ASTM A213 TP317 Stainless Steel Tube | ASTM A213 Stainless Steel - SHH STEEL

ASTM A213 TP317 Stainless Steel Tube

ASTM A213 TP317 / UNS S31700 higher-molybdenum seamless boiler, superheater and heat-exchanger tube — C ≤0.08%, Cr 18.0–20.0%, Ni 11.0–15.0%, Mo 3.0–4.0%, Table 4 75/30 ksi with elongation 34% min, hardness max 192 HBW / 90 HRB, 1900 °F solution anneal. SHH STEEL supplies cold-finished and hot-finished seamless tube with EN 10204 3.1 MTCs that report the elevated molybdenum band.
Grade
TP317 / UNS S31700
Standard
ASTM A213 / A213M
Product form
Seamless boiler / superheater / heat-exchanger tube (cold-finished and hot-finished)
Size
Typical OD × min wall (or average wall) within ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD and ~0.015–0.500 in. [0.4–12.7 mm] wall; other diameters by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is ASTM A213 TP317 Stainless Steel Tube

ASTM A213 / A213M is the product specification for seamless ferritic and austenitic alloy-steel boiler, superheater, and heat-exchanger tubes. Grade TP317 / UNS S31700 is the higher-molybdenum step up from the 316 family: melting carbon is capped at 0.08%, chromium moves to 18.0–20.0%, nickel to 11.0–15.0%, and molybdenum is held in a 3.0–4.0% band — a full percentage point above the 2.00–3.00% window on A213 TP316. Table 4 still sets tensile at 75 ksi [515 MPa] / 30 ksi [205 MPa], but elongation prints at 34% minimum rather than the 35% used on most sister austenitics — a small but real acceptance digit that receiving inspectors sometimes miss when they copy a 316 checklist onto a 317 heat.

SHH STEEL can supply ASTM A213 TP317 stainless steel tube as seamless cold-finished and hot-finished product in the usual boiler and heat-exchanger OD × wall / BWG band, shipped with EN 10204 3.1 mill test certificates that report the full ladle chemistry — molybdenum inside 3.0–4.0% — plus the Table 4 tensile, elongation, and hardness results. Dual A213 / SA-213 marking is offered only when the purchase order asks for both independent standards. Start from the A213/A213M hub for the rest of the Mo-bearing tube grades.

Commercial shorthand such as 317, S31700, or “high-Mo HX tube” never replaces the ASTM grade on the MTC or stencil. Sister grades under the same ASTM standard include A213 TP316, A213 TP316L, A213 TP317L, A213 TP316Ti, and A213 TP316LNM. A213 covers seamless tube only — there is no welded or HCW manufacturing type — so cold-finished versus hot-finished seamless route is the finish/process choice.

Chemical Composition of A213 TP317

Two chemistry layers matter for TP317 under ASTM A213. Melting analysis is mandatory for every heat; product analysis on finished tube applies only when Supplementary Requirement wording or the purchase order invokes it through ASTM A1016/A1016M, with tolerances typically from ASTM A480/A480M Table A1.1. The first line a reviewer should check is molybdenum 3.0–4.0% — a heat at 2.8% Mo can clear TP316 but fails TP317. The second line is the Cr–Ni balance: 18.0–20.0% chromium and 11.0–15.0% nickel, not the 16–18 / 10–14 window used on the 316 family. Nitrogen appears as an ellipsis (no requirement) in the public A213 stainless table for this grade.

The tables below reproduce the melt limits for TP317 / UNS S31700, the product-analysis limits from A480 Table A1.1 practice, and a short molybdenum / chromium / nickel snapshot against TP316 and TP317L. Later A213 editions place austenitic stainless grades in Table 2 (older editions used Table 1); confirm the ordered edition on the purchase order.

Melting analysis (heat / ladle analysis)

Element TP317 (UNS S31700) melting analysis
Carbon (C) ≤ 0.08
Manganese (Mn) ≤ 2.00
Phosphorus (P) ≤ 0.045
Sulfur (S) ≤ 0.030
Silicon (Si) ≤ 1.00
Chromium (Cr) 18.0 – 20.0
Nickel (Ni) 11.0 – 15.0
Molybdenum (Mo) 3.0 – 4.0
Nitrogen (N) … (no requirement; analysis method by agreement when reported)

Source: ASTM A213/A213M stainless chemistry table for Grade TP317 / UNS S31700 (public mill / specification PDF excerpt — _ref_a213.txt / A213–13 table text). Confirm the ordered edition. Where ellipses appear, the ordered edition sets no requirement for that element.

Product analysis — A480/A480M Table A1.1 tolerances applied

Element Melting Tolerance (A480 A1.1) Product analysis limit
Carbon (C) ≤ 0.08 0.01 over ≤ 0.09
Manganese (Mn) ≤ 2.00 0.04 over ≤ 2.04
Phosphorus (P) ≤ 0.045 0.010 over ≤ 0.055
Sulfur (S) ≤ 0.030 0.005 over ≤ 0.035
Silicon (Si) ≤ 1.00 0.05 over ≤ 1.05
Chromium (Cr) 18.0 – 20.0 0.20 under / over 17.80 – 20.20
Nickel (Ni) 11.0 – 15.0 0.15 under / over 10.85 – 15.15
Molybdenum (Mo) 3.0 – 4.0 0.10 under / over 2.90 – 4.10

Molybdenum / Cr–Ni snapshot — TP316 / TP317 / TP317L

Element TP316 (S31600) TP317 (S31700) TP317L (S31703)
C ≤ 0.08 ≤ 0.08 ≤ 0.035
Cr 16.0 – 18.0 18.0 – 20.0 18.0 – 20.0
Ni 10.0 – 14.0 11.0 – 15.0 11.0 – 15.0
Mo 2.00 – 3.00 3.0 – 4.0 3.0 – 4.0
Table 4 elong. min 35% 34% 35%

Read molybdenum first. A heat at 2.5% Mo is still a 316-family story; TP317 does not begin until the 3.0% floor is cleared. Versus A213 TP317L, the intentional chemistry change on TP317 is the higher carbon ceiling — L keeps C ≤0.035% for as-welded IGC strategy while sharing the same Mo and Cr–Ni bands. Dual TP317/TP316 is not a meaningful path: the Mo bands do not overlap.

When product analysis is ordered, finished tube may read C ≤0.09%, Mn ≤2.04%, P ≤0.055%, S ≤0.035%, Si ≤1.05%, Cr 17.80–20.20%, Ni 10.85–15.15%, and Mo 2.90–4.10%. Put any tighter project molybdenum floor on the purchase order before the heat is selected — the 3.0% minimum is intentional for the grade’s corrosion framing.

Mechanical Properties of A213 TP317

ASTM A213 Table 4 sets the tensile acceptance floor for TP317 at 75 ksi [515 MPa] tensile strength and 30 ksi [205 MPa] yield strength (0.2% offset), with elongation of 34% minimum in 2 in. or 50 mm — one point below the 35% used on TP316 and TP317L — and hardness max 192 HBW / 200 HV or 90 HRB. Receiving checklists copied from 316 heats often expect 35% elongation; for TP317 the contractual minimum is 34%. Confirm that digit on the ordered edition before rejecting a heat that clears 34% but not 35%.

Property TP317 requirement (Table 4)
Tensile strength, min 75 ksi [515 MPa]
Yield strength (0.2% offset), min 30 ksi [205 MPa]
Elongation in 2 in. or 50 mm, min 34%
Hardness, max 192 HBW / 200 HV or 90 HRB

Source: ASTM A213/A213M Table 4 for TP317 / UNS S31700 (public specification PDF excerpt — _ref_a213.txt). Mechanical property requirements do not apply to tubing smaller than 1/8 in. [3.2 mm] inside diameter or thinner than 0.015 in. [0.4 mm] wall. Flattening and flaring tests are also required on a lot basis.

A tensile-and-Mo MTC that omits elongation or reports a 35% checklist against a 34% grade is incomplete documentation practice for TP317. When low carbon is also required with the 3–4% Mo band, open A213 TP317L rather than stretching a standard TP317 heat into an L-grade story.

Dimensions and Tolerances

Dimensional supply for ASTM A213 TP317 is tube language — OD × wall (minimum or average) and commercially BWG / gauge — not ASME B36.19 pipe schedules as the primary size story. Usual A213 sizes run from about 1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD, with minimum wall about 0.015–0.500 in. [0.4–12.7 mm]; other diameters may be furnished when all other requirements are met. State min versus average wall on the purchase order — boiler and heat-exchanger datasheets almost always assume minimum wall.

OD and wall variations follow ASTM A1016/A1016M as invoked by A213. Cold-finished tubes commonly hold tighter OD control; hot-finished tubes allow wider windows. Cold-finished average-wall product is often summarized as ±10% of the specified average wall; minimum-wall product follows the A1016 minimum-wall tables. Confirm the exact rows for the OD and finish route on the ordered edition.

Item Typical A213 TP317 dimensional practice
Product form Seamless only (cold-finished or hot-finished)
Usual size band ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD; wall ~0.015–0.500 in. [0.4–12.7 mm] min (or average wall if PO says so)
Wall basis Minimum wall (default commercial practice) or average wall when specified
OD / wall tolerances Per ASTM A1016/A1016M for the finish route and size
Length Cut lengths for HX / boiler bundles, or mill random lengths by agreement
Secondary size note ASME B36.19 schedules only as a buyer-requested cross-reference — not the primary A213 callout

Put the cut list, U-bend preference, and end preparation on the enquiry. Minimum wall remains a first-class A213 concept regardless of the higher molybdenum band.

Equivalent Grades

Equivalence language around 317 tube often collapses plate and tube product forms into one nickname, or treats TP317 as “TP316 with a little more Mo.” ASTM A213 Grade TP317 / UNS S31700 is the governing designation for this article; EN 1.4449 and related wrought names that point to similar higher-Mo chemistry families are not automatic substitutes on an A213 MTC.

Designation Notes
ASTM A213 / A213M Grade TP317 Governing ASTM seamless boiler / HX tube product standard for this article
UNS S31700 Unified number in the stainless chemistry table
ASME SA-213 TP317 Separate ASME Code Book adoption — dual-mark only when the PO asks
Related 316 A213 TP316 — Mo 2–3%, Cr 16–18 / Ni 10–14
Related L-grade A213 TP317L — same Mo 3–4%, C ≤0.035, elong. 35%
Related higher-Mo L TP317LM / TP317LMN on the same hub — Mo 4–5% families (separate pages)
Related plate A240 / SA240 flat product in the 317 family — order plate and tube under their own standards

Dual A213/SA-213 marking is a purchase-order option. Compare TP316 and TP317L on their own ASTM A213 pages before swapping higher-Mo tube inside a boiler or exchanger list.

Heat Treatment and Delivery Condition

TP317 under ASTM A213 is furnished solution treated at a minimum of 1900 °F [1040 °C], then quenched in water or cooled rapidly by other means. The public heat-treatment table does not print a mandatory ASTM grain-size number for this grade. That heat-treatment row applies to both cold-finished and hot-finished seamless tube. Skipping or under-cooling the solution treatment can leave a structure that undermines corrosion performance even when ladle molybdenum looked acceptable on paper.

Cold-finished versus hot-finished is a process and dimensional route, not a substitute for the anneal. Delivery condition for SHH STEEL TP317 is solution annealed and pickled (or bright annealed by agreement), with anneal temperature, quench method, and molybdenum result on the EN 10204 3.1 certificate. Straightening, cutting, and end finishing follow heat treatment.

Unlike H grades such as A213 TP316H, TP317 has no carbon floor and no grain-size mandate. If a project datasheet asks for ASTM A262 Practice E on 317, put that Supplementary Requirement on the purchase order rather than assuming base A213 includes it. For as-welded IGC-critical lists, many owners move to A213 TP317L instead of relying on procedure alone to protect C ≤0.08% TP317.

Corrosion Resistance

TP317’s defining corrosion claim versus the 316 family is the higher molybdenum band: 3.0–4.0% Mo improves resistance to pitting and crevice attack in many chloride-leaning aqueous services relative to Mo 2–3% grades, while the 18–20 / 11–15 Cr–Ni balance supports the austenitic structure around that Mo level. It is still not a duplex or super-austenitic alloy, and it is still not an L-grade: carbon up to 0.08% means as-welded intergranular corrosion risk after tube-to-tubesheet welding needs separate review.

ASTM A213 itself does not publish a corrosion-rate table for TP317; selection remains engineering judgment against fluid, temperature, velocity, and inspection philosophy. When a specification calls for ASTM A262 Practice E, write that Supplementary Requirement onto the purchase order so the test is contractual. SHH STEEL will not claim TP317 equals TP317LM / TP317LMN (Mo 4–5% families) or superaustenitics in severe brine — those are separate grade rows with their own chemistries.

Applications of A213 TP317 Tube

Because TP317 steps molybdenum into the 3–4% band with a higher Cr–Ni balance, it shows up in process heat exchangers and condensers where 316-family Mo is judged insufficient, chemical-plant tube lists that historically named 317, and chloride-leaning aqueous services that still sit inside austenitic (not duplex) selection. The table below pairs typical application areas with a selection note so the grade is chosen for Mo level, weld sequence, and fluid — not only for the familiar “317” name on the BOM.

Application area Typical use of TP317 tube Selection note
Higher-Mo process HX Straight and U-bend tubes when Mo 3–4% is named Confirm Mo floor ≥3.0% on MTC, not PMI of “about 3”
Chloride-leaning condensers When TP316 Mo band is judged short Still not a duplex / superaustenitic substitute
As-welded IGC-critical joins Usually prefer TP317L rather than TP317 C ≤0.08% works against as-welded IGC strategy
Mo 2–3% sufficient Stay on TP316 / TP316L / TP316LNM Do not over-specify 317 for ordinary 316 Mo lists
Mo 4–5% families Open TP317LM / TP317LMN on the same hub Different Mo / Ni / N rows — not nickname upgrades

For as-welded higher-Mo tube open A213 TP317L; for Mo 2–3% open A213 TP316 or A213 TP316LNM; browse the rest on the A213/A213M hub.

Weldability

TP317 tube welds with matching or near-matching higher-molybdenum austenitic filler for tube-to-tubesheet joints, attachment welds, and fabrication joins. Common practice uses ER317 / ER317L under a qualified WPS so weld-metal molybdenum tracks the 3–4% base-metal band; some fabricators accept ER316L only when the procedure qualification and corrosion review explicitly allow the Mo step-down in the deposit. Heat input control, interpass limits, and post-weld cleaning remain the fabricator’s responsibility — A213 governs the seamless tube product, not the field or shop weld procedure.

Because A213 TP317 is seamless, there is no mill longitudinal weld to radiograph the way welded pipe standards describe. Focus inspection language on tube integrity (hydro or NDE of each length), tube-to-tubesheet joint quality, and any contractual corrosion test on the base metal. For tube that will enter service as-welded in a sensitizing environment, many owners change the base metal to A213 TP317L rather than relying on a perfect weld procedure alone to protect C ≤0.08% TP317. Specify end preparation and surface finish on the tube PO when orbital or clean-service joins are planned.

Surface Finishes

Standard mill delivery for ASTM A213 TP317 is solution annealed and pickled, leaving a clean matte finish suitable for most boiler and heat-exchanger tube duty. Bright annealing under protective atmosphere produces a smoother reflective surface used on some clean-process and instrumentation tube lines and must be called out because it changes the heat-treatment route. Light polish or specified Ra on the bore or OD is a commercial or service-center operation on top of A213 product, not automatic with the grade stamp.

When a hygienic or fouling-sensitive exchanger specification quotes an Ra maximum on the bore, put it on the tube purchase order with its own acceptance language and sampling plan. SHH STEEL stencils grade and heat treatment as standard requirements; polish, special OD grind, and passivation after fabrication remain commercial extras unless the contract says otherwise. End preparation (plain, slightly beveled, or as needed for tube expanding) should be ordered together with finish so receiving inspection shares one acceptance language.

Inspection and Testing

Lot testing for ASTM A213 TP317 follows tension, hardness, flattening, and flaring under A213 / A1016. Chemistry verification must include molybdenum 3.0–4.0%, chromium 18.0–20.0%, and nickel 11.0–15.0%. Tensile reporting must use the Table 4 elongation minimum of 34%, not a copied 35% 316 checklist. NDE follows the ordered edition and purchaser supplements — hydrostatic testing or non-destructive electric testing of each length is the usual A213 path unless the purchase order states otherwise.

EN 10204 3.1 certificates from SHH STEEL report ladle chemistry with Mo, Table 4 tensile / yield / 34% elongation / hardness, and heat-treatment condition. When A262 Practice E is ordered, those results appear as specified. Dual A213/SA-213 marking and third-party witness are available when written into the enquiry. A certificate missing molybdenum or using a wrong elongation minimum is not a complete TP317 release package.

Packaging and Shipping

TP317 tubes ship in capped or plugged bundles with weather protection matched to the route. Cut lengths for boiler and exchanger bundles are labeled by heat and size; export packing uses cases or steel-frame crates when required.

Marking includes ASTM A213, grade TP317 / UNS S31700, size, heat number, and SHH STEEL identification. Dual SA-213 marking appears only when the purchase order requests it. Packing lists track the same heat numbers shown on the EN 10204 3.1 certificates so the elevated molybdenum result stays tied to the shipped lengths.

Why Choose SHH STEEL

SHH STEEL treats ASTM A213 TP317 as a higher-molybdenum specification product: Mo 3.0–4.0%, Cr 18–20%, Ni 11–15%, Table 4 75/30 ksi, and elongation 34% minimum are checked together before a heat is offered. Quotations state OD × wall / BWG, wall basis, finish route, A262 options, and whether dual A213/SA-213 marking is required.

We refuse nickname assemblies that stamp TP316 as 317 without clearing the 3.0% molybdenum floor and the different Cr–Ni band. EN 10204 3.1 documentation includes Mo and the 34% elongation result. Compare sisters on the A213/A213M hub before freezing the exchanger tube list.

Supply Capability

SHH STEEL supplies ASTM A213 TP317 seamless stainless steel tube in cold-finished and hot-finished routes across the usual boiler, superheater, and heat-exchanger OD × wall / BWG band. Capability below is an enquiry range — not a frozen warehouse SKU or tonnage claim.

Capability SHH STEEL practice for TP317
Product form Seamless cold-finished and hot-finished tube
Standards ASTM A213 / A213M; dual SA-213 when PO asks
Size band Typical within ~1/8 in. ID to 5 in. OD; other diameters by agreement
Wall basis Minimum wall or average wall as specified
Documentation EN 10204 3.1 MTC with Mo 3–4% + 34% elong.; A262 / third-party witness on request
Trade terms FOB / CFR / CIF / EXW and other agreed Incoterms

Stock / Available sizes

SHH STEEL quotes TP317 against a stock-and-mill enquiry range rather than a frozen SKU/tonnage list. Representative OD × wall / BWG combinations for boiler and heat-exchanger tube appear below.

Item Typical stock / enquiry range for TP317
Outside diameter 19.05, 25.4, 31.8, 38.1, 42.4, 50.8, 60.3, 76.2 mm (and other boiler/HX ODs on enquiry; through the usual A213 ~5 in. [127 mm] band)
Wall / BWG BWG 10–18 class walls and metric min-wall equivalents; heavier walls by agreement
Common OD × wall examples 25.4 × 2.11 mm; 31.8 × 2.77 mm; 38.1 × 2.77 mm; 42.4 × 3.56 mm; 50.8 × 3.05 mm; 60.3 × 3.91 mm — illustrative, confirm min vs average wall
Length Cut lengths for boiler / exchanger bundles; bends and random mill lengths on enquiry
Special Non-standard OD/wall, bright anneal, dual A213/SA-213, A262 Practice E, third-party witness — confirm before heat reservation

Send OD × wall (or BWG), wall basis, finish route, quantity or cut list, marking (A213 or dual A213/SA-213), and Mo / A262 notes on one enquiry. We confirm C ≤0.08%, Cr 18–20% / Ni 11–15%, Mo 3.0–4.0%, Table 4 75/30 ksi, and elongation 34% minimum without inventing fake warehouse codes. Sisters A213 TP316, A213 TP317L, and A213 TP316LNM sit on the same hub.

FAQ

Is ASTM A213 the same as ASME SA-213 for TP317?
No. ASTM A213 / A213M is the ASTM International product specification for seamless boiler, superheater, and heat-exchanger tubes; ASME SA-213 / SA-213M is the separate ASME Code Book adoption. Dual-mark only when the purchase order asks for both names on the stencil and MTC. Chemistry and tensile floors align closely for a given referenced edition, but the standards remain independent documents.
Does ASTM A213 TP317 include welded or HCW tube?
No. ASTM A213 covers seamless boiler, superheater, and heat-exchanger tubes only. There is no WLD or HCW manufacturing-type letter under A213. Cold-finished versus hot-finished describes the seamless process route and dimensional tolerances — not a welded product form. Order welded stainless pipe under a different product standard when that form is required.
What is the chemistry of ASTM A213 TP317?
Melting analysis for TP317 / UNS S31700 is C ≤0.08%, Mn ≤2.00%, P ≤0.045%, S ≤0.030%, Si ≤1.00%, Cr 18.0–20.0%, Ni 11.0–15.0%, and Mo 3.0–4.0%, with nitrogen as a no-requirement ellipsis. Confirm the ordered A213 edition. Molybdenum’s 3.0% floor and the 18–20 / 11–15 Cr–Ni balance are mandatory — a 2.8% Mo heat is still a 316-family story, not TP317.
TP317 vs TP316 — why choose the higher molybdenum grade?
TP316 uses Mo 2.00–3.00%, Cr 16–18, Ni 10–14, and Table 4 elongation 35%. TP317 raises Mo to 3.0–4.0%, Cr to 18–20, Ni to 11–15, and prints elongation 34% with the same 75/30 ksi tensile/yield pair and hardness max 192 HBW / 90 HRB. Order TP317 when the datasheet names the higher Mo band; stay on TP316 when Mo 2–3% is sufficient.
TP317 vs TP317L — when do I need low carbon?
Both share Mo 3–4%, Cr 18–20, and Ni 11–15. TP317 allows C ≤0.08% and uses Table 4 elongation 34%. TP317L keeps C ≤0.035% and prints elongation 35% with the same 75/30 ksi tensile/yield pair. Choose TP317L for as-welded IGC strategy with higher Mo; choose TP317 when low carbon is not mandated.
Why is elongation 34% on TP317 instead of 35%?
ASTM A213 Table 4 prints 34% minimum elongation for TP317 / UNS S31700, while TP316 and TP317L print 35%. Receiving checklists copied from 316 heats often expect 35% and incorrectly reject a heat that clears 34%. Use the TP317 row on the ordered edition — do not import a sister grade’s elongation digit.
Does Table 4 set a hardness limit for TP317?
Yes. Table 4 lists hardness maximum 192 HBW / 200 HV or 90 HRB with 75 ksi tensile, 30 ksi yield, and 34% elongation. Hardness, molybdenum floor, Cr–Ni band, and elongation all belong on the release package — none replaces the others for 317 boiler or HX tube.
What heat treatment does A213 require for TP317?
Solution treatment at a minimum of 1900 °F [1040 °C], water quench or other rapid cool. Delivery is solution annealed and pickled unless bright anneal is agreed. No mandatory ASTM grain-size number appears for TP317 in the public heat-treatment table. Put A262 Practice E on the purchase order when IGC demonstration is contractual.
Minimum wall vs average wall for A213 TP317 — which should I specify?
Boiler and heat-exchanger datasheets almost always expect minimum wall. Average wall is allowed when the purchase order says so, with A1016/A1016M tolerances for that basis. State wall basis on the enquiry rather than relying on pipe schedule numbers as the primary A213 wall story.
Is TP317 a good choice for as-welded IGC-critical tube-to-tubesheet joints?
Often not as the first choice. Carbon up to 0.08% works against as-welded intergranular-corrosion strategy even when molybdenum is elevated. Many owners specify A213 TP317L for as-welded IGC duty with Mo 3–4%, and reserve TP317 for lists that need the higher Mo band without an L-grade carbon mandate. Put A262 Practice E on the PO when IGC demonstration is contractual.
Can I dual-certify TP317 with TP316 on the same heat?
No in any practical sense: the molybdenum bands do not overlap (TP316 max 3.00% versus TP317 min 3.0% is a knife-edge that still leaves Cr–Ni mismatched — TP317 needs Cr 18–20 / Ni 11–15, not 16–18 / 10–14). Order the grade the datasheet names rather than forcing a dual from a PMI gun that only reads "high Mo."
When should I step from TP317 to TP317LM or TP317LMN?
When the datasheet names Mo 4.0–5.0% families (and the matching Ni / N / Cu rows on those grades), not when a buyer simply wants "more Mo than 316." TP317 stops at Mo 3.0–4.0%. Open the TP317LM / TP317LMN pages on the A213/A213M hub when those chemistries are required — they are separate UNS rows, not nickname upgrades of TP317.

Conclusion

ASTM A213 TP317 / UNS S31700 is the higher-molybdenum seamless stainless steel tube for boiler, superheater, and heat-exchanger service when Mo 3.0–4.0% with Cr 18–20% / Ni 11–15% must sit above the 316-family Mo band. SHH STEEL supplies cold-finished and hot-finished seamless tube in the usual OD × wall / BWG band, solution annealed at 1900 °F [1040 °C], tested to Table 4 75/30 ksi, 34% elongation, and hardness limits, with molybdenum reported on EN 10204 3.1 certificates — dual SA-213 marking only when the purchase order asks.

Contact: admin@steelspecs.com

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X