ASTM A213 TP347W Stainless Steel Tube | ASTM A213 Stainless Steel - SHH STEEL

ASTM A213 TP347W Stainless Steel Tube

ASTM A213 TP347W / UNS S34705 seamless boiler, superheater and heat-exchanger tube with carbon ≤0.05%, Cr 17.0–20.0%, Ni 8.00–11.0%, nitrogen 0.10–0.25%, niobium 0.25–0.50%, vanadium 0.20–0.50%, tungsten 1.50–2.60%, Table 4 floor 90/38 ksi, hardness max 219 HBW / 95 HRB, and grain size 7–10. SHH STEEL supplies seamless tube solution treated at 2000 °F [1100 °C] with EN 10204 3.1 MTCs that report W, V, N, and Nb.
Grade
TP347W / UNS S34705
Standard
ASTM A213 / A213M
Product form
Seamless boiler / superheater / heat-exchanger tube (cold-finished and hot-finished)
Size
Typical OD × min wall (or average wall) within ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD and ~0.015–0.500 in. [0.4–12.7 mm] wall; other diameters by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is ASTM A213 TP347W Stainless Steel Tube

ASTM A213 / A213M is the ASTM International product specification for seamless ferritic and austenitic alloy-steel boiler, superheater, and heat-exchanger tubes. Grade TP347W / UNS S34705 is the tungsten-bearing, vanadium-bearing, nitrogen-strengthened member of the 347 family: melting carbon is capped at 0.05%, chromium 17.0–20.0%, nickel 8.00–11.0%, nitrogen 0.10–0.25%, niobium 0.25–0.50%, vanadium 0.20–0.50%, and tungsten 1.50–2.60%. That alloy package is why Table 4 raises the tensile floor to 90 ksi [620 MPa] and yield to 38 ksi [260 MPa] — well above the 75/30 ksi pair on A213 TP347 — and why the heat-treatment table prints grain size 7–10 with a 2000 °F [1100 °C] solution minimum. Buyers who write “347W tube” still need to name A213 (or the separate ASME SA-213 adoption) on the purchase order so the mill applies W/V/N/Nb chemistry, grain-size, heat-treatment, test, and marking clauses rather than a loose shop nickname.

SHH STEEL can supply ASTM A213 TP347W stainless steel tube as seamless cold-finished and hot-finished product in the usual boiler and heat-exchanger OD × wall / BWG band, shipped with EN 10204 3.1 mill test certificates that report the full ladle chemistry (including tungsten, vanadium, nitrogen, and niobium), the Table 4 tensile and hardness results (90/38 ksi, max 219 HBW / 95 HRB), grain size against the 7–10 window, and the anneal temperature for the heat-treatment lot. When a project also needs ASME Code Book marking, we dual-mark A213 / SA-213 on the same lengths only if the purchase order says so. Browse the grade family on the A213/A213M hub.

Commercially, TP347W tube is still called 347W, S34705, or W-bearing Nb-stabilized boiler tube; none of those shop names replace the ASTM grade on the MTC or stencil. Sister grades under the same ASTM standard include A213 TP347, A213 TP347H, A213 TP347HFG, A213 TP347LN, and A213 TP321H. A213 covers seamless tube only — no welded or HCW manufacturing type — so cold-finished versus hot-finished is the process choice, not a WLD/HCW stencil letter.

Chemical Composition of A213 TP347W

Two chemistry layers matter for TP347W under ASTM A213. Melting (heat or ladle) analysis is mandatory for every heat; product analysis on finished tube applies only when Supplementary Requirement wording or the purchase order invokes it through ASTM A1016/A1016M. Product-analysis tolerances typically flow from ASTM A480/A480M Table A1.1. SHH STEEL reports actual ladle values — and product values when ordered — and does not advertise unpublished tighter catalogue windows. Four lines define the grade for a reviewer: tungsten 1.50–2.60%, vanadium 0.20–0.50%, nitrogen 0.10–0.25%, and niobium 0.25–0.50%, with carbon capped at 0.05% and nickel narrowed to 8.00–11.0% versus TP347’s 9.0–13.0%. Phosphorus is also tightened to ≤0.040% versus the 0.045% ceiling on TP347. Do not treat a familiar “347” PMI reading as proof of W or V — those elements must appear on the ladle report.

The tables below reproduce the heat analysis for TP347W / UNS S34705, the product-analysis limits from A480 Table A1.1 practice, and a short W/V/N/Nb snapshot against TP347, TP347H, and TP347HFG. Later A213 editions place austenitic stainless grades in Table 2 (older editions used Table 1); confirm the ordered edition on the purchase order. Nitrogen analysis method is a matter of agreement (Footnote B) — write the method on the PO when N is contractual. A480 product-tolerance digits for W and V are applied from sister-pack practice and labeled UNCERTAIN pending the ordered A480 edition.

Melting analysis (heat / ladle analysis)

Element TP347W (UNS S34705) melting analysis
Carbon (C) ≤ 0.05
Manganese (Mn) ≤ 2.00
Phosphorus (P) ≤ 0.040
Sulfur (S) ≤ 0.030
Silicon (Si) ≤ 1.00
Chromium (Cr) 17.0 – 20.0
Nickel (Ni) 8.00 – 11.0
Molybdenum (Mo) … (no requirement)
Nitrogen (N) 0.10 – 0.25
Niobium (Nb / Cb) 0.25 – 0.50
Vanadium (V) 0.20 – 0.50
Tungsten (W) 1.50 – 2.60
Titanium (Ti) … (no requirement)

Source: ASTM A213/A213M stainless chemistry table for Grade TP347W / UNS S34705 (public mill / specification PDF excerpt — _ref_a213.txt / A213–13 table text). Confirm the ordered edition. Where ellipses appear, the ordered edition sets no requirement for that element.

Product analysis — A480/A480M Table A1.1 tolerances applied

Element Melting Tolerance (A480 A1.1) Product analysis limit
Carbon (C) ≤ 0.05 0.01 over ≤ 0.06
Manganese (Mn) ≤ 2.00 0.04 over ≤ 2.04
Phosphorus (P) ≤ 0.040 0.010 over ≤ 0.050
Sulfur (S) ≤ 0.030 0.005 over ≤ 0.035
Silicon (Si) ≤ 1.00 0.05 over ≤ 1.05
Chromium (Cr) 17.0 – 20.0 0.20 under / over 16.80 – 20.20
Nickel (Ni) 8.00 – 11.0 0.15 under / 0.20 over 7.85 – 11.20
Nitrogen (N) 0.10 – 0.25 0.01 under / 0.02 over (sister N practice) 0.09 – 0.27
Niobium (Nb) 0.25 – 0.50 0.05 under / over (Nb range practice) 0.20 – 0.55
Vanadium (V) 0.20 – 0.50 0.05 under / over (UNCERTAIN — confirm A480) 0.15 – 0.55
Tungsten (W) 1.50 – 2.60 0.05 under / over (UNCERTAIN — confirm A480) 1.45 – 2.65

W / V / N / Nb snapshot — TP347 / TP347W / TP347H / TP347HFG

Element TP347 (S34700) TP347W (S34705) TP347H (S34709) TP347HFG (S34710)
C ≤ 0.08 ≤ 0.05 0.04 – 0.10 0.06 – 0.10
Ni 9.0 – 13.0 8.00 – 11.0 9.0 – 13.0 9.0 – 13.0
N … 0.10 – 0.25 … …
Nb ≥ 10 × C, ≤ 1.10 0.25 – 0.50 ≥ 8 × C, ≤ 1.10 ≥ 8 × C, ≤ 1.10
V / W none V 0.20–0.50; W 1.50–2.60 none none
Table 4 TS/YS 75 / 30 ksi 90 / 38 ksi 75 / 30 ksi 80 / 30 ksi

Dual TP347W/TP347 is not a chemistry path: one grade requires tungsten, vanadium, and a nitrogen band the other does not list. Versus A213 TP347H, TP347W trades the H-grade carbon floor and 8 × C Nb formula for W/V/N strengthening and a higher Table 4 tensile pair. Put any tighter project tungsten or nitrogen floor on the purchase order before the heat is selected.

When product analysis is ordered, finished tube may read C ≤0.06%, Mn ≤2.04%, P ≤0.050%, S ≤0.035%, Si ≤1.05%, Cr 16.80–20.20%, Ni 7.85–11.20%, N 0.09–0.27%, Nb 0.20–0.55%, V 0.15–0.55%, and W 1.45–2.65% under the A480 practice digits above. Confirm A480 edition digits for W and V when product analysis is contractual.

Mechanical Properties of A213 TP347W

ASTM A213 Table 4 sets the room-temperature tensile acceptance floor for TP347W at 90 ksi [620 MPa] tensile strength and 38 ksi [260 MPa] yield strength (0.2% offset), with elongation of 30% minimum in 2 in. or 50 mm — a higher-strength, slightly lower-elongation pair than the 75/30/35 set on TP347. Hardness maximum is 219 HBW / 230 HV or 95 HRB, also higher than the 192 HBW / 90 HRB cap on the rest of the 347 family. The public heat-treatment table prints ASTM grain size 7–10 for TP347W, so grain-size reporting belongs on a complete MTC for this grade.

Property TP347W requirement
Tensile strength, min (Table 4) 90 ksi [620 MPa]
Yield strength (0.2% offset), min (Table 4) 38 ksi [260 MPa]
Elongation in 2 in. or 50 mm, min (Table 4) 30%
Hardness, max (Table 4) 219 HBW / 230 HV or 95 HRB
Grain size (Table 3) ASTM No. 7 – 10

Source: ASTM A213/A213M Table 4 and Table 3 for TP347W / UNS S34705 (public specification PDF excerpt — _ref_a213.txt / A213–13). Mechanical property requirements do not apply to tubing smaller than 1/8 in. [3.2 mm] inside diameter or thinner than 0.015 in. [0.4 mm] wall. Flattening and flaring tests are also required on a lot basis. For austenitic grades with a grain-size requirement, marking also includes heat number and heat-treatment lot identification.

Do not accept a TP347 tensile MTC (75/30 ksi, 192 HBW) as proof of TP347W — the floors and hardness cap are different rows. Ask for W, V, N, Nb, tensile, hardness, and grain size on the same certificate before releasing the heat. For fine-grain creep framing without tungsten open A213 TP347HFG; for H-grade Nb without W open A213 TP347H.

Dimensions and Tolerances

Dimensional supply for ASTM A213 TP347W is tube language — outside diameter × wall thickness (minimum wall or average wall) and, commercially, BWG / gauge — not ASME B36.19 pipe schedules as the primary size story. The sizes usually furnished under A213 run from about 1/8 in. [3.2 mm] inside diameter to 5 in. [127 mm] outside diameter, with minimum wall from about 0.015 to 0.500 in. [0.4 to 12.7 mm]; other diameters may be furnished when all other requirements are met. State on the purchase order whether wall is minimum or average — boiler and superheater datasheets that pick TP347W for elevated-temperature strength almost always assume a minimum-wall reading.

Outside-diameter and wall variations follow ASTM A1016/A1016M as invoked by A213. Cold-finished tubes commonly hold tighter OD control; hot-finished tubes allow wider OD and wall windows. Permissible variations from a specified average wall for cold-finished tube are often summarized as ±10% of the specified average wall. Confirm the exact A1016 rows for the OD and finish route on the ordered edition.

Item Typical A213 TP347W dimensional practice
Product form Seamless only (cold-finished or hot-finished)
Usual size band ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD; wall ~0.015–0.500 in. [0.4–12.7 mm] min (or average wall if PO says so)
Wall basis Minimum wall (default for boiler / HX) or average wall when specified
OD / wall tolerances Per ASTM A1016/A1016M for the finish route and size; cold-finished average wall often ±10%
Length Cut lengths for boiler / superheater / HX bundles, or mill random lengths by agreement
Secondary size note ASME B36.19 schedules may appear only when a buyer asks for a pipe-schedule cross-reference — not as the primary A213 size callout

Put the cut list and end preparation on the enquiry so mill and stock lengths can be mixed efficiently. Minimum wall is a first-class A213 concept: if the datasheet assumes average wall, say so explicitly before the heat is rolled.

Equivalent Grades

Equivalence language around TP347W tube is often looser than a tungsten-bearing purchase order can afford. ASTM A213 Grade TP347W / UNS S34705 is the governing designation for this article; shop nicknames that say “W-bearing 347” or “347W boiler tube” are not automatic substitutes on an A213 mill test certificate. When a datasheet says “equivalent to 347W,” confirm which product standard, tensile/hardness table, W/V/N/Nb package, grain-size window, and heat-treatment path the mill will actually certify.

Designation Notes
ASTM A213 / A213M Grade TP347W Governing ASTM seamless boiler / HX tube product standard for this article
UNS S34705 Unified number listed in the stainless chemistry table
ASME SA-213 TP347W Separate ASME Code Book adoption — dual-mark only when the PO asks
Related Nb grades TP347 / S34700, TP347H / S34709, TP347HFG / S34710 — no W/V mandatory bands
Related plate A240 / SA240 flat product in related UNS families — order plate and tube under their own product standards

Dual A213/SA-213 marking is a purchase-order option, not a claim that the two standards are one document. Compare TP347, TP347H, and TP347HFG on their own ASTM A213 pages before swapping grades on a familiar “347” PMI reading alone.

Heat Treatment and Delivery Condition

TP347W under ASTM A213 is furnished solution treated at a minimum of 2000 °F [1100 °C], then quenched in water or cooled rapidly by other means. That solution minimum is 100 °F [about 55 °C] higher than the 1900 °F path on TP347 and TP347LN. The public heat-treatment table prints ASTM grain size 7–10 for this grade — a bounded window, not an open “7 or coarser” H-grade note. Footnotes F and H are not printed beside the TP347W solution-temperature cell in the public A213–13 excerpt the way they sit beside TP347 / TP348.

Supplementary Requirement S2 in the public A213–13 excerpt lists TP347, TP347H, TP348, and TP348H among grades that shall receive a stabilization heat treatment when specified — TP347W is not on that printed list. Supplementary Requirement S1 likewise omits TP347W. Do not assume S1 or S2 from a verbal “treat like 347H” note; write negotiated stabilization language on the purchase order if the project needs it for this UNS.

Cold-finished versus hot-finished is a process and dimensional route, not a substitute for the anneal or the grain-size window. Delivery condition for SHH STEEL TP347W is solution annealed and pickled (or bright annealed by agreement), with anneal temperature, quench method, grain size, and the W / V / N / Nb results on the EN 10204 3.1 certificate. For standard Nb framing open A213 TP347; for H-grade carbon and grain-size controls open A213 TP347H; for fine-grain creep without tungsten open A213 TP347HFG.

Corrosion Resistance

TP347W’s chromium-rich passive film, niobium stabilization, and controlled carbon handle many boiler and superheater duties where sensitizing thermal cycles would otherwise deplete chromium at grain boundaries. Tungsten and vanadium are present primarily for elevated-temperature strength contribution alongside nitrogen — not as a molybdenum substitute for aqueous chloride pitting. In chloride-bearing cooling waters and many process exchangers, pitting and crevice attack become limiting, and buyers usually step to A213 TP316 / A213 TP316L or a higher-PREN grade rather than stretching W-bearing 18-8 into wet corrosive service.

ASTM A213 itself does not publish a corrosion-rate table for TP347W; selection remains engineering judgment against fluid, temperature, velocity, creep design data, and inspection philosophy. When a specification calls for ASTM A262 Practice E, write Supplementary Requirement S4 onto the purchase order and confirm whether a negotiated stabilization path is needed for this Nb-bearing grade. SHH STEEL will not market TP347W as a wet-chloride upgrade over molybdenum grades; the W designation is about the alloyed strength package, not about higher PREN.

Applications of A213 TP347W Tube

TP347W seamless tube under A213 is chosen for boiler, superheater, and heat-exchanger service where tungsten, vanadium, nitrogen, and niobium must deliver a higher Table 4 tensile pair (90/38 ksi) and a controlled grain-size window (7–10) that standard TP347 does not print. It is a selection when the datasheet names S34705 specifically for elevated-temperature strength framing. It is the wrong default for chloride-rich cooling water that really needs Mo, and it is not interchangeable with TP347H or TP347HFG on chemistry alone. The table below pairs typical application areas with a selection note.

Application area Typical use of TP347W tube Selection note
High-strength boiler / superheater Seamless A213 tube where 90/38 ksi and W/V/N are specified Confirm W 1.50–2.60, V, N, Nb, grain 7–10 on the MTC
Elevated-temperature steam tubing Stabilized W-bearing steam tubing ordered to S34705 Do not substitute TP347 (75/30) without design review
Vs TP347H duty When W/V/N strength is preferred over H-grade C floor alone Open TP347H if H carbon/Nb formula is the datasheet driver
Vs TP347HFG duty When tungsten is required, not only fine-grain Nb HFG has no W/V bands and a different tensile floor
Wet chloride service Not the first choice Prefer TP316L or higher-Mo grades

For standard Nb open A213 TP347; for H-grade Nb open A213 TP347H; for fine-grain creep without W open A213 TP347HFG on the A213/A213M hub.

Weldability

TP347W tube welds with matching or near-matching niobium-bearing austenitic filler for tube-to-tubesheet joints, attachment welds, and fabrication joins, with WPS qualification that accounts for the higher-strength base metal and the tungsten/vanadium/nitrogen chemistry. Common practice still leans on ER347 / E347 family fillers under a qualified procedure so weld-metal niobium supports stabilized service; do not assume a soft ER308L default when the base tube is W-bearing Nb-stabilized and the design assumes the alloyed strength package. Heat input control, interpass limits, and post-weld cleaning remain the fabricator’s responsibility under the applicable boiler or pressure-vessel code — A213 governs the seamless tube product, not the field or shop weld procedure.

Because A213 TP347W is seamless, there is no mill longitudinal weld to radiograph the way welded pipe standards describe. Focus inspection language on tube integrity (hydro or NDE of each length), tube-to-tubesheet joint quality, W / V / N / Nb documentation on the base metal, grain-size lot identity, and any contractual corrosion test. Specify end preparation and surface finish on the tube PO when orbital or clean-service joins are planned.

Surface Finishes

Standard mill delivery for ASTM A213 TP347W is solution annealed and pickled, leaving a clean matte finish suitable for most boiler and superheater tube duty. Bright annealing under protective atmosphere produces a smoother reflective surface used on some clean-process lines and must be called out because it changes the heat-treatment route. Light polish or specified Ra on the bore or OD is a commercial or service-center operation on top of A213 product, not automatic with the grade stamp.

When a fouling-sensitive exchanger specification quotes an Ra maximum on the bore, put it on the tube purchase order with its own acceptance language and sampling plan. SHH STEEL stencils grade, heat treatment, and (for grain-size grades) heat/lot identity as standard requirements; polish, special OD grind, and passivation after fabrication remain commercial extras unless the contract says otherwise. Order end preparation together with finish so receiving inspection shares one acceptance language.

Inspection and Testing

Base ASTM A213 testing for TP347W includes heat analysis (carbon ≤0.05%, nitrogen 0.10–0.25%, niobium 0.25–0.50%, vanadium 0.20–0.50%, tungsten 1.50–2.60%), tension tests to the Table 4 floors (90/38 ksi), hardness tests to the Table 4 maximum (219 HBW / 95 HRB), grain-size determination to the 7–10 window, flattening and flaring tests on a lot basis, and either hydrostatic testing or nondestructive electric testing of each length. The manufacturer may choose hydro versus NDE unless the purchase order fixes the method. Marking includes the ASTM designation, grade, size, heat number, heat-treatment lot identification (required for austenitic grades with a grain-size requirement), and other clause-required data.

Supplementary Requirements commonly added on TP347W tube orders are summarized below. Invoke them by number or clear purchase-order wording. Note that S1 and S2 are not printed for TP347W in the public A213–13 excerpt — negotiate separately if needed.

Option Purpose
Product analysis Confirms chemistry on finished tube — useful when W, V, N, or Nb sits near a band edge
S4 intergranular corrosion A262 Practice E when the project requires IGC evidence
Negotiated stabilization S2 is not printed for TP347W — write agreed temperature/time if needed
Nitrogen method Footnote B — analysis method by purchaser/producer agreement
Minimum vs average wall States which wall basis the size callout uses
Fixed hydro or NDE method Removes manufacturer’s option when the end user mandates one route
Third-party inspection / EN 10204 3.2 Witnessed testing and certificate when the project requires it

Ask the mill to state lot identity clearly on the certificate so hardness, tension, grain size, and W / V / N / Nb specimens map cleanly to the bundle you receive.

Packaging and Shipping

TP347W tube leaves SHH STEEL bundled, capped or end-protected, and tagged for export or domestic delivery according to the length mix and bend form on the order. Bundle tags repeat the ASTM A213 grade, OD × wall (or BWG), heat number, heat-treatment lot identity, and PO reference so site receiving can check the shipment without opening every certificate packet first. U-bent tubes need extra cradle or case protection so bend radii and legs are not distorted in transit.

Export packing can be bare bundles, wrapped bundles, or wooden-cased lengths for bright-annealed, polished, or small-bore material. We ship under the Incoterms on the order acknowledgement — FOB, CFR, CIF, EXW, or other agreed terms. Inland trucking, bilingual destination marks, or project color coding for bundle tags should be stated on the enquiry beside the metallurgical notes.

Why Choose SHH STEEL

SHH STEEL treats ASTM A213 TP347W as a product standard with enforceable chemistry (W, V, N, Nb bands), tensile, hardness, grain-size, heat-treatment, and marking rules — not as a catalogue nickname for “any strong 347 tube.” The MTC reports the full ladle chemistry including tungsten, vanadium, nitrogen, and niobium, the Table 4 tensile/hardness set (90/38 ksi, 219 HBW / 95 HRB), grain size against 7–10, and the anneal temperature; the stencil carries seamless tube identity under A213; and dual A213/SA-213 marking is offered only when requested.

We keep the W-bearing conversation honest for boiler and superheater duty. If standard Nb without tungsten is enough, we open A213 TP347. If H-grade carbon and grain size are required without W, we open A213 TP347H. If fine-grain creep framing without W is specified, we open A213 TP347HFG. If ultra-low C + N + 15 × C Nb is specified, we open A213 TP347LN. The A213/A213M hub is organized grade by grade under ASTM, seamless tube only.

Lead times combine near-term stock lengths with mill schedules; we say which is which on the quotation. Cut-to-length, U-bending, polish, and third-party inspection are defined extras. The tube that arrives should match the ASTM callout the engineer wrote, with paperwork a third-party inspector can read without translation.

Supply Capability

SHH STEEL can supply ASTM A213 TP347W stainless steel tube against the edition and finish route named on your enquiry. The capability table below summarizes the sizes, finishes, and documents we regularly quote for this grade, followed by the Stock / Available sizes map buyers ask for when they need a quick sense of what to enquire against for W-bearing Nb-stabilized boiler and superheater duty.

Item SHH STEEL capability for TP347W
Standard ASTM A213 / A213M (dual SA-213 marking on request) Grade TP347W / UNS S34705
Product form Seamless only — cold-finished and hot-finished
Size Typical OD × min wall (or average wall) in the A213 usual band; other diameters by agreement
Wall / gauge Minimum wall or average wall; BWG / gauge callouts accepted on enquiry
Length Cut-to-length for boiler / superheater / HX bundles; mill random by agreement; U-bends on enquiry
Finish Annealed and pickled; bright annealed or light polish by agreement
Testing Tension (90/38 ksi), hardness (max 219 HBW / 95 HRB), grain size 7–10, W/V/N/Nb, flattening, flaring, hydro or NDE per length; full ladle chemistry on MTC; product analysis / S4 on order
Documents EN 10204 3.1 with full ladle chemistry, W/V/N/Nb, and grain size; third-party inspection / 3.2 on request
Trade terms FOB / CFR / CIF / EXW and other agreed Incoterms

Stock / Available sizes

SHH STEEL quotes TP347W tube against a practical stock-and-mill enquiry range rather than a frozen warehouse SKU list. The sizes below are OD × wall / BWG combinations buyers most often request for W-bearing boiler and superheater tube; availability of any single line on a given week depends on mill drawing and our inbound schedule, so treat the table as a supply map for enquiry — not a guarantee of floor tonnage.

Item Typical stock / enquiry range for TP347W
Outside diameter 25.4, 31.8, 38.1, 44.5, 50.8, 63.5, 76.2 mm (and other boiler/superheater ODs on enquiry; up through the usual A213 ~5 in. [127 mm] band)
Wall / BWG BWG 10–16 class walls and metric min-wall equivalents; heavier walls for high-pressure duty by agreement
Common OD × wall examples 31.8 × 2.77 mm; 38.1 × 3.05 mm; 44.5 × 3.05 mm; 50.8 × 3.38 mm; 63.5 × 3.38 mm — illustrative boiler/superheater sizes, confirm min vs average wall
Length Cut lengths for boiler / superheater bundles; U-bends and straight random lengths on enquiry
Special Non-standard OD/wall, bright anneal, negotiated stabilization, dual A213/SA-213 marking, S4 IGC — confirm on enquiry before the heat is reserved

When you send an enquiry, list OD × wall (or BWG), wall basis (minimum or average), cold-finished or hot-finished preference, quantity or cut list, required marking (A213 alone or dual A213/SA-213), and any Supplementary Requirements (S4, product analysis, nitrogen method). We reply with what we can ship from near-term stock versus what needs a mill run, without inventing fake warehouse codes or tonnage claims.

Send the size list, finish route, quantity or cut lengths, required marking, Supplementary Requirements, and destination on one enquiry. We will confirm chemistry (including W/V/N/Nb), tensile, hardness, and grain size against the stainless chemistry table, Table 3, and Table 4, state what ships from near-term availability versus mill production, and keep the offer aligned with ASTM A213 / A213M. Related grades such as A213 TP347, A213 TP347H, and A213 TP347HFG sit on the same hub when the datasheet steps beyond TP347W.

FAQ

Is ASTM A213 the same as ASME SA-213 for TP347W?
No. ASTM A213 / A213M is the ASTM International product specification for seamless boiler, superheater, and heat-exchanger tubes; ASME SA-213 / SA-213M is the separate ASME Code Book adoption of that grade text. Chemistry, tensile, hardness, grain-size, and W/V/N/Nb rules align closely for a given referenced edition, but they remain two independent standards. Dual-mark A213/SA-213 tube only when the purchase order asks for both names on the stencil and MTC.
Does ASTM A213 TP347W include welded or HCW tube?
No. ASTM A213 covers seamless tube only. There is no WLD or HCW manufacturing type under this product standard the way ASTM A312 describes pipe. The process choice for TP347W under A213 is cold-finished versus hot-finished seamless tube, plus the W/V/N/Nb chemistry, 2000 °F solution path, grain-size 7–10, and testing clauses of the ordered edition.
What makes TP347W chemistry different from TP347?
TP347W adds tungsten 1.50–2.60%, vanadium 0.20–0.50%, and nitrogen 0.10–0.25%, holds niobium in a fixed 0.25–0.50% band (not the 10 × C formula), caps carbon at 0.05%, tightens phosphorus to ≤0.040%, and narrows nickel to 8.00–11.0%. TP347 uses Nb ≥10 × C ≤1.10% with C ≤0.08%, Cr 17–20 / Ni 9–13, and no W/V/N requirements. They are sister grades, not synonym stamps.
Why is the Table 4 tensile floor higher for TP347W?
Table 4 for TP347W requires 90 ksi [620 MPa] tensile and 38 ksi [260 MPa] yield with 30% elongation and hardness max 219 HBW / 95 HRB — a deliberate step up from TP347’s 75/30/35 and 192 HBW / 90 HRB. The W/V/N alloy package and the controlled grain-size window support that higher room-temperature acceptance floor. Do not accept a TP347 tensile MTC as proof of TP347W.
TP347W vs TP347H — which should I specify?
Order TP347W when the datasheet needs tungsten, vanadium, nitrogen, the 90/38 ksi tensile pair, and grain size 7–10 under a 2000 °F solution path. Order TP347H when H-grade carbon 0.04–0.10%, Nb ≥8 × C ≤1.10%, grain size No. 7 or coarser, and finish-route HT (CF 2000 °F / HR 1925 °F) are the drivers without a W/V mandate. They are not interchangeable on a "strong 347" nickname alone.
TP347W vs TP347HFG — tungsten or fine-grain only?
Both print a bounded grain-size window (TP347W 7–10; TP347HFG 7–10) and sit above plain TP347 in elevated-temperature framing, but TP347HFG has no tungsten or vanadium bands, uses C 0.06–0.10% with Nb ≥8 × C, lists Table 4 tensile 80 ksi, and uses a much higher Footnote I solution path. Choose TP347W when W/V/N chemistry is on the datasheet; choose TP347HFG when fine-grain Nb without W is specified.
What grain size and heat treatment does A213 require for TP347W?
Solution treatment at a minimum of 2000 °F [1100 °C] followed by water quench or other rapid cool, with ASTM grain size No. 7–10. Marking for austenitic grades with a grain-size requirement includes heat number and heat-treatment lot identification. S1 and S2 are not printed for TP347W in the public A213–13 excerpt — negotiate stabilization separately if the project needs it.
Does Table 4 set a hardness limit for TP347W?
Yes. Table 4 for TP347W lists a hardness maximum of 219 HBW / 230 HV or 95 HRB — higher than the 192 HBW / 90 HRB cap on TP347, TP347H, TP347LN, TP348, and TP348H. Hardness tests are part of lot acceptance under A213. Ask the mill to report hardness beside the tensile and grain-size results on the EN 10204 3.1 certificate.
Minimum wall vs average wall for A213 TP347W — which should I specify?
Order minimum wall when the boiler or superheater datasheet is written around a guaranteed minimum thickness after tolerance — the usual practice for A213 tube. Order average wall only when the purchase order explicitly allows average-wall product and the designer has accepted that basis. Put the wall basis on the enquiry before the mill selects A1016 tolerance tables.
Is Supplementary Requirement S2 listed for TP347W?
Not in the public A213–13 excerpt. S2 lists TP309HCb, TP310HCb, TP310HCbN, TP321, TP321H, TP347, TP347H, TP348, and TP348H. TP347W is absent from that printed list. If your project needs a lower-temperature stabilization after the 2000 °F solution anneal for S34705, negotiate the temperature and time on the purchase order rather than assuming S2 applies by grade nickname.
Is TP347W a good choice for chloride-rich cooling water?
Usually no as a first choice. Tungsten and vanadium support elevated-temperature strength and niobium helps intergranular corrosion resistance, but neither raises PREN the way molybdenum does. Prefer TP316L or a higher-Mo grade when chlorides dominate aqueous service; reserve TP347W for W-bearing boiler and superheater framing where the 90/38 ksi package earns its keep.
Can I dual-certify TP347W with TP347 on the same heat?
No as a chemistry path. TP347W requires tungsten, vanadium, and nitrogen bands that TP347 does not list, uses a fixed Nb band rather than the 10 × C formula, and carries a higher Table 4 tensile/hardness pair plus grain size 7–10. Spell any dual-marking fantasy on the enquiry and expect the mill to refuse unless a documented heat somehow clears both rows — do not assume it from a PMI gun.

Conclusion

ASTM A213 TP347W / UNS S34705 is the tungsten-bearing, vanadium-bearing, nitrogen-strengthened niobium stainless steel tube grade for boiler, superheater, and heat-exchanger service when W 1.50–2.60%, V 0.20–0.50%, N 0.10–0.25%, Nb 0.25–0.50%, Table 4 floors of 90/38 ksi, hardness max 219 HBW / 95 HRB, and grain size 7–10 must be certified together under a 2000 °F solution path. SHH STEEL supplies cold-finished and hot-finished seamless tube in the usual OD × wall / BWG band, solution annealed at 2000 °F [1100 °C], tested to Table 3 and Table 4 with W / V / N / Nb reported, and documented on EN 10204 3.1 certificates — with dual SA-213 marking only when the order asks for that separate ASME standard. For sister grades and stock-oriented size discussions, start from the A213/A213M hub, then send your OD × wall list, wall basis, dual-marking needs, and W/V/N/Nb requirements so we can align mill and near-term availability to the ASTM callout.

Contact: admin@steelspecs.com

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X