ASTM A213 TP316H Stainless Steel Tube | ASTM A213 Stainless Steel - SHH STEEL

ASTM A213 TP316H Stainless Steel Tube

ASTM A213 TP316H / UNS S31609 seamless boiler, superheater and heat-exchanger tube with controlled carbon 0.04–0.10%, Cr 16.0–18.0%, Ni 11.0–14.0%, Mo 2.00–3.00%, a 75/30 ksi Table 4 floor, hardness max 192 HBW / 90 HRB, 1900 °F solution anneal, and ASTM grain size No. 7 or coarser. SHH STEEL supplies cold-finished and hot-finished seamless tube with EN 10204 3.1 MTCs that report grain size and molybdenum.
Grade
TP316H / UNS S31609
Standard
ASTM A213 / A213M
Product form
Seamless boiler / superheater / heat-exchanger tube (cold-finished and hot-finished)
Size
Typical OD × min wall (or average wall) within ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD and ~0.015–0.500 in. [0.4–12.7 mm] wall; other diameters by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is ASTM A213 TP316H Stainless Steel Tube

ASTM A213 / A213M is the ASTM International product specification for seamless ferritic and austenitic alloy-steel boiler, superheater, and heat-exchanger tubes. Grade TP316H / UNS S31609 is the high-temperature carbon-controlled member of the molybdenum-bearing 316 family: melting carbon is held in a 0.04–0.10% range (both a floor and a ceiling), chromium 16.0–18.0%, nickel 11.0–14.0%, molybdenum 2.00–3.00%, and the heat-treatment path carries an ASTM grain-size requirement of No. 7 or coarser. That combination exists for creep-range boiler and superheater service that still needs molybdenum — not as a synonym stamp for ordinary A213 TP316, and not as a dual of A213 TP304H with “a little Mo.”

SHH STEEL can supply ASTM A213 TP316H stainless steel tube as seamless cold-finished and hot-finished product in the usual boiler and heat-exchanger OD × wall / BWG band, shipped with EN 10204 3.1 mill test certificates that report the full ladle chemistry including molybdenum, the Table 4 tensile and hardness results, and the grain-size result for the heat-treatment lot. When a project also needs ASME Code Book marking, we dual-mark A213 / SA-213 on the same lengths only if the purchase order says so. Browse the grade family on the A213/A213M hub.

Commercially, TP316H tube is still called 316H, S31609, or H-grade Mo boiler tube; none of those shop names replace the ASTM grade on the MTC or stencil. Sister grades under the same ASTM standard include A213 TP316, A213 TP316L, A213 TP304H, A213 TP321H, and A213 TP347H. A213 covers seamless tube only — no welded or HCW manufacturing type — so cold-finished versus hot-finished is the process choice, not a WLD/HCW stencil letter.

Chemical Composition of A213 TP316H

Two chemistry layers matter for TP316H under ASTM A213. Melting (heat or ladle) analysis is mandatory for every heat; product analysis on finished tube applies only when Supplementary Requirement wording or the purchase order invokes it through ASTM A1016/A1016M. Product-analysis tolerances typically flow from ASTM A480/A480M Table A1.1. The carbon range is the first line a reviewer should check: TP316H is not “316 with a little more carbon” written as a max — it is a 0.04–0.10% band with both floor and ceiling. The second line is molybdenum 2.00–3.00%, required the same way it is on TP316. The third line often missed: nickel starts at 11.0% on TP316H, not at the 10.0% floor used on TP316 / TP316L.

The tables below reproduce the heat analysis for TP316H / UNS S31609, the product-analysis limits from A480 Table A1.1, and a short carbon/nickel/molybdenum snapshot against TP316L and TP316. Later A213 editions place austenitic stainless grades in Table 2 (older editions used Table 1); confirm the ordered edition on the purchase order.

Melting analysis (heat / ladle analysis)

Element TP316H (UNS S31609) melting analysis
Carbon (C) 0.04 – 0.10
Manganese (Mn) ≤ 2.00
Phosphorus (P) ≤ 0.045
Sulfur (S) ≤ 0.030
Silicon (Si) ≤ 1.00
Chromium (Cr) 16.0 – 18.0
Nickel (Ni) 11.0 – 14.0
Molybdenum (Mo) 2.00 – 3.00
Nitrogen (N) … (no requirement; analysis method by agreement when reported)

Source: ASTM A213/A213M stainless chemistry table for Grade TP316H / UNS S31609 (public mill / specification PDF excerpt — _ref_a213.txt / A213–13 table text). Confirm the ordered edition. Where ellipses appear, the ordered edition sets no requirement for that element.

Product analysis — A480/A480M Table A1.1 tolerances applied

Element Melting Tolerance (A480 A1.1) Product analysis limit
Carbon (C) 0.04 – 0.10 0.01 under / over 0.03 – 0.11
Manganese (Mn) ≤ 2.00 0.04 over ≤ 2.04
Phosphorus (P) ≤ 0.045 0.010 over ≤ 0.055
Sulfur (S) ≤ 0.030 0.005 over ≤ 0.035
Silicon (Si) ≤ 1.00 0.05 over ≤ 1.05
Chromium (Cr) 16.0 – 18.0 0.20 under / over 15.80 – 18.20
Nickel (Ni) 11.0 – 14.0 0.10 under / 0.15 over 10.90 – 14.15
Molybdenum (Mo) 2.00 – 3.00 0.05 under / 0.10 over 1.95 – 3.10

Carbon, nickel and molybdenum snapshot — TP316L / TP316 / TP316H

Element TP316L (S31603) TP316 (S31600) TP316H (S31609)
C ≤ 0.035 ≤ 0.08 0.04 – 0.10
Cr 16.0 – 18.0 16.0 – 18.0 16.0 – 18.0
Ni 10.0 – 14.0 10.0 – 14.0 11.0 – 14.0
Mo 2.00 – 3.00 2.00 – 3.00 2.00 – 3.00

Heats that also meet the TP316 carbon ceiling and overlapping chemistry can be dual-certified TP316/TP316H when tensile, hardness, and grain-size results clear both rows — ask for that dual marking on the PO rather than assuming it from a PMI gun. Note the nickel floor: a heat at 10.5% Ni can clear TP316 but fails TP316H’s 11.0% minimum. Dual TP316H/TP316L is not a meaningful path: the carbon bands do not overlap. Versus A213 TP304H, TP316H adds mandatory molybdenum and uses the 16–18 / 11–14 Cr–Ni balance instead of 18–20 / 8–11.

When product analysis is ordered, finished tube may read C 0.03–0.11%, Mn ≤2.04%, P ≤0.055%, S ≤0.035%, Si ≤1.05%, Cr 15.80–18.20%, Ni 10.90–14.15%, and Mo 1.95–3.10%. Put any tighter project carbon floor or molybdenum floor on the purchase order before the heat is selected — the H-grade carbon floor is intentional for elevated-temperature strength.

Mechanical Properties of A213 TP316H

ASTM A213 Table 4 sets the room-temperature tensile acceptance floor for TP316H at 75 ksi [515 MPa] tensile strength and 30 ksi [205 MPa] yield strength (0.2% offset), with elongation of 35% minimum in 2 in. or 50 mm — the same room-temperature pair as TP316, not the lower L-grade floors. Hardness maximum is 192 HBW / 200 HV or 90 HRB, and hardness tests are part of lot acceptance under A213. What distinguishes the H grade mechanically in the product standard is the grain-size requirement: ASTM No. 7 or coarser, determined per heat-treatment lot under the ordered edition’s clause referencing ASTM E112.

Property TP316H requirement
Tensile strength, min (Table 4) 75 ksi [515 MPa]
Yield strength (0.2% offset), min (Table 4) 30 ksi [205 MPa]
Elongation in 2 in. or 50 mm, min (Table 4) 35%
Hardness, max (Table 4) 192 HBW / 200 HV or 90 HRB
Grain size ASTM No. 7 or coarser (per heat-treatment lot)

Source: ASTM A213/A213M Table 4 for TP316H / UNS S31609 and H-grade grain-size language (public specification PDF excerpt — _ref_a213.txt heat-treatment table showing grain-size column “7” for TP316H). Mechanical property requirements do not apply to tubing smaller than 1/8 in. [3.2 mm] inside diameter or thinner than 0.015 in. [0.4 mm] wall. Flattening and flaring tests are also required on a lot basis.

Room-temperature tensile equality with TP316 is why dual 316/316H stock is attractive when the heat also clears the H-grade carbon floor, the 11% nickel floor, and the grain-size rule; elevated-temperature allowables in the design code, the carbon floor, and the coarse-grain requirement are why the H grade exists. A tensile-only MTC that omits grain size or molybdenum is incomplete for TP316H — ask for the E112 result and Mo on the certificate before releasing the heat to fabrication.

Dimensions and Tolerances

Dimensional supply for ASTM A213 TP316H is tube language — outside diameter × wall thickness (minimum wall or average wall) and, commercially, BWG / gauge — not ASME B36.19 pipe schedules as the primary size story. The sizes usually furnished under A213 run from about 1/8 in. [3.2 mm] inside diameter to 5 in. [127 mm] outside diameter, with minimum wall from about 0.015 to 0.500 in. [0.4 to 12.7 mm]; other diameters may be furnished when all other requirements are met. State on the purchase order whether wall is minimum or average — boiler and superheater datasheets almost always assume a minimum-wall reading.

Outside-diameter and wall variations follow ASTM A1016/A1016M as invoked by A213. Cold-finished tubes commonly hold tighter OD control; hot-finished tubes allow wider OD and wall windows. Permissible variations from a specified average wall for cold-finished tube are often summarized as ±10% of the specified average wall. Confirm the exact A1016 rows for the OD and finish route on the ordered edition.

Item Typical A213 TP316H dimensional practice
Product form Seamless only (cold-finished or hot-finished)
Usual size band ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD; wall ~0.015–0.500 in. [0.4–12.7 mm] min (or average wall if PO says so)
Wall basis Minimum wall (default for boiler / superheater) or average wall when specified
OD / wall tolerances Per ASTM A1016/A1016M for the finish route and size; cold-finished average wall often ±10%
Length Cut lengths for boiler / superheater / HX bundles, or mill random lengths by agreement
Secondary size note ASME B36.19 schedules may appear only when a buyer asks for a pipe-schedule cross-reference — not as the primary A213 size callout

Put the cut list, design metal temperature context, and end preparation on the enquiry so mill and stock lengths can be mixed efficiently. Minimum wall is a first-class A213 concept: if the datasheet assumes average wall, say so explicitly before the heat is rolled.

Equivalent Grades

Equivalence language around 316H tube often collapses plate, cast, and tube product forms into one nickname, or treats TP316H as “TP304H with molybdenum.” ASTM A213 Grade TP316H / UNS S31609 is the governing designation for this article; EN and JIS wrought names that point to similar Mo-bearing H-grade chemistry families are not automatic substitutes on an A213 MTC.

Designation Notes
ASTM A213 / A213M Grade TP316H Governing ASTM seamless boiler / HX tube product standard for this article
UNS S31609 Unified number in the stainless chemistry table
ASME SA-213 TP316H Separate ASME Code Book adoption — dual-mark only when the PO asks
Related standard 316 A213 TP316 — C ≤0.08, Ni 10–14, no grain-size mandate
Related L-grade A213 TP316L — C ≤0.035, lower tensile floors, no H carbon floor
Related 304H A213 TP304H — H-grade without Mo; different Cr–Ni
Related plate A240 / SA240 flat product in the 316 family — order plate and tube under their own standards

Dual A213/SA-213 marking is a purchase-order option. Compare TP316, TP316L, and TP304H on their own ASTM A213 pages before swapping H-grade Mo tube inside a boiler list.

Heat Treatment and Delivery Condition

TP316H under ASTM A213 is furnished solution treated at a minimum of 1900 °F [1040 °C], then quenched in water or cooled rapidly by other means. The heat-treatment table carries the ASTM grain-size requirement of No. 7 or coarser for the heat-treatment lot. That heat-treatment row applies to both cold-finished and hot-finished seamless tube. Skipping or under-cooling the solution treatment can leave a structure that fails the grain-size check or sensitizes in service even when ladle chemistry looked acceptable on paper.

Cold-finished versus hot-finished is a process and dimensional route, not a substitute for the anneal or the grain-size check. Delivery condition for SHH STEEL TP316H is solution annealed and pickled (or bright annealed by agreement), with anneal temperature, quench method, molybdenum result, and E112 grain-size result on the EN 10204 3.1 certificate. Straightening, cutting, and end finishing follow heat treatment.

Unlike stabilized H grades such as A213 TP321H and A213 TP347H, TP316H has no titanium or niobium stabilization chemistry and is not listed under Supplementary Requirement S2 in the public A213 excerpt used for this pack. If a project datasheet asks for a stabilizing hold or A262 Practice E on 316H, put that requirement on the purchase order rather than assuming base A213 includes it.

Corrosion Resistance

TP316H inherits molybdenum’s contribution to pitting and crevice resistance from the 316 family while adding H-grade carbon and grain-size controls for creep-range lists. The 2.00–3.00% Mo band is why buyers step up from A213 TP304H when chloride-leaning or process-side aqueous corrosion sits beside elevated metal temperature. It is still not an L-grade: the intentional 0.04–0.10% carbon floor means as-welded intergranular corrosion risk after tube-to-tubesheet welding needs separate review — many owners use TP316L for as-welded IGC duty and reserve TP316H for creep-range sections that need the carbon floor.

ASTM A213 itself does not publish a corrosion-rate table for TP316H; selection remains engineering judgment against fluid, temperature, velocity, and inspection philosophy. When a specification calls for ASTM A262 Practice E, write that Supplementary Requirement onto the purchase order so the test is contractual rather than assumed from a verbal “full certs” note. SHH STEEL will not rank TP316H as equal to higher-Mo grades in severe chlorides — that claim is not supported by the product standard.

Applications of A213 TP316H Tube

Because TP316H combines molybdenum with H-grade carbon and grain-size controls, it shows up in creep-range boiler and superheater tubing where Mo is required, process heat exchangers at elevated metal temperature with chloride-leaning fluids, and Code-driven lists that name 316H rather than stretching standard TP316 or TP304H beyond their intended framing. The table below pairs typical application areas with a selection note so the grade is chosen for temperature, fluid, and fabrication route — not only for the familiar “316H” name on the BOM.

Application area Typical use of TP316H tube Selection note
Boiler and superheater Creep-range seamless generating and superheater tubing ordered to A213 with Mo Confirm design metal temperature and grain-size reporting on MTC
High-temperature process HX Straight and U-bend HX tubes where Mo and H-grade controls are both named State min vs average wall, BWG, and bend radius on the enquiry
Chloride-leaning elevated-temp service When TP304H lacks Mo and standard TP316 lacks H-grade carbon/grain-size Not a substitute for higher-Mo alloys in severe brine
As-welded IGC-critical joins Usually prefer TP316L rather than TP316H Carbon floor on H grade works against as-welded IGC strategy
General Mo boiler tube without H package Stay on TP316 when grain-size/carbon floor not required Do not over-specify H grade for non-creep lists

For as-welded tube-to-tubesheet joints in sensitizing service consider A213 TP316L; for creep-range without molybdenum open A213 TP304H; for stabilized H-grade lists open TP321H / TP347H on the same A213/A213M hub.

Weldability

TP316H tube welds readily with matching or near-matching molybdenum-bearing austenitic filler for tube-to-tubesheet joints, attachment welds, and fabrication joins. Common practice uses ER316 / ER316H (or equivalent covered electrodes) under a qualified WPS; some fabricators prefer ER316H deposits to keep weld-metal carbon aligned with the H-grade base metal. Heat input control, interpass limits, and post-weld cleaning remain the fabricator’s responsibility under the applicable boiler or pressure-vessel code — A213 governs the seamless tube product, not the field or shop weld procedure.

Because A213 TP316H is seamless, there is no mill longitudinal weld to radiograph the way welded pipe standards describe. Focus inspection language on tube integrity (hydro or NDE of each length), tube-to-tubesheet joint quality, and any contractual corrosion test on the base metal. For tube that will enter service as-welded in a sensitizing environment, many owners change the base metal to A213 TP316L rather than relying on a perfect weld procedure alone to protect H-grade carbon TP316H. Specify end preparation and surface finish on the tube PO when orbital or clean-service joins are planned.

Surface Finishes

Standard mill delivery for ASTM A213 TP316H is solution annealed and pickled, leaving a clean matte finish suitable for most boiler and heat-exchanger tube duty. Bright annealing under protective atmosphere produces a smoother reflective surface used on some clean-process and instrumentation tube lines and must be called out because it changes the heat-treatment route. Light polish or specified Ra on the bore or OD is a commercial or service-center operation on top of A213 product, not automatic with the grade stamp.

When a hygienic or fouling-sensitive exchanger specification quotes an Ra maximum on the bore, put it on the tube purchase order with its own acceptance language and sampling plan. SHH STEEL stencils grade and heat treatment as standard requirements; polish, special OD grind, and passivation after fabrication remain commercial extras unless the contract says otherwise. End preparation (plain, slightly beveled, or as needed for tube expanding) should be ordered together with finish so receiving inspection shares one acceptance language.

Inspection and Testing

Lot testing for ASTM A213 TP316H follows tension, hardness, flattening, and flaring under A213 / A1016, plus ASTM grain-size determination (E112) for the heat-treatment lot. Chemistry verification must include the 0.04–0.10% carbon band, the 11.0–14.0% nickel floor, and molybdenum 2.00–3.00%. NDE follows the ordered edition and purchaser supplements — hydrostatic testing or non-destructive electric testing of each length is the usual A213 path unless the purchase order states otherwise.

EN 10204 3.1 certificates from SHH STEEL report ladle chemistry with Mo, Table 4 tensile and hardness, heat-treatment condition, and grain-size result. When A262 Practice E is ordered, those results appear as specified. Dual A213/SA-213 marking and third-party witness are available when written into the enquiry. A certificate missing molybdenum or grain size is not a complete TP316H release package.

Packaging and Shipping

TP316H tubes ship in capped or plugged bundles with weather protection matched to the route. Cut lengths for boiler and exchanger bundles are labeled by heat and size; export packing uses cases or steel-frame crates when required.

Marking includes ASTM A213, grade TP316H / UNS S31609, size, heat number, and SHH STEEL identification. Dual SA-213 marking appears only when the purchase order requests it. Packing lists track the same heat numbers shown on the EN 10204 3.1 certificates, including grain-size lot identity where applicable.

Why Choose SHH STEEL

SHH STEEL treats ASTM A213 TP316H as an H-grade molybdenum specification product: carbon band 0.04–0.10%, nickel floor 11.0%, Mo 2–3%, Table 4 75/30 ksi floors, and grain size No. 7 or coarser are checked together before a heat is offered. Quotations state OD × wall / BWG, wall basis, finish route, A262 options, and whether dual A213/SA-213 marking is required.

We refuse nickname assemblies that stamp TP316 or TP304H as 316H without the missing carbon floor, nickel floor, molybdenum, or grain-size controls. EN 10204 3.1 documentation includes Mo and E112 grain size. Compare sisters on the A213/A213M hub before freezing the boiler or exchanger tube list.

Supply Capability

SHH STEEL supplies ASTM A213 TP316H seamless stainless steel tube in cold-finished and hot-finished routes across the usual boiler, superheater, and heat-exchanger OD × wall / BWG band. Capability below is an enquiry range — not a frozen warehouse SKU or tonnage claim.

Capability SHH STEEL practice for TP316H
Product form Seamless cold-finished and hot-finished tube
Standards ASTM A213 / A213M; dual SA-213 when PO asks
Size band Typical within ~1/8 in. ID to 5 in. OD; other diameters by agreement
Wall basis Minimum wall or average wall as specified
Documentation EN 10204 3.1 MTC with Mo + grain-size result; A262 / third-party witness on request
Trade terms FOB / CFR / CIF / EXW and other agreed Incoterms

Stock / Available sizes

SHH STEEL quotes TP316H against a stock-and-mill enquiry range rather than a frozen SKU/tonnage list. Representative OD × wall / BWG combinations for boiler, superheater, and heat-exchanger tube appear below.

Item Typical stock / enquiry range for TP316H
Outside diameter 19.05, 25.4, 31.8, 38.1, 42.4, 50.8, 60.3, 76.2 mm (and other boiler/HX ODs on enquiry; through the usual A213 ~5 in. [127 mm] band)
Wall / BWG BWG 10–18 class walls and metric min-wall equivalents; heavier walls by agreement
Common OD × wall examples 25.4 × 2.11 mm; 31.8 × 2.77 mm; 38.1 × 2.77 mm; 42.4 × 3.56 mm; 50.8 × 3.05 mm; 60.3 × 3.91 mm — illustrative, confirm min vs average wall
Length Cut lengths for boiler / superheater / exchanger bundles; bends and random mill lengths on enquiry
Special Non-standard OD/wall, bright anneal, dual A213/SA-213, A262 Practice E, third-party witness — confirm before heat reservation

Send OD × wall (or BWG), wall basis, finish route, quantity or cut list, marking (A213 or dual A213/SA-213), and A262 / grain-size notes on one enquiry. We confirm C 0.04–0.10%, Cr 16–18% / Ni 11–14%, Mo 2.00–3.00%, Table 4 75/30 ksi, and ASTM grain size No. 7 or coarser without inventing fake warehouse codes. Sisters A213 TP316, A213 TP316L, and A213 TP304H sit on the same hub.

FAQ

Is ASTM A213 the same as ASME SA-213 for TP316H?
No. ASTM A213 / A213M is the ASTM International product specification for seamless boiler, superheater, and heat-exchanger tubes; ASME SA-213 / SA-213M is the separate ASME Code Book adoption. Dual-mark only when the purchase order asks for both names on the stencil and MTC. Chemistry, tensile floors, and grain-size rules align closely for a given referenced edition, but the standards remain independent documents.
Does ASTM A213 TP316H include welded or HCW tube?
No. ASTM A213 covers seamless boiler, superheater, and heat-exchanger tubes only. There is no WLD or HCW manufacturing-type letter under A213. Cold-finished versus hot-finished describes the seamless process route and dimensional tolerances — not a welded product form. Order welded stainless pipe under a different product standard when that form is required.
What is the chemistry of ASTM A213 TP316H?
Melting analysis for TP316H / UNS S31609 is C 0.04–0.10%, Mn ≤2.00%, P ≤0.045%, S ≤0.030%, Si ≤1.00%, Cr 16.0–18.0%, Ni 11.0–14.0%, and Mo 2.00–3.00%, with nitrogen as a no-requirement ellipsis. Confirm the ordered A213 edition. Carbon band, nickel floor at 11.0%, and molybdenum are all mandatory — none is optional on a 316H heat.
TP316H vs TP316 — what does the H add?
Both grades share Mo 2–3%, Cr 16–18, and Table 4 75/30 ksi with hardness max 192 HBW / 90 HRB. TP316 uses C ≤0.08% and Ni 10–14% without a mandatory grain-size number. TP316H holds carbon in 0.04–0.10%, raises the nickel floor to 11.0%, and requires ASTM grain size No. 7 or coarser. Order H when creep-oriented carbon/grain-size controls are on the datasheet.
TP316H vs TP304H — why choose the molybdenum grade?
Both are H grades with C 0.04–0.10%, 75/30 ksi floors, and grain size No. 7 or coarser. TP304H uses Cr 18–20 / Ni 8–11 without molybdenum. TP316H adds Mo 2–3% and uses Cr 16–18 / Ni 11–14. Choose TP316H when molybdenum is required beside the H-grade package; choose TP304H when Mo is not part of the datasheet.
Why is the nickel floor 11.0% on TP316H instead of 10.0%?
The A213 stainless chemistry table for UNS S31609 prints nickel 11.0–14.0%, while TP316 / TP316L print 10.0–14.0%. A heat at 10.5% Ni can clear standard TP316 but fails TP316H. Check the nickel floor on every dual 316/316H candidate before assuming dual marking from carbon and molybdenum alone.
Why does A213 require grain size No. 7 or coarser for TP316H?
The coarse-grain requirement supports elevated-temperature / creep-oriented behavior expected from H-grade austenitic boiler tube. ASTM No. 7 or coarser is determined per heat-treatment lot under E112. A tensile-and-Mo MTC that omits grain size is incomplete for TP316H acceptance — ask for the E112 result on the EN 10204 3.1 certificate.
Does Table 4 set a hardness limit for TP316H?
Yes. Table 4 lists hardness maximum 192 HBW / 200 HV or 90 HRB with 75 ksi tensile, 30 ksi yield, and 35% elongation. Hardness, grain size, carbon band, nickel floor, and molybdenum all belong on the release package — none replaces the others for 316H boiler tube.
What heat treatment does A213 require for TP316H?
Solution treatment at a minimum of 1900 °F [1040 °C], water quench or other rapid cool, and ASTM grain size No. 7 or coarser. Delivery is solution annealed and pickled unless bright anneal is agreed. TP316H is not listed under Supplementary Requirement S2 in the public excerpt used here — put any stabilizing hold or A262 Practice E on the purchase order when required.
Minimum wall vs average wall for A213 TP316H — which should I specify?
Boiler and superheater datasheets almost always expect minimum wall. Average wall is allowed when the purchase order says so, with A1016/A1016M tolerances for that basis. State wall basis on the enquiry rather than relying on pipe schedule numbers as the primary A213 wall story.
Is TP316H a good choice for as-welded IGC-critical tube-to-tubesheet joints?
Often not as the first choice. The intentional 0.04–0.10% carbon floor that supports creep strength works against as-welded intergranular-corrosion strategy. Many owners specify A213 TP316L for as-welded IGC duty and reserve TP316H for creep-range sections that need the carbon floor and grain-size controls. Put A262 Practice E on the PO when IGC demonstration is contractual.
Can I dual-certify TP316H with TP316 on the same heat?
Yes when one heat simultaneously clears TP316’s C ≤0.08% ceiling and Ni 10–14% window, TP316H’s C 0.04–0.10% band and Ni 11–14% floor, Mo 2–3% for both, Table 4 75/30 ksi and hardness for both, and the H-grade grain-size rule — and the purchase order asks for dual marking. Do not assume dual marking from a PMI gun that only reads Mo.

Conclusion

ASTM A213 TP316H / UNS S31609 is the high-temperature carbon-controlled molybdenum-bearing seamless stainless steel tube for boiler, superheater, and heat-exchanger service when creep-oriented carbon/grain-size controls and Mo 2–3% must travel together. SHH STEEL supplies cold-finished and hot-finished seamless tube in the usual OD × wall / BWG band, solution annealed at 1900 °F [1040 °C], tested to Table 4 75/30 ksi and hardness limits, with molybdenum and ASTM grain size No. 7 or coarser reported on EN 10204 3.1 certificates — dual SA-213 marking only when the purchase order asks.

Contact: admin@steelspecs.com

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X