SHH STEEL offers ASME SA789/SA789M-compliant 304/316 stainless steel tubes. ASME SA789/SA789M specifies seamless and welded duplex stainless steel tubes for high-corrosion and high-strength environments. Certified quality, competitive prices, customizable. Trust SHH STEEL!

ASME SA789 UNS S83071 Super Duplex Stainless Steel Tube | ASME SA789 Stainless Steel - SHH STEEL

ASME SA789 UNS S83071 Super Duplex Stainless Steel Tube

ASME SA789 UNS S83071 super duplex stainless steel tube (seamless and welded, no filler metal) with Cr 29.0–31.0%, Ni 6.0–8.0%, Mo 3.0–4.0%, N 0.28–0.40%, tensile floor 120 ksi [830 MPa], yield 98 ksi [680 MPa], elong 25% min, hardness max 300 HBW / 32 HRC, solution treated 1830–2100 °F [1000–1150 °C]. SHH STEEL produces and supplies SA789 S83071 tube with EN 10204 3.1 MTC under ASME Section II Part A.
View More
ASME SA789 UNS S82441 Lean Duplex Stainless Steel Tube | ASME SA789 Stainless Steel - SHH STEEL

ASME SA789 UNS S82441 Lean Duplex Stainless Steel Tube

ASME SA789 UNS S82441 lean duplex stainless steel tube (seamless and welded, no filler metal) with Cr 23.0–25.0%, Ni 3.0–4.5%, Mo 1.00–2.00%, N 0.20–0.30%, Mn 2.50–4.00%, Cu 0.10–0.80%, wall-dependent tensile (107/78 ksi under 0.40 in. wall; 99/70 ksi above), hardness max 290 HBW / 30 HRC, solution treated 1830 °F [1000 °C] min. SHH STEEL produces and supplies SA789 S82441 tube with EN 10204 3.1 MTC under ASME Section II Part A.
View More
ASME SA789 UNS S82031 Lean Duplex Stainless Steel Tube | ASME SA789 Stainless Steel - SHH STEEL

ASME SA789 UNS S82031 Lean Duplex Stainless Steel Tube

ASME SA789 UNS S82031 lean duplex stainless steel tube (seamless and welded, no filler metal) with Cr 19.0–22.0%, Ni 2.0–4.0%, Mo 0.60–1.40%, N 0.14–0.24%, C 0.05 max, wall-dependent tensile (102/73 ksi ≤0.187 in. wall), elong 35% min, solution treated 1830 °F [1000 °C] min. SHH STEEL produces and supplies SA789 S82031 tube with EN 10204 3.1 MTC under ASME Section II Part A.
View More
ASME SA789 UNS S82011 Lean Duplex Stainless Steel Tube | ASME SA789 Stainless Steel - SHH STEEL

ASME SA789 UNS S82011 Lean Duplex Stainless Steel Tube

ASME SA789 UNS S82011 lean duplex stainless steel tube (seamless and welded, no filler metal) with Cr 20.5–23.5%, Ni 1.00–2.00%, Mo 0.10–1.00%, N 0.15–0.27%, Mn 2.0–3.0%, wall-dependent tensile (101/75 ksi ≤0.187 in. wall; 95/65 ksi above), hardness max 293 HBW / 31 HRC, solution treated 1850–2050 °F [1010–1120 °C]. SHH STEEL produces and supplies SA789 S82011 tube with EN 10204 3.1 MTC under ASME Section II Part A.
View More
ASME SA789 UNS S39277 Super Duplex Stainless Steel Tube | ASME SA789 Stainless Steel - SHH STEEL

ASME SA789 UNS S39277 Super Duplex Stainless Steel Tube

ASME SA789 UNS S39277 super duplex stainless steel tube (seamless and welded, no filler metal) with Cr 24.0–26.0%, Ni 6.5–8.0%, Mo 3.00–4.00%, N 0.23–0.33%, Cu 1.20–2.00%, W 0.80–1.21%, C 0.025 max, tensile floor 120 ksi [825 MPa], yield 90 ksi [620 MPa], elong 25% min, hardness max 290 HBW / 30 HRC, solution treated 1975–2155 °F [1080–1180 °C]. SHH STEEL produces and supplies SA789 S39277 tube with EN 10204 3.1 MTC under ASME Section II Part A.
View More
ASME SA789 UNS S39274 Super Duplex Stainless Steel Tube | ASME SA789 Stainless Steel - SHH STEEL

ASME SA789 UNS S39274 Super Duplex Stainless Steel Tube

ASME SA789 UNS S39274 super duplex stainless steel tube (seamless and welded, no filler metal) with Cr 24.0–26.0%, Ni 6.0–8.0%, Mo 2.5–3.5%, N 0.24–0.32%, Cu 0.20–0.80%, W 1.50–2.50%, tensile floor 116 ksi [800 MPa], yield 80 ksi [550 MPa], elong 15% min, hardness max 310 HBW / 32 HRC, solution treated 1920–2060 °F [1025–1125 °C]. SHH STEEL produces and supplies SA789 S39274 tube with EN 10204 3.1 MTC under ASME Section II Part A.
View More
ASME SA789 UNS S33207 Super Duplex Stainless Steel Tube | ASME SA789 Stainless Steel - SHH STEEL

ASME SA789 UNS S33207 Super Duplex Stainless Steel Tube

ASME SA789 UNS S33207 super duplex stainless steel tube (seamless and welded, no filler metal) with Cr 29.0–33.0%, Ni 6.0–9.0%, Mo 3.0–5.0%, N 0.40–0.60%, wall-dependent tensile (up to 138/112 ksi under 0.157 in. wall), hardness max 336 HBW / 36 HRC, solution treated 1905–2085 °F [1040–1140 °C]. SHH STEEL produces and supplies SA789 S33207 tube with EN 10204 3.1 MTC under ASME Section II Part A.
View More
ASME SA789 UNS S32950 Super Duplex Stainless Steel Tube | ASME SA789 Stainless Steel - SHH STEEL

ASME SA789 UNS S32950 Super Duplex Stainless Steel Tube

ASME SA789 UNS S32950 super duplex stainless steel tube (seamless and welded, no filler metal) with Cr 26.0–29.0%, Ni 3.5–5.2%, Mo 1.00–2.50%, N 0.15–0.35%, tensile floor 100 ksi [690 MPa], yield 70 ksi [480 MPa], elong 20% min, hardness max 290 HBW / 30 HRC, solution treated 1820–1880 °F [990–1025 °C]. SHH STEEL produces and supplies SA789 S32950 tube with EN 10204 3.1 MTC under ASME Section II Part A.
View More
ASME SA789 UNS S32906 Super Duplex Stainless Steel Tube | ASME SA789 Stainless Steel - SHH STEEL

ASME SA789 UNS S32906 Super Duplex Stainless Steel Tube

ASME SA789 UNS S32906 super duplex stainless steel tube (seamless and welded, no filler metal) with Cr 28.0–30.0%, Ni 5.8–7.5%, Mo 1.50–2.60%, N 0.30–0.40%, wall-dependent tensile (116/94 ksi under 0.40 in. wall; 109/80 ksi above), hardness max 300 HBW / 32 HRC, solution treated 1870–2100 °F [1020–1150 °C]. SHH STEEL produces and supplies SA789 S32906 tube with EN 10204 3.1 MTC under ASME Section II Part A.
View More
ASME SA789 UNS S32900 Duplex Stainless Steel Tube | ASME SA789 Stainless Steel - SHH STEEL

ASME SA789 UNS S32900 Duplex Stainless Steel Tube

ASME SA789 UNS S32900 duplex stainless steel tube (seamless and welded, no filler metal) with Cr 23.0–28.0%, Ni 2.5–5.0%, Mo 1.00–2.00%, C 0.08 max (N not required), tensile floor 90 ksi [620 MPa], yield 70 ksi [485 MPa], elong 20% min, hardness max 271 HBW / 28 HRC, solution treated 1700–1750 °F [925–955 °C]. SHH STEEL produces and supplies SA789 S32900 tube with EN 10204 3.1 MTC under ASME Section II Part A.
View More
ASME SA789 UNS S32808 Super Duplex Stainless Steel Tube | ASME SA789 Stainless Steel - SHH STEEL

ASME SA789 UNS S32808 Super Duplex Stainless Steel Tube

ASME SA789 UNS S32808 super duplex stainless steel tube (seamless and welded, no filler metal) with Cr 27.0–27.9%, Ni 7.0–8.2%, Mo 0.80–1.20%, N 0.30–0.40%, W 2.10–2.50%, tensile floor 116 ksi [800 MPa], yield 80 ksi [550 MPa], elong 15% min, hardness max 310 HBW / 32 HRC, solution treated 1920–2100 °F [1050–1150 °C]. SHH STEEL produces and supplies SA789 S32808 tube with EN 10204 3.1 MTC under ASME Section II Part A.
View More
ASME SA789 UNS S32760 Super Duplex Stainless Steel Tube | ASME SA789 Stainless Steel - SHH STEEL

ASME SA789 UNS S32760 Super Duplex Stainless Steel Tube

ASME SA789 UNS S32760 super duplex stainless steel tube (seamless and welded, no filler metal) with Cr 24.0–26.0%, Ni 6.0–8.0%, Mo 3.0–4.0%, N 0.20–0.30%, Cu 0.50–1.00%, W 0.50–1.00% (PREN ≥40 footnote), tensile floor 109 ksi [750 MPa], yield 80 ksi [550 MPa], elong 25% min, hardness max 310 HBW / 32 HRC, solution treated 1960–2085 °F [1070–1140 °C]. SHH STEEL produces and supplies SA789 S32760 tube with EN 10204 3.1 MTC under ASME Section II Part A.
View More

ASME SA 789/SA 789M Stainless Steel Products

Stainless Steel Pipes and Tubes supplier and exporter

Stainless Steel Pipes and Tubes

SHH STEEL, a premier Stainless Steel Pipes and Tubes exporter, produces and exports stainless steel pipes and tubes for chemical, marine, and food processing industries. Our seamless and welded products, like 304 and 316L (ASTM A312), ensure corrosion resistance and strength. With a 5,000-ton inventory, we deliver in 3–5 days, backed by SGS/TUV inspections and mill certificates. Choose SHH STEEL for seamless stainless steel pipes and custom solutions.

Stainless Steel Pipes and Tubes

SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

    *

    *

    *

    *


    X