ASTM A213 TP309S Stainless Steel Tube | ASTM A213 Stainless Steel - SHH STEEL

ASTM A213 TP309S Stainless Steel Tube

ASTM A213 TP309S / UNS S30908 seamless boiler, superheater and heat-exchanger tube — a 22–24% Cr / 12–15% Ni austenitic with C ≤0.08%, Table 4 floors of 75/30 ksi, hardness max 192 HBW / 90 HRB, and a 1900 °F solution anneal. Chosen for high-temperature oxidation resistance rather than molybdenum chloride framing. SHH STEEL supplies cold-finished and hot-finished seamless tube with EN 10204 3.1 MTCs.
Grade
TP309S / UNS S30908
Standard
ASTM A213 / A213M
Product form
Seamless boiler / superheater / heat-exchanger tube (cold-finished and hot-finished)
Size
Typical OD × min wall (or average wall) within ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD and ~0.015–0.500 in. [0.4–12.7 mm] wall; other diameters by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is ASTM A213 TP309S Stainless Steel Tube

ASTM A213 / A213M covers seamless ferritic and austenitic alloy-steel boiler, superheater, and heat-exchanger tubes. Grade TP309S is the low-carbon-ceiling (C ≤0.08%) 22–24% chromium / 12–15% nickel austenitic listed under UNS S30908 — a step up in chromium and nickel from the 18-8 TP304 family, aimed at high-temperature oxidation and furnace-atmosphere resistance rather than molybdenum-driven chloride pitting. Table 4 keeps a familiar 75 ksi [515 MPa] / 30 ksi [205 MPa] tensile pair with hardness max 192 HBW / 200 HV or 90 HRB and 35% elongation. Buyers who write “309S tube” or “309 HX tube” still need the A213 (or separate ASME SA-213) callout so wall basis, hardness, and marking clauses are contractual.

SHH STEEL can supply ASTM A213 TP309S stainless steel tube as seamless cold-finished and hot-finished product in the usual boiler, furnace, and heat-exchanger OD × wall / BWG band, shipped with EN 10204 3.1 mill test certificates that report the full stainless-table ladle chemistry and the Table 4 tensile/hardness set. Dual A213 / SA-213 marking is available only when the purchase order asks for both independent standards. Browse 309/310 family grades on the A213/A213M hub.

Shop names such as 309S, S30908, or “25-12 style” shorthand do not replace the ASTM grade on the MTC — and 309S is not chemically identical to every historical “Type 309” plate heat. Sister grades under the same ASTM standard include A213 TP309H, A213 TP309Cb, A213 TP310S, A213 TP304, and A213 TP316. A213 covers seamless tube only — cold-finished versus hot-finished is the process choice, not a WLD/HCW manufacturing-type letter.

Chemical Composition of A213 TP309S

Two chemistry layers matter for TP309S under ASTM A213. Melting analysis is mandatory for every heat; product analysis on finished tube applies only when Supplementary Requirement wording or the purchase order invokes it through ASTM A1016/A1016M, with tolerances typically from ASTM A480/A480M Table A1.1. The “S” in TP309S marks the ≤0.08% carbon ceiling relative to older high-carbon 309 compositions — it is not an L-grade ≤0.035% story, and it is not an H-grade carbon floor.

The tables below reproduce the melt limits for TP309S / UNS S30908 and the product-analysis limits from A480 Table A1.1. Values are maximum unless a range is shown; ellipsis (…) means no requirement.

Melting analysis (heat / ladle analysis)

Element TP309S (UNS S30908) melting analysis
Carbon (C) ≤ 0.08
Manganese (Mn) ≤ 2.00
Phosphorus (P) ≤ 0.045
Sulfur (S) ≤ 0.030
Silicon (Si) ≤ 1.00
Chromium (Cr) 22.0 – 24.0
Nickel (Ni) 12.0 – 15.0
Molybdenum (Mo) … (no requirement)
Nitrogen (N) … (no requirement)

Source: ASTM A213/A213M stainless chemistry table for Grade TP309S / UNS S30908 (public mill / specification PDF excerpt). Confirm the ordered edition on the purchase order. Chromium 22–24% and nickel 12–15% are the oxidation-resistance story; molybdenum and nitrogen are no-requirement ellipses under this row.

Product analysis — A480/A480M Table A1.1 tolerances applied

Element Melting Tolerance (A480 A1.1) Product analysis limit
Carbon (C) ≤ 0.08 0.01 over ≤ 0.09
Manganese (Mn) ≤ 2.00 0.04 over ≤ 2.04
Phosphorus (P) ≤ 0.045 0.010 over ≤ 0.055
Sulfur (S) ≤ 0.030 0.005 over ≤ 0.035
Silicon (Si) ≤ 1.00 0.05 over ≤ 1.05
Chromium (Cr) 22.0 – 24.0 0.25 under / over 21.75 – 24.25
Nickel (Ni) 12.0 – 15.0 0.15 under / over 11.85 – 15.15

Read chromium and nickel first: the jump from 18-8 to 22–24 / 12–15 is why TP309S is selected for hot gas, radiant, and furnace-adjacent tube duty where scale resistance matters. Carbon ≤0.08% is the S-grade ceiling — for controlled carbon floor plus grain-size language open A213 TP309H; for niobium stabilization open A213 TP309Cb. When even higher Cr–Ni is required, step to A213 TP310S.

When product analysis is ordered, finished tube may read up to C 0.09%, Mn 2.04%, P 0.055%, S 0.035%, and Si 1.05%, with Cr 21.75–24.25% and Ni 11.85–15.15%. Those are the only product limits we quote from the A480 A1.1 path for this grade. Put any tighter project carbon or sulfur ceiling on the purchase order before the heat is selected.

Mechanical Properties of A213 TP309S

ASTM A213 Table 4 sets the tensile acceptance floor for TP309S at 75 ksi [515 MPa] tensile strength and 30 ksi [205 MPa] yield strength (0.2% offset), with elongation of 35% minimum in 2 in. or 50 mm and hardness max 192 HBW / 200 HV or 90 HRB — the same room-temperature pair used for TP304 / TP304H under Table 4. The grade’s differentiation is chemistry and oxidation framing, not a unique tensile number.

Property TP309S requirement (Table 4)
Tensile strength, min 75 ksi [515 MPa]
Yield strength (0.2% offset), min 30 ksi [205 MPa]
Elongation in 2 in. or 50 mm, min 35%
Hardness, max 192 HBW / 200 HV or 90 HRB

Source: ASTM A213/A213M Table 4 for TP309S / UNS S30908 (public specification PDF excerpt / Peninsular mechanical summary cross-check). Mechanical property requirements do not apply to tubing smaller than 1/8 in. [3.2 mm] ID or thinner than 0.015 in. [0.4 mm] wall. Flattening and flaring tests sit beside tension and hardness on a lot basis.

Design calculations should use Table 4 unless the PO states higher guaranteed values the mill has accepted in writing. For creep-critical H-grade carbon and grain-size controls under the 309 family, open A213 TP309H rather than stretching standard TP309S beyond its intended framing.

Dimensions and Tolerances

Dimensional supply for ASTM A213 TP309S is tube language — OD × wall (minimum or average) and BWG / gauge — covering boiler, furnace, and heat-exchanger sizes rather than leading with ASME B36.19 pipe schedules. Usual A213 sizes run from about 1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD with min wall about 0.015–0.500 in. [0.4–12.7 mm]; other diameters by agreement. State wall basis on the purchase order.

OD and wall variations follow ASTM A1016/A1016M as invoked by A213. Cold-finished tubes commonly hold tighter OD; hot-finished tubes allow wider windows. Cold-finished average wall is often summarized as ±10% of specified average wall; minimum-wall product follows A1016 minimum-wall tables. Confirm exact rows for the OD and finish on the ordered edition.

Item Typical A213 TP309S dimensional practice
Product form Seamless only (cold-finished or hot-finished)
Usual size band ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD; wall ~0.015–0.500 in. [0.4–12.7 mm]
Wall basis Minimum wall (default) or average wall when specified
OD / wall tolerances Per ASTM A1016/A1016M for finish route and size
Length Cut lengths for furnace / HX / boiler bundles; mill random by agreement
Secondary note B36.19 schedules only as a buyer cross-reference

Put cut list, bend form, and end preparation on the enquiry. Minimum wall remains a first-class A213 concept for 309S the same way it does for 304-family tube.

Equivalent Grades

Equivalence language around 309S tube often collapses plate, cast, and tube product forms into one nickname. ASTM A213 Grade TP309S / UNS S30908 is the governing designation for this article; EN 1.4833 / X12CrNi23-13 and JIS SUS309S are approximate wrought names that point to similar chemistry families but are not automatic substitutes on an A213 MTC.

Designation Notes
ASTM A213 / A213M Grade TP309S Governing ASTM seamless boiler / HX tube product standard for this article
UNS S30908 Unified number in the stainless chemistry table
ASME SA-213 TP309S Separate ASME Code Book adoption — dual-mark only when the PO asks
EN 1.4833 (approx.) Approximate wrought designation; order EN tube under the relevant EN tube specs
JIS SUS309S (approx.) Approximate Japanese grade name; confirm the Japanese tube product standard
Related plate A240 / SA240 flat product in the 309S family — order plate and tube under their own standards

Dual A213/SA-213 marking is a purchase-order option. Compare TP309H, TP309Cb, and TP310S on their own ASTM A213 pages before swapping 309-family grades inside a furnace or boiler tube list.

Heat Treatment and Delivery Condition

TP309S under ASTM A213 is furnished solution treated at a minimum of 1900 °F [1040 °C], then quenched in water or cooled rapidly by other means. That Table 3 heat-treatment row applies to both cold-finished and hot-finished seamless tube. High chromium–nickel austenitics still need a thorough solution treatment so carbides and unwanted phases do not leave the tube in a condition that undercuts oxidation or corrosion performance in service.

Cold-finished versus hot-finished is a process and dimensional route, not a substitute for the anneal. Delivery condition for SHH STEEL TP309S is solution annealed and pickled (or bright annealed by agreement), with anneal temperature and quench method on the EN 10204 3.1 certificate. Straightening, cutting, and end finishing follow heat treatment.

H-grade grain-size rules belong to A213 TP309H (ASTM No. 7 or coarser in the public Table 3 excerpt), not to standard TP309S. When niobium stabilization is specified, open A213 TP309Cb rather than assuming S-grade chemistry covers Cb requirements.

Corrosion Resistance

TP309S is selected primarily for resistance to high-temperature oxidation and scaling in hot air, combustion, and furnace atmospheres where the higher chromium and nickel contents outperform 18-8 grades. It is not a molybdenum grade: in aqueous chloride pitting and crevice service, A213 TP316 / A213 TP316L remain the usual step-ups, and higher-Mo or superaustenitic grades go further.

Sulfur-bearing and reducing hot gases can still attack 309-family alloys; selection remains engineering judgment against atmosphere, temperature, and cyclic duty. ASTM A213 does not publish a corrosion-rate or oxidation-rate table for TP309S. When a project invokes a specific oxidation or IGC test, write that Supplementary Requirement onto the purchase order.

Applications of A213 TP309S Tube

TP309S shows up wherever seamless tube must survive hotter oxidizing environments than 18-8 is trusted for — furnace tubes, radiant sections, heat-recovery exchangers on hot gas, and some boiler/superheater locations where oxidation rather than creep-H design dominates the grade choice.

Application area Typical use of TP309S tube Selection note
Furnace / radiant tubes Seamless tube in oxidizing furnace atmospheres Confirm peak metal temperature and atmosphere chemistry
Heat-recovery / hot-gas HX Tube-side or shell-side circuits with hot oxidizing gas Step to TP310S if higher Cr–Ni is specified
Boiler / superheater (oxidation-led) Where 309S oxidation framing is accepted without H-grade carbon/grain-size Open TP309H when H-grade rules apply
Thermocouple / protection-style tube duty High-temp sensor and protection tubing ordered to A213 Confirm size and wall basis on enquiry
Aqueous chloride HX Usually not the first 309S use case Prefer Mo grades (TP316/TP316L)

Stay on the A213/A213M hub for 309H, 309Cb, and 310S sisters rather than mixing A312 pipe certificates into tube acceptance.

Weldability

TP309S tube welds with matching or near-matching 309/309L austenitic filler for tube-to-tubesheet, attachment, and fabrication joins under a qualified WPS. ER309 / ER309L (or equivalent covered electrodes) are common; fabricators sometimes use 309L deposits for lower carbon in the weld metal even when the base tube is TP309S. Heat input, interpass, and cleaning remain the fabricator’s code responsibility — A213 governs the seamless tube product, not the field weld procedure.

Because A213 TP309S is seamless, there is no mill longitudinal weld to radiograph as welded-pipe standards describe. Focus inspection on each-length hydro or NDE, joint quality, and any contractual oxidation or IGC tests. When H-grade carbon and grain-size controls are required in the base metal, change the tube grade to A213 TP309H rather than trying to weld-procedure a standard S grade into an H-grade datasheet.

Surface Finishes

Standard mill delivery for ASTM A213 TP309S is solution annealed and pickled. Bright annealing is a called-out route when a smoother reflective surface is needed. Specified Ra, light polish, and post-fabrication passivation are commercial extras on top of the A213 stamp.

Furnace and hot-gas tube often ships with a workmanlike pickled finish; cosmetic polish is uncommon unless the PO asks. End preparation for welding or expanding should be ordered with finish so receiving inspection shares one acceptance language.

Inspection and Testing

Base ASTM A213 testing for TP309S includes heat analysis, tension to the Table 4 75/30 ksi floors, hardness to the Table 4 maximum, flattening and flaring on a lot basis, and hydro or NDE of each length. The manufacturer may choose hydro versus NDE unless the purchase order fixes the method. Marking includes ASTM designation, grade, size, heat number, and other clause-required data.

Option Purpose
Product analysis Confirms chemistry on finished tube
Intergranular corrosion / oxidation tests Only when Supplementary Requirements or OEM specs add them
Minimum vs average wall States wall basis
Fixed hydro or NDE method Removes manufacturer’s option
Third-party inspection / EN 10204 3.2 Witnessed testing when the project requires it

Ask the mill to state lot identity clearly so hardness and tension specimens map cleanly to the bundle you receive.

Packaging and Shipping

TP309S tube leaves SHH STEEL bundled, end-protected, and tagged with ASTM A213 grade, OD × wall (or BWG), heat number, and PO reference. U-bent or specially cut furnace lengths need transit protection matched to bend radius and leg length. Export packing ranges from bare or wrapped bundles to wooden cases for bright-annealed or small-bore material.

We ship under the Incoterms on the order acknowledgement — FOB, CFR, CIF, EXW, or other agreed terms. Bilingual marks, inland trucking, and project color coding belong on the enquiry beside the metallurgical notes.

Why Choose SHH STEEL

SHH STEEL treats ASTM A213 TP309S as a high-Cr–Ni oxidation-oriented tube grade with enforceable chemistry, tensile, hardness, and heat-treatment rules — not as a catalogue nickname for “any 309 tube.” Certificates report the stainless-table ladle chemistry and Table 4 set; dual A213/SA-213 marking appears only when requested.

If the datasheet needs H-grade carbon and grain size, we open A213 TP309H. If niobium stabilization is specified, we open A213 TP309Cb. If still higher Cr–Ni is required, we open A213 TP310S. Wet chloride duty steers to the Mo family on the A213/A213M hub. Lead times mix near-term lengths with mill schedules; we say which is which.

Cut-to-length, U-bending, polish, and third-party inspection are defined extras. The tube on site should match the ASTM callout the engineer wrote.

Supply Capability

SHH STEEL can supply ASTM A213 TP309S stainless steel tube against the edition and finish route on your enquiry. Capability and Stock / Available sizes below frame furnace, boiler, and HX enquiries for this grade.

Item SHH STEEL capability for TP309S
Standard ASTM A213 / A213M (dual SA-213 marking on request) Grade TP309S / UNS S30908
Product form Seamless only — cold-finished and hot-finished
Size Typical OD × min wall (or average wall) in the A213 usual band; other diameters by agreement
Wall / gauge Minimum wall or average wall; BWG / gauge accepted
Length Cut-to-length for furnace / HX / boiler; mill random by agreement; bends on enquiry
Finish Annealed and pickled; bright annealed or light polish by agreement
Testing Tension (75/30 ksi), hardness (max 192 HBW / 90 HRB), flattening, flaring, hydro or NDE; full melt chemistry on MTC
Documents EN 10204 3.1; third-party / 3.2 on request
Trade terms FOB / CFR / CIF / EXW and other agreed Incoterms

Stock / Available sizes

SHH STEEL quotes TP309S against a stock-and-mill enquiry range rather than a frozen SKU/tonnage list. Representative OD × wall / BWG combinations for furnace, boiler, and heat-exchanger tube appear below.

Item Typical stock / enquiry range for TP309S
Outside diameter 19.05, 25.4, 31.8, 38.1, 42.4, 50.8, 60.3, 76.2 mm (and other furnace/HX ODs on enquiry; through the usual A213 ~5 in. [127 mm] band)
Wall / BWG BWG 10–18 class walls and metric min-wall equivalents; heavier walls by agreement
Common OD × wall examples 25.4 × 2.11 mm; 31.8 × 2.77 mm; 38.1 × 2.77 mm; 42.4 × 3.56 mm; 50.8 × 3.05 mm; 60.3 × 3.91 mm — illustrative, confirm min vs average wall
Length Cut lengths for furnace / exchanger bundles; bends and random mill lengths on enquiry
Special Non-standard OD/wall, bright anneal, dual A213/SA-213, third-party witness — confirm before heat reservation

Send OD × wall (or BWG), wall basis, finish route, quantity or cut list, marking (A213 or dual A213/SA-213), and Supplementary Requirements on one enquiry. We confirm Cr 22–24% / Ni 12–15% chemistry and Table 4 75/30 ksi without inventing fake warehouse codes. Sisters A213 TP309H, A213 TP310S, and A213 TP304 sit on the same hub.

FAQ

Is ASTM A213 the same as ASME SA-213 for TP309S?
No. ASTM A213 / A213M is the ASTM International product specification for seamless boiler, superheater, and heat-exchanger tubes; ASME SA-213 / SA-213M is the separate ASME Code Book adoption. Dual-mark only when the purchase order asks for both names on the stencil and MTC. Chemistry and tensile floors align closely for a given referenced edition, but the standards remain independent.
Does ASTM A213 TP309S include welded or HCW tube?
No. ASTM A213 covers seamless tube only. There is no WLD or HCW manufacturing type under this product standard. Cold-finished versus hot-finished seamless tube is the process choice. Welded stainless pipe belongs to a different product standard and page family.
What is the chemistry of ASTM A213 TP309S?
TP309S / UNS S30908 melt limits include carbon ≤0.08%, manganese ≤2.00%, phosphorus ≤0.045%, sulfur ≤0.030%, silicon ≤1.00%, chromium 22.0–24.0%, and nickel 12.0–15.0%, with molybdenum and nitrogen as no-requirement ellipses. Product-analysis limits apply only when ordered, typically from A480 Table A1.1 via the A1016 path.
TP309S vs TP304 — when do I need the higher Cr–Ni grade?
Order TP309S when high-temperature oxidation and hot-gas scale resistance need chromium 22–24% and nickel 12–15% rather than the 18-8 balance of TP304. Room-temperature Table 4 tensile floors are the same 75/30 ksi pair; the differentiation is chemistry and oxidation framing, not a unique tensile number. Do not use 309S as a casual substitute for molybdenum grades in aqueous chlorides.
TP309S vs TP309H — which A213 grade should I order?
Order TP309S when the ≤0.08% carbon ceiling and standard solution-treat path are enough. Order TP309H when the datasheet needs the H-grade carbon range (0.04–0.10%), grain-size controls (ASTM No. 7 or coarser in the public Table 3 excerpt), and creep-oriented framing. Do not treat "309H" as a synonym stamp for ordinary TP309S on the MTC.
TP309S vs TP310S — which oxidation grade is higher alloy?
TP310S carries still higher chromium and nickel (typically 24–26% Cr / 19–22% Ni under A213) than TP309S’s 22–24 / 12–15 windows. Order TP310S when the datasheet or temperature/atmosphere combination calls for that step-up. Both remain seamless A213 tube grades with their own chemistry rows — compare on the hub before swapping.
Does Table 4 set a hardness limit for TP309S?
Yes. Hardness maximum is 192 HBW / 200 HV or 90 HRB, alongside 75/30 ksi tensile/yield and 35% elongation. Hardness tests are part of lot acceptance under A213. Tighter project hardness windows must be written into the purchase order.
What heat treatment does A213 require for TP309S?
Solution treatment at a minimum of 1900 °F [1040 °C] with water quench or other rapid cool. Both cold-finished and hot-finished seamless tube follow that requirement. Ask the mill to state anneal temperature and quench method on the EN 10204 3.1 certificate.
Minimum wall vs average wall for A213 TP309S — which do I order?
Order minimum wall when the design assumes a guaranteed minimum thickness after tolerance. Order average wall only when the PO explicitly allows it and the designer accepts that basis. Put the wall basis on the enquiry before the mill selects A1016 tolerance tables.
Is TP309S a good choice for chloride-rich cooling water?
Usually no as a first choice. TP309S is framed for high-temperature oxidation resistance; it does not add molybdenum for aqueous chloride pitting. Prefer TP316/TP316L or higher-Mo grades on the A213 hub for seawater-leaning and brine exchangers. ASTM A213 does not publish a chloride ranking table.
Can you dual-certify A213 and SA-213 TP309S?
Yes when the purchase order requests both independent standards on the stencil and MTC. Dual marking with TP309H is only possible on heats that also meet H-grade carbon and grain-size rules — do not assume it from a PMI gun reading. Spell the required marking on the enquiry.

Conclusion

ASTM A213 TP309S / UNS S30908 is the 22–24% Cr / 12–15% Ni seamless stainless steel tube grade for boiler, furnace, and heat-exchanger service when high-temperature oxidation resistance — not molybdenum chloride framing — drives grade selection. SHH STEEL supplies cold-finished and hot-finished seamless tube in the usual OD × wall / BWG band, solution annealed at 1900 °F [1040 °C], tested to Table 4 75/30 ksi and hardness limits, and documented on EN 10204 3.1 certificates — with dual SA-213 marking only when the order asks. For sister 309H, 309Cb, and 310S grades, start from the A213/A213M hub, then send OD × wall, wall basis, and marking requirements so we can align mill and near-term availability.

Contact: admin@steelspecs.com

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X