ASTM A213 UNS S31277 Stainless Steel Tube | ASTM A213 Stainless Steel - SHH STEEL

ASTM A213 UNS S31277 Stainless Steel Tube

ASTM A213 UNS S31277 (27-7MO class — Footnote C, no TP letter) seamless boiler, superheater and heat-exchanger tube with C ≤0.020%, Cr 20.5–23.0%, Ni 26.0–28.0%, Mo 6.5–8.0%, N 0.30–0.40%, Cu 0.50–1.50%, Table 4 floors of 112/52 ksi, hardness max 241 HBW / 100 HRB, and 2050 °F [1120 °C] solution anneal. SHH STEEL supplies cold-finished and hot-finished seamless tube with EN 10204 3.1 MTCs.
Grade
UNS S31277 (no TP letter — 27-7MO class high-Mo/N austenitic)
Standard
ASTM A213 / A213M
Product form
Seamless boiler / superheater / heat-exchanger tube (cold-finished and hot-finished)
Size
Typical OD × min wall (or average wall) within ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD and ~0.015–0.500 in. [0.4–12.7 mm] wall; other diameters by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is ASTM A213 UNS S31277 Stainless Steel Tube

ASTM A213 / A213M lists UNS S31277 among the austenitic stainless grades that carry no common TP letter — Footnote C states the UNS number uniquely identifies the alloy. It sits above classic 6Mo chemistry: carbon ≤0.020%, manganese ≤3.00%, chromium 20.5–23.0%, nickel 26.0–28.0%, molybdenum 6.5–8.0%, nitrogen 0.30–0.40%, and copper 0.50–1.50%. Commercially buyers know it as 27-7MO / Alloy 27-7MO class tube chemistry; those shop names still need ASTM A213 (or the separate ASME SA-213 adoption) on the purchase order so seamless-tube minimum-wall, test, and marking clauses apply.

SHH STEEL can supply ASTM A213 UNS S31277 stainless steel tube as seamless cold-finished and hot-finished product in the usual boiler and heat-exchanger OD × wall / BWG band, shipped with EN 10204 3.1 mill test certificates that report the full Mo–N–Cu–Ni set and the Table 4 tensile and hardness results (112 ksi [770 MPa] / 52 ksi [360 MPa], hardness max 241 HBW / 100 HRB). Dual A213 / SA-213 marking is available only when the purchase order asks for both independent standards. Browse high-alloy austenitic sisters on the A213/A213M hub.

Do not paste an S31254 (254 SMO) chemistry block onto an S31277 certificate — nickel jumps to 26–28%, molybdenum opens to 6.5–8.0%, nitrogen climbs to 0.30–0.40%, and Table 4 tensile is 112/52 ksi rather than the wall-split 98/95 pattern of S31254. Sister grades under the same ASTM standard include A213 UNS S31254, A213 TP317LMN, A213 TP310MoLN, A213 TP316L, and A213 TPXM-19. A213 covers seamless tube only — cold-finished versus hot-finished is the process choice, not a WLD/HCW manufacturing type.

Chemical Composition of A213 UNS S31277

UNS S31277 chemistry is a high-PREN, high-nickel super-austenitic window: chromium 20.5–23.0%, nickel 26.0–28.0%, molybdenum 6.5–8.0%, nitrogen held high at 0.30–0.40%, copper 0.50–1.50%, and manganese allowed up to 3.00%. Carbon stays ≤0.020%. Melting analysis is mandatory; product analysis applies only when ordered through A1016 / A480 A1.1. Phosphorus ≤0.030% and sulfur ≤0.010% match the tight residual style of neighboring 6Mo rows. There is no TP grade letter — order and mark by UNS S31277 (Footnote C). Nitrogen analysis method is by agreement (Footnote B).

The tables below reproduce the melt limits from the public A213 stainless chemistry table, product-analysis limits from A480 Table A1.1 practice, and a short snapshot against S31254 / TP317LMN. Confirm the ordered edition before treating secondary catalogues as acceptance text. UNCERTAIN: A480 product-tolerance digits for Mo 6.5–8.0, N 0.30–0.40, Cu 0.50–1.50, and Mn ≤3.00 are applied from sister high-Mo / high-N austenitic practice — confirm the A480 edition if product analysis is contractual.

Melting analysis (heat / ladle analysis)

Element UNS S31277 melting analysis
Carbon (C) ≤ 0.020
Manganese (Mn) ≤ 3.00
Phosphorus (P) ≤ 0.030
Sulfur (S) ≤ 0.010
Silicon (Si) ≤ 0.50
Chromium (Cr) 20.5 – 23.0
Nickel (Ni) 26.0 – 28.0
Molybdenum (Mo) 6.5 – 8.0
Nitrogen (N) 0.30 – 0.40
Copper (Cu) 0.50 – 1.50
Niobium (Nb) … (no requirement)
Titanium (Ti) … (no requirement)

Source: ASTM A213/A213M stainless chemistry table for UNS S31277 (public htpipe A213 PDF excerpt — _ref_a213.txt A213/A213M − 13). Molybdenum 6.5–8.0%, nitrogen 0.30–0.40%, and nickel 26.0–28.0% must all appear on the certificate; an MTC that only shows “27-7MO nickname chemistry” without the A213 ranges is incomplete.

Product analysis — A480/A480M Table A1.1 tolerances applied

Element Melting Tolerance (A480 A1.1) Product analysis limit
Carbon (C) ≤ 0.020 0.005 over ≤ 0.025
Manganese (Mn) ≤ 3.00 0.04 over (UNCERTAIN) ≤ 3.04
Phosphorus (P) ≤ 0.030 0.005 over ≤ 0.035
Sulfur (S) ≤ 0.010 0.005 over ≤ 0.015
Silicon (Si) ≤ 0.50 0.05 over ≤ 0.55
Chromium (Cr) 20.5 – 23.0 0.25 under / over 20.25 – 23.25
Nickel (Ni) 26.0 – 28.0 0.15 under / 0.20 over (UNCERTAIN for 26–28 band) 25.85 – 28.20
Molybdenum (Mo) 6.5 – 8.0 0.10 under / over (UNCERTAIN) 6.40 – 8.10
Nitrogen (N) 0.30 – 0.40 0.01 under / 0.02 over (UNCERTAIN at this N level) 0.29 – 0.42
Copper (Cu) 0.50 – 1.50 0.03 under / over (UNCERTAIN) 0.47 – 1.53

Reading note: product analysis is not automatic — invoke it on the purchase order. High-Mo / high-N / high-Ni product digits above are sister-practice working values labeled UNCERTAIN until the ordered A480 edition is checked.

Mo / N / Ni snapshot — TP317LMN / S31254 / S31277

Element TP317LMN (S31726) UNS S31254 UNS S31277
C ≤ 0.03 ≤ 0.020 ≤ 0.020
Cr 17.0 – 20.0 19.5 – 20.5 20.5 – 23.0
Ni 13.5 – 17.5 17.5 – 18.5 26.0 – 28.0
Mo 4.0 – 5.0 6.0 – 6.5 6.5 – 8.0
N 0.10 – 0.20 0.18 – 0.22 0.30 – 0.40
Cu ≤ 0.75 0.50 – 1.00 0.50 – 1.50

S31277 is the step above S31254 when nickel, molybdenum, and nitrogen must all move together — not a relabel of 254 SMO chemistry with a higher tensile hope.

Mechanical Properties of A213 UNS S31277

Table 4 for UNS S31277 sets one of the highest austenitic tensile pairs in the A213 stainless list: 112 ksi [770 MPa] tensile and 52 ksi [360 MPa] yield, with 40% elongation and hardness max 241 HBW / 100 HRB. That strength level tracks the high nitrogen and high molybdenum design — do not apply a 75/30 or even an S31254 98/45 checklist to an S31277 lot.

Property UNS S31277 requirement
Tensile strength, min 112 ksi [770 MPa]
Yield strength (0.2% offset), min 52 ksi [360 MPa]
Elongation in 2 in. or 50 mm, min 40%
Hardness, max 241 HBW or 100 HRB

Source: ASTM A213/A213M Table 4 for UNS S31277 (public A213–13 excerpt). Mechanical property requirements generally do not apply to tubing smaller than 1/8 in. [3.2 mm] inside diameter or thinner than 0.015 in. [0.4 mm] wall. Flattening and flaring tests remain lot requirements under A213.

Hardness max 241 HBW / 100 HRB is well above the 192 HBW / 90 HRB commodity ceiling and above S31254’s 220 HBW / 96 HRB. A tensile-only MTC that omits nitrogen or reports a soft 90 HRB-only template is incomplete documentation practice for this grade.

Dimensions and Tolerances

Dimensional supply for ASTM A213 UNS S31277 remains tube language — OD × min wall (or average wall) and BWG / gauge — covering severe chloride coolers and chemical heat-exchanger sizes rather than leading with ASME B36.19 pipe schedules. Usual A213 sizes run from about 1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD with min wall about 0.015–0.500 in. [0.4–12.7 mm]; other diameters by agreement. High-alloy cold work can make thin-wall drawing more demanding — confirm mill capability for the exact OD × wall early.

OD and wall variations follow ASTM A1016/A1016M as invoked by A213. Cold-finished tubes commonly hold tighter OD; hot-finished tubes allow wider windows. Put “min wall” or “average wall” on the purchase order rather than assuming the mill will guess from a BWG number alone.

Length is ordered as specific cut lengths for exchanger bundles or as random mill lengths. End finish follows the fabrication drawing. B36.19 schedule references may appear only as a secondary commercial size hint — they are not the primary A213 size story for S31277 HX tube.

Equivalent Grades

Equivalence language around S31277 tube often collapses “27-7MO” and “Alloy 27-7MO” nicknames across plate, bar, and tube product forms. ASTM A213 UNS S31277 is the governing designation for this article; commercial 27-7MO aliases point to similar high-Mo/N chemistry families but are not automatic substitutes on an A213 MTC without matching the seamless-tube standard clauses.

Designation Notes
ASTM A213 / A213M UNS S31277 Governing ASTM seamless boiler / HX tube product standard — no TP letter (Footnote C)
UNS S31277 Unified number that uniquely identifies the alloy
27-7MO / Alloy 27-7MO (commercial) Shop names for high-Mo / high-N / high-Ni austenitic chemistry — do not replace A213 product marking
Near 6Mo sisters (not substitutes) S31254 / N08926-class chemistries are related PREN stories with different Ni–Mo–N–tensile packages
ASME SA-213 UNS S31277 Separate Code Book adoption — dual-mark only when the PO asks

Compare A213 UNS S31254 and A213 TP317LMN on the A213/A213M hub before deciding whether the datasheet truly needs the 26–28% Ni / 6.5–8.0% Mo step. Plate chemistry under A240 is a related alloy story, not an automatic tube MTC substitute.

Heat Treatment and Delivery Condition

UNS S31277 under ASTM A213 is furnished solution treated at a minimum of 2050 °F [1120 °C], then quenched in water or cooled rapidly by other means. That anneal sits between the 2100 °F S31254 floor and the 1900 °F commodity austenitic minimum — do not apply a generic 1900 °F stamp to an S31277 heat. Public Table 3 does not print a mandatory grain-size number for this grade (ellipsis).

Cold-finished versus hot-finished is a process and dimensional route, not a second product standard. Both routes still require the 2050 °F solution treatment on finished tube. Bright anneal may be agreed commercially when surface appearance matters, but it does not replace the Table 3 temperature floor unless the ordered edition and purchase order say so.

UNCERTAIN: public Table 3 OCR places a Footnote F marker near the S31277 heat-treatment row. Confirm ordered-edition footnote attachment — if Footnote F applies, quench capability must be sufficient to prevent carbide re-precipitation as demonstrable by A262 Practice E capability, and the manufacturer need not run the test unless the purchase order specifies it (Supplementary Requirement S4).

Corrosion Resistance

S31277’s corrosion story is aggressive-chloride and severe seawater PREN performance from Mo 6.5–8.0% / N 0.30–0.40% / Ni 26–28% / Cu 0.50–1.50%, stepping above classic 6Mo (S31254) when the process side outgrows the 6.0–6.5% Mo / 17.5–18.5% Ni window. It is selected for the harshest chloride coolers and chemical condensers in the A213 austenitic stainless set — not for high-temperature oxidation framing and not as a fancy relabel of TP316L.

Intergranular corrosion risk after welding stays low relative to higher-carbon austenitics because carbon is capped at ≤0.020%, but heat input control and post-weld cleaning still matter in chloride service. When the datasheet demands demonstrated IGC capability, order A262 Practice E explicitly. If the duty only needs classic 6Mo, prefer A213 UNS S31254 rather than over-specifying S31277.

Applications of A213 UNS S31277 Tube

Buyers specify ASTM A213 UNS S31277 when heat-exchanger duty needs a step above 254 SMO / 6Mo chemistry — higher nickel, higher molybdenum, and higher nitrogen together — with the matching 112/52 ksi Table 4 pair. Typical placements include severe seawater and chloride process coolers, aggressive chemical condensers, and scrubber exchangers where S31254 PREN margin is no longer enough.

Service theme Why S31277 is considered
Severe seawater / chloride coolers Mo 6.5–8.0% + N 0.30–0.40% + Ni 26–28%
Aggressive chemical condensers Cu 0.50–1.50% with high-Mo/N austenitic balance
Upgrade from S31254 lists When datasheets outgrow 6.0–6.5% Mo / 17.5–18.5% Ni
High-strength HX tube Table 4 112/52 ksi with 40% elongation

If the duty is furnace oxidation rather than wet chloride PREN, look at 310-family pages such as A213 TP310S instead of forcing S31277 into a radiant-tube narrative.

Weldability

S31277 tube welds with high-alloy austenitic / nickel-base practices using matching or over-alloyed fillers selected for the high Mo–N–Ni base and chloride service. The ≤0.020% carbon ceiling reduces sensitization risk; heat input control, interpass temperature, and thorough post-weld cleaning still matter. Do not assume ER316L or even a standard 6Mo filler automatically restores 6.5–8.0% Mo / 0.30–0.40% N performance without a qualified WPS review.

For tube-to-tubesheet welding into matching or higher-alloy sheets, keep filler PREN at or above the base metal and confirm any project restriction on ferrite or residual copper. When the datasheet demands A262 Practice E on welded samples, state that on the purchase order.

Surface Finishes

Standard delivery for ASTM A213 UNS S31277 from SHH STEEL is solution annealed and pickled, with a clean ID/OD suitable for severe chloride cooler and chemical exchanger fabrication. Bright annealed or polished finishes are available by agreement when the process side needs lower roughness or a brighter appearance.

State finish expectations on the enquiry together with OD × wall and end preparation. Do not assume a bright finish from a generic “27-7MO tube” line item — pickled anneal after the 2050 °F solution treatment is the default path unless the purchase order says otherwise.

Inspection and Testing

Lot testing for ASTM A213 UNS S31277 follows the tension, hardness, flattening, and flaring requirements of A213 together with A1016/A1016M. Chemistry is verified on the heat (and on product when ordered) — molybdenum 6.5–8.0%, nitrogen 0.30–0.40%, nickel 26.0–28.0%, and copper 0.50–1.50% must all clear. Non-destructive examination follows the ordered edition and any purchaser supplementary requirements.

EN 10204 3.1 mill test certificates from SHH STEEL report ladle chemistry, Table 4 tensile and hardness results (112/52 ksi; 241 HBW / 100 HRB), heat-treatment condition at ≥2050 °F [1120 °C], and dimensions. Ask for A262 Practice E on the PO when IGC capability must be demonstrated by actual test. Third-party witness and dual A213/SA-213 marking are available when specified.

Packaging and Shipping

S31277 tubes ship in capped or plugged bundles with weather protection suited to the destination and transport mode. Cut lengths for cooler and exchanger bundles are labeled by heat and size; export packing uses wooden cases or steel-frame crates when the route requires them.

Marking includes ASTM A213, UNS S31277, size, heat number, and SHH STEEL identification. Dual SA-213 marking appears only when the purchase order requests it. Packing lists reference the same heat numbers shown on the EN 10204 3.1 certificates.

Why Choose SHH STEEL

SHH STEEL treats ASTM A213 UNS S31277 as a specification high-Mo/N product: C ≤0.020%, Mo 6.5–8.0%, N 0.30–0.40%, Ni 26.0–28.0%, Cu 0.50–1.50%, Table 4 112/52 ksi, hardness max 241 HBW / 100 HRB, and the 2050 °F solution anneal are checked together before a heat is offered. Quotations state OD × wall / BWG, wall basis, finish route, A262 options, and whether dual A213/SA-213 marking is required.

We refuse nickname assemblies that stamp S31254 / 254 SMO chemistry onto an S31277 line item without clearing the higher Ni–Mo–N bands and 112/52 tensile pair, or that copy a 75/30 checklist onto this grade. EN 10204 3.1 documentation includes Mo, N, Ni, and Cu together. Compare sisters on the A213/A213M hub before freezing the cooler tube list.

Supply Capability

SHH STEEL supplies ASTM A213 UNS S31277 seamless stainless steel tube against purchase-order chemistry, mechanical, and dimensional requirements — cold-finished or hot-finished — with EN 10204 3.1 mill test certificates. The capability table below summarizes the enquiry window; it is not a frozen warehouse SKU list.

Capability SHH STEEL supply window for UNS S31277
Product form Seamless cold-finished / hot-finished boiler, superheater, and heat-exchanger tube
Grade / marking ASTM A213 UNS S31277; dual A213/SA-213 only when PO asks
Size band Typical OD × min wall (or average wall) within the A213 ~1/8 in. ID to 5 in. OD / 0.015–0.500 in. wall window; other diameters by agreement
Documentation EN 10204 3.1 MTC with Mo–N–Ni–Cu chemistry and Table 4 112/52 ksi tensile/hardness
Testing options A262 Practice E, PMI, third-party witness, supplementary NDE per PO
Trade terms FOB / CFR / CIF / EXW and other agreed Incoterms

Stock / Available sizes

SHH STEEL quotes S31277 against a stock-and-mill enquiry range rather than a frozen SKU/tonnage list. Representative OD × wall / BWG combinations for severe chloride cooler and chemical heat-exchanger tube appear below.

Item Typical stock / enquiry range for UNS S31277
Outside diameter 15.88, 19.05, 25.4, 31.8, 38.1, 42.4, 50.8 mm (and other HX ODs on enquiry; through the usual A213 ~5 in. [127 mm] band)
Wall / BWG BWG 12–18 class walls and metric min-wall equivalents; heavier walls by agreement
Common OD × wall examples 19.05 × 1.65 mm; 25.4 × 2.11 mm; 31.8 × 2.11 mm; 38.1 × 2.77 mm — illustrative, confirm min vs average wall
Length Cut lengths for cooler / exchanger bundles; U-bends and random mill lengths on enquiry
Special Non-standard OD/wall, bright anneal, dual A213/SA-213, A262 Practice E, third-party witness — confirm before heat reservation

Send OD × wall (or BWG), wall basis (min or average), finish route, quantity or cut list, marking (A213 or dual A213/SA-213), and any A262 / NDE extras with the enquiry so the high Mo–N–Ni chemistry and 2050 °F anneal path are reserved with the heat.

FAQ

Is ASTM A213 the same as ASME SA-213 for UNS S31277?
No. ASTM A213 / A213M is the ASTM International product specification for seamless boiler, superheater, and heat-exchanger tubes; ASME SA-213 / SA-213M is the separate ASME Code Book adoption. Dual-mark only when the purchase order asks for both names on the stencil and MTC. Chemistry and tensile floors align closely for a given referenced edition, but the standards remain independent.
Why does S31277 have no TP letter under A213?
Footnote C in the A213 stainless chemistry table states that for these alloys there is no common grade designation and the UNS number uniquely identifies them. Order, mark, and certify as UNS S31277 rather than inventing a TP27-7 or similar letter code on the stencil. Commercial nicknames such as 27-7MO remain useful shop language but do not replace the UNS product marking.
What is the chemistry of ASTM A213 UNS S31277?
Public A213 melt limits for S31277 are C ≤0.020%, Mn ≤3.00%, P ≤0.030%, S ≤0.010%, Si ≤0.50%, Cr 20.5–23.0%, Ni 26.0–28.0%, Mo 6.5–8.0%, N 0.30–0.40%, and Cu 0.50–1.50%. Nitrogen analysis method is by agreement (Footnote B). Confirm the ordered A213/A213M edition before treating catalogue reprints as acceptance text.
S31277 vs S31254 — which 6Mo-class A213 tube should I order?
S31254 is classic 6Mo / 254 SMO chemistry (Mo 6.0–6.5%, Ni 17.5–18.5%, N 0.18–0.22%, wall-split 98/95 ksi). S31277 raises Mo to 6.5–8.0%, Ni to 26–28%, N to 0.30–0.40%, and tensile to 112/52 ksi. Choose S31277 when the process side outgrows S31254; keep S31254 when the datasheet is written around classic 6Mo.
Is 27-7MO the same as ASTM A213 UNS S31277?
27-7MO / Alloy 27-7MO is a commercial shop name for high-Mo / high-N / high-Ni austenitic chemistry in the S31277 family. It is useful language on drawings and RFQs, but the governing ASTM seamless-tube product designation for this page is ASTM A213 UNS S31277. Always put A213 (and SA-213 only if Code dual-mark is required) on the purchase order.
What tensile and hardness floors does Table 4 set for S31277?
Tensile min 112 ksi [770 MPa], yield min 52 ksi [360 MPa], elongation min 40%, hardness max 241 HBW or 100 HRB. That pair is among the highest austenitic floors in A213 — do not accept a 75/30 or 98/45 checklist as a substitute for the S31277 row.
What heat treatment does A213 require for UNS S31277?
Solution treatment at a minimum of 2050 °F [1120 °C] followed by water quench or other rapid cool. Confirm whether Footnote F attaches to this row in the ordered edition; if it does, quench capability and optional A262 Practice E (S4) language follow the edition text. No mandatory grain-size number is printed for this row in the public Table 3 excerpt.
Does ASTM A213 UNS S31277 include welded or HCW tube?
No. ASTM A213 covers seamless boiler, superheater, and heat-exchanger tubes only. Cold-finished versus hot-finished is the process choice inside seamless manufacture. Welded or HCW product forms belong under other ASTM stainless tubular standards, not under an A213 S31277 line item.
Minimum wall vs average wall for A213 S31277 — which should I specify?
A213 treats minimum wall as the default ordering basis unless the purchase order specifies average wall. Heat-exchanger datasheets almost always assume minimum wall. Write “min wall” or “average wall” explicitly on the PO rather than leaving the mill to infer intent from a BWG number alone.
Can you dual-certify A213 and SA-213 UNS S31277?
Yes, when the purchase order asks for both independent standards on the stencil and MTC. ASTM A213 and ASME SA-213 remain separate documents; dual marking is a commercial/documentation choice, not an automatic merge of the two names into one title. SHH STEEL will not put SA-213 in the H1 or SEO title of the product page — that stays ASTM A213.
S31277 vs TP317LMN — is the 4–5% Mo grade enough?
TP317LMN (Mo 4.0–5.0%, N 0.10–0.20%, Ni 13.5–17.5%) is a strong nitrogen-bearing 317 step but sits well below S31277’s Mo 6.5–8.0% / N 0.30–0.40% / Ni 26–28% window and 112/52 ksi tensile. Use TP317LMN when the datasheet is written around that family; move to S31277 (or S31254) when PREN and nickel must climb further.

Conclusion

ASTM A213 UNS S31277 is the high-Mo / high-N / high-Ni seamless stainless steel tube grade for severe chloride coolers and chemical heat-exchanger service when Mo 6.5–8.0%, N 0.30–0.40%, and Ni 26.0–28.0% — not classic 6Mo or 317LMN checklists — drive grade selection. SHH STEEL supplies cold-finished and hot-finished seamless tube in the usual OD × wall / BWG band, solution annealed at 2050 °F [1120 °C], tested to Table 4 112/52 ksi and hardness limits, and documented on EN 10204 3.1 certificates — with dual SA-213 marking only when the purchase order asks.

Contact: admin@steelspecs.com

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X