ASTM A213/A213M

Product Showcase

ASTM A213/A213M Stainless Steel Products

ASTM A213 covers seamless ferritic and austenitic alloy-steel boiler, superheater and heat-exchanger tubes. Common grades include T5, T9, T11, T12, T22, T91, TP304, TP304L, TP316, TP316L, TP321 and TP347. These tubes are intended for elevated-temperature service in power plants, petrochemical and refinery applications. SHH STEEL supplies ASTM A213 tubes as a China mill-direct source with competitive pricing, full mill test certificates and reliable worldwide delivery.

ASTM A213 TP316H Stainless Steel Tube | ASTM A213 Stainless Steel - SHH STEEL

ASTM A213 TP316H Stainless Steel Tube

ASTM A213 TP316H / UNS S31609 seamless boiler, superheater and heat-exchanger tube with controlled carbon 0.04–0.10%, Cr 16.0–18.0%, Ni 11.0–14.0%, Mo 2.00–3.00%, a 75/30 ksi Table 4 floor, hardness max 192 HBW / 90 HRB, 1900 °F solution anneal, and ASTM grain size No. 7 or coarser. SHH STEEL supplies cold-finished and hot-finished seamless tube with EN 10204 3.1 MTCs that report grain size and molybdenum.
View More
ASTM A213 TP310MoCbN Stainless Steel Tube | ASTM A213 Stainless Steel - SHH STEEL

ASTM A213 TP310MoCbN Stainless Steel Tube

ASTM A213 TP310MoCbN / UNS S31025 seamless boiler, superheater and heat-exchanger tube — Mo+Nb+N+B austenitic with C ≤0.10%, Cr 19.5–23.0%, Ni 23.0–26.0%, Mo 1.0–2.0%, N 0.10–0.25%, Nb 0.10–0.40%, Ti ≤0.20%, B 0.002–0.010%, Table 4 floors of 93/39 ksi, hardness max 256 HBW / 100 HRB, 2100 °F solution anneal, and ASTM grain size No. 7 or coarser. SHH STEEL supplies cold-finished and hot-finished seamless tube with EN 10204 3.1 MTCs.
View More
ASTM A213 TP310MoLN Stainless Steel Tube | ASTM A213 Stainless Steel - SHH STEEL

ASTM A213 TP310MoLN Stainless Steel Tube

ASTM A213 TP310MoLN / UNS S31050 seamless boiler, superheater and heat-exchanger tube — low-carbon 24–26% Cr / 21–23% Ni austenitic with C ≤0.025%, Mo 2.00–3.00%, N 0.10–0.16%, Si ≤0.40%, wall-dependent Table 4 floors (84/39 or 78/37 ksi), and hardness max 217 HBW / 95 HRB. SHH STEEL supplies cold-finished and hot-finished seamless tube with EN 10204 3.1 MTCs that report Mo and N.
View More
ASTM A213 TP310HCbN Stainless Steel Tube | ASTM A213 Stainless Steel - SHH STEEL

ASTM A213 TP310HCbN Stainless Steel Tube

ASTM A213 TP310HCbN / UNS S31042 seamless boiler, superheater and heat-exchanger tube — H-grade 24–26% Cr / 19–22% Ni with C 0.04–0.10%, Nb 0.20–0.60%, N 0.15–0.35%, Table 4 floors of 95/43 ksi, hardness max 256 HBW / 100 HRB, 1900 °F solution anneal, and ASTM grain size No. 7 or coarser. SHH STEEL supplies cold-finished and hot-finished seamless tube with EN 10204 3.1 MTCs that report Nb, N, and grain size.
View More
ASTM A213 TP310HCb Stainless Steel Tube | ASTM A213 Stainless Steel - SHH STEEL

ASTM A213 TP310HCb Stainless Steel Tube

ASTM A213 TP310HCb / UNS S31041 seamless boiler, superheater and heat-exchanger tube — the H-grade niobium-stabilized 24–26% Cr / 19–22% Ni austenitic with C 0.04–0.10%, Nb 10×C–1.10%, Table 4 floors of 75/30 ksi, hardness max 192 HBW / 90 HRB, 1900 °F solution anneal (Footnote H), and ASTM grain size No. 7 or coarser. SHH STEEL supplies cold-finished and hot-finished seamless tube with EN 10204 3.1 MTCs that report Nb and grain size.
View More
ASTM A213 TP310Cb Stainless Steel Tube | ASTM A213 Stainless Steel - SHH STEEL

ASTM A213 TP310Cb Stainless Steel Tube

ASTM A213 TP310Cb / UNS S31040 seamless boiler, superheater and heat-exchanger tube — niobium-stabilized 24–26% Cr / 19–22% Ni austenitic with C ≤0.08%, Nb 10×C–1.10%, Table 4 floors of 75/30 ksi, hardness max 192 HBW / 90 HRB, and 1900 °F solution anneal. SHH STEEL supplies cold-finished and hot-finished seamless tube with EN 10204 3.1 MTCs that report niobium.
View More
ASTM A213 TP310H Stainless Steel Tube | ASTM A213 Stainless Steel - SHH STEEL

ASTM A213 TP310H Stainless Steel Tube

ASTM A213 TP310H / UNS S31009 seamless boiler, superheater and heat-exchanger tube — the H-grade 24–26% Cr / 19–22% Ni austenitic with controlled carbon 0.04–0.10%, Table 4 floors of 75/30 ksi, hardness max 192 HBW / 90 HRB, 1900 °F solution anneal, and ASTM grain size No. 7 or coarser. SHH STEEL supplies cold-finished and hot-finished seamless tube with EN 10204 3.1 MTCs that report grain size.
View More
ASTM A213 TP310S Stainless Steel Tube | ASTM A213 Stainless Steel - SHH STEEL

ASTM A213 TP310S Stainless Steel Tube

ASTM A213 TP310S / UNS S31008 seamless boiler, superheater and heat-exchanger tube — a 24–26% Cr / 19–22% Ni austenitic with C ≤0.08%, Table 4 floors of 75/30 ksi, hardness max 192 HBW / 90 HRB, and 1900 °F solution anneal with Footnote F quench capability. SHH STEEL supplies cold-finished and hot-finished seamless tube with EN 10204 3.1 MTCs.
View More
ASTM A213 TP309LMoN Stainless Steel Tube | ASTM A213 Stainless Steel - SHH STEEL

ASTM A213 TP309LMoN Stainless Steel Tube

ASTM A213 TP309LMoN / UNS S30925 seamless boiler, superheater and heat-exchanger tube — low-carbon (C ≤0.025%) 23–26% Cr / 13–16% Ni austenitic with Mo 0.5–1.2%, N 0.25–0.40%, Table 4 floors of 93/38 ksi, hardness max 256 HBW / 100 HRB, 1920 °F solution anneal, and ASTM grain size No. 7 or coarser. SHH STEEL supplies cold-finished and hot-finished seamless tube with EN 10204 3.1 MTCs that report Mo, N, and grain size.
View More
ASTM A213 TP309HCb Stainless Steel Tube | ASTM A213 Stainless Steel - SHH STEEL

ASTM A213 TP309HCb Stainless Steel Tube

ASTM A213 TP309HCb / UNS S30941 seamless boiler, superheater and heat-exchanger tube — the H-grade niobium-stabilized 22–24% Cr austenitic with C 0.04–0.10%, Ni 12.0–16.0%, Nb 10×C–1.10%, Table 4 floors of 75/30 ksi, hardness max 192 HBW / 90 HRB, 1900 °F solution anneal, and ASTM grain size No. 7 or coarser. SHH STEEL supplies cold-finished and hot-finished seamless tube with EN 10204 3.1 MTCs that report Nb and grain size.
View More
ASTM A213 TP309Cb Stainless Steel Tube | ASTM A213 Stainless Steel - SHH STEEL

ASTM A213 TP309Cb Stainless Steel Tube

ASTM A213 TP309Cb / UNS S30940 seamless boiler, superheater and heat-exchanger tube — niobium-stabilized 22–24% Cr austenitic with Ni 12.0–16.0%, C ≤0.08%, Nb 10×C–1.10%, Table 4 floors of 75/30 ksi, hardness max 192 HBW / 90 HRB, and a 1900 °F solution anneal. Chosen when 309-family oxidation resistance needs Cb stabilization rather than H-grade carbon/grain-size alone. SHH STEEL supplies cold-finished and hot-finished seamless tube with EN 10204 3.1 MTCs that report Nb.
View More
ASTM A213 TP309H Stainless Steel Tube | ASTM A213 Stainless Steel - SHH STEEL

ASTM A213 TP309H Stainless Steel Tube

ASTM A213 TP309H / UNS S30909 seamless boiler, superheater and heat-exchanger tube — the H-grade 22–24% Cr / 12–15% Ni austenitic with controlled carbon 0.04–0.10%, Table 4 floors of 75/30 ksi, hardness max 192 HBW / 90 HRB, 1900 °F solution anneal, and ASTM grain size No. 7 or coarser. SHH STEEL supplies cold-finished and hot-finished seamless tube with EN 10204 3.1 MTCs that report grain size.
View More

ASTM A213/A213M Stainless Steel Products

ASTM A213 UNS S35045 Stainless Steel Tube ASTM A213 UNS S31277 Stainless Steel Tube ASTM A213 UNS S31272 Stainless Steel Tube ASTM A213 UNS S31254 Stainless Steel Tube
ASTM A213 UNS S31002 Stainless Steel Tube ASTM A213 UNS S30815 Stainless Steel Tube ASTM A213 UNS S30615 Stainless Steel Tube ASTM A213 TP XM-15 Stainless Steel Tube
ASTM A213 TP348H Stainless Steel Tube ASTM A213 TP348 Stainless Steel Tube ASTM A213 TP347W Stainless Steel Tube ASTM A213 TP347LN Stainless Steel Tube
ASTM A213 TP347HFG Stainless Steel Tube ASTM A213 TP347H Stainless Steel Tube ASTM A213 TP347 Stainless Steel Tube ASTM A213 TP321H Stainless Steel Tube
ASTM A213 TP321 Stainless Steel Tube ASTM A213 TP317LMN Stainless Steel Tube ASTM A213 TP317LM Stainless Steel Tube ASTM A213 TP317L Stainless Steel Tube
ASTM A213 TP317 Stainless Steel Tube ASTM A213 TP316LNM Stainless Steel Tube ASTM A213 TP316N Stainless Steel Tube ASTM A213 TP316Ti Stainless Steel Tube
ASTM A213 TP316H Stainless Steel Tube ASTM A213 TP310MoCbN Stainless Steel Tube ASTM A213 TP310MoLN Stainless Steel Tube ASTM A213 TP310HCbN Stainless Steel Tube
ASTM A213 TP310HCb Stainless Steel Tube ASTM A213 TP310Cb Stainless Steel Tube ASTM A213 TP310H Stainless Steel Tube ASTM A213 TP310S Stainless Steel Tube
ASTM A213 TP309LMoN Stainless Steel Tube ASTM A213 TP309HCb Stainless Steel Tube ASTM A213 TP309Cb Stainless Steel Tube ASTM A213 TP309H Stainless Steel Tube
ASTM A213 TP309S Stainless Steel Tube ASTM A213 UNS S30432 Stainless Steel Tube ASTM A213 TP304LN Stainless Steel Tube ASTM A213 TP304N Stainless Steel Tube
ASTM A213 TP304H Stainless Steel Tube ASTM A213 TP XM-19 Stainless Steel Tube ASTM A213 TP202 Stainless Steel Tube ASTM A213 TP201 Stainless Steel Tube
ASTM A213 TP316L Stainless Steel Tube ASTM A213 TP316 Stainless Steel Tube ASTM A213 TP304L Stainless Steel Tube ASTM A213 TP304 Stainless Steel Tube
Stainless Steel Pipes and Tubes supplier and exporter

Stainless Steel Pipes and Tubes

SHH STEEL, a premier Stainless Steel Pipes and Tubes exporter, produces and exports stainless steel pipes and tubes for chemical, marine, and food processing industries. Our seamless and welded products, like 304 and 316L (ASTM A312), ensure corrosion resistance and strength. With a 5,000-ton inventory, we deliver in 3–5 days, backed by SGS/TUV inspections and mill certificates. Choose SHH STEEL for seamless stainless steel pipes and custom solutions.

Stainless Steel Pipes and Tubes

SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

    *

    *

    *

    *


    X