ASTM A213 TP201 Stainless Steel Tube | ASTM A213 Stainless Steel - SHH STEEL

ASTM A213 TP201 Stainless Steel Tube

ASTM A213 TP201 / UNS S20100 seamless boiler, superheater and heat-exchanger tube — a manganese-nitrogen austenitic with Mn 5.5–7.5%, Ni 3.5–5.5%, Cr 16.0–18.0%, N ≤0.25% and C ≤0.15%. Under A213 Table 4 the floor is 95/38 ksi with hardness max 219 HBW / 95 HRB. SHH STEEL supplies cold-finished and hot-finished seamless tube with EN 10204 3.1 MTCs.
Grade
TP201 / UNS S20100
Standard
ASTM A213 / A213M
Product form
Seamless boiler / superheater / heat-exchanger tube (cold-finished and hot-finished)
Size
Typical OD × min wall (or average wall) within ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD and ~0.015–0.500 in. [0.4–12.7 mm] wall; other diameters by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is ASTM A213 TP201 Stainless Steel Tube

ASTM A213 / A213M is the ASTM International product specification for seamless ferritic and austenitic alloy-steel boiler, superheater, and heat-exchanger tubes. Grade TP201 sits inside that stainless table as the lean manganese-nitrogen austenitic UNS S20100: carbon ≤0.15%, manganese 5.5–7.5%, chromium 16.0–18.0%, nickel only 3.5–5.5%, and nitrogen ≤0.25%. The Mn–N pair holds the austenite while nickel stays well below the classic 18-8 band, which is why buyers looking at nickel cost or availability still write TP201 on heat-exchanger and moderate-duty boiler tube enquiries — provided the fluid chemistry and temperature justify a leaner stainless than A213 TP304.

SHH STEEL can supply ASTM A213 TP201 stainless steel tube as seamless cold-finished and hot-finished product in the usual boiler and heat-exchanger OD × wall / BWG band, shipped with EN 10204 3.1 mill test certificates that report the full ladle chemistry and the Table 4 tensile and hardness results. When a project also needs ASME Code Book marking, we dual-mark A213 / SA-213 on the same lengths only if the purchase order says so — ASTM A213 and ASME SA-213 remain two independent standards. Browse the grade family on the A213/A213M hub.

Commercially, TP201 tube is still called 201, S20100, or Mn–N boiler/HX tube; none of those shop names replace the ASTM grade on the MTC or stencil. Sister grades under the same ASTM standard include A213 TP202 (higher Mn and Cr band), A213 TP304 / A213 TP304L, and the molybdenum grades A213 TP316 / A213 TP316L. A213 covers seamless tube only — there is no welded or HCW manufacturing type under this product standard — so cold-finished versus hot-finished seamless route is the finish/process choice, not a WLD/HCW stencil letter.

Chemical Composition of A213 TP201

Two chemistry layers matter for TP201 under ASTM A213. The melting (heat or ladle) analysis is mandatory for every heat, while product analysis on finished tube applies only when Supplementary Requirement wording or the purchase order invokes product analysis through the general requirements in ASTM A1016/A1016M. Product-analysis tolerances are not reprinted as a standalone chemistry table inside A213 itself; when ordered, they typically flow from ASTM A480/A480M Table A1.1 via that general-requirements path. SHH STEEL reports the actual ladle values — and the product values when ordered — and does not advertise tighter catalogue chemistry windows that the ASTM standard does not publish.

The tables below reproduce the heat analysis for TP201 / UNS S20100 and the product-analysis limits that result from applying A480 Table A1.1 tolerances. Values are maximum unless a range is shown. Later A213 editions place austenitic stainless grades in Table 2 (older editions used Table 1); confirm the ordered edition on the purchase order before treating any secondary catalogue as the acceptance text.

Melting analysis (heat / ladle analysis)

Element TP201 (UNS S20100) melting analysis
Carbon (C) ≤ 0.15
Manganese (Mn) 5.5 – 7.5
Phosphorus (P) ≤ 0.060
Sulfur (S) ≤ 0.030
Silicon (Si) ≤ 1.00
Chromium (Cr) 16.0 – 18.0
Nickel (Ni) 3.5 – 5.5
Molybdenum (Mo) … (no requirement)
Nitrogen (N) ≤ 0.25

Source: ASTM A213/A213M stainless chemistry table for Grade TP201 / UNS S20100 (public mill / specification summaries cross-checked — htpipe A213 PDF table text, Gangsteel / Ferrobend A213 grade pages). Confirm the ordered edition on the purchase order. Nitrogen analysis method is a matter of agreement between purchaser and producer per the standard’s nitrogen footnote.

Product analysis — A480/A480M Table A1.1 tolerances applied

Element Melting Tolerance (A480 A1.1) Product analysis limit
Carbon (C) ≤ 0.15 0.01 over ≤ 0.16
Manganese (Mn) 5.5 – 7.5 0.05 under / 0.06 over 5.45 – 7.56
Phosphorus (P) ≤ 0.060 0.010 over ≤ 0.070
Sulfur (S) ≤ 0.030 0.005 over ≤ 0.035
Silicon (Si) ≤ 1.00 0.05 over ≤ 1.05
Chromium (Cr) 16.0 – 18.0 0.20 under / over 15.80 – 18.20
Nickel (Ni) 3.5 – 5.5 0.07 under / 0.10 over 3.43 – 5.60
Nitrogen (N) ≤ 0.25 0.02 over ≤ 0.27

Read the Mn and N lines first: they are what make TP201 a lean austenitic rather than a nickel-heavy 18-8. Chromium at 16–18% builds the passive film; nickel at 3.5–5.5% is deliberately lean; carbon ≤0.15% sits above an L-grade ceiling, so as-welded sensitization risk needs an honest conversation before tube-to-tubesheet joints go into service without a post-weld solution anneal. Versus A213 TP202, TP201 carries the lower manganese band (5.5–7.5 vs 7.5–10.0) and a slightly leaner chromium window — the two grades are sisters, not substitutes.

When product analysis is ordered, finished tube may read up to C 0.16%, Mn 7.56%, P 0.070%, S 0.035%, Si 1.05%, and N 0.27%, with Cr 15.80–18.20% and Ni 3.43–5.60%. Those are the only product limits we quote from the A480 A1.1 path. Put any tighter project carbon, sulfur, or nitrogen ceiling on the purchase order before the heat is selected.

Mechanical Properties of A213 TP201

ASTM A213 Table 4 sets the tensile acceptance floor for TP201 at 95 ksi [655 MPa] tensile strength and 38 ksi [260 MPa] yield strength (0.2% offset), with elongation of 35% minimum in 2 in. or 50 mm. That 95 ksi tensile floor is noticeably higher than the 75 ksi floor A213 lists for TP304 — manganese and nitrogen strengthen the austenite, and the product standard captures that in the Table 4 row rather than leaving it as a catalogue claim. Hardness maximum is 219 HBW / 230 HV or 95 HRB, and hardness tests are part of the lot acceptance scheme under A213.

Property TP201 requirement (Table 4)
Tensile strength, min 95 ksi [655 MPa]
Yield strength (0.2% offset), min 38 ksi [260 MPa]
Elongation in 2 in. or 50 mm, min 35%
Hardness, max 219 HBW / 230 HV or 95 HRB

Source: ASTM A213/A213M Table 4 for TP201 / UNS S20100 (public specification summaries — htpipe A213 PDF, Blackburn Metals A213 tubular excerpt). Mechanical property requirements do not apply to tubing smaller than 1/8 in. [3.2 mm] inside diameter or thinner than 0.015 in. [0.4 mm] wall. Flattening and flaring tests are also required on a lot basis for finished tube; they sit beside tension and hardness rather than replacing them.

Do not import A312 pipe tensile numbers onto an A213 tube enquiry for this grade — A312 TP201 historically carried a different Table 4 pair, and the tube product standard’s 95/38 ksi floor is what the MTC must clear. Actual mill certificates often clear the floor with margin, but design calculations should still use Table 4 unless the purchase order states higher guaranteed values that the mill has accepted in writing.

Dimensions and Tolerances

Dimensional supply for ASTM A213 TP201 is tube language — outside diameter × wall thickness (minimum wall or average wall) and, commercially, BWG / gauge — not ASME B36.19 pipe schedules as the primary size story. The sizes usually furnished under A213 run from about 1/8 in. [3.2 mm] inside diameter to 5 in. [127 mm] outside diameter, with minimum wall from about 0.015 to 0.500 in. [0.4 to 12.7 mm]; tubing with other diameters may be furnished when all other requirements of the specification are met. State on the purchase order whether wall is minimum or average, because that choice changes how the mill interprets tolerance and how the designer reads remaining wall after fabrication.

Outside-diameter and wall variations follow ASTM A1016/A1016M as invoked by A213, with cold-finished and hot-finished routes carrying different practical bands. Cold-finished tubes commonly hold tighter OD control; hot-finished tubes allow wider OD and wall windows. Permissible variations from a specified average wall for cold-finished tube are often summarized as ±10% of the specified average wall, while minimum-wall product is accepted to the A1016 minimum-wall tables rather than a symmetric ± window. Confirm the exact A1016 rows for the OD and finish route on the ordered edition.

Item Typical A213 TP201 dimensional practice
Product form Seamless only (cold-finished or hot-finished)
Usual size band ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD; wall ~0.015–0.500 in. [0.4–12.7 mm] min (or average wall if PO says so)
Wall basis Minimum wall (default commercial practice) or average wall when specified
OD / wall tolerances Per ASTM A1016/A1016M for the finish route and size; cold-finished average wall often ±10%
Length Cut lengths for HX / boiler bundles, or mill random lengths by agreement
Secondary size note ASME B36.19 schedules may appear only when a buyer asks for a pipe-schedule cross-reference — not as the primary A213 size callout

Put the cut list, U-bend or straight-tube preference, and end preparation on the enquiry so mill and stock lengths can be mixed efficiently. Minimum wall is a first-class A213 concept: if the datasheet assumes average wall, say so explicitly before the heat is rolled.

Equivalent Grades

Equivalence language around TP201 tube is often looser than a boiler or heat-exchanger purchase order can afford. ASTM A213 Grade TP201 / UNS S20100 is the governing designation for this article; EN 1.4372 and JIS SUS201 are approximate wrought names that point to similar Mn–N chemistry families but are not automatic substitutes on an A213 mill test certificate. When a datasheet says “equivalent to 201,” confirm which product standard, tensile/hardness table, and heat-treatment clause the mill will actually certify.

Designation Notes
ASTM A213 / A213M Grade TP201 Governing ASTM seamless boiler / HX tube product standard for this article
UNS S20100 Unified number listed in the stainless chemistry table
ASME SA-213 TP201 Separate ASME Code Book adoption of the A213 grade text — dual-mark only when the PO asks
EN 1.4372 (X12CrMnNiN17-7-5) Approximate wrought Mn–N stainless designation; order EN tube forms under the relevant EN tube specs
JIS SUS201 Approximate Japanese grade name; confirm the Japanese tube product standard when ordering JIS product
Related plate A240 / SA240 flat product in the same UNS family — order plate and tube under their own product standards

ASME SA-213 TP201 is the separate Code Book adoption of the same grade text; dual A213/SA-213 marking is a purchase-order option, not a claim that the two standards are one document. Compare TP202 and the 18-8 sisters on their own ASTM A213 pages before swapping grades in a tube bundle on nickel-cost alone.

Heat Treatment and Delivery Condition

TP201 under ASTM A213 is furnished solution treated at a minimum of 1900 °F [1040 °C], then quenched in water or cooled rapidly by other means at a rate sufficient to prevent carbide reprecipitation. That heat-treatment row applies to both cold-finished and hot-finished seamless tube. Skipping or under-cooling the solution treatment can leave a structure that sensitizes in service even when ladle chemistry looked acceptable on paper — a real concern for a grade whose carbon ceiling sits at 0.15%.

Cold-finished versus hot-finished is a process and dimensional route, not a substitute for the anneal: cold-finished tube is typically drawn after hot working and then solution treated; hot-finished tube may be quenched after hot forming when the edition allows and finishing temperature is not below the minimum anneal. Delivery condition for SHH STEEL TP201 is solution annealed and pickled (or bright annealed by agreement), with heat-treatment temperature and quench method stated on the EN 10204 3.1 certificate. Straightening, cutting, and end finishing follow heat treatment.

When Supplementary Requirement language for intergranular-corrosion capability (commonly tied to ASTM A262 Practice E on specimens representative of the as-shipped condition for non-L grades) is ordered, the corrosion test report travels with the heat-treatment record. Do not treat a verbal “annealed” note as proof that the 1900 °F minimum and rapid cool were actually applied — ask for the temperature and quench method on the MTC.

Corrosion Resistance

TP201’s chromium-rich passive film handles many oxidizing process fluids, clean steam-side and water-side duties, and mild organic media that do not lean heavily on chlorides. Because nickel is lean and molybdenum is absent, pitting and crevice resistance in chloride-bearing waters sits below classic A213 TP304 and well below A213 TP316. Nitrogen helps a little on the PREN arithmetic, but it does not turn TP201 into a chloride-service grade. Coastal cooling circuits, brines, and many seawater-leaning exchangers are the wrong place to stretch this chemistry.

Intergranular corrosion risk after tube-to-tubesheet welding or after sensitizing thermal cycles is higher than for L grades because carbon may run up to 0.15%. Control that risk by solution treating after fabrication when the sequence allows, by invoking the contractual A262 Practice E test on the tube PO, or by stepping to a low-carbon or stabilized sister grade when as-welded service is non-negotiable. ASTM A213 itself does not publish a corrosion-rate table for TP201; selection remains engineering judgment against fluid, temperature, velocity, and inspection philosophy. SHH STEEL will not rank TP201 as equal to 304 or 316 in chlorides — that claim is not supported by the product standard.

Applications of A213 TP201 Tube

TP201 seamless tube under A213 shows up where nickel cost or availability pushes buyers toward a Mn–N austenitic, and where the process fluid is oxidizing or only mildly corrosive. It is not a universal stand-in for TP304 boiler tube: design metal temperature, chloride load, and weld procedure still decide whether the lean chemistry is acceptable. The table below pairs typical application areas with a selection note so the grade is chosen for the duty — not only for the familiar “201” name on the BOM.

Application area Typical use of TP201 tube Selection note
Utility / process heat exchangers Straight and U-bend HX tubes in low-chloride utility and process exchangers State min vs average wall, BWG, and bend radius; confirm chloride level
Moderate-temperature steam / condensate Seamless tube where A213 documentation is preferred and Ni cost is sensitive Not a creep-range H-grade substitute — open TP304H for that framing
Food / beverage utilities (non-chloride) Utility HX where 201 stainless tube is accepted by the end user Follow hygiene finish and welding procedure requirements
General corrosive tube duty (mild) Oxidizing or organic media that do not demand molybdenum Step to TP304/TP316 if chlorides or IGC risk rise
Cost-sensitive replacements Projects comparing Ni-lean tube against 18-8 on total installed cost Run corrosion and weld reviews before substituting for TP304

For as-welded tube-to-tubesheet joints in sensitizing service prefer an L grade or a post-weld solution anneal; for chloride-rich cooling water move to molybdenum grades on the same A213/A213M hub; for a Mn–N sister with a higher Cr/Mn band open A213 TP202.

Weldability

TP201 tube welds with matching or near-matching austenitic filler for tube-to-tubesheet joints, attachment welds, and fabrication joins, but the higher carbon ceiling and lean nickel demand more discipline than TP304L. Common practice uses ER201 / ER308L-family fillers under a qualified WPS, with heat-input and interpass limits written to limit sensitization in the HAZ. Many fabricators prefer a low-carbon deposit even when the base tube is standard TP201. Heat input control, interpass limits, and post-weld cleaning remain the fabricator’s responsibility under the applicable boiler or pressure-vessel code — A213 governs the seamless tube product, not the field or shop weld procedure.

Because A213 TP201 is seamless, there is no mill longitudinal weld to radiograph the way welded pipe standards describe. Focus inspection language on tube integrity (hydro or NDE of each length), tube-to-tubesheet joint quality, and any contractual corrosion test on the base metal. For tube that will enter service as-welded in a sensitizing environment, many owners either solution-treat after welding or change the base metal to a low-carbon sister rather than relying on a perfect weld procedure alone. Specify end preparation and surface finish on the tube PO when orbital or clean-service joins are planned.

Surface Finishes

Standard mill delivery for ASTM A213 TP201 is solution annealed and pickled, leaving a clean matte finish suitable for most boiler and heat-exchanger tube duty. Bright annealing under protective atmosphere produces a smoother reflective surface used on some clean-process and instrumentation tube lines and must be called out because it changes the heat-treatment route. Light polish or specified Ra on the bore or OD is a commercial or service-center operation on top of A213 product, not automatic with the grade stamp.

When a hygienic or fouling-sensitive exchanger specification quotes an Ra maximum on the bore, put it on the tube purchase order with its own acceptance language and sampling plan. SHH STEEL stencils grade and heat treatment as standard requirements; polish, special OD grind, and passivation after fabrication remain commercial extras unless the contract says otherwise. End preparation (plain, slightly beveled, or as needed for tube expanding) should be ordered together with finish so receiving inspection shares one acceptance language.

Inspection and Testing

Base ASTM A213 testing for TP201 includes heat analysis, tension tests to the Table 4 floors (95/38 ksi), hardness tests to the Table 4 maximum (219 HBW / 95 HRB), flattening and flaring tests on a lot basis, and either hydrostatic testing or nondestructive electric testing of each length. The manufacturer may choose hydro versus NDE unless the purchase order fixes the method; both are acceptance routes inside the product standard, not informal upgrades. Marking includes the ASTM designation, grade, size, heat number, and other clause-required data so receiving inspection can tie each length back to the MTC.

Supplementary Requirements commonly added on TP201 tube orders are summarized below. Invoke them by number or clear purchase-order wording; mills will not assume product analysis or intergranular-corrosion testing from a verbal “full certs” note.

Option Purpose
Product analysis Confirms chemistry on finished tube (via A1016 / PO language)
Intergranular corrosion A262 Practice E (or agreed practice) as a contractual Supplementary Requirement
Minimum vs average wall States which wall basis the size callout uses
Fixed hydro or NDE method Removes manufacturer’s option when the end user mandates one route
Third-party inspection / EN 10204 3.2 Witnessed testing and certificate when the project requires it

Lot definitions for continuous heat treatment or direct quench after hot forming follow the size-based lot sizes in A213; ask the mill to state lot identity clearly on the certificate so hardness and tension specimens map cleanly to the bundle you receive.

Packaging and Shipping

TP201 tube leaves SHH STEEL bundled, capped or end-protected, and tagged for export or domestic delivery according to the length mix and bend form on the order. Bundle tags repeat the ASTM A213 grade, OD × wall (or BWG), heat number, and PO reference so site receiving can check the shipment without opening every certificate packet first. U-bent tubes need extra cradle or case protection so bend radii and legs are not distorted in transit.

Export packing can be bare bundles, wrapped bundles, or wooden-cased lengths for bright-annealed, polished, or small-bore material. We ship under the Incoterms on the order acknowledgement — FOB, CFR, CIF, EXW, or other agreed terms. Inland trucking, bilingual destination marks, or project color coding for bundle tags should be stated on the enquiry beside the metallurgical notes.

Why Choose SHH STEEL

SHH STEEL treats ASTM A213 TP201 as a product standard with enforceable chemistry, tensile, hardness, heat-treatment, and marking rules — not as a catalogue nickname for “any 201 tube.” The MTC reports the full ladle chemistry and the Table 4 tensile/hardness set (95/38 ksi, 219 HBW / 95 HRB); the stencil carries seamless tube identity under A213; and dual A213/SA-213 marking is offered only when requested so Code and non-Code jobs stay cleanly documented.

We keep the Mn–N conversation honest for boiler and HX duty. If chlorides dominate the cooling water or process fluid, we steer toward A213 TP316 / A213 TP316L. If the project wants a classic 18-8 with higher nickel, we open A213 TP304 / A213 TP304L. If a sister Mn–N grade with the higher manganese band is preferred, we open A213 TP202. The A213/A213M hub is organized the same way — grade by grade under ASTM, seamless tube only.

Lead times combine near-term stock lengths with mill schedules; we say which is which on the quotation. Cut-to-length, U-bending, polish, and third-party inspection are defined extras. The tube that arrives should match the ASTM callout the engineer wrote, with paperwork a third-party inspector can read without translation.

Supply Capability

SHH STEEL can supply ASTM A213 TP201 stainless steel tube against the edition and finish route named on your enquiry. The capability table below summarizes the sizes, finishes, and documents we regularly quote for this grade, followed by the Stock / Available sizes map buyers ask for when they need a quick sense of what to enquire against for boiler and heat-exchanger duty.

Item SHH STEEL capability for TP201
Standard ASTM A213 / A213M (dual SA-213 marking on request) Grade TP201 / UNS S20100
Product form Seamless only — cold-finished and hot-finished
Size Typical OD × min wall (or average wall) in the A213 usual band; other diameters by agreement
Wall / gauge Minimum wall or average wall; BWG / gauge callouts accepted on enquiry
Length Cut-to-length for HX / boiler bundles; mill random by agreement; U-bends on enquiry
Finish Annealed and pickled; bright annealed or light polish by agreement
Testing Tension (95/38 ksi), hardness (max 219 HBW / 95 HRB), flattening, flaring, hydro or NDE per length; full ladle chemistry on MTC; product analysis / IGC on order
Documents EN 10204 3.1 with full ladle chemistry; third-party inspection / 3.2 on request
Trade terms FOB / CFR / CIF / EXW and other agreed Incoterms

Stock / Available sizes

SHH STEEL quotes TP201 tube against a practical stock-and-mill enquiry range rather than a frozen warehouse SKU list. The sizes below are the OD × wall / BWG combinations buyers most often request for utility and process heat-exchanger tube in the Mn–N family; availability of any single line on a given week depends on mill drawing and our inbound schedule, so treat the table as a supply map for enquiry — not a guarantee that every line sits on the floor with a published tonnage.

Item Typical stock / enquiry range for TP201
Outside diameter 12.7, 15.88, 19.05, 25.4, 31.8, 38.1, 50.8 mm (and other HX/boiler ODs on enquiry; up through the usual A213 ~5 in. [127 mm] band)
Wall / BWG BWG 12–20 class walls and metric min-wall equivalents; lighter and heavier walls by agreement
Common OD × wall examples 19.05 × 1.65 mm; 19.05 × 2.11 mm; 25.4 × 2.11 mm; 25.4 × 2.77 mm; 31.8 × 2.77 mm; 38.1 × 2.77 mm — illustrative HX sizes, confirm min vs average wall
Length Cut lengths for exchanger bundles; U-bends and straight random lengths on enquiry
Special Non-standard OD/wall, bright anneal, polished bore, and dual A213/SA-213 marking — confirm on enquiry before the heat is reserved

When you send an enquiry, list OD × wall (or BWG), wall basis (minimum or average), cold-finished or hot-finished preference, quantity or cut list, required marking (A213 alone or dual A213/SA-213), and any Supplementary Requirements. We reply with what we can ship from near-term stock versus what needs a mill run, without inventing fake warehouse codes or tonnage claims.

Send the size list, finish route, quantity or cut lengths, required marking (A213 or dual A213/SA-213), Supplementary Requirements, and destination on one enquiry. We will confirm chemistry, tensile, and hardness against the stainless chemistry table and Table 4, state what ships from near-term availability versus mill production, and keep the offer aligned with the ASTM A213 / A213M product standard that governs this page. Related grades such as A213 TP202, A213 TP304, and A213 TP XM-19 sit on the same hub when the datasheet steps beyond lean TP201.

FAQ

Is ASTM A213 the same as ASME SA-213 for TP201?
No. ASTM A213 / A213M is the ASTM International product specification for seamless boiler, superheater, and heat-exchanger tubes; ASME SA-213 / SA-213M is the separate ASME Code Book adoption of that grade text. Chemistry, tensile, and hardness floors align closely for a given referenced edition, but they remain two independent standards. Dual-mark A213/SA-213 tube only when the purchase order asks for both names on the stencil and MTC.
Does ASTM A213 TP201 include welded or HCW tube?
No. ASTM A213 covers seamless tube only. There is no WLD or HCW manufacturing type under this product standard the way ASTM A312 describes pipe. The process choice for TP201 under A213 is cold-finished versus hot-finished seamless tube, plus the heat-treatment and testing clauses of the ordered edition. If you need welded stainless pipe, that is a different product standard and a different steelspecs page family.
Minimum wall vs average wall — which should I order for A213 TP201?
Order minimum wall when the design and datasheet are written around a guaranteed minimum thickness after tolerance. Order average wall only when the purchase order explicitly allows average-wall product and the designer has accepted that basis. The two readings produce different tube from the same OD × wall line, so put the wall basis on the enquiry before the mill selects tooling and tolerance tables from A1016.
What is the UNS number and chemistry of ASTM A213 TP201?
TP201 is UNS S20100. Melting limits include carbon ≤0.15%, manganese 5.5–7.5%, phosphorus ≤0.060%, sulfur ≤0.030%, silicon ≤1.00%, chromium 16.0–18.0%, nickel 3.5–5.5%, and nitrogen ≤0.25%, with molybdenum as a no-requirement ellipsis. Product-analysis limits apply only when ordered, typically from A480 Table A1.1 tolerances via the A1016 general-requirements path. Confirm the ordered A213 edition for the exact stainless-table number.
Why is A213 TP201 tensile 95 ksi when A312 TP201 is often listed at 75 ksi?
Because they are different product standards with different Table 4 rows for the same UNS number. ASTM A213 Table 4 for TP201 lists 95 ksi [655 MPa] tensile and 38 ksi [260 MPa] yield with a 219 HBW / 95 HRB hardness maximum. Do not copy A312 pipe tensile language onto an A213 tube purchase order — the MTC must clear the A213 floors that govern this page.
Does A213 Table 4 set a hardness limit for TP201?
Yes. Table 4 for TP201 lists tensile strength, yield strength, elongation, and a hardness maximum of 219 HBW / 230 HV or 95 HRB. Hardness tests are part of lot acceptance under A213. If a project needs a tighter hardness window than Table 4, write it into the purchase order as an additional requirement rather than assuming a catalogue figure.
TP201 vs TP202 — which A213 Mn–N tube should I order?
Order TP201 when the specification calls for the S20100 chemistry (Mn 5.5–7.5, Cr 16–18, Ni 3.5–5.5) and the 95/38 ksi Table 4 floor. Order TP202 when the datasheet wants the higher manganese band (7.5–10.0), slightly higher chromium (17–19), and the 90/45 ksi Table 4 pair. They are sister lean austenitics, not interchangeable stamps — match the UNS number on the PO to the datasheet.
TP201 vs TP304 — when is the lean grade acceptable under A213?
TP201 can be acceptable when nickel cost or availability drives the selection and the fluid is oxidizing or only mildly corrosive with low chlorides. TP304 remains the default 18-8 when higher nickel, a lower carbon ceiling, and broader industry acceptance matter more than Ni lean. ASTM A213 does not publish a ranking table; open the TP304 tube page when the end user expects classic 18-8 paperwork.
What heat treatment does ASTM A213 require for TP201?
TP201 is solution treated at a minimum of 1900 °F [1040 °C] and then water quenched or rapidly cooled to prevent carbide reprecipitation. Both cold-finished and hot-finished seamless tube follow that heat-treatment requirement. Ask the mill to state anneal temperature and quench method on the EN 10204 3.1 certificate so receiving inspection can clear the heat without chasing verbal confirmations.
Hydrostatic test vs NDE — which do I get on TP201 tube?
ASTM A213 requires each tube to be hydrostatically tested or nondestructively electrically tested. The manufacturer may choose the method unless the purchase order fixes one. Neither route is an informal upgrade over the other inside the product standard. State the preferred method on the enquiry if your end user or inspector mandates hydro only or a named NDE technique.
Can you dual-certify ASTM A213 and ASME SA-213 TP201?
Yes when the heat and testing support it. Dual A213/SA-213 marking is available when the purchase order requests both independent standards on the stencil and MTC. Spell the required marking on the enquiry so the heat is selected and documented correctly. Dual TP201/TP304 is not a routine path — the chemistry bands do not overlap enough for a meaningful dual grade stamp.

Conclusion

ASTM A213 TP201 / UNS S20100 is the lean manganese-nitrogen seamless stainless steel tube grade for boiler, superheater, and heat-exchanger service when nickel cost or availability favors Mn–N austenite and the fluid chemistry stays out of aggressive chlorides. SHH STEEL supplies cold-finished and hot-finished seamless tube in the usual OD × wall / BWG band, solution annealed, tested to the Table 4 95/38 ksi tensile floor and 219 HBW / 95 HRB hardness maximum, and documented on EN 10204 3.1 certificates — with dual SA-213 marking only when the order asks for that separate ASME standard. For sister grades and stock-oriented size discussions, start from the A213/A213M hub, then send your OD × wall list, wall basis, and marking requirements so we can align mill and near-term availability to the ASTM callout.

Contact: admin@steelspecs.com

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X