ASTM A213 TP310MoCbN Stainless Steel Tube | ASTM A213 Stainless Steel - SHH STEEL

ASTM A213 TP310MoCbN Stainless Steel Tube

ASTM A213 TP310MoCbN / UNS S31025 seamless boiler, superheater and heat-exchanger tube — Mo+Nb+N+B austenitic with C ≤0.10%, Cr 19.5–23.0%, Ni 23.0–26.0%, Mo 1.0–2.0%, N 0.10–0.25%, Nb 0.10–0.40%, Ti ≤0.20%, B 0.002–0.010%, Table 4 floors of 93/39 ksi, hardness max 256 HBW / 100 HRB, 2100 °F solution anneal, and ASTM grain size No. 7 or coarser. SHH STEEL supplies cold-finished and hot-finished seamless tube with EN 10204 3.1 MTCs.
Grade
TP310MoCbN / UNS S31025
Standard
ASTM A213 / A213M
Product form
Seamless boiler / superheater / heat-exchanger tube (cold-finished and hot-finished)
Size
Typical OD × min wall (or average wall) within ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD and ~0.015–0.500 in. [0.4–12.7 mm] wall; other diameters by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is ASTM A213 TP310MoCbN Stainless Steel Tube

ASTM A213 / A213M covers seamless ferritic and austenitic alloy-steel boiler, superheater, and heat-exchanger tubes. Grade TP310MoCbN / UNS S31025 is not a casual “310 with Mo and Nb” nickname — its chromium and nickel windows are inverted relative to classic 310S: melting chromium 19.5–23.0%, nickel 23.0–26.0%, with carbon ≤0.10%, molybdenum 1.0–2.0%, nitrogen 0.10–0.25%, niobium 0.10–0.40%, titanium ≤0.20%, boron 0.002–0.010%, manganese ≤1.50%, and ASTM grain size No. 7 or coarser after a 2100 °F [1150 °C] solution treatment. That package exists for specialized high-temperature boiler and heat-exchanger lists that name S31025 explicitly — not as a dual stamp of A213 TP310MoLN plus columbium.

SHH STEEL can supply ASTM A213 TP310MoCbN stainless steel tube as seamless cold-finished and hot-finished product in the usual boiler and heat-exchanger OD × wall / BWG band, shipped with EN 10204 3.1 mill test certificates that report the full multi-element ladle chemistry (including Nb, N, Ti, and B), Table 4 tensile and hardness, and the E112 grain-size result. Dual A213 / SA-213 marking is available only when the purchase order asks for both independent standards. Browse 310-family grades on the A213/A213M hub.

Shop names such as 310MoCbN, S31025, or “Mo-Nb-N 310-type tube” do not replace the ASTM grade on the MTC. Sister grades under the same ASTM standard include A213 TP310MoLN, A213 TP310HCbN, A213 TP310HCb, A213 TP310S, and A213 TP316H. A213 covers seamless tube only — cold-finished versus hot-finished is the process choice, not a WLD/HCW manufacturing-type letter. Note also that UNS S31035 appears as a separate chemistry row near S31025 in the public table and is not the TP310MoCbN grade.

Chemical Composition of A213 TP310MoCbN

Two chemistry layers matter for TP310MoCbN under ASTM A213. Melting analysis is mandatory for every heat; product analysis on finished tube applies only when Supplementary Requirement wording or the purchase order invokes it through ASTM A1016/A1016M, with tolerances typically from ASTM A480/A480M Table A1.1. Reviewers should check the inverted Cr–Ni windows first (19.5–23.0 / 23.0–26.0), then Mo 1.0–2.0%, N 0.10–0.25%, Nb 0.10–0.40%, Ti ≤0.20%, and B 0.002–0.010% together — missing boron or treating the grade as classic 24–26 / 19–22 310 chemistry means the heat is not TP310MoCbN. Nitrogen analysis method is a matter of agreement between purchaser and producer (Footnote B).

The tables below reproduce the melt limits for TP310MoCbN / UNS S31025, product-analysis limits from A480 Table A1.1 practice where applied, and a short snapshot against TP310MoLN and TP310HCbN. Values are maximum unless a range is shown.

Melting analysis (heat / ladle analysis)

Element TP310MoCbN (UNS S31025) melting analysis
Carbon (C) ≤ 0.10
Manganese (Mn) ≤ 1.50
Phosphorus (P) ≤ 0.030
Sulfur (S) ≤ 0.030
Silicon (Si) ≤ 1.00
Chromium (Cr) 19.5 – 23.0
Nickel (Ni) 23.0 – 26.0
Molybdenum (Mo) 1.0 – 2.0
Nitrogen (N) 0.10 – 0.25
Niobium (Nb / Cb) 0.10 – 0.40
Titanium (Ti) ≤ 0.20
Boron (B) 0.002 – 0.010

Source: ASTM A213/A213M stainless chemistry table for Grade TP310MoCbN / UNS S31025 (public mill / specification PDF excerpt — _ref_a213.txt / A213–13 table text). Confirm the ordered edition. The titanium column prints 0.20 without a range marker — treated here as a maximum of 0.20% per usual A213 max-unless-range practice; confirm on the ordered edition if a floor is also intended.

Product analysis — A480/A480M Table A1.1 tolerances applied

Element Melting Tolerance (A480 A1.1) Product analysis limit
Carbon (C) ≤ 0.10 0.01 over ≤ 0.11
Manganese (Mn) ≤ 1.50 0.04 over ≤ 1.54
Phosphorus (P) ≤ 0.030 0.005 over ≤ 0.035
Sulfur (S) ≤ 0.030 0.005 over ≤ 0.035
Silicon (Si) ≤ 1.00 0.05 over ≤ 1.05
Chromium (Cr) 19.5 – 23.0 0.25 under / over 19.25 – 23.25
Nickel (Ni) 23.0 – 26.0 0.15 under / 0.20 over 22.85 – 26.20
Molybdenum (Mo) 1.0 – 2.0 0.05 under / over 0.95 – 2.05
Nitrogen (N) 0.10 – 0.25 0.01 under / 0.02 over 0.09 – 0.27
Niobium (Nb) 0.10 – 0.40 0.05 under / over 0.05 – 0.45
Titanium (Ti) ≤ 0.20 0.05 over ≤ 0.25
Boron (B) 0.002 – 0.010 UNCERTAIN — confirm A480 path confirm ordered A480 / PO

MoCbN vs MoLN vs HCbN snapshot

Element TP310MoCbN (S31025) TP310MoLN (S31050) TP310HCbN (S31042)
C ≤ 0.10 ≤ 0.025 0.04 – 0.10
Cr / Ni 19.5–23 / 23–26 24–26 / 21–23 24–26 / 19–22
Mo 1.0 – 2.0 2.00 – 3.00 …
N 0.10 – 0.25 0.10 – 0.16 0.15 – 0.35
Nb 0.10 – 0.40 … 0.20 – 0.60
B 0.002 – 0.010 … …
Table 4 TS/YS 93 / 39 ksi 84/39 or 78/37 95 / 43 ksi

Do not collapse these three grades into one “310 Mo N” shop name. TP310MoCbN’s inverted Cr–Ni, boron band, titanium max, and 2100 °F anneal are unique among them. When L-carbon Mo 2–3% on classic-high Cr is required, stay on A213 TP310MoLN; when H-grade Nb+N on 24–26 / 19–22 is required, open A213 TP310HCbN.

When product analysis is ordered, finished tube may read C ≤0.11%, Mn ≤1.54%, P ≤0.035%, S ≤0.035%, Si ≤1.05%, Cr 19.25–23.25%, Ni 22.85–26.20%, Mo 0.95–2.05%, N 0.09–0.27%, Nb 0.05–0.45%, and Ti ≤0.25% under the A480 practice above. Boron product-analysis tolerance is left UNCERTAIN — confirm the A480 edition path if product analysis of boron is contractual. Put any tighter project floors on the purchase order before heat selection.

Mechanical Properties of A213 TP310MoCbN

ASTM A213 Table 4 sets the room-temperature tensile acceptance floor for TP310MoCbN at 93 ksi [640 MPa] tensile strength and 39 ksi [270 MPa] yield strength (0.2% offset), with elongation of 30% minimum in 2 in. or 50 mm. Hardness maximum is 256 HBW / 270 HV or 100 HRB. Those floors sit well above ordinary 310S / 310H 75/30 ksi rows and reflect the nitrogen-plus-molybdenum-plus-niobium strengthening package. ASTM grain size No. 7 or coarser is mandatory on the heat-treatment lot after the 2100 °F solution treatment.

Property TP310MoCbN requirement
Tensile strength, min (Table 4) 93 ksi [640 MPa]
Yield strength (0.2% offset), min (Table 4) 39 ksi [270 MPa]
Elongation in 2 in. or 50 mm, min (Table 4) 30%
Hardness, max (Table 4) 256 HBW / 270 HV or 100 HRB
Grain size ASTM No. 7 or coarser (per heat-treatment lot)

Source: ASTM A213/A213M Table 4 for TP310MoCbN / UNS S31025 and heat-treatment grain-size column (public specification PDF excerpt — _ref_a213.txt). Mechanical property requirements do not apply to tubing smaller than 1/8 in. [3.2 mm] ID or thinner than 0.015 in. [0.4 mm] wall. Flattening and flaring tests sit beside tension and hardness on a lot basis.

A complete TP310MoCbN release package reports tensile, hardness, the multi-element chemistry (Mo, N, Nb, Ti, B), and grain size together. Omitting boron or grain size turns an MoCbN certificate into an incomplete surrogate for a simpler 310 nickname.

Dimensions and Tolerances

Dimensional supply for ASTM A213 TP310MoCbN is tube language — OD × wall (minimum or average) and BWG / gauge — covering specialized boiler and heat-exchanger sizes rather than leading with ASME B36.19 pipe schedules. Usual A213 sizes run from about 1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD with min wall about 0.015–0.500 in. [0.4–12.7 mm]; other diameters by agreement. State wall basis on the purchase order — boiler datasheets almost always assume minimum wall.

OD and wall variations follow ASTM A1016/A1016M as invoked by A213. Cold-finished tubes commonly hold tighter OD; hot-finished tubes allow wider windows. Confirm exact rows for the OD and finish on the ordered edition.

Item Typical A213 TP310MoCbN dimensional practice
Product form Seamless only (cold-finished or hot-finished)
Usual size band ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD; wall ~0.015–0.500 in. [0.4–12.7 mm]
Wall basis Minimum wall (default for boiler / HX) or average wall when specified
OD / wall tolerances Per ASTM A1016/A1016M for finish route and size
Length Cut lengths for boiler / HX bundles; mill random by agreement
Secondary note B36.19 schedules only as a buyer cross-reference

Put cut list, design metal temperature, boron/Nb reporting expectations, and end preparation on the enquiry. Minimum wall remains first-class for MoCbN tube.

Equivalent Grades

Equivalence language around MoCbN often tries to assemble the grade from MoLN plus HCbN nicknames. ASTM A213 Grade TP310MoCbN / UNS S31025 is the governing designation for this article; UNS S31035 (printed as a separate chemistry row near S31025) is not this grade.

Designation Notes
ASTM A213 / A213M Grade TP310MoCbN Governing ASTM seamless boiler / HX tube product standard for this article
UNS S31025 Unified number in the stainless chemistry table — not S31035
ASME SA-213 TP310MoCbN Separate ASME Code Book adoption — dual-mark only when the PO asks
Related MoLN A213 TP310MoLN — L carbon, Mo 2–3, classic-high Cr, no Nb/B
Related HCbN A213 TP310HCbN — H-grade Nb+N on 24–26 / 19–22, no Mo/B
Related 310S A213 TP310S — classic 24–26 / 19–22 without Mo/Nb/N/B
Related plate A240 / SA240 flat product — order plate and tube under their own standards

Dual A213/SA-213 marking is a purchase-order option. Compare MoLN and HCbN on their own pages before assuming a mixed nickname equals TP310MoCbN on the MTC.

Heat Treatment and Delivery Condition

TP310MoCbN under ASTM A213 is furnished solution treated at a minimum of 2100 °F [1150 °C], then quenched in water or cooled rapidly by other means — a distinctly higher anneal temperature than the 1900 °F [1040 °C] used on classic 310S / 310H / HCbN rows. The heat-treatment table carries ASTM grain size No. 7 or coarser for the heat-treatment lot. That higher solution temperature belongs with the multi-element Mo–Nb–N–B chemistry and should appear on the mill certificate.

Cold-finished versus hot-finished is a process and dimensional route, not a substitute for the 2100 °F anneal or the grain-size check. Delivery condition for SHH STEEL TP310MoCbN is solution annealed and pickled (or bright annealed by agreement), with anneal temperature, quench method, full multi-element chemistry, and E112 grain-size result on the EN 10204 3.1 certificate.

Do not apply a 1900 °F classic-310 anneal and call the product TP310MoCbN. If a project datasheet asks for A262 Practice E or other Supplementary Requirements, write them onto the purchase order rather than assuming base A213 includes them automatically.

Corrosion Resistance

TP310MoCbN combines moderate molybdenum (1–2%) for aqueous corrosion contribution, niobium for stabilization, nitrogen for strength, and a nickel-rich austenitic balance (Ni above Cr) that differs from classic 25Cr–20Ni 310S oxidation framing. Selection is project-specific against the named fluid and temperature — ASTM A213 does not publish a corrosion-rate or PREN table for S31025.

Versus A213 TP310MoLN, MoCbN carries less Mo (1–2% vs 2–3%), higher carbon ceiling, Nb+Ti+B, and inverted Cr–Ni windows — they are not interchangeable chloride or urea strategies. Versus A213 TP310HCbN, MoCbN adds Mo and B but uses different Cr–Ni and a higher anneal temperature. Put A262 Practice E on the PO when demonstrated IGC performance is contractual.

Applications of A213 TP310MoCbN Tube

Buyers specify ASTM A213 TP310MoCbN when a datasheet names S31025 / TP310MoCbN for specialized boiler or heat-exchanger service that needs the inverted Cr–Ni windows, Mo+Nb+N+B chemistry, 93/39 ksi floors, and 2100 °F solution treatment together. Typical placements follow project specifications that already selected this UNS number rather than a generic “310 Mo” nickname.

Do not assemble MoCbN by dual-stamping unrelated MoLN and HCbN heats. When L-carbon Mo 2–3% on 24–26 / 21–23 is required, stay on A213 TP310MoLN. When H-grade Nb+N on classic 310 Cr–Ni is required, open A213 TP310HCbN. SHH STEEL quotes OD × wall / BWG against the full multi-element chemistry and grain-size rule on the datasheet.

Service theme Why TP310MoCbN is considered
Named S31025 boiler / HX lists Inverted Cr–Ni + Mo + Nb + N + B package
High-strength austenitic tube Table 4 93/39 ksi + grain size No. 7
Stabilized Mo-bearing 310-family duty Nb 0.10–0.40 + Ti ≤0.20 with Mo 1–2
Classic 25-20 oxidation-only duty Usually TP310S / TP310H — not MoCbN

Weldability

TP310MoCbN welds with austenitic practices using matching or near-matching Mo- and Nb-bearing fillers selected so deposit chemistry tracks the base-metal Mo, Nb, and N windows. The boron and titanium residuals also belong in procedure qualification — treat the grade as MoCbN base metal, not as generic 310S or as MoLN without niobium.

For tube-to-tubesheet and coil welding, confirm project limits on grain size, A262, and any post-weld heat-treatment restrictions given the 2100 °F solution-treatment history of the base metal. Repair welding, when permitted, follows A1016/A1016M as invoked by A213.

Surface Finishes

Standard delivery for ASTM A213 TP310MoCbN from SHH STEEL is solution annealed and pickled. Bright annealed finishes are available by agreement when process-side roughness requires them.

State finish together with OD × wall, end preparation, and chemistry reporting expectations (Nb, N, B). Grain-size and multi-element reporting on the MTC are independent of pickled versus bright surface.

Inspection and Testing

Lot testing for ASTM A213 TP310MoCbN follows tension, hardness, flattening, and flaring under A213 / A1016, plus ASTM grain-size determination (E112) for the heat-treatment lot. Chemistry verification must include Cr–Ni windows, Mo, N, Nb, Ti, and B band compliance. NDE follows the ordered edition and purchaser supplements.

EN 10204 3.1 certificates from SHH STEEL report ladle chemistry with Mo/N/Nb/Ti/B, Table 4 tensile and hardness (93/39 ksi floors), 2100 °F heat-treatment condition, and grain-size result. When A262 Practice E is ordered, those results appear as specified. Dual A213/SA-213 marking and third-party witness are available when written into the enquiry. A certificate missing boron, niobium, or grain size is not a complete TP310MoCbN release package.

Packaging and Shipping

TP310MoCbN tubes ship in capped or plugged bundles with weather protection matched to the route. Cut lengths for boiler and exchanger bundles are labeled by heat and size; export packing uses cases or steel-frame crates when required.

Marking includes ASTM A213, grade TP310MoCbN / UNS S31025, size, heat number, and SHH STEEL identification. Dual SA-213 marking appears only when the purchase order requests it. Packing lists track the same heat numbers shown on the EN 10204 3.1 certificates, including grain-size lot identity where applicable.

Why Choose SHH STEEL

SHH STEEL treats ASTM A213 TP310MoCbN as a multi-element specification product: inverted Cr–Ni windows, Mo 1–2%, N, Nb, Ti, B, Table 4 93/39 ksi floors, 2100 °F anneal, and grain size No. 7 or coarser are checked together before a heat is offered. Quotations state OD × wall / BWG, wall basis, finish route, A262 options, and whether dual A213/SA-213 marking is required.

We refuse nickname assemblies that stamp MoLN or HCbN as MoCbN without the missing chemistry and anneal controls. EN 10204 3.1 documentation includes the full element set and E112 grain size. Compare sisters on the A213/A213M hub before freezing the tube list.

Supply Capability

SHH STEEL supplies ASTM A213 TP310MoCbN seamless stainless steel tube in cold-finished and hot-finished routes across the usual boiler and heat-exchanger OD × wall / BWG band. Capability below is an enquiry range — not a frozen warehouse SKU or tonnage claim.

Capability SHH STEEL practice for TP310MoCbN
Product form Seamless cold-finished and hot-finished tube
Standards ASTM A213 / A213M; dual SA-213 when PO asks
Size band Typical within ~1/8 in. ID to 5 in. OD; other diameters by agreement
Wall basis Minimum wall or average wall as specified
Documentation EN 10204 3.1 MTC with Mo/N/Nb/Ti/B + grain-size result; A262 / third-party witness on request
Trade terms FOB / CFR / CIF / EXW and other agreed Incoterms

Stock / Available sizes

SHH STEEL quotes TP310MoCbN against a stock-and-mill enquiry range rather than a frozen SKU/tonnage list. Representative OD × wall / BWG combinations for boiler and heat-exchanger tube appear below.

Item Typical stock / enquiry range for TP310MoCbN
Outside diameter 19.05, 25.4, 31.8, 38.1, 42.4, 50.8, 60.3, 76.2 mm (and other boiler/HX ODs on enquiry; through the usual A213 ~5 in. [127 mm] band)
Wall / BWG BWG 10–18 class walls and metric min-wall equivalents; heavier walls by agreement
Common OD × wall examples 25.4 × 2.11 mm; 31.8 × 2.77 mm; 38.1 × 2.77 mm; 42.4 × 3.56 mm; 50.8 × 3.05 mm; 60.3 × 3.91 mm — illustrative, confirm min vs average wall
Length Cut lengths for boiler / exchanger bundles; bends and random mill lengths on enquiry
Special Non-standard OD/wall, bright anneal, dual A213/SA-213, A262 Practice E, full B/Nb/N reporting, third-party witness — confirm before heat reservation

Send OD × wall (or BWG), wall basis, finish route, quantity or cut list, marking (A213 or dual A213/SA-213), and A262 / chemistry-reporting notes on one enquiry. We confirm C ≤0.10%, Cr 19.5–23.0% / Ni 23.0–26.0%, Mo 1.0–2.0%, N 0.10–0.25%, Nb 0.10–0.40%, Ti ≤0.20%, B 0.002–0.010%, Table 4 93/39 ksi, 2100 °F anneal, and ASTM grain size No. 7 or coarser without inventing fake warehouse codes. Sisters A213 TP310MoLN, A213 TP310HCbN, and A213 TP310S sit on the same hub.

FAQ

Is ASTM A213 the same as ASME SA-213 for TP310MoCbN?
No. ASTM A213 / A213M is the ASTM International product specification for seamless boiler, superheater, and heat-exchanger tubes; ASME SA-213 / SA-213M is the separate ASME Code Book adoption. Dual-mark only when the purchase order asks for both names on the stencil and MTC. Chemistry, tensile floors, and grain-size rules align closely for a given referenced edition, but the standards remain independent documents.
Does ASTM A213 TP310MoCbN include welded or HCW tube?
No. ASTM A213 covers seamless boiler, superheater, and heat-exchanger tubes only. There is no WLD or HCW manufacturing-type letter under A213. Cold-finished versus hot-finished describes the seamless process route and dimensional tolerances — not a welded product form. Order welded stainless pipe under a different product standard when that form is required.
What is the chemistry of ASTM A213 TP310MoCbN?
Melting analysis for TP310MoCbN / UNS S31025 is C ≤0.10%, Mn ≤1.50%, P ≤0.030%, S ≤0.030%, Si ≤1.00%, Cr 19.5–23.0%, Ni 23.0–26.0%, Mo 1.0–2.0%, N 0.10–0.25%, Nb 0.10–0.40%, Ti ≤0.20%, and B 0.002–0.010%. Confirm the ordered A213 edition. The inverted Cr–Ni windows and boron band are mandatory — this is not classic 24–26 / 19–22 310 chemistry.
TP310MoCbN vs TP310MoLN — how do they differ?
TP310MoLN uses C ≤0.025%, Cr 24–26 / Ni 21–23, Mo 2–3%, N 0.10–0.16%, no Nb/B, and wall-dependent tensile floors. TP310MoCbN uses C ≤0.10%, inverted Cr 19.5–23 / Ni 23–26, Mo 1–2%, N 0.10–0.25%, Nb 0.10–0.40%, Ti ≤0.20%, B 0.002–0.010%, 93/39 ksi floors, and a 2100 °F anneal. They are not interchangeable nicknames.
Is UNS S31035 the same as TP310MoCbN?
No. The public A213 chemistry table prints UNS S31035 as a separate row near S31025 with its own W/Co/Cu/B chemistry and a different heat-treatment temperature range. TP310MoCbN is UNS S31025 only. Do not accept an S31035 certificate as TP310MoCbN unless the purchase order and ordered edition explicitly dual-list both — they are different designations.
Why is the solution anneal 2100 °F for TP310MoCbN?
Table 3 for TP310MoCbN / S31025 sets solution treatment at a minimum of 2100 °F [1150 °C] with water quench or other rapid cool and ASTM grain size No. 7 or coarser. That is higher than the 1900 °F used on classic 310S / 310H / HCbN rows and belongs with this multi-element chemistry. A 1900 °F anneal alone does not meet the MoCbN heat-treatment row.
Why does A213 require grain size No. 7 or coarser for TP310MoCbN?
The heat-treatment table lists ASTM grain size No. 7 or coarser for the S31025 row, determined per heat-treatment lot under E112. Together with the 2100 °F anneal and 93/39 ksi tensile floors, grain size is part of MoCbN acceptance — a tensile-and-chemistry MTC that omits E112 is incomplete for this grade.
Does Table 4 set a hardness limit for TP310MoCbN?
Yes. Table 4 lists hardness maximum 256 HBW / 270 HV or 100 HRB together with 93 ksi tensile, 39 ksi yield, and 30% elongation. Hardness, grain size, and the full Mo/N/Nb/Ti/B chemistry all belong on the release package — none replaces the others for MoCbN tube.
Minimum wall vs average wall for A213 TP310MoCbN — which should I specify?
Boiler and heat-exchanger datasheets almost always expect minimum wall. Average wall is allowed when the purchase order says so, with A1016/A1016M tolerances for that basis. State wall basis on the enquiry rather than relying on pipe schedule numbers as the primary A213 wall story.
Can I dual-certify TP310MoCbN with TP310MoLN on the same heat?
Only when one heat simultaneously clears both chemistry rows, both tensile/hardness tables, and both heat-treatment/grain-size rules — which is unlikely given inverted versus classic-high Cr–Ni windows, different Mo bands, Nb/B presence, and different anneal temperatures. Do not assume dual marking from a shop nickname or PMI gun alone.
Is boron required on every TP310MoCbN MTC?
Yes for melting analysis. The stainless chemistry table lists boron 0.002–0.010% for UNS S31025, so ladle chemistry on the EN 10204 3.1 certificate should report boron inside that band. Product-analysis tolerance for boron is edition-dependent — confirm the A480 path if product analysis of boron is contractual on the purchase order.

Conclusion

ASTM A213 TP310MoCbN / UNS S31025 is the Mo+Nb+N+B seamless stainless steel tube with inverted 19.5–23% Cr / 23–26% Ni windows for specialized boiler and heat-exchanger service that names this multi-element package explicitly. SHH STEEL supplies cold-finished and hot-finished seamless tube in the usual OD × wall / BWG band, solution annealed at 2100 °F [1150 °C], tested to Table 4 93/39 ksi and hardness limits, with Mo, N, Nb, Ti, B, and ASTM grain size No. 7 or coarser reported on EN 10204 3.1 certificates — dual SA-213 marking only when the purchase order asks.

Contact: admin@steelspecs.com

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X