SHH STEEL offers ISO 9329-4-compliant 304/316 stainless steel tubes. ISO 9329-4 specifies seamless stainless steel tubes for pressure purposes, ideal for high-temperature and corrosive environments. Certified quality, competitive prices, customizable. Trust SHH STEEL!
-
ISO 9329-4 X2CrNiMoN17-13 Seamless Stainless Steel Tube
ISO 9329-4 X2CrNiMoN17-13 seamless stainless steel tube (316LN / UNS S31653 / EN 1.4429 (approx)), austenitic low-carbon Mo+N 17-13-3, Table 1 heat analysis, Rp0.2 min 280 N/mm² / Rm 580–800 N/mm², seamless pressure tube. SHH STEEL can produce and supply with mill certificates.View More -
ISO 9329-4 X2CrNiN18-10 Seamless Stainless Steel Tube
ISO 9329-4 X2CrNiN18-10 seamless stainless steel tube (304LN / UNS S30453 / EN 1.4311 (approx)), austenitic low-carbon N-strengthened 18-10, Table 1 heat analysis, Rp0.2 min 270 N/mm² / Rm 580–780 N/mm², seamless pressure tube. SHH STEEL can produce and supply with mill certificates.View More -
ISO 9329-4 X5CrNiMo17-13 Seamless Stainless Steel Tube
ISO 9329-4 X5CrNiMo17-13 seamless stainless steel tube (316 higher-Mo / EN 1.4436 (approx)), austenitic standard higher-Mo 17-13-3, Table 1 heat analysis, Rp0.2 min 205 N/mm² / Rm 510–710 N/mm², seamless pressure tube. SHH STEEL can produce and supply with mill certificates.View More -
ISO 9329-4 X6CrNiMoNb17-12 Seamless Stainless Steel Tube
ISO 9329-4 X6CrNiMoNb17-12 seamless stainless steel tube (316Nb / EN 1.4580 (approx)), austenitic Nb-stabilised Mo 17-12-2, Table 1 heat analysis, Rp0.2 min 215 N/mm² / Rm 510–740 N/mm², seamless pressure tube. SHH STEEL can produce and supply with mill certificates.View More -
ISO 9329-4 X6CrNiMoTi17-12 Seamless Stainless Steel Tube
ISO 9329-4 X6CrNiMoTi17-12 seamless stainless steel tube (316Ti / UNS S31635 / EN 1.4571 (approx)), austenitic Ti-stabilised Mo 17-12-2, Table 1 heat analysis, Rp0.2 min 210 N/mm² / Rm 510–710 N/mm², seamless pressure tube. SHH STEEL can produce and supply with mill certificates.View More -
ISO 9329-4 X7CrNiMoB17-12 Seamless Stainless Steel Tube
ISO 9329-4 X7CrNiMoB17-12 seamless stainless steel tube (316H+B creep variant (approx — ISO-unique boron window)), austenitic elevated-carbon Mo+B 17-12-2 (creep-oriented), Table 1 heat analysis, Rp0.2 min 205 N/mm² / Rm 510–710 N/mm², seamless pressure tube. SHH STEEL can produce and supply with mill certificates.View More -
ISO 9329-4 X7CrNiMo17-12 Seamless Stainless Steel Tube
ISO 9329-4 X7CrNiMo17-12 seamless stainless steel tube (316H-class / EN 1.4919-family (approx)), austenitic elevated-carbon Mo 17-12-2, Table 1 heat analysis, Rp0.2 min 205 N/mm² / Rm 510–710 N/mm², seamless pressure tube. SHH STEEL can produce and supply with mill certificates.View More -
ISO 9329-4 X5CrNiMo17-12 Seamless Stainless Steel Tube
ISO 9329-4 X5CrNiMo17-12 seamless stainless steel tube (316 / UNS S31600 / EN 1.4401 (approx)), austenitic standard Mo 17-12-2, Table 1 heat analysis, Rp0.2 min 205 N/mm² / Rm 510–710 N/mm², seamless pressure tube. SHH STEEL can produce and supply with mill certificates.View More -
ISO 9329-4 X2CrNiMo17-13 Seamless Stainless Steel Tube
ISO 9329-4 X2CrNiMo17-13 seamless stainless steel tube (316L higher-Mo / EN 1.4435 (approx)), austenitic low-carbon higher-Mo 17-13-3, Table 1 heat analysis, Rp0.2 min 190 N/mm² / Rm 490–690 N/mm², seamless pressure tube. SHH STEEL can produce and supply with mill certificates.View More -
ISO 9329-4 X2CrNiMo17-12 Seamless Stainless Steel Tube
ISO 9329-4 X2CrNiMo17-12 seamless stainless steel tube (316L / UNS S31603 / EN 1.4404 (approx)), austenitic low-carbon Mo 17-12-2, Table 1 heat analysis, Rp0.2 min 190 N/mm² / Rm 490–690 N/mm², seamless pressure tube. SHH STEEL can produce and supply with mill certificates.View More -
ISO 9329-4 X7CrNiTi18-10 Seamless Stainless Steel Tube
ISO 9329-4 X7CrNiTi18-10 seamless stainless steel tube (321H-class / EN 1.4541-H family (approx)), austenitic elevated-carbon Ti-stabilised 18-10, Table 1 heat analysis, Rp0.2 min 175 N/mm² / Rm 490–690 N/mm², seamless pressure tube. SHH STEEL can produce and supply with mill certificates.View More -
ISO 9329-4 X6CrNiTi18-10 Seamless Stainless Steel Tube
ISO 9329-4 X6CrNiTi18-10 seamless stainless steel tube (321 / UNS S32100 / EN 1.4541 (approx)), austenitic Ti-stabilised 18-10, Table 1 heat analysis, Rp0.2 min 175 N/mm² / Rm 490–690 N/mm², seamless pressure tube. SHH STEEL can produce and supply with mill certificates.View More
ISO 9329-4 Stainless Steel Products
Stainless Steel Pipes and Tubes
SHH STEEL, a premier Stainless Steel Pipes and Tubes exporter, produces and exports stainless steel pipes and tubes for chemical, marine, and food processing industries. Our seamless and welded products, like 304 and 316L (ASTM A312), ensure corrosion resistance and strength. With a 5,000-ton inventory, we deliver in 3–5 days, backed by SGS/TUV inspections and mill certificates. Choose SHH STEEL for seamless stainless steel pipes and custom solutions.