ASTM A213 TP316Ti Stainless Steel Tube | ASTM A213 Stainless Steel - SHH STEEL

ASTM A213 TP316Ti Stainless Steel Tube

ASTM A213 TP316Ti / UNS S31635 titanium-stabilized molybdenum seamless boiler, superheater and heat-exchanger tube — C ≤0.08%, Si ≤0.75%, Cr 16.0–18.0%, Ni 10.0–14.0%, Mo 2.00–3.00%, N ≤0.10%, Ti ≥5×(C+N) to 0.70% max, Table 4 75/30 ksi, hardness max 192 HBW / 90 HRB, 1900 °F solution anneal. SHH STEEL supplies cold-finished and hot-finished seamless tube with EN 10204 3.1 MTCs that report titanium and molybdenum.
Grade
TP316Ti / UNS S31635
Standard
ASTM A213 / A213M
Product form
Seamless boiler / superheater / heat-exchanger tube (cold-finished and hot-finished)
Size
Typical OD × min wall (or average wall) within ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD and ~0.015–0.500 in. [0.4–12.7 mm] wall; other diameters by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is ASTM A213 TP316Ti Stainless Steel Tube

ASTM A213 / A213M covers seamless ferritic and austenitic alloy-steel boiler, superheater, and heat-exchanger tubes. Grade TP316Ti / UNS S31635 is the titanium-stabilized member of the molybdenum-bearing 316 family: melting carbon is capped at 0.08%, silicon at a tighter 0.75% ceiling, chromium 16.0–18.0%, nickel 10.0–14.0%, molybdenum 2.00–3.00%, nitrogen at 0.10% maximum, and titanium held to a formula minimum of five times (C + N) with a 0.70% absolute ceiling. That titanium rule is the reason the grade exists — it ties free carbon (and nitrogen) as titanium carbides/nitrides so grain-boundary chromium carbides are less likely to form during slow cooling or repeated thermal exposure, while molybdenum still does the pitting work that plain A213 TP321 cannot claim.

SHH STEEL can supply ASTM A213 TP316Ti stainless steel tube as seamless cold-finished and hot-finished product in the usual boiler and heat-exchanger OD × wall / BWG band, shipped with EN 10204 3.1 mill test certificates that report the full ladle chemistry — titanium and molybdenum both visible — plus the Table 4 tensile and hardness results. When a project also needs ASME Code Book marking, we dual-mark A213 / SA-213 on the same lengths only if the purchase order says so. Browse the grade family on the A213/A213M hub.

Commercially, TP316Ti tube is still called 316Ti, S31635, or Ti-stabilized Mo HX tube; none of those shop names replace the ASTM grade on the MTC or stencil. Sister grades under the same ASTM standard include A213 TP316, A213 TP316L, A213 TP316H, A213 TP321, and A213 TP317. A213 covers seamless tube only — no welded or HCW manufacturing type — so cold-finished versus hot-finished is the process choice, not a WLD/HCW stencil letter.

Chemical Composition of A213 TP316Ti

Two chemistry layers matter for TP316Ti under ASTM A213. Melting (heat or ladle) analysis is mandatory for every heat; product analysis on finished tube applies only when Supplementary Requirement wording or the purchase order invokes it through ASTM A1016/A1016M. Product-analysis tolerances typically flow from ASTM A480/A480M Table A1.1. Three lines separate this row from ordinary 316: silicon is capped at 0.75% rather than 1.00%; nitrogen has an explicit 0.10% maximum instead of an ellipsis; and titanium must clear 5 × (C + N) while staying at or below 0.70%. Molybdenum 2.00–3.00% remains mandatory the same way it does on TP316.

The tables below reproduce the heat analysis for TP316Ti / UNS S31635, the product-analysis limits from A480 Table A1.1 practice, and a short titanium / silicon / molybdenum snapshot against TP316L and TP321. Later A213 editions place austenitic stainless grades in Table 2 (older editions used Table 1); confirm the ordered edition on the purchase order.

Melting analysis (heat / ladle analysis)

Element TP316Ti (UNS S31635) melting analysis
Carbon (C) ≤ 0.08
Manganese (Mn) ≤ 2.00
Phosphorus (P) ≤ 0.045
Sulfur (S) ≤ 0.030
Silicon (Si) ≤ 0.75
Chromium (Cr) 16.0 – 18.0
Nickel (Ni) 10.0 – 14.0
Molybdenum (Mo) 2.00 – 3.00
Nitrogen (N) ≤ 0.10
Titanium (Ti) ≥ 5 × (C + N), ≤ 0.70

Source: ASTM A213/A213M stainless chemistry table for Grade TP316Ti / UNS S31635 (public mill / specification PDF excerpt — _ref_a213.txt / A213–13 table text). Confirm the ordered edition. Nitrogen analysis method is a matter of agreement (Footnote B) when the element is reported.

Product analysis — A480/A480M Table A1.1 tolerances applied

Element Melting Tolerance (A480 A1.1) Product analysis limit
Carbon (C) ≤ 0.08 0.01 over ≤ 0.09
Manganese (Mn) ≤ 2.00 0.04 over ≤ 2.04
Phosphorus (P) ≤ 0.045 0.010 over ≤ 0.055
Sulfur (S) ≤ 0.030 0.005 over ≤ 0.035
Silicon (Si) ≤ 0.75 0.05 over ≤ 0.80
Chromium (Cr) 16.0 – 18.0 0.20 under / over 15.80 – 18.20
Nickel (Ni) 10.0 – 14.0 0.10 under / 0.15 over 9.90 – 14.15
Molybdenum (Mo) 2.00 – 3.00 0.05 under / 0.10 over 1.95 – 3.10
Nitrogen (N) ≤ 0.10 0.01 over ≤ 0.11
Titanium (Ti) ≥ 5 × (C+N), ≤ 0.70 0.05 over on max (Ti to 1.00 band practice) max ≤ 0.75 product; min tied to heat C+N

Stabilization / Mo snapshot — TP316L / TP316Ti / TP321

Element TP316L (S31603) TP316Ti (S31635) TP321 (S32100)
C ≤ 0.035 ≤ 0.08 ≤ 0.08
Si ≤ 1.00 ≤ 0.75 ≤ 1.00
Mo 2.00 – 3.00 2.00 – 3.00 … (no requirement)
N … ≤ 0.10 …
Ti … ≥ 5 × (C+N), ≤ 0.70 ≥ 5 × (C+N), ≤ 0.70

Read titanium against measured carbon and nitrogen on the same heat — a heat with C + N = 0.09% needs at least 0.45% Ti, while a leaner C + N heat can clear the formula with less titanium, still capped at 0.70%. Versus A213 TP316L, TP316Ti accepts a higher carbon ceiling because titanium does the stabilization work; versus A213 TP321, TP316Ti adds mandatory molybdenum and the tighter silicon ceiling. Dual TP316Ti/TP316L is not a meaningful path: the carbon bands and titanium requirement do not line up as a single heat story.

When product analysis is ordered, finished tube may read C ≤0.09%, Mn ≤2.04%, P ≤0.055%, S ≤0.035%, Si ≤0.80%, Cr 15.80–18.20%, Ni 9.90–14.15%, Mo 1.95–3.10%, N ≤0.11%, and Ti max ≤0.75% with the formula minimum still tied to heat C + N. Put any tighter project titanium floor or molybdenum floor on the purchase order before the heat is selected.

Mechanical Properties of A213 TP316Ti

ASTM A213 Table 4 sets the room-temperature tensile acceptance floor for TP316Ti at 75 ksi [515 MPa] tensile strength and 30 ksi [205 MPa] yield strength (0.2% offset), with elongation of 35% minimum in 2 in. or 50 mm — the same room-temperature pair as TP316 and TP321, not the lower L-grade floors. Hardness maximum is 192 HBW / 200 HV or 90 HRB. Unlike H grades, the heat-treatment table does not print a mandatory ASTM grain-size number for TP316Ti; titanium stabilization, not coarse-grain control, is the elevated-temperature differentiation this grade brings.

Property TP316Ti requirement
Tensile strength, min (Table 4) 75 ksi [515 MPa]
Yield strength (0.2% offset), min (Table 4) 30 ksi [205 MPa]
Elongation in 2 in. or 50 mm, min (Table 4) 35%
Hardness, max (Table 4) 192 HBW / 200 HV or 90 HRB
Grain size No mandatory ASTM grain-size number in the public heat-treatment table for TP316Ti

Source: ASTM A213/A213M Table 4 for TP316Ti / UNS S31635 (public specification PDF excerpt — _ref_a213.txt). Mechanical property requirements do not apply to tubing smaller than 1/8 in. [3.2 mm] inside diameter or thinner than 0.015 in. [0.4 mm] wall. Flattening and flaring tests are also required on a lot basis.

A tensile-only MTC that omits titanium or molybdenum is incomplete for TP316Ti — ask for both on the EN 10204 3.1 certificate before releasing the heat to fabrication. When a datasheet also wants H-grade carbon and grain-size controls with molybdenum, open A213 TP316H rather than stretching a Ti-stabilized heat into an H-grade story.

Dimensions and Tolerances

Dimensional supply for ASTM A213 TP316Ti is tube language — outside diameter × wall thickness (minimum wall or average wall) and, commercially, BWG / gauge — not ASME B36.19 pipe schedules as the primary size story. The sizes usually furnished under A213 run from about 1/8 in. [3.2 mm] inside diameter to 5 in. [127 mm] outside diameter, with minimum wall from about 0.015 to 0.500 in. [0.4 to 12.7 mm]; other diameters may be furnished when all other requirements are met. State on the purchase order whether wall is minimum or average — boiler and heat-exchanger datasheets almost always assume a minimum-wall reading.

Outside-diameter and wall variations follow ASTM A1016/A1016M as invoked by A213. Cold-finished tubes commonly hold tighter OD control; hot-finished tubes allow wider OD and wall windows. Permissible variations from a specified average wall for cold-finished tube are often summarized as ±10% of the specified average wall. Confirm the exact A1016 rows for the OD and finish route on the ordered edition.

Item Typical A213 TP316Ti dimensional practice
Product form Seamless only (cold-finished or hot-finished)
Usual size band ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD; wall ~0.015–0.500 in. [0.4–12.7 mm] min (or average wall if PO says so)
Wall basis Minimum wall (default for boiler / HX) or average wall when specified
OD / wall tolerances Per ASTM A1016/A1016M for the finish route and size; cold-finished average wall often ±10%
Length Cut lengths for boiler / HX bundles, or mill random lengths by agreement
Secondary size note ASME B36.19 schedules may appear only when a buyer asks for a pipe-schedule cross-reference — not as the primary A213 size callout

Put the cut list, bend radius, and end preparation on the enquiry so mill and stock lengths can be mixed efficiently. Minimum wall is a first-class A213 concept: if the datasheet assumes average wall, say so explicitly before the heat is rolled.

Equivalent Grades

Equivalence language around 316Ti tube often collapses plate, cast, and tube product forms into one nickname, or treats TP316Ti as “TP321 with molybdenum.” ASTM A213 Grade TP316Ti / UNS S31635 is the governing designation for this article; EN 1.4571 and related wrought names that point to similar Ti-stabilized Mo chemistry families are not automatic substitutes on an A213 MTC.

Designation Notes
ASTM A213 / A213M Grade TP316Ti Governing ASTM seamless boiler / HX tube product standard for this article
UNS S31635 Unified number in the stainless chemistry table
ASME SA-213 TP316Ti Separate ASME Code Book adoption — dual-mark only when the PO asks
Related Mo grade A213 TP316 — same Mo band, no Ti formula
Related L-grade A213 TP316L — C ≤0.035, no Ti
Related Ti grade A213 TP321 — Ti formula without Mo
Related plate A240 / SA240 flat product in the 316Ti family — order plate and tube under their own standards

Dual A213/SA-213 marking is a purchase-order option. Compare TP316, TP316L, and TP321 on their own ASTM A213 pages before swapping Ti-stabilized Mo tube inside a boiler or exchanger list.

Heat Treatment and Delivery Condition

TP316Ti under ASTM A213 is furnished solution treated at a minimum of 1900 °F [1040 °C], then quenched in water or cooled rapidly by other means. The public heat-treatment table does not print a mandatory ASTM grain-size number for this grade. That heat-treatment row applies to both cold-finished and hot-finished seamless tube. Skipping or under-cooling the solution treatment can leave undissolved phases or a structure that undermines the intended titanium-carbide balance even when ladle chemistry looked acceptable on paper.

Cold-finished versus hot-finished is a process and dimensional route, not a substitute for the anneal. Delivery condition for SHH STEEL TP316Ti is solution annealed and pickled (or bright annealed by agreement), with anneal temperature, quench method, molybdenum result, and titanium result on the EN 10204 3.1 certificate. Straightening, cutting, and end finishing follow heat treatment.

Stabilized grades such as TP316Ti and A213 TP321 are often discussed under Supplementary Requirement S2 stabilizing-treatment language when a purchaser wants a lower-temperature hold after the high solution anneal. Put any S2 stabilizing hold or ASTM A262 Practice E requirement on the purchase order rather than assuming base A213 includes it for every Ti heat.

Corrosion Resistance

TP316Ti inherits molybdenum’s contribution to pitting and crevice resistance from the 316 family while using titanium stabilization to reduce chromium-carbide precipitation at grain boundaries during welding or slow cooling through the sensitizing range. That is a different strategy from A213 TP316L, which simply keeps carbon low enough that there is little carbon left to precipitate. Buyers often pick TP316Ti when they want Mo plus stabilization without forcing every heat down to the L-grade carbon ceiling — especially on thicker walls or repeated thermal cycles where titanium’s gettering remains useful after fabrication.

ASTM A213 itself does not publish a corrosion-rate table for TP316Ti; selection remains engineering judgment against fluid, temperature, velocity, and inspection philosophy. When a specification calls for ASTM A262 Practice E, write that Supplementary Requirement onto the purchase order so the test is contractual rather than assumed from a verbal “full certs” note. SHH STEEL will not rank TP316Ti as equal to higher-Mo grades such as A213 TP317 in severe chlorides — that claim is not supported by the product standard.

Applications of A213 TP316Ti Tube

Because TP316Ti combines molybdenum with titanium stabilization, it shows up in heat-exchanger and process tubing where chloride-leaning fluids sit beside weld or thermal cycles that would otherwise argue for an L grade, chemical-plant condensers that historically used 316Ti plate or tube, and lists that want Mo without accepting TP316L’s lower tensile floor. The table below pairs typical application areas with a selection note so the grade is chosen for fluid, fabrication route, and stabilization strategy — not only for the familiar “316Ti” name on the BOM.

Application area Typical use of TP316Ti tube Selection note
Process heat exchangers Straight and U-bend HX tubes needing Mo + Ti stabilization State min vs average wall, BWG, and bend radius on the enquiry
Welded tube-to-tubesheet service When Ti gettering is preferred over L-grade carbon alone Still put A262 Practice E on the PO when IGC is contractual
Mo without L tensile floor When TP316L’s 70/25 ksi is too low and Ti is acceptable Confirm Ti formula vs measured C+N on MTC
Ti without molybdenum Stay on TP321 when Mo is not on the datasheet Do not treat TP316Ti as a free upgrade of TP321
Creep-range H-grade Mo Prefer TP316H when carbon floor and grain size are named TP316Ti is not an H-grade substitute

For as-welded low-carbon Mo tube without titanium open A213 TP316L; for Ti without Mo open A213 TP321; for higher molybdenum open A213 TP317 on the same A213/A213M hub.

Weldability

TP316Ti tube welds with matching or near-matching molybdenum-bearing austenitic filler for tube-to-tubesheet joints, attachment welds, and fabrication joins. Common practice uses ER316 / ER316L / ER316LSi under a qualified WPS; some fabricators prefer titanium-bearing or low-carbon deposits when the base metal’s stabilization story must carry into the weld metal. Heat input control, interpass limits, and post-weld cleaning remain the fabricator’s responsibility under the applicable boiler or pressure-vessel code — A213 governs the seamless tube product, not the field or shop weld procedure.

Because A213 TP316Ti is seamless, there is no mill longitudinal weld to radiograph the way welded pipe standards describe. Focus inspection language on tube integrity (hydro or NDE of each length), tube-to-tubesheet joint quality, and any contractual corrosion test on the base metal. Specify end preparation and surface finish on the tube PO when orbital or clean-service joins are planned. Titanium in the base metal does not automatically make every weld immune to sensitization — procedure and filler still matter.

Surface Finishes

Standard mill delivery for ASTM A213 TP316Ti is solution annealed and pickled, leaving a clean matte finish suitable for most boiler and heat-exchanger tube duty. Bright annealing under protective atmosphere produces a smoother reflective surface used on some clean-process and instrumentation tube lines and must be called out because it changes the heat-treatment route. Light polish or specified Ra on the bore or OD is a commercial or service-center operation on top of A213 product, not automatic with the grade stamp.

When a hygienic or fouling-sensitive exchanger specification quotes an Ra maximum on the bore, put it on the tube purchase order with its own acceptance language and sampling plan. SHH STEEL stencils grade and heat treatment as standard requirements; polish, special OD grind, and passivation after fabrication remain commercial extras unless the contract says otherwise. End preparation (plain, slightly beveled, or as needed for tube expanding) should be ordered together with finish so receiving inspection shares one acceptance language.

Inspection and Testing

Lot testing for ASTM A213 TP316Ti follows tension, hardness, flattening, and flaring under A213 / A1016. Chemistry verification must include the titanium formula against measured carbon and nitrogen, the 0.75% silicon ceiling, and molybdenum 2.00–3.00%. NDE follows the ordered edition and purchaser supplements — hydrostatic testing or non-destructive electric testing of each length is the usual A213 path unless the purchase order states otherwise.

EN 10204 3.1 certificates from SHH STEEL report ladle chemistry with Ti and Mo, Table 4 tensile and hardness, and heat-treatment condition. When A262 Practice E or an S2 stabilizing hold is ordered, those results appear as specified. Dual A213/SA-213 marking and third-party witness are available when written into the enquiry. A certificate missing titanium or molybdenum is not a complete TP316Ti release package.

Packaging and Shipping

TP316Ti tubes ship in capped or plugged bundles with weather protection matched to the route. Cut lengths for boiler and exchanger bundles are labeled by heat and size; export packing uses cases or steel-frame crates when required.

Marking includes ASTM A213, grade TP316Ti / UNS S31635, size, heat number, and SHH STEEL identification. Dual SA-213 marking appears only when the purchase order requests it. Packing lists track the same heat numbers shown on the EN 10204 3.1 certificates so titanium and molybdenum results stay tied to the shipped lengths.

Why Choose SHH STEEL

SHH STEEL treats ASTM A213 TP316Ti as a titanium-stabilized molybdenum specification product: Si ≤0.75%, Mo 2–3%, N ≤0.10%, Ti ≥5 × (C + N) to 0.70% max, and Table 4 75/30 ksi floors are checked together before a heat is offered. Quotations state OD × wall / BWG, wall basis, finish route, A262 / S2 options, and whether dual A213/SA-213 marking is required.

We refuse nickname assemblies that stamp TP316 or TP321 as 316Ti without the missing titanium formula, silicon ceiling, or molybdenum. EN 10204 3.1 documentation includes Ti and Mo. Compare sisters on the A213/A213M hub before freezing the exchanger tube list.

Supply Capability

SHH STEEL supplies ASTM A213 TP316Ti seamless stainless steel tube in cold-finished and hot-finished routes across the usual boiler, superheater, and heat-exchanger OD × wall / BWG band. Capability below is an enquiry range — not a frozen warehouse SKU or tonnage claim.

Capability SHH STEEL practice for TP316Ti
Product form Seamless cold-finished and hot-finished tube
Standards ASTM A213 / A213M; dual SA-213 when PO asks
Size band Typical within ~1/8 in. ID to 5 in. OD; other diameters by agreement
Wall basis Minimum wall or average wall as specified
Documentation EN 10204 3.1 MTC with Ti + Mo; A262 / S2 / third-party witness on request
Trade terms FOB / CFR / CIF / EXW and other agreed Incoterms

Stock / Available sizes

SHH STEEL quotes TP316Ti against a stock-and-mill enquiry range rather than a frozen SKU/tonnage list. Representative OD × wall / BWG combinations for boiler and heat-exchanger tube appear below.

Item Typical stock / enquiry range for TP316Ti
Outside diameter 19.05, 25.4, 31.8, 38.1, 42.4, 50.8, 60.3, 76.2 mm (and other boiler/HX ODs on enquiry; through the usual A213 ~5 in. [127 mm] band)
Wall / BWG BWG 10–18 class walls and metric min-wall equivalents; heavier walls by agreement
Common OD × wall examples 25.4 × 2.11 mm; 31.8 × 2.77 mm; 38.1 × 2.77 mm; 42.4 × 3.56 mm; 50.8 × 3.05 mm; 60.3 × 3.91 mm — illustrative, confirm min vs average wall
Length Cut lengths for boiler / exchanger bundles; bends and random mill lengths on enquiry
Special Non-standard OD/wall, bright anneal, dual A213/SA-213, A262 Practice E, S2 stabilizing hold, third-party witness — confirm before heat reservation

Send OD × wall (or BWG), wall basis, finish route, quantity or cut list, marking (A213 or dual A213/SA-213), and Ti / A262 notes on one enquiry. We confirm C ≤0.08%, Si ≤0.75%, Cr 16–18% / Ni 10–14%, Mo 2.00–3.00%, N ≤0.10%, Ti ≥5 × (C+N) ≤0.70%, and Table 4 75/30 ksi without inventing fake warehouse codes. Sisters A213 TP316, A213 TP316L, and A213 TP321 sit on the same hub.

FAQ

Is ASTM A213 the same as ASME SA-213 for TP316Ti?
No. ASTM A213 / A213M is the ASTM International product specification for seamless boiler, superheater, and heat-exchanger tubes; ASME SA-213 / SA-213M is the separate ASME Code Book adoption. Dual-mark only when the purchase order asks for both names on the stencil and MTC. Chemistry and tensile floors align closely for a given referenced edition, but the standards remain independent documents.
Does ASTM A213 TP316Ti include welded or HCW tube?
No. ASTM A213 covers seamless boiler, superheater, and heat-exchanger tubes only. There is no WLD or HCW manufacturing-type letter under A213. Cold-finished versus hot-finished describes the seamless process route and dimensional tolerances — not a welded product form. Order welded stainless pipe under a different product standard when that form is required.
What is the chemistry of ASTM A213 TP316Ti?
Melting analysis for TP316Ti / UNS S31635 is C ≤0.08%, Mn ≤2.00%, P ≤0.045%, S ≤0.030%, Si ≤0.75%, Cr 16.0–18.0%, Ni 10.0–14.0%, Mo 2.00–3.00%, N ≤0.10%, and Ti ≥5 × (C + N) with a 0.70% maximum. Confirm the ordered A213 edition. Silicon’s 0.75% ceiling, the nitrogen maximum, and the titanium formula are all mandatory — none is optional on a 316Ti heat.
TP316Ti vs TP316L — which stabilization path should I order?
TP316L keeps carbon ≤0.035% (Footnote D to 0.040% on small OD / thin wall) and carries no titanium requirement, with a lower Table 4 floor of 70/25 ksi. TP316Ti allows C ≤0.08% because titanium ≥5 × (C + N) does the gettering work, keeps Mo 2–3%, and holds the 75/30 ksi floor. Order L when the datasheet mandates low carbon; order Ti when stabilization plus Mo and the higher tensile floor are the named strategy.
TP316Ti vs TP321 — why does molybdenum matter?
Both grades use a titanium formula of 5 × (C + N) to 0.70% max and a 75/30 ksi Table 4 pair. TP321 has no molybdenum requirement and uses Cr 17–19 / Ni 9–12. TP316Ti adds Mo 2–3%, uses Cr 16–18 / Ni 10–14, and tightens silicon to ≤0.75%. Choose TP316Ti when molybdenum is on the datasheet beside titanium stabilization; choose TP321 when Mo is not part of the fluid story.
Why is silicon capped at 0.75% on TP316Ti instead of 1.00%?
The A213 stainless chemistry table for UNS S31635 prints silicon ≤0.75%, while TP316 / TP316L print ≤1.00%. A heat at 0.90% Si can clear standard TP316 but fails TP316Ti. Check the silicon ceiling on every candidate heat before assuming a 316 family dual from molybdenum alone.
How is the titanium minimum calculated for TP316Ti?
Titanium must be at least five times the sum of carbon plus nitrogen, and not more than 0.70%. Example: if C = 0.05% and N = 0.04%, then C + N = 0.09% and Ti must be at least 0.45% while staying ≤0.70%. Report measured C, N, and Ti together on the MTC so the formula can be verified — a titanium number without C + N is incomplete.
Does Table 4 set a hardness limit for TP316Ti?
Yes. Table 4 lists hardness maximum 192 HBW / 200 HV or 90 HRB with 75 ksi tensile, 30 ksi yield, and 35% elongation. Hardness, titanium formula, silicon ceiling, and molybdenum all belong on the release package — none replaces the others for 316Ti boiler or HX tube.
What heat treatment does A213 require for TP316Ti?
Solution treatment at a minimum of 1900 °F [1040 °C], water quench or other rapid cool. Delivery is solution annealed and pickled unless bright anneal is agreed. Put any Supplementary Requirement S2 stabilizing hold or A262 Practice E on the purchase order when the project datasheet asks for them — they are not assumed from the Ti stamp alone.
Minimum wall vs average wall for A213 TP316Ti — which should I specify?
Boiler and heat-exchanger datasheets almost always expect minimum wall. Average wall is allowed when the purchase order says so, with A1016/A1016M tolerances for that basis. State wall basis on the enquiry rather than relying on pipe schedule numbers as the primary A213 wall story.
Can I dual-certify TP316Ti with TP316 on the same heat?
Only when one heat simultaneously clears TP316’s chemistry (including Si ≤1.00% and no Ti mandate) and TP316Ti’s tighter Si ≤0.75%, N ≤0.10%, Ti formula, Mo 2–3%, and Table 4 75/30 ksi for both — and the purchase order asks for dual marking. Do not assume dual marking from a PMI gun that only reads Mo.
Is TP316Ti a substitute for TP316H in creep-range boiler lists?
No. TP316H carries a mandatory carbon band of 0.04–0.10%, a nickel floor of 11.0%, and ASTM grain size No. 7 or coarser. TP316Ti uses titanium stabilization without those H-grade controls. When the datasheet names H-grade carbon and grain size with molybdenum, order A213 TP316H rather than substituting Ti-stabilized tube.

Conclusion

ASTM A213 TP316Ti / UNS S31635 is the titanium-stabilized molybdenum-bearing seamless stainless steel tube for boiler, superheater, and heat-exchanger service when Mo 2–3% and a Ti ≥5 × (C + N) stabilization path must travel together. SHH STEEL supplies cold-finished and hot-finished seamless tube in the usual OD × wall / BWG band, solution annealed at 1900 °F [1040 °C], tested to Table 4 75/30 ksi and hardness limits, with titanium and molybdenum reported on EN 10204 3.1 certificates — dual SA-213 marking only when the purchase order asks.

Contact: admin@steelspecs.com

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X