4 floors of 73/30 ksi, hardness max 192 HBW / 90 HRB, and 1900 °F solution anneal. SHH STEEL supplies cold-finished and hot-finished seamless tube with EN 10204 3.1 MTCs.View More -
ASTM A213 UNS S30815 Stainless Steel Tube
ASTM A213 UNS S30815 (no TP letter — Ce–N high-temperature austenitic, commercially 253 MA) seamless boiler, superheater and heat-exchanger tube with C 0.05–0.10%, Si 1.40–2.00%, Cr 20.0–22.0%, Ni 10.0–12.0%, N 0.14–0.20%, Ce 0.03–0.08%, Table 4 floors of 87/45 ksi, hardness max 217 HBW / 95 HRB, and 1920 °F solution anneal. SHH STEEL supplies cold-finished and hot-finished seamless tube with EN 10204 3.1 MTCs.View More -
ASTM A213 UNS S30615 Stainless Steel Tube
ASTM A213 UNS S30615 (no TP letter — high-Si Al austenitic) seamless boiler, superheater and heat-exchanger tube with C 0.16–0.24%, Si 3.2–4.0%, Al 0.8–1.5%, Cr 17.0–19.5%, Ni 13.5–16.0%, Table 4 floors of 90/40 ksi, hardness max 192 HBW / 90 HRB, and 1900 °F solution anneal with Footnote F. SHH STEEL supplies cold-finished and hot-finished seamless tube with EN 10204 3.1 MTCs.View More -
ASTM A213 TP XM-15 Stainless Steel Tube
ASTM A213 XM-15 / UNS S38100 seamless boiler, superheater and heat-exchanger tube — a high-silicon 17–19% Cr / 17.5–18.5% Ni austenitic with Si 1.50–2.50%, C ≤0.08%, Table 4 floors of 75/30 ksi, hardness max 192 HBW / 90 HRB, and 1900 °F solution anneal with Footnote F quench capability. SHH STEEL supplies cold-finished and hot-finished seamless tube with EN 10204 3.1 MTCs.View More -
ASTM A213 TP348H Stainless Steel Tube
ASTM A213 TP348H / UNS S34809 seamless boiler, superheater and heat-exchanger tube with carbon 0.04–0.10%, Cr 17.0–19.0%, Ni 9.0–13.0%, Nb+Ta ≥8×C ≤1.10%, cobalt ≤0.20%, tantalum ≤0.10%, Table 4 floor 75/30 ksi, hardness max 192 HBW / 90 HRB, and grain size No. 7 or coarser. SHH STEEL supplies seamless tube with finish-route solution treatment (CF 2000 °F [1100 °C] / HR 1925 °F [1050 °C]) and EN 10204 3.1 MTCs that report Nb+Ta, Co, Ta, and grain size.View More -
ASTM A213 TP348 Stainless Steel Tube
ASTM A213 TP348 / UNS S34800 seamless boiler, superheater and heat-exchanger tube with carbon ≤0.08%, Cr 17.0–19.0%, Ni 9.0–13.0%, Nb+Ta ≥10×C ≤1.10%, cobalt ≤0.20%, tantalum ≤0.10%, Table 4 floor 75/30 ksi, and hardness max 192 HBW / 90 HRB. SHH STEEL supplies cold-finished and hot-finished seamless tube solution treated at 1900 °F [1040 °C] with EN 10204 3.1 MTCs that report Nb+Ta, Co, and Ta.View More -
ASTM A213 TP347W Stainless Steel Tube
ASTM A213 TP347W / UNS S34705 seamless boiler, superheater and heat-exchanger tube with carbon ≤0.05%, Cr 17.0–20.0%, Ni 8.00–11.0%, nitrogen 0.10–0.25%, niobium 0.25–0.50%, vanadium 0.20–0.50%, tungsten 1.50–2.60%, Table 4 floor 90/38 ksi, hardness max 219 HBW / 95 HRB, and grain size 7–10. SHH STEEL supplies seamless tube solution treated at 2000 °F [1100 °C] with EN 10204 3.1 MTCs that report W, V, N, and Nb.View More -
ASTM A213 TP347LN Stainless Steel Tube
ASTM A213 TP347LN / UNS S34751 seamless boiler, superheater and heat-exchanger tube with ultra-low carbon 0.005–0.020%, nitrogen 0.06–0.10%, Cr 17.0–19.0%, Ni 9.0–13.0%, niobium 0.20–0.50% and ≥15×C, Table 4 floor 75/30 ksi, and hardness max 192 HBW / 90 HRB. SHH STEEL supplies cold-finished and hot-finished seamless tube solution treated at 1900 °F [1040 °C] with EN 10204 3.1 MTCs that report C, N, and Nb against the 15×C formula.View More
ASTM A213/A213M Stainless Steel Products
Stainless Steel Pipes and Tubes
SHH STEEL, a premier Stainless Steel Pipes and Tubes exporter, produces and exports stainless steel pipes and tubes for chemical, marine, and food processing industries. Our seamless and welded products, like 304 and 316L (ASTM A312), ensure corrosion resistance and strength. With a 5,000-ton inventory, we deliver in 3–5 days, backed by SGS/TUV inspections and mill certificates. Choose SHH STEEL for seamless stainless steel pipes and custom solutions.
Stainless Steel Pipes and Tubes
X