ASTM A213 TP309HCb Stainless Steel Tube
What is ASTM A213 TP309HCb Stainless Steel Tube
ASTM A213 / A213M covers seamless ferritic and austenitic alloy-steel boiler, superheater, and heat-exchanger tubes. Grade TP309HCb / UNS S30941 combines the two control stories that split the 309 family: H-grade carbon held in a 0.04–0.10% band with ASTM grain size No. 7 or coarser, plus niobium stabilization at 10×C–1.10%, on a 22.0–24.0% chromium / 12.0–16.0% nickel austenitic. That combination exists for creep-range boiler and furnace duty where oxidation resistance, elevated-temperature carbon/grain-size controls, and Nb stabilization against sensitization are all contractual — not as a synonym stamp for A213 TP309H or A213 TP309Cb alone.
SHH STEEL can supply ASTM A213 TP309HCb stainless steel tube as seamless cold-finished and hot-finished product in the usual boiler, furnace, and heat-exchanger OD × wall / BWG band, shipped with EN 10204 3.1 mill test certificates that report the full ladle chemistry including niobium, the Table 4 tensile and hardness results, and the grain-size result for the heat-treatment lot. Dual A213 / SA-213 marking is available only when the purchase order asks for both independent standards. Browse 309-family grades on the A213/A213M hub.
Shop names such as 309HCb, 309HNb, S30941, or “H-grade niobium 309 tube” do not replace the ASTM grade on the MTC. Sister grades under the same ASTM standard include A213 TP309H, A213 TP309Cb, A213 TP309S, A213 TP347H, and A213 TP310HCb. A213 covers seamless tube only — cold-finished versus hot-finished is the process choice, not a WLD/HCW manufacturing-type letter.
Chemical Composition of A213 TP309HCb
Two chemistry layers matter for TP309HCb under ASTM A213. Melting analysis is mandatory for every heat; product analysis on finished tube applies only when Supplementary Requirement wording or the purchase order invokes it through ASTM A1016/A1016M, with tolerances typically from ASTM A480/A480M Table A1.1. Two lines drive selection before anything else: carbon 0.04–0.10% (H-grade floor and ceiling) and niobium 10×C–1.10%. An MTC that omits either carbon band compliance or niobium is incomplete for S30941. Nickel sits at 12.0–16.0% — the wider window shared with TP309Cb, not the 12.0–15.0% window of TP309H.
The tables below reproduce the melt limits for TP309HCb / UNS S30941, the product-analysis limits from A480 Table A1.1, and a short snapshot against TP309H and TP309Cb. Values are maximum unless a range is shown; ellipsis (…) means no requirement.
Melting analysis (heat / ladle analysis)
| Element | TP309HCb (UNS S30941) melting analysis |
|---|---|
| Carbon (C) | 0.04 – 0.10 |
| Manganese (Mn) | ≤ 2.00 |
| Phosphorus (P) | ≤ 0.045 |
| Sulfur (S) | ≤ 0.030 |
| Silicon (Si) | ≤ 1.00 |
| Chromium (Cr) | 22.0 – 24.0 |
| Nickel (Ni) | 12.0 – 16.0 |
| Molybdenum (Mo) | … (no requirement) |
| Nitrogen (N) | … (no requirement) |
| Niobium (Nb / Cb) | 10×C – 1.10 |
Source: ASTM A213/A213M stainless chemistry table for Grade TP309HCb / UNS S30941 (public mill / specification PDF excerpt — htpipe A213 table text). Confirm the ordered edition on the purchase order. Stainless table number is edition-dependent (Table 2 later / Table 1 older).
Product analysis — A480/A480M Table A1.1 tolerances applied
| Element | Melting | Tolerance (A480 A1.1) | Product analysis limit |
|---|---|---|---|
| Carbon (C) | 0.04 – 0.10 | 0.01 under / over | 0.03 – 0.11 |
| Manganese (Mn) | ≤ 2.00 | 0.04 over | ≤ 2.04 |
| Phosphorus (P) | ≤ 0.045 | 0.010 over | ≤ 0.055 |
| Sulfur (S) | ≤ 0.030 | 0.005 over | ≤ 0.035 |
| Silicon (Si) | ≤ 1.00 | 0.05 over | ≤ 1.05 |
| Chromium (Cr) | 22.0 – 24.0 | 0.25 under / over | 21.75 – 24.25 |
| Nickel (Ni) | 12.0 – 16.0 | 0.15 under / over | 11.85 – 16.15 |
| Niobium (Nb) | 10×C – 1.10 | 0.05 under / over on max; min remains formula-tied | max ≤ 1.15; min still ≥10×C on melt basis — confirm A480 path if contractual |
Carbon / Nb / Ni snapshot — TP309H / TP309Cb / TP309HCb
| Element | TP309H (S30909) | TP309Cb (S30940) | TP309HCb (S30941) |
|---|---|---|---|
| C | 0.04 – 0.10 | ≤ 0.08 | 0.04 – 0.10 |
| Ni | 12.0 – 15.0 | 12.0 – 16.0 | 12.0 – 16.0 |
| Nb (Cb) | … | 10×C – 1.10 | 10×C – 1.10 |
| Grain size | No. 7 or coarser | no mandatory number | No. 7 or coarser |
Heats that meet TP309HCb chemistry can sometimes dual-certify toward TP309H or TP309Cb only when every overlapping row clears — including Nb for Cb duals and grain size for H duals. Ask for dual marking on the PO rather than assuming it from a PMI gun. Molybdenum remains a no-requirement ellipsis; chloride-heavy exchangers still step to Mo grades on the hub.
When product analysis is ordered, finished tube may read C 0.03–0.11%, Mn ≤2.04%, P ≤0.055%, S ≤0.035%, Si ≤1.05%, Cr 21.75–24.25%, and Ni 11.85–16.15%. Put any tighter project carbon floor or Nb floor on the purchase order before the heat is selected.
Mechanical Properties of A213 TP309HCb
ASTM A213 Table 4 sets the room-temperature tensile acceptance floor for TP309HCb at 75 ksi [515 MPa] tensile strength and 30 ksi [205 MPa] yield strength (0.2% offset), with elongation of 35% minimum in 2 in. or 50 mm and hardness max 192 HBW / 200 HV or 90 HRB — the same room-temperature pair as TP309H and TP309Cb. What distinguishes the grade mechanically in the product standard is the grain-size requirement: ASTM No. 7 or coarser, determined per heat-treatment lot, together with the chemistry controls that make HCb a separate row.
| Property | TP309HCb requirement |
|---|---|
| Tensile strength, min (Table 4) | 75 ksi [515 MPa] |
| Yield strength (0.2% offset), min (Table 4) | 30 ksi [205 MPa] |
| Elongation in 2 in. or 50 mm, min (Table 4) | 35% |
| Hardness, max (Table 4) | 192 HBW / 200 HV or 90 HRB |
| Grain size | ASTM No. 7 or coarser (per heat-treatment lot) |
Source: ASTM A213/A213M Table 4 for TP309HCb / UNS S30941 and H-grade grain-size language (public specification PDF excerpt — htpipe A213 heat-treatment table showing grain-size column “7” for TP309HCb). Mechanical property requirements do not apply to tubing smaller than 1/8 in. [3.2 mm] ID or thinner than 0.015 in. [0.4 mm] wall. Flattening and flaring tests sit beside tension and hardness on a lot basis.
A tensile-only MTC that omits grain size or niobium is incomplete for TP309HCb — ask for both the E112 result and the Nb result on the certificate before releasing the heat to fabrication.
Dimensions and Tolerances
Dimensional supply for ASTM A213 TP309HCb is tube language — OD × wall (minimum or average) and BWG / gauge — covering boiler, furnace, and heat-exchanger sizes rather than leading with ASME B36.19 pipe schedules. Usual A213 sizes run from about 1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD with min wall about 0.015–0.500 in. [0.4–12.7 mm]; other diameters by agreement. Boiler and superheater datasheets almost always assume a minimum-wall reading — state wall basis on the purchase order.
OD and wall variations follow ASTM A1016/A1016M as invoked by A213. Cold-finished tubes commonly hold tighter OD; hot-finished tubes allow wider windows. Cold-finished average wall is often summarized as ±10% of specified average wall; minimum-wall product follows A1016 minimum-wall tables. Confirm exact rows for the OD and finish on the ordered edition.
| Item | Typical A213 TP309HCb dimensional practice |
|---|---|
| Product form | Seamless only (cold-finished or hot-finished) |
| Usual size band | ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD; wall ~0.015–0.500 in. [0.4–12.7 mm] |
| Wall basis | Minimum wall (default for boiler / superheater) or average wall when specified |
| OD / wall tolerances | Per ASTM A1016/A1016M for finish route and size |
| Length | Cut lengths for boiler / furnace / HX bundles; mill random by agreement |
| Secondary note | B36.19 schedules only as a buyer cross-reference |
Put cut list, design metal temperature context, and end preparation on the enquiry. Minimum wall remains a first-class A213 concept for 309HCb the same way it does for other H-grade tube.
Equivalent Grades
Equivalence language around 309HCb tube often collapses plate, cast, and tube product forms into one nickname. ASTM A213 Grade TP309HCb / UNS S30941 is the governing designation for this article; EN and JIS wrought names that point to similar H+Nb high-Cr–Ni chemistry families are not automatic substitutes on an A213 MTC.
| Designation | Notes |
|---|---|
| ASTM A213 / A213M Grade TP309HCb | Governing ASTM seamless boiler / HX tube product standard for this article |
| UNS S30941 | Unified number in the stainless chemistry table |
| ASME SA-213 TP309HCb | Separate ASME Code Book adoption — dual-mark only when the PO asks |
| Related H without Nb | A213 TP309H — H carbon/grain-size, Ni 12–15, no Nb |
| Related Cb without H | A213 TP309Cb — Nb stabilization, C ≤0.08, no mandatory grain size |
| Related 18-8 H+Nb | A213 TP347H — H-grade Nb-stabilized at lower Cr–Ni |
| Related plate | A240 / SA240 flat product in the 309 family — order plate and tube under their own standards |
Dual A213/SA-213 marking is a purchase-order option. Compare TP309H, TP309Cb, and TP347H on their own ASTM A213 pages before swapping grades inside a furnace or boiler tube list.
Heat Treatment and Delivery Condition
TP309HCb under ASTM A213 is furnished solution treated at a minimum of 1900 °F [1040 °C], then quenched in water or cooled rapidly by other means. That Table 3 heat-treatment row also carries the ASTM grain-size requirement of No. 7 or coarser for the heat-treatment lot — the clause that separates HCb acceptance from ordinary TP309Cb solution treatment at the same temperature.
Cold-finished versus hot-finished is a process and dimensional route, not a substitute for the anneal or the grain-size check. Delivery condition for SHH STEEL TP309HCb is solution annealed and pickled (or bright annealed by agreement), with anneal temperature, quench method, niobium result, and E112 grain-size result on the EN 10204 3.1 certificate. Straightening, cutting, and end finishing follow heat treatment.
Supplementary Requirement S2 (stabilizing heat treatment) explicitly lists TP309HCb among the grades that shall be given a stabilizing treatment after the solution anneal when the purchaser specifies S2. Write S2 onto the purchase order when the datasheet requires that post-solution stabilizing hold — do not assume base A213 includes it automatically for every HCb shipment.
Corrosion Resistance
TP309HCb is selected for high-temperature oxidation resistance from the 22–24% Cr / 12–16% Ni balance, H-grade carbon and coarse-grain controls for creep-range duty, and niobium stabilization against chromium-carbide sensitization. It is not a molybdenum grade: in aqueous chloride pitting and crevice service, A213 TP316 / A213 TP316L remain the usual step-ups.
The H-grade carbon floor means TP309HCb is not marketed as an L-grade wet-IGC first choice; stabilization and H rules address different service concerns. ASTM A213 does not publish a corrosion-rate or oxidation-rate table for TP309HCb. When a project invokes Practice A262, S2 stabilizing, or a specific oxidation test, write those requirements onto the purchase order.
Applications of A213 TP309HCb Tube
TP309HCb shows up wherever seamless tube must survive hotter oxidizing environments than 18-8 is trusted for, and the datasheet also demands both H-grade carbon/grain-size controls and niobium stabilization — furnace tubes, radiant sections, heat-recovery exchangers, and boiler/superheater locations where oxidation, creep framing, and sensitization resistance all appear on the same grade callout.
| Application area | Typical use of TP309HCb tube | Selection note |
|---|---|---|
| Boiler / superheater (creep + oxidation + Nb) | Seamless tube where H rules and Nb stabilization both apply | Confirm design metal temperature and Code allowable |
| Furnace / radiant tubes | Oxidizing atmospheres with H+Cb acceptance | Open TP309H or TP309Cb if only one control story is needed |
| Heat-recovery / hot-gas HX | Hot oxidizing gas with elevated-temp and sensitization framing | Step to TP310HCb if higher Cr–Ni is specified |
| S2 stabilizing required | Post-solution stabilizing hold when PO specifies S2 | Write S2 on the enquiry |
| Aqueous chloride HX | Usually not the first 309HCb use case | Prefer Mo grades (TP316/TP316L) |
Stay on the A213/A213M hub for 309H, 309Cb, 347H, and 310HCb sisters rather than mixing A312 pipe certificates into tube acceptance.
Weldability
TP309HCb tube welds with matching or near-matching 309H / Nb-bearing austenitic filler for tube-to-tubesheet, attachment, and fabrication joins under a qualified WPS. ER309H or Nb-bearing deposits are common when the weld metal must carry H-grade carbon or stabilization philosophy; fabricators sometimes use 309L deposits for lower carbon in the weld metal when the joint design allows it. Heat input, interpass, and cleaning remain the fabricator’s code responsibility — A213 governs the seamless tube product, not the field weld procedure.
Because A213 TP309HCb is seamless, there is no mill longitudinal weld to radiograph as welded-pipe standards describe. Focus inspection on each-length hydro or NDE, joint quality, grain size and niobium on the MTC, and any contractual S2, IGC, or oxidation tests. Do not try to weld-procedure a plain TP309H or TP309Cb heat into an HCb datasheet — change the tube grade when both H and Cb are required.
Surface Finishes
Standard mill delivery for ASTM A213 TP309HCb is solution annealed and pickled. Bright annealing is a called-out route when a smoother reflective surface is needed. Specified Ra, light polish, and post-fabrication passivation are commercial extras on top of the A213 stamp.
Furnace and boiler tube often ships with a workmanlike pickled finish; cosmetic polish is uncommon unless the PO asks. End preparation for welding or expanding should be ordered with finish so receiving inspection shares one acceptance language. Grain-size and niobium reporting are metallurgical requirements on the MTC, not surface-finish options.
Inspection and Testing
Base ASTM A213 testing for TP309HCb includes heat analysis (with niobium), tension to the Table 4 75/30 ksi floors, hardness to the Table 4 maximum, grain size (ASTM No. 7 or coarser) per heat-treatment lot, flattening and flaring on a lot basis, and hydro or NDE of each length. The manufacturer may choose hydro versus NDE unless the purchase order fixes the method. Marking includes ASTM designation, grade, size, heat number, and other clause-required data.
| Option | Purpose |
|---|---|
| Product analysis | Confirms chemistry — including Nb — on finished tube |
| Grain-size reporting (mandatory for H) | E112 result on the MTC for the heat-treatment lot |
| Stabilizing heat treatment (S2) | TP309HCb is listed under S2 when the purchaser specifies it |
| Intergranular corrosion / oxidation tests | Only when Supplementary Requirements or OEM specs add them |
| Minimum vs average wall | States wall basis |
| Fixed hydro or NDE method | Removes manufacturer’s option |
| Third-party inspection / EN 10204 3.2 | Witnessed testing when the project requires it |
Ask the mill to state lot identity clearly so hardness, tension, grain-size, and Nb specimens map cleanly to the bundle you receive. An MTC without grain size or niobium is incomplete for TP309HCb.
Packaging and Shipping
TP309HCb tube leaves SHH STEEL bundled, end-protected, and tagged with ASTM A213 grade, OD × wall (or BWG), heat number, and PO reference. U-bent or specially cut furnace and boiler lengths need transit protection matched to bend radius and leg length. Export packing ranges from bare or wrapped bundles to wooden cases for bright-annealed or small-bore material.
We ship under the Incoterms on the order acknowledgement — FOB, CFR, CIF, EXW, or other agreed terms. Bilingual marks, inland trucking, and project color coding belong on the enquiry beside the metallurgical notes (carbon floor, Nb, grain size, S2, dual marking).
Why Choose SHH STEEL
SHH STEEL treats ASTM A213 TP309HCb as the combined H-grade and niobium-stabilized 309 tube product with enforceable chemistry, tensile, hardness, grain-size, and heat-treatment rules — not as a catalogue nickname for “any 309H or 309Cb tube.” Certificates report the stainless-table ladle chemistry with Nb, Table 4 set, and E112 grain size; dual A213/SA-213 marking appears only when requested.
If only H rules are needed without Nb, we open A213 TP309H. If only Nb is needed without H, we open A213 TP309Cb. If neither is needed, we open A213 TP309S. Wet chloride duty steers to the Mo family on the A213/A213M hub. Lead times mix near-term lengths with mill schedules; we say which is which.
Cut-to-length, U-bending, polish, S2 stabilizing, and third-party inspection are defined extras. The tube on site should match the ASTM callout the engineer wrote — including Nb and grain size on the MTC.
Supply Capability
SHH STEEL can supply ASTM A213 TP309HCb stainless steel tube against the edition and finish route on your enquiry. Capability and Stock / Available sizes below frame furnace, boiler, and HX enquiries for this H+Cb grade.
| Item | SHH STEEL capability for TP309HCb |
|---|---|
| Standard | ASTM A213 / A213M (dual SA-213 marking on request) Grade TP309HCb / UNS S30941 |
| Product form | Seamless only — cold-finished and hot-finished |
| Size | Typical OD × min wall (or average wall) in the A213 usual band; other diameters by agreement |
| Wall / gauge | Minimum wall or average wall; BWG / gauge accepted |
| Length | Cut-to-length for furnace / HX / boiler; mill random by agreement; bends on enquiry |
| Finish | Annealed and pickled; bright annealed or light polish by agreement |
| Testing | Tension (75/30 ksi), hardness (max 192 HBW / 90 HRB), grain size (No. 7 or coarser), flattening, flaring, hydro or NDE; full melt chemistry including Nb on MTC; S2 on request |
| Documents | EN 10204 3.1 with Nb and grain-size results; third-party / 3.2 on request |
| Trade terms | FOB / CFR / CIF / EXW and other agreed Incoterms |
Stock / Available sizes
SHH STEEL quotes TP309HCb against a stock-and-mill enquiry range rather than a frozen SKU/tonnage list. Representative OD × wall / BWG combinations for furnace, boiler, and heat-exchanger tube appear below.
| Item | Typical stock / enquiry range for TP309HCb |
|---|---|
| Outside diameter | 19.05, 25.4, 31.8, 38.1, 42.4, 50.8, 60.3, 76.2 mm (and other furnace/boiler ODs on enquiry; through the usual A213 ~5 in. [127 mm] band) |
| Wall / BWG | BWG 10–18 class walls and metric min-wall equivalents; heavier walls by agreement |
| Common OD × wall examples | 25.4 × 2.11 mm; 31.8 × 2.77 mm; 38.1 × 2.77 mm; 42.4 × 3.56 mm; 50.8 × 3.05 mm; 60.3 × 3.91 mm — illustrative, confirm min vs average wall |
| Length | Cut lengths for furnace / boiler / exchanger bundles; bends and random mill lengths on enquiry |
| Special | Non-standard OD/wall, bright anneal, dual A213/SA-213, S2 stabilizing, third-party witness — confirm before heat reservation |
Send OD × wall (or BWG), wall basis, finish route, quantity or cut list, marking (A213 or dual A213/SA-213), Nb and grain-size reporting expectation, S2 if required, and Supplementary Requirements on one enquiry. We confirm C 0.04–0.10%, Cr 22–24% / Ni 12–16%, Nb 10×C–1.10, Table 4 75/30 ksi, and ASTM No. 7 or coarser without inventing fake warehouse codes. Sisters A213 TP309H, A213 TP309Cb, and A213 TP347H sit on the same hub.
FAQ
-
Is ASTM A213 the same as ASME SA-213 for TP309HCb?
- No. ASTM A213 / A213M is the ASTM International product specification for seamless boiler, superheater, and heat-exchanger tubes; ASME SA-213 / SA-213M is the separate ASME Code Book adoption. Dual-mark only when the purchase order asks for both names on the stencil and MTC. Chemistry, tensile floors, and grain-size rules align closely for a given referenced edition, but the standards remain independent.
-
Does ASTM A213 TP309HCb include welded or HCW tube?
- No. ASTM A213 covers seamless tube only. There is no WLD or HCW manufacturing type under this product standard. Cold-finished versus hot-finished seamless tube is the process choice. Welded stainless pipe belongs to a different product standard and page family.
-
What is the chemistry of ASTM A213 TP309HCb?
- TP309HCb / UNS S30941 melt limits include carbon 0.04–0.10%, manganese ≤2.00%, phosphorus ≤0.045%, sulfur ≤0.030%, silicon ≤1.00%, chromium 22.0–24.0%, nickel 12.0–16.0%, and niobium 10×C–1.10%, with molybdenum and nitrogen as no-requirement ellipses. Product-analysis limits apply only when ordered, typically from A480 Table A1.1 via the A1016 path.
-
TP309HCb vs TP309H — when do I need niobium as well?
- Order TP309HCb when the datasheet needs both H-grade carbon/grain-size controls and niobium stabilization. Order TP309H when H rules alone are enough and Nb is a no-requirement ellipsis. Both share Table 4 75/30 ksi and ASTM No. 7 or coarser; TP309HCb also widens nickel to 12–16% and requires Nb 10×C–1.10. Do not treat "309HCb" as a synonym stamp for plain TP309H on the MTC.
-
TP309HCb vs TP309Cb — which A213 grade should I order?
- Order TP309HCb when the datasheet needs the H-grade carbon range (0.04–0.10%), grain-size controls (ASTM No. 7 or coarser), and Nb stabilization together. Order TP309Cb when niobium stabilization is required without H-grade carbon floor and mandatory grain size. Both share Nb 10×C–1.10 and Ni 12–16%; the H rules are what split them.
-
Why does A213 require grain size for TP309HCb?
- The H-grade grain-size requirement (ASTM No. 7 or coarser per heat-treatment lot) exists because elevated-temperature creep strength in austenitic stainless is sensitive to grain size. Coarser grains generally improve creep resistance. A tensile-only certificate that omits the E112 result is incomplete for TP309HCb acceptance under A213, even when niobium is reported.
-
What is Supplementary Requirement S2 for TP309HCb?
- S2 is the stabilizing heat treatment Supplementary Requirement. When the purchaser specifies S2, listed grades including TP309HCb shall be given a stabilizing treatment after the solution anneal. Base A213 solution treatment alone does not automatically include S2 — write it onto the purchase order when the datasheet requires the post-solution stabilizing hold.
-
Does Table 4 set a hardness limit for TP309HCb?
- Yes. Hardness maximum is 192 HBW / 200 HV or 90 HRB, alongside 75/30 ksi tensile/yield and 35% elongation. Hardness tests are part of lot acceptance under A213. Tighter project hardness windows must be written into the purchase order.
-
What heat treatment does A213 require for TP309HCb?
- Solution treatment at a minimum of 1900 °F [1040 °C] with water quench or other rapid cool, plus ASTM grain size No. 7 or coarser for the heat-treatment lot. Both cold-finished and hot-finished seamless tube follow that requirement. Ask the mill to state anneal temperature, quench method, niobium, and grain-size result on the EN 10204 3.1 certificate. Add S2 when stabilizing is required.
-
Minimum wall vs average wall for A213 TP309HCb — which do I order?
- Order minimum wall when the design assumes a guaranteed minimum thickness after tolerance — the usual boiler and superheater assumption. Order average wall only when the PO explicitly allows it and the designer accepts that basis. Put the wall basis on the enquiry before the mill selects A1016 tolerance tables.
-
Is TP309HCb a good choice for chloride-rich cooling water?
- Usually no as a first choice. TP309HCb is framed for high-temperature oxidation plus H-grade creep controls and Nb stabilization; it does not add molybdenum for aqueous chloride pitting. Prefer TP316/TP316L or higher-Mo grades on the A213 hub for seawater-leaning and brine exchangers.
-
Can you dual-certify A213 and SA-213 TP309HCb?
- Yes when the purchase order requests both independent standards on the stencil and MTC. Dual marking toward TP309H or TP309Cb is only possible on heats that also meet every overlapping chemistry and grain-size row — do not assume it from a carbon or PMI reading alone. Spell the required marking on the enquiry.
Conclusion
ASTM A213 TP309HCb / UNS S30941 is the H-grade niobium-stabilized 22–24% Cr / 12–16% Ni seamless stainless steel tube for boiler, furnace, and heat-exchanger service when oxidation resistance, creep-oriented carbon/grain-size controls, and Cb stabilization all drive grade selection. SHH STEEL supplies cold-finished and hot-finished seamless tube in the usual OD × wall / BWG band, solution annealed at 1900 °F [1040 °C], tested to Table 4 75/30 ksi and hardness limits with ASTM No. 7 or coarser grain size and niobium on the MTC, and documented on EN 10204 3.1 certificates — with dual SA-213 marking and S2 stabilizing only when the order asks. For sister 309H, 309Cb, and 347H grades, start from the A213/A213M hub, then send OD × wall, wall basis, Nb/grain-size expectation, and marking requirements so we can align mill and near-term availability.