Product Showcase
ASME SA 312/SA 312M Stainless Steel Products
SHH STEEL offers ASME SA 312/SA 312M-compliant 304/316 stainless steel pipes. ASME SA312/SA312M specifies seamless, welded, and heavily cold-worked austenitic stainless steel pipes for high-temperature and corrosive environments. Certified quality, competitive prices, customizable. Trust SHH STEEL!
-
ASME SA312 UNS S35315 Stainless Steel Pipe | SA 312/SA 312M
ASME SA312 UNS S35315 (no TP) Si–N–Ce stainless steel pipe in SML, WLD and HCW, with Si 1.20–2.00%, N 0.12–0.18%, Ce 0.03–0.08%, welded 94/39 / seamless 87/38 ksi Table 4 floors and a 2010 °F anneal, supplied by SHH STEEL with EN 10204 3.1 MTCs.View More -
ASME SA312 UNS S35045 Stainless Steel Pipe | SA 312/SA 312M
ASME SA312 UNS S35045 (no TP) high-Cr/Ni Ti+Al stainless steel pipe in SML, WLD and HCW, with Cr 25–29%, Ni 32–37%, Ti/Al 0.15–0.60%, a 70/25 ksi Table 4 floor and a 1900 °F default anneal, supplied by SHH STEEL with EN 10204 3.1 MTCs.View More -
ASME SA312 TP348H Stainless Steel Pipe | SA 312/SA 312M
ASME SA312 TP348H (UNS S34809) H-grade Nb+Ta stainless steel pipe to SA-312/SA-312M (ASTM A312/A312M), supplied by SHH STEEL in SML, WLD and HCW routes with C 0.04–0.10%, Nb ≥8×C, Ta ≤0.10%, grain size No. 7 or coarser, 75/30 ksi Table 4 minima and EN 10204 3.1 MTCs.View More -
ASME SA312 TP348 Stainless Steel Pipe | SA 312/SA 312M
ASME SA312 TP348 (UNS S34800) Nb-stabilized stainless steel pipe with Ta ≤0.10% to SA-312/SA-312M (ASTM A312/A312M), supplied by SHH STEEL in SML, WLD and HCW routes with footnote G Nb ≥10×C, 75/30 ksi Table 4 minima and EN 10204 3.1 MTCs.View More -
ASME SA312 TP347LN Stainless Steel Pipe | SA 312/SA 312M
ASME SA312 TP347LN (UNS S34751) stainless steel pipe under SA-312/SA-312M (ASTM A312/A312M): seamless (SML), welded (WLD) and heavily cold-worked (HCW); C 0.005–0.020%, N 0.06–0.10%, Nb 0.20–0.50% (≥15×C); Table 4 minima 75/30 ksi; solution annealed. SHH STEEL supplies with EN 10204 3.1 MTCs.View More -
ASME SA312 TP347H Stainless Steel Pipe | SA 312/SA 312M
ASME SA312 TP347H (UNS S34709) Nb-stabilized stainless steel pipe to SA-312/SA-312M (ASTM A312/A312M), supplied by SHH STEEL in SML, WLD and HCW routes with Nb ≥8×C and ≤1.0% (footnote H), 75/30 ksi Table 4 minima, No. 7 or coarser grain size and EN 10204 3.1 MTCs.View More -
ASME SA312 TP347 Stainless Steel Pipe | SA 312/SA 312M
ASME SA312 TP347 (UNS S34700) Nb-stabilized stainless steel pipe to SA-312/SA-312M (ASTM A312/A312M), supplied by SHH STEEL in SML, WLD and HCW routes with Nb ≥10×C and ≤1.00% (footnote G), 75/30 ksi Table 4 minima and EN 10204 3.1 MTCs.View More -
ASME SA312 TP321H Stainless Steel Pipe | SA 312/SA 312M
ASME SA312 TP321H (UNS S32109) Ti-stabilized stainless steel pipe to SA-312/SA-312M (ASTM A312/A312M), supplied by SHH STEEL in SML, WLD and HCW routes with Ti 4×(C+N) min, 0.70% max, route- and wall-dependent 75/30 or 70/25 ksi Table 4 minima, No. 7 or coarser grain size and EN 10204 3.1 MTCs.View More -
ASME SA312 TP321 Stainless Steel Pipe | SA 312/SA 312M
ASME SA312 TP321 (UNS S32100) Ti-stabilized stainless steel pipe to SA-312/SA-312M (ASTM A312/A312M), supplied by SHH STEEL in SML, WLD and HCW routes with Ti 5×(C+N) min, 0.70% max (footnote F), route- and wall-dependent 75/30 or 70/25 ksi Table 4 minima and EN 10204 3.1 MTCs.View More -
ASME SA312 UNS S32053 Stainless Steel Pipe | SA 312/SA 312M
ASME SA312 UNS S32053 stainless steel pipe under SA-312/SA-312M (ASTM A312/A312M), no TP designation: SML, WLD, and HCW routes with Cr 22.0–24.0%, Ni 24.0–26.0%, Mo 5.0–6.0%, and N 0.17–0.22%, 93/43 ksi minimums, and solution anneal at 1975–2155 °F [1080–1180 °C], supplied by SHH STEEL with EN 10204 3.1 MTCs.View More -
ASME SA312 UNS S31730 Stainless Steel Pipe | SA 312/SA 312M
ASME SA312 UNS S31730 stainless steel pipe under SA-312/SA-312M (ASTM A312/A312M), no TP designation: SML, WLD, and HCW routes with Cu 4.0–5.0%, Mo 3.0–4.0%, N ≤0.045%, and S ≤0.010%, 70/25 ksi minimums, and solution anneal at 1900 °F [1040 °C] minimum, supplied by SHH STEEL with EN 10204 3.1 MTCs.View More -
ASME SA312 UNS S31727 Stainless Steel Pipe | SA 312/SA 312M
ASME SA312 UNS S31727 stainless steel pipe under SA-312/SA-312M (ASTM A312/A312M), no TP designation: SML, WLD, and HCW routes with Cu 2.8–4.0%, Mo 3.8–4.5%, N 0.15–0.21%, and Mn ≤1.00%, 80/36 ksi minimums, and solution anneal at 1975–2155 °F [1080–1180 °C], supplied by SHH STEEL with EN 10204 3.1 MTCs.View More
ASME SA 312/SA 312M Stainless Steel Products
Stainless Steel Pipes and Tubes
SHH STEEL, a premier Stainless Steel Pipes and Tubes exporter, produces and exports stainless steel pipes and tubes for chemical, marine, and food processing industries. Our seamless and welded products, like 304 and 316L (ASTM A312), ensure corrosion resistance and strength. With a 5,000-ton inventory, we deliver in 3–5 days, backed by SGS/TUV inspections and mill certificates. Choose SHH STEEL for seamless stainless steel pipes and custom solutions.
Stainless Steel Pipes and Tubes
X