ASTM A213 TP347 Stainless Steel Tube | ASTM A213 Stainless Steel - SHH STEEL

ASTM A213 TP347 Stainless Steel Tube

ASTM A213 TP347 / UNS S34700 seamless boiler, superheater and heat-exchanger tube with carbon ≤0.08%, Cr 17.0–20.0%, Ni 9.0–13.0%, niobium ≥10×C ≤1.10%, Table 4 floor 75/30 ksi, and hardness max 192 HBW / 90 HRB. SHH STEEL supplies cold-finished and hot-finished seamless tube solution treated at 1900 °F [1040 °C] with EN 10204 3.1 MTCs that report Nb against the carbon formula.
Grade
TP347 / UNS S34700
Standard
ASTM A213 / A213M
Product form
Seamless boiler / superheater / heat-exchanger tube (cold-finished and hot-finished)
Size
Typical OD × min wall (or average wall) within ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD and ~0.015–0.500 in. [0.4–12.7 mm] wall; other diameters by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is ASTM A213 TP347 Stainless Steel Tube

ASTM A213 / A213M is the ASTM International product specification for seamless ferritic and austenitic alloy-steel boiler, superheater, and heat-exchanger tubes. Grade TP347 / UNS S34700 is the niobium-stabilized (columbium-stabilized) austenitic stainless member of that stainless table: melting carbon is capped at 0.08%, chromium 17.0–20.0%, nickel 9.0–13.0%, and niobium is held at ≥10 × C and ≤1.10%. Unlike the H grades beside it, the public heat-treatment table does not print a mandatory ASTM grain-size number for TP347 — the grade’s defining line is niobium tying up carbon so chromium carbides are less likely to form at grain boundaries during sensitizing thermal cycles. Buyers who write “347 tube” still need to name A213 (or the separate ASME SA-213 adoption) on the purchase order so the mill applies Nb-formula chemistry, heat-treatment, test, and marking clauses rather than a loose shop nickname.

SHH STEEL can supply ASTM A213 TP347 stainless steel tube as seamless cold-finished and hot-finished product in the usual boiler and heat-exchanger OD × wall / BWG band, shipped with EN 10204 3.1 mill test certificates that report the full ladle chemistry (including niobium against the 10 × C formula), the Table 4 tensile and hardness results, and the anneal temperature for the heat-treatment lot. When a project also needs ASME Code Book marking, we dual-mark A213 / SA-213 on the same lengths only if the purchase order says so. Browse the grade family on the A213/A213M hub.

Commercially, TP347 tube is still called 347, S34700, or Nb/Cb-stabilized boiler tube; none of those shop names replace the ASTM grade on the MTC or stencil. Sister grades under the same ASTM standard include A213 TP347H, A213 TP347HFG, A213 TP321, A213 TP321H, and A213 TP304. A213 covers seamless tube only — no welded or HCW manufacturing type — so cold-finished versus hot-finished is the process choice, not a WLD/HCW stencil letter.

Chemical Composition of A213 TP347

Two chemistry layers matter for TP347 under ASTM A213. Melting (heat or ladle) analysis is mandatory for every heat; product analysis on finished tube applies only when Supplementary Requirement wording or the purchase order invokes it through ASTM A1016/A1016M. Product-analysis tolerances typically flow from ASTM A480/A480M Table A1.1. SHH STEEL reports actual ladle values — and product values when ordered — and does not advertise unpublished tighter catalogue windows. The line that defines the grade is niobium ≥10 × C and ≤1.10%: a heat with 0.06% carbon needs at least 0.60% Nb, while a leaner-carbon heat can clear the formula with less niobium, still capped at 1.10%. Chromium 17.0–20.0% and nickel 9.0–13.0% sit near the 18-8 family but are wider than TP304’s 18–20 / 8–11 windows and different from TP321’s 17–19 / 9–12 windows.

The tables below reproduce the heat analysis for TP347 / UNS S34700, the product-analysis limits from A480 Table A1.1 practice, and a short niobium / titanium snapshot against TP321, TP347H, and TP304L. Later A213 editions place austenitic stainless grades in Table 2 (older editions used Table 1); confirm the ordered edition on the purchase order.

Melting analysis (heat / ladle analysis)

Element TP347 (UNS S34700) melting analysis
Carbon (C) ≤ 0.08
Manganese (Mn) ≤ 2.00
Phosphorus (P) ≤ 0.045
Sulfur (S) ≤ 0.030
Silicon (Si) ≤ 1.00
Chromium (Cr) 17.0 – 20.0
Nickel (Ni) 9.0 – 13.0
Molybdenum (Mo) … (no requirement)
Nitrogen (N) … (no requirement)
Niobium (Nb / Cb) ≥ 10 × C, ≤ 1.10
Titanium (Ti) … (no requirement)

Source: ASTM A213/A213M stainless chemistry table for Grade TP347 / UNS S34700 (public mill / specification PDF excerpt — _ref_a213.txt / A213–13 table text). Confirm the ordered edition. Where ellipses appear, the ordered edition sets no requirement for that element. Older shop language still says “columbium”; modern MTCs usually print Nb.

Product analysis — A480/A480M Table A1.1 tolerances applied

Element Melting Tolerance (A480 A1.1) Product analysis limit
Carbon (C) ≤ 0.08 0.01 over ≤ 0.09
Manganese (Mn) ≤ 2.00 0.04 over ≤ 2.04
Phosphorus (P) ≤ 0.045 0.010 over ≤ 0.055
Sulfur (S) ≤ 0.030 0.005 over ≤ 0.035
Silicon (Si) ≤ 1.00 0.05 over ≤ 1.05
Chromium (Cr) 17.0 – 20.0 0.20 under / over 16.80 – 20.20
Nickel (Ni) 9.0 – 13.0 0.15 under / 0.20 over 8.85 – 13.20
Niobium (Nb) ≥ 10 × C, ≤ 1.10 0.05 over on max (Nb formula practice) max ≤ 1.15 product; min tied to heat C

Stabilizer snapshot — TP304L / TP321 / TP347 / TP347H

Element TP304L (S30403) TP321 (S32100) TP347 (S34700) TP347H (S34709)
C ≤ 0.035 ≤ 0.08 ≤ 0.08 0.04 – 0.10
Cr 18.0 – 20.0 17.0 – 19.0 17.0 – 20.0 17.0 – 19.0
Ni 8.0 – 12.0 9.0 – 12.0 9.0 – 13.0 9.0 – 13.0
Stabilizer / C path low C (no Ti/Nb) Ti ≥ 5 × (C+N), ≤ 0.70 Nb ≥ 10 × C, ≤ 1.10 Nb ≥ 8 × C, ≤ 1.10

Heats that also meet an H-grade carbon floor while clearing the TP347 carbon ceiling, the tighter H-grade Nb formula (8 × C), tensile, hardness, and grain-size paths can be dual-certified TP347/TP347H when the purchase order asks — do not assume it from a PMI gun. Dual TP347/TP321 is not a chemistry path: one grade requires niobium, the other titanium. Versus A213 TP304L, TP347 accepts higher carbon because niobium, not an L-grade carbon ceiling, is the IGC strategy.

When product analysis is ordered, finished tube may read C ≤0.09%, Mn ≤2.04%, P ≤0.055%, S ≤0.035%, Si ≤1.05%, Cr 16.80–20.20%, Ni 8.85–13.20%, and Nb max ≤1.15% with the formula minimum still tied to heat carbon. Put any tighter project niobium floor on the purchase order before the heat is selected.

Mechanical Properties of A213 TP347

ASTM A213 Table 4 sets the room-temperature tensile acceptance floor for TP347 at 75 ksi [515 MPa] tensile strength and 30 ksi [205 MPa] yield strength (0.2% offset), with elongation of 35% minimum in 2 in. or 50 mm — the same room-temperature pair as TP321 and TP304. Hardness maximum is 192 HBW / 200 HV or 90 HRB, and hardness tests are part of lot acceptance under A213. The public heat-treatment table does not print a mandatory ASTM grain-size number for TP347 (unlike TP347H’s “7” and TP347HFG’s “7–10”), so a tensile-and-hardness MTC without grain size can still be complete for non-H TP347 unless the purchase order adds a grain-size Supplementary Requirement.

Property TP347 requirement
Tensile strength, min (Table 4) 75 ksi [515 MPa]
Yield strength (0.2% offset), min (Table 4) 30 ksi [205 MPa]
Elongation in 2 in. or 50 mm, min (Table 4) 35%
Hardness, max (Table 4) 192 HBW / 200 HV or 90 HRB
Grain size No mandatory ASTM number in the public Table 3 row (confirm ordered edition)

Source: ASTM A213/A213M Table 4 for TP347 / UNS S34700 (public specification PDF excerpt — _ref_a213.txt / A213–13). Mechanical property requirements do not apply to tubing smaller than 1/8 in. [3.2 mm] inside diameter or thinner than 0.015 in. [0.4 mm] wall. Flattening and flaring tests are also required on a lot basis.

Room-temperature tensile equality with sister 18-8 grades is why buyers sometimes look for dual marking; niobium chemistry and the 1900 °F solution path are why TP347 exists as its own row. A tensile-only MTC that omits niobium is incomplete — ask for the Nb / C check on the certificate before releasing the heat to fabrication. For H-grade grain-size and carbon-floor framing open A213 TP347H.

Dimensions and Tolerances

Dimensional supply for ASTM A213 TP347 is tube language — outside diameter × wall thickness (minimum wall or average wall) and, commercially, BWG / gauge — not ASME B36.19 pipe schedules as the primary size story. The sizes usually furnished under A213 run from about 1/8 in. [3.2 mm] inside diameter to 5 in. [127 mm] outside diameter, with minimum wall from about 0.015 to 0.500 in. [0.4 to 12.7 mm]; other diameters may be furnished when all other requirements are met. State on the purchase order whether wall is minimum or average — boiler and heat-exchanger datasheets almost always assume a minimum-wall reading.

Outside-diameter and wall variations follow ASTM A1016/A1016M as invoked by A213. Cold-finished tubes commonly hold tighter OD control; hot-finished tubes allow wider OD and wall windows. Permissible variations from a specified average wall for cold-finished tube are often summarized as ±10% of the specified average wall. Confirm the exact A1016 rows for the OD and finish route on the ordered edition.

Item Typical A213 TP347 dimensional practice
Product form Seamless only (cold-finished or hot-finished)
Usual size band ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD; wall ~0.015–0.500 in. [0.4–12.7 mm] min (or average wall if PO says so)
Wall basis Minimum wall (default for boiler / HX) or average wall when specified
OD / wall tolerances Per ASTM A1016/A1016M for the finish route and size; cold-finished average wall often ±10%
Length Cut lengths for boiler / superheater / HX bundles, or mill random lengths by agreement
Secondary size note ASME B36.19 schedules may appear only when a buyer asks for a pipe-schedule cross-reference — not as the primary A213 size callout

Put the cut list and end preparation on the enquiry so mill and stock lengths can be mixed efficiently. Minimum wall is a first-class A213 concept: if the datasheet assumes average wall, say so explicitly before the heat is rolled.

Equivalent Grades

Equivalence language around TP347 tube is often looser than a stabilized-boiler purchase order can afford. ASTM A213 Grade TP347 / UNS S34700 is the governing designation for this article; EN 1.4550 / X6CrNiNb18-10 and JIS SUS347 / SUS347TB are approximate wrought names that point to similar niobium-stabilized 18-8 families but are not automatic substitutes on an A213 mill test certificate. When a datasheet says “equivalent to 347,” confirm which product standard, tensile/hardness table, niobium formula, and heat-treatment path the mill will actually certify.

Designation Notes
ASTM A213 / A213M Grade TP347 Governing ASTM seamless boiler / HX tube product standard for this article
UNS S34700 Unified number listed in the stainless chemistry table
ASME SA-213 TP347 Separate ASME Code Book adoption — dual-mark only when the PO asks
EN 1.4550 (X6CrNiNb18-10) Approximate wrought Nb-stabilized designation; order EN tube forms under the relevant EN tube specs
JIS SUS347 / SUS347TB Approximate Japanese grade / boiler-tube names; confirm the Japanese tube product standard
Related plate A240 / SA240 flat product in the same UNS family — order plate and tube under their own product standards

Dual A213/SA-213 marking is a purchase-order option, not a claim that the two standards are one document. Compare TP347H, TP321, and TP304L on their own ASTM A213 pages before swapping grades on a familiar “347” PMI reading alone.

Heat Treatment and Delivery Condition

TP347 under ASTM A213 is furnished solution treated at a minimum of 1900 °F [1040 °C], then quenched in water or cooled rapidly by other means. The public heat-treatment table marks this row with Footnotes F and H. Footnote F ties quench capability to A262 Practice E demonstrability when that test is ordered (Supplementary Requirement S4); Footnote H warns that a solution treating temperature above 1950 °F [1065 °C] may impair intergranular-corrosion resistance after subsequent sensitizing exposure, and allows a purchaser-specified lower-temperature stabilization or resolution anneal after the higher solution anneal. The public table does not print a mandatory ASTM grain-size number for TP347.

Supplementary Requirement S2 lists TP347 among grades that shall be given a stabilization heat treatment at a temperature lower than the initial solution anneal when the purchaser specifies S2 — temperature as agreed between purchaser and vendor. Supplementary Requirement S1 allows stress-relieved annealed TP347 (1500–1650 °F [815–900 °C] after roll straightening) for certain chloride stress-corrosion services when ordered. Neither S1 nor S2 is automatic with the grade stamp.

Cold-finished versus hot-finished is a process and dimensional route, not a substitute for the anneal. Delivery condition for SHH STEEL TP347 is solution annealed and pickled (or bright annealed by agreement), with anneal temperature, quench method, and niobium result on the EN 10204 3.1 certificate. For H-grade carbon and grain-size controls open A213 TP347H; for fine-grain creep framing open A213 TP347HFG.

Corrosion Resistance

TP347’s chromium-rich passive film and niobium stabilization handle many boiler, superheater, and heat-exchanger duties where sensitizing thermal cycles would otherwise deplete chromium at grain boundaries. Niobium forms preferential carbides so chromium stays available for the passive film — that is the grade’s IGC strategy, not an L-grade carbon ceiling and not a molybdenum addition for chlorides. In chloride-bearing cooling waters and many process exchangers, pitting and crevice attack become limiting, and buyers usually step to A213 TP316 / A213 TP316L or a higher-PREN grade rather than stretching Nb-stabilized 18-8 into wet corrosive service.

ASTM A213 itself does not publish a corrosion-rate table for TP347; selection remains engineering judgment against fluid, temperature, velocity, and inspection philosophy. When a specification calls for ASTM A262 Practice E, write Supplementary Requirement S4 onto the purchase order — and note that for niobium-bearing grades a stabilization heat treatment under S2 may be necessary and is permitted to meet that requirement. SHH STEEL will not market TP347 as a wet-chloride upgrade over molybdenum grades; the Nb designation is about stabilization chemistry, not about higher PREN.

Applications of A213 TP347 Tube

TP347 seamless tube under A213 is chosen for boiler, superheater, and heat-exchanger service where niobium stabilization must deliver intergranular-corrosion resistance without forcing an L-grade carbon mandate or a molybdenum addition. It is a common selection for as-welded or thermally cycled steam and process tubing when the datasheet names S34700. It is the wrong default for chloride-rich cooling water that really needs Mo, and it is not an H-grade creep row unless the PO also clears TP347H chemistry and grain size. The table below pairs typical application areas with a selection note.

Application area Typical use of TP347 tube Selection note
Boiler / steam HX Seamless A213 tube where Nb stabilization is specified Confirm Nb ≥10 × C on the MTC
Superheater (non-H datasheet) Stabilized steam tubing ordered to A213 TP347 If H-grade carbon/grain size is required, open TP347H
Process heat exchangers Seamless tube for sensitizing thermal cycles without L-grade C Prefer TP316L when chlorides dominate
Stress-relieved service (S1) TP347 ordered stress-relieved annealed for certain chloride SCC duties S1 is PO language — not automatic
Dual TP347/TP347H stock Heats that clear both chemistry and H-grade grain-size / tensile rows Ask for dual marking on the PO

For titanium stabilization open A213 TP321; for H-grade Nb open A213 TP347H / A213 TP347HFG; for low-carbon without stabilizer open A213 TP304L on the A213/A213M hub.

Weldability

TP347 tube welds with matching or near-matching niobium-bearing austenitic filler for tube-to-tubesheet joints, attachment welds, and fabrication joins. Common practice uses ER347 / E347 (or equivalent covered electrodes) under a qualified WPS so weld-metal niobium supports stabilized service; many fabricators avoid defaulting to ER308L when the base tube is Nb-stabilized and the design assumes stabilization chemistry in the joint. Heat input control, interpass limits, and post-weld cleaning remain the fabricator’s responsibility under the applicable boiler or pressure-vessel code — A213 governs the seamless tube product, not the field or shop weld procedure.

Because A213 TP347 is seamless, there is no mill longitudinal weld to radiograph the way welded pipe standards describe. Focus inspection language on tube integrity (hydro or NDE of each length), tube-to-tubesheet joint quality, niobium documentation on the base metal, and any contractual corrosion test. For tube that will enter wet as-welded service where an L-grade carbon ceiling is preferred over Nb chemistry, many owners change the base metal to A213 TP304L. Specify end preparation and surface finish on the tube PO when orbital or clean-service joins are planned.

Surface Finishes

Standard mill delivery for ASTM A213 TP347 is solution annealed and pickled, leaving a clean matte finish suitable for most boiler and heat-exchanger tube duty. Bright annealing under protective atmosphere produces a smoother reflective surface used on some clean-process lines and must be called out because it changes the heat-treatment route. Light polish or specified Ra on the bore or OD is a commercial or service-center operation on top of A213 product, not automatic with the grade stamp.

When a fouling-sensitive exchanger specification quotes an Ra maximum on the bore, put it on the tube purchase order with its own acceptance language and sampling plan. SHH STEEL stencils grade and heat treatment as standard requirements; polish, special OD grind, and passivation after fabrication remain commercial extras unless the contract says otherwise. Order end preparation together with finish so receiving inspection shares one acceptance language.

Inspection and Testing

Base ASTM A213 testing for TP347 includes heat analysis (carbon ≤0.08%, niobium meeting ≥10 × C ≤1.10%), tension tests to the Table 4 floors (75/30 ksi), hardness tests to the Table 4 maximum (192 HBW / 90 HRB), flattening and flaring tests on a lot basis, and either hydrostatic testing or nondestructive electric testing of each length. The manufacturer may choose hydro versus NDE unless the purchase order fixes the method. Marking includes the ASTM designation, grade, size, heat number, and other clause-required data. Grain-size reporting is not a mandatory Table 3 item for TP347 in the public excerpt unless the PO adds it.

Supplementary Requirements commonly added on TP347 tube orders are summarized below. Invoke them by number or clear purchase-order wording; mills will not assume product analysis, S1 stress relief, S2 stabilization, or IGC testing from a verbal “full certs” note.

Option Purpose
Product analysis Confirms chemistry on finished tube — useful when Nb sits near the 10 × C floor
S1 stress-relieved anneal 1500–1650 °F [815–900 °C] after roll straightening for certain chloride SCC duties
S2 stabilizing heat treatment Lower-temperature stabilization after the solution anneal — listed for TP347 when specified
S4 intergranular corrosion A262 Practice E; S2 may be necessary for Nb-bearing grades to meet S4
Minimum vs average wall States which wall basis the size callout uses
Fixed hydro or NDE method Removes manufacturer’s option when the end user mandates one route
Third-party inspection / EN 10204 3.2 Witnessed testing and certificate when the project requires it

Ask the mill to state lot identity clearly on the certificate so hardness, tension, and niobium specimens map cleanly to the bundle you receive.

Packaging and Shipping

TP347 tube leaves SHH STEEL bundled, capped or end-protected, and tagged for export or domestic delivery according to the length mix and bend form on the order. Bundle tags repeat the ASTM A213 grade, OD × wall (or BWG), heat number, and PO reference so site receiving can check the shipment without opening every certificate packet first. U-bent tubes need extra cradle or case protection so bend radii and legs are not distorted in transit.

Export packing can be bare bundles, wrapped bundles, or wooden-cased lengths for bright-annealed, polished, or small-bore material. We ship under the Incoterms on the order acknowledgement — FOB, CFR, CIF, EXW, or other agreed terms. Inland trucking, bilingual destination marks, or project color coding for bundle tags should be stated on the enquiry beside the metallurgical notes.

Why Choose SHH STEEL

SHH STEEL treats ASTM A213 TP347 as a product standard with enforceable chemistry (niobium formula), tensile, hardness, heat-treatment, and marking rules — not as a catalogue nickname for “any 347 tube.” The MTC reports the full ladle chemistry including niobium against 10 × C, the Table 4 tensile/hardness set (75/30 ksi, 192 HBW / 90 HRB), and the anneal temperature; the stencil carries seamless tube identity under A213; and dual A213/SA-213 marking is offered only when requested.

We keep the Nb-stabilized conversation honest for boiler and HX duty. If H-grade carbon and grain size are required, we open A213 TP347H. If fine-grain creep framing is specified, we open A213 TP347HFG. If titanium is preferred over niobium, we open A213 TP321 / A213 TP321H. If chlorides dominate, we open A213 TP316L. The A213/A213M hub is organized grade by grade under ASTM, seamless tube only.

Lead times combine near-term stock lengths with mill schedules; we say which is which on the quotation. Cut-to-length, U-bending, polish, and third-party inspection are defined extras. The tube that arrives should match the ASTM callout the engineer wrote, with paperwork a third-party inspector can read without translation.

Supply Capability

SHH STEEL can supply ASTM A213 TP347 stainless steel tube against the edition and finish route named on your enquiry. The capability table below summarizes the sizes, finishes, and documents we regularly quote for this grade, followed by the Stock / Available sizes map buyers ask for when they need a quick sense of what to enquire against for Nb-stabilized boiler and heat-exchanger duty.

Item SHH STEEL capability for TP347
Standard ASTM A213 / A213M (dual SA-213 marking on request) Grade TP347 / UNS S34700
Product form Seamless only — cold-finished and hot-finished
Size Typical OD × min wall (or average wall) in the A213 usual band; other diameters by agreement
Wall / gauge Minimum wall or average wall; BWG / gauge callouts accepted on enquiry
Length Cut-to-length for boiler / superheater / HX bundles; mill random by agreement; U-bends on enquiry
Finish Annealed and pickled; bright annealed or light polish by agreement
Testing Tension (75/30 ksi), hardness (max 192 HBW / 90 HRB), Nb vs 10×C, flattening, flaring, hydro or NDE per length; full ladle chemistry on MTC; product analysis / S1 / S2 / S4 on order
Documents EN 10204 3.1 with full ladle chemistry and Nb result; third-party inspection / 3.2 on request
Trade terms FOB / CFR / CIF / EXW and other agreed Incoterms

Stock / Available sizes

SHH STEEL quotes TP347 tube against a practical stock-and-mill enquiry range rather than a frozen warehouse SKU list. The sizes below are OD × wall / BWG combinations buyers most often request for Nb-stabilized boiler and heat-exchanger tube; availability of any single line on a given week depends on mill drawing and our inbound schedule, so treat the table as a supply map for enquiry — not a guarantee of floor tonnage.

Item Typical stock / enquiry range for TP347
Outside diameter 19.05, 25.4, 31.8, 38.1, 44.5, 50.8, 63.5, 76.2 mm (and other boiler/HX ODs on enquiry; up through the usual A213 ~5 in. [127 mm] band)
Wall / BWG BWG 12–18 class walls and metric min-wall equivalents; heavier walls for high-pressure duty by agreement
Common OD × wall examples 25.4 × 2.11 mm; 31.8 × 2.41 mm; 38.1 × 2.77 mm; 50.8 × 2.77 mm; 50.8 × 3.05 mm; 63.5 × 3.05 mm — illustrative HX/boiler sizes, confirm min vs average wall
Length Cut lengths for boiler / exchanger bundles; U-bends and straight random lengths on enquiry
Special Non-standard OD/wall, bright anneal, S1 stress relief, S2 stabilization, dual TP347/TP347H marking, dual A213/SA-213 marking — confirm on enquiry before the heat is reserved

When you send an enquiry, list OD × wall (or BWG), wall basis (minimum or average), cold-finished or hot-finished preference, quantity or cut list, required marking (A213 alone, dual A213/SA-213, and/or dual TP347/TP347H), and any Supplementary Requirements (S1, S2, S4, product analysis). We reply with what we can ship from near-term stock versus what needs a mill run, without inventing fake warehouse codes or tonnage claims.

Send the size list, finish route, quantity or cut lengths, required marking, Supplementary Requirements, and destination on one enquiry. We will confirm chemistry (including the Nb formula), tensile, and hardness against the stainless chemistry table and Table 4, state what ships from near-term availability versus mill production, and keep the offer aligned with ASTM A213 / A213M. Related grades such as A213 TP347H, A213 TP321, and A213 TP304L sit on the same hub when the datasheet steps beyond TP347.

FAQ

Is ASTM A213 the same as ASME SA-213 for TP347?
No. ASTM A213 / A213M is the ASTM International product specification for seamless boiler, superheater, and heat-exchanger tubes; ASME SA-213 / SA-213M is the separate ASME Code Book adoption of that grade text. Chemistry, tensile, hardness, and niobium-formula rules align closely for a given referenced edition, but they remain two independent standards. Dual-mark A213/SA-213 tube only when the purchase order asks for both names on the stencil and MTC.
Does ASTM A213 TP347 include welded or HCW tube?
No. ASTM A213 covers seamless tube only. There is no WLD or HCW manufacturing type under this product standard the way ASTM A312 describes pipe. The process choice for TP347 under A213 is cold-finished versus hot-finished seamless tube, plus the Nb-formula chemistry, heat-treatment, and testing clauses of the ordered edition.
What is the UNS number and chemistry of ASTM A213 TP347?
TP347 is UNS S34700. Melting limits include carbon ≤0.08%, manganese ≤2.00%, phosphorus ≤0.045%, sulfur ≤0.030%, silicon ≤1.00%, chromium 17.0–20.0%, nickel 9.0–13.0%, and niobium ≥10 × C ≤1.10%, with molybdenum, nitrogen, and titanium as no-requirement ellipses. Product-analysis limits apply only when ordered, typically from A480 Table A1.1 via A1016. Confirm the ordered A213 edition for the exact stainless-table number.
TP347 vs TP321 — niobium or titanium stabilization?
Both are stabilized austenitics with carbon ≤0.08% and no mandatory Table 3 grain-size number in the public excerpt. TP347 uses niobium ≥10 × C ≤1.10% with Cr 17–20% / Ni 9–13%; TP321 uses titanium ≥5 × (C + N) ≤0.70% with Cr 17–19% / Ni 9–12%. Filler metal (ER347 vs ER321), high-temperature preference, and end-user standards often decide; do not swap them on a familiar "stabilized" PMI reading without checking the datasheet’s stabilizer.
TP347 vs TP347H — when do I need the H grade?
Order TP347H when the boiler or superheater datasheet needs H-grade carbon 0.04–0.10%, niobium ≥8 × C ≤1.10%, ASTM grain size No. 7 or coarser, and the finish-route solution temperatures written for the H row. Order TP347 when Nb ≥10 × C with C ≤0.08% and the 1900 °F solution path are enough without H-grade grain-size framing. They share a family but are not synonym stamps on the MTC.
What do Footnotes F and H mean for TP347 heat treatment?
Footnote F ties the quench rate to A262 Practice E capability when that test is ordered under Supplementary Requirement S4. Footnote H warns that solution treating above 1950 °F [1065 °C] may impair intergranular-corrosion resistance after later sensitizing exposure, and allows a purchaser-specified lower-temperature stabilization or resolution anneal after the higher solution anneal. Neither footnote makes S2 or S4 automatic — write those Supplementary Requirements on the PO when needed.
What is Supplementary Requirement S2 for TP347?
S2 requires a stabilization heat treatment at a temperature lower than the initial solution anneal, with the temperature agreed between purchaser and vendor. The public A213–13 excerpt lists TP347 among grades that shall receive S2 when specified. For niobium-bearing grades, S2 may also be necessary and is permitted to meet Supplementary Requirement S4 (A262 Practice E). S2 is never automatic with the grade stamp alone.
What is Supplementary Requirement S1 for TP347?
S1 allows TP347 (along with TP304L, TP316L, TP321, and TP348) to be ordered in the stress-relieved annealed condition at 1500–1650 °F [815–900 °C] after roll straightening for certain chloride stress-corrosion services. No mechanical straightening is permitted after that treatment. S1 is purchase-order language — mills will not assume stress-relieved delivery from a verbal note about chlorides.
Does Table 4 set a hardness limit for TP347?
Yes. Table 4 for TP347 lists tensile strength, yield strength, elongation, and a hardness maximum of 192 HBW / 200 HV or 90 HRB. Hardness tests are part of lot acceptance under A213, which differs from many A312 pipe rows for the same UNS number that omit a Table 4 hardness cap. Ask the mill to report hardness beside the tensile results on the EN 10204 3.1 certificate.
Minimum wall vs average wall for A213 TP347 — which should I specify?
Order minimum wall when the boiler or heat-exchanger datasheet is written around a guaranteed minimum thickness after tolerance — the usual practice for A213 tube. Order average wall only when the purchase order explicitly allows average-wall product and the designer has accepted that basis. Put the wall basis on the enquiry before the mill selects A1016 tolerance tables.
Can I dual-certify TP347 with TP347H on the same heat?
Yes when ladle carbon meets the H-grade 0.04–0.10% band while also clearing the TP347 ≤0.08% ceiling, when niobium clears both the 10 × C and 8 × C floors for the heat’s carbon, and when tensile, hardness, and (for the H path) grain-size results clear both acceptance paths. Spell the required dual marking and heat-treatment route on the enquiry before the heat is selected.
Is TP347 a good choice for chloride-rich cooling water?
Usually no as a first choice. Niobium helps intergranular corrosion resistance but does not raise PREN the way molybdenum does. Prefer TP316L or a higher-Mo grade when chlorides dominate aqueous service; reserve TP347 for stabilized boiler and heat-exchanger framing where the Nb formula earns its keep. S1 stress-relieved delivery can help certain chloride SCC cases but does not replace Mo for pitting.

Conclusion

ASTM A213 TP347 / UNS S34700 is the niobium-stabilized seamless stainless steel tube grade for boiler, superheater, and heat-exchanger service when Nb ≥10 × C ≤1.10% with Cr 17–20% / Ni 9–13% and C ≤0.08% must deliver IGC resistance without an L-grade carbon mandate or a molybdenum addition. SHH STEEL supplies cold-finished and hot-finished seamless tube in the usual OD × wall / BWG band, solution annealed at 1900 °F [1040 °C], tested to Table 4 tensile and hardness limits with niobium reported, and documented on EN 10204 3.1 certificates — with dual SA-213 marking only when the order asks for that separate ASME standard. For sister grades and stock-oriented size discussions, start from the A213/A213M hub, then send your OD × wall list, wall basis, dual-marking needs, and S1 / S2 / Nb requirements so we can align mill and near-term availability to the ASTM callout.

Contact: admin@steelspecs.com

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response