ASTM A213/A213M

Product Showcase

ASTM A213/A213M Stainless Steel Products

ASTM A213 covers seamless ferritic and austenitic alloy-steel boiler, superheater and heat-exchanger tubes. Common grades include T5, T9, T11, T12, T22, T91, TP304, TP304L, TP316, TP316L, TP321 and TP347. These tubes are intended for elevated-temperature service in power plants, petrochemical and refinery applications. SHH STEEL supplies ASTM A213 tubes as a China mill-direct source with competitive pricing, full mill test certificates and reliable worldwide delivery.

ASTM A213 TP309S Stainless Steel Tube | ASTM A213 Stainless Steel - SHH STEEL

ASTM A213 TP309S Stainless Steel Tube

ASTM A213 TP309S / UNS S30908 seamless boiler, superheater and heat-exchanger tube — a 22–24% Cr / 12–15% Ni austenitic with C ≤0.08%, Table 4 floors of 75/30 ksi, hardness max 192 HBW / 90 HRB, and a 1900 °F solution anneal. Chosen for high-temperature oxidation resistance rather than molybdenum chloride framing. SHH STEEL supplies cold-finished and hot-finished seamless tube with EN 10204 3.1 MTCs.
View More
ASTM A213 UNS S30432 Stainless Steel Tube | ASTM A213 Stainless Steel - SHH STEEL

ASTM A213 UNS S30432 Stainless Steel Tube

ASTM A213 UNS S30432 (commercially Super304H / 18Cr-9Ni-3Cu-Nb-N) seamless boiler and superheater tube with C 0.07–0.13%, Cu 2.5–3.5%, Nb 0.30–0.60%, N 0.05–0.12%, a 2000 °F [1100 °C] solution anneal, and Table 4 floors of 86/34 ksi with hardness max 219 HBW / 95 HRB. SHH STEEL supplies cold-finished and hot-finished seamless tube with EN 10204 3.1 MTCs.
View More
ASTM A213 TP304LN Stainless Steel Tube | ASTM A213 Stainless Steel - SHH STEEL

ASTM A213 TP304LN Stainless Steel Tube

ASTM A213 TP304LN / UNS S30453 seamless boiler, superheater and heat-exchanger tube — low-carbon nitrogen-strengthened 18-8 with C ≤0.035% (Footnote D to 0.040%), N 0.10–0.16%, Cr 18.0–20.0%, Ni 8.0–11.0%, and a Table 4 floor of 75/30 ksi with hardness max 192 HBW / 90 HRB. SHH STEEL supplies cold-finished and hot-finished seamless tube with EN 10204 3.1 MTCs.
View More
ASTM A213 TP304N Stainless Steel Tube | ASTM A213 Stainless Steel - SHH STEEL

ASTM A213 TP304N Stainless Steel Tube

ASTM A213 TP304N / UNS S30451 seamless boiler, superheater and heat-exchanger tube — nitrogen-strengthened 18-8 with N 0.10–0.16%, Cr 18.0–20.0%, Ni 8.0–11.0%, C ≤0.08%, and a Table 4 floor of 80/35 ksi with hardness max 192 HBW / 90 HRB. SHH STEEL supplies cold-finished and hot-finished seamless tube with EN 10204 3.1 MTCs.
View More
ASTM A213 TP304H Stainless Steel Tube | ASTM A213 Stainless Steel - SHH STEEL

ASTM A213 TP304H Stainless Steel Tube

ASTM A213 TP304H / UNS S30409 seamless boiler, superheater and heat-exchanger tube with controlled carbon 0.04–0.10%, Cr 18.0–20.0%, Ni 8.0–11.0%, a 75/30 ksi Table 4 floor, hardness max 192 HBW / 90 HRB, 1900 °F solution anneal, and ASTM grain size No. 7 or coarser. SHH STEEL supplies cold-finished and hot-finished seamless tube with EN 10204 3.1 MTCs that report grain size.
View More
ASTM A213 TP XM-19 Stainless Steel Tube | ASTM A213 Stainless Steel - SHH STEEL

ASTM A213 TP XM-19 Stainless Steel Tube

ASTM A213 XM-19 / UNS S20910 (Nitronic 50) seamless boiler, superheater and heat-exchanger tube with Cr 20.5–23.5%, Ni 11.5–13.5%, Mo 1.50–3.00%, N 0.20–0.40%, Nb and V 0.10–0.30% each. Under A213 Table 4 the floor is 100/55 ksi with hardness max 250 HBW / 25 HRC. SHH STEEL supplies cold-finished and hot-finished seamless tube with EN 10204 3.1 MTCs.
View More
ASTM A213 TP202 Stainless Steel Tube | ASTM A213 Stainless Steel - SHH STEEL

ASTM A213 TP202 Stainless Steel Tube

ASTM A213 TP202 / UNS S20200 seamless boiler, superheater and heat-exchanger tube — the higher-manganese Mn–N austenitic with Mn 7.5–10.0%, Ni 4.0–6.0%, Cr 17.0–19.0%, N ≤0.25% and C ≤0.15%. Under A213 Table 4 the floor is 90/45 ksi with hardness max 219 HBW / 95 HRB. SHH STEEL supplies cold-finished and hot-finished seamless tube with EN 10204 3.1 MTCs.
View More
ASTM A213 TP201 Stainless Steel Tube | ASTM A213 Stainless Steel - SHH STEEL

ASTM A213 TP201 Stainless Steel Tube

ASTM A213 TP201 / UNS S20100 seamless boiler, superheater and heat-exchanger tube — a manganese-nitrogen austenitic with Mn 5.5–7.5%, Ni 3.5–5.5%, Cr 16.0–18.0%, N ≤0.25% and C ≤0.15%. Under A213 Table 4 the floor is 95/38 ksi with hardness max 219 HBW / 95 HRB. SHH STEEL supplies cold-finished and hot-finished seamless tube with EN 10204 3.1 MTCs.
View More
ASTM A213 TP316L Stainless Steel Tube | ASTM A213 Stainless Steel - SHH STEEL

ASTM A213 TP316L Stainless Steel Tube

ASTM A213 TP316L / UNS S31603 seamless boiler, superheater and heat-exchanger tube with C ≤0.035% (Footnote D to 0.040% on small-OD / light-wall), Cr 16.0–18.0%, Ni 10.0–14.0%, Mo 2.00–3.00%, a 70/25 ksi Table 4 floor, hardness max 192 HBW / 90 HRB, and a 1900 °F solution anneal. SHH STEEL supplies cold-finished and hot-finished seamless tube with EN 10204 3.1 MTCs.
View More
ASTM A213 TP316 Stainless Steel Tube | ASTM A213 Stainless Steel - SHH STEEL

ASTM A213 TP316 Stainless Steel Tube

ASTM A213 TP316 / UNS S31600 seamless boiler, superheater and heat-exchanger tube with Cr 16.0–18.0%, Ni 10.0–14.0%, Mo 2.00–3.00% and C ≤0.08%, a 75/30 ksi Table 4 floor, hardness max 192 HBW / 90 HRB, and a 1900 °F solution anneal. SHH STEEL supplies cold-finished and hot-finished seamless tube with EN 10204 3.1 MTCs.
View More
ASTM A213 TP304L Stainless Steel Tube | ASTM A213 Stainless Steel - SHH STEEL

ASTM A213 TP304L Stainless Steel Tube

ASTM A213 TP304L / UNS S30403 seamless boiler, superheater and heat-exchanger tube with C ≤0.035% (Footnote D to 0.040% on small-OD / light-wall), Cr 18.0–20.0%, Ni 8.0–12.0%, a 70/25 ksi Table 4 floor, hardness max 192 HBW / 90 HRB, and a 1900 °F solution anneal. SHH STEEL supplies cold-finished and hot-finished seamless tube with EN 10204 3.1 MTCs.
View More
ASTM A213 TP304 Stainless Steel Tube | ASTM A213 Stainless Steel - SHH STEEL

ASTM A213 TP304 Stainless Steel Tube

ASTM A213 TP304 / UNS S30400 seamless boiler, superheater and heat-exchanger tube with Cr 18.0–20.0%, Ni 8.0–11.0% and C ≤0.08%, a 75/30 ksi Table 4 floor, hardness max 192 HBW / 90 HRB, and a 1900 °F solution anneal. SHH STEEL supplies cold-finished and hot-finished seamless tube with EN 10204 3.1 MTCs.
View More

ASTM A213/A213M Stainless Steel Products

ASTM A213 UNS S35045 Stainless Steel Tube ASTM A213 UNS S31277 Stainless Steel Tube ASTM A213 UNS S31272 Stainless Steel Tube ASTM A213 UNS S31254 Stainless Steel Tube
ASTM A213 UNS S31002 Stainless Steel Tube ASTM A213 UNS S30815 Stainless Steel Tube ASTM A213 UNS S30615 Stainless Steel Tube ASTM A213 TP XM-15 Stainless Steel Tube
ASTM A213 TP348H Stainless Steel Tube ASTM A213 TP348 Stainless Steel Tube ASTM A213 TP347W Stainless Steel Tube ASTM A213 TP347LN Stainless Steel Tube
ASTM A213 TP347HFG Stainless Steel Tube ASTM A213 TP347H Stainless Steel Tube ASTM A213 TP347 Stainless Steel Tube ASTM A213 TP321H Stainless Steel Tube
ASTM A213 TP321 Stainless Steel Tube ASTM A213 TP317LMN Stainless Steel Tube ASTM A213 TP317LM Stainless Steel Tube ASTM A213 TP317L Stainless Steel Tube
ASTM A213 TP317 Stainless Steel Tube ASTM A213 TP316LNM Stainless Steel Tube ASTM A213 TP316N Stainless Steel Tube ASTM A213 TP316Ti Stainless Steel Tube
ASTM A213 TP316H Stainless Steel Tube ASTM A213 TP310MoCbN Stainless Steel Tube ASTM A213 TP310MoLN Stainless Steel Tube ASTM A213 TP310HCbN Stainless Steel Tube
ASTM A213 TP310HCb Stainless Steel Tube ASTM A213 TP310Cb Stainless Steel Tube ASTM A213 TP310H Stainless Steel Tube ASTM A213 TP310S Stainless Steel Tube
ASTM A213 TP309LMoN Stainless Steel Tube ASTM A213 TP309HCb Stainless Steel Tube ASTM A213 TP309Cb Stainless Steel Tube ASTM A213 TP309H Stainless Steel Tube
ASTM A213 TP309S Stainless Steel Tube ASTM A213 UNS S30432 Stainless Steel Tube ASTM A213 TP304LN Stainless Steel Tube ASTM A213 TP304N Stainless Steel Tube
ASTM A213 TP304H Stainless Steel Tube ASTM A213 TP XM-19 Stainless Steel Tube ASTM A213 TP202 Stainless Steel Tube ASTM A213 TP201 Stainless Steel Tube
ASTM A213 TP316L Stainless Steel Tube ASTM A213 TP316 Stainless Steel Tube ASTM A213 TP304L Stainless Steel Tube ASTM A213 TP304 Stainless Steel Tube
Stainless Steel Pipes and Tubes supplier and exporter

Stainless Steel Pipes and Tubes

SHH STEEL, a premier Stainless Steel Pipes and Tubes exporter, produces and exports stainless steel pipes and tubes for chemical, marine, and food processing industries. Our seamless and welded products, like 304 and 316L (ASTM A312), ensure corrosion resistance and strength. With a 5,000-ton inventory, we deliver in 3–5 days, backed by SGS/TUV inspections and mill certificates. Choose SHH STEEL for seamless stainless steel pipes and custom solutions.

Stainless Steel Pipes and Tubes

SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

    *

    *

    *

    *


    X