ASTM A213 TP310MoLN Stainless Steel Tube | ASTM A213 Stainless Steel - SHH STEEL

ASTM A213 TP310MoLN Stainless Steel Tube

ASTM A213 TP310MoLN / UNS S31050 seamless boiler, superheater and heat-exchanger tube — low-carbon 24–26% Cr / 21–23% Ni austenitic with C ≤0.025%, Mo 2.00–3.00%, N 0.10–0.16%, Si ≤0.40%, wall-dependent Table 4 floors (84/39 or 78/37 ksi), and hardness max 217 HBW / 95 HRB. SHH STEEL supplies cold-finished and hot-finished seamless tube with EN 10204 3.1 MTCs that report Mo and N.
Grade
TP310MoLN / UNS S31050
Standard
ASTM A213 / A213M
Product form
Seamless boiler / superheater / heat-exchanger tube (cold-finished and hot-finished)
Size
Typical OD × min wall (or average wall) within ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD and ~0.015–0.500 in. [0.4–12.7 mm] wall; other diameters by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is ASTM A213 TP310MoLN Stainless Steel Tube

ASTM A213 / A213M covers seamless ferritic and austenitic alloy-steel boiler, superheater, and heat-exchanger tubes. Grade TP310MoLN / UNS S31050 is the low-carbon molybdenum-nitrogen member of the 310 family: melting carbon ≤0.025%, chromium 24.0–26.0%, nickel 21.0–23.0%, molybdenum 2.00–3.00%, nitrogen 0.10–0.16%, with silicon capped at ≤0.40% and phosphorus at ≤0.020%. That chemistry is built for urea-stripper, nitric-acid, and other highly oxidizing process heat-exchanger duty that needs 25Cr-class oxidation resistance plus real molybdenum for aqueous corrosion — not an H-grade carbon-floor story and not a niobium-stabilized HCbN package.

SHH STEEL can supply ASTM A213 TP310MoLN stainless steel tube as seamless cold-finished and hot-finished product in the usual boiler and heat-exchanger OD × wall / BWG band, shipped with EN 10204 3.1 mill test certificates that report ladle chemistry including molybdenum and nitrogen, and the wall-dependent Table 4 tensile and hardness results. Dual A213 / SA-213 marking is available only when the purchase order asks for both independent standards. Browse 310-family grades on the A213/A213M hub.

Shop names such as 310MoLN, S31050, or “25-22-2 MoLN tube” do not replace the ASTM grade on the MTC. Sister grades under the same ASTM standard include A213 TP310S, A213 TP310HCbN, A213 TP310MoCbN, A213 TP316LN, and A213 TP309LMoN. A213 covers seamless tube only — cold-finished versus hot-finished is the process choice, not a WLD/HCW manufacturing-type letter.

Chemical Composition of A213 TP310MoLN

Two chemistry layers matter for TP310MoLN under ASTM A213. Melting analysis is mandatory for every heat; product analysis on finished tube applies only when Supplementary Requirement wording or the purchase order invokes it through ASTM A1016/A1016M, with tolerances typically from ASTM A480/A480M Table A1.1. Four lines drive selection before anything else: carbon ≤0.025% (tighter than classic L ≤0.035%), molybdenum 2.00–3.00%, nitrogen 0.10–0.16%, and the raised nickel window 21.0–23.0% against chromium 24.0–26.0%. Silicon ≤0.40% and phosphorus ≤0.020% are also tighter than ordinary 310S rows. Nitrogen analysis method is a matter of agreement between purchaser and producer (Footnote B) — put the agreed method on the PO when N reporting must follow a named technique.

The tables below reproduce the melt limits for TP310MoLN / UNS S31050, the product-analysis limits from A480 Table A1.1 practice, and a short snapshot against TP310S and TP316LN. Values are maximum unless a range is shown; ellipsis (…) means no requirement.

Melting analysis (heat / ladle analysis)

Element TP310MoLN (UNS S31050) melting analysis
Carbon (C) ≤ 0.025
Manganese (Mn) ≤ 2.00
Phosphorus (P) ≤ 0.020
Sulfur (S) ≤ 0.030
Silicon (Si) ≤ 0.40
Chromium (Cr) 24.0 – 26.0
Nickel (Ni) 21.0 – 23.0
Molybdenum (Mo) 2.00 – 3.00
Nitrogen (N) 0.10 – 0.16
Niobium (Nb / Cb) … (no requirement)

Source: ASTM A213/A213M stainless chemistry table for Grade TP310MoLN / UNS S31050 (public mill / specification PDF excerpt — _ref_a213.txt / A213–13 table text). Confirm the ordered edition on the purchase order. Stainless table number is edition-dependent.

Product analysis — A480/A480M Table A1.1 tolerances applied

Element Melting Tolerance (A480 A1.1) Product analysis limit
Carbon (C) ≤ 0.025 0.005 over ≤ 0.030
Manganese (Mn) ≤ 2.00 0.04 over ≤ 2.04
Phosphorus (P) ≤ 0.020 0.005 over ≤ 0.025
Sulfur (S) ≤ 0.030 0.005 over ≤ 0.035
Silicon (Si) ≤ 0.40 0.05 over ≤ 0.45
Chromium (Cr) 24.0 – 26.0 0.25 under / over 23.75 – 26.25
Nickel (Ni) 21.0 – 23.0 0.15 under / 0.20 over 20.85 – 23.20
Molybdenum (Mo) 2.00 – 3.00 0.05 under / 0.10 over 1.95 – 3.10
Nitrogen (N) 0.10 – 0.16 0.01 under / 0.02 over 0.09 – 0.18

Key chemistry snapshot — TP310S / TP310MoLN / TP316LN

Element TP310S (S31008) TP310MoLN (S31050) TP316LN (S31653)
C ≤ 0.08 ≤ 0.025 ≤ 0.035
Cr 24.0 – 26.0 24.0 – 26.0 16.0 – 18.0
Ni 19.0 – 22.0 21.0 – 23.0 10.0 – 13.0
Mo … 2.00 – 3.00 2.00 – 3.00
N … 0.10 – 0.16 0.10 – 0.16
Si ≤ 1.00 ≤ 0.40 ≤ 1.00

Read Mo and the L carbon ceiling together with the raised nickel window: TP310MoLN is not “310S with a little molybdenum,” and it is not a drop-in for A213 TP316LN (same Mo and N bands, but much lower Cr–Ni and a higher carbon ceiling). Versus A213 TP310S, this grade adds mandatory Mo, mandatory N, tighter C/P/Si, and a higher Ni floor. Niobium remains a no-requirement ellipsis — for Nb stabilization open the Cb / HCb / HCbN pages.

When product analysis is ordered, finished tube may read up to C 0.030%, Mn 2.04%, P 0.025%, S 0.035%, and Si 0.45%, with Cr 23.75–26.25%, Ni 20.85–23.20%, Mo 1.95–3.10%, and N 0.09–0.18%. Phosphorus product tolerance for the tight ≤0.020% melt max is taken from low-P A480 practice — confirm the A480 edition if product analysis is contractual. Put any tighter project molybdenum floor or nitrogen floor on the purchase order before heat selection.

Mechanical Properties of A213 TP310MoLN

ASTM A213 Table 4 sets wall-dependent tensile floors for TP310MoLN — a pattern shared with a few other high-alloy austenitic rows and different from the single 75/30 ksi pair on ordinary 310S. For wall thickness ≤0.25 in. [6 mm], tensile strength minimum is 84 ksi [580 MPa] and yield strength minimum is 39 ksi [270 MPa]. For wall thickness >0.25 in. [6 mm], the floors drop to 78 ksi [540 MPa] tensile and 37 ksi [255 MPa] yield. Elongation is 25% minimum in 2 in. or 50 mm for both wall classes. Hardness maximum is 217 HBW or 95 HRB.

Property t ≤ 0.25 in. [6 mm] t > 0.25 in. [6 mm]
Tensile strength, min (Table 4) 84 ksi [580 MPa] 78 ksi [540 MPa]
Yield strength (0.2% offset), min (Table 4) 39 ksi [270 MPa] 37 ksi [255 MPa]
Elongation in 2 in. or 50 mm, min (Table 4) 25% 25%
Hardness, max (Table 4) 217 HBW or 95 HRB

Source: ASTM A213/A213M Table 4 for TP310MoLN / UNS S31050 (public specification PDF excerpt — _ref_a213.txt). Mechanical property requirements do not apply to tubing smaller than 1/8 in. [3.2 mm] ID or thinner than 0.015 in. [0.4 mm] wall. Flattening and flaring tests sit beside tension and hardness on a lot basis.

State the ordered wall on the enquiry so the correct Table 4 row is applied on the MTC. A certificate that quotes a single tensile number without identifying which wall class was used is incomplete for TP310MoLN release. Nitrogen and molybdenum chemistry must clear their bands alongside the wall-class tensile result — none replaces the others.

Dimensions and Tolerances

Dimensional supply for ASTM A213 TP310MoLN is tube language — OD × wall (minimum or average) and BWG / gauge — covering urea-stripper, nitric-process, and heat-exchanger sizes rather than leading with ASME B36.19 pipe schedules. Usual A213 sizes run from about 1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD with min wall about 0.015–0.500 in. [0.4–12.7 mm]; other diameters by agreement. Because Table 4 tensile floors change at 0.25 in. [6 mm] wall, state both wall basis and nominal wall on the purchase order.

OD and wall variations follow ASTM A1016/A1016M as invoked by A213. Cold-finished tubes commonly hold tighter OD; hot-finished tubes allow wider windows. Confirm exact rows for the OD and finish on the ordered edition.

Item Typical A213 TP310MoLN dimensional practice
Product form Seamless only (cold-finished or hot-finished)
Usual size band ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD; wall ~0.015–0.500 in. [0.4–12.7 mm]
Wall basis Minimum wall (default for HX / process tube) or average wall when specified
Table 4 wall class ≤0.25 in. [6 mm] vs >0.25 in. [6 mm] — name the ordered wall so the correct tensile row applies
OD / wall tolerances Per ASTM A1016/A1016M for finish route and size
Length Cut lengths for exchanger / stripper bundles; mill random by agreement
Secondary note B36.19 schedules only as a buyer cross-reference

Put cut list, process-fluid context, nitrogen analysis method, and end preparation on the enquiry. Minimum wall remains first-class for MoLN tube the same way it does for other A213 austenitic HX grades.

Equivalent Grades

Equivalence language around 310MoLN often collapses urea-grade shop names, 25-22-2 cast forms, and ordinary 310S into one nickname. ASTM A213 Grade TP310MoLN / UNS S31050 is the governing designation for this article; near-chemistry plate or cast forms are not automatic A213 substitutes.

Designation Notes
ASTM A213 / A213M Grade TP310MoLN Governing ASTM seamless boiler / HX tube product standard for this article
UNS S31050 Unified number in the stainless chemistry table
ASME SA-213 TP310MoLN Separate ASME Code Book adoption — dual-mark only when the PO asks
Related 310S A213 TP310S — same Cr band, lower Ni, no Mo/N, C ≤0.08
Related Mo+Cb+N A213 TP310MoCbN — different Cr–Ni windows, Nb+B, higher tensile
Related 316LN A213 TP316LN — same Mo/N bands at much lower Cr–Ni
Related plate A240 / SA240 flat product in related families — order plate and tube under their own standards

Dual A213/SA-213 marking is a purchase-order option. Compare TP310S and TP316LN on their own pages before assuming a mixed nickname equals TP310MoLN on the MTC.

Heat Treatment and Delivery Condition

TP310MoLN under ASTM A213 is furnished in the solution-treated condition with water quench or other rapid cool, as required for austenitic grades in Section 6. The A213/A213M–13 PDF excerpt used as the chem/mech source for this pack prints TP310MoLN in the chemistry and Table 4 mechanical tables, but does not print a dedicated S31050 heat-treatment temperature line between S31042 and S31060 in Table 3 — treat the exact minimum solution temperature and any grain-size column entry as UNCERTAIN pending the ordered edition. Confirm the Table 3 row for TP310MoLN / S31050 on the purchase order before freezing anneal temperature language on the MTC.

Cold-finished versus hot-finished is a process and dimensional route, not a substitute for the solution anneal. Delivery condition for SHH STEEL TP310MoLN is solution annealed and pickled (or bright annealed by agreement), with anneal temperature, quench method, molybdenum, and nitrogen stated on the EN 10204 3.1 certificate once the ordered edition’s Table 3 values are confirmed.

Because carbon is already at an L-grade ceiling (≤0.025%), intergranular-corrosion capability after welding is stronger than on standard-carbon 310S — but ASTM A213 still does not run A262 Practice E automatically. Put S4 / A262 Practice E on the purchase order when demonstrated IGC performance is contractual. Do not invent an H-grade grain-size mandate for MoLN unless the ordered edition’s Table 3 row lists one.

Corrosion Resistance

TP310MoLN earns its place through a combination of high chromium for oxidizing media, molybdenum 2–3% for aqueous corrosion resistance, low carbon for weld-heat IGC control, and nitrogen for strength. That is a different story from plain A213 TP310S (no Mo requirement) and from A213 TP310HCbN (Nb+N H-grade without Mo).

Typical selection conversations include urea stripper and related carbamate circuits, nitric-acid condensers and heaters, and other oxidizing process exchangers where 25Cr-class chemistry plus Mo is specified by name. Seawater and heavy brine still need project-specific review — Mo at 2–3% helps versus 310S, but ASTM A213 does not publish a PREN ranking table for this grade. Put A262 Practice E on the PO when IGC demonstration is required rather than assumed from the L carbon ceiling alone.

Applications of A213 TP310MoLN Tube

Buyers specify ASTM A213 TP310MoLN when seamless tube must combine 24–26% Cr oxidation resistance, 2–3% Mo aqueous corrosion resistance, an L-grade carbon ceiling, and nitrogen-assisted tensile floors on a raised 21–23% nickel window. Typical placements include urea-plant heat-exchanger and stripper tubing, nitric-acid process heaters and condensers, and selected oxidizing chemical-process bundles that name S31050 or TP310MoLN explicitly.

Do not substitute ordinary 310S paperwork for MoLN acceptance, and do not treat A213 TP316LN as interchangeable simply because Mo and N bands overlap — Cr–Ni windows and tensile tables differ. When Nb+B molybdenum chemistry on inverted Cr–Ni windows is required, open A213 TP310MoCbN. SHH STEEL quotes OD × wall / BWG against the wall-class tensile row and the Mo/N chemistry on the datasheet.

Service theme Why TP310MoLN is considered
Urea / carbamate HX C ≤0.025 + Mo 2–3 + 24–26 Cr / 21–23 Ni
Nitric / oxidizing process HX High Cr + low C + Mo
Strength above classic 310S Wall-dependent 84/39 or 78/37 ksi + N 0.10–0.16
Nb-stabilized H-grade duty Not MoLN — open TP310HCb / TP310HCbN

Weldability

TP310MoLN welds with austenitic practices using matching or near-matching 310MoLN / 25-22-2 Mo fillers selected for the joint design and process fluid. The ≤0.025% carbon ceiling improves as-welded IGC resistance relative to standard-carbon 310, but heat input control, interpass limits, and post-weld cleaning remain the fabricator’s responsibility under the applicable code.

For tube-to-tubesheet and coil welding, keep filler Mo and N aligned with the base-metal windows and confirm any project restriction on ferrite or residual elements. When the datasheet demands niobium stabilization rather than L-carbon Mo+N, do not “solve” that with filler alone — specify the Cb / HCb / HCbN grade that matches the stabilization story. Repair welding, when permitted, follows A1016/A1016M as invoked by A213.

Surface Finishes

Standard delivery for ASTM A213 TP310MoLN from SHH STEEL is solution annealed and pickled, with a clean ID/OD suitable for process exchanger fabrication. Bright annealed or polished finishes are available by agreement when the process side needs lower roughness.

State finish expectations on the enquiry together with OD × wall, wall class for Table 4, and end preparation. Do not assume a bright finish from a generic “stainless tube” line item — pickled anneal is the default HX path unless the purchase order says otherwise.

Inspection and Testing

Lot testing for ASTM A213 TP310MoLN follows tension, hardness, flattening, and flaring under A213 / A1016. Chemistry verification must include carbon ≤0.025%, molybdenum 2.00–3.00%, and nitrogen 0.10–0.16%. Tension results must identify which Table 4 wall class (≤0.25 in. or >0.25 in.) applies to the ordered tube. NDE follows the ordered edition and purchaser supplements.

EN 10204 3.1 certificates from SHH STEEL report ladle chemistry with Mo and N, the correct wall-class Table 4 tensile and hardness, and heat-treatment condition per the ordered edition. When A262 Practice E is ordered, those results appear as specified. Dual A213/SA-213 marking and third-party witness are available when written into the enquiry. A certificate missing Mo, N, or wall-class tensile identity is not a complete TP310MoLN release package.

Packaging and Shipping

TP310MoLN tubes ship in capped or plugged bundles with weather protection matched to the route. Cut lengths for exchanger and stripper bundles are labeled by heat and size; export packing uses cases or steel-frame crates when required.

Marking includes ASTM A213, grade TP310MoLN / UNS S31050, size, heat number, and SHH STEEL identification. Dual SA-213 marking appears only when the purchase order requests it. Packing lists track the same heat numbers shown on the EN 10204 3.1 certificates.

Why Choose SHH STEEL

SHH STEEL treats ASTM A213 TP310MoLN as a distinct L+Mo+N specification product: carbon ≤0.025%, Mo 2–3%, N 0.10–0.16%, raised Ni 21–23%, tight Si/P, and the correct wall-class Table 4 floors are checked together before a heat is offered. Quotations state OD × wall / BWG, wall basis, Table 4 wall class, finish route, A262 options, nitrogen analysis expectations, and whether dual A213/SA-213 marking is required.

We refuse nickname substitutions that stamp TP310S or TP316LN as MoLN without the missing chemistry and tensile controls. EN 10204 3.1 documentation includes Mo, N, and wall-class tensile identity. Compare sisters on the A213/A213M hub before freezing the process tube list.

Supply Capability

SHH STEEL supplies ASTM A213 TP310MoLN seamless stainless steel tube in cold-finished and hot-finished routes across the usual heat-exchanger and process OD × wall / BWG band. Capability below is an enquiry range — not a frozen warehouse SKU or tonnage claim.

Capability SHH STEEL practice for TP310MoLN
Product form Seamless cold-finished and hot-finished tube
Standards ASTM A213 / A213M; dual SA-213 when PO asks
Size band Typical within ~1/8 in. ID to 5 in. OD; other diameters by agreement
Wall basis Minimum wall or average wall as specified; name wall for Table 4 class
Documentation EN 10204 3.1 MTC with Mo + N + wall-class tensile; A262 / third-party witness on request
Trade terms FOB / CFR / CIF / EXW and other agreed Incoterms

Stock / Available sizes

SHH STEEL quotes TP310MoLN against a stock-and-mill enquiry range rather than a frozen SKU/tonnage list. Representative OD × wall / BWG combinations for process and heat-exchanger tube appear below.

Item Typical stock / enquiry range for TP310MoLN
Outside diameter 19.05, 25.4, 31.8, 38.1, 42.4, 50.8, 60.3, 76.2 mm (and other HX/process ODs on enquiry; through the usual A213 ~5 in. [127 mm] band)
Wall / BWG BWG 10–18 class walls and metric min-wall equivalents; note ≤6 mm vs >6 mm for Table 4; heavier walls by agreement
Common OD × wall examples 25.4 × 2.11 mm; 31.8 × 2.77 mm; 38.1 × 2.77 mm; 42.4 × 3.56 mm; 50.8 × 3.05 mm; 60.3 × 5.54 mm — illustrative, confirm min vs average wall and Table 4 class
Length Cut lengths for exchanger / stripper bundles; bends and random mill lengths on enquiry
Special Non-standard OD/wall, bright anneal, dual A213/SA-213, A262 Practice E, agreed N analysis method, third-party witness — confirm before heat reservation

Send OD × wall (or BWG), wall basis, finish route, quantity or cut list, marking (A213 or dual A213/SA-213), and A262 / N-method notes on one enquiry. We confirm C ≤0.025%, Mo 2.00–3.00%, N 0.10–0.16%, Cr 24–26% / Ni 21–23%, and the correct wall-class Table 4 floors without inventing fake warehouse codes. Sisters A213 TP310S, A213 TP310MoCbN, and A213 TP316LN sit on the same hub.

FAQ

Is ASTM A213 the same as ASME SA-213 for TP310MoLN?
No. ASTM A213 / A213M is the ASTM International product specification for seamless boiler, superheater, and heat-exchanger tubes; ASME SA-213 / SA-213M is the separate ASME Code Book adoption. Dual-mark only when the purchase order asks for both names on the stencil and MTC. Chemistry and tensile rules align closely for a given referenced edition, but the standards remain independent documents.
Does ASTM A213 TP310MoLN include welded or HCW tube?
No. ASTM A213 covers seamless boiler, superheater, and heat-exchanger tubes only. There is no WLD or HCW manufacturing-type letter under A213. Cold-finished versus hot-finished describes the seamless process route and dimensional tolerances — not a welded product form. Order welded stainless pipe under a different product standard when that form is required.
What is the chemistry of ASTM A213 TP310MoLN?
Melting analysis for TP310MoLN / UNS S31050 is C ≤0.025%, Mn ≤2.00%, P ≤0.020%, S ≤0.030%, Si ≤0.40%, Cr 24.0–26.0%, Ni 21.0–23.0%, Mo 2.00–3.00%, and N 0.10–0.16%, with Nb as a no-requirement ellipsis. Confirm the ordered A213 edition. Carbon, molybdenum, and nitrogen are all mandatory — none is optional on a MoLN heat.
TP310MoLN vs TP310S — what does MoLN add?
Both grades share the 24–26% chromium band, but TP310S uses Ni 19–22%, C ≤0.08%, and no Mo or N requirement, with Table 4 at 75/30 ksi. TP310MoLN raises Ni to 21–23%, caps C at ≤0.025%, adds Mo 2–3% and N 0.10–0.16%, tightens Si and P, and uses wall-dependent tensile floors of 84/39 or 78/37 ksi. Order MoLN when L-carbon Mo+N chemistry is on the datasheet — not as a nickname for 310S.
TP310MoLN vs TP316LN — are they interchangeable?
No. Both carry Mo 2–3% and N 0.10–0.16% with low carbon, but Cr–Ni windows differ sharply: TP310MoLN is 24–26 / 21–23 while TP316LN is 16–18 / 10–13. Tensile tables and intended oxidizing-service framing also differ. Order the grade named on the datasheet rather than swapping on overlapping Mo/N bands alone.
Why does Table 4 have two tensile rows for TP310MoLN?
A213 Table 4 sets higher floors for thinner wall (≤0.25 in. [6 mm]: 84/39 ksi) and slightly lower floors for thicker wall (>0.25 in. [6 mm]: 78/37 ksi), with 25% elongation and hardness max 217 HBW / 95 HRB on both. Name the ordered wall on the enquiry so the mill applies the correct row on the MTC — a single tensile number without wall-class identity is incomplete for MoLN.
What heat treatment does A213 require for TP310MoLN?
Solution treatment with water quench or other rapid cool is required for austenitic A213 tube. The A213–13 PDF excerpt used for this pack does not print a dedicated S31050 temperature line in Table 3 between S31042 and S31060 — confirm the ordered edition’s Table 3 row before freezing anneal temperature or grain-size language on the purchase order. Delivery is solution annealed and pickled unless bright anneal is agreed.
Does TP310MoLN require ASTM grain size No. 7?
Not from the A213–13 Table 3 excerpt used here, which omits a dedicated S31050 heat-treatment row and therefore does not print a grain-size column entry for this grade. Do not invent an H-grade grain-size mandate. If a project datasheet asks for an E112 report on MoLN, put that supplementary requirement on the purchase order and confirm against the ordered edition.
Minimum wall vs average wall for A213 TP310MoLN — which should I specify?
Process and heat-exchanger datasheets almost always expect minimum wall. Average wall is allowed when the purchase order says so, with A1016/A1016M tolerances for that basis. Also name the nominal wall so the correct Table 4 wall class (≤6 mm vs >6 mm) is applied. State both on the enquiry rather than relying on pipe schedule numbers.
Is TP310MoLN suitable for urea stripper service?
It is one of the A213 grades commonly considered for urea-related and highly oxidizing process exchangers because of C ≤0.025%, Mo 2–3%, and 24–26 / 21–23 Cr–Ni. Final selection remains engineering judgment against fluid, temperature, velocity, and the project specification — ASTM A213 does not publish a urea-service approval table. Put any required corrosion test on the purchase order.
Does Table 4 set a hardness limit for TP310MoLN?
Yes. Table 4 lists hardness maximum 217 HBW or 95 HRB for both wall classes, together with the wall-dependent tensile and 25% elongation floors. Hardness and the correct wall-class tensile result both belong on the release package — neither replaces molybdenum and nitrogen chemistry for MoLN acceptance.

Conclusion

ASTM A213 TP310MoLN / UNS S31050 is the low-carbon molybdenum-nitrogen 24–26% Cr / 21–23% Ni seamless stainless steel tube for process and heat-exchanger service when L-grade carbon, Mo 2–3%, N 0.10–0.16%, and wall-dependent tensile floors must travel together on a raised nickel window. SHH STEEL supplies cold-finished and hot-finished seamless tube in the usual OD × wall / BWG band, solution annealed per the ordered edition, tested to the correct Table 4 wall-class floors and hardness limits, with molybdenum and nitrogen reported on EN 10204 3.1 certificates — dual SA-213 marking only when the purchase order asks.

Contact: admin@steelspecs.com

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X