ASTM A213 TP321H Stainless Steel Tube | ASTM A213 Stainless Steel - SHH STEEL

ASTM A213 TP321H Stainless Steel Tube

ASTM A213 TP321H / UNS S32109 seamless boiler, superheater and heat-exchanger tube with carbon 0.04–0.10%, Cr 17.0–19.0%, Ni 9.0–12.0%, titanium ≥4×(C+N) ≤0.70%, Table 4 floor 75/30 ksi, hardness max 192 HBW / 90 HRB, and ASTM grain size No. 7 or coarser. SHH STEEL supplies cold-finished and hot-finished seamless tube with EN 10204 3.1 MTCs that report Ti, grain size, and the finish-route anneal temperature.
Grade
TP321H / UNS S32109
Standard
ASTM A213 / A213M
Product form
Seamless boiler / superheater / heat-exchanger tube (cold-finished and hot-finished)
Size
Typical OD × min wall (or average wall) within ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD and ~0.015–0.500 in. [0.4–12.7 mm] wall; other diameters by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is ASTM A213 TP321H Stainless Steel Tube

ASTM A213 / A213M is the ASTM International product specification for seamless ferritic and austenitic alloy-steel boiler, superheater, and heat-exchanger tubes. Grade TP321H / UNS S32109 is the high-temperature, titanium-stabilized member of the 321 family: melting carbon sits in a 0.04–0.10% band (floor and ceiling), chromium 17.0–19.0%, nickel 9.0–12.0%, and titanium is held at ≥4 × (C + N) and ≤0.70%. The heat-treatment path carries an ASTM grain-size requirement of No. 7 or coarser, with separate solution-temperature floors for cold-worked and hot-rolled routes. That package exists for creep-range boiler and superheater service where titanium stabilization and H-grade carbon share one datasheet — not as a synonym stamp for ordinary A213 TP321. Buyers who write “321H tube” still need to name A213 (or the separate ASME SA-213 adoption) on the purchase order so the mill applies H-grade chemistry, grain-size, Ti-formula, test, and marking clauses.

SHH STEEL can supply ASTM A213 TP321H stainless steel tube as seamless cold-finished and hot-finished product in the usual boiler and heat-exchanger OD × wall / BWG band, shipped with EN 10204 3.1 mill test certificates that report the full ladle chemistry (including titanium against the 4 × (C + N) formula), the Table 4 tensile and hardness results, and the grain-size result for the heat-treatment lot. When a project also needs ASME Code Book marking, we dual-mark A213 / SA-213 on the same lengths only if the purchase order says so. Browse the grade family on the A213/A213M hub.

Commercially, TP321H tube is still called 321H, S32109, or titanium-stabilized H-grade boiler tube; none of those shop names replace the ASTM grade on the MTC or stencil. Sister grades under the same ASTM standard include A213 TP321, A213 TP304H, A213 TP347H, A213 TP347, and A213 TP347HFG. A213 covers seamless tube only — no welded or HCW manufacturing type — so cold-finished versus hot-finished is the process choice, not a WLD/HCW stencil letter.

Chemical Composition of A213 TP321H

Two chemistry layers matter for TP321H under ASTM A213. Melting (heat or ladle) analysis is mandatory for every heat; product analysis on finished tube applies only when Supplementary Requirement wording or the purchase order invokes it through ASTM A1016/A1016M. Product-analysis tolerances typically flow from ASTM A480/A480M Table A1.1. SHH STEEL reports actual ladle values — and product values when ordered — and does not advertise unpublished tighter catalogue windows. Two lines define the grade for a reviewer: the carbon band 0.04–0.10%, and titanium ≥4 × (C + N) with a 0.70% ceiling. That Ti multiplier is deliberately lower than the 5 × (C + N) rule on non-H A213 TP321, so do not copy a TP321 titanium check onto a TP321H heat without reopening the formula.

The tables below reproduce the heat analysis for TP321H / UNS S32109, the product-analysis limits from A480 Table A1.1 practice, and a short carbon / titanium snapshot against TP321, TP304H, and TP347H. Later A213 editions place austenitic stainless grades in Table 2 (older editions used Table 1); confirm the ordered edition on the purchase order.

Melting analysis (heat / ladle analysis)

Element TP321H (UNS S32109) melting analysis
Carbon (C) 0.04 – 0.10
Manganese (Mn) ≤ 2.00
Phosphorus (P) ≤ 0.045
Sulfur (S) ≤ 0.030
Silicon (Si) ≤ 1.00
Chromium (Cr) 17.0 – 19.0
Nickel (Ni) 9.0 – 12.0
Molybdenum (Mo) … (no requirement)
Nitrogen (N) … (no requirement; analysis method by agreement when reported for the Ti formula)
Niobium (Nb) … (no requirement)
Titanium (Ti) ≥ 4 × (C + N), ≤ 0.70

Source: ASTM A213/A213M stainless chemistry table for Grade TP321H / UNS S32109 (public mill / specification PDF excerpt — _ref_a213.txt / A213–13 table text). Confirm the ordered edition. Where ellipses appear, the ordered edition sets no requirement for that element; nitrogen must still be known when titanium is checked against the 4 × (C + N) formula. Footnote B states the nitrogen analysis method is by agreement between purchaser and producer.

Product analysis — A480/A480M Table A1.1 tolerances applied

Element Melting Tolerance (A480 A1.1) Product analysis limit
Carbon (C) 0.04 – 0.10 0.01 under / over 0.03 – 0.11
Manganese (Mn) ≤ 2.00 0.04 over ≤ 2.04
Phosphorus (P) ≤ 0.045 0.010 over ≤ 0.055
Sulfur (S) ≤ 0.030 0.005 over ≤ 0.035
Silicon (Si) ≤ 1.00 0.05 over ≤ 1.05
Chromium (Cr) 17.0 – 19.0 0.20 under / over 16.80 – 19.20
Nickel (Ni) 9.0 – 12.0 0.10 under / 0.15 over 8.90 – 12.15
Titanium (Ti) ≥ 4 × (C+N), ≤ 0.70 0.05 over on max (Ti to 1.00 band practice) max ≤ 0.75 product; min tied to heat C+N

Carbon and stabilizer snapshot — TP321 / TP321H / TP304H / TP347H

Element TP321 (S32100) TP321H (S32109) TP304H (S30409) TP347H (S34709)
C ≤ 0.08 0.04 – 0.10 0.04 – 0.10 0.04 – 0.10
Cr 17.0 – 19.0 17.0 – 19.0 18.0 – 20.0 17.0 – 19.0
Ni 9.0 – 12.0 9.0 – 12.0 8.0 – 11.0 9.0 – 13.0
Stabilizer Ti ≥ 5 × (C+N), ≤ 0.70 Ti ≥ 4 × (C+N), ≤ 0.70 none Nb ≥ 8 × C, ≤ 1.10

Heats that also meet a non-H TP321 carbon ceiling while clearing the H-grade floor, titanium formula, tensile, hardness, and grain-size paths can be dual-certified TP321/TP321H when the purchase order asks for that dual marking — do not assume it from a PMI gun. Dual TP321H/TP304H is not a chemistry path: one grade requires titanium, the other does not. Versus niobium-stabilized A213 TP347H, TP321H carries titanium rather than niobium and uses the 4 × (C + N) formula instead of 8 × C.

When product analysis is ordered, finished tube may read C 0.03–0.11%, Mn ≤2.04%, P ≤0.055%, S ≤0.035%, Si ≤1.05%, Cr 16.80–19.20%, Ni 8.90–12.15%, and Ti max ≤0.75% with the formula minimum still tied to heat C + N. Put any tighter project carbon floor or titanium floor on the purchase order before the heat is selected — the H-grade carbon floor and Ti formula are intentional for elevated-temperature stabilized service.

Mechanical Properties of A213 TP321H

ASTM A213 Table 4 sets the room-temperature tensile acceptance floor for TP321H at 75 ksi [515 MPa] tensile strength and 30 ksi [205 MPa] yield strength (0.2% offset), with elongation of 35% minimum in 2 in. or 50 mm — the same room-temperature pair as TP321 and TP304H. Hardness maximum is 192 HBW / 200 HV or 90 HRB, and hardness tests are part of lot acceptance under A213. What distinguishes the H grade mechanically in the product standard is the grain-size requirement: ASTM No. 7 or coarser, determined per heat-treatment lot under the ordered edition’s clause referencing ASTM E112, sitting beside the titanium stabilization chemistry.

Property TP321H requirement
Tensile strength, min (Table 4) 75 ksi [515 MPa]
Yield strength (0.2% offset), min (Table 4) 30 ksi [205 MPa]
Elongation in 2 in. or 50 mm, min (Table 4) 35%
Hardness, max (Table 4) 192 HBW / 200 HV or 90 HRB
Grain size ASTM No. 7 or coarser (per heat-treatment lot)

Source: ASTM A213/A213M Table 4 for TP321H / UNS S32109 and H-grade grain-size language (public specification PDF excerpt — _ref_a213.txt / A213–13 heat-treatment table showing grain-size column “7” for TP321H). Mechanical property requirements do not apply to tubing smaller than 1/8 in. [3.2 mm] inside diameter or thinner than 0.015 in. [0.4 mm] wall. Flattening and flaring tests are also required on a lot basis.

Room-temperature tensile equality with TP321 is why dual 321/321H stock can look attractive when carbon and Ti clear both rows; elevated-temperature allowables in the design code, the carbon floor, the coarser grain, and the H-grade heat-treatment temperatures are why the H designation exists. A tensile-only MTC that omits grain size or titanium is incomplete for TP321H — ask for the E112 result and the Ti / (C+N) check on the certificate before releasing the heat to fabrication.

Dimensions and Tolerances

Dimensional supply for ASTM A213 TP321H is tube language — outside diameter × wall thickness (minimum wall or average wall) and, commercially, BWG / gauge — not ASME B36.19 pipe schedules as the primary size story. The sizes usually furnished under A213 run from about 1/8 in. [3.2 mm] inside diameter to 5 in. [127 mm] outside diameter, with minimum wall from about 0.015 to 0.500 in. [0.4 to 12.7 mm]; other diameters may be furnished when all other requirements are met. State on the purchase order whether wall is minimum or average — boiler and superheater datasheets almost always assume a minimum-wall reading.

Outside-diameter and wall variations follow ASTM A1016/A1016M as invoked by A213. Cold-finished tubes commonly hold tighter OD control; hot-finished tubes allow wider OD and wall windows. Permissible variations from a specified average wall for cold-finished tube are often summarized as ±10% of the specified average wall. Confirm the exact A1016 rows for the OD and finish route on the ordered edition.

Item Typical A213 TP321H dimensional practice
Product form Seamless only (cold-finished or hot-finished)
Usual size band ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD; wall ~0.015–0.500 in. [0.4–12.7 mm] min (or average wall if PO says so)
Wall basis Minimum wall (default for boiler / superheater) or average wall when specified
OD / wall tolerances Per ASTM A1016/A1016M for the finish route and size; cold-finished average wall often ±10%
Length Cut lengths for boiler / superheater / HX bundles, or mill random lengths by agreement
Secondary size note ASME B36.19 schedules may appear only when a buyer asks for a pipe-schedule cross-reference — not as the primary A213 size callout

Put the cut list, design metal temperature context, and end preparation on the enquiry so mill and stock lengths can be mixed efficiently. Minimum wall is a first-class A213 concept: if the datasheet assumes average wall, say so explicitly before the heat is rolled. For niobium-stabilized H-grade sizes under the same standard, compare A213 TP347H.

Equivalent Grades

Equivalence language around TP321H tube is often looser than a creep-range boiler purchase order can afford. ASTM A213 Grade TP321H / UNS S32109 is the governing designation for this article; EN 1.4941 / X8CrNiTi18-10 family names and JIS SUS321H / SUS321HTB are approximate wrought names that point to similar titanium-stabilized high-temperature 18-8 families but are not automatic substitutes on an A213 mill test certificate. When a datasheet says “equivalent to 321H,” confirm which product standard, tensile/hardness table, grain-size clause, titanium formula, and heat-treatment path the mill will actually certify.

Designation Notes
ASTM A213 / A213M Grade TP321H Governing ASTM seamless boiler / HX tube product standard for this article
UNS S32109 Unified number listed in the stainless chemistry table
ASME SA-213 TP321H Separate ASME Code Book adoption — dual-mark only when the PO asks
EN 1.4941 family (approx.) Approximate wrought Ti-stabilized H-grade designation; order EN tube forms under the relevant EN tube specs
JIS SUS321H / SUS321HTB Approximate Japanese grade / boiler-tube names; confirm the Japanese tube product standard
Related plate A240 / SA240 flat product in the same UNS family — order plate and tube under their own product standards

Dual A213/SA-213 marking is a purchase-order option, not a claim that the two standards are one document. Compare TP321, TP304H, and the niobium H grades on their own ASTM A213 pages before swapping grades on a familiar “321” PMI reading alone.

Heat Treatment and Delivery Condition

TP321H under ASTM A213 is furnished solution treated, then quenched in water or cooled rapidly by other means. The public heat-treatment table sets separate minimum solution temperatures by finish route: cold-worked tube at 2000 °F [1090 °C], and hot-rolled tube at 1925 °F [1050 °C], with Footnote H on the hot-rolled path. Grain size after heat treatment must meet ASTM No. 7 or coarser for the heat-treatment lot. That combination — finish-route solution temperature, titanium chemistry, and coarse-grain control — is what separates TP321H paperwork from a tensile-only TP321 certificate.

Footnote H warns that a solution treating temperature above 1950 °F [1065 °C] may impair intergranular-corrosion resistance after subsequent sensitizing exposure in the indicated grades, and allows a purchaser-specified lower-temperature stabilization or resolution anneal after the higher solution anneal. Supplementary Requirement S2 lists TP321H among grades that shall be given a stabilization heat treatment at a temperature lower than the initial solution anneal when the purchaser specifies S2 — temperature as agreed between purchaser and vendor. S2 is not automatic with the grade stamp.

Cold-finished versus hot-finished is a process and dimensional route that also selects which solution-temperature floor applies; it is not a substitute for the anneal or the grain-size check. Delivery condition for SHH STEEL TP321H is solution annealed and pickled (or bright annealed by agreement), with anneal temperature, quench method, titanium result, and grain-size result stated on the EN 10204 3.1 certificate. For non-H titanium stabilization open A213 TP321; for niobium H-grade open A213 TP347H; for fine-grain niobium H-grade open A213 TP347HFG.

Corrosion Resistance

TP321H’s chromium-rich passive film and titanium stabilization handle the oxidizing steam-side and many water-side duties typical of boiler and superheater service, with titanium tying up carbon that would otherwise form chromium carbides at grain boundaries during sensitizing thermal cycles. It is not selected primarily as a wet-chloride corrosion grade: the carbon floor that helps elevated-temperature strength still raises as-welded sensitization risk relative to low-carbon L grades when titanium is under-applied or when weld procedures leave unstabilized zones. In chloride-bearing cooling waters and many process exchangers, pitting and crevice attack become limiting, and buyers usually step to molybdenum-bearing grades rather than stretching H-grade Ti-stabilized 18-8 into wet corrosive service.

ASTM A213 itself does not publish a corrosion-rate table for TP321H; selection remains engineering judgment against fluid, temperature, velocity, and inspection philosophy inside the boiler or exchanger. When a specification calls for ASTM A262 Practice E, write Supplementary Requirement S4 onto the purchase order — and note that for titanium-bearing H grades a stabilization heat treatment under S2 may be necessary and is permitted to meet that requirement. SHH STEEL will not market TP321H as a wet-service upgrade over A213 TP304L — the H designation is about creep-range carbon, grain size, and Ti stabilization, not about better aqueous chloride resistance.

Applications of A213 TP321H Tube

TP321H seamless tube under A213 is chosen for creep-range boiler, superheater, and reheater service where the design code’s elevated-temperature allowables for S32109, the carbon floor, titanium stabilization, and the coarse-grain requirement earn their keep. It is the wrong default for as-welded wet corrosive exchangers that really need an L grade, and it is not a molybdenum grade for chlorides. The table below pairs typical application areas with a selection note.

Application area Typical use of TP321H tube Selection note
Boiler generating / screen tubes Seamless A213 tube where Ti-stabilized H-grade carbon and grain size are specified Confirm design metal temperature and code allowables for S32109
Superheater / reheater Creep-range steam tubing ordered to A213 TP321H For Nb-stabilized H grades open TP347H; for fine-grain TP347HFG open that page
High-temperature process HX Seamless tube where elevated-temperature strength plus Ti stabilization matter Prefer TP321 if H-grade carbon/grain size is not required; prefer TP304L if as-welded aqueous IGC is the only driver
Dual TP321/TP321H stock Heats that clear both chemistry (incl. Ti formula) and grain-size / tensile rows Ask for dual marking on the PO — do not assume from PMI alone
Stabilized 18-8 boiler tube Where A213 documentation is preferred over pipe product forms Do not substitute A312 pipe paperwork for A213 tube acceptance

For non-H titanium stabilization open A213 TP321; for unstabilized H-grade open A213 TP304H; for niobium H-grade open A213 TP347H / A213 TP347HFG on the A213/A213M hub.

Weldability

TP321H tube welds with matching or near-matching titanium-bearing austenitic filler for tube-to-tubesheet joints, attachment welds, and fabrication joins. Common practice uses ER321 / ER321H (or equivalent covered electrodes) under a qualified WPS so weld-metal titanium and carbon support elevated-temperature stabilized service; many fabricators avoid defaulting to ER308L when the base tube is H-grade Ti-stabilized and the design allowables assume H-grade carbon with stabilization. Heat input control, interpass limits, and post-weld cleaning remain the fabricator’s responsibility under the applicable boiler or pressure-vessel code — A213 governs the seamless tube product, not the field or shop weld procedure.

Because A213 TP321H is seamless, there is no mill longitudinal weld to radiograph the way welded pipe standards describe. Focus inspection language on tube integrity (hydro or NDE of each length), tube-to-tubesheet joint quality, grain-size and titanium documentation on the base metal, and any contractual corrosion test. For tube that will enter wet as-welded service in a sensitizing environment without relying on titanium, many owners change the base metal to A213 TP304L rather than stretching H-grade carbon into aqueous IGC duty. Specify end preparation and surface finish on the tube PO when orbital or clean-service joins are planned.

Surface Finishes

Standard mill delivery for ASTM A213 TP321H is solution annealed and pickled, leaving a clean matte finish suitable for most boiler and heat-exchanger tube duty. Bright annealing under protective atmosphere produces a smoother reflective surface used on some clean-process lines and must be called out because it changes the heat-treatment route — and must still deliver the required grain size and titanium chemistry. Light polish or specified Ra on the bore or OD is a commercial or service-center operation on top of A213 product, not automatic with the grade stamp.

When a fouling-sensitive exchanger specification quotes an Ra maximum on the bore, put it on the tube purchase order with its own acceptance language and sampling plan. SHH STEEL stencils grade, heat treatment, and (on request) H-grade / Ti identity as standard requirements; polish, special OD grind, and passivation after fabrication remain commercial extras unless the contract says otherwise. Order end preparation together with finish so receiving inspection shares one acceptance language.

Inspection and Testing

Base ASTM A213 testing for TP321H includes heat analysis (carbon inside 0.04–0.10%, titanium meeting ≥4 × (C + N) ≤0.70%), tension tests to the Table 4 floors (75/30 ksi), hardness tests to the Table 4 maximum (192 HBW / 90 HRB), grain-size determination (ASTM No. 7 or coarser) per heat-treatment lot, flattening and flaring tests on a lot basis, and either hydrostatic testing or nondestructive electric testing of each length. The manufacturer may choose hydro versus NDE unless the purchase order fixes the method. Marking includes the ASTM designation, grade, size, heat number, and other clause-required data.

Supplementary Requirements commonly added on TP321H tube orders are summarized below. Invoke them by number or clear purchase-order wording; mills will not assume product analysis, S2 stabilization, IGC testing, or dual TP321/TP321H marking from a verbal “full certs” note.

Option Purpose
Product analysis Confirms chemistry on finished tube — useful when carbon sits near the 0.04% floor or 0.10% ceiling, or when Ti is near the formula minimum
S2 stabilizing heat treatment Lower-temperature stabilization after the solution anneal — listed for TP321H when specified
S4 intergranular corrosion A262 Practice E; S2 may be necessary for Ti-bearing H grades to meet S4
Grain-size reporting Ensures E112 result appears on the MTC for the heat-treatment lot
Minimum vs average wall States which wall basis the size callout uses
Fixed hydro or NDE method Removes manufacturer’s option when the end user mandates one route
Third-party inspection / EN 10204 3.2 Witnessed testing and certificate when the project requires it

Ask the mill to state lot identity clearly on the certificate so hardness, tension, titanium, and grain-size specimens map cleanly to the bundle you receive. A tensile-only MTC without grain size or Ti is incomplete for TP321H.

Packaging and Shipping

TP321H tube leaves SHH STEEL bundled, capped or end-protected, and tagged for export or domestic delivery according to the length mix and bend form on the order. Bundle tags repeat the ASTM A213 grade, OD × wall (or BWG), heat number, and PO reference so site receiving can check the shipment without opening every certificate packet first. U-bent tubes need extra cradle or case protection so bend radii and legs are not distorted in transit.

Export packing can be bare bundles, wrapped bundles, or wooden-cased lengths for bright-annealed, polished, or small-bore material. We ship under the Incoterms on the order acknowledgement — FOB, CFR, CIF, EXW, or other agreed terms. Inland trucking, bilingual destination marks, or project color coding for bundle tags should be stated on the enquiry beside the metallurgical notes.

Why Choose SHH STEEL

SHH STEEL treats ASTM A213 TP321H as a product standard with enforceable chemistry (carbon floor and ceiling, titanium formula), tensile, hardness, grain-size, finish-route heat-treatment, and marking rules — not as a catalogue nickname for “any 321H tube.” The MTC reports the full ladle chemistry including titanium against 4 × (C + N), the Table 4 tensile/hardness set (75/30 ksi, 192 HBW / 90 HRB), and the grain-size result; the stencil carries seamless tube identity under A213; and dual A213/SA-213 marking is offered only when requested.

We keep the Ti-stabilized H-grade conversation honest for boiler and HX duty. If H-grade carbon and grain size are not required, we open A213 TP321. If the datasheet wants niobium instead of titanium, we open A213 TP347H or A213 TP347. If fine-grain creep framing is specified, we open A213 TP347HFG. If unstabilized H-grade 18-8 is enough, we open A213 TP304H. The A213/A213M hub is organized grade by grade under ASTM, seamless tube only.

Lead times combine near-term stock lengths with mill schedules; we say which is which on the quotation. Cut-to-length, U-bending, polish, and third-party inspection are defined extras. The tube that arrives should match the ASTM callout the engineer wrote, with paperwork a third-party inspector can read without translation.

Supply Capability

SHH STEEL can supply ASTM A213 TP321H stainless steel tube against the edition and finish route named on your enquiry. The capability table below summarizes the sizes, finishes, and documents we regularly quote for this grade, followed by the Stock / Available sizes map buyers ask for when they need a quick sense of what to enquire against for Ti-stabilized H-grade boiler and superheater duty.

Item SHH STEEL capability for TP321H
Standard ASTM A213 / A213M (dual SA-213 marking on request) Grade TP321H / UNS S32109
Product form Seamless only — cold-finished and hot-finished
Size Typical OD × min wall (or average wall) in the A213 usual band; other diameters by agreement
Wall / gauge Minimum wall or average wall; BWG / gauge callouts accepted on enquiry
Length Cut-to-length for boiler / superheater / HX bundles; mill random by agreement; U-bends on enquiry
Finish Annealed and pickled; bright annealed or light polish by agreement
Testing Tension (75/30 ksi), hardness (max 192 HBW / 90 HRB), grain size No. 7 or coarser, Ti vs 4×(C+N), flattening, flaring, hydro or NDE per length; full ladle chemistry on MTC; product analysis / S2 / S4 on order
Documents EN 10204 3.1 with full ladle chemistry, Ti, and grain-size result; third-party inspection / 3.2 on request
Trade terms FOB / CFR / CIF / EXW and other agreed Incoterms

Stock / Available sizes

SHH STEEL quotes TP321H tube against a practical stock-and-mill enquiry range rather than a frozen warehouse SKU list. The sizes below are OD × wall / BWG combinations buyers most often request for Ti-stabilized H-grade boiler and superheater tube; availability of any single line on a given week depends on mill drawing and our inbound schedule, so treat the table as a supply map for enquiry — not a guarantee of floor tonnage.

Item Typical stock / enquiry range for TP321H
Outside diameter 25.4, 31.8, 38.1, 44.5, 50.8, 63.5, 76.2, 88.9 mm (and other boiler/HX ODs on enquiry; up through the usual A213 ~5 in. [127 mm] band)
Wall / BWG BWG 10–16 class walls and metric min-wall equivalents; heavier walls for high-pressure boiler duty by agreement
Common OD × wall examples 31.8 × 2.77 mm; 38.1 × 3.05 mm; 50.8 × 3.05 mm; 50.8 × 3.40 mm; 63.5 × 3.40 mm; 76.2 × 3.40 mm — illustrative boiler/HX sizes, confirm min vs average wall
Length Cut lengths for boiler / superheater / exchanger bundles; U-bends and straight random lengths on enquiry
Special Non-standard OD/wall, bright anneal, dual TP321/TP321H marking, dual A213/SA-213 marking, S2 stabilization — confirm on enquiry before the heat is reserved

When you send an enquiry, list OD × wall (or BWG), wall basis (minimum or average), cold-finished or hot-finished preference, quantity or cut list, required marking (A213 alone, dual A213/SA-213, and/or dual TP321/TP321H), and any Supplementary Requirements (S2, S4, product analysis). We reply with what we can ship from near-term stock versus what needs a mill run, without inventing fake warehouse codes or tonnage claims.

Send the size list, finish route, quantity or cut lengths, required marking, Supplementary Requirements, and destination on one enquiry. We will confirm chemistry (including the carbon band and Ti formula), tensile, hardness, and grain size against the stainless chemistry table, Table 4, and the H-grade grain-size rule, state what ships from near-term availability versus mill production, and keep the offer aligned with ASTM A213 / A213M. Related grades such as A213 TP321, A213 TP347H, and A213 TP304H sit on the same hub when the datasheet steps beyond TP321H.

FAQ

Is ASTM A213 the same as ASME SA-213 for TP321H?
No. ASTM A213 / A213M is the ASTM International product specification for seamless boiler, superheater, and heat-exchanger tubes; ASME SA-213 / SA-213M is the separate ASME Code Book adoption of that grade text. Chemistry, tensile, hardness, titanium formula, and grain-size rules align closely for a given referenced edition, but they remain two independent standards. Dual-mark A213/SA-213 tube only when the purchase order asks for both names on the stencil and MTC.
Does ASTM A213 TP321H include welded or HCW tube?
No. ASTM A213 covers seamless tube only. There is no WLD or HCW manufacturing type under this product standard the way ASTM A312 describes pipe. The process choice for TP321H under A213 is cold-finished versus hot-finished seamless tube, plus the H-grade heat-treatment temperatures, grain-size, titanium, and testing clauses of the ordered edition.
How does TP321H differ from TP321 under ASTM A213?
TP321H holds carbon in a 0.04–0.10% range, uses titanium ≥4 × (C + N) ≤0.70% instead of the non-H 5 × (C + N) rule, requires ASTM grain size No. 7 or coarser, and applies finish-route solution temperatures (cold-worked 2000 °F [1090 °C]; hot-rolled 1925 °F [1050 °C]). TP321 allows carbon ≤0.08% with Ti ≥5 × (C + N) and no H-grade grain-size rule. Room-temperature Table 4 tensile (75/30 ksi) and hardness match; do not treat "321H" as a synonym stamp for ordinary TP321 on the MTC.
What is the UNS number and chemistry of ASTM A213 TP321H?
TP321H is UNS S32109. Melting limits include carbon 0.04–0.10%, manganese ≤2.00%, phosphorus ≤0.045%, sulfur ≤0.030%, silicon ≤1.00%, chromium 17.0–19.0%, nickel 9.0–12.0%, and titanium ≥4 × (C + N) ≤0.70%, with molybdenum and niobium as no-requirement ellipses. Nitrogen has no mandatory limit but must be known for the Ti formula; analysis method is by agreement (Footnote B). Confirm the ordered A213 edition for the exact stainless-table number.
Does A213 Table 4 set a hardness limit for TP321H?
Yes. Table 4 for TP321H lists tensile strength, yield strength, elongation, and a hardness maximum of 192 HBW / 200 HV or 90 HRB. Hardness tests are part of lot acceptance under A213, which differs from many A312 pipe rows for the same UNS number that omit a Table 4 hardness cap. Grain size (No. 7 or coarser) sits beside those Table 4 numbers as an H-grade acceptance item.
Why does ASTM A213 control grain size on TP321H?
Coarse grain (ASTM No. 7 or coarser) after the finish-route solution treatment supports the elevated-temperature creep-rupture behavior that the H designation is written for, sitting beside titanium stabilization. A tensile-only MTC without an E112 grain-size result is incomplete for TP321H. Ask the mill to report grain size per heat-treatment lot on the EN 10204 3.1 certificate before releasing the heat to fabrication.
What heat treatment does ASTM A213 require for TP321H?
TP321H is solution treated at a minimum of 2000 °F [1090 °C] for cold-worked tube or 1925 °F [1050 °C] for hot-rolled tube, then water quenched or rapidly cooled, with grain size No. 7 or coarser for the heat-treatment lot. Footnote H and Supplementary Requirement S2 address high solution temperature / stabilization when ordered. Ask the mill to state anneal temperature, quench method, titanium, and grain-size result on the EN 10204 3.1 certificate.
What is Supplementary Requirement S2 for TP321H?
S2 requires a stabilization heat treatment at a temperature lower than the initial solution anneal, with the temperature agreed between purchaser and vendor. The public A213–13 excerpt lists TP321H among grades that shall receive S2 when specified. For titanium-bearing H grades, S2 may also be necessary and is permitted to meet Supplementary Requirement S4 (A262 Practice E). S2 is never automatic with the grade stamp alone.
TP321H vs TP347H — titanium or niobium for H-grade tube?
Both are H-grade stabilized austenitics with carbon 0.04–0.10% and grain size No. 7 or coarser. TP321H uses titanium ≥4 × (C + N) ≤0.70% with Ni 9–12%; TP347H uses niobium ≥8 × C ≤1.10% with Ni 9–13%. Filler metal, high-temperature allowables, and end-user preference often decide; do not swap them on a familiar "stabilized 321/347" PMI reading without checking the datasheet’s stabilizer and UNS number.
Can TP321H tube be dual certified TP321/TP321H?
Yes when ladle carbon meets the H-grade band while also clearing the TP321 carbon ceiling, when titanium clears both the 4 × and 5 × (C + N) floors for the heat’s C + N, and when tensile, hardness, and grain-size results clear both acceptance paths. Spell the required dual marking on the enquiry so the heat and heat-treatment route are selected correctly before rolling.
Minimum wall vs average wall — which should I order for A213 TP321H?
Order minimum wall when the boiler or superheater datasheet is written around a guaranteed minimum thickness after tolerance — the usual practice for A213 H-grade tube. Order average wall only when the purchase order explicitly allows average-wall product and the designer has accepted that basis. Put the wall basis on the enquiry before the mill selects A1016 tolerance tables.
Is TP321H a good choice for wet corrosive heat-exchanger service?
Usually no as a first choice for chloride-rich aqueous duty. The carbon floor that helps elevated-temperature strength and the absence of molybdenum mean pitting and crevice attack can limit life; titanium helps IGC when properly applied but does not replace Mo for chlorides. Prefer TP304L or TP316L for wet as-welded service; reserve TP321H for creep-range boiler and superheater framing where Ti-stabilized H-grade rules earn their keep.

Conclusion

ASTM A213 TP321H / UNS S32109 is the titanium-stabilized, carbon-controlled, coarse-grain seamless stainless steel tube grade for creep-range boiler, superheater, and heat-exchanger service when elevated-temperature allowables, a 0.04–0.10% carbon band, titanium ≥4 × (C + N) ≤0.70%, finish-route solution temperatures, and ASTM grain size No. 7 or coarser share one datasheet. SHH STEEL supplies cold-finished and hot-finished seamless tube in the usual OD × wall / BWG band, solution annealed, tested to Table 4 tensile and hardness limits with titanium and grain size reported, and documented on EN 10204 3.1 certificates — with dual SA-213 marking only when the order asks for that separate ASME standard. For sister grades and stock-oriented size discussions, start from the A213/A213M hub, then send your OD × wall list, wall basis, dual-marking needs, and Ti / grain-size / S2 requirements so we can align mill and near-term availability to the ASTM callout.

Contact: admin@steelspecs.com

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X