ASTM A213 TP309LMoN Stainless Steel Tube | ASTM A213 Stainless Steel - SHH STEEL

ASTM A213 TP309LMoN Stainless Steel Tube

ASTM A213 TP309LMoN / UNS S30925 seamless boiler, superheater and heat-exchanger tube — low-carbon (C ≤0.025%) 23–26% Cr / 13–16% Ni austenitic with Mo 0.5–1.2%, N 0.25–0.40%, Table 4 floors of 93/38 ksi, hardness max 256 HBW / 100 HRB, 1920 °F solution anneal, and ASTM grain size No. 7 or coarser. SHH STEEL supplies cold-finished and hot-finished seamless tube with EN 10204 3.1 MTCs that report Mo, N, and grain size.
Grade
TP309LMoN / UNS S30925
Standard
ASTM A213 / A213M
Product form
Seamless boiler / superheater / heat-exchanger tube (cold-finished and hot-finished)
Size
Typical OD × min wall (or average wall) within ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD and ~0.015–0.500 in. [0.4–12.7 mm] wall; other diameters by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is ASTM A213 TP309LMoN Stainless Steel Tube

ASTM A213 / A213M covers seamless ferritic and austenitic alloy-steel boiler, superheater, and heat-exchanger tubes. Grade TP309LMoN / UNS S30925 sits apart from the ordinary 309S/H/Cb family: carbon is held to ≤0.025%, chromium 23.0–26.0%, nickel 13.0–16.0%, molybdenum 0.5–1.2%, and nitrogen 0.25–0.40%, with phosphorus ≤0.040% and silicon ≤0.70% tighter than classic 309 rows. Table 4 then lifts tensile acceptance to 93 ksi [640 MPa] and yield to 38 ksi [260 MPa] — well above the 75/30 ksi pair of TP309S — with hardness max 256 HBW / 270 HV or 100 HRB. Buyers who write “309LMoN tube” still need the A213 (or separate ASME SA-213) callout so wall basis, grain size, Mo/N reporting, and marking clauses are contractual.

SHH STEEL can supply ASTM A213 TP309LMoN stainless steel tube as seamless cold-finished and hot-finished product in the usual boiler, furnace, and heat-exchanger OD × wall / BWG band, shipped with EN 10204 3.1 mill test certificates that report the full stainless-table ladle chemistry — including molybdenum and nitrogen — plus the Table 4 tensile/hardness set and the grain-size result for the heat-treatment lot. Dual A213 / SA-213 marking is available only when the purchase order asks for both independent standards. Browse 309-family and nitrogen-strengthened grades on the A213/A213M hub.

Shop names such as 309LMoN, S30925, or “low-carbon moly-nitrogen 309 tube” do not replace the ASTM grade on the MTC — and this row is not a casual substitute for TP309S or TP316L. Sister grades under the same ASTM standard include A213 TP309S, A213 TP309H, A213 TP316LN, A213 XM-19, and A213 TP304LN. A213 covers seamless tube only — cold-finished versus hot-finished is the process choice, not a WLD/HCW manufacturing-type letter.

Chemical Composition of A213 TP309LMoN

Two chemistry layers matter for TP309LMoN under ASTM A213. Melting analysis is mandatory for every heat; product analysis on finished tube applies only when Supplementary Requirement wording or the purchase order invokes it through ASTM A1016/A1016M, with tolerances typically from ASTM A480/A480M Table A1.1. Four lines drive selection before anything else: carbon ≤0.025% (true L-grade ceiling, tighter than classic L ≤0.035%), molybdenum 0.5–1.2%, nitrogen 0.25–0.40%, and chromium 23.0–26.0% / nickel 13.0–16.0%. The nitrogen analysis method is a matter of agreement between purchaser and producer (Footnote B in the public table text) — put the agreed method on the PO when N reporting must follow a named technique.

The tables below reproduce the melt limits for TP309LMoN / UNS S30925 and the product-analysis limits from A480 Table A1.1. Values are maximum unless a range is shown; ellipsis (…) means no requirement.

Melting analysis (heat / ladle analysis)

Element TP309LMoN (UNS S30925) melting analysis
Carbon (C) ≤ 0.025
Manganese (Mn) ≤ 2.00
Phosphorus (P) ≤ 0.040
Sulfur (S) ≤ 0.030
Silicon (Si) ≤ 0.70
Chromium (Cr) 23.0 – 26.0
Nickel (Ni) 13.0 – 16.0
Molybdenum (Mo) 0.5 – 1.2
Nitrogen (N) 0.25 – 0.40
Niobium (Nb / Cb) … (no requirement)

Source: ASTM A213/A213M stainless chemistry table for Grade TP309LMoN / UNS S30925 (public mill / specification PDF excerpt — htpipe A213 table text). Confirm the ordered edition on the purchase order. Note the tighter P (≤0.040) and Si (≤0.70) versus classic 309 rows, and Cr/Ni windows that sit above ordinary TP309S.

Product analysis — A480/A480M Table A1.1 tolerances applied

Element Melting Tolerance (A480 A1.1) Product analysis limit
Carbon (C) ≤ 0.025 0.005 over ≤ 0.030
Manganese (Mn) ≤ 2.00 0.04 over ≤ 2.04
Phosphorus (P) ≤ 0.040 0.010 over ≤ 0.050
Sulfur (S) ≤ 0.030 0.005 over ≤ 0.035
Silicon (Si) ≤ 0.70 0.05 over ≤ 0.75
Chromium (Cr) 23.0 – 26.0 0.25 under / over 22.75 – 26.25
Nickel (Ni) 13.0 – 16.0 0.15 under / over 12.85 – 16.15
Molybdenum (Mo) 0.5 – 1.2 0.05 under / over 0.45 – 1.25
Nitrogen (N) 0.25 – 0.40 0.02 under / 0.04 over 0.23 – 0.44

Key chemistry snapshot — TP309S / TP309LMoN / TP316LN

Element TP309S (S30908) TP309LMoN (S30925) TP316LN (S31653)
C ≤ 0.08 ≤ 0.025 ≤ 0.035
Cr 22.0 – 24.0 23.0 – 26.0 16.0 – 18.0
Ni 12.0 – 15.0 13.0 – 16.0 10.0 – 14.0
Mo … 0.5 – 1.2 2.00 – 3.00
N … 0.25 – 0.40 0.10 – 0.16

Read Mo and N together with the L carbon ceiling: TP309LMoN is not “309S with a little nitrogen,” and it is not a drop-in for A213 TP316LN (which carries higher Mo 2–3% at lower Cr–Ni and a lower N band). Versus A213 TP309S, this grade adds Mo, a mandatory high nitrogen floor, tighter C/P/Si, and a higher Cr–Ni window. Niobium remains a no-requirement ellipsis — for Nb stabilization open the Cb / HCb pages.

When product analysis is ordered, finished tube may read up to C 0.030%, Mn 2.04%, P 0.050%, S 0.035%, and Si 0.75%, with Cr 22.75–26.25%, Ni 12.85–16.15%, Mo 0.45–1.25%, and N 0.23–0.44%. Put any tighter project nitrogen floor or molybdenum ceiling on the purchase order before the heat is selected. Carbon product tolerance for ≤0.025% max uses the low-carbon A480 practice (0.005 over) — confirm A480 edition if product analysis is contractual.

Mechanical Properties of A213 TP309LMoN

ASTM A213 Table 4 sets the tensile acceptance floor for TP309LMoN at 93 ksi [640 MPa] tensile strength and 38 ksi [260 MPa] yield strength (0.2% offset), with elongation of 30% minimum in 2 in. or 50 mm — a distinctly higher strength pair than the 75/30 ksi / 35% elongation story of TP309S. Hardness maximum is 256 HBW / 270 HV or 100 HRB. Public Table 3 also assigns ASTM grain size No. 7 or coarser to this grade, determined per heat-treatment lot.

Property TP309LMoN requirement
Tensile strength, min (Table 4) 93 ksi [640 MPa]
Yield strength (0.2% offset), min (Table 4) 38 ksi [260 MPa]
Elongation in 2 in. or 50 mm, min (Table 4) 30%
Hardness, max (Table 4) 256 HBW / 270 HV or 100 HRB
Grain size ASTM No. 7 or coarser (per heat-treatment lot)

Source: ASTM A213/A213M Table 4 for TP309LMoN / UNS S30925 and heat-treatment table grain-size column “7” (public specification PDF excerpt — htpipe A213). Mechanical property requirements do not apply to tubing smaller than 1/8 in. [3.2 mm] ID or thinner than 0.015 in. [0.4 mm] wall. Flattening and flaring tests sit beside tension and hardness on a lot basis.

The nitrogen floor is the commercial reason the strength pair sits above classic 309: do not expect a TP309S heat to clear 93/38 ksi by re-stamping. A tensile-only MTC that omits grain size, molybdenum, or nitrogen is incomplete for TP309LMoN — ask for the full set on the certificate before releasing the heat to fabrication.

Dimensions and Tolerances

Dimensional supply for ASTM A213 TP309LMoN is tube language — OD × wall (minimum or average) and BWG / gauge — covering boiler, furnace, and heat-exchanger sizes rather than leading with ASME B36.19 pipe schedules. Usual A213 sizes run from about 1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD with min wall about 0.015–0.500 in. [0.4–12.7 mm]; other diameters by agreement. The higher yield floor can allow thinner walls in some designs, but wall basis and Code allowables still govern — state minimum versus average wall on the purchase order.

OD and wall variations follow ASTM A1016/A1016M as invoked by A213. Cold-finished tubes commonly hold tighter OD; hot-finished tubes allow wider windows. Cold-finished average wall is often summarized as ±10% of specified average wall; minimum-wall product follows A1016 minimum-wall tables. Confirm exact rows for the OD and finish on the ordered edition.

Item Typical A213 TP309LMoN dimensional practice
Product form Seamless only (cold-finished or hot-finished)
Usual size band ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD; wall ~0.015–0.500 in. [0.4–12.7 mm]
Wall basis Minimum wall (default) or average wall when specified
OD / wall tolerances Per ASTM A1016/A1016M for finish route and size
Length Cut lengths for furnace / HX / boiler bundles; mill random by agreement
Secondary note B36.19 schedules only as a buyer cross-reference

Put cut list, design metal temperature context, and end preparation on the enquiry. Minimum wall remains a first-class A213 concept even when the higher yield invites thinner-wall thinking.

Equivalent Grades

Equivalence language around 309LMoN tube is sparse in shop nicknames — the UNS number S30925 is often the cleanest cross-reference. ASTM A213 Grade TP309LMoN / UNS S30925 is the governing designation for this article; do not treat it as automatic dual-cert stock with TP309S, TP316LN, or XM-19.

Designation Notes
ASTM A213 / A213M Grade TP309LMoN Governing ASTM seamless boiler / HX tube product standard for this article
UNS S30925 Unified number in the stainless chemistry table
ASME SA-213 TP309LMoN Separate ASME Code Book adoption — dual-mark only when the PO asks
Related classic 309 A213 TP309S — lower strength, no Mo/N mandate
Related LN Mo grade A213 TP316LN — higher Mo 2–3%, lower Cr–Ni, lower N band
Related high-N austenitic A213 XM-19 — different chem/strength story (100/55 ksi)
Related plate A240 / SA240 flat product — order plate and tube under their own standards

Dual A213/SA-213 marking is a purchase-order option. Compare chemistry and Table 4 floors on the hub before swapping nitrogen-strengthened grades inside a furnace or exchanger tube list.

Heat Treatment and Delivery Condition

TP309LMoN under ASTM A213 is furnished solution treated at a minimum of 1920 °F [1050 °C], then quenched in water or cooled rapidly by other means — note the 20 °F [about 10 °C] higher minimum versus the 1900 °F [1040 °C] row used for TP309S / TP309H / TP309Cb. That Table 3 heat-treatment row also carries ASTM grain size No. 7 or coarser for the heat-treatment lot.

Cold-finished versus hot-finished is a process and dimensional route, not a substitute for the anneal or the grain-size check. Delivery condition for SHH STEEL TP309LMoN is solution annealed and pickled (or bright annealed by agreement), with anneal temperature, quench method, Mo/N results, and E112 grain-size result on the EN 10204 3.1 certificate. Straightening, cutting, and end finishing follow heat treatment.

Do not assume a TP309S anneal certificate covers TP309LMoN — the minimum solution temperature and grain-size mandate differ. When Nb stabilization is required instead of Mo+N strengthening, open the A213 TP309Cb / A213 TP309HCb pages rather than stretching this grade’s chemistry.

Corrosion Resistance

TP309LMoN combines high-Cr–Ni oxidation framing (Cr 23–26% / Ni 13–16%) with a modest molybdenum addition (0.5–1.2%) and a true L-grade carbon ceiling (≤0.025%) that helps as-welded intergranular resistance relative to standard-carbon 309. The nitrogen band supports the higher Table 4 strength pair. It is not a full substitute for TP316/TP316L in aqueous chloride duty: molybdenum here tops out at 1.2%, well below the 2–3% Mo band of the 316 family.

Selection remains engineering judgment against atmosphere, temperature, chloride level, and cyclic duty. ASTM A213 does not publish a corrosion-rate, PREN ranking, or oxidation-rate table for TP309LMoN. When a project invokes Practice A262 or a specific oxidation/chloride test, write that Supplementary Requirement onto the purchase order. For heavier Mo chloride framing, open A213 TP316L / A213 TP316LN.

Applications of A213 TP309LMoN Tube

TP309LMoN shows up wherever seamless tube needs 309-family high-Cr–Ni oxidation resistance, a low carbon ceiling, modest molybdenum, and nitrogen-driven strength above classic 309 — furnace and heat-recovery circuits, selected boiler/HX locations, and projects that specify S30925 by UNS rather than a shop nickname.

Application area Typical use of TP309LMoN tube Selection note
Hot-gas / furnace HX Oxidizing atmospheres with L carbon and modest Mo Confirm Mo band vs TP316 family needs
Boiler / HX (strength + L carbon) Where 93/38 ksi and C ≤0.025% are on the datasheet Confirm grain-size reporting on MTC
Nitrogen-strengthened austenitic duty When N 0.25–0.40% is specified with 309-range Cr–Ni Compare XM-19 if 100/55 ksi is required
Heavy aqueous chloride Usually not first choice at Mo ≤1.2% Prefer TP316L / TP316LN / higher-Mo grades
Nb-stabilized 309 duty Not TP309LMoN (Nb is ellipsis) Open TP309Cb / TP309HCb

Stay on the A213/A213M hub for 309S, 316LN, and XM-19 sisters rather than mixing A312 pipe certificates into tube acceptance.

Weldability

TP309LMoN tube welds with matching or near-matching low-carbon 309 / Mo-bearing austenitic filler for tube-to-tubesheet, attachment, and fabrication joins under a qualified WPS. ER309L or Mo-bearing low-carbon deposits are common when weld-metal carbon must stay low to match the L-grade base philosophy; filler selection remains the fabricator’s code responsibility under a qualified WPS. Heat input, interpass, and cleaning are likewise fabricator responsibilities — A213 governs the seamless tube product, not the field weld procedure.

Because A213 TP309LMoN is seamless, there is no mill longitudinal weld to radiograph as welded-pipe standards describe. Focus inspection on each-length hydro or NDE, joint quality, Mo/N and grain size on the MTC, and any contractual IGC or oxidation tests. Do not try to weld-procedure a TP309S heat into an LMoN datasheet — the carbon, Mo, N, and strength floors do not overlap.

Surface Finishes

Standard mill delivery for ASTM A213 TP309LMoN is solution annealed and pickled. Bright annealing is a called-out route when a smoother reflective surface is needed. Specified Ra, light polish, and post-fabrication passivation are commercial extras on top of the A213 stamp.

Furnace and HX tube often ships with a workmanlike pickled finish; cosmetic polish is uncommon unless the PO asks. End preparation for welding or expanding should be ordered with finish so receiving inspection shares one acceptance language. Molybdenum, nitrogen, and grain-size reporting are metallurgical requirements on the MTC, not surface-finish options.

Inspection and Testing

Base ASTM A213 testing for TP309LMoN includes heat analysis (with molybdenum and nitrogen), tension to the Table 4 93/38 ksi floors, hardness to the Table 4 maximum, grain size (ASTM No. 7 or coarser) per heat-treatment lot, flattening and flaring on a lot basis, and hydro or NDE of each length. The manufacturer may choose hydro versus NDE unless the purchase order fixes the method. Marking includes ASTM designation, grade, size, heat number, and other clause-required data.

Option Purpose
Product analysis Confirms chemistry — including Mo and N — on finished tube
Grain-size reporting E112 result on the MTC for the heat-treatment lot
Agreed nitrogen analysis method Footnote B — put the method on the PO when required
Intergranular corrosion / oxidation tests Only when Supplementary Requirements or OEM specs add them
Minimum vs average wall States wall basis
Fixed hydro or NDE method Removes manufacturer’s option
Third-party inspection / EN 10204 3.2 Witnessed testing when the project requires it

Ask the mill to state lot identity clearly so hardness, tension, grain-size, Mo, and N specimens map cleanly to the bundle you receive. An MTC without Mo, N, or grain size is incomplete for TP309LMoN.

Packaging and Shipping

TP309LMoN tube leaves SHH STEEL bundled, end-protected, and tagged with ASTM A213 grade, OD × wall (or BWG), heat number, and PO reference. U-bent or specially cut furnace and HX lengths need transit protection matched to bend radius and leg length. Export packing ranges from bare or wrapped bundles to wooden cases for bright-annealed or small-bore material.

We ship under the Incoterms on the order acknowledgement — FOB, CFR, CIF, EXW, or other agreed terms. Bilingual marks, inland trucking, and project color coding belong on the enquiry beside the metallurgical notes (C ≤0.025%, Mo, N, grain size, dual marking).

Why Choose SHH STEEL

SHH STEEL treats ASTM A213 TP309LMoN as a distinct low-carbon, molybdenum-bearing, nitrogen-strengthened 309-range tube product with enforceable chemistry, tensile, hardness, grain-size, and heat-treatment rules — not as a catalogue nickname for “any 309 tube.” Certificates report Mo, N, Table 4 93/38 ksi, and E112 grain size; dual A213/SA-213 marking appears only when requested.

If classic 309 oxidation without Mo/N is enough, we open A213 TP309S. If heavier Mo chloride framing is the real need, we open A213 TP316L / A213 TP316LN. If still higher nitrogen-strengthened austenitic strength is required, we open A213 XM-19. The A213/A213M hub is organized grade by grade under ASTM, seamless tube only. Lead times mix near-term lengths with mill schedules; we say which is which.

Cut-to-length, U-bending, polish, and third-party inspection are defined extras. The tube on site should match the ASTM callout the engineer wrote — including Mo, N, and grain size on the MTC.

Supply Capability

SHH STEEL can supply ASTM A213 TP309LMoN stainless steel tube against the edition and finish route on your enquiry. Capability and Stock / Available sizes below frame furnace, boiler, and HX enquiries for this L+Mo+N grade.

Item SHH STEEL capability for TP309LMoN
Standard ASTM A213 / A213M (dual SA-213 marking on request) Grade TP309LMoN / UNS S30925
Product form Seamless only — cold-finished and hot-finished
Size Typical OD × min wall (or average wall) in the A213 usual band; other diameters by agreement
Wall / gauge Minimum wall or average wall; BWG / gauge accepted
Length Cut-to-length for furnace / HX / boiler; mill random by agreement; bends on enquiry
Finish Annealed and pickled; bright annealed or light polish by agreement
Testing Tension (93/38 ksi), hardness (max 256 HBW / 100 HRB), grain size (No. 7 or coarser), flattening, flaring, hydro or NDE; full melt chemistry including Mo and N on MTC
Documents EN 10204 3.1 with Mo, N, and grain-size results; third-party / 3.2 on request
Trade terms FOB / CFR / CIF / EXW and other agreed Incoterms

Stock / Available sizes

SHH STEEL quotes TP309LMoN against a stock-and-mill enquiry range rather than a frozen SKU/tonnage list. Representative OD × wall / BWG combinations for furnace, boiler, and heat-exchanger tube appear below.

Item Typical stock / enquiry range for TP309LMoN
Outside diameter 19.05, 25.4, 31.8, 38.1, 42.4, 50.8, 60.3, 76.2 mm (and other furnace/HX ODs on enquiry; through the usual A213 ~5 in. [127 mm] band)
Wall / BWG BWG 10–18 class walls and metric min-wall equivalents; thinner walls exploiting 38 ksi yield by agreement after design review
Common OD × wall examples 25.4 × 1.65 mm; 25.4 × 2.11 mm; 31.8 × 2.11 mm; 38.1 × 2.77 mm; 50.8 × 2.77 mm; 60.3 × 3.05 mm — illustrative, confirm min vs average wall
Length Cut lengths for furnace / exchanger bundles; bends and random mill lengths on enquiry
Special Non-standard OD/wall, bright anneal, dual A213/SA-213, agreed N analysis method, third-party witness — confirm before heat reservation

Send OD × wall (or BWG), wall basis, finish route, quantity or cut list, marking (A213 or dual A213/SA-213), Mo/N/grain-size reporting expectation, nitrogen analysis method if required, and Supplementary Requirements on one enquiry. We confirm C ≤0.025%, Cr 23–26% / Ni 13–16%, Mo 0.5–1.2%, N 0.25–0.40%, Table 4 93/38 ksi, and ASTM No. 7 or coarser without inventing fake warehouse codes. Sisters A213 TP309S, A213 TP316LN, and A213 XM-19 sit on the same hub.

FAQ

Is ASTM A213 the same as ASME SA-213 for TP309LMoN?
No. ASTM A213 / A213M is the ASTM International product specification for seamless boiler, superheater, and heat-exchanger tubes; ASME SA-213 / SA-213M is the separate ASME Code Book adoption. Dual-mark only when the purchase order asks for both names on the stencil and MTC. Chemistry, tensile floors, and grain-size rules align closely for a given referenced edition, but the standards remain independent.
Does ASTM A213 TP309LMoN include welded or HCW tube?
No. ASTM A213 covers seamless tube only. There is no WLD or HCW manufacturing type under this product standard. Cold-finished versus hot-finished seamless tube is the process choice. Welded stainless pipe belongs to a different product standard and page family.
What is the chemistry of ASTM A213 TP309LMoN?
TP309LMoN / UNS S30925 melt limits include carbon ≤0.025%, manganese ≤2.00%, phosphorus ≤0.040%, sulfur ≤0.030%, silicon ≤0.70%, chromium 23.0–26.0%, nickel 13.0–16.0%, molybdenum 0.5–1.2%, and nitrogen 0.25–0.40%, with niobium as a no-requirement ellipsis. Product-analysis limits apply only when ordered. Nitrogen analysis method is by agreement (Footnote B).
TP309LMoN vs TP309S — why is the strength higher?
TP309LMoN carries a mandatory nitrogen band of 0.25–0.40% plus molybdenum 0.5–1.2% and a ≤0.025% carbon ceiling, which together support Table 4 floors of 93/38 ksi versus the 75/30 ksi pair of TP309S. Chromium and nickel also sit higher (23–26 / 13–16 versus 22–24 / 12–15). Do not expect a TP309S heat to clear LMoN chemistry or tensile by re-stamping.
TP309LMoN vs TP316LN — which Mo+N grade should I order?
Order TP309LMoN when the datasheet needs 309-range Cr–Ni (23–26 / 13–16), Mo 0.5–1.2%, N 0.25–0.40%, and the 93/38 ksi pair. Order TP316LN when classic 316-family Mo 2.00–3.00% with N 0.10–0.16% and lower Cr–Ni is specified. They are not automatic substitutes — compare chemistry and Table 4 on the A213 hub before swapping.
Does TP309LMoN require grain size under A213?
Yes. Public Table 3 assigns ASTM grain size No. 7 or coarser to TP309LMoN per heat-treatment lot, alongside solution treatment at a minimum of 1920 °F [1050 °C]. A tensile-only certificate that omits the E112 result is incomplete for this grade under A213.
What heat treatment does A213 require for TP309LMoN?
Solution treatment at a minimum of 1920 °F [1050 °C] with water quench or other rapid cool, plus ASTM grain size No. 7 or coarser for the heat-treatment lot. Note the higher minimum versus the 1900 °F [1040 °C] row used for TP309S/H/Cb. Ask the mill to state anneal temperature, quench method, Mo, N, and grain-size result on the EN 10204 3.1 certificate.
Does Table 4 set a hardness limit for TP309LMoN?
Yes. Hardness maximum is 256 HBW / 270 HV or 100 HRB — higher than the 192 HBW / 90 HRB ceiling of TP309S — alongside 93/38 ksi tensile/yield and 30% elongation. Hardness tests are part of lot acceptance under A213. Tighter project hardness windows must be written into the purchase order.
Minimum wall vs average wall for A213 TP309LMoN — which do I order?
Order minimum wall when the design assumes a guaranteed minimum thickness after tolerance. Order average wall only when the PO explicitly allows it and the designer accepts that basis. The higher yield can invite thinner-wall thinking, but wall basis still belongs on the enquiry before the mill selects A1016 tolerance tables.
Is TP309LMoN enough molybdenum for seawater-leaning exchangers?
Often not as a first choice. Molybdenum on TP309LMoN is only 0.5–1.2%, well below the 2–3% Mo band of TP316/TP316L/TP316LN. Prefer the 316 family or higher-Mo grades on the A213 hub for seawater-leaning and brine exchangers. ASTM A213 does not publish a chloride ranking table for this grade.
Can you dual-certify A213 and SA-213 TP309LMoN?
Yes when the purchase order requests both independent standards on the stencil and MTC. Dual marking toward TP309S is not a meaningful path: carbon, Mo, N, and tensile floors do not overlap. Spell the required marking and any agreed nitrogen analysis method on the enquiry before the heat is reserved.

Conclusion

ASTM A213 TP309LMoN / UNS S30925 is the low-carbon, molybdenum-bearing, nitrogen-strengthened 23–26% Cr / 13–16% Ni seamless stainless steel tube grade for boiler, furnace, and heat-exchanger service when oxidation framing, L-grade carbon, modest Mo, and a 93/38 ksi strength pair all drive grade selection. SHH STEEL supplies cold-finished and hot-finished seamless tube in the usual OD × wall / BWG band, solution annealed at 1920 °F [1050 °C], tested to Table 4 93/38 ksi and hardness limits with ASTM No. 7 or coarser grain size and Mo/N on the MTC, and documented on EN 10204 3.1 certificates — with dual SA-213 marking only when the order asks. For sister 309S, 316LN, and XM-19 grades, start from the A213/A213M hub, then send OD × wall, wall basis, Mo/N/grain-size expectation, and marking requirements so we can align mill and near-term availability.

Contact: admin@steelspecs.com

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X