ASTM A213 TP348H Stainless Steel Tube | ASTM A213 Stainless Steel - SHH STEEL

ASTM A213 TP348H Stainless Steel Tube

ASTM A213 TP348H / UNS S34809 seamless boiler, superheater and heat-exchanger tube with carbon 0.04–0.10%, Cr 17.0–19.0%, Ni 9.0–13.0%, Nb+Ta ≥8×C ≤1.10%, cobalt ≤0.20%, tantalum ≤0.10%, Table 4 floor 75/30 ksi, hardness max 192 HBW / 90 HRB, and grain size No. 7 or coarser. SHH STEEL supplies seamless tube with finish-route solution treatment (CF 2000 °F [1100 °C] / HR 1925 °F [1050 °C]) and EN 10204 3.1 MTCs that report Nb+Ta, Co, Ta, and grain size.
Grade
TP348H / UNS S34809
Standard
ASTM A213 / A213M
Product form
Seamless boiler / superheater / heat-exchanger tube (cold-finished and hot-finished)
Size
Typical OD × min wall (or average wall) within ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD and ~0.015–0.500 in. [0.4–12.7 mm] wall; other diameters by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is ASTM A213 TP348H Stainless Steel Tube

ASTM A213 / A213M is the ASTM International product specification for seamless ferritic and austenitic alloy-steel boiler, superheater, and heat-exchanger tubes. Grade TP348H / UNS S34809 is the H-grade, cobalt- and tantalum-controlled, Nb+Ta-stabilized austenitic stainless member of that stainless table: melting carbon is held in 0.04–0.10%, chromium 17.0–19.0%, nickel 9.0–13.0%, niobium-plus-tantalum at ≥8 × C and ≤1.10% (Footnote H on the chemistry table), cobalt ≤0.20%, and tantalum ≤0.10%. Unlike non-H A213 TP348, the public heat-treatment table prints ASTM grain size No. 7 or coarser and splits the solution minimum by finish route — cold-worked 2000 °F [1100 °C] versus hot-rolled 1925 °F [1050 °C] with Footnote H on the heat-treatment row. Buyers who write “348H tube” still need to name A213 (or the separate ASME SA-213 adoption) on the purchase order so the mill applies H-grade C / Nb+Ta / Co / Ta / grain-size / finish-route HT clauses rather than a loose shop nickname.

SHH STEEL can supply ASTM A213 TP348H stainless steel tube as seamless cold-finished and hot-finished product in the usual boiler and superheater OD × wall / BWG band, shipped with EN 10204 3.1 mill test certificates that report the full ladle chemistry (including Nb + Ta against the 8 × C formula, cobalt, and tantalum), the Table 4 tensile and hardness results, grain size against No. 7 or coarser, and the finish-route anneal temperature for the heat-treatment lot. When a project also needs ASME Code Book marking, we dual-mark A213 / SA-213 on the same lengths only if the purchase order says so. Browse the grade family on the A213/A213M hub.

Commercially, TP348H tube is still called 348H, S34809, or H-grade Co-controlled Nb-stabilized boiler tube; none of those shop names replace the ASTM grade on the MTC or stencil. Sister grades under the same ASTM standard include A213 TP348, A213 TP347H, A213 TP347, A213 TP321H, and A213 TP347HFG. A213 covers seamless tube only — no welded or HCW manufacturing type — so cold-finished versus hot-finished is the process choice that also sets the solution-temperature minimum, not a WLD/HCW stencil letter.

Chemical Composition of A213 TP348H

Two chemistry layers matter for TP348H under ASTM A213. Melting (heat or ladle) analysis is mandatory for every heat; product analysis on finished tube applies only when Supplementary Requirement wording or the purchase order invokes it through ASTM A1016/A1016M. Product-analysis tolerances typically flow from ASTM A480/A480M Table A1.1. SHH STEEL reports actual ladle values — and product values when ordered — and does not advertise unpublished tighter catalogue windows. Four lines define the grade for a reviewer: carbon 0.04–0.10%, Nb + Ta ≥8 × C ≤1.10% (chemistry Footnote H), cobalt ≤0.20%, and tantalum ≤0.10%. That Nb+Ta multiplier is deliberately lower than the 10 × C rule on non-H A213 TP348, so do not copy a TP348 niobium check onto a TP348H heat without reopening the formula. Versus A213 TP347H, TP348H adds Co/Ta ceilings and writes the stabilizer as Nb + Ta rather than Nb alone.

The tables below reproduce the heat analysis for TP348H / UNS S34809, the product-analysis limits from A480 Table A1.1 practice, and a short C / Nb+Ta / Co / Ta snapshot against TP348, TP347H, and TP347. Later A213 editions place austenitic stainless grades in Table 2 (older editions used Table 1); confirm the ordered edition on the purchase order. A480 product-tolerance digits for Co and Ta maxima are applied from sister-pack practice and labeled UNCERTAIN pending the ordered A480 edition.

Melting analysis (heat / ladle analysis)

Element TP348H (UNS S34809) melting analysis
Carbon (C) 0.04 – 0.10
Manganese (Mn) ≤ 2.00
Phosphorus (P) ≤ 0.045
Sulfur (S) ≤ 0.030
Silicon (Si) ≤ 1.00
Chromium (Cr) 17.0 – 19.0
Nickel (Ni) 9.0 – 13.0
Molybdenum (Mo) … (no requirement)
Nitrogen (N) … (no requirement)
Niobium + Tantalum (Nb + Ta) ≥ 8 × C, ≤ 1.10 (chemistry Footnote H)
Cobalt (Co) ≤ 0.20
Tantalum (Ta) ≤ 0.10
Titanium (Ti) … (no requirement)

Source: ASTM A213/A213M stainless chemistry table for Grade TP348H / UNS S34809 (public mill / specification PDF excerpt — _ref_a213.txt / A213–13 table text). Confirm the ordered edition. Where ellipses appear, the ordered edition sets no requirement for that element.

Product analysis — A480/A480M Table A1.1 tolerances applied

Element Melting Tolerance (A480 A1.1) Product analysis limit
Carbon (C) 0.04 – 0.10 0.01 under / over 0.03 – 0.11
Manganese (Mn) ≤ 2.00 0.04 over ≤ 2.04
Phosphorus (P) ≤ 0.045 0.010 over ≤ 0.055
Sulfur (S) ≤ 0.030 0.005 over ≤ 0.035
Silicon (Si) ≤ 1.00 0.05 over ≤ 1.05
Chromium (Cr) 17.0 – 19.0 0.20 under / over 16.80 – 19.20
Nickel (Ni) 9.0 – 13.0 0.15 under / 0.20 over 8.85 – 13.20
Nb + Ta ≥ 8 × C, ≤ 1.10 0.05 over on max (Nb formula practice) max ≤ 1.15 product; min tied to heat C
Cobalt (Co) ≤ 0.20 0.03 over (UNCERTAIN — confirm A480) ≤ 0.23
Tantalum (Ta) ≤ 0.10 0.02 over (UNCERTAIN — confirm A480) ≤ 0.12

Carbon / stabilizer / Co snapshot — TP348 / TP348H / TP347H / TP347

Element TP348 (S34800) TP348H (S34809) TP347H (S34709) TP347 (S34700)
C ≤ 0.08 0.04 – 0.10 0.04 – 0.10 ≤ 0.08
Cr 17.0 – 19.0 17.0 – 19.0 17.0 – 19.0 17.0 – 20.0
Stabilizer Nb+Ta ≥ 10 × C, ≤ 1.10 Nb+Ta ≥ 8 × C, ≤ 1.10 Nb ≥ 8 × C, ≤ 1.10 Nb ≥ 10 × C, ≤ 1.10
Co / Ta Co ≤ 0.20; Ta ≤ 0.10 Co ≤ 0.20; Ta ≤ 0.10 not listed not listed
Grain size no mandatory number No. 7 or coarser No. 7 or coarser no mandatory number

Heats that also meet the non-H TP348 carbon ceiling while clearing the H-grade carbon floor, both Nb+Ta formulas, Co/Ta ceilings, tensile, hardness, and grain-size paths can be dual-certified TP348/TP348H when the purchase order asks — do not assume it from a PMI gun. Dual TP348H/TP347H is not a chemistry path: one grade requires Co/Ta ceilings and writes Nb+Ta; the other writes Nb alone without Co/Ta. Put any tighter project cobalt ceiling or Nb+Ta floor on the purchase order before the heat is selected.

When product analysis is ordered, finished tube may read C 0.03–0.11%, Mn ≤2.04%, P ≤0.055%, S ≤0.035%, Si ≤1.05%, Cr 16.80–19.20%, Ni 8.85–13.20%, Nb+Ta max ≤1.15% with the formula minimum still tied to heat carbon, Co ≤0.23%, and Ta ≤0.12% under the A480 practice digits above. Confirm A480 edition digits for Co and Ta when product analysis is contractual.

Mechanical Properties of A213 TP348H

ASTM A213 Table 4 sets the room-temperature tensile acceptance floor for TP348H at 75 ksi [515 MPa] tensile strength and 30 ksi [205 MPa] yield strength (0.2% offset), with elongation of 35% minimum in 2 in. or 50 mm — the same room-temperature pair as TP348 and TP347H. Hardness maximum is 192 HBW / 200 HV or 90 HRB, and hardness tests are part of lot acceptance under A213. The public heat-treatment table prints ASTM grain size No. 7 or coarser for TP348H, so grain-size reporting belongs on a complete MTC for this H grade — unlike non-H TP348, where the public Table 3 row leaves grain size blank.

Property TP348H requirement
Tensile strength, min (Table 4) 75 ksi [515 MPa]
Yield strength (0.2% offset), min (Table 4) 30 ksi [205 MPa]
Elongation in 2 in. or 50 mm, min (Table 4) 35%
Hardness, max (Table 4) 192 HBW / 200 HV or 90 HRB
Grain size (Table 3) ASTM No. 7 or coarser

Source: ASTM A213/A213M Table 4 and Table 3 for TP348H / UNS S34809 (public specification PDF excerpt — _ref_a213.txt / A213–13). Mechanical property requirements do not apply to tubing smaller than 1/8 in. [3.2 mm] inside diameter or thinner than 0.015 in. [0.4 mm] wall. Flattening and flaring tests are also required on a lot basis. For austenitic grades with a grain-size requirement, marking also includes heat number and heat-treatment lot identification.

Room-temperature tensile equality with sister H grades is why buyers sometimes look for dual marking with TP348 or TP347H; the Co/Ta ceilings, Nb+Ta formula, and finish-route HT are why TP348H exists as its own row. A tensile-only MTC that omits Nb+Ta, Co, Ta, or grain size is incomplete — ask for those checks on the certificate before releasing the heat. For non-H Co/Ta framing open A213 TP348; for Nb-only H-grade framing open A213 TP347H.

Dimensions and Tolerances

Dimensional supply for ASTM A213 TP348H is tube language — outside diameter × wall thickness (minimum wall or average wall) and, commercially, BWG / gauge — not ASME B36.19 pipe schedules as the primary size story. The sizes usually furnished under A213 run from about 1/8 in. [3.2 mm] inside diameter to 5 in. [127 mm] outside diameter, with minimum wall from about 0.015 to 0.500 in. [0.4 to 12.7 mm]; other diameters may be furnished when all other requirements are met. State on the purchase order whether wall is minimum or average — boiler and superheater datasheets that pick the H grade almost always assume a minimum-wall reading.

Outside-diameter and wall variations follow ASTM A1016/A1016M as invoked by A213. Cold-finished tubes commonly hold tighter OD control; hot-finished tubes allow wider OD and wall windows. Permissible variations from a specified average wall for cold-finished tube are often summarized as ±10% of the specified average wall. Confirm the exact A1016 rows for the OD and finish route on the ordered edition — and remember that finish route also sets the solution-temperature minimum for TP348H.

Item Typical A213 TP348H dimensional practice
Product form Seamless only (cold-finished or hot-finished) — finish route also sets HT minimum
Usual size band ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD; wall ~0.015–0.500 in. [0.4–12.7 mm] min (or average wall if PO says so)
Wall basis Minimum wall (default for boiler / HX) or average wall when specified
OD / wall tolerances Per ASTM A1016/A1016M for the finish route and size; cold-finished average wall often ±10%
Length Cut lengths for boiler / superheater / HX bundles, or mill random lengths by agreement
Secondary size note ASME B36.19 schedules may appear only when a buyer asks for a pipe-schedule cross-reference — not as the primary A213 size callout

Put the cut list, finish route, and end preparation on the enquiry so mill and stock lengths can be mixed efficiently. Minimum wall is a first-class A213 concept: if the datasheet assumes average wall, say so explicitly before the heat is rolled.

Equivalent Grades

Equivalence language around TP348H tube is often looser than an H-grade Co/Ta purchase order can afford. ASTM A213 Grade TP348H / UNS S34809 is the governing designation for this article; shop nicknames that say “348H boiler tube” or “H-grade low-cobalt 348” are not automatic substitutes on an A213 mill test certificate. When a datasheet says “equivalent to 348H,” confirm which product standard, tensile/hardness table, Nb+Ta formula, Co/Ta ceilings, grain-size window, and finish-route heat-treatment path the mill will actually certify.

Designation Notes
ASTM A213 / A213M Grade TP348H Governing ASTM seamless boiler / HX tube product standard for this article
UNS S34809 Unified number listed in the stainless chemistry table
ASME SA-213 TP348H Separate ASME Code Book adoption — dual-mark only when the PO asks
Related grades TP348 / S34800 (non-H Co/Ta); TP347H / S34709 (H-grade Nb without Co/Ta)
Related plate A240 / SA240 flat product in related UNS families — order plate and tube under their own product standards

Dual A213/SA-213 marking is a purchase-order option, not a claim that the two standards are one document. Compare TP348, TP347H, and TP321H on their own ASTM A213 pages before swapping grades on a familiar “348H” PMI reading alone.

Heat Treatment and Delivery Condition

TP348H under ASTM A213 is furnished solution treated on a finish-route schedule: cold-worked tube at a minimum of 2000 °F [1100 °C], hot-rolled tube at a minimum of 1925 °F [1050 °C], then quenched in water or cooled rapidly by other means. The public heat-treatment table marks the hot-rolled path with Footnote H — the same footnote family that warns a solution treating temperature above 1950 °F [1065 °C] may impair intergranular-corrosion resistance after subsequent sensitizing exposure, and allows a purchaser-specified lower-temperature stabilization or resolution anneal after the higher solution anneal. ASTM grain size No. 7 or coarser is mandatory for TP348H.

Supplementary Requirement S2 lists TP348H among grades that shall be given a stabilization heat treatment at a temperature lower than the initial solution anneal when the purchaser specifies S2 — temperature as agreed between purchaser and vendor. For niobium/tantalum-bearing H grades, S2 may also be necessary and is permitted to meet Supplementary Requirement S4 (A262 Practice E). Supplementary Requirement S1 does not list TP348H in the public A213–13 excerpt (S1 names TP304L, TP316L, TP321, TP347, and TP348). Neither S1 nor S2 is automatic with the grade stamp.

Cold-finished versus hot-finished is therefore both a dimensional route and a heat-treatment route for TP348H. Delivery condition for SHH STEEL TP348H is solution annealed and pickled (or bright annealed by agreement), with finish-route anneal temperature, quench method, grain size, and Nb+Ta / Co / Ta results on the EN 10204 3.1 certificate. For non-H Co/Ta framing open A213 TP348; for Nb-only H-grade framing open A213 TP347H.

Corrosion Resistance

TP348H’s chromium-rich passive film and Nb+Ta stabilization handle many boiler and superheater duties where sensitizing thermal cycles would otherwise deplete chromium at grain boundaries. The H-grade carbon floor supports elevated-temperature strength framing; the Co and Ta ceilings satisfy controlled-chemistry purchase orders. Neither package is a molybdenum addition for aqueous chlorides. In chloride-bearing cooling waters and many process exchangers, pitting and crevice attack become limiting, and buyers usually step to A213 TP316 / A213 TP316L or a higher-PREN grade rather than stretching H-grade Nb-stabilized 18-8 into wet corrosive service.

ASTM A213 itself does not publish a corrosion-rate table for TP348H; selection remains engineering judgment against fluid, temperature, velocity, creep design data, and inspection philosophy. When a specification calls for ASTM A262 Practice E, write Supplementary Requirement S4 onto the purchase order — and note that for niobium/tantalum-bearing H grades a stabilization heat treatment under S2 may be necessary and is permitted to meet that requirement. Footnote H on the heat-treatment path also reminds purchasers that a high solution temperature can impair later IGC resistance. SHH STEEL will not market TP348H as a wet-chloride upgrade over molybdenum grades; the H + Co/Ta designation is about elevated-temperature framing and controlled chemistry, not about higher PREN.

Applications of A213 TP348H Tube

TP348H seamless tube under A213 is chosen for boiler and superheater service where H-grade carbon, Nb+Ta ≥8 × C, grain size No. 7 or coarser, finish-route solution temperatures, and Co/Ta ceilings must appear together on the mill certificate. It is a selection when nuclear or low-cobalt specifications name S34809 rather than S34709 or S34800. It is the wrong default for chloride-rich cooling water that really needs Mo, and it is not interchangeable with TP347H on chemistry alone. The table below pairs typical application areas with a selection note.

Application area Typical use of TP348H tube Selection note
H-grade boiler / superheater Seamless A213 tube where C 0.04–0.10, Nb+Ta ≥8×C, grain 7, and Co/Ta are specified Confirm finish-route HT and grain size on the MTC
Low-cobalt H-grade specs Stabilized steam tubing ordered to S34809 Do not substitute TP347H without checking Co/Ta
Vs non-H TP348 duty When H carbon floor and grain size are required on top of Co/Ta Open TP348 if H framing is not on the datasheet
Vs TP347H duty When Co/Ta control is required on an H-grade Nb path Open TP347H if Co/Ta ceilings are not required
Wet chloride service Not the first choice Prefer TP316L or higher-Mo grades

For non-H Co/Ta open A213 TP348; for Nb-only H-grade open A213 TP347H; for titanium H-grade open A213 TP321H on the A213/A213M hub.

Weldability

TP348H tube welds with matching or near-matching niobium-bearing austenitic filler for tube-to-tubesheet joints, attachment welds, and fabrication joins. Common practice uses ER347 / ER347H / E347 (or ER348 when Co/Ta control extends into the filler specification) under a qualified WPS so weld-metal niobium supports stabilized H-grade service. Many fabricators avoid defaulting to ER308L when the base tube is Nb+Ta-stabilized H-grade and the design assumes stabilization chemistry in the joint. Heat input control, interpass limits, and post-weld cleaning remain the fabricator’s responsibility under the applicable boiler or pressure-vessel code — A213 governs the seamless tube product, not the field or shop weld procedure.

Because A213 TP348H is seamless, there is no mill longitudinal weld to radiograph the way welded pipe standards describe. Focus inspection language on tube integrity (hydro or NDE of each length), tube-to-tubesheet joint quality, Nb+Ta / Co / Ta and grain-size documentation on the base metal, and any contractual corrosion test. Specify end preparation and surface finish on the tube PO when orbital or clean-service joins are planned.

Surface Finishes

Standard mill delivery for ASTM A213 TP348H is solution annealed and pickled, leaving a clean matte finish suitable for most boiler and superheater tube duty. Bright annealing under protective atmosphere produces a smoother reflective surface used on some clean-process lines and must be called out because it changes the heat-treatment route. Light polish or specified Ra on the bore or OD is a commercial or service-center operation on top of A213 product, not automatic with the grade stamp.

When a fouling-sensitive exchanger specification quotes an Ra maximum on the bore, put it on the tube purchase order with its own acceptance language and sampling plan. SHH STEEL stencils grade, heat treatment, and (for grain-size grades) heat/lot identity as standard requirements; polish, special OD grind, and passivation after fabrication remain commercial extras unless the contract says otherwise. Order end preparation together with finish so receiving inspection shares one acceptance language.

Inspection and Testing

Base ASTM A213 testing for TP348H includes heat analysis (carbon 0.04–0.10%, Nb+Ta meeting ≥8 × C ≤1.10%, cobalt ≤0.20%, tantalum ≤0.10%), tension tests to the Table 4 floors (75/30 ksi), hardness tests to the Table 4 maximum (192 HBW / 90 HRB), grain-size determination to No. 7 or coarser, flattening and flaring tests on a lot basis, and either hydrostatic testing or nondestructive electric testing of each length. The manufacturer may choose hydro versus NDE unless the purchase order fixes the method. Marking includes the ASTM designation, grade, size, heat number, heat-treatment lot identification (required for austenitic grades with a grain-size requirement), and other clause-required data.

Supplementary Requirements commonly added on TP348H tube orders are summarized below. Invoke them by number or clear purchase-order wording; mills will not assume product analysis, S2 stabilization, or IGC testing from a verbal “full certs” note. Note that S1 is not printed for TP348H in the public A213–13 excerpt.

Option Purpose
Product analysis Confirms chemistry on finished tube — useful when Nb+Ta, Co, or Ta sits near a limit
S2 stabilizing heat treatment Lower-temperature stabilization after the solution anneal — listed for TP348H when specified
S4 intergranular corrosion A262 Practice E; S2 may be necessary for Nb/Ta-bearing H grades to meet S4
Finish-route callout States cold-finished vs hot-finished so the correct solution minimum applies
Minimum vs average wall States which wall basis the size callout uses
Fixed hydro or NDE method Removes manufacturer’s option when the end user mandates one route
Third-party inspection / EN 10204 3.2 Witnessed testing and certificate when the project requires it

Ask the mill to state lot identity clearly on the certificate so hardness, tension, grain size, and Nb+Ta / Co / Ta specimens map cleanly to the bundle you receive.

Packaging and Shipping

TP348H tube leaves SHH STEEL bundled, capped or end-protected, and tagged for export or domestic delivery according to the length mix and bend form on the order. Bundle tags repeat the ASTM A213 grade, OD × wall (or BWG), heat number, heat-treatment lot identity, and PO reference so site receiving can check the shipment without opening every certificate packet first. U-bent tubes need extra cradle or case protection so bend radii and legs are not distorted in transit.

Export packing can be bare bundles, wrapped bundles, or wooden-cased lengths for bright-annealed, polished, or small-bore material. We ship under the Incoterms on the order acknowledgement — FOB, CFR, CIF, EXW, or other agreed terms. Inland trucking, bilingual destination marks, or project color coding for bundle tags should be stated on the enquiry beside the metallurgical notes.

Why Choose SHH STEEL

SHH STEEL treats ASTM A213 TP348H as a product standard with enforceable chemistry (H-grade C, Nb+Ta formula, Co and Ta ceilings), tensile, hardness, grain-size, finish-route heat-treatment, and marking rules — not as a catalogue nickname for “any 348H tube.” The MTC reports the full ladle chemistry including Nb + Ta against 8 × C, cobalt, and tantalum, the Table 4 tensile/hardness set (75/30 ksi, 192 HBW / 90 HRB), grain size against No. 7 or coarser, and the finish-route anneal temperature; the stencil carries seamless tube identity under A213; and dual A213/SA-213 marking is offered only when requested.

We keep the H-grade Co/Ta conversation honest for boiler and superheater duty. If non-H Co/Ta without grain-size framing is enough, we open A213 TP348. If H-grade Nb without Co/Ta ceilings is enough, we open A213 TP347H. If fine-grain creep framing without Co/Ta is specified, we open A213 TP347HFG. If titanium H-grade is preferred, we open A213 TP321H. The A213/A213M hub is organized grade by grade under ASTM, seamless tube only.

Lead times combine near-term stock lengths with mill schedules; we say which is which on the quotation. Cut-to-length, U-bending, polish, and third-party inspection are defined extras. The tube that arrives should match the ASTM callout the engineer wrote, with paperwork a third-party inspector can read without translation.

Supply Capability

SHH STEEL can supply ASTM A213 TP348H stainless steel tube against the edition and finish route named on your enquiry. The capability table below summarizes the sizes, finishes, and documents we regularly quote for this grade, followed by the Stock / Available sizes map buyers ask for when they need a quick sense of what to enquire against for H-grade Co/Ta-controlled Nb-stabilized boiler and superheater duty.

Item SHH STEEL capability for TP348H
Standard ASTM A213 / A213M (dual SA-213 marking on request) Grade TP348H / UNS S34809
Product form Seamless only — cold-finished and hot-finished (finish route sets HT minimum)
Size Typical OD × min wall (or average wall) in the A213 usual band; other diameters by agreement
Wall / gauge Minimum wall or average wall; BWG / gauge callouts accepted on enquiry
Length Cut-to-length for boiler / superheater / HX bundles; mill random by agreement; U-bends on enquiry
Finish Annealed and pickled; bright annealed or light polish by agreement
Testing Tension (75/30 ksi), hardness (max 192 HBW / 90 HRB), grain size No. 7 or coarser, Nb+Ta vs 8×C, Co, Ta, flattening, flaring, hydro or NDE per length; full ladle chemistry on MTC; product analysis / S2 / S4 on order
Documents EN 10204 3.1 with full ladle chemistry, Nb+Ta / Co / Ta, and grain size; third-party inspection / 3.2 on request
Trade terms FOB / CFR / CIF / EXW and other agreed Incoterms

Stock / Available sizes

SHH STEEL quotes TP348H tube against a practical stock-and-mill enquiry range rather than a frozen warehouse SKU list. The sizes below are OD × wall / BWG combinations buyers most often request for H-grade Co/Ta-controlled boiler and superheater tube; availability of any single line on a given week depends on mill drawing and our inbound schedule, so treat the table as a supply map for enquiry — not a guarantee of floor tonnage.

Item Typical stock / enquiry range for TP348H
Outside diameter 25.4, 31.8, 38.1, 44.5, 50.8, 63.5, 76.2 mm (and other boiler/superheater ODs on enquiry; up through the usual A213 ~5 in. [127 mm] band)
Wall / BWG BWG 10–16 class walls and metric min-wall equivalents; heavier walls for high-pressure duty by agreement
Common OD × wall examples 31.8 × 2.77 mm; 38.1 × 3.05 mm; 44.5 × 3.05 mm; 50.8 × 3.38 mm; 63.5 × 3.38 mm — illustrative boiler/superheater sizes, confirm min vs average wall
Length Cut lengths for boiler / superheater bundles; U-bends and straight random lengths on enquiry
Special Non-standard OD/wall, bright anneal, S2 stabilization, dual TP348/TP348H marking, dual A213/SA-213 marking, finish-route callout — confirm on enquiry before the heat is reserved

When you send an enquiry, list OD × wall (or BWG), wall basis (minimum or average), cold-finished or hot-finished preference (this sets the HT minimum), quantity or cut list, required marking (A213 alone, dual A213/SA-213, and/or dual TP348/TP348H), and any Supplementary Requirements (S2, S4, product analysis). We reply with what we can ship from near-term stock versus what needs a mill run, without inventing fake warehouse codes or tonnage claims.

Send the size list, finish route, quantity or cut lengths, required marking, Supplementary Requirements, and destination on one enquiry. We will confirm chemistry (including the Nb+Ta formula and Co/Ta ceilings), tensile, hardness, and grain size against the stainless chemistry table, Table 3, and Table 4, state what ships from near-term availability versus mill production, and keep the offer aligned with ASTM A213 / A213M. Related grades such as A213 TP348, A213 TP347H, and A213 TP321H sit on the same hub when the datasheet steps beyond TP348H.

FAQ

Is ASTM A213 the same as ASME SA-213 for TP348H?
No. ASTM A213 / A213M is the ASTM International product specification for seamless boiler, superheater, and heat-exchanger tubes; ASME SA-213 / SA-213M is the separate ASME Code Book adoption of that grade text. Chemistry, tensile, hardness, grain-size, and Nb+Ta / Co / Ta rules align closely for a given referenced edition, but they remain two independent standards. Dual-mark A213/SA-213 tube only when the purchase order asks for both names on the stencil and MTC.
Does ASTM A213 TP348H include welded or HCW tube?
No. ASTM A213 covers seamless tube only. There is no WLD or HCW manufacturing type under this product standard the way ASTM A312 describes pipe. The process choice for TP348H under A213 is cold-finished versus hot-finished seamless tube — and that finish route also sets the solution-temperature minimum — plus the H-grade C / Nb+Ta / Co / Ta / grain-size and testing clauses of the ordered edition.
TP348H vs TP348 — when do I need the H grade?
Order TP348H when the boiler or superheater datasheet needs H-grade carbon 0.04–0.10%, Nb+Ta ≥8 × C ≤1.10%, ASTM grain size No. 7 or coarser, and finish-route solution temperatures (CF 2000 °F / HR 1925 °F). Order TP348 when Nb+Ta ≥10 × C with C ≤0.08%, Co/Ta ceilings, and the single 1900 °F solution path are enough without H-grade grain-size framing. They share Co/Ta control but are not synonym stamps on the MTC.
TP348H vs TP347H — cobalt control or Nb-only H grade?
Both are H-grade stabilized austenitics with C 0.04–0.10%, Cr 17–19 / Ni 9–13, grain size No. 7 or coarser, and finish-route HT. TP348H writes the stabilizer as Nb + Ta ≥8 × C ≤1.10% and adds Co ≤0.20% and Ta ≤0.10%. TP347H writes Nb alone ≥8 × C ≤1.10% without Co/Ta ceilings. Order TP348H when Co/Ta control is on the H-grade datasheet; order TP347H when Nb-only H-grade chemistry is enough.
What carbon and Nb+Ta limits apply to A213 TP348H?
Melting carbon is 0.04–0.10%, and Footnote H on the chemistry table requires Nb + Ta not less than 8 times the carbon content and not more than 1.10%. Cobalt is ≤0.20% and tantalum is ≤0.10%. That Nb+Ta multiplier is lower than TP348’s 10 × C rule, so do not copy a non-H formula check onto an H-grade heat. Confirm the ordered A213 edition for the exact stainless-table number.
What heat treatment and grain size does A213 require for TP348H?
Finish-route solution treatment: cold-worked tube at 2000 °F [1100 °C] minimum, hot-rolled tube at 1925 °F [1050 °C] minimum, then water quench or other rapid cool, with ASTM grain size No. 7 or coarser. Footnote H on the heat-treatment path warns about high solution temperatures and IGC after later sensitizing exposure. Marking includes heat number and heat-treatment lot identification because grain size is required.
What is Supplementary Requirement S2 for TP348H?
S2 requires a stabilization heat treatment at a temperature lower than the initial solution anneal, with the temperature agreed between purchaser and vendor. The public A213–13 excerpt lists TP348H among grades that shall receive S2 when specified. For niobium/tantalum-bearing H grades, S2 may also be necessary and is permitted to meet Supplementary Requirement S4 (A262 Practice E). S2 is never automatic with the grade stamp alone.
Is Supplementary Requirement S1 listed for TP348H?
Not in the public A213–13 excerpt. S1 lists TP304L, TP316L, TP321, TP347, and TP348 for stress-relieved annealed delivery at 1500–1650 °F [815–900 °C] after roll straightening. TP348H is absent from that printed list. If your project needs stress-relieved delivery for S34809, negotiate the treatment on the purchase order rather than assuming S1 applies by grade nickname.
Does Table 4 set a hardness limit for TP348H?
Yes. Table 4 for TP348H lists tensile strength 75 ksi [515 MPa], yield strength 30 ksi [205 MPa], elongation 35%, and a hardness maximum of 192 HBW / 200 HV or 90 HRB. Hardness tests are part of lot acceptance under A213. Ask the mill to report hardness beside the tensile and grain-size results on the EN 10204 3.1 certificate.
Minimum wall vs average wall for A213 TP348H — which should I specify?
Order minimum wall when the boiler or superheater datasheet is written around a guaranteed minimum thickness after tolerance — the usual practice for A213 tube. Order average wall only when the purchase order explicitly allows average-wall product and the designer has accepted that basis. Put the wall basis and the finish route on the enquiry before the mill selects A1016 tolerance tables and the matching solution-temperature minimum.
Can I dual-certify TP348H with TP348 on the same heat?
Yes when ladle carbon meets the H-grade 0.04–0.10% band while also clearing the TP348 ≤0.08% ceiling, when Nb+Ta clears both the 8 × C and 10 × C floors for the heat’s carbon, when Co and Ta clear both ceilings, and when tensile, hardness, and (for the H path) grain-size results clear both acceptance paths. Spell the required dual marking and finish-route heat treatment on the enquiry before the heat is selected.
Is TP348H a good choice for chloride-rich cooling water?
Usually no as a first choice. H-grade carbon and Nb+Ta help elevated-temperature and intergranular framing, and Co/Ta ceilings satisfy controlled-chemistry specs, but neither raises PREN the way molybdenum does. Prefer TP316L or a higher-Mo grade when chlorides dominate aqueous service; reserve TP348H for H-grade boiler and superheater framing where Co/Ta control earns its keep.

Conclusion

ASTM A213 TP348H / UNS S34809 is the H-grade, cobalt- and tantalum-controlled, Nb+Ta-stabilized seamless stainless steel tube grade for boiler and superheater service when C 0.04–0.10%, Nb + Ta ≥8 × C ≤1.10%, Co ≤0.20%, Ta ≤0.10%, grain size No. 7 or coarser, and finish-route solution temperatures must be certified together. SHH STEEL supplies cold-finished and hot-finished seamless tube in the usual OD × wall / BWG band, solution annealed on the finish-route schedule (CF 2000 °F [1100 °C] / HR 1925 °F [1050 °C]), tested to Table 3 and Table 4 with Nb+Ta / Co / Ta and grain size reported, and documented on EN 10204 3.1 certificates — with dual SA-213 marking only when the order asks for that separate ASME standard. For sister grades and stock-oriented size discussions, start from the A213/A213M hub, then send your OD × wall list, wall basis, finish route, dual-marking needs, and Co/Ta / Nb+Ta requirements so we can align mill and near-term availability to the ASTM callout.

Contact: admin@steelspecs.com

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X