EN 10296-2 Stainless Steel Products

SHH STEEL offers EN 10296-2-compliant 304/316 stainless steel tubes. EN 10296-2 specifies welded stainless steel tubes for general purposes, ideal for mechanical, decorative, and structural applications. Certified quality, competitive prices, customizable. Trust SHH STEEL!

EN 10296-2 1.4854 Welded Stainless Steel Tube | EN 10296-2 Stainless Steel - SHH STEEL

EN 10296-2 1.4854 Welded Stainless Steel Tube

EN 10296-2 1.4854 / X6NiCrSiNCe35-25 welded stainless general-purpose tube (353MA), austenitic heat-resisting, cast analysis per EN table, ambient Rp0.2 min 300 MPa, Rm min 650 MPa, A long. min 40%, delivery +AT. SHH STEEL can produce and supply with EN 10204 3.1 MTCs and ordered Annex A finishes.
View More
EN 10296-2 1.4818 Welded Stainless Steel Tube | EN 10296-2 Stainless Steel - SHH STEEL

EN 10296-2 1.4818 Welded Stainless Steel Tube

EN 10296-2 1.4818 / X6CrNiSiNCe19-10 welded stainless general-purpose tube (153MA / Ce-Si-N 19-10), austenitic heat-resisting, cast analysis per EN table, ambient Rp0.2 min 290 MPa, Rm min 600 MPa, A long. min 40%, delivery +AT. SHH STEEL can produce and supply with EN 10204 3.1 MTCs and ordered Annex A finishes.
View More
EN 10296-2 1.4845 Welded Stainless Steel Tube | EN 10296-2 Stainless Steel - SHH STEEL

EN 10296-2 1.4845 Welded Stainless Steel Tube

EN 10296-2 1.4845 / X8CrNi25-21 welded stainless general-purpose tube (310S), austenitic heat-resisting, cast analysis per EN table, ambient Rp0.2 min 210 MPa, Rm min 500 MPa, A long. min 35%, delivery +AT. SHH STEEL can produce and supply with EN 10204 3.1 MTCs and ordered Annex A finishes.
View More
EN 10296-2 1.4833 Welded Stainless Steel Tube | EN 10296-2 Stainless Steel - SHH STEEL

EN 10296-2 1.4833 Welded Stainless Steel Tube

EN 10296-2 1.4833 / X12CrNi23-13 welded stainless general-purpose tube (309S), austenitic heat-resisting, cast analysis per EN table, ambient Rp0.2 min 210 MPa, Rm min 500 MPa, A long. min 35%, delivery +AT. SHH STEEL can produce and supply with EN 10204 3.1 MTCs and ordered Annex A finishes.
View More
EN 10296-2 1.4835 Welded Stainless Steel Tube | EN 10296-2 Stainless Steel - SHH STEEL

EN 10296-2 1.4835 Welded Stainless Steel Tube

EN 10296-2 1.4835 / X9CrNiSiNCe21-11-2 welded stainless general-purpose tube (253MA), austenitic heat-resisting, cast analysis per EN table, ambient Rp0.2 min 310 MPa, Rm min 650 MPa, A long. min 40%, delivery +AT. SHH STEEL can produce and supply with EN 10204 3.1 MTCs and ordered Annex A finishes.
View More
EN 10296-2 1.4828 Welded Stainless Steel Tube | EN 10296-2 Stainless Steel - SHH STEEL

EN 10296-2 1.4828 Welded Stainless Steel Tube

EN 10296-2 1.4828 / X15CrNiSi20-12 welded stainless general-purpose tube (309Si / Si-bearing 20-12), austenitic heat-resisting, cast analysis per EN table, ambient Rp0.2 min 230 MPa, Rm min 550 MPa, A long. min 30%, delivery +AT. SHH STEEL can produce and supply with EN 10204 3.1 MTCs and ordered Annex A finishes.
View More
EN 10296-2 1.4410 Welded Stainless Steel Tube | EN 10296-2 Stainless Steel - SHH STEEL

EN 10296-2 1.4410 Welded Stainless Steel Tube

EN 10296-2 1.4410 / X2CrNiMoN25-7-4 welded stainless general-purpose tube (2507 / superduplex), duplex (austenitic-ferritic), cast analysis per EN table, ambient Rp0.2 min 550 MPa, Rm min 800 MPa, A long. min 15%, delivery +AT. SHH STEEL can produce and supply with EN 10204 3.1 MTCs and ordered Annex A finishes.
View More
EN 10296-2 1.4462 Welded Stainless Steel Tube | EN 10296-2 Stainless Steel - SHH STEEL

EN 10296-2 1.4462 Welded Stainless Steel Tube

EN 10296-2 1.4462 / X2CrNiMoN22-5-3 welded stainless general-purpose tube (2205), duplex (austenitic-ferritic), cast analysis per EN table, ambient Rp0.2 min 450 MPa, Rm min 700 MPa, A long. min 22%, delivery +AT. SHH STEEL can produce and supply with EN 10204 3.1 MTCs and ordered Annex A finishes.
View More
EN 10296-2 1.4362 Welded Stainless Steel Tube | EN 10296-2 Stainless Steel - SHH STEEL

EN 10296-2 1.4362 Welded Stainless Steel Tube

EN 10296-2 1.4362 / X2CrNiN23-4 welded stainless general-purpose tube (2304 / lean duplex), duplex (austenitic-ferritic), cast analysis per EN table, ambient Rp0.2 min 400 MPa, Rm min 600 MPa, A long. min 20%, delivery +AT. SHH STEEL can produce and supply with EN 10204 3.1 MTCs and ordered Annex A finishes.
View More
EN 10296-2 1.4547 Welded Stainless Steel Tube | EN 10296-2 Stainless Steel - SHH STEEL

EN 10296-2 1.4547 Welded Stainless Steel Tube

EN 10296-2 1.4547 / X1CrNiMoCuN20-18-7 welded stainless general-purpose tube (254 SMO / 6Mo), austenitic corrosion-resisting, cast analysis per EN table, ambient Rp0.2 min 300 MPa, Rm min 650 MPa, A long. min 35%, delivery +AT. SHH STEEL can produce and supply with EN 10204 3.1 MTCs and ordered Annex A finishes.
View More
EN 10296-2 1.4539 Welded Stainless Steel Tube | EN 10296-2 Stainless Steel - SHH STEEL

EN 10296-2 1.4539 Welded Stainless Steel Tube

EN 10296-2 1.4539 / X1NiCrMoCu25-20-5 welded stainless general-purpose tube (904L), austenitic corrosion-resisting, cast analysis per EN table, ambient Rp0.2 min 220 MPa, Rm min 520 MPa, A long. min 35%, delivery +AT. SHH STEEL can produce and supply with EN 10204 3.1 MTCs and ordered Annex A finishes.
View More
EN 10296-2 1.4439 Welded Stainless Steel Tube | EN 10296-2 Stainless Steel - SHH STEEL

EN 10296-2 1.4439 Welded Stainless Steel Tube

EN 10296-2 1.4439 / X2CrNiMoN17-13-5 welded stainless general-purpose tube (317LMN), austenitic corrosion-resisting, cast analysis per EN table, ambient Rp0.2 min 285 MPa, Rm min 580 MPa, A long. min 35%, delivery +AT. SHH STEEL can produce and supply with EN 10204 3.1 MTCs and ordered Annex A finishes.
View More

EN 10296-2 Stainless Steel Products

EN 10296-2 1.4854 Welded Stainless Steel Tube EN 10296-2 1.4818 Welded Stainless Steel Tube EN 10296-2 1.4845 Welded Stainless Steel Tube EN 10296-2 1.4833 Welded Stainless Steel Tube
EN 10296-2 1.4835 Welded Stainless Steel Tube EN 10296-2 1.4828 Welded Stainless Steel Tube EN 10296-2 1.4410 Welded Stainless Steel Tube EN 10296-2 1.4462 Welded Stainless Steel Tube
EN 10296-2 1.4362 Welded Stainless Steel Tube EN 10296-2 1.4547 Welded Stainless Steel Tube EN 10296-2 1.4539 Welded Stainless Steel Tube EN 10296-2 1.4439 Welded Stainless Steel Tube
EN 10296-2 1.4435 Welded Stainless Steel Tube EN 10296-2 1.4436 Welded Stainless Steel Tube EN 10296-2 1.4429 Welded Stainless Steel Tube EN 10296-2 1.4432 Welded Stainless Steel Tube
EN 10296-2 1.4571 Welded Stainless Steel Tube EN 10296-2 1.4401 Welded Stainless Steel Tube EN 10296-2 1.4404 Welded Stainless Steel Tube EN 10296-2 1.4550 Welded Stainless Steel Tube
EN 10296-2 1.4541 Welded Stainless Steel Tube EN 10296-2 1.4301 Welded Stainless Steel Tube EN 10296-2 1.4311 Welded Stainless Steel Tube EN 10296-2 1.4306 Welded Stainless Steel Tube
EN 10296-2 1.4307 Welded Stainless Steel Tube EN 10296-2 1.4318 Welded Stainless Steel Tube EN 10296-2 1.4509 Welded Stainless Steel Tube EN 10296-2 1.4526 Welded Stainless Steel Tube
EN 10296-2 1.4521 Welded Stainless Steel Tube EN 10296-2 1.4510 Welded Stainless Steel Tube EN 10296-2 1.4016 Welded Stainless Steel Tube EN 10296-2 1.4512 Welded Stainless Steel Tube
EN 10296-2 1.4003 Welded Stainless Steel Tube
Stainless Steel Pipes and Tubes supplier and exporter

Stainless Steel Pipes and Tubes

SHH STEEL, a premier Stainless Steel Pipes and Tubes exporter, produces and exports stainless steel pipes and tubes for chemical, marine, and food processing industries. Our seamless and welded products, like 304 and 316L (ASTM A312), ensure corrosion resistance and strength. With a 5,000-ton inventory, we deliver in 3–5 days, backed by SGS/TUV inspections and mill certificates. Choose SHH STEEL for seamless stainless steel pipes and custom solutions.

Stainless Steel Pipes and Tubes

SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

    *

    *

    *

    *


    X