ASTM A213 TP310S Stainless Steel Tube | ASTM A213 Stainless Steel - SHH STEEL

ASTM A213 TP310S Stainless Steel Tube

ASTM A213 TP310S / UNS S31008 seamless boiler, superheater and heat-exchanger tube — a 24–26% Cr / 19–22% Ni austenitic with C ≤0.08%, Table 4 floors of 75/30 ksi, hardness max 192 HBW / 90 HRB, and 1900 °F solution anneal with Footnote F quench capability. SHH STEEL supplies cold-finished and hot-finished seamless tube with EN 10204 3.1 MTCs.
Grade
TP310S / UNS S31008
Standard
ASTM A213 / A213M
Product form
Seamless boiler / superheater / heat-exchanger tube (cold-finished and hot-finished)
Size
Typical OD × min wall (or average wall) within ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD and ~0.015–0.500 in. [0.4–12.7 mm] wall; other diameters by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is ASTM A213 TP310S Stainless Steel Tube

ASTM A213 / A213M covers seamless ferritic and austenitic alloy-steel boiler, superheater, and heat-exchanger tubes. Grade TP310S / UNS S31008 is the low-carbon-ceiling member of the 310 family: melting carbon ≤0.08%, chromium 24.0–26.0%, nickel 19.0–22.0%, with molybdenum, nitrogen, and niobium listed as no-requirement ellipses. That Cr–Ni jump above the 309 family is the oxidation-resistance story for furnace, radiant, and high-temperature heat-exchanger tube — not a molybdenum chloride framing and not an H-grade carbon-floor story.

SHH STEEL can supply ASTM A213 TP310S stainless steel tube as seamless cold-finished and hot-finished product in the usual boiler, furnace, and heat-exchanger OD × wall / BWG band, shipped with EN 10204 3.1 mill test certificates that report ladle chemistry and Table 4 tensile and hardness results. Dual A213 / SA-213 marking is available only when the purchase order asks for both independent standards. Browse 310-family grades on the A213/A213M hub.

Shop names such as 310S, S31008, or “25-20 furnace tube” do not replace the ASTM grade on the MTC. Sister grades under the same ASTM standard include A213 TP310H, A213 TP310Cb, A213 TP310HCb, A213 TP309S, and A213 TP304. A213 covers seamless tube only — cold-finished versus hot-finished is the process choice, not a WLD/HCW manufacturing-type letter.

Chemical Composition of A213 TP310S

Two chemistry layers matter for TP310S under ASTM A213. Melting analysis is mandatory for every heat; product analysis on finished tube applies only when Supplementary Requirement wording or the purchase order invokes it through ASTM A1016/A1016M, with tolerances typically from ASTM A480/A480M Table A1.1. The “S” in TP310S marks the ≤0.08% carbon ceiling relative to older high-carbon 310 compositions — it is not an L-grade ≤0.035% story, and it is not an H-grade 0.04% carbon floor.

The tables below reproduce the melt limits for TP310S / UNS S31008, the product-analysis limits from A480 Table A1.1, and a short carbon snapshot against TP310H and TP310Cb. Values are maximum unless a range is shown; ellipsis (…) means no requirement.

Melting analysis (heat / ladle analysis)

Element TP310S (UNS S31008) melting analysis
Carbon (C) ≤ 0.08
Manganese (Mn) ≤ 2.00
Phosphorus (P) ≤ 0.045
Sulfur (S) ≤ 0.030
Silicon (Si) ≤ 1.00
Chromium (Cr) 24.0 – 26.0
Nickel (Ni) 19.0 – 22.0
Molybdenum (Mo) … (no requirement)
Nitrogen (N) … (no requirement)
Niobium (Nb / Cb) … (no requirement)

Source: ASTM A213/A213M stainless chemistry table for Grade TP310S / UNS S31008 (public mill / specification PDF excerpt — htpipe A213 table text / _ref_a213.txt). Confirm the ordered edition on the purchase order. Stainless table number is edition-dependent (Table 2 later / Table 1 older). Chromium 24–26% and nickel 19–22% are the oxidation-resistance story relative to the 309 family.

Product analysis — A480/A480M Table A1.1 tolerances applied

Element Melting Tolerance (A480 A1.1) Product analysis limit
Carbon (C) ≤ 0.08 0.01 over ≤ 0.09
Manganese (Mn) ≤ 2.00 0.04 over ≤ 2.04
Phosphorus (P) ≤ 0.045 0.010 over ≤ 0.055
Sulfur (S) ≤ 0.030 0.005 over ≤ 0.035
Silicon (Si) ≤ 1.00 0.05 over ≤ 1.05
Chromium (Cr) 24.0 – 26.0 0.25 under / over 23.75 – 26.25
Nickel (Ni) 19.0 – 22.0 0.15 under / 0.20 over 18.85 – 22.20

Carbon snapshot — TP310S / TP310H / TP310Cb

Element TP310S (S31008) TP310H (S31009) TP310Cb (S31040)
C ≤ 0.08 0.04 – 0.10 ≤ 0.08
Cr 24.0 – 26.0 24.0 – 26.0 24.0 – 26.0
Ni 19.0 – 22.0 19.0 – 22.0 19.0 – 22.0
Nb (Cb) … … 10×C – 1.10

Read chromium and nickel first: the step from 22–24 / 12–15 on A213 TP309S to 24–26 / 19–22 on TP310S is why buyers move up the oxidation ladder. Heats that also meet the TP310H carbon floor and grain-size rule can be dual-certified TP310S/TP310H when tensile and hardness clear both rows — ask for that dual marking on the PO. Dual TP310S/TP310Cb is not automatic: niobium is a no-requirement ellipsis on TP310S.

When product analysis is ordered, finished tube may read C ≤0.09%, Mn ≤2.04%, P ≤0.055%, S ≤0.035%, Si ≤1.05%, Cr 23.75–26.25%, and Ni 18.85–22.20%. Put any tighter project carbon ceiling on the purchase order before the heat is selected.

Mechanical Properties of A213 TP310S

ASTM A213 Table 4 sets the room-temperature tensile acceptance floor for TP310S at 75 ksi [515 MPa] tensile strength and 30 ksi [205 MPa] yield strength (0.2% offset), with elongation of 35% minimum in 2 in. or 50 mm. Hardness maximum is 192 HBW / 200 HV or 90 HRB. Unlike the H grades, TP310S does not carry a mandatory ASTM grain-size number in the heat-treatment table — acceptance is chemistry plus Table 4 tensile/hardness plus the usual flattening and flaring lot tests.

Property TP310S requirement
Tensile strength, min (Table 4) 75 ksi [515 MPa]
Yield strength (0.2% offset), min (Table 4) 30 ksi [205 MPa]
Elongation in 2 in. or 50 mm, min (Table 4) 35%
Hardness, max (Table 4) 192 HBW / 200 HV or 90 HRB
Grain size No mandatory ASTM grain-size number (unlike TP310H)

Source: ASTM A213/A213M Table 4 for TP310S / UNS S31008 (public specification PDF excerpt — htpipe A213 table text). Mechanical property requirements do not apply to tubing smaller than 1/8 in. [3.2 mm] ID or thinner than 0.015 in. [0.4 mm] wall. Flattening and flaring tests sit beside tension and hardness on a lot basis under A213 / A1016 practice.

Room-temperature tensile equality with TP310H is why dual 310S/310H stock is attractive when the heat also clears the H-grade carbon floor and grain-size rule; elevated-temperature allowables and the carbon floor are why the H grade exists separately. A tensile-only MTC that omits hardness is incomplete for boiler-tube release — ask for both Table 4 results on the certificate.

Dimensions and Tolerances

Dimensional supply for ASTM A213 TP310S is tube language — OD × wall (minimum or average) and BWG / gauge — covering boiler, furnace, and heat-exchanger sizes rather than leading with ASME B36.19 pipe schedules. Usual A213 sizes run from about 1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD with min wall about 0.015–0.500 in. [0.4–12.7 mm]; other diameters by agreement. Furnace and radiant-tube datasheets almost always assume a minimum-wall reading — state wall basis on the purchase order.

OD and wall variations follow ASTM A1016/A1016M as invoked by A213. Cold-finished tubes commonly hold tighter OD; hot-finished tubes allow wider windows. Cold-finished average wall is often summarized as ±10% of specified average wall; minimum-wall product follows A1016 minimum-wall tables. Confirm exact rows for the OD and finish on the ordered edition.

Item Typical A213 TP310S dimensional practice
Product form Seamless only (cold-finished or hot-finished)
Usual size band ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD; wall ~0.015–0.500 in. [0.4–12.7 mm]
Wall basis Minimum wall (default for boiler / furnace / HX) or average wall when specified
OD / wall tolerances Per ASTM A1016/A1016M for finish route and size
Length Cut lengths for furnace / boiler / HX bundles; mill random by agreement
Secondary note B36.19 schedules only as a buyer cross-reference

Put cut list, design metal temperature context, and end preparation on the enquiry. Minimum wall remains a first-class A213 concept for 310S the same way it does for other austenitic boiler tube.

Equivalent Grades

Equivalence language around 310S tube often collapses plate, cast, and tube product forms into one nickname. ASTM A213 Grade TP310S / UNS S31008 is the governing designation for this article; EN and JIS wrought names that point to similar 25Cr–20Ni chemistry families are not automatic substitutes on an A213 MTC.

Designation Notes
ASTM A213 / A213M Grade TP310S Governing ASTM seamless boiler / HX tube product standard for this article
UNS S31008 Unified number in the stainless chemistry table
ASME SA-213 TP310S Separate ASME Code Book adoption — dual-mark only when the PO asks
Related H-grade A213 TP310H — same Cr–Ni, C 0.04–0.10, grain size No. 7 or coarser
Related Nb grade A213 TP310Cb — C ≤0.08 plus niobium stabilization
Related 309 A213 TP309S — lower Cr–Ni oxidation step
Related plate A240 / SA240 flat product in the 310 family — order plate and tube under their own standards

Dual A213/SA-213 marking is a purchase-order option. Compare TP310H, TP310Cb, and TP310HCb on their own ASTM A213 pages before swapping 310-family grades inside a furnace or boiler tube list.

Heat Treatment and Delivery Condition

TP310S under ASTM A213 is furnished solution treated at a minimum of 1900 °F [1040 °C], then quenched in water or cooled rapidly by other means. The heat-treatment table carries Footnote F for this grade: quench rate must be sufficient to prevent carbide re-precipitation, as demonstrable by the capability of tubes — heat treated by separate solution annealing or by direct quenching — to pass Practices A262, Practice E. The manufacturer is not required to run the A262 test unless the purchase order specifies it (see Supplementary Requirement S4).

Cold-finished versus hot-finished is a process and dimensional route, not a substitute for the anneal. Delivery condition for SHH STEEL TP310S is solution annealed and pickled (or bright annealed by agreement), with anneal temperature and quench method on the EN 10204 3.1 certificate. Straightening, cutting, and end finishing follow heat treatment.

Unlike A213 TP310H, TP310S has no mandatory ASTM grain-size number in the heat-treatment column. If a project datasheet asks for an E112 grain-size report on 310S, put that supplementary requirement on the purchase order rather than assuming base A213 includes it.

Corrosion Resistance

TP310S earns its place through high-temperature oxidation and scaling resistance from the 24–26% Cr / 19–22% Ni balance — not through molybdenum pitting resistance. Mo is a no-requirement ellipsis on this row, so wet chloride cooling-water or seawater exchanger framing belongs with molybdenum grades such as A213 TP316L, not with TP310S.

The ≤0.08% carbon ceiling improves resistance to sensitization relative to older high-carbon 310 compositions, but TP310S is still not an L-grade and not a niobium-stabilized grade. When intergranular corrosion after welding or thermal cycling is the primary concern, evaluate A213 TP310Cb or ask for A262 Practice E on the PO (Footnote F capability language already sits on the heat-treatment row). Sulfidation, carburizing, and molten-salt environments need process-specific review beyond a generic stainless catalogue claim.

Applications of A213 TP310S Tube

Buyers specify ASTM A213 TP310S when furnace, radiant, reformer, or high-temperature heat-exchanger duty needs the 25Cr–20Ni oxidation step above 309, without an H-grade carbon floor or niobium stabilization. Typical placements include furnace tubes and hangers, radiant coils, muffles, retorts, and heat-exchanger bundles where scaling resistance at elevated metal temperature drives grade selection more than wet-side chloride PREN.

Power and process boiler lists sometimes mix 304H, 309H, and 310S on different temperature bands — do not treat those as interchangeable stamps. When creep-range carbon and grain-size controls are mandatory, move to A213 TP310H. When Nb stabilization is mandatory for weld-heat IGC control, open A213 TP310Cb. SHH STEEL quotes OD × wall / BWG, wall basis, and finish route against the actual datasheet rather than a nickname.

Service theme Why TP310S is considered
Furnace / radiant tube 24–26 Cr / 19–22 Ni oxidation resistance
High-temperature HX Seamless A213 tube form + scaling resistance
Boiler / superheater (oxidation-led) When H-grade carbon/grain-size is not the PO driver
Not primary for wet chlorides No Mo requirement — use Mo grades instead

Weldability

TP310S welds with conventional austenitic practices using matching or near-matching 310 / 25-20 fillers selected for the joint design and service temperature. The ≤0.08% carbon ceiling reduces — but does not eliminate — sensitization risk in the heat-affected zone relative to high-carbon 310; heat input control and post-weld cleaning still matter for corrosive or cyclic thermal service.

For tube-to-tubesheet and coil welding, keep the filler chemistry aligned with the base-metal Cr–Ni windows and confirm any project restriction on ferrite or residual elements. When the datasheet demands niobium-stabilized base metal for IGC after welding, do not “solve” that with filler alone — specify A213 TP310Cb or A213 TP310HCb. Repair welding, when permitted, follows A1016/A1016M practice invoked by A213.

Surface Finishes

Standard delivery for ASTM A213 TP310S from SHH STEEL is solution annealed and pickled, with a clean ID/OD suitable for furnace and exchanger fabrication. Bright annealed or polished finishes are available by agreement when the process side needs lower roughness or a brighter appearance.

State finish expectations on the enquiry together with OD × wall and end preparation. Do not assume a bright finish from a generic “stainless tube” line item — pickled anneal is the default boiler/HX path unless the purchase order says otherwise.

Inspection and Testing

Lot testing for ASTM A213 TP310S follows the tension, hardness, flattening, and flaring requirements of A213 together with the general requirements of A1016/A1016M. Chemistry is verified on the heat (and on product when ordered). Non-destructive examination — eddy current, ultrasonic, or hydrostatic — follows the ordered edition and any purchaser supplementary requirements.

EN 10204 3.1 mill test certificates from SHH STEEL report ladle chemistry, tensile and hardness results, heat-treatment condition, and dimensions. Ask for A262 Practice E on the PO when Footnote F capability must be demonstrated by actual test rather than process capability alone. Third-party witness and dual A213/SA-213 marking are available when written into the enquiry.

Packaging and Shipping

TP310S tubes ship in capped or plugged bundles with weather protection suited to the destination and transport mode. Cut lengths for furnace and exchanger bundles are labeled by heat and size; export packing uses wooden cases or steel-frame crates when the route requires them.

Marking includes ASTM A213, grade TP310S / UNS S31008, size, heat number, and SHH STEEL identification. Dual SA-213 marking appears only when the purchase order requests it. Packing lists reference the same heat numbers shown on the EN 10204 3.1 certificates.

Why Choose SHH STEEL

SHH STEEL treats ASTM A213 TP310S as a specification-led tube product, not a nickname swap for 309S or 304. Every quotation ties OD × wall / BWG, wall basis (min or average), finish route, and marking language to the ordered edition — so furnace and boiler buyers receive chemistry and Table 4 results that match what the datasheet actually called.

We keep the 310-family distinctions honest: S-grade carbon ceiling versus H-grade floor and grain size versus Cb stabilization. Dual A213/SA-213 marking, A262 when ordered, and EN 10204 3.1 documentation are written options, not assumed extras. Browse sister grades on the A213/A213M hub before locking a furnace tube list.

Supply Capability

SHH STEEL supplies ASTM A213 TP310S seamless stainless steel tube in cold-finished and hot-finished routes across the usual boiler, furnace, and heat-exchanger OD × wall / BWG band. Capability below is an enquiry range — not a frozen warehouse SKU or tonnage claim.

Capability SHH STEEL practice for TP310S
Product form Seamless cold-finished and hot-finished tube
Standards ASTM A213 / A213M; dual SA-213 when PO asks
Size band Typical within ~1/8 in. ID to 5 in. OD; other diameters by agreement
Wall basis Minimum wall or average wall as specified
Documentation EN 10204 3.1 MTC; third-party witness on request
Trade terms FOB / CFR / CIF / EXW and other agreed Incoterms

Stock / Available sizes

SHH STEEL quotes TP310S against a stock-and-mill enquiry range rather than a frozen SKU/tonnage list. Representative OD × wall / BWG combinations for furnace, boiler, and heat-exchanger tube appear below.

Item Typical stock / enquiry range for TP310S
Outside diameter 19.05, 25.4, 31.8, 38.1, 42.4, 50.8, 60.3, 76.2 mm (and other furnace/HX ODs on enquiry; through the usual A213 ~5 in. [127 mm] band)
Wall / BWG BWG 10–18 class walls and metric min-wall equivalents; heavier walls by agreement
Common OD × wall examples 25.4 × 2.11 mm; 31.8 × 2.77 mm; 38.1 × 2.77 mm; 42.4 × 3.56 mm; 50.8 × 3.05 mm; 60.3 × 3.91 mm — illustrative, confirm min vs average wall
Length Cut lengths for furnace / exchanger bundles; bends and random mill lengths on enquiry
Special Non-standard OD/wall, bright anneal, dual A213/SA-213, A262 Practice E, third-party witness — confirm before heat reservation

Send OD × wall (or BWG), wall basis, finish route, quantity or cut list, marking (A213 or dual A213/SA-213), and Supplementary Requirements on one enquiry. We confirm Cr 24–26% / Ni 19–22% chemistry and Table 4 75/30 ksi without inventing fake warehouse codes. Sisters A213 TP310H, A213 TP309S, and A213 TP304 sit on the same hub.

FAQ

Is ASTM A213 the same as ASME SA-213 for TP310S?
No. ASTM A213 / A213M is the ASTM International product specification for seamless boiler, superheater, and heat-exchanger tubes; ASME SA-213 / SA-213M is the separate ASME Code Book adoption. Dual-mark only when the purchase order asks for both names on the stencil and MTC. Chemistry and tensile floors align closely for a given referenced edition, but the standards remain independent.
Does ASTM A213 TP310S include welded or HCW tube?
No. ASTM A213 covers seamless boiler, superheater, and heat-exchanger tubes only. There is no WLD or HCW manufacturing-type letter under A213. Cold-finished versus hot-finished describes the seamless process route and dimensional tolerances — not a welded product form. Order welded stainless pipe under a different product standard when that form is required.
What is the chemistry of ASTM A213 TP310S?
Melting analysis for TP310S / UNS S31008 is C ≤0.08%, Mn ≤2.00%, P ≤0.045%, S ≤0.030%, Si ≤1.00%, Cr 24.0–26.0%, Ni 19.0–22.0%, with Mo, N, and Nb as no-requirement ellipses. Confirm the ordered A213 edition on the purchase order; stainless table number is edition-dependent. Product-analysis tolerances from A480 Table A1.1 apply only when product analysis is invoked.
TP310S vs TP309S — which oxidation grade should I order?
TP310S raises chromium to 24–26% and nickel to 19–22%, while TP309S sits at 22–24% Cr / 12–15% Ni. Both share a ≤0.08% carbon ceiling and Table 4 75/30 ksi floors under A213. Order TP310S when the datasheet needs the higher Cr–Ni oxidation step for furnace or radiant duty; stay with TP309S when that lower step is sufficient and cost or availability favors 309.
TP310S vs TP310H — which A213 grade should I order?
TP310S uses C ≤0.08% and has no mandatory ASTM grain-size number. TP310H holds carbon in a 0.04–0.10% band and requires ASTM grain size No. 7 or coarser. Room-temperature Table 4 tensile floors are the same 75/30 ksi. Order TP310H when creep-range carbon and coarse-grain controls drive the datasheet; order TP310S when the S-grade carbon ceiling without grain-size mandate is what the PO asks for.
TP310S vs TP304 — when do I need the higher Cr–Ni?
TP304 / TP304H chemistry sits near 18–20% Cr / 8–11% Ni. TP310S moves to 24–26% Cr / 19–22% Ni for high-temperature oxidation and scaling resistance. If the service is ordinary boiler water-side or moderate-temperature HX where 18-8 oxidation resistance is enough, TP304-family grades may be correct. Furnace and radiant metal temperatures that outrun 304 oxidation performance are why buyers step to 310S.
Does Table 4 set a hardness limit for TP310S?
Yes. ASTM A213 Table 4 lists a hardness maximum of 192 HBW / 200 HV or 90 HRB for TP310S, together with the 75 ksi tensile / 30 ksi yield / 35% elongation floors. Hardness is part of lot acceptance — a tensile-only certificate that omits hardness is incomplete for boiler-tube release under the usual A213 reading.
What heat treatment does A213 require for TP310S?
Solution treatment at a minimum of 1900 °F [1040 °C], followed by water quench or other rapid cool. Footnote F on the heat-treatment row requires quench capability sufficient to prevent carbide re-precipitation as demonstrable by A262 Practice E capability; the manufacturer need not run the test unless the purchase order specifies it (Supplementary Requirement S4).
Minimum wall vs average wall for A213 TP310S — which should I specify?
Boiler, furnace, and superheater datasheets almost always expect minimum wall. Average wall is allowed when the purchase order says so and tolerances follow A1016/A1016M for that basis. State the wall basis explicitly on the enquiry — do not assume a schedule-number pipe reading replaces min-wall tube language under A213.
Is TP310S a good choice for chloride-rich cooling water?
Usually no as a primary chloride strategy. Molybdenum is a no-requirement ellipsis on TP310S, so pitting resistance in wet chlorides is not the grade’s design story. Use molybdenum-bearing grades such as TP316L for chloride-rich cooling service, and reserve TP310S for high-temperature oxidation-led furnace and HX duty.
Can you dual-certify A213 and SA-213 TP310S?
Yes, when the purchase order asks for both independent standard names on the stencil and MTC, and the heat clears the chemistry and mechanical requirements of the referenced editions. Dual marking is a documentation and stamping option — it does not merge ASTM A213 and ASME SA-213 into one standard. Write the dual-mark request into the enquiry before heat reservation.

Conclusion

ASTM A213 TP310S / UNS S31008 is the 24–26% Cr / 19–22% Ni seamless stainless steel tube grade for boiler, furnace, and heat-exchanger service when high-temperature oxidation resistance — not molybdenum chloride framing or H-grade carbon/grain-size controls — drives grade selection. SHH STEEL supplies cold-finished and hot-finished seamless tube in the usual OD × wall / BWG band, solution annealed at 1900 °F [1040 °C], tested to Table 4 75/30 ksi and hardness limits, and documented on EN 10204 3.1 certificates — with dual SA-213 marking only when the purchase order asks.

Contact: admin@steelspecs.com

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X