ASTM A213 TP304H Stainless Steel Tube | ASTM A213 Stainless Steel - SHH STEEL

ASTM A213 TP304H Stainless Steel Tube

ASTM A213 TP304H / UNS S30409 seamless boiler, superheater and heat-exchanger tube with controlled carbon 0.04–0.10%, Cr 18.0–20.0%, Ni 8.0–11.0%, a 75/30 ksi Table 4 floor, hardness max 192 HBW / 90 HRB, 1900 °F solution anneal, and ASTM grain size No. 7 or coarser. SHH STEEL supplies cold-finished and hot-finished seamless tube with EN 10204 3.1 MTCs that report grain size.
Grade
TP304H / UNS S30409
Standard
ASTM A213 / A213M
Product form
Seamless boiler / superheater / heat-exchanger tube (cold-finished and hot-finished)
Size
Typical OD × min wall (or average wall) within ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD and ~0.015–0.500 in. [0.4–12.7 mm] wall; other diameters by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is ASTM A213 TP304H Stainless Steel Tube

ASTM A213 / A213M is the ASTM International product specification for seamless ferritic and austenitic alloy-steel boiler, superheater, and heat-exchanger tubes. Grade TP304H / UNS S30409 is the high-temperature carbon-controlled member of the 304 family: melting carbon is held in a 0.04–0.10% range (both a floor and a ceiling), chromium 18.0–20.0%, nickel 8.0–11.0%, and the heat-treatment path carries an ASTM grain-size requirement of No. 7 or coarser. That combination exists for creep-range boiler and superheater service — not as a synonym stamp for ordinary A213 TP304. Buyers who write “304H tube” still need to name A213 (or the separate ASME SA-213 adoption) on the purchase order so the mill applies H-grade chemistry, grain-size, test, and marking clauses.

SHH STEEL can supply ASTM A213 TP304H stainless steel tube as seamless cold-finished and hot-finished product in the usual boiler and heat-exchanger OD × wall / BWG band, shipped with EN 10204 3.1 mill test certificates that report the full ladle chemistry, the Table 4 tensile and hardness results, and the grain-size result for the heat-treatment lot. When a project also needs ASME Code Book marking, we dual-mark A213 / SA-213 on the same lengths only if the purchase order says so. Browse the grade family on the A213/A213M hub.

Commercially, TP304H tube is still called 304H, S30409, or H-grade 18-8 boiler tube; none of those shop names replace the ASTM grade on the MTC or stencil. Sister grades under the same ASTM standard include A213 TP304, A213 TP304L, A213 TP321H, A213 TP347H, and A213 TP316H. A213 covers seamless tube only — no welded or HCW manufacturing type — so cold-finished versus hot-finished is the process choice, not a WLD/HCW stencil letter.

Chemical Composition of A213 TP304H

Two chemistry layers matter for TP304H under ASTM A213. Melting (heat or ladle) analysis is mandatory for every heat; product analysis on finished tube applies only when Supplementary Requirement wording or the purchase order invokes it through ASTM A1016/A1016M. Product-analysis tolerances typically flow from ASTM A480/A480M Table A1.1. SHH STEEL reports actual ladle values — and product values when ordered — and does not advertise unpublished tighter catalogue windows. The carbon range is the first line a reviewer should check: TP304H is not “304 with a little more carbon” written as a max — it is a 0.04–0.10% band with both floor and ceiling.

The tables below reproduce the heat analysis for TP304H / UNS S30409, the product-analysis limits from A480 Table A1.1, and a short carbon/nickel snapshot against TP304L and TP304. Later A213 editions place austenitic stainless grades in Table 2 (older editions used Table 1); confirm the ordered edition on the purchase order.

Melting analysis (heat / ladle analysis)

Element TP304H (UNS S30409) melting analysis
Carbon (C) 0.04 – 0.10
Manganese (Mn) ≤ 2.00
Phosphorus (P) ≤ 0.045
Sulfur (S) ≤ 0.030
Silicon (Si) ≤ 1.00
Chromium (Cr) 18.0 – 20.0
Nickel (Ni) 8.0 – 11.0
Molybdenum (Mo) … (no requirement)
Nitrogen (N) … (no requirement)

Source: ASTM A213/A213M stainless chemistry table for Grade TP304H / UNS S30409 (public mill / specification summaries cross-checked — htpipe A213 PDF table text). Confirm the ordered edition. Where ellipses appear, the ordered edition sets no requirement for that element.

Product analysis — A480/A480M Table A1.1 tolerances applied

Element Melting Tolerance (A480 A1.1) Product analysis limit
Carbon (C) 0.04 – 0.10 0.01 under / over 0.03 – 0.11
Manganese (Mn) ≤ 2.00 0.04 over ≤ 2.04
Phosphorus (P) ≤ 0.045 0.010 over ≤ 0.055
Sulfur (S) ≤ 0.030 0.005 over ≤ 0.035
Silicon (Si) ≤ 1.00 0.05 over ≤ 1.05
Chromium (Cr) 18.0 – 20.0 0.20 under / over 17.80 – 20.20
Nickel (Ni) 8.0 – 11.0 0.10 under / 0.15 over 7.90 – 11.15

Carbon and nickel snapshot — TP304L / TP304 / TP304H

Element TP304L (S30403) TP304 (S30400) TP304H (S30409)
C ≤ 0.035 ≤ 0.08 0.04 – 0.10
Mn ≤ 2.00 ≤ 2.00 ≤ 2.00
Cr 18.0 – 20.0 18.0 – 20.0 18.0 – 20.0
Ni 8.0 – 12.0 8.0 – 11.0 8.0 – 11.0

Heats that also meet the TP304 carbon ceiling and overlapping nickel band can be dual-certified TP304/TP304H when tensile, hardness, and grain-size results clear both rows — ask for that dual marking on the PO rather than assuming it from a PMI gun. Dual TP304H/TP304L is not a meaningful path: the carbon bands do not overlap. Versus stabilized H grades such as A213 TP321H and A213 TP347H, TP304H has no titanium or niobium stabilization chemistry.

When product analysis is ordered, finished tube may read C 0.03–0.11%, Mn ≤2.04%, P ≤0.055%, S ≤0.035%, Si ≤1.05%, Cr 17.80–20.20%, and Ni 7.90–11.15%. Put any tighter project carbon floor or ceiling on the purchase order before the heat is selected — the H-grade carbon floor is intentional for elevated-temperature strength.

Mechanical Properties of A213 TP304H

ASTM A213 Table 4 sets the room-temperature tensile acceptance floor for TP304H at 75 ksi [515 MPa] tensile strength and 30 ksi [205 MPa] yield strength (0.2% offset), with elongation of 35% minimum in 2 in. or 50 mm — the same room-temperature pair as TP304. Hardness maximum is 192 HBW / 200 HV or 90 HRB, and hardness tests are part of lot acceptance under A213 (a point that differs from many A312 pipe rows for the same UNS number). What distinguishes the H grade mechanically in the product standard is the grain-size requirement: ASTM No. 7 or coarser, determined per heat-treatment lot under the ordered edition’s clause referencing ASTM E112.

Property TP304H requirement
Tensile strength, min (Table 4) 75 ksi [515 MPa]
Yield strength (0.2% offset), min (Table 4) 30 ksi [205 MPa]
Elongation in 2 in. or 50 mm, min (Table 4) 35%
Hardness, max (Table 4) 192 HBW / 200 HV or 90 HRB
Grain size ASTM No. 7 or coarser (per heat-treatment lot)

Source: ASTM A213/A213M Table 4 for TP304H / UNS S30409 and H-grade grain-size language (public specification summaries — htpipe A213 PDF heat-treatment table showing grain-size column “7” for TP304H; Peninsular mechanical-properties excerpt for A213 TP304H 75/30 ksi / 90 HRB). Mechanical property requirements do not apply to tubing smaller than 1/8 in. [3.2 mm] inside diameter or thinner than 0.015 in. [0.4 mm] wall. Flattening and flaring tests are also required on a lot basis.

Room-temperature tensile equality with TP304 is why dual 304/304H stock is attractive; elevated-temperature allowables in the design code, the carbon floor, and the coarse-grain requirement are why the H grade exists. A tensile-only MTC that omits grain size is incomplete for TP304H — ask for the E112 result on the certificate before releasing the heat to fabrication.

Dimensions and Tolerances

Dimensional supply for ASTM A213 TP304H is tube language — outside diameter × wall thickness (minimum wall or average wall) and, commercially, BWG / gauge — not ASME B36.19 pipe schedules as the primary size story. The sizes usually furnished under A213 run from about 1/8 in. [3.2 mm] inside diameter to 5 in. [127 mm] outside diameter, with minimum wall from about 0.015 to 0.500 in. [0.4 to 12.7 mm]; other diameters may be furnished when all other requirements are met. State on the purchase order whether wall is minimum or average — boiler and superheater datasheets almost always assume a minimum-wall reading.

Outside-diameter and wall variations follow ASTM A1016/A1016M as invoked by A213. Cold-finished tubes commonly hold tighter OD control; hot-finished tubes allow wider OD and wall windows. Permissible variations from a specified average wall for cold-finished tube are often summarized as ±10% of the specified average wall. Confirm the exact A1016 rows for the OD and finish route on the ordered edition.

Item Typical A213 TP304H dimensional practice
Product form Seamless only (cold-finished or hot-finished)
Usual size band ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD; wall ~0.015–0.500 in. [0.4–12.7 mm] min (or average wall if PO says so)
Wall basis Minimum wall (default for boiler / superheater) or average wall when specified
OD / wall tolerances Per ASTM A1016/A1016M for the finish route and size; cold-finished average wall often ±10%
Length Cut lengths for boiler / superheater / HX bundles, or mill random lengths by agreement
Secondary size note ASME B36.19 schedules may appear only when a buyer asks for a pipe-schedule cross-reference — not as the primary A213 size callout

Put the cut list, design metal temperature context, and end preparation on the enquiry so mill and stock lengths can be mixed efficiently. Minimum wall is a first-class A213 concept: if the datasheet assumes average wall, say so explicitly before the heat is rolled.

Equivalent Grades

Equivalence language around TP304H tube is often looser than a creep-range boiler purchase order can afford. ASTM A213 Grade TP304H / UNS S30409 is the governing designation for this article; EN 1.4948 and JIS SUS304H are approximate wrought names that point to similar high-temperature 18-8 families but are not automatic substitutes on an A213 mill test certificate. When a datasheet says “equivalent to 304H,” confirm which product standard, tensile/hardness table, grain-size clause, and heat-treatment path the mill will actually certify.

Designation Notes
ASTM A213 / A213M Grade TP304H Governing ASTM seamless boiler / HX tube product standard for this article
UNS S30409 Unified number listed in the stainless chemistry table
ASME SA-213 TP304H Separate ASME Code Book adoption — dual-mark only when the PO asks
EN 1.4948 (X6CrNi18-11) Approximate wrought H-grade designation; order EN tube forms under the relevant EN tube specs
JIS SUS304H / SUS304HTB Approximate Japanese grade / boiler-tube names; confirm the Japanese tube product standard
Related plate A240 / SA240 flat product in the same UNS family — order plate and tube under their own product standards

Dual A213/SA-213 marking is a purchase-order option, not a claim that the two standards are one document. Compare TP304, TP304L, and the stabilized H grades on their own ASTM A213 pages before swapping grades on a familiar “304” PMI reading alone.

Heat Treatment and Delivery Condition

TP304H under ASTM A213 is furnished solution treated at a minimum of 1900 °F [1040 °C], then quenched in water or cooled rapidly by other means at a rate sufficient to prevent carbide reprecipitation. The H-grade path also requires that grain size after heat treatment meet ASTM No. 7 or coarser for the heat-treatment lot. That combination — solution treatment plus coarse-grain control — is what separates TP304H paperwork from a tensile-only TP304 certificate. Both cold-finished and hot-finished seamless tube follow the heat-treatment requirement.

Cold-finished versus hot-finished is a process and dimensional route, not a substitute for the anneal or the grain-size check. Delivery condition for SHH STEEL TP304H is solution annealed and pickled (or bright annealed by agreement), with anneal temperature, quench method, and grain-size result stated on the EN 10204 3.1 certificate. Straightening after anneal is controlled so cold work does not undermine the coarse-grain objective at the ends.

Stabilizing heat treatments used on titanium- or niobium-bearing grades are not the TP304H route; if the process needs stabilization chemistry, open A213 TP321H or A213 TP347H instead of stretching 304H beyond its design intent. When Supplementary Requirement language for intergranular-corrosion capability is ordered, the corrosion test report travels with the heat-treatment and grain-size record.

Corrosion Resistance

TP304H’s chromium-rich passive film handles the oxidizing steam-side and many water-side duties typical of boiler and superheater service. It is not selected primarily as a wet-chloride corrosion grade: the carbon floor that helps elevated-temperature strength also raises as-welded sensitization risk relative to A213 TP304L. In chloride-bearing cooling waters and many process exchangers, pitting and crevice attack become limiting, and buyers usually step to A213 TP316 / A213 TP316L or a higher-PREN grade rather than stretching H-grade 18-8 into wet corrosive service.

ASTM A213 itself does not publish a corrosion-rate table for TP304H; selection remains engineering judgment against fluid, temperature, velocity, and inspection philosophy inside the boiler or exchanger. When a specification calls for ASTM A262 Practice E, write that Supplementary Requirement onto the purchase order. SHH STEEL will not market TP304H as a wet-service upgrade over TP304L — the H designation is about creep-range carbon and grain size, not about better aqueous corrosion resistance.

Applications of A213 TP304H Tube

TP304H seamless tube under A213 is chosen for creep-range boiler, superheater, and reheater service where the design code’s elevated-temperature allowables for S30409, the carbon floor, and the coarse-grain requirement earn their keep. It is the wrong default for as-welded wet corrosive exchangers that really need TP304L, and it is not a molybdenum grade for chlorides. The table below pairs typical application areas with a selection note.

Application area Typical use of TP304H tube Selection note
Boiler generating / screen tubes Seamless A213 tube where H-grade carbon and grain size are specified Confirm design metal temperature and code allowables for S30409
Superheater / reheater Creep-range steam tubing ordered to A213 TP304H For stabilized H grades open TP321H / TP347H; for fine-grain TP347HFG open that page
High-temperature process HX Seamless tube where elevated-temperature strength matters more than wet IGC Prefer TP304L if as-welded aqueous IGC is the driver
Dual TP304/TP304H stock Heats that clear both chemistry and grain-size / tensile rows Ask for dual marking on the PO — do not assume from PMI alone
General 18-8 boiler tube Where A213 documentation is preferred over pipe product forms Do not substitute A312 pipe paperwork for A213 tube acceptance

For as-welded intergranular resistance in wet service open A213 TP304L; for stabilized high-temperature service open A213 TP321H / A213 TP347H; for molybdenum H-grade open A213 TP316H on the A213/A213M hub.

Weldability

TP304H tube welds with matching or near-matching austenitic filler for tube-to-tubesheet joints, attachment welds, and fabrication joins. Common practice uses ER308H / ER308 (or equivalent covered electrodes) under a qualified WPS so weld-metal carbon supports elevated-temperature service; many fabricators avoid defaulting to ER308L when the base tube is H-grade and the design allowables assume H-grade carbon. Heat input control, interpass limits, and post-weld cleaning remain the fabricator’s responsibility under the applicable boiler or pressure-vessel code — A213 governs the seamless tube product, not the field or shop weld procedure.

Because A213 TP304H is seamless, there is no mill longitudinal weld to radiograph the way welded pipe standards describe. Focus inspection language on tube integrity (hydro or NDE of each length), tube-to-tubesheet joint quality, grain-size documentation on the base metal, and any contractual corrosion test. For tube that will enter wet as-welded service in a sensitizing environment, many owners change the base metal to A213 TP304L rather than relying on H-grade carbon in aqueous IGC duty. Specify end preparation and surface finish on the tube PO when orbital or clean-service joins are planned.

Surface Finishes

Standard mill delivery for ASTM A213 TP304H is solution annealed and pickled, leaving a clean matte finish suitable for most boiler and heat-exchanger tube duty. Bright annealing under protective atmosphere produces a smoother reflective surface used on some clean-process lines and must be called out because it changes the heat-treatment route — and must still deliver the required grain size. Light polish or specified Ra on the bore or OD is a commercial or service-center operation on top of A213 product, not automatic with the grade stamp.

When a fouling-sensitive exchanger specification quotes an Ra maximum on the bore, put it on the tube purchase order with its own acceptance language and sampling plan. SHH STEEL stencils grade, heat treatment, and (on request) H-grade identity as standard requirements; polish, special OD grind, and passivation after fabrication remain commercial extras unless the contract says otherwise. Order end preparation together with finish so receiving inspection shares one acceptance language.

Inspection and Testing

Base ASTM A213 testing for TP304H includes heat analysis (with carbon inside the 0.04–0.10% band), tension tests to the Table 4 floors (75/30 ksi), hardness tests to the Table 4 maximum (192 HBW / 90 HRB), grain-size determination (ASTM No. 7 or coarser) per heat-treatment lot, flattening and flaring tests on a lot basis, and either hydrostatic testing or nondestructive electric testing of each length. The manufacturer may choose hydro versus NDE unless the purchase order fixes the method. Marking includes the ASTM designation, grade, size, heat number, and other clause-required data.

Supplementary Requirements commonly added on TP304H tube orders are summarized below. Invoke them by number or clear purchase-order wording; mills will not assume product analysis, IGC testing, or dual TP304/TP304H marking from a verbal “full certs” note.

Option Purpose
Product analysis Confirms chemistry on finished tube — useful when carbon sits near the 0.04% floor or 0.10% ceiling
Intergranular corrosion A262 Practice E (or agreed practice) as a contractual Supplementary Requirement
Grain-size reporting Ensures E112 result appears on the MTC for the heat-treatment lot
Minimum vs average wall States which wall basis the size callout uses
Fixed hydro or NDE method Removes manufacturer’s option when the end user mandates one route
Third-party inspection / EN 10204 3.2 Witnessed testing and certificate when the project requires it

Ask the mill to state lot identity clearly on the certificate so hardness, tension, and grain-size specimens map cleanly to the bundle you receive. A tensile-only MTC without grain size is incomplete for TP304H.

Packaging and Shipping

TP304H tube leaves SHH STEEL bundled, capped or end-protected, and tagged for export or domestic delivery according to the length mix and bend form on the order. Bundle tags repeat the ASTM A213 grade, OD × wall (or BWG), heat number, and PO reference so site receiving can check the shipment without opening every certificate packet first. U-bent tubes need extra cradle or case protection so bend radii and legs are not distorted in transit.

Export packing can be bare bundles, wrapped bundles, or wooden-cased lengths for bright-annealed, polished, or small-bore material. We ship under the Incoterms on the order acknowledgement — FOB, CFR, CIF, EXW, or other agreed terms. Inland trucking, bilingual destination marks, or project color coding for bundle tags should be stated on the enquiry beside the metallurgical notes.

Why Choose SHH STEEL

SHH STEEL treats ASTM A213 TP304H as a product standard with enforceable chemistry (carbon floor and ceiling), tensile, hardness, grain-size, heat-treatment, and marking rules — not as a catalogue nickname for “any 304H tube.” The MTC reports the full ladle chemistry, the Table 4 tensile/hardness set (75/30 ksi, 192 HBW / 90 HRB), and the grain-size result; the stencil carries seamless tube identity under A213; and dual A213/SA-213 marking is offered only when requested.

We keep the H-grade conversation honest for boiler and HX duty. If as-welded aqueous IGC is the driver, we steer toward A213 TP304L. If the datasheet does not need H-grade carbon or grain size, we open A213 TP304. If stabilization chemistry is required, we open A213 TP321H / A213 TP347H. If chlorides dominate, we open A213 TP316 / A213 TP316H. The A213/A213M hub is organized grade by grade under ASTM, seamless tube only.

Lead times combine near-term stock lengths with mill schedules; we say which is which on the quotation. Cut-to-length, U-bending, polish, and third-party inspection are defined extras. The tube that arrives should match the ASTM callout the engineer wrote, with paperwork a third-party inspector can read without translation.

Supply Capability

SHH STEEL can supply ASTM A213 TP304H stainless steel tube against the edition and finish route named on your enquiry. The capability table below summarizes the sizes, finishes, and documents we regularly quote for this grade, followed by the Stock / Available sizes map buyers ask for when they need a quick sense of what to enquire against for boiler and superheater duty.

Item SHH STEEL capability for TP304H
Standard ASTM A213 / A213M (dual SA-213 marking on request) Grade TP304H / UNS S30409
Product form Seamless only — cold-finished and hot-finished
Size Typical OD × min wall (or average wall) in the A213 usual band; other diameters by agreement
Wall / gauge Minimum wall or average wall; BWG / gauge callouts accepted on enquiry
Length Cut-to-length for boiler / superheater / HX bundles; mill random by agreement; U-bends on enquiry
Finish Annealed and pickled; bright annealed or light polish by agreement
Testing Tension (75/30 ksi), hardness (max 192 HBW / 90 HRB), grain size No. 7 or coarser, flattening, flaring, hydro or NDE per length; full ladle chemistry on MTC; product analysis / IGC on order
Documents EN 10204 3.1 with full ladle chemistry and grain-size result; third-party inspection / 3.2 on request
Trade terms FOB / CFR / CIF / EXW and other agreed Incoterms

Stock / Available sizes

SHH STEEL quotes TP304H tube against a practical stock-and-mill enquiry range rather than a frozen warehouse SKU list. The sizes below are OD × wall / BWG combinations buyers most often request for boiler and superheater tube in the H-grade 18-8 family; availability of any single line on a given week depends on mill drawing and our inbound schedule, so treat the table as a supply map for enquiry — not a guarantee of floor tonnage.

Item Typical stock / enquiry range for TP304H
Outside diameter 25.4, 31.8, 38.1, 44.5, 50.8, 63.5, 76.2, 88.9 mm (and other boiler/HX ODs on enquiry; up through the usual A213 ~5 in. [127 mm] band)
Wall / BWG BWG 10–16 class walls and metric min-wall equivalents; heavier walls for high-pressure boiler duty by agreement
Common OD × wall examples 31.8 × 2.77 mm; 38.1 × 3.05 mm; 50.8 × 3.05 mm; 50.8 × 3.40 mm; 63.5 × 3.40 mm; 76.2 × 3.40 mm — illustrative boiler/HX sizes, confirm min vs average wall
Length Cut lengths for boiler / superheater / exchanger bundles; U-bends and straight random lengths on enquiry
Special Non-standard OD/wall, bright anneal, dual TP304/TP304H marking, dual A213/SA-213 marking — confirm on enquiry before the heat is reserved

When you send an enquiry, list OD × wall (or BWG), wall basis (minimum or average), cold-finished or hot-finished preference, quantity or cut list, required marking (A213 alone, dual A213/SA-213, and/or dual TP304/TP304H), and any Supplementary Requirements. We reply with what we can ship from near-term stock versus what needs a mill run, without inventing fake warehouse codes or tonnage claims.

Send the size list, finish route, quantity or cut lengths, required marking, Supplementary Requirements, and destination on one enquiry. We will confirm chemistry (including the carbon band), tensile, hardness, and grain size against the stainless chemistry table, Table 4, and the H-grade grain-size rule, state what ships from near-term availability versus mill production, and keep the offer aligned with ASTM A213 / A213M. Related grades such as A213 TP304, A213 TP347H, and A213 UNS S30432 sit on the same hub when the datasheet steps beyond TP304H.

FAQ

Is ASTM A213 the same as ASME SA-213 for TP304H?
No. ASTM A213 / A213M is the ASTM International product specification for seamless boiler, superheater, and heat-exchanger tubes; ASME SA-213 / SA-213M is the separate ASME Code Book adoption of that grade text. Chemistry, tensile, hardness, and grain-size rules align closely for a given referenced edition, but they remain two independent standards. Dual-mark A213/SA-213 tube only when the purchase order asks for both names on the stencil and MTC.
Does ASTM A213 TP304H include welded or HCW tube?
No. ASTM A213 covers seamless tube only. There is no WLD or HCW manufacturing type under this product standard the way ASTM A312 describes pipe. The process choice for TP304H under A213 is cold-finished versus hot-finished seamless tube, plus the H-grade heat-treatment, grain-size, and testing clauses of the ordered edition.
How does TP304H differ from TP304 under ASTM A213?
TP304H holds carbon in a 0.04–0.10% range (floor and ceiling) and requires ASTM grain size No. 7 or coarser after solution treatment. TP304 allows carbon ≤0.08% with no H-grade grain-size rule in the product standard. Room-temperature Table 4 tensile (75/30 ksi) and hardness (192 HBW / 90 HRB) match; elevated-temperature allowables, carbon floor, and grain size are why the H designation exists. Do not treat "304H" as a synonym stamp for ordinary TP304 on the MTC.
What is the UNS number and chemistry of ASTM A213 TP304H?
TP304H is UNS S30409. Melting limits include carbon 0.04–0.10%, manganese ≤2.00%, phosphorus ≤0.045%, sulfur ≤0.030%, silicon ≤1.00%, chromium 18.0–20.0%, and nickel 8.0–11.0%, with molybdenum and nitrogen as no-requirement ellipses. Product-analysis limits apply only when ordered, typically from A480 Table A1.1 via A1016. Confirm the ordered A213 edition for the exact stainless-table number.
Does A213 Table 4 set a hardness limit for TP304H?
Yes. Table 4 for TP304H lists tensile strength, yield strength, elongation, and a hardness maximum of 192 HBW / 200 HV or 90 HRB. Hardness tests are part of lot acceptance under A213, which differs from many A312 pipe rows for the same UNS number that omit a Table 4 hardness cap. Grain size (No. 7 or coarser) sits beside those Table 4 numbers as an H-grade acceptance item.
Why does ASTM A213 control grain size on TP304H?
Coarse grain (ASTM No. 7 or coarser) after the 1900 °F [1040 °C] solution treatment supports the elevated-temperature creep-rupture behavior that the H designation is written for. A tensile-only MTC without an E112 grain-size result is incomplete for TP304H. Ask the mill to report grain size per heat-treatment lot on the EN 10204 3.1 certificate before releasing the heat to fabrication.
Can TP304H tube be dual certified TP304/TP304H?
Yes when ladle carbon meets the H-grade band while also clearing the TP304 carbon ceiling, and when tensile, hardness, and grain-size results clear both acceptance paths. Dual TP304H/TP304L is not meaningful because the carbon bands do not overlap. Spell the required dual marking on the enquiry so the heat is selected correctly.
TP304H vs TP304L — which A213 tube should I order?
Order TP304H when the boiler or superheater datasheet needs H-grade carbon, grain-size controls, and creep-range framing. Order TP304L when as-welded intergranular resistance in wet or sensitizing service is the driver and the lower 70/25 ksi floor is acceptable. They solve different problems — do not swap them on a familiar "304" PMI reading alone.
What heat treatment does ASTM A213 require for TP304H?
TP304H is solution treated at a minimum of 1900 °F [1040 °C] and then water quenched or rapidly cooled to prevent carbide reprecipitation, with grain size No. 7 or coarser for the heat-treatment lot. Both cold-finished and hot-finished seamless tube follow that path. Ask the mill to state anneal temperature, quench method, and grain-size result on the EN 10204 3.1 certificate.
Minimum wall vs average wall — which should I order for A213 TP304H?
Order minimum wall when the boiler or superheater datasheet is written around a guaranteed minimum thickness after tolerance — the usual practice for A213 H-grade tube. Order average wall only when the purchase order explicitly allows average-wall product and the designer has accepted that basis. Put the wall basis on the enquiry before the mill selects A1016 tolerance tables.
Is TP304H a good choice for wet corrosive heat-exchanger service?
Usually no as a first choice. The carbon floor that helps elevated-temperature strength raises as-welded sensitization risk relative to TP304L, and TP304H carries no molybdenum for chloride pitting. Prefer TP304L for as-welded aqueous IGC duty and TP316/TP316L when chlorides dominate; reserve TP304H for creep-range boiler and superheater framing where the H designation earns its keep.
Hydrostatic test vs NDE — which do I get on TP304H tube?
ASTM A213 requires each tube to be hydrostatically tested or nondestructively electrically tested. The manufacturer may choose the method unless the purchase order fixes one. Neither route is an informal upgrade over the other inside the product standard. State the preferred method on the enquiry if your end user or inspector mandates hydro only or a named NDE technique.

Conclusion

ASTM A213 TP304H / UNS S30409 is the carbon-controlled, coarse-grain seamless stainless steel tube grade for creep-range boiler, superheater, and heat-exchanger service when elevated-temperature allowables, a 0.04–0.10% carbon band, and ASTM grain size No. 7 or coarser share one datasheet. SHH STEEL supplies cold-finished and hot-finished seamless tube in the usual OD × wall / BWG band, solution annealed, tested to Table 4 tensile and hardness limits with grain size reported, and documented on EN 10204 3.1 certificates — with dual SA-213 marking only when the order asks for that separate ASME standard. For sister grades and stock-oriented size discussions, start from the A213/A213M hub, then send your OD × wall list, wall basis, dual-marking needs, and grain-size / marking requirements so we can align mill and near-term availability to the ASTM callout.

Contact: admin@steelspecs.com

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X