EN 10216-5

Product Showcase

EN 10216-5 Stainless Steel Products

SHH STEEL offers EN 10216-5-compliant 304/316 stainless steel tubes. EN 10216-5 specifies seamless stainless steel tubes for pressure purposes, suitable for high/low-temperature and corrosive environments. Certified quality, competitive prices, customizable. Trust SHH STEEL!

EN 10216-5 1.4982 Seamless Stainless Steel Tube | EN 10216-5 Stainless Steel - SHH STEEL

EN 10216-5 1.4982 Seamless Stainless Steel Tube

EN 10216-5 1.4982 / X10CrNiMoMnNbVB15-10-1 seamless stainless pressure tube, austenitic creep-resisting, cast analysis per EN table, ambient Rp0.2 min 220 MPa, Rm 540–740, solution annealed at 1050–1150 °C. SHH STEEL can produce and supply with EN 10204 3.1 MTCs, TC1/TC2 testing.
View More
EN 10216-5 1.4981 Seamless Stainless Steel Tube | EN 10216-5 Stainless Steel - SHH STEEL

EN 10216-5 1.4981 Seamless Stainless Steel Tube

EN 10216-5 1.4981 / X8CrNiMoNb16-16 seamless stainless pressure tube, austenitic creep-resisting, cast analysis per EN table, ambient Rp0.2 min 215 MPa, Rm 530–690, solution annealed at 1050–1100 °C. SHH STEEL can produce and supply with EN 10204 3.1 MTCs, TC1/TC2 testing.
View More
EN 10216-5 1.4988 Seamless Stainless Steel Tube | EN 10216-5 Stainless Steel - SHH STEEL

EN 10216-5 1.4988 Seamless Stainless Steel Tube

EN 10216-5 1.4988 / X8CrNiMoVNb16-13 seamless stainless pressure tube, austenitic creep-resisting, cast analysis per EN table, ambient Rp0.2 min 255 MPa, Rm 540–740, solution annealed at 1100–1150 °C. SHH STEEL can produce and supply with EN 10204 3.1 MTCs, TC1/TC2 testing.
View More
EN 10216-5 1.4961 Seamless Stainless Steel Tube | EN 10216-5 Stainless Steel - SHH STEEL

EN 10216-5 1.4961 Seamless Stainless Steel Tube

EN 10216-5 1.4961 / X8CrNiNb16-13 seamless stainless pressure tube, austenitic creep-resisting, cast analysis per EN table, ambient Rp0.2 min 205 MPa, Rm 510–690, solution annealed at 1050–1100 °C. SHH STEEL can produce and supply with EN 10204 3.1 MTCs, TC1/TC2 testing.
View More
EN 10216-5 1.4910 Seamless Stainless Steel Tube | EN 10216-5 Stainless Steel - SHH STEEL

EN 10216-5 1.4910 Seamless Stainless Steel Tube

EN 10216-5 1.4910 / X3CrNiMoBN17-13-3 seamless stainless pressure tube, austenitic creep-resisting, cast analysis per EN table, ambient Rp0.2 min 260 MPa, Rm 550–750, solution annealed at 1020–1100 °C. SHH STEEL can produce and supply with EN 10204 3.1 MTCs, TC1/TC2 testing.
View More
EN 10216-5 1.4941 Seamless Stainless Steel Tube | EN 10216-5 Stainless Steel - SHH STEEL

EN 10216-5 1.4941 Seamless Stainless Steel Tube

EN 10216-5 1.4941 / X6CrNiTiB18-10 seamless stainless pressure tube, austenitic creep-resisting, cast analysis per EN table, ambient Rp0.2 min 195 MPa, Rm 490–680, solution annealed at 1070–1150 °C. SHH STEEL can produce and supply with EN 10204 3.1 MTCs, TC1/TC2 testing.
View More
EN 10216-5 1.4959 Seamless Stainless Steel Tube | EN 10216-5 Stainless Steel - SHH STEEL

EN 10216-5 1.4959 Seamless Stainless Steel Tube

EN 10216-5 1.4959 / X8NiCrAlTi32-21 seamless stainless pressure tube (Alloy 800H / N08810), austenitic creep-resisting, cast analysis per EN table, ambient Rp0.2 min 170 MPa, Rm 500–750, solution annealed at 1150–1200 °C. SHH STEEL can produce and supply with EN 10204 3.1 MTCs, TC1/TC2 testing.
View More
EN 10216-5 1.4958 Seamless Stainless Steel Tube | EN 10216-5 Stainless Steel - SHH STEEL

EN 10216-5 1.4958 Seamless Stainless Steel Tube

EN 10216-5 1.4958 / X5NiCrAlTi31-20 seamless stainless pressure tube (Alloy 800 / N08800), austenitic creep-resisting, cast analysis per EN table, ambient Rp0.2 min 170 MPa, Rm 500–750, solution annealed at 1150–1200 °C. SHH STEEL can produce and supply with EN 10204 3.1 MTCs, TC1/TC2 testing.
View More
EN 10216-5 1.4918 Seamless Stainless Steel Tube | EN 10216-5 Stainless Steel - SHH STEEL

EN 10216-5 1.4918 Seamless Stainless Steel Tube

EN 10216-5 1.4918 / X6CrNiMo17-13-2 seamless stainless pressure tube (316H-type creep), austenitic creep-resisting, cast analysis per EN table, ambient Rp0.2 min 205 MPa, Rm 490–690, solution annealed at 1020–1100 °C. SHH STEEL can produce and supply with EN 10204 3.1 MTCs, TC1/TC2 testing.
View More
EN 10216-5 1.4912 Seamless Stainless Steel Tube | EN 10216-5 Stainless Steel - SHH STEEL

EN 10216-5 1.4912 Seamless Stainless Steel Tube

EN 10216-5 1.4912 / X7CrNiNb18-10 seamless stainless pressure tube (347H-type creep), austenitic creep-resisting, cast analysis per EN table, ambient Rp0.2 min 205 MPa, Rm 510–710, solution annealed at 1070–1125 °C. SHH STEEL can produce and supply with EN 10204 3.1 MTCs, TC1/TC2 testing.
View More
EN 10216-5 1.4940 Seamless Stainless Steel Tube | EN 10216-5 Stainless Steel - SHH STEEL

EN 10216-5 1.4940 Seamless Stainless Steel Tube

EN 10216-5 1.4940 / X7CrNiTi18-10 seamless stainless pressure tube (321H-type creep), austenitic creep-resisting, cast analysis per EN table, ambient Rp0.2 min 190 MPa, Rm 510–710, solution annealed at 1100–1150 °C. SHH STEEL can produce and supply with EN 10204 3.1 MTCs, TC1/TC2 testing.
View More
EN 10216-5 1.4948 Seamless Stainless Steel Tube | EN 10216-5 Stainless Steel - SHH STEEL

EN 10216-5 1.4948 Seamless Stainless Steel Tube

EN 10216-5 1.4948 / X6CrNi18-10 seamless stainless pressure tube (304H-type creep), austenitic creep-resisting, cast analysis per EN table, ambient Rp0.2 min 185 MPa, Rm 500–700, solution annealed at 1000–1080 °C. SHH STEEL can produce and supply with EN 10204 3.1 MTCs, TC1/TC2 testing.
View More

EN 10216-5 Stainless Steel Products

EN 10216-5 1.4982 Seamless Stainless Steel Tube EN 10216-5 1.4981 Seamless Stainless Steel Tube EN 10216-5 1.4988 Seamless Stainless Steel Tube EN 10216-5 1.4961 Seamless Stainless Steel Tube
EN 10216-5 1.4910 Seamless Stainless Steel Tube EN 10216-5 1.4941 Seamless Stainless Steel Tube EN 10216-5 1.4959 Seamless Stainless Steel Tube EN 10216-5 1.4958 Seamless Stainless Steel Tube
EN 10216-5 1.4918 Seamless Stainless Steel Tube EN 10216-5 1.4912 Seamless Stainless Steel Tube EN 10216-5 1.4940 Seamless Stainless Steel Tube EN 10216-5 1.4948 Seamless Stainless Steel Tube
EN 10216-5 1.4424 Seamless Stainless Steel Tube EN 10216-5 1.4507 Seamless Stainless Steel Tube EN 10216-5 1.4558 Seamless Stainless Steel Tube EN 10216-5 1.4563 Seamless Stainless Steel Tube
EN 10216-5 1.4335 Seamless Stainless Steel Tube EN 10216-5 1.4466 Seamless Stainless Steel Tube EN 10216-5 1.4580 Seamless Stainless Steel Tube EN 10216-5 1.4439 Seamless Stainless Steel Tube
EN 10216-5 1.4436 Seamless Stainless Steel Tube EN 10216-5 1.4529 Seamless Stainless Steel Tube EN 10216-5 1.4547 Seamless Stainless Steel Tube EN 10216-5 1.4501 Seamless Stainless Steel Tube
EN 10216-5 1.4362 Seamless Stainless Steel Tube EN 10216-5 1.4429 Seamless Stainless Steel Tube EN 10216-5 1.4435 Seamless Stainless Steel Tube EN 10216-5 1.4311 Seamless Stainless Steel Tube
EN 10216-5 1.4306 Seamless Stainless Steel Tube EN 10216-5 1.4410 Seamless Stainless Steel Tube EN 10216-5 1.4539 Seamless Stainless Steel Tube EN 10216-5 1.4550 Seamless Stainless Steel Tube
EN 10216-5 1.4541 Seamless Stainless Steel Tube EN 10216-5 1.4571 Seamless Stainless Steel Tube EN 10216-5 1.4462 Seamless Stainless Steel Tube EN 10216-5 1.4401 Seamless Stainless Steel Tube
EN 10216-5 1.4404 Seamless Stainless Steel Tube EN 10216-5 1.4307 Seamless Stainless Steel Tube EN 10216-5 1.4301 Seamless Stainless Steel Tube
Stainless Steel Pipes and Tubes supplier and exporter

Stainless Steel Pipes and Tubes

SHH STEEL, a premier Stainless Steel Pipes and Tubes exporter, produces and exports stainless steel pipes and tubes for chemical, marine, and food processing industries. Our seamless and welded products, like 304 and 316L (ASTM A312), ensure corrosion resistance and strength. With a 5,000-ton inventory, we deliver in 3–5 days, backed by SGS/TUV inspections and mill certificates. Choose SHH STEEL for seamless stainless steel pipes and custom solutions.

Stainless Steel Pipes and Tubes

SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

    *

    *

    *

    *


    X