ASTM A213 TP348 Stainless Steel Tube | ASTM A213 Stainless Steel - SHH STEEL

ASTM A213 TP348 Stainless Steel Tube

ASTM A213 TP348 / UNS S34800 seamless boiler, superheater and heat-exchanger tube with carbon ≤0.08%, Cr 17.0–19.0%, Ni 9.0–13.0%, Nb+Ta ≥10×C ≤1.10%, cobalt ≤0.20%, tantalum ≤0.10%, Table 4 floor 75/30 ksi, and hardness max 192 HBW / 90 HRB. SHH STEEL supplies cold-finished and hot-finished seamless tube solution treated at 1900 °F [1040 °C] with EN 10204 3.1 MTCs that report Nb+Ta, Co, and Ta.
Grade
TP348 / UNS S34800
Standard
ASTM A213 / A213M
Product form
Seamless boiler / superheater / heat-exchanger tube (cold-finished and hot-finished)
Size
Typical OD × min wall (or average wall) within ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD and ~0.015–0.500 in. [0.4–12.7 mm] wall; other diameters by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is ASTM A213 TP348 Stainless Steel Tube

ASTM A213 / A213M is the ASTM International product specification for seamless ferritic and austenitic alloy-steel boiler, superheater, and heat-exchanger tubes. Grade TP348 / UNS S34800 is the cobalt- and tantalum-controlled niobium-stabilized austenitic stainless member of that stainless table: melting carbon is capped at 0.08%, chromium 17.0–19.0%, nickel 9.0–13.0%, niobium-plus-tantalum held at ≥10 × C and ≤1.10% (Footnote G), cobalt ≤0.20%, and tantalum ≤0.10%. Versus A213 TP347, the stabilizer is written as Nb + Ta rather than Nb alone, chromium narrows to 17–19%, and the Co/Ta ceilings are first-class melting limits — historically important for nuclear and low-cobalt purchase orders that still show up on boiler and HX enquiries. Buyers who write “348 tube” still need to name A213 (or the separate ASME SA-213 adoption) on the purchase order so the mill applies Nb+Ta / Co / Ta chemistry, heat-treatment, test, and marking clauses rather than a loose shop nickname.

SHH STEEL can supply ASTM A213 TP348 stainless steel tube as seamless cold-finished and hot-finished product in the usual boiler and heat-exchanger OD × wall / BWG band, shipped with EN 10204 3.1 mill test certificates that report the full ladle chemistry (including Nb + Ta against the 10 × C formula, cobalt, and tantalum), the Table 4 tensile and hardness results, and the anneal temperature for the heat-treatment lot. When a project also needs ASME Code Book marking, we dual-mark A213 / SA-213 on the same lengths only if the purchase order says so. Browse the grade family on the A213/A213M hub.

Commercially, TP348 tube is still called 348, S34800, or Co-controlled Nb-stabilized boiler tube; none of those shop names replace the ASTM grade on the MTC or stencil. Sister grades under the same ASTM standard include A213 TP348H, A213 TP347, A213 TP347H, A213 TP321, and A213 TP347LN. A213 covers seamless tube only — no welded or HCW manufacturing type — so cold-finished versus hot-finished is the process choice, not a WLD/HCW stencil letter.

Chemical Composition of A213 TP348

Two chemistry layers matter for TP348 under ASTM A213. Melting (heat or ladle) analysis is mandatory for every heat; product analysis on finished tube applies only when Supplementary Requirement wording or the purchase order invokes it through ASTM A1016/A1016M. Product-analysis tolerances typically flow from ASTM A480/A480M Table A1.1. SHH STEEL reports actual ladle values — and product values when ordered — and does not advertise unpublished tighter catalogue windows. Three lines define the grade for a reviewer: Nb + Ta ≥10 × C and ≤1.10% (Footnote G), cobalt ≤0.20%, and tantalum ≤0.10%. A heat with 0.06% carbon needs at least 0.60% Nb + Ta, while a leaner-carbon heat can clear the formula with less stabilizer, still capped at 1.10%. Chromium 17.0–19.0% is narrower than TP347’s 17.0–20.0% window. Do not treat a familiar “347” PMI reading as proof of Co/Ta control — those ceilings must appear on the ladle report.

The tables below reproduce the heat analysis for TP348 / UNS S34800, the product-analysis limits from A480 Table A1.1 practice, and a short Nb+Ta / Co / Ta snapshot against TP347, TP348H, and TP347H. Later A213 editions place austenitic stainless grades in Table 2 (older editions used Table 1); confirm the ordered edition on the purchase order. A480 product-tolerance digits for Co and Ta maxima are applied from sister-pack practice and labeled UNCERTAIN pending the ordered A480 edition.

Melting analysis (heat / ladle analysis)

Element TP348 (UNS S34800) melting analysis
Carbon (C) ≤ 0.08
Manganese (Mn) ≤ 2.00
Phosphorus (P) ≤ 0.045
Sulfur (S) ≤ 0.030
Silicon (Si) ≤ 1.00
Chromium (Cr) 17.0 – 19.0
Nickel (Ni) 9.0 – 13.0
Molybdenum (Mo) … (no requirement)
Nitrogen (N) … (no requirement)
Niobium + Tantalum (Nb + Ta) ≥ 10 × C, ≤ 1.10 (Footnote G)
Cobalt (Co) ≤ 0.20
Tantalum (Ta) ≤ 0.10
Titanium (Ti) … (no requirement)

Source: ASTM A213/A213M stainless chemistry table for Grade TP348 / UNS S34800 (public mill / specification PDF excerpt — _ref_a213.txt / A213–13 table text). Confirm the ordered edition. Where ellipses appear, the ordered edition sets no requirement for that element. Older shop language still says “columbium”; modern MTCs usually print Nb, with Ta reported separately against the ≤0.10% ceiling.

Product analysis — A480/A480M Table A1.1 tolerances applied

Element Melting Tolerance (A480 A1.1) Product analysis limit
Carbon (C) ≤ 0.08 0.01 over ≤ 0.09
Manganese (Mn) ≤ 2.00 0.04 over ≤ 2.04
Phosphorus (P) ≤ 0.045 0.010 over ≤ 0.055
Sulfur (S) ≤ 0.030 0.005 over ≤ 0.035
Silicon (Si) ≤ 1.00 0.05 over ≤ 1.05
Chromium (Cr) 17.0 – 19.0 0.20 under / over 16.80 – 19.20
Nickel (Ni) 9.0 – 13.0 0.15 under / 0.20 over 8.85 – 13.20
Nb + Ta ≥ 10 × C, ≤ 1.10 0.05 over on max (Nb formula practice) max ≤ 1.15 product; min tied to heat C
Cobalt (Co) ≤ 0.20 0.03 over (UNCERTAIN — confirm A480) ≤ 0.23
Tantalum (Ta) ≤ 0.10 0.02 over (UNCERTAIN — confirm A480) ≤ 0.12

Stabilizer / Co / Ta snapshot — TP347 / TP348 / TP348H / TP347H

Element TP347 (S34700) TP348 (S34800) TP348H (S34809) TP347H (S34709)
C ≤ 0.08 ≤ 0.08 0.04 – 0.10 0.04 – 0.10
Cr 17.0 – 20.0 17.0 – 19.0 17.0 – 19.0 17.0 – 19.0
Stabilizer Nb ≥ 10 × C, ≤ 1.10 Nb+Ta ≥ 10 × C, ≤ 1.10 Nb+Ta ≥ 8 × C, ≤ 1.10 Nb ≥ 8 × C, ≤ 1.10
Co / Ta not listed Co ≤ 0.20; Ta ≤ 0.10 Co ≤ 0.20; Ta ≤ 0.10 not listed

Heats that also meet an H-grade carbon floor while clearing the TP348 carbon ceiling, the tighter H-grade Nb+Ta formula (8 × C), Co/Ta ceilings, tensile, hardness, and grain-size paths can be dual-certified TP348/TP348H when the purchase order asks — do not assume it from a PMI gun. Dual TP348/TP347 is not automatic either: TP347 lacks Co/Ta ceilings and writes the stabilizer as Nb alone with a wider Cr window. Versus A213 TP347, order TP348 when Co and Ta control are on the datasheet.

When product analysis is ordered, finished tube may read C ≤0.09%, Mn ≤2.04%, P ≤0.055%, S ≤0.035%, Si ≤1.05%, Cr 16.80–19.20%, Ni 8.85–13.20%, Nb+Ta max ≤1.15% with the formula minimum still tied to heat carbon, Co ≤0.23%, and Ta ≤0.12% under the A480 practice digits above. Put any tighter project cobalt or tantalum ceiling on the purchase order before the heat is selected.

Mechanical Properties of A213 TP348

ASTM A213 Table 4 sets the room-temperature tensile acceptance floor for TP348 at 75 ksi [515 MPa] tensile strength and 30 ksi [205 MPa] yield strength (0.2% offset), with elongation of 35% minimum in 2 in. or 50 mm — the same room-temperature pair as TP347 and TP321. Hardness maximum is 192 HBW / 200 HV or 90 HRB, and hardness tests are part of lot acceptance under A213. The public heat-treatment table does not print a mandatory ASTM grain-size number for TP348 (unlike TP348H’s “7”), so a tensile-and-hardness MTC without grain size can still be complete for non-H TP348 unless the purchase order adds a grain-size Supplementary Requirement.

Property TP348 requirement
Tensile strength, min (Table 4) 75 ksi [515 MPa]
Yield strength (0.2% offset), min (Table 4) 30 ksi [205 MPa]
Elongation in 2 in. or 50 mm, min (Table 4) 35%
Hardness, max (Table 4) 192 HBW / 200 HV or 90 HRB
Grain size No mandatory ASTM number in the public Table 3 row (confirm ordered edition)

Source: ASTM A213/A213M Table 4 for TP348 / UNS S34800 (public specification PDF excerpt — _ref_a213.txt / A213–13). Mechanical property requirements do not apply to tubing smaller than 1/8 in. [3.2 mm] inside diameter or thinner than 0.015 in. [0.4 mm] wall. Flattening and flaring tests are also required on a lot basis.

Room-temperature tensile equality with sister 18-8 grades is why buyers sometimes look for dual marking with TP347; Co/Ta ceilings and the Nb+Ta formula are why TP348 exists as its own row. A tensile-only MTC that omits Nb+Ta, Co, or Ta is incomplete — ask for those checks on the certificate before releasing the heat to fabrication. For H-grade grain-size and carbon-floor framing open A213 TP348H.

Dimensions and Tolerances

Dimensional supply for ASTM A213 TP348 is tube language — outside diameter × wall thickness (minimum wall or average wall) and, commercially, BWG / gauge — not ASME B36.19 pipe schedules as the primary size story. The sizes usually furnished under A213 run from about 1/8 in. [3.2 mm] inside diameter to 5 in. [127 mm] outside diameter, with minimum wall from about 0.015 to 0.500 in. [0.4 to 12.7 mm]; other diameters may be furnished when all other requirements are met. State on the purchase order whether wall is minimum or average — boiler and heat-exchanger datasheets almost always assume a minimum-wall reading.

Outside-diameter and wall variations follow ASTM A1016/A1016M as invoked by A213. Cold-finished tubes commonly hold tighter OD control; hot-finished tubes allow wider OD and wall windows. Permissible variations from a specified average wall for cold-finished tube are often summarized as ±10% of the specified average wall. Confirm the exact A1016 rows for the OD and finish route on the ordered edition.

Item Typical A213 TP348 dimensional practice
Product form Seamless only (cold-finished or hot-finished)
Usual size band ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD; wall ~0.015–0.500 in. [0.4–12.7 mm] min (or average wall if PO says so)
Wall basis Minimum wall (default for boiler / HX) or average wall when specified
OD / wall tolerances Per ASTM A1016/A1016M for the finish route and size; cold-finished average wall often ±10%
Length Cut lengths for boiler / superheater / HX bundles, or mill random lengths by agreement
Secondary size note ASME B36.19 schedules may appear only when a buyer asks for a pipe-schedule cross-reference — not as the primary A213 size callout

Put the cut list and end preparation on the enquiry so mill and stock lengths can be mixed efficiently. Minimum wall is a first-class A213 concept: if the datasheet assumes average wall, say so explicitly before the heat is rolled.

Equivalent Grades

Equivalence language around TP348 tube is often looser than a Co/Ta-controlled purchase order can afford. ASTM A213 Grade TP348 / UNS S34800 is the governing designation for this article; EN or JIS wrought names that mention “348” or low-cobalt Nb-stabilized 18-8 point to related families but are not automatic substitutes on an A213 mill test certificate. When a datasheet says “equivalent to 348,” confirm which product standard, tensile/hardness table, Nb+Ta formula, Co/Ta ceilings, and heat-treatment path the mill will actually certify.

Designation Notes
ASTM A213 / A213M Grade TP348 Governing ASTM seamless boiler / HX tube product standard for this article
UNS S34800 Unified number listed in the stainless chemistry table
ASME SA-213 TP348 Separate ASME Code Book adoption — dual-mark only when the PO asks
Related Nb grades TP347 / S34700 (Nb alone, no Co/Ta ceilings); TP348H / S34809 (H-grade Nb+Ta)
Related plate A240 / SA240 flat product in related UNS families — order plate and tube under their own product standards

Dual A213/SA-213 marking is a purchase-order option, not a claim that the two standards are one document. Compare TP347, TP348H, and TP321 on their own ASTM A213 pages before swapping grades on a familiar “348” PMI reading alone.

Heat Treatment and Delivery Condition

TP348 under ASTM A213 is furnished solution treated at a minimum of 1900 °F [1040 °C], then quenched in water or cooled rapidly by other means. The public heat-treatment table marks this row with Footnotes F and H. Footnote F ties quench capability to A262 Practice E demonstrability when that test is ordered (Supplementary Requirement S4); Footnote H warns that a solution treating temperature above 1950 °F [1065 °C] may impair intergranular-corrosion resistance after subsequent sensitizing exposure, and allows a purchaser-specified lower-temperature stabilization or resolution anneal after the higher solution anneal. The public table does not print a mandatory ASTM grain-size number for TP348.

Supplementary Requirement S2 lists TP348 among grades that shall be given a stabilization heat treatment at a temperature lower than the initial solution anneal when the purchaser specifies S2 — temperature as agreed between purchaser and vendor. Supplementary Requirement S1 allows stress-relieved annealed TP348 (1500–1650 °F [815–900 °C] after roll straightening) for certain chloride stress-corrosion services when ordered — S1 names TP304L, TP316L, TP321, TP347, and TP348. Neither S1 nor S2 is automatic with the grade stamp.

Cold-finished versus hot-finished is a process and dimensional route, not a substitute for the anneal. Delivery condition for SHH STEEL TP348 is solution annealed and pickled (or bright annealed by agreement), with anneal temperature, quench method, and Nb+Ta / Co / Ta results on the EN 10204 3.1 certificate. For H-grade carbon and grain-size controls open A213 TP348H; for Nb-only framing without Co/Ta ceilings open A213 TP347.

Corrosion Resistance

TP348’s chromium-rich passive film and Nb+Ta stabilization handle many boiler, superheater, and heat-exchanger duties where sensitizing thermal cycles would otherwise deplete chromium at grain boundaries. Niobium and tantalum form preferential carbides so chromium stays available for the passive film — that is the grade’s IGC strategy, not an L-grade carbon ceiling and not a molybdenum addition for chlorides. The Co and Ta ceilings are purchase-order chemistry controls, not corrosion upgrades. In chloride-bearing cooling waters and many process exchangers, pitting and crevice attack become limiting, and buyers usually step to A213 TP316 / A213 TP316L or a higher-PREN grade rather than stretching Nb-stabilized 18-8 into wet corrosive service.

ASTM A213 itself does not publish a corrosion-rate table for TP348; selection remains engineering judgment against fluid, temperature, velocity, and inspection philosophy. When a specification calls for ASTM A262 Practice E, write Supplementary Requirement S4 onto the purchase order — and note that for niobium/tantalum-bearing grades a stabilization heat treatment under S2 may be necessary and is permitted to meet that requirement. SHH STEEL will not market TP348 as a wet-chloride upgrade over molybdenum grades; the Co/Ta designation is about controlled chemistry, not about higher PREN.

Applications of A213 TP348 Tube

TP348 seamless tube under A213 is chosen for boiler, superheater, and heat-exchanger service where Nb+Ta stabilization plus cobalt and tantalum ceilings must appear on the mill certificate. It is a common selection when nuclear, low-cobalt, or Co/Ta-controlled specifications name S34800 rather than S34700. It is the wrong default for chloride-rich cooling water that really needs Mo, and it is not an H-grade creep row unless the PO also clears TP348H chemistry and grain size. The table below pairs typical application areas with a selection note.

Application area Typical use of TP348 tube Selection note
Boiler / steam HX Seamless A213 tube where Nb+Ta and Co/Ta control are specified Confirm Nb+Ta ≥10×C, Co ≤0.20, Ta ≤0.10 on the MTC
Low-cobalt / Co-controlled specs Stabilized steam tubing ordered to S34800 Do not substitute TP347 without checking Co/Ta
Process heat exchangers Seamless tube for sensitizing thermal cycles with Co control Prefer TP316L when chlorides dominate
Stress-relieved service (S1) TP348 ordered stress-relieved annealed for certain chloride SCC duties S1 is PO language — not automatic
Dual TP348/TP348H stock Heats that clear both chemistry and H-grade grain-size / tensile rows Ask for dual marking on the PO

For Nb-only framing open A213 TP347; for H-grade Co/Ta open A213 TP348H; for titanium stabilization open A213 TP321 on the A213/A213M hub.

Weldability

TP348 tube welds with matching or near-matching niobium-bearing austenitic filler for tube-to-tubesheet joints, attachment welds, and fabrication joins. Common practice uses ER347 / E347 (or equivalent covered electrodes; some specifications call ER348 when Co/Ta control extends into the filler) under a qualified WPS so weld-metal niobium supports stabilized service. Many fabricators avoid defaulting to ER308L when the base tube is Nb+Ta-stabilized and the design assumes stabilization chemistry in the joint. Heat input control, interpass limits, and post-weld cleaning remain the fabricator’s responsibility under the applicable boiler or pressure-vessel code — A213 governs the seamless tube product, not the field or shop weld procedure.

Because A213 TP348 is seamless, there is no mill longitudinal weld to radiograph the way welded pipe standards describe. Focus inspection language on tube integrity (hydro or NDE of each length), tube-to-tubesheet joint quality, Nb+Ta / Co / Ta documentation on the base metal, and any contractual corrosion test. For tube that will enter wet as-welded service where an L-grade carbon ceiling is preferred over Nb chemistry, many owners change the base metal to A213 TP304L. Specify end preparation and surface finish on the tube PO when orbital or clean-service joins are planned.

Surface Finishes

Standard mill delivery for ASTM A213 TP348 is solution annealed and pickled, leaving a clean matte finish suitable for most boiler and heat-exchanger tube duty. Bright annealing under protective atmosphere produces a smoother reflective surface used on some clean-process lines and must be called out because it changes the heat-treatment route. Light polish or specified Ra on the bore or OD is a commercial or service-center operation on top of A213 product, not automatic with the grade stamp.

When a fouling-sensitive exchanger specification quotes an Ra maximum on the bore, put it on the tube purchase order with its own acceptance language and sampling plan. SHH STEEL stencils grade and heat treatment as standard requirements; polish, special OD grind, and passivation after fabrication remain commercial extras unless the contract says otherwise. Order end preparation together with finish so receiving inspection shares one acceptance language.

Inspection and Testing

Base ASTM A213 testing for TP348 includes heat analysis (carbon ≤0.08%, Nb+Ta meeting ≥10 × C ≤1.10%, cobalt ≤0.20%, tantalum ≤0.10%), tension tests to the Table 4 floors (75/30 ksi), hardness tests to the Table 4 maximum (192 HBW / 90 HRB), flattening and flaring tests on a lot basis, and either hydrostatic testing or nondestructive electric testing of each length. The manufacturer may choose hydro versus NDE unless the purchase order fixes the method. Marking includes the ASTM designation, grade, size, heat number, and other clause-required data. Grain-size reporting is not a mandatory Table 3 item for TP348 in the public excerpt unless the PO adds it.

Supplementary Requirements commonly added on TP348 tube orders are summarized below. Invoke them by number or clear purchase-order wording; mills will not assume product analysis, S1 stress relief, S2 stabilization, or IGC testing from a verbal “full certs” note.

Option Purpose
Product analysis Confirms chemistry on finished tube — useful when Nb+Ta, Co, or Ta sits near a limit
S1 stress-relieved anneal 1500–1650 °F [815–900 °C] after roll straightening for certain chloride SCC duties (listed for TP348)
S2 stabilizing heat treatment Lower-temperature stabilization after the solution anneal — listed for TP348 when specified
S4 intergranular corrosion A262 Practice E; S2 may be necessary for Nb/Ta-bearing grades to meet S4
Minimum vs average wall States which wall basis the size callout uses
Fixed hydro or NDE method Removes manufacturer’s option when the end user mandates one route
Third-party inspection / EN 10204 3.2 Witnessed testing and certificate when the project requires it

Ask the mill to state lot identity clearly on the certificate so hardness, tension, and Nb+Ta / Co / Ta specimens map cleanly to the bundle you receive.

Packaging and Shipping

TP348 tube leaves SHH STEEL bundled, capped or end-protected, and tagged for export or domestic delivery according to the length mix and bend form on the order. Bundle tags repeat the ASTM A213 grade, OD × wall (or BWG), heat number, and PO reference so site receiving can check the shipment without opening every certificate packet first. U-bent tubes need extra cradle or case protection so bend radii and legs are not distorted in transit.

Export packing can be bare bundles, wrapped bundles, or wooden-cased lengths for bright-annealed, polished, or small-bore material. We ship under the Incoterms on the order acknowledgement — FOB, CFR, CIF, EXW, or other agreed terms. Inland trucking, bilingual destination marks, or project color coding for bundle tags should be stated on the enquiry beside the metallurgical notes.

Why Choose SHH STEEL

SHH STEEL treats ASTM A213 TP348 as a product standard with enforceable chemistry (Nb+Ta formula, Co and Ta ceilings), tensile, hardness, heat-treatment, and marking rules — not as a catalogue nickname for “any 348 tube.” The MTC reports the full ladle chemistry including Nb + Ta against 10 × C, cobalt, and tantalum, the Table 4 tensile/hardness set (75/30 ksi, 192 HBW / 90 HRB), and the anneal temperature; the stencil carries seamless tube identity under A213; and dual A213/SA-213 marking is offered only when requested.

We keep the Co/Ta conversation honest for boiler and HX duty. If Nb-only without Co/Ta ceilings is enough, we open A213 TP347. If H-grade carbon and grain size with Co/Ta are required, we open A213 TP348H. If titanium is preferred over Nb+Ta, we open A213 TP321 / A213 TP321H. If chlorides dominate, we open A213 TP316L. The A213/A213M hub is organized grade by grade under ASTM, seamless tube only.

Lead times combine near-term stock lengths with mill schedules; we say which is which on the quotation. Cut-to-length, U-bending, polish, and third-party inspection are defined extras. The tube that arrives should match the ASTM callout the engineer wrote, with paperwork a third-party inspector can read without translation.

Supply Capability

SHH STEEL can supply ASTM A213 TP348 stainless steel tube against the edition and finish route named on your enquiry. The capability table below summarizes the sizes, finishes, and documents we regularly quote for this grade, followed by the Stock / Available sizes map buyers ask for when they need a quick sense of what to enquire against for Co/Ta-controlled Nb-stabilized boiler and heat-exchanger duty.

Item SHH STEEL capability for TP348
Standard ASTM A213 / A213M (dual SA-213 marking on request) Grade TP348 / UNS S34800
Product form Seamless only — cold-finished and hot-finished
Size Typical OD × min wall (or average wall) in the A213 usual band; other diameters by agreement
Wall / gauge Minimum wall or average wall; BWG / gauge callouts accepted on enquiry
Length Cut-to-length for boiler / superheater / HX bundles; mill random by agreement; U-bends on enquiry
Finish Annealed and pickled; bright annealed or light polish by agreement
Testing Tension (75/30 ksi), hardness (max 192 HBW / 90 HRB), Nb+Ta vs 10×C, Co, Ta, flattening, flaring, hydro or NDE per length; full ladle chemistry on MTC; product analysis / S1 / S2 / S4 on order
Documents EN 10204 3.1 with full ladle chemistry and Nb+Ta / Co / Ta results; third-party inspection / 3.2 on request
Trade terms FOB / CFR / CIF / EXW and other agreed Incoterms

Stock / Available sizes

SHH STEEL quotes TP348 tube against a practical stock-and-mill enquiry range rather than a frozen warehouse SKU list. The sizes below are OD × wall / BWG combinations buyers most often request for Co/Ta-controlled Nb-stabilized boiler and heat-exchanger tube; availability of any single line on a given week depends on mill drawing and our inbound schedule, so treat the table as a supply map for enquiry — not a guarantee of floor tonnage.

Item Typical stock / enquiry range for TP348
Outside diameter 19.05, 25.4, 31.8, 38.1, 44.5, 50.8, 63.5, 76.2 mm (and other boiler/HX ODs on enquiry; up through the usual A213 ~5 in. [127 mm] band)
Wall / BWG BWG 12–18 class walls and metric min-wall equivalents; heavier walls for high-pressure duty by agreement
Common OD × wall examples 25.4 × 2.11 mm; 31.8 × 2.41 mm; 38.1 × 2.77 mm; 50.8 × 2.77 mm; 50.8 × 3.05 mm — illustrative HX/boiler sizes, confirm min vs average wall
Length Cut lengths for boiler / exchanger bundles; U-bends and straight random lengths on enquiry
Special Non-standard OD/wall, bright anneal, S1 stress relief, S2 stabilization, dual TP348/TP348H marking, dual A213/SA-213 marking — confirm on enquiry before the heat is reserved

When you send an enquiry, list OD × wall (or BWG), wall basis (minimum or average), cold-finished or hot-finished preference, quantity or cut list, required marking (A213 alone, dual A213/SA-213, and/or dual TP348/TP348H), and any Supplementary Requirements (S1, S2, S4, product analysis). We reply with what we can ship from near-term stock versus what needs a mill run, without inventing fake warehouse codes or tonnage claims.

Send the size list, finish route, quantity or cut lengths, required marking, Supplementary Requirements, and destination on one enquiry. We will confirm chemistry (including the Nb+Ta formula and Co/Ta ceilings), tensile, and hardness against the stainless chemistry table and Table 4, state what ships from near-term availability versus mill production, and keep the offer aligned with ASTM A213 / A213M. Related grades such as A213 TP348H, A213 TP347, and A213 TP321 sit on the same hub when the datasheet steps beyond TP348.

FAQ

Is ASTM A213 the same as ASME SA-213 for TP348?
No. ASTM A213 / A213M is the ASTM International product specification for seamless boiler, superheater, and heat-exchanger tubes; ASME SA-213 / SA-213M is the separate ASME Code Book adoption of that grade text. Chemistry, tensile, hardness, and Nb+Ta / Co / Ta rules align closely for a given referenced edition, but they remain two independent standards. Dual-mark A213/SA-213 tube only when the purchase order asks for both names on the stencil and MTC.
Does ASTM A213 TP348 include welded or HCW tube?
No. ASTM A213 covers seamless tube only. There is no WLD or HCW manufacturing type under this product standard the way ASTM A312 describes pipe. The process choice for TP348 under A213 is cold-finished versus hot-finished seamless tube, plus the Nb+Ta formula, Co/Ta ceilings, heat-treatment, and testing clauses of the ordered edition.
What is the UNS number and chemistry of ASTM A213 TP348?
TP348 is UNS S34800. Melting limits include carbon ≤0.08%, manganese ≤2.00%, phosphorus ≤0.045%, sulfur ≤0.030%, silicon ≤1.00%, chromium 17.0–19.0%, nickel 9.0–13.0%, Nb + Ta ≥10 × C ≤1.10% (Footnote G), cobalt ≤0.20%, and tantalum ≤0.10%. Product-analysis limits apply only when ordered, typically from A480 Table A1.1 via A1016. Confirm the ordered A213 edition for the exact stainless-table number.
TP348 vs TP347 — why control cobalt and tantalum?
Both are Nb-family stabilized austenitics with carbon ≤0.08% and no mandatory Table 3 grain-size number in the public excerpt. TP348 writes the stabilizer as Nb + Ta ≥10 × C ≤1.10%, narrows chromium to 17–19%, and adds Co ≤0.20% and Ta ≤0.10%. TP347 uses Nb alone ≥10 × C ≤1.10% with Cr 17–20% and no Co/Ta ceilings. Order TP348 when Co/Ta control is on the datasheet; order TP347 when Nb-only chemistry is enough.
TP348 vs TP348H — when do I need the H grade?
Order TP348H when the boiler or superheater datasheet needs H-grade carbon 0.04–0.10%, Nb+Ta ≥8 × C ≤1.10%, ASTM grain size No. 7 or coarser, and the finish-route solution temperatures written for the H row. Order TP348 when Nb+Ta ≥10 × C with C ≤0.08%, Co/Ta ceilings, and the 1900 °F solution path are enough without H-grade grain-size framing. They share Co/Ta control but are not synonym stamps on the MTC.
What do Footnotes F and H mean for TP348 heat treatment?
Footnote F ties the quench rate to A262 Practice E capability when that test is ordered under Supplementary Requirement S4. Footnote H warns that solution treating above 1950 °F [1065 °C] may impair intergranular-corrosion resistance after later sensitizing exposure, and allows a purchaser-specified lower-temperature stabilization or resolution anneal after the higher solution anneal. Neither footnote makes S2 or S4 automatic — write those Supplementary Requirements on the PO when needed.
What is Supplementary Requirement S2 for TP348?
S2 requires a stabilization heat treatment at a temperature lower than the initial solution anneal, with the temperature agreed between purchaser and vendor. The public A213–13 excerpt lists TP348 among grades that shall receive S2 when specified. For niobium/tantalum-bearing grades, S2 may also be necessary and is permitted to meet Supplementary Requirement S4 (A262 Practice E). S2 is never automatic with the grade stamp alone.
What is Supplementary Requirement S1 for TP348?
S1 allows TP348 (along with TP304L, TP316L, TP321, and TP347) to be ordered in the stress-relieved annealed condition at 1500–1650 °F [815–900 °C] after roll straightening for certain chloride stress-corrosion services. No mechanical straightening is permitted after that treatment. S1 is purchase-order language — mills will not assume stress-relieved delivery from a verbal note about chlorides.
Does Table 4 set a hardness limit for TP348?
Yes. Table 4 for TP348 lists tensile strength, yield strength, elongation, and a hardness maximum of 192 HBW / 200 HV or 90 HRB. Hardness tests are part of lot acceptance under A213, which differs from many A312 pipe rows for the same UNS number that omit a Table 4 hardness cap. Ask the mill to report hardness beside the tensile results on the EN 10204 3.1 certificate.
Minimum wall vs average wall for A213 TP348 — which should I specify?
Order minimum wall when the boiler or heat-exchanger datasheet is written around a guaranteed minimum thickness after tolerance — the usual practice for A213 tube. Order average wall only when the purchase order explicitly allows average-wall product and the designer has accepted that basis. Put the wall basis on the enquiry before the mill selects A1016 tolerance tables.
Can I dual-certify TP348 with TP348H on the same heat?
Yes when ladle carbon meets the H-grade 0.04–0.10% band while also clearing the TP348 ≤0.08% ceiling, when Nb+Ta clears both the 10 × C and 8 × C floors for the heat’s carbon, when Co and Ta clear both ceilings, and when tensile, hardness, and (for the H path) grain-size results clear both acceptance paths. Spell the required dual marking and heat-treatment route on the enquiry before the heat is selected.
Is TP348 a good choice for chloride-rich cooling water?
Usually no as a first choice. Nb+Ta helps intergranular corrosion resistance and Co/Ta ceilings satisfy controlled-chemistry specs, but neither raises PREN the way molybdenum does. Prefer TP316L or a higher-Mo grade when chlorides dominate aqueous service; reserve TP348 for stabilized boiler and heat-exchanger framing where Co/Ta control earns its keep. S1 stress-relieved delivery can help certain chloride SCC cases but does not replace Mo for pitting.

Conclusion

ASTM A213 TP348 / UNS S34800 is the cobalt- and tantalum-controlled, Nb+Ta-stabilized seamless stainless steel tube grade for boiler, superheater, and heat-exchanger service when Nb + Ta ≥10 × C ≤1.10% with Co ≤0.20%, Ta ≤0.10%, Cr 17–19% / Ni 9–13%, and C ≤0.08% must deliver IGC resistance under controlled-chemistry purchase orders. SHH STEEL supplies cold-finished and hot-finished seamless tube in the usual OD × wall / BWG band, solution annealed at 1900 °F [1040 °C], tested to Table 4 tensile and hardness limits with Nb+Ta / Co / Ta reported, and documented on EN 10204 3.1 certificates — with dual SA-213 marking only when the order asks for that separate ASME standard. For sister grades and stock-oriented size discussions, start from the A213/A213M hub, then send your OD × wall list, wall basis, dual-marking needs, and Co/Ta / Nb+Ta requirements so we can align mill and near-term availability to the ASTM callout.

Contact: admin@steelspecs.com

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X