ASTM A213 TP309Cb Stainless Steel Tube
What is ASTM A213 TP309Cb Stainless Steel Tube
ASTM A213 / A213M covers seamless ferritic and austenitic alloy-steel boiler, superheater, and heat-exchanger tubes. Grade TP309Cb is the niobium-stabilized (columbium-stabilized) member of the 309 family, listed under UNS S30940: carbon ≤0.08%, chromium 22.0–24.0%, nickel 12.0–16.0% — note the wider nickel window versus TP309S/TP309H — and niobium held at 10×C minimum up to 1.10% maximum. That Nb addition exists to stabilize carbon as niobium carbides, reducing the risk of chromium-carbide sensitization in service temperature bands where unstabilized 309 can suffer intergranular attack, while keeping the high-Cr–Ni oxidation framing of the 309 family.
SHH STEEL can supply ASTM A213 TP309Cb stainless steel tube as seamless cold-finished and hot-finished product in the usual boiler, furnace, and heat-exchanger OD × wall / BWG band, shipped with EN 10204 3.1 mill test certificates that report the full stainless-table ladle chemistry — including the niobium result — and the Table 4 tensile/hardness set. Dual A213 / SA-213 marking is available only when the purchase order asks for both independent standards. Browse 309-family grades on the A213/A213M hub.
Shop names such as 309Cb, 309Nb, S30940, or “niobium 309 tube” do not replace the ASTM grade on the MTC — and Cb is not chemically identical to every historical “Type 309” plate heat. Sister grades under the same ASTM standard include A213 TP309S, A213 TP309H, A213 TP309HCb, A213 TP347, and A213 TP310Cb. A213 covers seamless tube only — cold-finished versus hot-finished is the process choice, not a WLD/HCW manufacturing-type letter.
Chemical Composition of A213 TP309Cb
Two chemistry layers matter for TP309Cb under ASTM A213. Melting analysis is mandatory for every heat; product analysis on finished tube applies only when Supplementary Requirement wording or the purchase order invokes it through ASTM A1016/A1016M, with tolerances typically from ASTM A480/A480M Table A1.1. Read the niobium line first: Nb must be at least ten times the carbon content and not more than 1.10%. An MTC that omits niobium is incomplete for S30940. Also note nickel 12.0–16.0% — one percentage point wider on the high side than the 12.0–15.0% window on TP309S and TP309H.
The tables below reproduce the melt limits for TP309Cb / UNS S30940 and the product-analysis limits from A480 Table A1.1. Values are maximum unless a range is shown; ellipsis (…) means no requirement.
Melting analysis (heat / ladle analysis)
| Element | TP309Cb (UNS S30940) melting analysis |
|---|---|
| Carbon (C) | ≤ 0.08 |
| Manganese (Mn) | ≤ 2.00 |
| Phosphorus (P) | ≤ 0.045 |
| Sulfur (S) | ≤ 0.030 |
| Silicon (Si) | ≤ 1.00 |
| Chromium (Cr) | 22.0 – 24.0 |
| Nickel (Ni) | 12.0 – 16.0 |
| Molybdenum (Mo) | … (no requirement) |
| Nitrogen (N) | … (no requirement) |
| Niobium (Nb / Cb) | 10×C – 1.10 |
Source: ASTM A213/A213M stainless chemistry table for Grade TP309Cb / UNS S30940 (public mill / specification PDF excerpt — htpipe A213 table text). Confirm the ordered edition on the purchase order. “Cb” on the grade name is the historical columbium designation; the chemistry table reports niobium (Nb).
Product analysis — A480/A480M Table A1.1 tolerances applied
| Element | Melting | Tolerance (A480 A1.1) | Product analysis limit |
|---|---|---|---|
| Carbon (C) | ≤ 0.08 | 0.01 over | ≤ 0.09 |
| Manganese (Mn) | ≤ 2.00 | 0.04 over | ≤ 2.04 |
| Phosphorus (P) | ≤ 0.045 | 0.010 over | ≤ 0.055 |
| Sulfur (S) | ≤ 0.030 | 0.005 over | ≤ 0.035 |
| Silicon (Si) | ≤ 1.00 | 0.05 over | ≤ 1.05 |
| Chromium (Cr) | 22.0 – 24.0 | 0.25 under / over | 21.75 – 24.25 |
| Nickel (Ni) | 12.0 – 16.0 | 0.15 under / over | 11.85 – 16.15 |
| Niobium (Nb) | 10×C – 1.10 | 0.05 under / over on max; min remains formula-tied | max ≤ 1.15; min still ≥10×C on melt basis — confirm A480 path if contractual |
Chromium 22–24% and the wider nickel 12–16% window are the oxidation-resistance story; niobium is the stabilization story. Carbon ≤0.08% is the same ceiling as TP309S — not an H-grade floor. For controlled carbon floor plus grain-size language open A213 TP309H; for H-grade carbon plus Nb open A213 TP309HCb. Molybdenum remains a no-requirement ellipsis — chloride-heavy exchangers still step to Mo grades.
When product analysis is ordered, finished tube may read up to C 0.09%, Mn 2.04%, P 0.055%, S 0.035%, and Si 1.05%, with Cr 21.75–24.25% and Ni 11.85–16.15%. Niobium product-analysis practice for formula-minimum grades is edition- and A480-sensitive — put any tighter Nb floor or sulfur ceiling on the purchase order before the heat is selected, and confirm the A480 edition if product analysis is contractual.
Mechanical Properties of A213 TP309Cb
ASTM A213 Table 4 sets the tensile acceptance floor for TP309Cb at 75 ksi [515 MPa] tensile strength and 30 ksi [205 MPa] yield strength (0.2% offset), with elongation of 35% minimum in 2 in. or 50 mm and hardness max 192 HBW / 200 HV or 90 HRB — the same room-temperature pair used for TP309S and TP309H. The grade’s differentiation is niobium stabilization chemistry and the wider nickel window, not a unique tensile number. Public Table 3 does not assign a mandatory ASTM grain-size number to TP309Cb (unlike TP309H / TP309HCb).
| Property | TP309Cb requirement (Table 4) |
|---|---|
| Tensile strength, min | 75 ksi [515 MPa] |
| Yield strength (0.2% offset), min | 30 ksi [205 MPa] |
| Elongation in 2 in. or 50 mm, min | 35% |
| Hardness, max | 192 HBW / 200 HV or 90 HRB |
| Grain size | No mandatory ASTM number in public Table 3 excerpt (unlike H grades) |
Source: ASTM A213/A213M Table 4 for TP309Cb / UNS S30940 (public specification PDF excerpt). Mechanical property requirements do not apply to tubing smaller than 1/8 in. [3.2 mm] ID or thinner than 0.015 in. [0.4 mm] wall. Flattening and flaring tests sit beside tension and hardness on a lot basis.
Design calculations should use Table 4 unless the PO states higher guaranteed values the mill has accepted in writing. For creep-critical H-grade carbon and grain-size controls under the 309 family, open A213 TP309H or A213 TP309HCb rather than stretching standard TP309Cb beyond its intended framing.
Dimensions and Tolerances
Dimensional supply for ASTM A213 TP309Cb is tube language — OD × wall (minimum or average) and BWG / gauge — covering boiler, furnace, and heat-exchanger sizes rather than leading with ASME B36.19 pipe schedules. Usual A213 sizes run from about 1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD with min wall about 0.015–0.500 in. [0.4–12.7 mm]; other diameters by agreement. State wall basis on the purchase order.
OD and wall variations follow ASTM A1016/A1016M as invoked by A213. Cold-finished tubes commonly hold tighter OD; hot-finished tubes allow wider windows. Cold-finished average wall is often summarized as ±10% of specified average wall; minimum-wall product follows A1016 minimum-wall tables. Confirm exact rows for the OD and finish on the ordered edition.
| Item | Typical A213 TP309Cb dimensional practice |
|---|---|
| Product form | Seamless only (cold-finished or hot-finished) |
| Usual size band | ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD; wall ~0.015–0.500 in. [0.4–12.7 mm] |
| Wall basis | Minimum wall (default) or average wall when specified |
| OD / wall tolerances | Per ASTM A1016/A1016M for finish route and size |
| Length | Cut lengths for furnace / HX / boiler bundles; mill random by agreement |
| Secondary note | B36.19 schedules only as a buyer cross-reference |
Put cut list, bend form, and end preparation on the enquiry. Minimum wall remains a first-class A213 concept for 309Cb the same way it does for other 309-family tube.
Equivalent Grades
Equivalence language around 309Cb tube often collapses plate, cast, and tube product forms into one nickname. ASTM A213 Grade TP309Cb / UNS S30940 is the governing designation for this article; EN and JIS wrought names that point to similar Nb-stabilized high-Cr–Ni chemistry families are not automatic substitutes on an A213 MTC.
| Designation | Notes |
|---|---|
| ASTM A213 / A213M Grade TP309Cb | Governing ASTM seamless boiler / HX tube product standard for this article |
| UNS S30940 | Unified number in the stainless chemistry table |
| ASME SA-213 TP309Cb | Separate ASME Code Book adoption — dual-mark only when the PO asks |
| Related S-grade | A213 TP309S — same Cr band, Ni 12–15, no Nb |
| Related H+Cb | A213 TP309HCb — H-grade carbon + Nb + grain size |
| Related 18-8 stabilized | A213 TP347 — Nb-stabilized at lower Cr–Ni |
| Related plate | A240 / SA240 flat product in the 309Cb family — order plate and tube under their own standards |
Dual A213/SA-213 marking is a purchase-order option. Compare TP309S, TP309H, and TP309HCb on their own ASTM A213 pages before swapping 309-family grades inside a furnace or boiler tube list.
Heat Treatment and Delivery Condition
TP309Cb under ASTM A213 is furnished solution treated at a minimum of 1900 °F [1040 °C], then quenched in water or cooled rapidly by other means. That Table 3 heat-treatment row applies to both cold-finished and hot-finished seamless tube. Public Table 3 does not assign a mandatory ASTM grain-size number to TP309Cb — grain-size language belongs to the H grades (TP309H, TP309HCb).
Cold-finished versus hot-finished is a process and dimensional route, not a substitute for the anneal. Delivery condition for SHH STEEL TP309Cb is solution annealed and pickled (or bright annealed by agreement), with anneal temperature, quench method, and niobium result on the EN 10204 3.1 certificate. Straightening, cutting, and end finishing follow heat treatment.
Stabilizing heat treatment under Supplementary Requirement S2 is written for listed stabilized grades including TP309HCb (and TP321 / TP347 family); if your datasheet needs a post-solution stabilizing hold on TP309Cb specifically, write that Supplementary Requirement onto the purchase order rather than assuming base A213 includes it. When H-grade carbon and grain size are also required with Nb, open A213 TP309HCb.
Corrosion Resistance
TP309Cb is selected for high-temperature oxidation resistance from the 22–24% Cr / 12–16% Ni balance, plus niobium stabilization against chromium-carbide sensitization in temperature bands where unstabilized 309 can suffer intergranular attack. It is not a molybdenum grade: in aqueous chloride pitting and crevice service, A213 TP316 / A213 TP316L remain the usual step-ups.
Stabilization does not make TP309Cb immune to every IGC or hot-gas attack mode — selection remains engineering judgment against atmosphere, temperature, and cyclic duty. ASTM A213 does not publish a corrosion-rate or oxidation-rate table for TP309Cb. When a project invokes Practice A262 or a specific oxidation test, write that Supplementary Requirement onto the purchase order.
Applications of A213 TP309Cb Tube
TP309Cb shows up wherever seamless 309-family tube must survive hotter oxidizing environments than 18-8 is trusted for, and the datasheet also demands niobium stabilization — furnace tubes, radiant sections, heat-recovery exchangers, and some boiler locations where sensitization resistance matters alongside oxidation framing.
| Application area | Typical use of TP309Cb tube | Selection note |
|---|---|---|
| Furnace / radiant tubes | Oxidizing atmospheres with Nb-stabilized base metal | Confirm peak metal temperature and atmosphere |
| Heat-recovery / hot-gas HX | Hot oxidizing gas circuits needing sensitization resistance | Step to TP310Cb if higher Cr–Ni is specified |
| Boiler locations (stabilization-led) | Where Nb stabilization is accepted without H-grade carbon/grain-size | Open TP309HCb when H rules also apply |
| Creep-H without Nb | Usually not TP309Cb | Open A213 TP309H |
| Aqueous chloride HX | Usually not the first 309Cb use case | Prefer Mo grades (TP316/TP316L) |
Stay on the A213/A213M hub for 309S, 309H, 309HCb, and 310Cb sisters rather than mixing A312 pipe certificates into tube acceptance.
Weldability
TP309Cb tube welds with matching or near-matching 309/309L or Nb-bearing austenitic filler for tube-to-tubesheet, attachment, and fabrication joins under a qualified WPS. Fabricators often select ER309L for lower carbon in the weld metal, or a Nb-bearing filler when the WPS requires weld-metal stabilization to match the base tube philosophy. Heat input, interpass, and cleaning remain the fabricator’s code responsibility — A213 governs the seamless tube product, not the field weld procedure.
Because A213 TP309Cb is seamless, there is no mill longitudinal weld to radiograph as welded-pipe standards describe. Focus inspection on each-length hydro or NDE, joint quality, niobium on the MTC, and any contractual IGC or oxidation tests. When H-grade carbon and grain-size controls are also required in the base metal, change the tube grade to A213 TP309HCb rather than trying to weld-procedure a standard Cb grade into an H-grade datasheet.
Surface Finishes
Standard mill delivery for ASTM A213 TP309Cb is solution annealed and pickled. Bright annealing is a called-out route when a smoother reflective surface is needed. Specified Ra, light polish, and post-fabrication passivation are commercial extras on top of the A213 stamp.
Furnace and hot-gas tube often ships with a workmanlike pickled finish; cosmetic polish is uncommon unless the PO asks. End preparation for welding or expanding should be ordered with finish so receiving inspection shares one acceptance language. Niobium reporting is a chemistry requirement on the MTC, not a surface-finish option.
Inspection and Testing
Base ASTM A213 testing for TP309Cb includes heat analysis (with niobium), tension to the Table 4 75/30 ksi floors, hardness to the Table 4 maximum, flattening and flaring on a lot basis, and hydro or NDE of each length. The manufacturer may choose hydro versus NDE unless the purchase order fixes the method. Marking includes ASTM designation, grade, size, heat number, and other clause-required data.
| Option | Purpose |
|---|---|
| Product analysis | Confirms chemistry — including Nb — on finished tube |
| Intergranular corrosion (e.g. A262) | Only when Supplementary Requirements or OEM specs add them |
| Stabilizing heat treatment (S2-style) | Write onto the PO if required for this grade path |
| Minimum vs average wall | States wall basis |
| Fixed hydro or NDE method | Removes manufacturer’s option |
| Third-party inspection / EN 10204 3.2 | Witnessed testing when the project requires it |
Ask the mill to state lot identity clearly so hardness and tension specimens map cleanly to the bundle you receive. An MTC without niobium is incomplete for TP309Cb.
Packaging and Shipping
TP309Cb tube leaves SHH STEEL bundled, end-protected, and tagged with ASTM A213 grade, OD × wall (or BWG), heat number, and PO reference. U-bent or specially cut furnace lengths need transit protection matched to bend radius and leg length. Export packing ranges from bare or wrapped bundles to wooden cases for bright-annealed or small-bore material.
We ship under the Incoterms on the order acknowledgement — FOB, CFR, CIF, EXW, or other agreed terms. Bilingual marks, inland trucking, and project color coding belong on the enquiry beside the metallurgical notes (Nb result, dual marking, any stabilizing SR).
Why Choose SHH STEEL
SHH STEEL treats ASTM A213 TP309Cb as a niobium-stabilized oxidation-oriented tube grade with enforceable chemistry (including Nb), tensile, hardness, and heat-treatment rules — not as a catalogue nickname for “any 309 tube.” Certificates report the stainless-table ladle chemistry with niobium and the Table 4 set; dual A213/SA-213 marking appears only when requested.
If the datasheet does not need Nb, we open A213 TP309S. If H-grade carbon and grain size are required without Nb, we open A213 TP309H. If both H and Cb are required, we open A213 TP309HCb. Wet chloride duty steers to the Mo family on the A213/A213M hub. Lead times mix near-term lengths with mill schedules; we say which is which.
Cut-to-length, U-bending, polish, and third-party inspection are defined extras. The tube on site should match the ASTM callout the engineer wrote — including the niobium line on the MTC.
Supply Capability
SHH STEEL can supply ASTM A213 TP309Cb stainless steel tube against the edition and finish route on your enquiry. Capability and Stock / Available sizes below frame furnace, boiler, and HX enquiries for this Nb-stabilized grade.
| Item | SHH STEEL capability for TP309Cb |
|---|---|
| Standard | ASTM A213 / A213M (dual SA-213 marking on request) Grade TP309Cb / UNS S30940 |
| Product form | Seamless only — cold-finished and hot-finished |
| Size | Typical OD × min wall (or average wall) in the A213 usual band; other diameters by agreement |
| Wall / gauge | Minimum wall or average wall; BWG / gauge accepted |
| Length | Cut-to-length for furnace / HX / boiler; mill random by agreement; bends on enquiry |
| Finish | Annealed and pickled; bright annealed or light polish by agreement |
| Testing | Tension (75/30 ksi), hardness (max 192 HBW / 90 HRB), flattening, flaring, hydro or NDE; full melt chemistry including Nb on MTC |
| Documents | EN 10204 3.1 with Nb result; third-party / 3.2 on request |
| Trade terms | FOB / CFR / CIF / EXW and other agreed Incoterms |
Stock / Available sizes
SHH STEEL quotes TP309Cb against a stock-and-mill enquiry range rather than a frozen SKU/tonnage list. Representative OD × wall / BWG combinations for furnace, boiler, and heat-exchanger tube appear below.
| Item | Typical stock / enquiry range for TP309Cb |
|---|---|
| Outside diameter | 19.05, 25.4, 31.8, 38.1, 42.4, 50.8, 60.3, 76.2 mm (and other furnace/HX ODs on enquiry; through the usual A213 ~5 in. [127 mm] band) |
| Wall / BWG | BWG 10–18 class walls and metric min-wall equivalents; heavier walls by agreement |
| Common OD × wall examples | 25.4 × 2.11 mm; 31.8 × 2.77 mm; 38.1 × 2.77 mm; 42.4 × 3.56 mm; 50.8 × 3.05 mm; 60.3 × 3.91 mm — illustrative, confirm min vs average wall |
| Length | Cut lengths for furnace / exchanger bundles; bends and random mill lengths on enquiry |
| Special | Non-standard OD/wall, bright anneal, dual A213/SA-213, stabilizing SR, third-party witness — confirm before heat reservation |
Send OD × wall (or BWG), wall basis, finish route, quantity or cut list, marking (A213 or dual A213/SA-213), Nb reporting expectation, and Supplementary Requirements on one enquiry. We confirm Cr 22–24% / Ni 12–16%, Nb 10×C–1.10, and Table 4 75/30 ksi without inventing fake warehouse codes. Sisters A213 TP309S, A213 TP309HCb, and A213 TP347 sit on the same hub.
FAQ
-
Is ASTM A213 the same as ASME SA-213 for TP309Cb?
- No. ASTM A213 / A213M is the ASTM International product specification for seamless boiler, superheater, and heat-exchanger tubes; ASME SA-213 / SA-213M is the separate ASME Code Book adoption. Dual-mark only when the purchase order asks for both names on the stencil and MTC. Chemistry and tensile floors align closely for a given referenced edition, but the standards remain independent.
-
Does ASTM A213 TP309Cb include welded or HCW tube?
- No. ASTM A213 covers seamless tube only. There is no WLD or HCW manufacturing type under this product standard. Cold-finished versus hot-finished seamless tube is the process choice. Welded stainless pipe belongs to a different product standard and page family.
-
What is the chemistry of ASTM A213 TP309Cb?
- TP309Cb / UNS S30940 melt limits include carbon ≤0.08%, manganese ≤2.00%, phosphorus ≤0.045%, sulfur ≤0.030%, silicon ≤1.00%, chromium 22.0–24.0%, nickel 12.0–16.0%, and niobium 10×C–1.10%, with molybdenum and nitrogen as no-requirement ellipses. Note the wider nickel window versus TP309S/TP309H. Product-analysis limits apply only when ordered.
-
What does Cb mean in TP309Cb?
- Cb is the historical designation for columbium, the same element now listed as niobium (Nb) in the stainless chemistry table. Under A213 the grade requires Nb of not less than 10 times the carbon content and not more than 1.10%. An MTC that omits niobium is incomplete for TP309Cb, regardless of which synonym the shop drawing uses.
-
TP309Cb vs TP309S — when do I need niobium stabilization?
- Order TP309Cb when the datasheet requires niobium stabilization against chromium-carbide sensitization together with 309-family oxidation resistance. Order TP309S when the ≤0.08% carbon ceiling without Nb is enough. Both share Cr 22–24% and Table 4 75/30 ksi; TP309Cb also widens nickel to 12–16%. Do not treat "309Cb" as a synonym stamp for ordinary TP309S on the MTC.
-
TP309Cb vs TP309H — which A213 grade should I order?
- Order TP309Cb when niobium stabilization is the driver and H-grade carbon/grain-size rules are not required. Order TP309H when the datasheet needs carbon 0.04–0.10% and ASTM No. 7 or coarser grain size without Nb. When both H rules and Nb are required, open TP309HCb rather than trying to dual-stamp mismatched chemistries.
-
TP309Cb vs TP347 — which stabilized grade fits?
- TP309Cb carries 22–24% Cr and 12–16% Ni with Nb 10×C–1.10 for high-temperature oxidation plus stabilization. TP347 is the Nb-stabilized 18-8-family grade at lower chromium and nickel. Order TP309Cb when the oxidation framing of 309 is required; order TP347 when classic stabilized 18-8 chemistry is specified. Compare on the A213 hub before swapping.
-
Does Table 4 set a hardness limit for TP309Cb?
- Yes. Hardness maximum is 192 HBW / 200 HV or 90 HRB, alongside 75/30 ksi tensile/yield and 35% elongation. Hardness tests are part of lot acceptance under A213. Tighter project hardness windows must be written into the purchase order.
-
What heat treatment does A213 require for TP309Cb?
- Solution treatment at a minimum of 1900 °F [1040 °C] with water quench or other rapid cool. Public Table 3 does not assign a mandatory ASTM grain-size number to TP309Cb. Ask the mill to state anneal temperature, quench method, and niobium result on the EN 10204 3.1 certificate. Write any stabilizing Supplementary Requirement onto the PO if required.
-
Minimum wall vs average wall for A213 TP309Cb — which do I order?
- Order minimum wall when the design assumes a guaranteed minimum thickness after tolerance. Order average wall only when the PO explicitly allows it and the designer accepts that basis. Put the wall basis on the enquiry before the mill selects A1016 tolerance tables.
-
Is TP309Cb a good choice for chloride-rich cooling water?
- Usually no as a first choice. TP309Cb is framed for high-temperature oxidation plus niobium stabilization; it does not add molybdenum for aqueous chloride pitting. Prefer TP316/TP316L or higher-Mo grades on the A213 hub for seawater-leaning and brine exchangers. ASTM A213 does not publish a chloride ranking table.
Conclusion
ASTM A213 TP309Cb / UNS S30940 is the niobium-stabilized 22–24% Cr / 12–16% Ni seamless stainless steel tube grade for boiler, furnace, and heat-exchanger service when high-temperature oxidation resistance and Cb stabilization both drive grade selection. SHH STEEL supplies cold-finished and hot-finished seamless tube in the usual OD × wall / BWG band, solution annealed at 1900 °F [1040 °C], tested to Table 4 75/30 ksi and hardness limits with niobium reported on EN 10204 3.1 certificates — with dual SA-213 marking only when the order asks. For sister 309S, 309H, and 309HCb grades, start from the A213/A213M hub, then send OD × wall, wall basis, Nb expectation, and marking requirements so we can align mill and near-term availability.
Contact: admin@steelspecs.com