ASTM A213 TP309H Stainless Steel Tube | ASTM A213 Stainless Steel - SHH STEEL

ASTM A213 TP309H Stainless Steel Tube

ASTM A213 TP309H / UNS S30909 seamless boiler, superheater and heat-exchanger tube — the H-grade 22–24% Cr / 12–15% Ni austenitic with controlled carbon 0.04–0.10%, Table 4 floors of 75/30 ksi, hardness max 192 HBW / 90 HRB, 1900 °F solution anneal, and ASTM grain size No. 7 or coarser. SHH STEEL supplies cold-finished and hot-finished seamless tube with EN 10204 3.1 MTCs that report grain size.
Grade
TP309H / UNS S30909
Standard
ASTM A213 / A213M
Product form
Seamless boiler / superheater / heat-exchanger tube (cold-finished and hot-finished)
Size
Typical OD × min wall (or average wall) within ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD and ~0.015–0.500 in. [0.4–12.7 mm] wall; other diameters by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is ASTM A213 TP309H Stainless Steel Tube

ASTM A213 / A213M covers seamless ferritic and austenitic alloy-steel boiler, superheater, and heat-exchanger tubes. Grade TP309H / UNS S30909 is the high-temperature carbon-controlled member of the 309 family: melting carbon is held in a 0.04–0.10% band (both floor and ceiling), chromium 22.0–24.0%, nickel 12.0–15.0%, and the heat-treatment path carries an ASTM grain-size requirement of No. 7 or coarser. That combination exists for creep-range boiler and furnace duty where the higher Cr–Ni oxidation resistance of 309 is needed together with H-grade carbon and coarse-grain controls — not as a synonym stamp for ordinary A213 TP309S.

SHH STEEL can supply ASTM A213 TP309H stainless steel tube as seamless cold-finished and hot-finished product in the usual boiler, furnace, and heat-exchanger OD × wall / BWG band, shipped with EN 10204 3.1 mill test certificates that report the full ladle chemistry, the Table 4 tensile and hardness results, and the grain-size result for the heat-treatment lot. Dual A213 / SA-213 marking is available only when the purchase order asks for both independent standards. Browse 309-family grades on the A213/A213M hub.

Shop names such as 309H, S30909, or “H-grade 25-12 boiler tube” do not replace the ASTM grade on the MTC. Sister grades under the same ASTM standard include A213 TP309S, A213 TP309Cb, A213 TP309HCb, A213 TP310H, and A213 TP304H. A213 covers seamless tube only — cold-finished versus hot-finished is the process choice, not a WLD/HCW manufacturing-type letter.

Chemical Composition of A213 TP309H

Two chemistry layers matter for TP309H under ASTM A213. Melting analysis is mandatory for every heat; product analysis on finished tube applies only when Supplementary Requirement wording or the purchase order invokes it through ASTM A1016/A1016M, with tolerances typically from ASTM A480/A480M Table A1.1. The carbon range is the first line a reviewer should check: TP309H is not “309S with a little more carbon” written as a max — it is a 0.04–0.10% band with both floor and ceiling, paired with the same 22–24 / 12–15 Cr–Ni windows as TP309S.

The tables below reproduce the melt limits for TP309H / UNS S30909, the product-analysis limits from A480 Table A1.1, and a short carbon snapshot against TP309S and TP309Cb. Values are maximum unless a range is shown; ellipsis (…) means no requirement.

Melting analysis (heat / ladle analysis)

Element TP309H (UNS S30909) melting analysis
Carbon (C) 0.04 – 0.10
Manganese (Mn) ≤ 2.00
Phosphorus (P) ≤ 0.045
Sulfur (S) ≤ 0.030
Silicon (Si) ≤ 1.00
Chromium (Cr) 22.0 – 24.0
Nickel (Ni) 12.0 – 15.0
Molybdenum (Mo) … (no requirement)
Nitrogen (N) … (no requirement)
Niobium (Nb / Cb) … (no requirement)

Source: ASTM A213/A213M stainless chemistry table for Grade TP309H / UNS S30909 (public mill / specification PDF excerpt — htpipe A213 table text). Confirm the ordered edition on the purchase order. Stainless table number is edition-dependent (Table 2 later / Table 1 older).

Product analysis — A480/A480M Table A1.1 tolerances applied

Element Melting Tolerance (A480 A1.1) Product analysis limit
Carbon (C) 0.04 – 0.10 0.01 under / over 0.03 – 0.11
Manganese (Mn) ≤ 2.00 0.04 over ≤ 2.04
Phosphorus (P) ≤ 0.045 0.010 over ≤ 0.055
Sulfur (S) ≤ 0.030 0.005 over ≤ 0.035
Silicon (Si) ≤ 1.00 0.05 over ≤ 1.05
Chromium (Cr) 22.0 – 24.0 0.25 under / over 21.75 – 24.25
Nickel (Ni) 12.0 – 15.0 0.15 under / over 11.85 – 15.15

Carbon snapshot — TP309S / TP309H / TP309Cb

Element TP309S (S30908) TP309H (S30909) TP309Cb (S30940)
C ≤ 0.08 0.04 – 0.10 ≤ 0.08
Cr 22.0 – 24.0 22.0 – 24.0 22.0 – 24.0
Ni 12.0 – 15.0 12.0 – 15.0 12.0 – 16.0
Nb (Cb) … … 10×C – 1.10

Heats that also meet the TP309S carbon ceiling can be dual-certified TP309S/TP309H when tensile, hardness, and grain-size results clear both rows — ask for that dual marking on the PO rather than assuming it from a PMI reading. Dual TP309H/TP309Cb is not automatic: niobium is a no-requirement ellipsis on TP309H. When Nb stabilization plus H-grade carbon is required, open A213 TP309HCb.

When product analysis is ordered, finished tube may read C 0.03–0.11%, Mn ≤2.04%, P ≤0.055%, S ≤0.035%, Si ≤1.05%, Cr 21.75–24.25%, and Ni 11.85–15.15%. Put any tighter project carbon floor on the purchase order before the heat is selected — the H-grade carbon floor is intentional for elevated-temperature strength.

Mechanical Properties of A213 TP309H

ASTM A213 Table 4 sets the room-temperature tensile acceptance floor for TP309H at 75 ksi [515 MPa] tensile strength and 30 ksi [205 MPa] yield strength (0.2% offset), with elongation of 35% minimum in 2 in. or 50 mm — the same room-temperature pair as TP309S. Hardness maximum is 192 HBW / 200 HV or 90 HRB. What distinguishes the H grade mechanically in the product standard is the grain-size requirement: ASTM No. 7 or coarser, determined per heat-treatment lot under the ordered edition’s clause referencing ASTM E112.

Property TP309H requirement
Tensile strength, min (Table 4) 75 ksi [515 MPa]
Yield strength (0.2% offset), min (Table 4) 30 ksi [205 MPa]
Elongation in 2 in. or 50 mm, min (Table 4) 35%
Hardness, max (Table 4) 192 HBW / 200 HV or 90 HRB
Grain size ASTM No. 7 or coarser (per heat-treatment lot)

Source: ASTM A213/A213M Table 4 for TP309H / UNS S30909 and H-grade grain-size language (public specification PDF excerpt — htpipe A213 heat-treatment table showing grain-size column “7” for TP309H). Mechanical property requirements do not apply to tubing smaller than 1/8 in. [3.2 mm] ID or thinner than 0.015 in. [0.4 mm] wall. Flattening and flaring tests sit beside tension and hardness on a lot basis.

Room-temperature tensile equality with TP309S is why dual 309S/309H stock is attractive; elevated-temperature allowables, the carbon floor, and the coarse-grain requirement are why the H grade exists. A tensile-only MTC that omits grain size is incomplete for TP309H — ask for the E112 result on the certificate before releasing the heat to fabrication.

Dimensions and Tolerances

Dimensional supply for ASTM A213 TP309H is tube language — OD × wall (minimum or average) and BWG / gauge — covering boiler, furnace, and heat-exchanger sizes rather than leading with ASME B36.19 pipe schedules. Usual A213 sizes run from about 1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD with min wall about 0.015–0.500 in. [0.4–12.7 mm]; other diameters by agreement. Boiler and superheater datasheets almost always assume a minimum-wall reading — state wall basis on the purchase order.

OD and wall variations follow ASTM A1016/A1016M as invoked by A213. Cold-finished tubes commonly hold tighter OD; hot-finished tubes allow wider windows. Cold-finished average wall is often summarized as ±10% of specified average wall; minimum-wall product follows A1016 minimum-wall tables. Confirm exact rows for the OD and finish on the ordered edition.

Item Typical A213 TP309H dimensional practice
Product form Seamless only (cold-finished or hot-finished)
Usual size band ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD; wall ~0.015–0.500 in. [0.4–12.7 mm]
Wall basis Minimum wall (default for boiler / superheater) or average wall when specified
OD / wall tolerances Per ASTM A1016/A1016M for finish route and size
Length Cut lengths for boiler / furnace / HX bundles; mill random by agreement
Secondary note B36.19 schedules only as a buyer cross-reference

Put cut list, design metal temperature context, and end preparation on the enquiry. Minimum wall remains a first-class A213 concept for 309H the same way it does for other H-grade tube.

Equivalent Grades

Equivalence language around 309H tube often collapses plate, cast, and tube product forms into one nickname. ASTM A213 Grade TP309H / UNS S30909 is the governing designation for this article; EN and JIS wrought names that point to similar high-Cr–Ni chemistry families are not automatic substitutes on an A213 MTC.

Designation Notes
ASTM A213 / A213M Grade TP309H Governing ASTM seamless boiler / HX tube product standard for this article
UNS S30909 Unified number in the stainless chemistry table
ASME SA-213 TP309H Separate ASME Code Book adoption — dual-mark only when the PO asks
Related S-grade A213 TP309S — same Cr–Ni, C ≤0.08, no grain-size mandate
Related H+Cb A213 TP309HCb — H-grade carbon plus niobium stabilization
Related plate A240 / SA240 flat product in the 309 family — order plate and tube under their own standards

Dual A213/SA-213 marking is a purchase-order option. Compare TP309S, TP309Cb, and TP309HCb on their own ASTM A213 pages before swapping 309-family grades inside a furnace or boiler tube list.

Heat Treatment and Delivery Condition

TP309H under ASTM A213 is furnished solution treated at a minimum of 1900 °F [1040 °C], then quenched in water or cooled rapidly by other means. That Table 3 heat-treatment row also carries the ASTM grain-size requirement of No. 7 or coarser for the heat-treatment lot — the clause that separates H-grade acceptance from ordinary TP309S solution treatment at the same temperature.

Cold-finished versus hot-finished is a process and dimensional route, not a substitute for the anneal or the grain-size check. Delivery condition for SHH STEEL TP309H is solution annealed and pickled (or bright annealed by agreement), with anneal temperature, quench method, and E112 grain-size result on the EN 10204 3.1 certificate. Straightening, cutting, and end finishing follow heat treatment.

When niobium stabilization is also required on top of H-grade carbon and grain size, open A213 TP309HCb rather than assuming a standard TP309H heat covers Cb. Stabilizing heat treatment under Supplementary Requirement S2 applies to listed stabilized H grades (including TP309HCb), not to plain TP309H.

Corrosion Resistance

TP309H is selected primarily for high-temperature oxidation and scaling resistance in hot air, combustion, and furnace atmospheres, combined with H-grade carbon and coarse-grain controls for creep-range duty. It is not a molybdenum grade: in aqueous chloride pitting and crevice service, A213 TP316 / A213 TP316L remain the usual step-ups.

The H-grade carbon floor (0.04% min) means TP309H is not the first choice for as-welded wet intergranular corrosion duty — that conversation belongs to L grades or stabilized grades. Sulfur-bearing and reducing hot gases can still attack 309-family alloys; selection remains engineering judgment. ASTM A213 does not publish a corrosion-rate or oxidation-rate table for TP309H. When a project invokes a specific oxidation or IGC test, write that Supplementary Requirement onto the purchase order.

Applications of A213 TP309H Tube

TP309H shows up wherever seamless tube must survive hotter oxidizing environments than 18-8 is trusted for, and the datasheet also demands H-grade carbon plus grain-size controls — furnace tubes, radiant sections, heat-recovery exchangers on hot gas, and boiler/superheater locations where both oxidation and creep framing drive grade choice.

Application area Typical use of TP309H tube Selection note
Boiler / superheater (creep + oxidation) Seamless tube where H-grade carbon/grain-size and 309 Cr–Ni both apply Confirm design metal temperature and Code allowable
Furnace / radiant tubes Oxidizing furnace atmospheres with H-grade acceptance Open TP309S if grain-size is not required
Heat-recovery / hot-gas HX Tube circuits with hot oxidizing gas and elevated-temp strength framing Step to TP310H if higher Cr–Ni is specified
Stabilized H duty Usually not TP309H — needs Nb Open A213 TP309HCb
Aqueous chloride HX Usually not the first 309H use case Prefer Mo grades (TP316/TP316L)

Stay on the A213/A213M hub for 309S, 309Cb, 309HCb, and 310H sisters rather than mixing A312 pipe certificates into tube acceptance.

Weldability

TP309H tube welds with matching or near-matching 309/309H austenitic filler for tube-to-tubesheet, attachment, and fabrication joins under a qualified WPS. ER309H (or equivalent covered electrodes) are preferred when the weld metal must also carry H-grade carbon; fabricators sometimes use 309L deposits for lower carbon in the weld metal when the joint design allows it. Heat input, interpass, and cleaning remain the fabricator’s code responsibility — A213 governs the seamless tube product, not the field weld procedure.

Because A213 TP309H is seamless, there is no mill longitudinal weld to radiograph as welded-pipe standards describe. Focus inspection on each-length hydro or NDE, joint quality, grain-size on the MTC, and any contractual oxidation or IGC tests. When niobium stabilization is required in the base metal, change the tube grade to A213 TP309HCb or A213 TP309Cb rather than trying to weld-procedure a plain H grade into a stabilized datasheet.

Surface Finishes

Standard mill delivery for ASTM A213 TP309H is solution annealed and pickled. Bright annealing is a called-out route when a smoother reflective surface is needed. Specified Ra, light polish, and post-fabrication passivation are commercial extras on top of the A213 stamp.

Furnace and boiler tube often ships with a workmanlike pickled finish; cosmetic polish is uncommon unless the PO asks. End preparation for welding or expanding should be ordered with finish so receiving inspection shares one acceptance language. Grain-size reporting is a metallurgical requirement, not a surface-finish option — it belongs on the MTC regardless of pickle or bright anneal.

Inspection and Testing

Base ASTM A213 testing for TP309H includes heat analysis, tension to the Table 4 75/30 ksi floors, hardness to the Table 4 maximum, grain size (ASTM No. 7 or coarser) per heat-treatment lot, flattening and flaring on a lot basis, and hydro or NDE of each length. The manufacturer may choose hydro versus NDE unless the purchase order fixes the method. Marking includes ASTM designation, grade, size, heat number, and other clause-required data.

Option Purpose
Product analysis Confirms chemistry on finished tube
Grain-size reporting (mandatory for H) E112 result on the MTC for the heat-treatment lot
Intergranular corrosion / oxidation tests Only when Supplementary Requirements or OEM specs add them
Minimum vs average wall States wall basis
Fixed hydro or NDE method Removes manufacturer’s option
Third-party inspection / EN 10204 3.2 Witnessed testing when the project requires it

Ask the mill to state lot identity clearly so hardness, tension, and grain-size specimens map cleanly to the bundle you receive. An MTC without grain size is incomplete for TP309H.

Packaging and Shipping

TP309H tube leaves SHH STEEL bundled, end-protected, and tagged with ASTM A213 grade, OD × wall (or BWG), heat number, and PO reference. U-bent or specially cut furnace and boiler lengths need transit protection matched to bend radius and leg length. Export packing ranges from bare or wrapped bundles to wooden cases for bright-annealed or small-bore material.

We ship under the Incoterms on the order acknowledgement — FOB, CFR, CIF, EXW, or other agreed terms. Bilingual marks, inland trucking, and project color coding belong on the enquiry beside the metallurgical notes (carbon floor, grain size, dual marking).

Why Choose SHH STEEL

SHH STEEL treats ASTM A213 TP309H as an H-grade oxidation-oriented tube product with enforceable chemistry, tensile, hardness, grain-size, and heat-treatment rules — not as a catalogue nickname for “any 309 tube.” Certificates report the stainless-table ladle chemistry, Table 4 set, and E112 grain size; dual A213/SA-213 marking appears only when requested.

If the datasheet does not need H-grade carbon and grain size, we open A213 TP309S. If niobium stabilization is specified without H rules, we open A213 TP309Cb. If both H and Cb are required, we open A213 TP309HCb. Wet chloride duty steers to the Mo family on the A213/A213M hub. Lead times mix near-term lengths with mill schedules; we say which is which.

Cut-to-length, U-bending, polish, and third-party inspection are defined extras. The tube on site should match the ASTM callout the engineer wrote — including the grain-size line on the MTC.

Supply Capability

SHH STEEL can supply ASTM A213 TP309H stainless steel tube against the edition and finish route on your enquiry. Capability and Stock / Available sizes below frame furnace, boiler, and HX enquiries for this H-grade.

Item SHH STEEL capability for TP309H
Standard ASTM A213 / A213M (dual SA-213 marking on request) Grade TP309H / UNS S30909
Product form Seamless only — cold-finished and hot-finished
Size Typical OD × min wall (or average wall) in the A213 usual band; other diameters by agreement
Wall / gauge Minimum wall or average wall; BWG / gauge accepted
Length Cut-to-length for furnace / HX / boiler; mill random by agreement; bends on enquiry
Finish Annealed and pickled; bright annealed or light polish by agreement
Testing Tension (75/30 ksi), hardness (max 192 HBW / 90 HRB), grain size (No. 7 or coarser), flattening, flaring, hydro or NDE; full melt chemistry on MTC
Documents EN 10204 3.1 with grain-size result; third-party / 3.2 on request
Trade terms FOB / CFR / CIF / EXW and other agreed Incoterms

Stock / Available sizes

SHH STEEL quotes TP309H against a stock-and-mill enquiry range rather than a frozen SKU/tonnage list. Representative OD × wall / BWG combinations for furnace, boiler, and heat-exchanger tube appear below.

Item Typical stock / enquiry range for TP309H
Outside diameter 19.05, 25.4, 31.8, 38.1, 42.4, 50.8, 60.3, 76.2 mm (and other furnace/boiler ODs on enquiry; through the usual A213 ~5 in. [127 mm] band)
Wall / BWG BWG 10–18 class walls and metric min-wall equivalents; heavier walls by agreement
Common OD × wall examples 25.4 × 2.11 mm; 31.8 × 2.77 mm; 38.1 × 2.77 mm; 42.4 × 3.56 mm; 50.8 × 3.05 mm; 60.3 × 3.91 mm — illustrative, confirm min vs average wall
Length Cut lengths for furnace / boiler / exchanger bundles; bends and random mill lengths on enquiry
Special Non-standard OD/wall, bright anneal, dual A213/SA-213, dual 309S/309H, third-party witness — confirm before heat reservation

Send OD × wall (or BWG), wall basis, finish route, quantity or cut list, marking (A213 or dual A213/SA-213), grain-size reporting expectation, and Supplementary Requirements on one enquiry. We confirm C 0.04–0.10%, Cr 22–24% / Ni 12–15%, Table 4 75/30 ksi, and ASTM No. 7 or coarser without inventing fake warehouse codes. Sisters A213 TP309S, A213 TP309HCb, and A213 TP304H sit on the same hub.

FAQ

Is ASTM A213 the same as ASME SA-213 for TP309H?
No. ASTM A213 / A213M is the ASTM International product specification for seamless boiler, superheater, and heat-exchanger tubes; ASME SA-213 / SA-213M is the separate ASME Code Book adoption. Dual-mark only when the purchase order asks for both names on the stencil and MTC. Chemistry, tensile floors, and grain-size rules align closely for a given referenced edition, but the standards remain independent.
Does ASTM A213 TP309H include welded or HCW tube?
No. ASTM A213 covers seamless tube only. There is no WLD or HCW manufacturing type under this product standard. Cold-finished versus hot-finished seamless tube is the process choice. Welded stainless pipe belongs to a different product standard and page family.
What is the chemistry of ASTM A213 TP309H?
TP309H / UNS S30909 melt limits include carbon 0.04–0.10%, manganese ≤2.00%, phosphorus ≤0.045%, sulfur ≤0.030%, silicon ≤1.00%, chromium 22.0–24.0%, and nickel 12.0–15.0%, with molybdenum, nitrogen, and niobium as no-requirement ellipses. Product-analysis limits apply only when ordered, typically from A480 Table A1.1 via the A1016 path.
TP309H vs TP309S — which A213 grade should I order?
Order TP309H when the datasheet needs the H-grade carbon range (0.04–0.10%), grain-size controls (ASTM No. 7 or coarser), and creep-oriented framing together with 309 Cr–Ni oxidation resistance. Order TP309S when the ≤0.08% carbon ceiling and standard solution-treat path without mandatory grain size are enough. Do not treat "309H" as a synonym stamp for ordinary TP309S on the MTC.
TP309H vs TP304H — when do I need the higher Cr–Ni H grade?
Order TP309H when high-temperature oxidation and hot-gas scale resistance need chromium 22–24% and nickel 12–15% rather than the 18-8 balance of TP304H. Both carry H-grade carbon 0.04–0.10% and ASTM No. 7 or coarser grain size, with the same Table 4 75/30 ksi floors. The differentiation is chemistry and oxidation framing, not a unique tensile number.
Why does A213 require grain size for TP309H?
The H-grade grain-size requirement (ASTM No. 7 or coarser per heat-treatment lot) exists because elevated-temperature creep strength in austenitic stainless is sensitive to grain size. Coarser grains generally improve creep resistance. A tensile-only certificate that omits the E112 result is incomplete for TP309H acceptance under A213.
Does Table 4 set a hardness limit for TP309H?
Yes. Hardness maximum is 192 HBW / 200 HV or 90 HRB, alongside 75/30 ksi tensile/yield and 35% elongation. Hardness tests are part of lot acceptance under A213. Tighter project hardness windows must be written into the purchase order.
What heat treatment does A213 require for TP309H?
Solution treatment at a minimum of 1900 °F [1040 °C] with water quench or other rapid cool, plus ASTM grain size No. 7 or coarser for the heat-treatment lot. Both cold-finished and hot-finished seamless tube follow that requirement. Ask the mill to state anneal temperature, quench method, and grain-size result on the EN 10204 3.1 certificate.
Minimum wall vs average wall for A213 TP309H — which do I order?
Order minimum wall when the design assumes a guaranteed minimum thickness after tolerance — the usual boiler and superheater assumption. Order average wall only when the PO explicitly allows it and the designer accepts that basis. Put the wall basis on the enquiry before the mill selects A1016 tolerance tables.
Is TP309H a good choice for chloride-rich cooling water?
Usually no as a first choice. TP309H is framed for high-temperature oxidation plus H-grade creep controls; it does not add molybdenum for aqueous chloride pitting, and the carbon floor is not an L-grade IGC story. Prefer TP316/TP316L or higher-Mo grades on the A213 hub for seawater-leaning and brine exchangers.
Can you dual-certify A213 TP309S and TP309H?
Yes when the heat meets both the TP309S carbon ceiling and the TP309H carbon floor/ceiling, and tensile, hardness, and grain-size results clear both rows. Dual marking is a purchase-order option, not an automatic PMI outcome. Spell the required marking on the enquiry before the heat is reserved.
Can you dual-certify A213 and SA-213 TP309H?
Yes when the purchase order requests both independent standards on the stencil and MTC. Dual marking with TP309HCb is only possible on heats that also meet niobium stabilization chemistry — do not assume it from a carbon reading alone. Spell the required marking on the enquiry.

Conclusion

ASTM A213 TP309H / UNS S30909 is the H-grade 22–24% Cr / 12–15% Ni seamless stainless steel tube for boiler, furnace, and heat-exchanger service when high-temperature oxidation resistance and creep-oriented carbon/grain-size controls both drive grade selection. SHH STEEL supplies cold-finished and hot-finished seamless tube in the usual OD × wall / BWG band, solution annealed at 1900 °F [1040 °C], tested to Table 4 75/30 ksi and hardness limits with ASTM No. 7 or coarser grain size on the MTC, and documented on EN 10204 3.1 certificates — with dual SA-213 marking only when the order asks. For sister 309S, 309Cb, and 309HCb grades, start from the A213/A213M hub, then send OD × wall, wall basis, grain-size expectation, and marking requirements so we can align mill and near-term availability.

Contact: admin@steelspecs.com

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X