ASTM A213 TP202 Stainless Steel Tube | ASTM A213 Stainless Steel - SHH STEEL

ASTM A213 TP202 Stainless Steel Tube

ASTM A213 TP202 / UNS S20200 seamless boiler, superheater and heat-exchanger tube — the higher-manganese Mn–N austenitic with Mn 7.5–10.0%, Ni 4.0–6.0%, Cr 17.0–19.0%, N ≤0.25% and C ≤0.15%. Under A213 Table 4 the floor is 90/45 ksi with hardness max 219 HBW / 95 HRB. SHH STEEL supplies cold-finished and hot-finished seamless tube with EN 10204 3.1 MTCs.
Grade
TP202 / UNS S20200
Standard
ASTM A213 / A213M
Product form
Seamless boiler / superheater / heat-exchanger tube (cold-finished and hot-finished)
Size
Typical OD × min wall (or average wall) within ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD and ~0.015–0.500 in. [0.4–12.7 mm] wall; other diameters by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is ASTM A213 TP202 Stainless Steel Tube

ASTM A213 / A213M covers seamless ferritic and austenitic alloy-steel boiler, superheater, and heat-exchanger tubes. Inside the stainless chemistry table, Grade TP202 / UNS S20200 is the higher-manganese partner to TP201: carbon ≤0.15%, manganese 7.5–10.0%, chromium 17.0–19.0%, nickel 4.0–6.0%, and nitrogen ≤0.25%. The extra manganese and roughly one percentage point more chromium move corrosion and strength slightly upward versus A213 TP201, while nickel stays lean compared with A213 TP304. Buyers who write “202 HX tube” still need to name A213 (or the separate ASME SA-213 adoption) on the purchase order so the mill applies the tube product standard’s minimum-wall rules, tests, and marking clauses.

SHH STEEL can supply ASTM A213 TP202 stainless steel tube as seamless cold-finished and hot-finished product in the usual boiler and heat-exchanger OD × wall / BWG band, shipped with EN 10204 3.1 mill test certificates that report the full ladle chemistry and the Table 4 tensile and hardness results. When a project also needs ASME Code Book marking, we dual-mark A213 / SA-213 on the same lengths only if the purchase order says so — ASTM A213 and ASME SA-213 remain two independent standards. Browse the grade family on the A213/A213M hub.

Shop names such as 202, S20200, or high-Mn boiler/HX tube do not replace the ASTM grade on the MTC or stencil. Sister grades under the same ASTM standard include A213 TP201, A213 TP304 / A213 TP304L, and A213 TP316 / A213 TP316L. A213 is seamless tube only — no welded or HCW manufacturing type — so cold-finished versus hot-finished is the process choice, not a WLD/HCW letter on the stencil.

Chemical Composition of A213 TP202

Two chemistry layers matter for TP202 under ASTM A213. Melting (heat or ladle) analysis is mandatory for every heat; product analysis on finished tube applies only when Supplementary Requirement wording or the purchase order invokes it through ASTM A1016/A1016M. Product-analysis tolerances are not reprinted as a standalone chemistry table inside A213; when ordered, they typically flow from ASTM A480/A480M Table A1.1. SHH STEEL reports actual ladle values — and product values when ordered — and does not advertise unpublished tighter catalogue windows.

The tables below reproduce the heat analysis for TP202 / UNS S20200 and the product-analysis limits from A480 Table A1.1 tolerances. Values are maximum unless a range is shown. Later A213 editions place austenitic stainless grades in Table 2 (older editions used Table 1); confirm the ordered edition before treating secondary catalogues as acceptance text. Public PDF excerpts sometimes OCR the nitrogen max as “.025”; the accepted stainless-table value used here is N ≤0.25%, matching Gangsteel / Ferrobend A213 TP202 summaries and the A240/A312 sister chemistry for S20200.

Melting analysis (heat / ladle analysis)

Element TP202 (UNS S20200) melting analysis
Carbon (C) ≤ 0.15
Manganese (Mn) 7.5 – 10.0
Phosphorus (P) ≤ 0.060
Sulfur (S) ≤ 0.030
Silicon (Si) ≤ 1.00
Chromium (Cr) 17.0 – 19.0
Nickel (Ni) 4.0 – 6.0
Molybdenum (Mo) … (no requirement)
Nitrogen (N) ≤ 0.25

Source: ASTM A213/A213M stainless chemistry table for Grade TP202 / UNS S20200 (public mill / specification summaries cross-checked — htpipe A213 PDF, Gangsteel A213 TP202 page). Confirm the ordered edition. Nitrogen analysis method is a matter of agreement between purchaser and producer per the standard’s nitrogen footnote.

Product analysis — A480/A480M Table A1.1 tolerances applied

Element Melting Tolerance (A480 A1.1) Product analysis limit
Carbon (C) ≤ 0.15 0.01 over ≤ 0.16
Manganese (Mn) 7.5 – 10.0 0.06 under / 0.10 over 7.44 – 10.10
Phosphorus (P) ≤ 0.060 0.010 over ≤ 0.070
Sulfur (S) ≤ 0.030 0.005 over ≤ 0.035
Silicon (Si) ≤ 1.00 0.05 over ≤ 1.05
Chromium (Cr) 17.0 – 19.0 0.20 under / over 16.80 – 19.20
Nickel (Ni) 4.0 – 6.0 0.07 under / 0.15 over 3.93 – 6.15
Nitrogen (N) ≤ 0.25 0.02 over ≤ 0.27

Manganese at 7.5–10.0% is the first line a reviewer should check on a TP202 certificate — it separates this grade from TP201’s 5.5–7.5% band and from TP304’s ≤2.00% ceiling. Chromium 17–19% and nickel 4–6% sit a step above TP201; nitrogen ≤0.25% reinforces austenite and contributes to strength. Carbon ≤0.15% still sits above an L-grade ceiling, so as-welded intergranular risk needs the same honest review as TP201. Versus A213 TP304, TP202 remains nickel-lean and molybdenum-free.

When product analysis is ordered, finished tube may read up to C 0.16%, Mn 10.10%, P 0.070%, S 0.035%, Si 1.05%, and N 0.27%, with Cr 16.80–19.20% and Ni 3.93–6.15%. Those are the product limits we quote from the A480 A1.1 path for this grade. Put any tighter project manganese or nitrogen ceiling on the purchase order before the heat is selected — high-Mn heats can run toward the top of the band.

Mechanical Properties of A213 TP202

ASTM A213 Table 4 sets the tensile acceptance floor for TP202 at 90 ksi [620 MPa] tensile strength and 45 ksi [310 MPa] yield strength (0.2% offset), with elongation of 35% minimum in 2 in. or 50 mm. The yield floor is higher than TP201’s 38 ksi and substantially higher than TP304’s 30 ksi — a direct result of the manganese-nitrogen solid-solution strengthening that the product standard captures in this row. Hardness maximum is 219 HBW / 230 HV or 95 HRB, matching the TP201 hardness cap, and hardness tests are part of lot acceptance under A213.

Property TP202 requirement (Table 4)
Tensile strength, min 90 ksi [620 MPa]
Yield strength (0.2% offset), min 45 ksi [310 MPa]
Elongation in 2 in. or 50 mm, min 35%
Hardness, max 219 HBW / 230 HV or 95 HRB

Source: ASTM A213/A213M Table 4 for TP202 / UNS S20200 (public specification summaries — htpipe A213 PDF, Gangsteel A213 TP202, Blackburn Metals A213 tubular excerpt). Mechanical property requirements do not apply to tubing smaller than 1/8 in. [3.2 mm] inside diameter or thinner than 0.015 in. [0.4 mm] wall. Flattening and flaring tests are also required on a lot basis for finished tube.

The 45 ksi yield floor is why some designers look at TP202 when wall thickness or pressure drop is tight in a utility exchanger — but only after corrosion and weld reviews clear the lean chemistry. Do not import A312 pipe tensile language onto this A213 tube page; clear the Table 4 numbers that govern the ordered edition. Actual mill certificates often clear the floor with margin; design calculations should still use Table 4 unless the PO states higher guaranteed values the mill has accepted in writing.

Dimensions and Tolerances

Dimensional supply for ASTM A213 TP202 is tube language — outside diameter × wall thickness (minimum wall or average wall) and, commercially, BWG / gauge — not ASME B36.19 pipe schedules as the primary size story. The sizes usually furnished under A213 run from about 1/8 in. [3.2 mm] inside diameter to 5 in. [127 mm] outside diameter, with minimum wall from about 0.015 to 0.500 in. [0.4 to 12.7 mm]; tubing with other diameters may be furnished when all other requirements of the specification are met. State on the purchase order whether wall is minimum or average.

Outside-diameter and wall variations follow ASTM A1016/A1016M as invoked by A213. Cold-finished tubes commonly hold tighter OD control; hot-finished tubes allow wider OD and wall windows. Permissible variations from a specified average wall for cold-finished tube are often summarized as ±10% of the specified average wall, while minimum-wall product is accepted to the A1016 minimum-wall tables. Confirm the exact A1016 rows for the OD and finish route on the ordered edition.

Item Typical A213 TP202 dimensional practice
Product form Seamless only (cold-finished or hot-finished)
Usual size band ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD; wall ~0.015–0.500 in. [0.4–12.7 mm] min (or average wall if PO says so)
Wall basis Minimum wall (default commercial practice) or average wall when specified
OD / wall tolerances Per ASTM A1016/A1016M for the finish route and size; cold-finished average wall often ±10%
Length Cut lengths for HX / boiler bundles, or mill random lengths by agreement
Secondary size note ASME B36.19 schedules may appear only when a buyer asks for a pipe-schedule cross-reference — not as the primary A213 size callout

High-Mn austenitics work-harden quickly in bending, so state U-bend radius and whether cold bends will be solution-treated afterward. Minimum wall remains a first-class A213 concept — if the datasheet assumes average wall, say so before the heat is rolled.

Equivalent Grades

Equivalence language around TP202 tube is often looser than a heat-exchanger purchase order can afford. ASTM A213 Grade TP202 / UNS S20200 is the governing designation for this article; EN 1.4373 and JIS SUS202 are approximate wrought names that point to similar high-Mn chemistry families but are not automatic substitutes on an A213 mill test certificate. When a datasheet says “equivalent to 202,” confirm which product standard, tensile/hardness table, and heat-treatment clause the mill will actually certify.

Designation Notes
ASTM A213 / A213M Grade TP202 Governing ASTM seamless boiler / HX tube product standard for this article
UNS S20200 Unified number listed in the stainless chemistry table
ASME SA-213 TP202 Separate ASME Code Book adoption — dual-mark only when the PO asks
EN 1.4373 (X12CrMnNiN18-9-5) Approximate wrought high-Mn stainless designation; order EN tube forms under the relevant EN tube specs
JIS SUS202 Approximate Japanese grade name; confirm the Japanese tube product standard when ordering JIS product
Related plate A240 / SA240 flat product in the same UNS family — order plate and tube under their own product standards

Dual A213/SA-213 marking is a purchase-order option, not a claim that the two standards are one document. Compare TP201 and the 18-8 sisters on their own ASTM A213 pages before swapping grades on nickel-cost or yield-strength alone.

Heat Treatment and Delivery Condition

TP202 under ASTM A213 is furnished solution treated at a minimum of 1900 °F [1040 °C], then quenched in water or cooled rapidly by other means at a rate sufficient to prevent carbide reprecipitation. That heat-treatment row applies to both cold-finished and hot-finished seamless tube. With carbon allowed up to 0.15%, incomplete solution treatment or slow cool is an invitation to sensitization — not a paperwork detail.

Cold-finished versus hot-finished is a process and dimensional route, not a substitute for the anneal. Cold-finished tube is typically drawn after hot working and then solution treated; hot-finished tube may be quenched after hot forming when the edition allows and finishing temperature is not below the minimum anneal. Delivery condition for SHH STEEL TP202 is solution annealed and pickled (or bright annealed by agreement), with heat-treatment temperature and quench method stated on the EN 10204 3.1 certificate.

When Supplementary Requirement language for intergranular-corrosion capability (commonly ASTM A262 Practice E on as-shipped specimens for non-L grades) is ordered, the corrosion test report travels with the heat-treatment record. After heavy U-bending, ask whether a re-solution anneal of the bend zone is part of the fabrication sequence — high-Mn grades work-harden and can pick up residual stress that a fabricator needs to manage deliberately.

Corrosion Resistance

TP202’s chromium band (17–19%) and modest nickel give a passive film that handles many oxidizing process fluids, clean steam and condensate duties, and mild organic media. Relative to A213 TP201, the extra chromium and manganese usually put TP202 a half-step ahead in general corrosion resistance, but neither grade carries molybdenum, so chloride pitting and crevice attack remain limiting in coastal cooling water, brines, and seawater-leaning exchangers. Step up to A213 TP316 / A213 TP316L when chlorides dominate.

Intergranular corrosion risk after tube-to-tubesheet welding tracks the carbon ceiling: at ≤0.15% C, as-welded service in a sensitizing temperature window needs a post-weld solution anneal, a contractual A262 Practice E test, or a switch to a low-carbon sister. ASTM A213 does not publish a corrosion-rate table for TP202; selection remains engineering judgment against fluid, temperature, velocity, and inspection philosophy. SHH STEEL will not market TP202 as a chloride equal of 316 or even of well-specified 304 — that claim is not supported by the product standard.

Applications of A213 TP202 Tube

TP202 seamless tube under A213 is chosen when a Mn–N austenitic with a higher yield floor and a slightly richer Cr/Mn band than TP201 fits the duty, and when nickel cost still rules out classic 18-8. It is a heat-exchanger and moderate-duty tube grade first — not an automatic creep-range boiler substitute for H grades. The table below pairs typical application areas with a selection note.

Application area Typical use of TP202 tube Selection note
Utility / process heat exchangers Straight and U-bend HX tubes where 45 ksi yield helps wall selection Confirm chloride level; state bend radius and post-bend anneal if needed
Condensers / coolers (low chloride) Seamless tube in fresh-water or low-chloride cooling circuits Prefer TP316/L if cooling water is coastal or brine-leaning
Food / beverage utilities Utility HX where 202 stainless tube is accepted by the end user Follow hygiene finish and WPS requirements
Cost-sensitive Ni-lean projects Comparisons against TP304 on installed cost with higher yield Run corrosion and sensitization reviews before substituting
General mild corrosive tube duty Oxidizing or organic media that do not demand molybdenum Open TP304/TP316 when industry acceptance of 18-8 matters more

For a leaner Mn band open A213 TP201; for classic 18-8 open A213 TP304; for creep-range boiler framing open A213 TP304H on the same A213/A213M hub.

Weldability

TP202 tube welds with matching or near-matching austenitic filler for tube-to-tubesheet joints and fabrication joins, but high manganese and the 0.15% carbon ceiling make procedure discipline non-optional. Common practice uses ER202 / ER308L-family fillers under a qualified WPS, with heat-input and interpass limits written to limit HAZ sensitization. Many fabricators prefer a low-carbon deposit even when the base tube is standard TP202. A213 governs the seamless tube product, not the field or shop weld procedure — heat input, interpass, and post-weld cleaning remain the fabricator’s responsibility under the applicable code.

Because A213 TP202 is seamless, there is no mill longitudinal weld to radiograph the way welded pipe standards describe. Focus inspection language on tube integrity (hydro or NDE of each length), tube-to-tubesheet joint quality, and any contractual corrosion test on the base metal. Work-hardening during expanding or bending is more pronounced than in TP304; specify expander settings and bend radii on the enquiry so the mill and fabricator share one expectation. For as-welded sensitizing service, plan a post-weld solution anneal or change the base metal rather than hoping the WPS alone protects standard-carbon TP202.

Surface Finishes

Standard mill delivery for ASTM A213 TP202 is solution annealed and pickled, leaving a clean matte finish suitable for most boiler and heat-exchanger tube duty. Bright annealing under protective atmosphere produces a smoother reflective surface used on some clean-process lines and must be called out because it changes the heat-treatment route. Light polish or specified Ra on the bore or OD is a commercial or service-center operation on top of A213 product, not automatic with the grade stamp.

When a fouling-sensitive or hygienic exchanger specification quotes an Ra maximum on the bore, put it on the tube purchase order with its own acceptance language and sampling plan. SHH STEEL stencils grade and heat treatment as standard requirements; polish, special OD grind, and passivation after fabrication remain commercial extras unless the contract says otherwise. Order end preparation together with finish so receiving inspection shares one acceptance language.

Inspection and Testing

Base ASTM A213 testing for TP202 includes heat analysis, tension tests to the Table 4 floors (90/45 ksi), hardness tests to the Table 4 maximum (219 HBW / 95 HRB), flattening and flaring tests on a lot basis, and either hydrostatic testing or nondestructive electric testing of each length. The manufacturer may choose hydro versus NDE unless the purchase order fixes the method. Marking includes the ASTM designation, grade, size, heat number, and other clause-required data so receiving inspection can tie each length back to the MTC.

Supplementary Requirements commonly added on TP202 tube orders are summarized below. Invoke them by number or clear purchase-order wording; mills will not assume product analysis or intergranular-corrosion testing from a verbal “full certs” note.

Option Purpose
Product analysis Confirms chemistry on finished tube (via A1016 / PO language) — useful when Mn sits near the top of the 7.5–10.0% band
Intergranular corrosion A262 Practice E (or agreed practice) as a contractual Supplementary Requirement
Minimum vs average wall States which wall basis the size callout uses
Fixed hydro or NDE method Removes manufacturer’s option when the end user mandates one route
Third-party inspection / EN 10204 3.2 Witnessed testing and certificate when the project requires it

Lot definitions for continuous heat treatment or direct quench after hot forming follow the size-based lot sizes in A213; ask the mill to state lot identity clearly on the certificate so hardness and tension specimens map cleanly to the bundle you receive.

Packaging and Shipping

TP202 tube leaves SHH STEEL bundled, capped or end-protected, and tagged for export or domestic delivery according to the length mix and bend form on the order. Bundle tags repeat the ASTM A213 grade, OD × wall (or BWG), heat number, and PO reference so site receiving can check the shipment without opening every certificate packet first. U-bent tubes need extra cradle or case protection so bend radii and legs are not distorted in transit — especially important when bends were not re-annealed.

Export packing can be bare bundles, wrapped bundles, or wooden-cased lengths for bright-annealed, polished, or small-bore material. We ship under the Incoterms on the order acknowledgement — FOB, CFR, CIF, EXW, or other agreed terms. Inland trucking, bilingual destination marks, or project color coding for bundle tags should be stated on the enquiry beside the metallurgical notes.

Why Choose SHH STEEL

SHH STEEL treats ASTM A213 TP202 as a product standard with enforceable chemistry, tensile, hardness, heat-treatment, and marking rules — not as a catalogue nickname for “any 202 tube.” The MTC reports the full ladle chemistry and the Table 4 tensile/hardness set (90/45 ksi, 219 HBW / 95 HRB); the stencil carries seamless tube identity under A213; and dual A213/SA-213 marking is offered only when requested.

We keep the high-Mn conversation honest. If the datasheet really wants the leaner TP201 band, we open A213 TP201. If chlorides dominate, we steer toward A213 TP316 / A213 TP316L. If classic 18-8 paperwork is non-negotiable, we open A213 TP304. The A213/A213M hub is organized grade by grade under ASTM, seamless tube only.

Lead times combine near-term stock lengths with mill schedules; we say which is which on the quotation. Cut-to-length, U-bending, polish, and third-party inspection are defined extras. The tube that arrives should match the ASTM callout the engineer wrote, with paperwork a third-party inspector can read without translation.

Supply Capability

SHH STEEL can supply ASTM A213 TP202 stainless steel tube against the edition and finish route named on your enquiry. The capability table below summarizes the sizes, finishes, and documents we regularly quote for this grade, followed by the Stock / Available sizes map buyers ask for when they need a quick sense of what to enquire against.

Item SHH STEEL capability for TP202
Standard ASTM A213 / A213M (dual SA-213 marking on request) Grade TP202 / UNS S20200
Product form Seamless only — cold-finished and hot-finished
Size Typical OD × min wall (or average wall) in the A213 usual band; other diameters by agreement
Wall / gauge Minimum wall or average wall; BWG / gauge callouts accepted on enquiry
Length Cut-to-length for HX / boiler bundles; mill random by agreement; U-bends on enquiry
Finish Annealed and pickled; bright annealed or light polish by agreement
Testing Tension (90/45 ksi), hardness (max 219 HBW / 95 HRB), flattening, flaring, hydro or NDE per length; full ladle chemistry on MTC; product analysis / IGC on order
Documents EN 10204 3.1 with full ladle chemistry; third-party inspection / 3.2 on request
Trade terms FOB / CFR / CIF / EXW and other agreed Incoterms

Stock / Available sizes

SHH STEEL quotes TP202 tube against a practical stock-and-mill enquiry range rather than a frozen warehouse SKU list. The sizes below are OD × wall / BWG combinations buyers most often request for utility and process heat-exchanger tube in the high-Mn family; availability of any single line on a given week depends on mill drawing and our inbound schedule, so treat the table as a supply map for enquiry — not a guarantee of floor tonnage.

Item Typical stock / enquiry range for TP202
Outside diameter 15.88, 19.05, 25.4, 31.8, 38.1, 50.8, 63.5 mm (and other HX/boiler ODs on enquiry; up through the usual A213 ~5 in. [127 mm] band)
Wall / BWG BWG 12–18 class walls and metric min-wall equivalents; lighter and heavier walls by agreement
Common OD × wall examples 19.05 × 2.11 mm; 25.4 × 2.11 mm; 25.4 × 2.77 mm; 31.8 × 2.77 mm; 38.1 × 2.77 mm; 50.8 × 2.77 mm — illustrative HX sizes, confirm min vs average wall
Length Cut lengths for exchanger bundles; U-bends and straight random lengths on enquiry
Special Non-standard OD/wall, bright anneal, polished bore, post-bend anneal notes, and dual A213/SA-213 marking — confirm on enquiry

When you send an enquiry, list OD × wall (or BWG), wall basis (minimum or average), cold-finished or hot-finished preference, quantity or cut list, required marking (A213 alone or dual A213/SA-213), and any Supplementary Requirements. We reply with what we can ship from near-term stock versus what needs a mill run, without inventing fake warehouse codes or tonnage claims.

Send the size list, finish route, quantity or cut lengths, required marking, Supplementary Requirements, and destination on one enquiry. We will confirm chemistry, tensile, and hardness against the stainless chemistry table and Table 4, state what ships from near-term availability versus mill production, and keep the offer aligned with ASTM A213 / A213M. Related grades such as A213 TP201, A213 TP304, and A213 TP XM-19 sit on the same hub when the datasheet steps beyond TP202.

FAQ

Is ASTM A213 the same as ASME SA-213 for TP202?
No. ASTM A213 / A213M is the ASTM International product specification for seamless boiler, superheater, and heat-exchanger tubes; ASME SA-213 / SA-213M is the separate ASME Code Book adoption of that grade text. Chemistry, tensile, and hardness floors align closely for a given referenced edition, but they remain two independent standards. Dual-mark A213/SA-213 tube only when the purchase order asks for both names on the stencil and MTC.
Does ASTM A213 TP202 include welded or HCW tube?
No. ASTM A213 covers seamless tube only. There is no WLD or HCW manufacturing type under this product standard the way ASTM A312 describes pipe. The process choice for TP202 under A213 is cold-finished versus hot-finished seamless tube, plus the heat-treatment and testing clauses of the ordered edition. If you need welded stainless pipe, open the appropriate pipe product-standard family instead.
What is the UNS number and chemistry of ASTM A213 TP202?
TP202 is UNS S20200. Melting limits include carbon ≤0.15%, manganese 7.5–10.0%, phosphorus ≤0.060%, sulfur ≤0.030%, silicon ≤1.00%, chromium 17.0–19.0%, nickel 4.0–6.0%, and nitrogen ≤0.25%, with molybdenum as a no-requirement ellipsis. Product-analysis limits apply only when ordered, typically from A480 Table A1.1 via A1016. Confirm the ordered A213 edition for the exact stainless-table number.
What tensile and hardness floors does A213 Table 4 set for TP202?
Table 4 for TP202 lists 90 ksi [620 MPa] tensile strength, 45 ksi [310 MPa] yield strength, 35% elongation, and a hardness maximum of 219 HBW / 230 HV or 95 HRB. Hardness tests are part of lot acceptance under A213. The 45 ksi yield floor is higher than TP201 (38 ksi) and TP304 (30 ksi) under the same product standard — match the grade to the design, not only to a familiar "202" name.
TP202 vs TP201 — which A213 Mn–N tube should I order?
Order TP202 when the datasheet wants Mn 7.5–10.0%, Cr 17–19%, Ni 4–6%, and the 90/45 ksi Table 4 pair. Order TP201 when the specification calls for Mn 5.5–7.5%, Cr 16–18%, Ni 3.5–5.5%, and the 95/38 ksi floor. They are sister lean austenitics with different chemistry bands and different tensile rows — do not swap them on a PMI gun reading alone.
TP202 vs TP304 — when is the high-Mn grade acceptable?
TP202 can be acceptable when nickel cost drives the selection, the 45 ksi yield floor helps the wall calculation, and the fluid is oxidizing or only mildly corrosive with low chlorides. TP304 remains the default 18-8 when higher nickel, a lower carbon ceiling, and broader industry acceptance matter more. ASTM A213 does not publish a ranking table; open the TP304 tube page when the end user expects classic 18-8 paperwork.
Minimum wall vs average wall — which should I order for A213 TP202?
Order minimum wall when the design and datasheet are written around a guaranteed minimum thickness after tolerance. Order average wall only when the purchase order explicitly allows average-wall product and the designer has accepted that basis. Put the wall basis on the enquiry before the mill selects tooling and A1016 tolerance tables — the two readings produce different tube from the same OD × wall line.
What heat treatment does ASTM A213 require for TP202?
TP202 is solution treated at a minimum of 1900 °F [1040 °C] and then water quenched or rapidly cooled to prevent carbide reprecipitation. Both cold-finished and hot-finished seamless tube follow that heat-treatment requirement. Ask the mill to state anneal temperature and quench method on the EN 10204 3.1 certificate, and discuss post-bend re-anneal when heavy U-bends are part of the fabrication sequence.
Does high manganese make TP202 harder to bend and expand?
High-Mn austenitics work-harden faster than classic 18-8, so expander settings, bend radii, and whether bends will be re-solution-treated afterward should be stated on the enquiry. That is a fabrication reality, not a reason to skip the grade when chemistry and tensile fit. Share the bend schedule with mill and fabricator early so residual stress and dimensional recovery are planned rather than discovered at hydrotest.
Hydrostatic test vs NDE — which do I get on TP202 tube?
ASTM A213 requires each tube to be hydrostatically tested or nondestructively electrically tested. The manufacturer may choose the method unless the purchase order fixes one. Neither route is an informal upgrade over the other inside the product standard. State the preferred method on the enquiry if your end user or inspector mandates hydro only or a named NDE technique.
Can you dual-certify ASTM A213 and ASME SA-213 TP202?
Yes when the heat and testing support it. Dual A213/SA-213 marking is available when the purchase order requests both independent standards on the stencil and MTC. Spell the required marking on the enquiry so the heat is selected and documented correctly. Dual TP202/TP201 is not routine — the manganese bands do not overlap.

Conclusion

ASTM A213 TP202 / UNS S20200 is the higher-manganese Mn–N seamless stainless steel tube grade for boiler, superheater, and heat-exchanger service when a 90/45 ksi Table 4 floor and a richer Cr/Mn band than TP201 fit the duty, and when nickel cost still rules out classic 18-8. SHH STEEL supplies cold-finished and hot-finished seamless tube in the usual OD × wall / BWG band, solution annealed, tested to Table 4 tensile and hardness limits, and documented on EN 10204 3.1 certificates — with dual SA-213 marking only when the order asks for that separate ASME standard. For sister grades and stock-oriented size discussions, start from the A213/A213M hub, then send your OD × wall list, wall basis, bend notes, and marking requirements so we can align mill and near-term availability to the ASTM callout.

Contact: admin@steelspecs.com

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X