ASTM A312/A312M

Product Showcase

ASTM A312/A312M Stainless Steel Products

SHH STEEL offers ASTM A312/A312M-compliant 304/316 stainless steel pipes. ASTM A312/A312M specifies seamless, welded, and heavily cold-worked austenitic stainless steel pipes for high-temperature and corrosive environments. Certified quality, competitive prices, customizable. Trust SHH STEEL!

ASTM A312 UNS S35315 Stainless Steel Pipe | ASTM A312 Stainless Steel - SHH STEEL

ASTM A312 UNS S35315 Stainless Steel Pipe

ASTM A312 UNS S35315 silicon-nitrogen-cerium heat-resistant stainless steel pipe in SML, WLD and HCW, with a Table 4 floor of 94/39 ksi welded or 87/38 ksi seamless and a 2010 °F [1100 °C] minimum anneal, supplied by SHH STEEL to B36.19 or special sizes with EN 10204 3.1 MTCs.
View More
ASTM A312 UNS S35045 Stainless Steel Pipe | ASTM A312 Stainless Steel - SHH STEEL

ASTM A312 UNS S35045 Stainless Steel Pipe

ASTM A312 UNS S35045 high-nickel, high-chromium heat-resistant stainless steel pipe in SML, WLD and HCW, with a Table 4 floor of 70/25 ksi and a 1900 °F [1040 °C] minimum anneal, supplied by SHH STEEL to B36.19 or special sizes with EN 10204 3.1 MTCs.
View More
ASTM A312 UNS S32053 Stainless Steel Pipe | ASTM A312 Stainless Steel - SHH STEEL

ASTM A312 UNS S32053 Stainless Steel Pipe

ASTM A312 UNS S32053 23Cr-25Ni-5.5Mo-N superaustenitic stainless steel pipe in SML, WLD and HCW, with a Table 4 floor of 93/43 ksi and a 1975–2155 °F [1080–1180 °C] anneal, supplied by SHH STEEL to B36.19 or special sizes with EN 10204 3.1 MTCs.
View More
ASTM A312 UNS S31730 Stainless Steel Pipe | ASTM A312 Stainless Steel - SHH STEEL

ASTM A312 UNS S31730 Stainless Steel Pipe

ASTM A312 UNS S31730 high-copper 3–4% molybdenum stainless steel pipe in SML, WLD and HCW, with a Table 4 floor of 70/25 ksi and a 1900 °F [1040 °C] minimum anneal, supplied by SHH STEEL to B36.19 or special sizes with EN 10204 3.1 MTCs.
View More
ASTM A312 UNS S31727 Stainless Steel Pipe | ASTM A312 Stainless Steel - SHH STEEL

ASTM A312 UNS S31727 Stainless Steel Pipe

ASTM A312 UNS S31727 copper-bearing 4% molybdenum nitrogen stainless steel pipe in SML, WLD and HCW, with a Table 4 floor of 80/36 ksi and a 1975–2155 °F [1080–1180 °C] anneal, supplied by SHH STEEL to B36.19 or special sizes with EN 10204 3.1 MTCs.
View More
ASTM A312 UNS S31726 Stainless Steel Pipe | ASTM A312 Stainless Steel - SHH STEEL

ASTM A312 UNS S31726 Stainless Steel Pipe

ASTM A312 UNS S31726 nitrogen-strengthened 4–5% molybdenum 317-type stainless steel pipe in SML, WLD and HCW, with a Table 4 floor of 80/35 ksi and a 1900 °F [1040 °C] minimum anneal, supplied by SHH STEEL to B36.19 or special sizes with EN 10204 3.1 MTCs.
View More
ASTM A312 UNS S31725 Stainless Steel Pipe | ASTM A312 Stainless Steel - SHH STEEL

ASTM A312 UNS S31725 Stainless Steel Pipe

ASTM A312 UNS S31725 4–5% molybdenum low-carbon 317-type stainless steel pipe in SML, WLD and HCW, with a Table 4 floor of 75/30 ksi and a 1900 °F [1040 °C] minimum anneal, supplied by SHH STEEL to B36.19 or special sizes with EN 10204 3.1 MTCs.
View More
ASTM A312 UNS S31655 Stainless Steel Pipe | ASTM A312 Stainless Steel - SHH STEEL

ASTM A312 UNS S31655 Stainless Steel Pipe

ASTM A312 UNS S31655 lean-nickel, nitrogen-strengthened stainless steel pipe in SML, WLD and HCW, with a Table 4 floor of 92/45 ksi and a 1900 °F [1040 °C] minimum anneal, supplied by SHH STEEL to B36.19 or special sizes with EN 10204 3.1 MTCs.
View More
ASTM A312 UNS S31277 Stainless Steel Pipe | ASTM A312 Stainless Steel - SHH STEEL

ASTM A312 UNS S31277 Stainless Steel Pipe

ASTM A312 UNS S31277 7% molybdenum superaustenitic stainless steel pipe in SML, WLD and HCW, with a Table 4 floor of 112/52 ksi and a 2050 °F [1120 °C] minimum anneal, supplied by SHH STEEL to B36.19 or special sizes with EN 10204 3.1 MTCs.
View More
ASTM A312 UNS S31272 Stainless Steel Pipe | ASTM A312 Stainless Steel - SHH STEEL

ASTM A312 UNS S31272 Stainless Steel Pipe

ASTM A312 UNS S31272 titanium-boron stabilized 15Cr-15Ni-Mo stainless steel pipe in SML, WLD and HCW, with a Table 4 floor of 65/29 ksi and a 1920 °F [1050 °C] minimum anneal, supplied by SHH STEEL to B36.19 or special sizes with EN 10204 3.1 MTCs.
View More
ASTM A312 UNS S31266 Stainless Steel Pipe | ASTM A312 Stainless Steel - SHH STEEL

ASTM A312 UNS S31266 Stainless Steel Pipe

ASTM A312 UNS S31266 high-strength tungsten-bearing superaustenitic stainless steel pipe in SML, WLD and HCW, with a Table 4 floor of 109/61 ksi and a 2100 °F [1150 °C] minimum anneal, supplied by SHH STEEL to B36.19 or special sizes with EN 10204 3.1 MTCs.
View More
ASTM A312 UNS S31254 Stainless Steel Pipe | ASTM A312 Stainless Steel - SHH STEEL

ASTM A312 UNS S31254 Stainless Steel Pipe

ASTM A312 UNS S31254 6% molybdenum superaustenitic stainless steel pipe in SML, WLD and HCW, with a Table 4 floor of 98/45 ksi (t ≤ 0.187 in.) or 95/45 ksi and a 2100 °F [1150 °C] minimum anneal, supplied by SHH STEEL to B36.19 or special sizes with EN 10204 3.1 MTCs.
View More

ASTM A312/A312M Stainless Steel Products

ASTM A312 UNS S35315 Stainless Steel Pipe ASTM A312 UNS S35045 Stainless Steel Pipe ASTM A312 UNS S32053 Stainless Steel Pipe ASTM A312 UNS S31730 Stainless Steel Pipe
ASTM A312 UNS S31727 Stainless Steel Pipe ASTM A312 UNS S31726 Stainless Steel Pipe ASTM A312 UNS S31725 Stainless Steel Pipe ASTM A312 UNS S31655 Stainless Steel Pipe
ASTM A312 UNS S31277 Stainless Steel Pipe ASTM A312 UNS S31272 Stainless Steel Pipe ASTM A312 UNS S31266 Stainless Steel Pipe ASTM A312 UNS S31254 Stainless Steel Pipe
ASTM A312 UNS S31050 Stainless Steel Pipe ASTM A312 UNS S31002 Stainless Steel Pipe ASTM A312 UNS S30815 Stainless Steel Pipe ASTM A312 UNS S30615 Stainless Steel Pipe
ASTM A312 UNS S30601 Stainless Steel Pipe ASTM A312 UNS S30600 Stainless Steel Pipe ASTM A312 UNS S30415 Stainless Steel Pipe ASTM A312 UNS S20400 Stainless Steel Pipe
ASTM A312 TP XM-29 Stainless Steel Pipe ASTM A312 TP XM-19 Stainless Steel Pipe ASTM A312 TP XM-11 Stainless Steel Pipe ASTM A312 TP XM-10 Stainless Steel Pipe
ASTM A312 TP348H Stainless Steel Pipe ASTM A312 TP348 Stainless Steel Pipe ASTM A312 TP347LN Stainless Steel Pipe ASTM A312 TP347H Stainless Steel Pipe
ASTM A312 TP347 Stainless Steel Pipe ASTM A312 TP321H Stainless Steel Pipe ASTM A312 TP321 Stainless Steel Pipe ASTM A312 TP317L Stainless Steel Pipe
ASTM A312 TP317 Stainless Steel Pipe ASTM A312 TP316Ti Stainless Steel Pipe ASTM A312 TP316N Stainless Steel Pipe ASTM A312 TP316LN Stainless Steel Pipe
ASTM A312 TP316L Stainless Steel Pipe ASTM A312 TP316H Stainless Steel Pipe ASTM A312 TP316 Stainless Steel Pipe ASTM A312 TP310S Stainless Steel Pipe
ASTM A312 TP310HCb Stainless Steel Pipe ASTM A312 TP310H Stainless Steel Pipe ASTM A312 TP310Cb Stainless Steel Pipe ASTM A312 TP309S Stainless Steel Pipe
ASTM A312 TP309HCb Stainless Steel Pipe ASTM A312 TP309H Stainless Steel Pipe ASTM A312 TP309Cb Stainless Steel Pipe ASTM A312 TP304N Stainless Steel Pipe
ASTM A312 TP304LN Stainless Steel Pipe ASTM A312 TP304H Stainless Steel Pipe ASTM A312 TP304L Stainless Steel Pipe ASTM A312 TP304 Stainless Steel Pipe
ASTM A312 TP201LN Stainless Steel Pipe ASTM A312 TP201 Stainless Steel Pipe
Stainless Steel Pipes and Tubes supplier and exporter

Stainless Steel Pipes and Tubes

SHH STEEL, a premier Stainless Steel Pipes and Tubes exporter, produces and exports stainless steel pipes and tubes for chemical, marine, and food processing industries. Our seamless and welded products, like 304 and 316L (ASTM A312), ensure corrosion resistance and strength. With a 5,000-ton inventory, we deliver in 3–5 days, backed by SGS/TUV inspections and mill certificates. Choose SHH STEEL for seamless stainless steel pipes and custom solutions.

Stainless Steel Pipes and Tubes

SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

    *

    *

    *

    *


    X