ASTM A213 UNS S31272 Stainless Steel Tube | ASTM A213 Stainless Steel - SHH STEEL

ASTM A213 UNS S31272 Stainless Steel Tube

ASTM A213 UNS S31272 (Footnote C, no TP letter — Ti–B microalloyed 14–16Cr / 14–16Ni austenitic) seamless boiler, superheater and heat-exchanger tube with C 0.08–0.12%, Mo 1.00–1.40%, Ti 0.30–0.60%, B 0.004–0.008%, Table 4 floors of 65/29 ksi, hardness max 217 HBW / 95 HRB, and 1920 °F [1050 °C] solution anneal. SHH STEEL supplies cold-finished and hot-finished seamless tube with EN 10204 3.1 MTCs.
Grade
UNS S31272 (no TP letter — Ti–B microalloyed 14Cr–14Ni austenitic)
Standard
ASTM A213 / A213M
Product form
Seamless boiler / superheater / heat-exchanger tube (cold-finished and hot-finished)
Size
Typical OD × min wall (or average wall) within ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD and ~0.015–0.500 in. [0.4–12.7 mm] wall; other diameters by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is ASTM A213 UNS S31272 Stainless Steel Tube

ASTM A213 / A213M lists UNS S31272 among the austenitic stainless grades that carry no common TP letter — Footnote C states the UNS number uniquely identifies the alloy. Unlike the 6Mo PREN grades around it in the table, S31272 is a titanium- and boron-bearing austenitic with a deliberate carbon floor: carbon 0.08–0.12%, manganese 1.50–2.00%, silicon 0.30–0.70%, chromium 14.0–16.0%, nickel 14.0–16.0%, molybdenum 1.00–1.40%, titanium 0.30–0.60%, and boron 0.004–0.008%. Shop nicknames are uncommon; the purchase order should carry ASTM A213 UNS S31272 (or the separate ASME SA-213 adoption) so seamless-tube minimum-wall, test, and marking clauses apply.

SHH STEEL can supply ASTM A213 UNS S31272 stainless steel tube as seamless cold-finished and hot-finished product in the usual boiler and heat-exchanger OD × wall / BWG band, shipped with EN 10204 3.1 mill test certificates that report the full Ti–B–Mo set and the Table 4 tensile and hardness results (65 ksi [450 MPa] / 29 ksi [200 MPa], hardness max 217 HBW / 95 HRB). Dual A213 / SA-213 marking is available only when the purchase order asks for both independent standards. Browse austenitic sisters on the A213/A213M hub.

Do not paste a TP321 or TP316Ti chemistry block onto an S31272 certificate — the carbon range 0.08–0.12%, fixed Ti 0.30–0.60% (not a Ti ≥5×C formula alone), boron 0.004–0.008%, and Mo 1.00–1.40% are a different microalloy package, and Table 4 tensile is 65/29 ksi rather than the 75/30 commodity pattern. Sister grades under the same ASTM standard include A213 TP321, A213 TP316Ti, A213 TP321H, A213 UNS S31254, and A213 TP304H. A213 covers seamless tube only — cold-finished versus hot-finished is the process choice, not a WLD/HCW manufacturing type.

Chemical Composition of A213 UNS S31272

UNS S31272 chemistry is a Ti–B microalloyed austenitic window rather than a PREN-first 6Mo design: chromium and nickel both sit in balanced 14.0–16.0% bands, molybdenum is a moderate 1.00–1.40%, titanium is held in a fixed 0.30–0.60% range, and boron is deliberately present at 0.004–0.008%. Carbon is a range (0.08–0.12%), not a low-C max — that matters when someone tries to treat the grade as a “soft L” substitute. Melting analysis is mandatory; product analysis applies only when ordered through A1016 / A480 A1.1. There is no TP grade letter — order and mark by UNS S31272 (Footnote C).

The tables below reproduce the melt limits from the public A213 stainless chemistry table, product-analysis limits from A480 Table A1.1 practice, and a short snapshot against TP321 / TP316Ti. Confirm the ordered edition before treating secondary catalogues as acceptance text. UNCERTAIN: A480 product-tolerance digits for Ti 0.30–0.60 and especially B 0.004–0.008 are applied from sister Ti-bearing practice and labeled honestly — confirm the A480 edition if product analysis is contractual. Boron reporting on the MTC should not be skipped just because the digit is small.

Melting analysis (heat / ladle analysis)

Element UNS S31272 melting analysis
Carbon (C) 0.08 – 0.12
Manganese (Mn) 1.50 – 2.00
Phosphorus (P) ≤ 0.030
Sulfur (S) ≤ 0.015
Silicon (Si) 0.30 – 0.70
Chromium (Cr) 14.0 – 16.0
Nickel (Ni) 14.0 – 16.0
Molybdenum (Mo) 1.00 – 1.40
Nitrogen (N) … (no requirement)
Niobium (Nb) … (no requirement)
Titanium (Ti) 0.30 – 0.60
Boron (B) 0.004 – 0.008

Source: ASTM A213/A213M stainless chemistry table for UNS S31272 (public htpipe A213 PDF excerpt — _ref_a213.txt A213/A213M − 13). Titanium 0.30–0.60% and boron 0.004–0.008% must both appear on the certificate; an MTC that only shows “Ti-stabilized 316-ish” without the boron band is incomplete for S31272.

Product analysis — A480/A480M Table A1.1 tolerances applied

Element Melting Tolerance (A480 A1.1) Product analysis limit
Carbon (C) 0.08 – 0.12 0.01 under / over 0.07 – 0.13
Manganese (Mn) 1.50 – 2.00 0.04 under / over 1.46 – 2.04
Phosphorus (P) ≤ 0.030 0.005 over ≤ 0.035
Sulfur (S) ≤ 0.015 0.005 over ≤ 0.020
Silicon (Si) 0.30 – 0.70 0.05 under / over 0.25 – 0.75
Chromium (Cr) 14.0 – 16.0 0.20 under / over 13.80 – 16.20
Nickel (Ni) 14.0 – 16.0 0.15 under / 0.20 over 13.85 – 16.20
Molybdenum (Mo) 1.00 – 1.40 0.05 under / over 0.95 – 1.45
Titanium (Ti) 0.30 – 0.60 0.05 under / over (UNCERTAIN) 0.25 – 0.65
Boron (B) 0.004 – 0.008 confirm A480 edition (UNCERTAIN) confirm ordered A480

Reading note: product analysis is not automatic — invoke it on the purchase order. Boron product digits are intentionally left as “confirm ordered A480” rather than inventing a false precision band.

Ti / B / Mo snapshot — TP321 / TP316Ti / S31272

Element TP321 (S32100) TP316Ti (S31635) UNS S31272
C ≤ 0.08 ≤ 0.08 0.08 – 0.12
Cr 17.0 – 19.0 16.0 – 18.0 14.0 – 16.0
Ni 9.0 – 12.0 10.0 – 14.0 14.0 – 16.0
Mo … 2.00 – 3.00 1.00 – 1.40
Ti ≥5(C+N) ≤0.70 ≥5(C+N) ≤0.70 0.30 – 0.60 (fixed band)
B … … 0.004 – 0.008

S31272 is not “TP321 with a little boron” and not “TP316Ti with less Mo” — the balanced 14–16 Cr/Ni, fixed Ti band, carbon floor, and mandatory boron set it apart from formula-Ti commodity grades.

Mechanical Properties of A213 UNS S31272

Table 4 for UNS S31272 sets a lower tensile and yield floor than commodity TP304/TP316 austenitics: 65 ksi [450 MPa] tensile and 29 ksi [200 MPa] yield, with 35% elongation and hardness max 217 HBW / 95 HRB. That lower strength pair is intentional table text — do not “upgrade” an S31272 MTC to a 75/30 checklist, and do not reject a conforming 65/29 heat because a buyer expected 304 numbers.

Property UNS S31272 requirement
Tensile strength, min 65 ksi [450 MPa]
Yield strength (0.2% offset), min 29 ksi [200 MPa]
Elongation in 2 in. or 50 mm, min 35%
Hardness, max 217 HBW or 95 HRB

Source: ASTM A213/A213M Table 4 for UNS S31272 (public A213–13 excerpt). Mechanical property requirements generally do not apply to tubing smaller than 1/8 in. [3.2 mm] inside diameter or thinner than 0.015 in. [0.4 mm] wall. Flattening and flaring tests remain lot requirements under A213.

Hardness max 217 HBW / 95 HRB sits slightly above the 192 HBW / 90 HRB commodity ceiling — expect that on the certificate. A tensile-only MTC that omits titanium or boron is incomplete documentation practice for this grade.

Dimensions and Tolerances

Dimensional supply for ASTM A213 UNS S31272 remains tube language — OD × min wall (or average wall) and BWG / gauge — covering boiler and heat-exchanger sizes rather than leading with ASME B36.19 pipe schedules. Usual A213 sizes run from about 1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD with min wall about 0.015–0.500 in. [0.4–12.7 mm]; other diameters by agreement. State wall basis on the purchase order — minimum wall is the A213 default unless average wall is specified.

OD and wall variations follow ASTM A1016/A1016M as invoked by A213. Cold-finished tubes commonly hold tighter OD; hot-finished tubes allow wider windows. Because S31272 is ordered less often than commodity 304/316 tube, confirm mill drawing and finishing capability for the exact OD × wall before freezing a large cut list.

Length is ordered as specific cut lengths for exchanger or superheater bundles or as random mill lengths. End finish follows the fabrication drawing. B36.19 schedule references may appear only as a secondary commercial size hint — they are not the primary A213 size story for S31272 tube.

Equivalent Grades

Equivalence language around S31272 is sparse because the grade has no common TP letter and few shop nicknames. ASTM A213 UNS S31272 is the governing designation for this article; do not substitute TP321, TP316Ti, or TP304H on the MTC just because those grades also carry titanium or a carbon floor.

Designation Notes
ASTM A213 / A213M UNS S31272 Governing ASTM seamless boiler / HX tube product standard — no TP letter (Footnote C)
UNS S31272 Unified number that uniquely identifies the alloy
Near Ti-bearing sisters (not substitutes) TP321 / TP316Ti share titanium themes but different Cr–Ni–Mo–B packages and tensile floors
ASME SA-213 UNS S31272 Separate Code Book adoption — dual-mark only when the PO asks

Compare Ti-bearing sisters such as A213 TP321 and A213 TP316Ti, and the 6Mo neighbor A213 UNS S31254, on the A213/A213M hub before freezing the tube list. Plate listings under A240 are a related alloy story only when the same UNS appears — not an automatic tube MTC substitute.

Heat Treatment and Delivery Condition

UNS S31272 under ASTM A213 is furnished solution treated at a minimum of 1920 °F [1050 °C], then quenched in water or cooled rapidly by other means. That anneal sits slightly above the 1900 °F commodity austenitic minimum — do not apply a generic “solution anneal 1900 °F” stamp without checking the S31272 row. Public Table 3 does not print a mandatory grain-size number for this grade (ellipsis).

Cold-finished versus hot-finished is a process and dimensional route, not a second product standard. Both routes still require the 1920 °F solution treatment on finished tube. Titanium and boron in the melt do not create an H-grade grain-size obligation under the public Table 3 excerpt.

UNCERTAIN: public Table 3 OCR places a Footnote F marker in the vicinity of the S31272 heat-treatment row. Confirm ordered-edition footnote attachment — if Footnote F applies, quench capability must be sufficient to prevent carbide re-precipitation as demonstrable by A262 Practice E capability, and the manufacturer need not run the test unless the purchase order specifies it (Supplementary Requirement S4).

Corrosion Resistance

S31272’s corrosion framing is not a seawater PREN story — molybdenum is only 1.00–1.40%, far below the 6Mo grades. Chromium 14–16% with balanced nickel and titanium stabilization points toward general austenitic corrosion resistance with Ti-assisted resistance to sensitization, while boron is present as a microalloying addition rather than a corrosion driver. Do not market S31272 as a 254 SMO substitute or as a drop-in for A213 UNS S31254.

When IGC after welding is a project concern, the titanium band helps relative to unstabilized higher-carbon austenitics, but heat input control and cleaning still matter. Order A262 Practice E explicitly when demonstrated IGC capability is required. For chloride PREN duty, move to Mo–N grades such as A213 TP317LMN or S31254 rather than stretching S31272’s 1% Mo window.

Applications of A213 UNS S31272 Tube

Buyers specify ASTM A213 UNS S31272 when a seamless boiler or heat-exchanger datasheet calls out this exact UNS — typically for specialized austenitic service that wants the Ti–B microalloy package and the 65/29 ksi Table 4 pair, not a commodity 304/321 substitution. Typical placements follow project specifications that already name S31272 rather than open “pick any Ti-stabilized tube” language.

Service theme Why S31272 is considered
Specified Ti–B austenitic HX / boiler tube Fixed Ti 0.30–0.60% + B 0.004–0.008% with C 0.08–0.12%
Moderate-Mo austenitic exchangers Mo 1.00–1.40% without jumping to 6Mo PREN grades
Balanced 14Cr–14Ni tube lists Cr and Ni both 14.0–16.0% — not a 18-8 or 25-20 window
Code dual-mark projects A213 product form with optional SA-213 stencil when PO asks

If the enquiry only says “Ti-stabilized stainless tube” without the UNS, clarify whether the engineer meant A213 TP321, A213 TP316Ti, or true S31272 before reserving a heat.

Weldability

S31272 tube welds with austenitic practices using matching or near-matching fillers selected for the 14Cr–14Ni–Mo–Ti base chemistry and service temperature. Titanium in the base metal aids resistance to sensitization relative to unstabilized grades in the same carbon band; boron at the 0.004–0.008% level is a microalloying addition that should be respected in WPS development rather than ignored. Do not assume ER321 or ER316Ti automatically restores every property without a qualified procedure review.

For tube-to-tubesheet and coil welding, keep filler chemistry aligned with the base-metal Cr–Ni–Mo window and confirm any project restriction on ferrite or residual titanium. When the datasheet demands A262 Practice E on welded samples, state that on the purchase order.

Surface Finishes

Standard delivery for ASTM A213 UNS S31272 from SHH STEEL is solution annealed and pickled, with a clean ID/OD suitable for boiler and exchanger fabrication. Bright annealed or polished finishes are available by agreement when the process side needs lower roughness or a brighter appearance.

State finish expectations on the enquiry together with OD × wall and end preparation. Do not assume a bright finish from a generic “Ti stainless tube” line item — pickled anneal after the 1920 °F solution treatment is the default path unless the purchase order says otherwise.

Inspection and Testing

Lot testing for ASTM A213 UNS S31272 follows the tension, hardness, flattening, and flaring requirements of A213 together with A1016/A1016M. Chemistry is verified on the heat (and on product when ordered) — carbon 0.08–0.12%, titanium 0.30–0.60%, boron 0.004–0.008%, and molybdenum 1.00–1.40% must all clear. Non-destructive examination follows the ordered edition and any purchaser supplementary requirements.

EN 10204 3.1 mill test certificates from SHH STEEL report ladle chemistry including Ti and B, tensile and hardness results (65/29 ksi; 217 HBW / 95 HRB), heat-treatment condition at ≥1920 °F [1050 °C], and dimensions. Ask for A262 Practice E on the PO when IGC capability must be demonstrated by actual test. Third-party witness and dual A213/SA-213 marking are available when specified.

Packaging and Shipping

S31272 tubes ship in capped or plugged bundles with weather protection suited to the destination and transport mode. Cut lengths for boiler and exchanger bundles are labeled by heat and size; export packing uses wooden cases or steel-frame crates when the route requires them.

Marking includes ASTM A213, UNS S31272, size, heat number, and SHH STEEL identification. Dual SA-213 marking appears only when the purchase order requests it. Packing lists reference the same heat numbers shown on the EN 10204 3.1 certificates.

Why Choose SHH STEEL

SHH STEEL treats ASTM A213 UNS S31272 as a specification Ti–B microalloy product: C 0.08–0.12%, Mo 1.00–1.40%, Ti 0.30–0.60%, B 0.004–0.008%, Table 4 65/29 ksi, hardness max 217 HBW / 95 HRB, and the 1920 °F solution anneal are checked together before a heat is offered. Quotations state OD × wall / BWG, wall basis, finish route, A262 options, and whether dual A213/SA-213 marking is required.

We refuse substitutions that stamp TP321 or TP316Ti onto an S31272 line item without clearing the boron band and the 65/29 tensile pair, or that omit boron from the MTC because the digit looks small. EN 10204 3.1 documentation includes Ti and B together with Mo. Compare sisters on the A213/A213M hub before freezing the tube list.

Supply Capability

SHH STEEL supplies ASTM A213 UNS S31272 seamless stainless steel tube against purchase-order chemistry, mechanical, and dimensional requirements — cold-finished or hot-finished — with EN 10204 3.1 mill test certificates. The capability table below summarizes the enquiry window; it is not a frozen warehouse SKU list.

Capability SHH STEEL supply window for UNS S31272
Product form Seamless cold-finished / hot-finished boiler, superheater, and heat-exchanger tube
Grade / marking ASTM A213 UNS S31272; dual A213/SA-213 only when PO asks
Size band Typical OD × min wall (or average wall) within the A213 ~1/8 in. ID to 5 in. OD / 0.015–0.500 in. wall window; other diameters by agreement
Documentation EN 10204 3.1 MTC with Ti–B–Mo chemistry and Table 4 65/29 ksi tensile/hardness
Testing options A262 Practice E, PMI, third-party witness, supplementary NDE per PO
Trade terms FOB / CFR / CIF / EXW and other agreed Incoterms

Stock / Available sizes

SHH STEEL quotes S31272 against a stock-and-mill enquiry range rather than a frozen SKU/tonnage list. Representative OD × wall / BWG combinations for boiler and heat-exchanger tube appear below.

Item Typical stock / enquiry range for UNS S31272
Outside diameter 19.05, 25.4, 31.8, 38.1, 42.4, 50.8, 60.3 mm (and other boiler/HX ODs on enquiry; through the usual A213 ~5 in. [127 mm] band)
Wall / BWG BWG 10–18 class walls and metric min-wall equivalents; heavier walls by agreement
Common OD × wall examples 25.4 × 2.11 mm; 31.8 × 2.77 mm; 38.1 × 2.77 mm; 50.8 × 3.05 mm — illustrative, confirm min vs average wall
Length Cut lengths for boiler / exchanger bundles; random mill lengths on enquiry
Special Non-standard OD/wall, bright anneal, dual A213/SA-213, A262 Practice E, third-party witness — confirm before heat reservation

Send OD × wall (or BWG), wall basis (min or average), finish route, quantity or cut list, marking (A213 or dual A213/SA-213), and any A262 / NDE extras with the enquiry so the Ti–B chemistry and 1920 °F anneal path are reserved with the heat.

FAQ

Is ASTM A213 the same as ASME SA-213 for UNS S31272?
No. ASTM A213 / A213M is the ASTM International product specification for seamless boiler, superheater, and heat-exchanger tubes; ASME SA-213 / SA-213M is the separate ASME Code Book adoption. Dual-mark only when the purchase order asks for both names on the stencil and MTC. Chemistry and tensile floors align closely for a given referenced edition, but the standards remain independent.
Why does S31272 have no TP letter under A213?
Footnote C in the A213 stainless chemistry table states that for these alloys there is no common grade designation and the UNS number uniquely identifies them. Order, mark, and certify as UNS S31272 rather than inventing a TP letter code on the stencil. Commercial nicknames are uncommon for this grade — the UNS is the practical ordering name.
What is the chemistry of ASTM A213 UNS S31272?
Public A213 melt limits for S31272 are C 0.08–0.12%, Mn 1.50–2.00%, P ≤0.030%, S ≤0.015%, Si 0.30–0.70%, Cr 14.0–16.0%, Ni 14.0–16.0%, Mo 1.00–1.40%, Ti 0.30–0.60%, and B 0.004–0.008%. Nitrogen and niobium are no-requirement ellipses. Confirm the ordered A213/A213M edition before treating catalogue reprints as acceptance text.
S31272 vs TP321 — can I substitute a Ti-stabilized 321 tube?
Not as an automatic substitute. TP321 uses a Ti ≥5(C+N) ≤0.70 formula with Cr 17–19 / Ni 9–12 and no boron requirement, plus a 75/30 ksi tensile pair. S31272 requires a fixed Ti 0.30–0.60% band, boron 0.004–0.008%, Mo 1.00–1.40%, balanced 14–16 Cr/Ni, carbon 0.08–0.12%, and only 65/29 ksi. Substitute only when the engineer revises the datasheet to the other UNS/TP grade.
S31272 vs TP316Ti — what is the practical difference?
TP316Ti keeps Mo 2.00–3.00% with a Ti ≥5(C+N) formula and 75/30 ksi tensile. S31272 uses Mo only 1.00–1.40%, a fixed Ti band, mandatory boron, lower Cr, higher balanced Ni, a carbon floor of 0.08–0.12%, and 65/29 ksi. They share a titanium theme but are not interchangeable on an A213 MTC.
Why is Table 4 tensile only 65 ksi for S31272?
That is the published A213 Table 4 minimum for UNS S31272 — 65 ksi [450 MPa] tensile, 29 ksi [200 MPa] yield, 35% elongation, hardness max 217 HBW / 95 HRB. It is lower than commodity 304/316 floors by design of the table, not a mill defect. Do not rewrite the MTC to 75/30 to match a different grade’s checklist.
What heat treatment does A213 require for UNS S31272?
Solution treatment at a minimum of 1920 °F [1050 °C] followed by water quench or other rapid cool. Confirm whether Footnote F attaches to this row in the ordered edition; if it does, quench capability and optional A262 Practice E (S4) language follow the edition text. No mandatory grain-size number is printed for this row in the public Table 3 excerpt.
Does ASTM A213 UNS S31272 include welded or HCW tube?
No. ASTM A213 covers seamless boiler, superheater, and heat-exchanger tubes only. Cold-finished versus hot-finished is the process choice inside seamless manufacture. Welded or HCW product forms belong under other ASTM stainless tubular standards, not under an A213 S31272 line item.
Minimum wall vs average wall for A213 S31272 — which should I specify?
A213 treats minimum wall as the default ordering basis unless the purchase order specifies average wall. Heat-exchanger and boiler datasheets almost always assume minimum wall. Write “min wall” or “average wall” explicitly on the PO rather than leaving the mill to infer intent from a BWG number alone.
Must boron appear on the EN 10204 3.1 certificate?
Yes for a complete S31272 chemistry report — boron 0.004–0.008% is a melting-analysis requirement, not an optional footnote. An MTC that lists Ti and Mo but skips B is incomplete for this UNS. Product analysis of boron, if contractually required, must follow the ordered A480 edition (digits labeled UNCERTAIN in this pack until confirmed).
Can you dual-certify A213 and SA-213 UNS S31272?
Yes, when the purchase order asks for both independent standards on the stencil and MTC. ASTM A213 and ASME SA-213 remain separate documents; dual marking is a commercial/documentation choice, not an automatic merge of the two names into one title. SHH STEEL will not put SA-213 in the H1 or SEO title of the product page — that stays ASTM A213.

Conclusion

ASTM A213 UNS S31272 is the Ti–B microalloyed 14Cr–14Ni seamless stainless steel tube grade for boiler and heat-exchanger service when a fixed titanium band, mandatory boron, moderate molybdenum, and the Table 4 65/29 ksi pair — not a TP321 or TP316Ti substitution — drive grade selection. SHH STEEL supplies cold-finished and hot-finished seamless tube in the usual OD × wall / BWG band, solution annealed at 1920 °F [1050 °C], tested to Table 4 tensile and hardness limits, and documented on EN 10204 3.1 certificates — with dual SA-213 marking only when the purchase order asks.

Contact: admin@steelspecs.com

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X