ASTM A213 TP317LMN Stainless Steel Tube | ASTM A213 Stainless Steel - SHH STEEL

ASTM A213 TP317LMN Stainless Steel Tube

ASTM A213 TP317LMN / UNS S31726 nitrogen-bearing Mo 4–5% seamless boiler, superheater and heat-exchanger tube — C ≤0.03%, Cr 17.0–20.0%, Ni 13.5–17.5%, Mo 4.0–5.0%, N 0.10–0.20%, Cu ≤0.75%, working Table 4 floor 80/35 ksi with elongation 35% min and hardness max 192 HBW / 90 HRB (UNCERTAIN — A213–13 Table 4 OCR omits S31726; confirm ordered edition), 1900 °F solution anneal (HT row also UNCERTAIN in local excerpt). SHH STEEL supplies cold-finished and hot-finished seamless tube with EN 10204 3.1 MTCs that report the mandatory nitrogen range with Mo and Cu.
Grade
TP317LMN / UNS S31726
Standard
ASTM A213 / A213M
Product form
Seamless boiler / superheater / heat-exchanger tube (cold-finished and hot-finished)
Size
Typical OD × min wall (or average wall) within ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD and ~0.015–0.500 in. [0.4–12.7 mm] wall; other diameters by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is ASTM A213 TP317LMN Stainless Steel Tube

ASTM A213 / A213M covers seamless ferritic and austenitic alloy-steel boiler, superheater, and heat-exchanger tubes. Grade TP317LMN / UNS S31726 is the nitrogen-bearing partner to A213 TP317LM: melting carbon is capped at 0.03%, chromium widens to 17.0–20.0%, nickel stays at 13.5–17.5%, molybdenum remains in the 4.0–5.0% band, nitrogen is required in a 0.10–0.20% range (not a ≤0.20% maximum), and copper is held at 0.75% maximum. That mandatory nitrogen range is why the grade letter ends in N — it is solid-solution strengthening and PREN contribution, not optional reporting. Buyers who write “317LMN HX tube” still need to name A213 on the purchase order so the mill applies the tube product standard together with the N-range and Mo 4–5% checks.

SHH STEEL can supply ASTM A213 TP317LMN stainless steel tube as seamless cold-finished and hot-finished product in the usual boiler and heat-exchanger OD × wall / BWG band, shipped with EN 10204 3.1 mill test certificates that report the full ladle chemistry — nitrogen inside 0.10–0.20% and molybdenum inside 4.0–5.0% — plus tensile and hardness results against the ordered edition’s Table 4 row. Dual A213 / SA-213 marking is offered only when the purchase order asks for both independent standards. Browse the grade family on the A213/A213M hub.

Commercial shorthand such as 317LMN, S31726, or “N-bearing 4–5 Mo tube” never replaces the ASTM grade on the MTC or stencil. Sister grades under the same ASTM standard include A213 TP317LM, A213 TP317L, A213 TP316N, A213 TP316LNM, and A213 UNS S31254. A213 covers seamless tube only — no welded or HCW manufacturing type — so cold-finished versus hot-finished is the process choice.

Chemical Composition of A213 TP317LMN

Two chemistry layers matter for TP317LMN under ASTM A213. Melting analysis is mandatory for every heat; product analysis on finished tube applies only when Supplementary Requirement wording or the purchase order invokes it through ASTM A1016/A1016M, with tolerances typically from ASTM A480/A480M Table A1.1. The first line a reviewer should check is nitrogen 0.10–0.20% — a heat at 0.08% N can clear TP317LM’s ≤0.20% maximum but fails the LMN floor. The second line is molybdenum 4.0–5.0% with nickel 13.5–17.5% and chromium 17.0–20.0% (a wider Cr window than TP317LM’s 18–20%). Copper ≤0.75% and carbon ≤0.03% complete the row.

The tables below reproduce the melt limits for TP317LMN / UNS S31726, the product-analysis limits from A480 Table A1.1 practice, and a short N / Mo / Cr snapshot against TP317LM and TP317L. Later A213 editions place austenitic stainless grades in Table 2 (older editions used Table 1); confirm the ordered edition on the purchase order.

Melting analysis (heat / ladle analysis)

Element TP317LMN (UNS S31726) melting analysis
Carbon (C) ≤ 0.03
Manganese (Mn) ≤ 2.00
Phosphorus (P) ≤ 0.045
Sulfur (S) ≤ 0.030
Silicon (Si) ≤ 1.00
Chromium (Cr) 17.0 – 20.0
Nickel (Ni) 13.5 – 17.5
Molybdenum (Mo) 4.0 – 5.0
Nitrogen (N) 0.10 – 0.20
Copper (Cu) ≤ 0.75

Source: ASTM A213/A213M stainless chemistry table for Grade TP317LMN / UNS S31726 (public mill / specification PDF excerpt — _ref_a213.txt / A213–13 table text). Confirm the ordered edition. Nitrogen analysis method is a matter of agreement (Footnote B) when the element is reported.

Product analysis — A480/A480M Table A1.1 tolerances applied

Element Melting Tolerance (A480 A1.1) Product analysis limit
Carbon (C) ≤ 0.03 0.005 over ≤ 0.035
Manganese (Mn) ≤ 2.00 0.04 over ≤ 2.04
Phosphorus (P) ≤ 0.045 0.010 over ≤ 0.055
Sulfur (S) ≤ 0.030 0.005 over ≤ 0.035
Silicon (Si) ≤ 1.00 0.05 over ≤ 1.05
Chromium (Cr) 17.0 – 20.0 0.20 under / over 16.80 – 20.20
Nickel (Ni) 13.5 – 17.5 0.15 under / 0.20 over 13.35 – 17.70
Molybdenum (Mo) 4.0 – 5.0 0.10 under / over 3.90 – 5.10
Nitrogen (N) 0.10 – 0.20 0.01 under / 0.02 over 0.09 – 0.22
Copper (Cu) ≤ 0.75 0.03 over ≤ 0.78

N / Mo / Cr snapshot — TP317L / TP317LM / TP317LMN

Element TP317L (S31703) TP317LM (S31725) TP317LMN (S31726)
C ≤ 0.035 ≤ 0.03 ≤ 0.03
Cr 18.0 – 20.0 18.0 – 20.0 17.0 – 20.0
Ni 11.0 – 15.0 13.5 – 17.5 13.5 – 17.5
Mo 3.0 – 4.0 4.0 – 5.0 4.0 – 5.0
N … ≤ 0.20 0.10 – 0.20
Working Table 4 tensile 75/30 ksi 75/30 ksi 80/35 ksi (UNCERTAIN)

Read nitrogen as a range, not a ceiling. Versus A213 TP317LM, the intentional chemistry change is the mandatory 0.10% N floor and the wider 17–20% chromium window. Dual TP317LMN/TP317LM is not automatic: a heat at 0.05% N fails LMN even when Mo and Ni clear both rows. Put any tighter project nitrogen floor on the purchase order before the heat is selected.

When product analysis is ordered, finished tube may read C ≤0.035%, Mn ≤2.04%, P ≤0.055%, S ≤0.035%, Si ≤1.05%, Cr 16.80–20.20%, Ni 13.35–17.70%, Mo 3.90–5.10%, N 0.09–0.22%, and Cu ≤0.78%.

Mechanical Properties of A213 TP317LMN

UNCERTAIN — confirm on the ordered A213/A213M edition. The local A213–13 Table 4 PDF excerpt used for this series omits a printed S31726 / TP317LMN tensile row between S31725 and S32050. Working acceptance digits below follow sister nitrogen-bearing A213 austenitic practice (TP304N / TP316N pattern: 80/35 ksi, 35% elongation, hardness max 192 HBW / 90 HRB) and align with public A240 plate listings for S31726 on the 80/35 ksi tensile/yield pair (A240 plate elongation and hardness digits differ — 40% / 96 HRB — and must not be copied blindly onto an A213 tube MTC). Do not treat these working digits as verified A213–13 table text until the ordered edition is checked.

Property TP317LMN working requirement (UNCERTAIN)
Tensile strength, min 80 ksi [550 MPa] (working; confirm ordered edition)
Yield strength (0.2% offset), min 35 ksi [240 MPa] (working; confirm ordered edition)
Elongation in 2 in. or 50 mm, min 35% (working A213 austenitic pattern; A240 plate lists 40%)
Hardness, max 192 HBW / 200 HV or 90 HRB (working A213 pattern; A240 plate lists 96 HRB)

Source note: A213–13 Table 4 OCR omits S31726; working digits from sister N-bearing A213 rows plus public mill / A240 cross-checks. Mechanical property requirements generally do not apply to tubing smaller than 1/8 in. [3.2 mm] inside diameter or thinner than 0.015 in. [0.4 mm] wall. Flattening and flaring tests remain lot requirements under A213.

A tensile-only MTC that omits nitrogen or reports a 75/30 checklist against an 80/35 grade is incomplete documentation practice when the ordered edition uses the higher floor. When nitrogen is only a maximum and Mo 4–5% is enough, open A213 TP317LM rather than stretching an LM heat into an LMN story.

Dimensions and Tolerances

Dimensional supply for ASTM A213 TP317LMN is tube language — OD × wall (minimum or average) and commercially BWG / gauge — not ASME B36.19 pipe schedules as the primary size story. Usual A213 sizes run from about 1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD, with minimum wall about 0.015–0.500 in. [0.4–12.7 mm]; other diameters may be furnished when all other requirements are met. State min versus average wall on the purchase order.

OD and wall variations follow ASTM A1016/A1016M as invoked by A213. Cold-finished tubes commonly hold tighter OD control; hot-finished tubes allow wider windows. Confirm the exact A1016 rows for the OD and finish route on the ordered edition.

Item Typical A213 TP317LMN dimensional practice
Product form Seamless only (cold-finished or hot-finished)
Usual size band ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD; wall ~0.015–0.500 in. [0.4–12.7 mm] min (or average wall if PO says so)
Wall basis Minimum wall (default commercial practice) or average wall when specified
OD / wall tolerances Per ASTM A1016/A1016M for the finish route and size
Length Cut lengths for HX / boiler bundles, or mill random lengths by agreement
Secondary size note ASME B36.19 schedules only as a buyer-requested cross-reference — not the primary A213 callout

Put the cut list, U-bend preference, and end preparation on the enquiry. Minimum wall remains a first-class A213 concept regardless of the nitrogen-bearing Mo 4–5% chemistry.

Equivalent Grades

Equivalence language around 317LMN tube often collapses it with TP317LM or with A240 plate nicknames. ASTM A213 Grade TP317LMN / UNS S31726 is the governing designation for this article; EN 1.4439 and related wrought names that point to similar N-bearing Mo 4–5% chemistry families are not automatic substitutes on an A213 MTC.

Designation Notes
ASTM A213 / A213M Grade TP317LMN Governing ASTM seamless boiler / HX tube product standard for this article
UNS S31726 Unified number in the stainless chemistry table
ASME SA-213 TP317LMN Separate ASME Code Book adoption — dual-mark only when the PO asks
Related N-max sister A213 TP317LM — Mo 4–5%, N ≤0.20 max, Cr 18–20, 75/30 ksi
Related Mo 3–4% L A213 TP317L — Mo 3–4%, N ellipsis
Related superaustenitic A213 UNS S31254 — Mo ~6%, separate UNS row
Related plate A240 / SA240 flat product in the 317LMN family — order plate and tube under their own standards

Dual A213/SA-213 marking is a purchase-order option. Compare TP317LM and S31254 on their own ASTM A213 pages before swapping N-bearing Mo 4–5% tube inside an exchanger list.

Heat Treatment and Delivery Condition

UNCERTAIN — confirm on the ordered edition. The local A213–13 heat-treatment table excerpt lists UNS S31725 (TP317LM) at 1900 °F [1040 °C] solution treatment with water or other rapid cool, but does not print a separate S31726 row in the OCR layout between S31725 and S32050. Working practice for this pack treats TP317LMN the same way as its Mo 4–5% sister — solution treated at a minimum of 1900 °F [1040 °C], then quenched in water or cooled rapidly by other means — until the ordered edition is verified. No mandatory ASTM grain-size number is assumed.

Cold-finished versus hot-finished is a process and dimensional route, not a substitute for the anneal. Delivery condition for SHH STEEL TP317LMN is solution annealed and pickled (or bright annealed by agreement), with anneal temperature, quench method, Mo, Ni, N-range, and Cu results on the EN 10204 3.1 certificate. Straightening, cutting, and end finishing follow heat treatment.

If a project datasheet asks for ASTM A262 Practice E, put that Supplementary Requirement on the purchase order. For 6Mo superaustenitic lists, open A213 UNS S31254 instead of stretching a 4–5% Mo heat.

Corrosion Resistance

TP317LMN’s defining corrosion claim pairs Mo 4.0–5.0% with a mandatory nitrogen range (0.10–0.20%) that raises PREN relative to TP317LM’s nitrogen-maximum row, while low carbon supports as-welded IGC strategy and higher nickel (13.5–17.5%) supports the austenitic structure around that Mo–N balance. It is aimed at more aggressive chloride-leaning aqueous and acid-chloride services where Mo 3–4% 317L and N-max 317LM are judged short. It is still not a 6% Mo superaustenitic substitute such as A213 UNS S31254.

ASTM A213 itself does not publish a corrosion-rate or PREN table for TP317LMN; selection remains engineering judgment against fluid, temperature, velocity, and inspection philosophy. When a specification calls for ASTM A262 Practice E, write that Supplementary Requirement onto the purchase order so the test is contractual. SHH STEEL will not claim TP317LMN equals S31254 in severe brine.

Applications of A213 TP317LMN Tube

Because TP317LMN combines Mo 4–5% with mandatory nitrogen, it shows up in process heat exchangers and condensers where N-bearing higher-Mo austenitic tube is named, flue-gas and chemical circuits that historically specified 317LMN, and chloride-acid services that still sit inside austenitic selection. The table below pairs typical application areas with a selection note.

Application area Typical use of TP317LMN tube Selection note
N-bearing Mo 4–5% process HX Straight and U-bend tubes when N 0.10–0.20% is named Confirm N range and Mo floor on MTC — not N-max only
Chloride-acid condensers When TP317LM N-max chemistry is judged short Still not a 6Mo / duplex substitute
N-max Mo 4–5% sufficient Stay on TP317LM Do not over-specify LMN for ordinary LM lists
Mo 3–4% sufficient Stay on TP317L / TP317 Different Mo / Ni / N rows
6Mo superaustenitic Open UNS S31254 on the same hub Separate UNS chemistry

For N-max Mo 4–5% open A213 TP317LM; for Mo 3–4% L-grade open A213 TP317L; browse the rest on the A213/A213M hub.

Weldability

TP317LMN tube welds with matching or overalloyed austenitic / nickel-base filler for tube-to-tubesheet joints so weld-metal molybdenum and nitrogen strategy track the Mo 4–5% / N-bearing base metal. Common practice uses higher-Mo austenitic filler or Alloy 625-class overalloyed wire under a qualified WPS when the corrosion review will not accept a Mo step-down in the deposit. Heat input control, interpass limits, and post-weld cleaning remain the fabricator’s responsibility — A213 governs the seamless tube product, not the field or shop weld procedure.

Because A213 TP317LMN is seamless, there is no mill longitudinal weld to radiograph the way welded pipe standards describe. Focus inspection language on tube integrity (hydro or NDE of each length), tube-to-tubesheet joint quality, and any contractual corrosion test on the base metal. If PREN after welding still falls short, changing the base metal to A213 UNS S31254 is usually a better move than relying on filler selection alone.

Surface Finishes

Standard mill delivery for ASTM A213 TP317LMN is solution annealed and pickled, leaving a clean matte finish suitable for most boiler and heat-exchanger tube duty. Bright annealing under protective atmosphere produces a smoother reflective surface used on some clean-process lines and must be called out because it changes the heat-treatment route. Light polish or specified Ra on the bore or OD is a commercial operation on top of A213 product, not automatic with the grade stamp.

When a fouling-sensitive exchanger specification quotes an Ra maximum on the bore, put it on the tube purchase order with its own acceptance language. SHH STEEL stencils grade and heat treatment as standard requirements; polish and passivation after fabrication remain commercial extras unless the contract says otherwise. End preparation should be ordered together with finish so receiving inspection shares one acceptance language.

Inspection and Testing

Lot testing for ASTM A213 TP317LMN follows tension, hardness, flattening, and flaring under A213 / A1016. Chemistry verification must include nitrogen 0.10–0.20%, molybdenum 4.0–5.0%, nickel 13.5–17.5%, chromium 17.0–20.0%, carbon ≤0.03%, and copper ≤0.75%. Tensile reporting must use the ordered edition’s Table 4 row for S31726 — working practice in this pack is 80/35 ksi with 35% elongation and hardness max 192 HBW / 90 HRB, labeled UNCERTAIN until the edition is confirmed. NDE follows the ordered edition — hydrostatic testing or non-destructive electric testing of each length is the usual A213 path unless the purchase order states otherwise.

EN 10204 3.1 certificates from SHH STEEL report ladle chemistry with the N range, Mo, Ni, and Cu, Table 4 tensile / hardness against the ordered edition, and heat-treatment condition. When A262 Practice E is ordered, those results appear as specified. A certificate missing nitrogen or molybdenum is not a complete TP317LMN release package.

Packaging and Shipping

TP317LMN tubes ship in capped or plugged bundles with weather protection matched to the route. Cut lengths for boiler and exchanger bundles are labeled by heat and size; export packing uses cases or steel-frame crates when required.

Marking includes ASTM A213, grade TP317LMN / UNS S31726, size, heat number, and SHH STEEL identification. Dual SA-213 marking appears only when the purchase order requests it. Packing lists track the same heat numbers shown on the EN 10204 3.1 certificates so the mandatory nitrogen range and Mo 4–5% results stay tied to the shipped lengths.

Why Choose SHH STEEL

SHH STEEL treats ASTM A213 TP317LMN as a nitrogen-bearing Mo 4–5% specification product: C ≤0.03%, Mo 4.0–5.0%, Ni 13.5–17.5%, N 0.10–0.20%, Cu ≤0.75%, and the ordered edition’s Table 4 tensile/hardness row are checked together before a heat is offered. Quotations state OD × wall / BWG, wall basis, finish route, A262 options, and whether dual A213/SA-213 marking is required.

We refuse nickname assemblies that stamp TP317LM as 317LMN without clearing the 0.10% nitrogen floor, or that copy A240 plate elongation/hardness digits onto an A213 tube MTC without checking the tube table. EN 10204 3.1 documentation includes the N range with Mo and Cu. Compare sisters on the A213/A213M hub before freezing the exchanger tube list.

Supply Capability

SHH STEEL supplies ASTM A213 TP317LMN seamless stainless steel tube in cold-finished and hot-finished routes across the usual boiler, superheater, and heat-exchanger OD × wall / BWG band. Capability below is an enquiry range — not a frozen warehouse SKU or tonnage claim.

Capability SHH STEEL practice for TP317LMN
Product form Seamless cold-finished and hot-finished tube
Standards ASTM A213 / A213M; dual SA-213 when PO asks
Size band Typical within ~1/8 in. ID to 5 in. OD; other diameters by agreement
Wall basis Minimum wall or average wall as specified
Documentation EN 10204 3.1 MTC with N 0.10–0.20% + Mo 4–5% + Cu; tensile vs ordered edition Table 4; A262 / third-party witness on request
Trade terms FOB / CFR / CIF / EXW and other agreed Incoterms

Stock / Available sizes

SHH STEEL quotes TP317LMN against a stock-and-mill enquiry range rather than a frozen SKU/tonnage list. Representative OD × wall / BWG combinations for boiler and heat-exchanger tube appear below.

Item Typical stock / enquiry range for TP317LMN
Outside diameter 19.05, 25.4, 31.8, 38.1, 42.4, 50.8, 60.3, 76.2 mm (and other boiler/HX ODs on enquiry; through the usual A213 ~5 in. [127 mm] band)
Wall / BWG BWG 10–18 class walls and metric min-wall equivalents; heavier walls by agreement
Common OD × wall examples 25.4 × 2.11 mm; 31.8 × 2.77 mm; 38.1 × 2.77 mm; 42.4 × 3.56 mm; 50.8 × 3.05 mm; 60.3 × 3.91 mm — illustrative, confirm min vs average wall
Length Cut lengths for boiler / exchanger bundles; bends and random mill lengths on enquiry
Special Non-standard OD/wall, bright anneal, dual A213/SA-213, A262 Practice E, third-party witness — confirm before heat reservation

Send OD × wall (or BWG), wall basis, finish route, quantity or cut list, marking (A213 or dual A213/SA-213), and N-range / Mo / A262 notes on one enquiry. We confirm C ≤0.03%, Cr 17–20% / Ni 13.5–17.5%, Mo 4.0–5.0%, N 0.10–0.20%, Cu ≤0.75%, and Table 4 digits against the ordered edition without inventing fake warehouse codes. Sisters A213 TP317LM, A213 TP317L, and A213 UNS S31254 sit on the same hub.

FAQ

Is ASTM A213 the same as ASME SA-213 for TP317LMN?
No. ASTM A213 / A213M is the ASTM International product specification for seamless boiler, superheater, and heat-exchanger tubes; ASME SA-213 / SA-213M is the separate ASME Code Book adoption. Dual-mark only when the purchase order asks for both names on the stencil and MTC. Chemistry and tensile floors align closely for a given referenced edition, but the standards remain independent documents.
Does ASTM A213 TP317LMN include welded or HCW tube?
No. ASTM A213 covers seamless boiler, superheater, and heat-exchanger tubes only. There is no WLD or HCW manufacturing-type letter under A213. Cold-finished versus hot-finished describes the seamless process route and dimensional tolerances — not a welded product form. Order welded stainless pipe under a different product standard when that form is required.
What is the chemistry of ASTM A213 TP317LMN?
Melting analysis for TP317LMN / UNS S31726 is C ≤0.03%, Mn ≤2.00%, P ≤0.045%, S ≤0.030%, Si ≤1.00%, Cr 17.0–20.0%, Ni 13.5–17.5%, Mo 4.0–5.0%, N 0.10–0.20%, and Cu ≤0.75%. Confirm the ordered A213 edition. Nitrogen’s 0.10% floor is mandatory — a heat at 0.08% N can clear TP317LM’s ≤0.20% maximum but fails TP317LMN.
TP317LMN vs TP317LM — what does the N letter change?
Both share Mo 4–5%, Ni 13.5–17.5%, C ≤0.03%, and Cu ≤0.75%. TP317LM treats nitrogen as a maximum (≤0.20%) and keeps Cr 18–20% with Table 4 75/30 ksi. TP317LMN requires nitrogen in a 0.10–0.20% range, widens chromium to 17–20%, and typically uses a higher tensile floor (working 80/35 ksi on tube — UNCERTAIN until ordered edition confirmed). Do not treat LM and LMN as interchangeable nicknames.
Why are tensile digits labeled UNCERTAIN on this TP317LMN page?
The local A213–13 Table 4 PDF excerpt omits a printed S31726 row between S31725 and S32050. Working digits of 80 ksi / 35 ksi / 35% / 192 HBW follow sister nitrogen-bearing A213 austenitic practice and align with public A240 plate tensile/yield for S31726, but A240 plate elongation and hardness differ. Confirm the Table 4 row on the ordered A213/A213M edition before rejecting or releasing a heat.
Does Table 4 set a hardness limit for TP317LMN?
Working A213 austenitic practice for this pack uses hardness maximum 192 HBW / 200 HV or 90 HRB with the 80/35 ksi tensile pair — labeled UNCERTAIN because the S31726 Table 4 row is missing from the local A213–13 excerpt. Public A240 plate listings for S31726 cite 96 HRB maximum; do not copy plate hardness onto an A213 tube MTC without checking the tube table on the ordered edition.
What heat treatment does A213 require for TP317LMN?
Working practice is solution treatment at a minimum of 1900 °F [1040 °C], water quench or other rapid cool — the same row printed for sister UNS S31725 — but the local A213–13 heat-treatment excerpt does not show a separate S31726 line, so confirm the ordered edition. Delivery is solution annealed and pickled unless bright anneal is agreed. Put A262 Practice E on the purchase order when IGC demonstration is contractual.
Minimum wall vs average wall for A213 TP317LMN — which should I specify?
Boiler and heat-exchanger datasheets almost always expect minimum wall. Average wall is allowed when the purchase order says so, with A1016/A1016M tolerances for that basis. State wall basis on the enquiry rather than relying on pipe schedule numbers as the primary A213 wall story.
Can I dual-certify TP317LMN with TP317LM on the same heat?
Only when ladle nitrogen clears the 0.10–0.20% LMN range and every other overlapping limit is met — a heat at 0.05% N that is fine for TP317LM’s ≤0.20% maximum fails LMN. Chromium windows also differ (17–20 vs 18–20). Ask for dual marking on the purchase order rather than assuming it from a PMI gun that only reads "high Mo and some N."
When should I step from TP317LMN to UNS S31254?
When the datasheet names approximately 6% molybdenum with the matching N and Cu bands of UNS S31254, not when a buyer simply wants "more Mo than 317L." TP317LMN stops at Mo 4.0–5.0% with N 0.10–0.20%. Open the S31254 page on the A213/A213M hub when that chemistry is required — it is a separate UNS row, not a nickname upgrade of TP317LMN.
Does A213 require copper reporting on TP317LMN?
Yes. The stainless chemistry table lists Cu ≤0.75% for TP317LMN / UNS S31726, so copper belongs on the ladle analysis and the EN 10204 3.1 certificate with molybdenum, nickel, and the nitrogen range. A certificate that only shows Cr–Ni–Mo without N and Cu is incomplete documentation practice for this grade row.
TP317LMN vs TP316N — are the nitrogen grades interchangeable?
No. TP316N uses Mo 2–3%, Ni 10–13, N 0.10–0.16, and C ≤0.08% under a different UNS row. TP317LMN uses Mo 4–5%, Ni 13.5–17.5, N 0.10–0.20, C ≤0.03%, and Cu ≤0.75%. Both may share an 80/35 ksi tensile pattern on A213, but chemistry does not overlap. Order the grade the datasheet names.

Conclusion

ASTM A213 TP317LMN / UNS S31726 is the nitrogen-bearing Mo 4–5% seamless stainless steel tube for boiler, superheater, and heat-exchanger service when Mo 4.0–5.0% with N 0.10–0.20%, Ni 13.5–17.5%, and Cu ≤0.75% must sit above the TP317LM nitrogen-maximum row. SHH STEEL supplies cold-finished and hot-finished seamless tube in the usual OD × wall / BWG band, solution annealed (working 1900 °F [1040 °C] — confirm HT row on ordered edition), tested to the ordered edition’s Table 4 digits (working 80/35 ksi, 35% elongation, hardness max 192 HBW / 90 HRB — UNCERTAIN), with N-range, Mo, and Cu reported on EN 10204 3.1 certificates — dual SA-213 marking only when the purchase order asks.

Contact: admin@steelspecs.com

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X