GOST 9940

Product Showcase

GOST 9940 Stainless Steel Products

SHH STEEL offers GOST 9940-compliant 304/316 stainless steel tubes. GOST 9940 specifies seamless corrosion-resistant and heat-resistant stainless steel tubes for high-temperature and high-pressure environments. Certified quality, competitive prices, customizable. Trust SHH STEEL!

GOST 9940 08Х22Н6Т Seamless Stainless Steel Pipe

GOST 9940 08Х22Н6Т seamless stainless steel pipe (lean duplex / 22Cr-6Ni Ti (approx)), austenitic-ferritic (duplex-lean) Ti-stabilised, GOST 5632 cast analysis, Rm min 588 N/mm² / δ5 min 24%, hot-deformed seamless. SHH STEEL can produce and supply with mill certificates.
View More

GOST 9940 17Х18Н9 Seamless Stainless Steel Pipe

GOST 9940 17Х18Н9 seamless stainless steel pipe (302 / high-C 18-8 (approx)), austenitic high-carbon 18-9, GOST 5632 cast analysis, Rm min 568 N/mm² / δ5 min 40%, hot-deformed seamless. SHH STEEL can produce and supply with mill certificates.
View More

GOST 9940 12Х18Н12Т Seamless Stainless Steel Pipe

GOST 9940 12Х18Н12Т seamless stainless steel pipe (321 (higher-Ni) / UNS S32100 family), austenitic Ti-stabilised 18-12, GOST 5632 cast analysis, Rm min 529 N/mm² / δ5 min 40%, hot-deformed seamless. SHH STEEL can produce and supply with mill certificates.
View More

GOST 9940 12Х18Н10Т Seamless Stainless Steel Pipe

GOST 9940 12Х18Н10Т seamless stainless steel pipe (321 / UNS S32100 (approx)), austenitic Ti-stabilised 18-10, GOST 5632 cast analysis, Rm min 529 N/mm² / δ5 min 40%, hot-deformed seamless. SHH STEEL can produce and supply with mill certificates.
View More

GOST 9940 12Х18Н9 Seamless Stainless Steel Pipe

GOST 9940 12Х18Н9 seamless stainless steel pipe (302 / UNS S30200 (approx)), austenitic 18-9 (higher C), GOST 5632 cast analysis, Rm min 529 N/mm² / δ5 min 40%, hot-deformed seamless. SHH STEEL can produce and supply with mill certificates.
View More

GOST 9940 10Х17Н13М2Т Seamless Stainless Steel Pipe

GOST 9940 10Х17Н13М2Т seamless stainless steel pipe (316Ti / UNS S31635 (approx)), austenitic Mo + Ti (316Ti class), GOST 5632 cast analysis, Rm min 529 N/mm² / δ5 min 35%, hot-deformed seamless. SHH STEEL can produce and supply with mill certificates.
View More

GOST 9940 08Х20Н14С2 Seamless Stainless Steel Pipe

GOST 9940 08Х20Н14С2 seamless stainless steel pipe (309Si / heat-resisting Si grade (approx)), austenitic heat-resisting Si-bearing, GOST 5632 cast analysis, Rm min 510 N/mm² / δ5 min 35%, hot-deformed seamless. SHH STEEL can produce and supply with mill certificates.
View More

GOST 9940 08Х18Н12Т Seamless Stainless Steel Pipe

GOST 9940 08Х18Н12Т seamless stainless steel pipe (321 (higher-Ni) / UNS S32100 family), austenitic Ti-stabilised 18-12, GOST 5632 cast analysis, Rm min 510 N/mm² / δ5 min 40%, hot-deformed seamless. SHH STEEL can produce and supply with mill certificates.
View More

GOST 9940 08Х18Н12Б Seamless Stainless Steel Pipe

GOST 9940 08Х18Н12Б seamless stainless steel pipe (347 / UNS S34700 (approx)), austenitic Nb-stabilised 18-12, GOST 5632 cast analysis, Rm min 510 N/mm² / δ5 min 38%, hot-deformed seamless. SHH STEEL can produce and supply with mill certificates.
View More

GOST 9940 08Х18Н10Т Seamless Stainless Steel Pipe

GOST 9940 08Х18Н10Т seamless stainless steel pipe (321 / UNS S32100 (approx)), austenitic Ti-stabilised 18-8, GOST 5632 cast analysis, Rm min 510 N/mm² / δ5 min 40%, hot-deformed seamless. SHH STEEL can produce and supply with mill certificates.
View More

GOST 9940 08Х18Н10 Seamless Stainless Steel Pipe

GOST 9940 08Х18Н10 seamless stainless steel pipe (304 / UNS S30400 (approx)), austenitic 18-8, GOST 5632 cast analysis, Rm min 510 N/mm² / δ5 min 40%, hot-deformed seamless. SHH STEEL can produce and supply with mill certificates.
View More

GOST 9940 08Х17Н15М3Т Seamless Stainless Steel Pipe

GOST 9940 08Х17Н15М3Т seamless stainless steel pipe (317Ti / UNS S31726 family (approx)), austenitic Mo + Ti (317Ti class), GOST 5632 cast analysis, Rm min 510 N/mm² / δ5 min 35%, hot-deformed seamless. SHH STEEL can produce and supply with mill certificates.
View More
Stainless Steel Pipes and Tubes supplier and exporter

Stainless Steel Pipes and Tubes

SHH STEEL, a premier Stainless Steel Pipes and Tubes exporter, produces and exports stainless steel pipes and tubes for chemical, marine, and food processing industries. Our seamless and welded products, like 304 and 316L (ASTM A312), ensure corrosion resistance and strength. With a 5,000-ton inventory, we deliver in 3–5 days, backed by SGS/TUV inspections and mill certificates. Choose SHH STEEL for seamless stainless steel pipes and custom solutions.

Stainless Steel Pipes and Tubes

SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

    *

    *

    *

    *


    X