ASTM A213 TP310Cb Stainless Steel Tube
What is ASTM A213 TP310Cb Stainless Steel Tube
ASTM A213 / A213M covers seamless ferritic and austenitic alloy-steel boiler, superheater, and heat-exchanger tubes. Grade TP310Cb / UNS S31040 is the niobium-stabilized member of the 310 family: melting carbon ≤0.08%, chromium 24.0–26.0%, nickel 19.0–22.0%, and niobium (columbium) held to the formula band 10×C–1.10%. The “Cb” suffix is the stabilization story — not an H-grade carbon floor and not a molybdenum chloride grade. Buyers reach for TP310Cb when 25Cr–20Ni oxidation resistance must sit together with Nb binding of carbon against intergranular attack after welding or thermal exposure.
SHH STEEL can supply ASTM A213 TP310Cb stainless steel tube as seamless cold-finished and hot-finished product in the usual boiler, furnace, and heat-exchanger OD × wall / BWG band, shipped with EN 10204 3.1 mill test certificates that report ladle chemistry including niobium and the Table 4 tensile and hardness results. Dual A213 / SA-213 marking is available only when the purchase order asks for both independent standards. Browse 310-family grades on the A213/A213M hub.
Shop names such as 310Cb, 310Nb, S31040, or “stabilized 25-20 tube” do not replace the ASTM grade on the MTC. Sister grades under the same ASTM standard include A213 TP310S, A213 TP310H, A213 TP310HCb, A213 TP309Cb, and A213 TP347. A213 covers seamless tube only — cold-finished versus hot-finished is the process choice, not a WLD/HCW manufacturing-type letter.
Chemical Composition of A213 TP310Cb
Two chemistry layers matter for TP310Cb under ASTM A213. Melting analysis is mandatory for every heat; product analysis on finished tube applies only when Supplementary Requirement wording or the purchase order invokes it through ASTM A1016/A1016M, with tolerances typically from ASTM A480/A480M Table A1.1. Niobium is the first line a stabilization reviewer should check: the melt must satisfy Nb ≥10×C and Nb ≤1.10% together with C ≤0.08% and the 24–26 / 19–22 Cr–Ni windows.
The tables below reproduce the melt limits for TP310Cb / UNS S31040, the product-analysis limits from A480 Table A1.1, and a short snapshot against TP310S and TP310H. Values are maximum unless a range or formula is shown; ellipsis (…) means no requirement.
Melting analysis (heat / ladle analysis)
| Element | TP310Cb (UNS S31040) melting analysis |
|---|---|
| Carbon (C) | ≤ 0.08 |
| Manganese (Mn) | ≤ 2.00 |
| Phosphorus (P) | ≤ 0.045 |
| Sulfur (S) | ≤ 0.030 |
| Silicon (Si) | ≤ 1.00 |
| Chromium (Cr) | 24.0 – 26.0 |
| Nickel (Ni) | 19.0 – 22.0 |
| Molybdenum (Mo) | … (no requirement) |
| Nitrogen (N) | … (no requirement) |
| Niobium (Nb / Cb) | 10×C – 1.10 |
Source: ASTM A213/A213M stainless chemistry table for Grade TP310Cb / UNS S31040 (public mill / specification PDF excerpt — htpipe A213 table text / _ref_a213.txt). Confirm the ordered edition on the purchase order. Stainless table number is edition-dependent (Table 2 later / Table 1 older). “Cb” and “Nb” are the same stabilizer element in this grade row.
Product analysis — A480/A480M Table A1.1 tolerances applied
| Element | Melting | Tolerance (A480 A1.1) | Product analysis limit |
|---|---|---|---|
| Carbon (C) | ≤ 0.08 | 0.01 over | ≤ 0.09 |
| Manganese (Mn) | ≤ 2.00 | 0.04 over | ≤ 2.04 |
| Phosphorus (P) | ≤ 0.045 | 0.010 over | ≤ 0.055 |
| Sulfur (S) | ≤ 0.030 | 0.005 over | ≤ 0.035 |
| Silicon (Si) | ≤ 1.00 | 0.05 over | ≤ 1.05 |
| Chromium (Cr) | 24.0 – 26.0 | 0.25 under / over | 23.75 – 26.25 |
| Nickel (Ni) | 19.0 – 22.0 | 0.15 under / 0.20 over | 18.85 – 22.20 |
| Niobium (Nb) | 10×C – 1.10 | 0.05 under / over on max; min remains formula-tied | max ≤ 1.15; min still ≥10×C on melt basis — confirm A480 path if contractual |
Stabilization snapshot — TP310S / TP310Cb / TP310HCb
| Element | TP310S (S31008) | TP310Cb (S31040) | TP310HCb (S31041) |
|---|---|---|---|
| C | ≤ 0.08 | ≤ 0.08 | 0.04 – 0.10 |
| Cr / Ni | 24–26 / 19–22 | 24–26 / 19–22 | 24–26 / 19–22 |
| Nb (Cb) | … | 10×C – 1.10 | 10×C – 1.10 |
| Grain size | no mandate | no mandate | No. 7 or coarser |
Chromium 24–26% and nickel 19–22% are the oxidation-resistance story; niobium is the stabilization story. Carbon ≤0.08% is the same ceiling as TP310S — not an H-grade floor. For combined H-grade carbon plus Nb, open A213 TP310HCb. Dual TP310S/TP310Cb is not automatic: niobium must be intentionally melted to the formula band.
When product analysis is ordered, finished tube may read up to C 0.09%, Mn 2.04%, P 0.055%, S 0.035%, and Si 1.05%, with Cr 23.75–26.25% and Ni 18.85–22.20%. Niobium product-analysis practice for formula minima is edition-sensitive — confirm the A480 path if product Nb is contractual.
Mechanical Properties of A213 TP310Cb
ASTM A213 Table 4 sets the room-temperature tensile acceptance floor for TP310Cb at 75 ksi [515 MPa] tensile strength and 30 ksi [205 MPa] yield strength (0.2% offset), with elongation of 35% minimum in 2 in. or 50 mm — the same room-temperature pair as TP310S. Hardness maximum is 192 HBW / 200 HV or 90 HRB. Unlike TP310H / TP310HCb, TP310Cb does not carry a mandatory ASTM grain-size number in the heat-treatment table.
| Property | TP310Cb requirement |
|---|---|
| Tensile strength, min (Table 4) | 75 ksi [515 MPa] |
| Yield strength (0.2% offset), min (Table 4) | 30 ksi [205 MPa] |
| Elongation in 2 in. or 50 mm, min (Table 4) | 35% |
| Hardness, max (Table 4) | 192 HBW / 200 HV or 90 HRB |
| Grain size | No mandatory ASTM grain-size number (unlike TP310H / TP310HCb) |
Source: ASTM A213/A213M Table 4 for TP310Cb / UNS S31040 (public specification PDF excerpt — htpipe A213 table text). Mechanical property requirements do not apply to tubing smaller than 1/8 in. [3.2 mm] ID or thinner than 0.015 in. [0.4 mm] wall. Flattening and flaring tests sit beside tension and hardness on a lot basis.
Niobium stabilization is a chemistry acceptance story, not a higher Table 4 tensile floor. Ask for the Nb result on the EN 10204 3.1 certificate together with tensile and hardness — a 310S-looking MTC without Nb does not prove TP310Cb.
Dimensions and Tolerances
Dimensional supply for ASTM A213 TP310Cb is tube language — OD × wall (minimum or average) and BWG / gauge — covering boiler, furnace, and heat-exchanger sizes rather than leading with ASME B36.19 pipe schedules. Usual A213 sizes run from about 1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD with min wall about 0.015–0.500 in. [0.4–12.7 mm]; other diameters by agreement. State minimum versus average wall on the purchase order.
OD and wall variations follow ASTM A1016/A1016M as invoked by A213. Cold-finished tubes commonly hold tighter OD; hot-finished tubes allow wider windows. Confirm exact tolerance rows for the OD and finish on the ordered edition.
| Item | Typical A213 TP310Cb dimensional practice |
|---|---|
| Product form | Seamless only (cold-finished or hot-finished) |
| Usual size band | ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD; wall ~0.015–0.500 in. [0.4–12.7 mm] |
| Wall basis | Minimum wall (default for boiler / furnace / HX) or average wall when specified |
| OD / wall tolerances | Per ASTM A1016/A1016M for finish route and size |
| Length | Cut lengths for furnace / boiler / HX bundles; mill random by agreement |
| Secondary note | B36.19 schedules only as a buyer cross-reference |
Put cut list, welding/IGC context, and end preparation on the enquiry. Minimum wall remains a first-class A213 concept for stabilized 310 tube.
Equivalent Grades
Equivalence language around 310Cb tube often confuses Nb-stabilized 310 with Ti-stabilized 321 or Nb-stabilized 347 families. ASTM A213 Grade TP310Cb / UNS S31040 is the governing designation for this article; other product forms and near-chemistries are not automatic A213 substitutes.
| Designation | Notes |
|---|---|
| ASTM A213 / A213M Grade TP310Cb | Governing ASTM seamless boiler / HX tube product standard for this article |
| UNS S31040 | Unified number in the stainless chemistry table |
| ASME SA-213 TP310Cb | Separate ASME Code Book adoption — dual-mark only when the PO asks |
| Related S-grade | A213 TP310S — same Cr–Ni / C ceiling, no Nb requirement |
| Related H+Cb | A213 TP310HCb — H-grade carbon + Nb + grain size No. 7 or coarser |
| Related Nb 18-8 | A213 TP347 — Nb-stabilized but different Cr–Ni windows |
| Related plate | A240 / SA240 flat product in the 310 family — order plate and tube under their own standards |
Dual A213/SA-213 marking is a purchase-order option. Compare TP310S and TP310HCb on their own ASTM A213 pages before swapping stabilized versus unstabilized 310 inside a tube list.
Heat Treatment and Delivery Condition
TP310Cb under ASTM A213 is furnished solution treated at a minimum of 1900 °F [1040 °C], then quenched in water or cooled rapidly by other means. The heat-treatment table does not list a mandatory ASTM grain-size number for TP310Cb (unlike TP310H / TP310HCb).
Cold-finished versus hot-finished is a process and dimensional route, not a substitute for the anneal. Delivery condition for SHH STEEL TP310Cb is solution annealed and pickled (or bright annealed by agreement), with anneal temperature, quench method, and niobium result on the EN 10204 3.1 certificate. Straightening, cutting, and end finishing follow heat treatment.
Supplementary Requirement S2 (stabilizing heat treatment) in the public A213 excerpt explicitly lists TP310HCb among grades that shall receive a post-solution stabilizing treatment when S2 is specified; TP310Cb is not assumed from that HCb listing alone. If a project datasheet requires a stabilizing hold after solution anneal for TP310Cb, write the exact requirement onto the purchase order and confirm the ordered edition wording rather than assuming base A213 includes S2 for every Cb shipment.
Corrosion Resistance
TP310Cb combines 24–26% Cr / 19–22% Ni oxidation resistance with niobium stabilization against intergranular corrosion after welding or sensitizing exposure. Molybdenum remains a no-requirement ellipsis, so wet chloride pitting framing still belongs with A213 TP316L or higher-Mo grades — not with TP310Cb.
Nb ties up carbon as niobium carbides/carbonitrides so chromium stays available for passive-film continuity at grain boundaries. That is why datasheets calling for stabilized 310 after heavy welding or cyclic thermal exposure name TP310Cb rather than TP310S. For H-grade carbon plus the same stabilizer, use A213 TP310HCb. Ask for A262 Practice E on the PO when the project requires a demonstrated IGC test rather than chemistry-only assurance.
Applications of A213 TP310Cb Tube
Buyers specify ASTM A213 TP310Cb when furnace, radiant, or high-temperature heat-exchanger duty needs 25Cr–20Ni oxidation resistance together with niobium stabilization for weld-heat or cyclic IGC control — without an H-grade carbon floor. Typical placements include welded furnace coils, reformer-related tubing, and HX bundles where the datasheet explicitly calls for Cb/Nb-stabilized 310.
Do not treat TP310Cb as a nickname for A213 TP347 — Cr–Ni windows differ. When creep-range carbon and grain size are also mandatory, open A213 TP310HCb. SHH STEEL quotes OD × wall / BWG and confirms Nb on the MTC against the actual stabilization requirement.
| Service theme | Why TP310Cb is considered |
|---|---|
| Welded furnace / radiant coils | Nb stabilization + 24–26 / 19–22 oxidation resistance |
| HX with IGC concern after fabrication | Formula Nb 10×C–1.10 with C ≤0.08 |
| Not primary for creep H-grade lists | No mandatory grain size / no C floor — use TP310H or TP310HCb |
| Not primary for wet chlorides | No Mo requirement — use Mo grades instead |
Weldability
TP310Cb is intended for fabrications where niobium stabilization of the base metal matters after welding. Use matching or near-matching Nb-bearing 310 / 25-20 fillers when the joint design calls for stabilized deposit chemistry, and keep heat input controlled so the stabilization benefit is not undone by poor practice.
Tube-to-tubesheet and coil welding should confirm any project A262 or ferrite limits. Do not order TP310S and “fix” stabilization with filler alone when the datasheet names TP310Cb base metal. When H-grade carbon is also required, specify A213 TP310HCb. Repair welding, when permitted, follows A1016/A1016M as invoked by A213.
Surface Finishes
Standard delivery for ASTM A213 TP310Cb from SHH STEEL is solution annealed and pickled. Bright annealed finishes are available by agreement when process-side roughness or appearance requires them.
State finish together with OD × wall and end preparation. Niobium reporting on the MTC is independent of pickled versus bright surface — both finishes still need the chemistry line complete.
Inspection and Testing
Lot testing for ASTM A213 TP310Cb follows tension, hardness, flattening, and flaring under A213 / A1016. Chemistry verification must include niobium against the 10×C–1.10 formula on the heat (and on product when ordered). NDE follows the ordered edition and purchaser supplements.
EN 10204 3.1 certificates from SHH STEEL report ladle chemistry with Nb, Table 4 tensile and hardness, and heat-treatment condition. Request A262 Practice E or a stabilizing supplementary treatment explicitly when the datasheet requires them — do not assume they ride along with the Cb grade name. Dual A213/SA-213 marking and third-party witness are available when written into the enquiry.
Packaging and Shipping
TP310Cb tubes ship in capped or plugged bundles with weather protection matched to the route. Cut lengths for furnace and exchanger bundles are labeled by heat and size; export packing uses cases or steel-frame crates when required.
Marking includes ASTM A213, grade TP310Cb / UNS S31040, size, heat number, and SHH STEEL identification. Dual SA-213 marking appears only when the purchase order requests it. Packing lists track the same heat numbers shown on the EN 10204 3.1 certificates.
Why Choose SHH STEEL
SHH STEEL treats ASTM A213 TP310Cb as a stabilized specification product: Nb formula compliance is checked with Cr–Ni and Table 4 results before a heat is offered against an IGC-sensitive 310 tube list. Quotations state OD × wall / BWG, wall basis, finish route, and whether A262 or dual A213/SA-213 marking is required.
We keep S / H / Cb / HCb distinctions explicit so buyers do not receive unstabilized 310S labeled as 310Cb by nickname. EN 10204 3.1 documentation includes the niobium result. Compare sisters on the A213/A213M hub before freezing the tube bill of materials.
Supply Capability
SHH STEEL supplies ASTM A213 TP310Cb seamless stainless steel tube in cold-finished and hot-finished routes across the usual boiler, furnace, and heat-exchanger OD × wall / BWG band. Capability below is an enquiry range — not a frozen warehouse SKU or tonnage claim.
| Capability | SHH STEEL practice for TP310Cb |
|---|---|
| Product form | Seamless cold-finished and hot-finished tube |
| Standards | ASTM A213 / A213M; dual SA-213 when PO asks |
| Size band | Typical within ~1/8 in. ID to 5 in. OD; other diameters by agreement |
| Wall basis | Minimum wall or average wall as specified |
| Documentation | EN 10204 3.1 MTC with Nb result; A262 / third-party witness on request |
| Trade terms | FOB / CFR / CIF / EXW and other agreed Incoterms |
Stock / Available sizes
SHH STEEL quotes TP310Cb against a stock-and-mill enquiry range rather than a frozen SKU/tonnage list. Representative OD × wall / BWG combinations for furnace, boiler, and heat-exchanger tube appear below.
| Item | Typical stock / enquiry range for TP310Cb |
|---|---|
| Outside diameter | 19.05, 25.4, 31.8, 38.1, 42.4, 50.8, 60.3, 76.2 mm (and other furnace/HX ODs on enquiry; through the usual A213 ~5 in. [127 mm] band) |
| Wall / BWG | BWG 10–18 class walls and metric min-wall equivalents; heavier walls by agreement |
| Common OD × wall examples | 25.4 × 2.11 mm; 31.8 × 2.77 mm; 38.1 × 2.77 mm; 42.4 × 3.56 mm; 50.8 × 3.05 mm; 60.3 × 3.91 mm — illustrative, confirm min vs average wall |
| Length | Cut lengths for furnace / exchanger bundles; bends and random mill lengths on enquiry |
| Special | Non-standard OD/wall, bright anneal, dual A213/SA-213, A262 Practice E, stabilizing S2 if edition/PO requires — confirm before heat reservation |
Send OD × wall (or BWG), wall basis, finish route, quantity or cut list, marking (A213 or dual A213/SA-213), and any IGC or Supplementary Requirements on one enquiry. We confirm Cr 24–26% / Ni 19–22%, C ≤0.08%, Nb 10×C–1.10%, and Table 4 75/30 ksi without inventing fake warehouse codes. Sisters A213 TP310S, A213 TP310HCb, and A213 TP309Cb sit on the same hub.
FAQ
-
Is ASTM A213 the same as ASME SA-213 for TP310Cb?
- No. ASTM A213 / A213M is the ASTM International product specification for seamless boiler, superheater, and heat-exchanger tubes; ASME SA-213 / SA-213M is the separate ASME Code Book adoption. Dual-mark only when the purchase order asks for both names on the stencil and MTC. Chemistry and tensile floors align closely for a given referenced edition, but the standards remain independent.
-
Does ASTM A213 TP310Cb include welded or HCW tube?
- No. ASTM A213 covers seamless boiler, superheater, and heat-exchanger tubes only. There is no WLD or HCW manufacturing-type letter under A213. Cold-finished versus hot-finished describes the seamless process route and dimensional tolerances — not a welded product form. Order welded stainless pipe under a different product standard when that form is required.
-
What is the chemistry of ASTM A213 TP310Cb?
- Melting analysis for TP310Cb / UNS S31040 is C ≤0.08%, Mn ≤2.00%, P ≤0.045%, S ≤0.030%, Si ≤1.00%, Cr 24.0–26.0%, Ni 19.0–22.0%, Nb 10×C–1.10%, with Mo and N as no-requirement ellipses. Confirm the ordered A213 edition. Niobium must meet both the formula minimum and the 1.10% maximum on the heat analysis.
-
What does Cb mean in TP310Cb?
- Cb is the traditional designation for columbium, the same element as niobium (Nb). In ASTM A213 TP310Cb the stabilizer is specified as Nb (Cb) in the formula band 10×C–1.10%. Shop language saying "310Nb" or "Cb-stabilized 310" should still map to the ASTM grade and UNS S31040 on the MTC — not to a different product form.
-
TP310Cb vs TP310S — which A213 grade should I order?
- Order TP310Cb when the datasheet requires niobium stabilization (Nb 10×C–1.10) with the 24–26 / 19–22 Cr–Ni windows and C ≤0.08%. Order TP310S when the same Cr–Ni and carbon ceiling are enough without an Nb requirement. Dual marking is not automatic: Nb must be intentionally melted and reported.
-
TP310Cb vs TP310H — when is stabilization more important than the H-grade floor?
- TP310H focuses on C 0.04–0.10% and grain size No. 7 or coarser for creep-oriented service, without an Nb requirement. TP310Cb focuses on Nb stabilization with C ≤0.08% and no mandatory grain-size number. If you need both the H-grade carbon/grain-size package and Nb, order A213 TP310HCb rather than hoping one grade covers the other.
-
TP310Cb vs TP347 — are they interchangeable?
- No. Both are niobium-stabilized austenitics, but TP347 sits in the 18-8 Cr–Ni family while TP310Cb uses 24–26% Cr / 19–22% Ni. Oxidation resistance, allowables, and weld procedure bases differ. Order each under its own ASTM A213 grade page and do not swap them by "stabilized stainless" nickname alone.
-
Does Table 4 set a hardness limit for TP310Cb?
- Yes. Table 4 lists hardness maximum 192 HBW / 200 HV or 90 HRB with 75 ksi tensile, 30 ksi yield, and 35% elongation. Hardness belongs on the release package together with the niobium chemistry result — tensile alone does not prove TP310Cb.
-
What heat treatment does A213 require for TP310Cb?
- Solution treatment at a minimum of 1900 °F [1040 °C], followed by water quench or other rapid cool. There is no mandatory ASTM grain-size number for TP310Cb in the public heat-treatment table. If a stabilizing supplementary treatment is required, write it onto the PO and confirm edition wording — S2 listing for HCb grades is not assumed to auto-apply to TP310Cb.
-
Minimum wall vs average wall for A213 TP310Cb — which should I specify?
- Boiler, furnace, and HX datasheets almost always expect minimum wall. Average wall is allowed when the purchase order says so, with A1016/A1016M tolerances for that basis. State wall basis explicitly — do not rely on pipe schedule numbers as the primary A213 wall story.
-
Is TP310Cb a good choice for chloride-rich cooling water?
- Not as a primary chloride strategy. Molybdenum is a no-requirement ellipsis on TP310Cb, so wet chloride pitting resistance is not the grade’s design story. Use Mo-bearing grades for chloride-rich cooling; reserve TP310Cb for oxidation-led service that also needs Nb stabilization.
Conclusion
ASTM A213 TP310Cb / UNS S31040 is the niobium-stabilized 24–26% Cr / 19–22% Ni seamless stainless steel tube for boiler, furnace, and heat-exchanger service when high-temperature oxidation resistance and Cb/Nb stabilization against intergranular attack both drive grade selection — without an H-grade carbon floor. SHH STEEL supplies cold-finished and hot-finished seamless tube in the usual OD × wall / BWG band, solution annealed at 1900 °F [1040 °C], tested to Table 4 75/30 ksi and hardness limits, with niobium reported on EN 10204 3.1 certificates — and dual SA-213 marking only when the purchase order asks.