ASTM A213 UNS S30815 Stainless Steel Tube | ASTM A213 Stainless Steel - SHH STEEL

ASTM A213 UNS S30815 Stainless Steel Tube

ASTM A213 UNS S30815 (no TP letter — Ce–N high-temperature austenitic, commercially 253 MA) seamless boiler, superheater and heat-exchanger tube with C 0.05–0.10%, Si 1.40–2.00%, Cr 20.0–22.0%, Ni 10.0–12.0%, N 0.14–0.20%, Ce 0.03–0.08%, Table 4 floors of 87/45 ksi, hardness max 217 HBW / 95 HRB, and 1920 °F solution anneal. SHH STEEL supplies cold-finished and hot-finished seamless tube with EN 10204 3.1 MTCs.
Grade
UNS S30815 (no TP letter — Ce–N high-temperature austenitic)
Standard
ASTM A213 / A213M
Product form
Seamless boiler / superheater / heat-exchanger tube (cold-finished and hot-finished)
Size
Typical OD × min wall (or average wall) within ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD and ~0.015–0.500 in. [0.4–12.7 mm] wall; other diameters by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is ASTM A213 UNS S30815 Stainless Steel Tube

ASTM A213 / A213M lists UNS S30815 among the austenitic stainless grades that carry no common TP letter — Footnote C states the UNS number uniquely identifies the alloy. The chemistry is a cerium- and nitrogen-bearing, high-silicon high-temperature austenitic: carbon 0.05–0.10%, manganese ≤0.80%, silicon 1.40–2.00%, chromium 20.0–22.0%, nickel 10.0–12.0%, nitrogen 0.14–0.20%, and cerium 0.03–0.08%. Commercially the grade is widely known as 253 MA; that trade name still needs A213 (or the separate ASME SA-213 adoption) on the purchase order so tube product-standard minimum-wall, test, and marking clauses apply.

SHH STEEL can supply ASTM A213 UNS S30815 stainless steel tube as seamless cold-finished and hot-finished product in the usual boiler, furnace, and heat-exchanger OD × wall / BWG band, shipped with EN 10204 3.1 mill test certificates that report the full Ce–N–Si chemistry set and the Table 4 tensile and hardness results (87 ksi [600 MPa] / 45 ksi [310 MPa], hardness max 217 HBW / 95 HRB). Dual A213 / SA-213 marking is available only when the purchase order asks for both independent standards. Browse high-temperature austenitic sisters on the A213/A213M hub.

Shop names such as 253 MA, 253MA, or S30815 furnace tube do not replace UNS S30815 on the MTC. Sister grades under the same ASTM standard include A213 TP XM-15 for high-Si / high-Ni without Ce–N, A213 UNS S30615 for Si–Al heat-resistant austenitic, A213 TP310S for 25Cr–20Ni oxidation, and A213 TP309S for the lower 22–24 Cr oxidation step. A213 covers seamless tube only — cold-finished versus hot-finished is the process choice, not a WLD/HCW manufacturing type.

Chemical Composition of A213 UNS S30815

UNS S30815 chemistry is built around three intentional additions that ordinary 18-8 and 309 rows do not share together: silicon 1.40–2.00%, nitrogen 0.14–0.20%, and cerium 0.03–0.08%. Melting analysis is mandatory; product analysis applies only when ordered through A1016 / A480 A1.1. Manganese is capped at ≤0.80% — tighter than most TP304-family rows — and carbon sits in a 0.05–0.10% band. There is no TP grade letter — order and mark by UNS S30815 (Footnote C). Nitrogen analysis method is by agreement (Footnote B).

The tables below reproduce the melt limits from the public A213 stainless chemistry table and product-analysis limits from A480 Table A1.1 practice. Confirm the ordered edition before treating secondary catalogues as acceptance text.

Melting analysis (heat / ladle analysis)

Element UNS S30815 melting analysis
Carbon (C) 0.05 – 0.10
Manganese (Mn) ≤ 0.80
Phosphorus (P) ≤ 0.040
Sulfur (S) ≤ 0.030
Silicon (Si) 1.40 – 2.00
Chromium (Cr) 20.0 – 22.0
Nickel (Ni) 10.0 – 12.0
Molybdenum (Mo) … (no requirement)
Nitrogen (N) 0.14 – 0.20
Niobium (Nb) … (no requirement)
Titanium (Ti) … (no requirement)
Cerium (Ce) 0.03 – 0.08

Source: ASTM A213/A213M stainless chemistry table for UNS S30815 (public htpipe A213 PDF excerpt — _ref_a213.txt A213/A213M − 13). Cerium and nitrogen must both appear on the certificate; an MTC that reports only Cr–Ni–Si without Ce and N is incomplete for S30815.

Product analysis — A480/A480M Table A1.1 tolerances applied

Element Melting Tolerance (A480 A1.1) Product analysis limit
Carbon (C) 0.05 – 0.10 0.01 under / over 0.04 – 0.11
Manganese (Mn) ≤ 0.80 0.03 over ≤ 0.83
Phosphorus (P) ≤ 0.040 0.010 over ≤ 0.050
Sulfur (S) ≤ 0.030 0.005 over ≤ 0.035
Silicon (Si) 1.40 – 2.00 0.05 under / over 1.35 – 2.05
Chromium (Cr) 20.0 – 22.0 0.25 under / over 19.75 – 22.25
Nickel (Ni) 10.0 – 12.0 0.15 under / over 9.85 – 12.15
Nitrogen (N) 0.14 – 0.20 0.01 under / 0.02 over 0.13 – 0.22
Cerium (Ce) 0.03 – 0.08 edition-dependent rare-earth tolerance confirm A480 edition if contractual (UNCERTAIN)

Read Ce, N, and Si first: cerium supports oxide-scale adherence at elevated temperature; nitrogen strengthens and helps oxidation resistance; silicon adds further scaling resistance. Versus A213 TP309S, chromium sits in a similar 20–22 band while silicon, nitrogen, and cerium are intentional additions TP309S does not require. Versus A213 UNS S30615, S30815 has no aluminum requirement, a lower silicon ceiling, and a Ce–N package instead of Al. Molybdenum remains a no-requirement ellipsis.

When product analysis is ordered, use the A480 path above and put any tighter Ce floor, N floor, or S ceiling on the purchase order before the heat is selected. Cerium product-tolerance digits are edition-sensitive — labeled UNCERTAIN until the ordered A480 edition is confirmed.

Mechanical Properties of A213 UNS S30815

ASTM A213 Table 4 sets UNS S30815 tensile acceptance at 87 ksi [600 MPa] tensile strength and 45 ksi [310 MPa] yield strength (0.2% offset), with elongation 40% minimum in 2 in. or 50 mm and hardness max 217 HBW or 95 HRB. That yield floor sits above XM-15’s 30 ksi and even above S30615’s 40 ksi under the same product standard — nitrogen strengthening is a large part of why designers look at S30815 when high-temperature oxidation and a higher room-temperature yield share one datasheet. Elongation at 40% minimum is also higher than the 35% floor used on many sister austenitics.

Property UNS S30815 requirement (Table 4)
Tensile strength, min 87 ksi [600 MPa]
Yield strength (0.2% offset), min 45 ksi [310 MPa]
Elongation in 2 in. or 50 mm, min 40%
Hardness, max 217 HBW or 95 HRB
Grain size No mandatory ASTM grain-size number in public Table 3 excerpt

Source: ASTM A213/A213M Table 4 for UNS S30815 (public htpipe A213 PDF excerpt). Mechanical property requirements do not apply to tubing smaller than 1/8 in. [3.2 mm] ID or thinner than 0.015 in. [0.4 mm] wall. Flattening and flaring tests apply on a lot basis beside tension and hardness.

Do not accept a TP309S or TP310S certificate as S30815 clearance — cerium, nitrogen, the silicon band, and the 87/45 ksi / 217 HBW pair must all match. Room-temperature Table 4 is still only the acceptance floor; elevated-temperature design allowables come from the project’s material tables, not from inventing numbers on this page.

Dimensions and Tolerances

Dimensional supply for ASTM A213 UNS S30815 remains tube language — OD × min wall (or average wall) and BWG / gauge — aimed at furnace, boiler, and heat-exchanger bundles rather than B36.19 pipe schedules. Usual A213 sizes run from about 1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD with min wall about 0.015–0.500 in. [0.4–12.7 mm]; other diameters by agreement. State wall basis on the PO before tooling is set.

OD and wall variations follow ASTM A1016/A1016M. Cold-finished routes hold tighter OD; hot-finished routes allow wider windows. Cold-finished average wall is often summarized as ±10%; minimum-wall product follows A1016 minimum-wall tables. Confirm edition rows for the size and finish ordered.

Item Typical A213 UNS S30815 dimensional practice
Product form Seamless only (cold-finished or hot-finished)
Usual size band ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD; wall ~0.015–0.500 in. [0.4–12.7 mm]
Wall basis Minimum wall (default) or average wall when specified
OD / wall tolerances Per ASTM A1016/A1016M for finish route and size
Length Furnace / boiler / HX cut lengths; mill random by agreement
Secondary note B36.19 schedules only as a buyer cross-reference

Because designers sometimes thin the wall to exploit the 45 ksi yield, minimum-wall callouts and remaining wall after expanding deserve extra attention on the enquiry. Put cut list, bend form, and end preparation on the order with the metallurgical notes.

Equivalent Grades

Equivalence language around S30815 tube often collapses plate, bar, and tube product forms into one nickname. ASTM A213 UNS S30815 is the governing designation for this article; 253 MA is the common trade name; EN 1.4835 is an approximate wrought designation that points to a similar Ce–N–Si chemistry family but is not an automatic substitute on an A213 MTC.

Designation Notes
ASTM A213 / A213M UNS S30815 Governing ASTM seamless boiler / HX tube product standard — no TP letter (Footnote C)
UNS S30815 Unified number that uniquely identifies the alloy
253 MA (commercial) Common trade name — does not replace S30815 on the MTC
EN 1.4835 (approx.) Approximate wrought designation; order EN tube forms under the relevant EN tube specs
ASME SA-213 UNS S30815 Separate ASME Code Book adoption — dual-mark only when the PO asks
Related high-Si A213 TP XM-15 / A213 UNS S30615
Related 309 / 310 A213 TP309S / A213 TP310S

Dual A213/SA-213 marking is a purchase-order option. Compare Si–Al, high-Si, and 25-20 grades on their own ASTM A213 pages before swapping high-temperature austenitics inside a furnace tube list.

Heat Treatment and Delivery Condition

UNS S30815 under ASTM A213 is furnished solution treated at a minimum of 1920 °F [1050 °C], then quenched in water or cooled rapidly by other means. That solution temperature sits 20 °F [about 10 °C] above the 1900 °F [1040 °C] minimum used for XM-15, S30615, and TP310S — do not paste a 1900 °F heat-treatment block onto an S30815 certificate. Public Table 3 excerpt for S30815 does not show a Footnote F superscript on the temperature cell the way XM-15 and S30615 do; confirm ordered-edition footnote attachment if A262 capability language is contractual.

Cold-finished versus hot-finished is a process and dimensional route, not a substitute for the anneal. Nitrogen- and cerium-bearing austenitics need a thorough solution treatment so N and Ce stay effective rather than precipitating as unwanted phases. Delivery condition for SHH STEEL S30815 is solution annealed and pickled (or bright annealed by agreement), with anneal temperature and quench method on the EN 10204 3.1 certificate.

Public Table 3 excerpt shows no mandatory ASTM grain-size number for S30815. If a project datasheet asks for an E112 grain-size report, put that supplementary requirement on the purchase order rather than assuming base A213 includes it.

Corrosion Resistance

S30815 earns its place through high-temperature oxidation resistance from the Ce–N–Si package on a 20–22% Cr / 10–12% Ni base — cerium helping scale adherence, nitrogen and silicon supporting oxidation performance and strength. Molybdenum is a no-requirement ellipsis, so wet chloride cooling-water framing belongs with A213 TP316L, not with S30815.

Carbon 0.05–0.10% is an intentional band for high-temperature service, not an L-grade IGC strategy. When intergranular corrosion after welding or thermal cycling is a project concern, ask for A262 Practice E on the PO rather than assuming Footnote F language from a sister grade. Sulfidation, carburizing, and molten-salt environments need process-specific review — S30815 is often the Ce–N answer when 309/310 oxidation alone is not enough and Si–Al S30615 is not the datasheet chemistry.

Applications of A213 UNS S30815 Tube

Buyers specify ASTM A213 UNS S30815 when furnace, radiant, combustion, or high-temperature heat-exchanger duty needs the Ce–N–Si package and the 87/45 ksi Table 4 floor that ordinary 309/310 rows do not share. Typical placements include furnace tubes and hangers, radiant coils, heat-recovery exchangers, and process heaters where oxidation resistance at elevated metal temperature and a higher yield share one datasheet.

Service theme Why S30815 is considered
Furnace / radiant tube Ce–N–Si oxidation resistance on 20–22 Cr / 10–12 Ni
High-temperature HX Seamless A213 tube form + 87/45 ksi Table 4 floor
Strength vs 309S/310S Higher yield than TP309S / TP310S 30 ksi floors
Not primary for wet chlorides No Mo requirement — use Mo grades instead

When Si–Al chemistry is the datasheet answer, open A213 UNS S30615. When high-Si / high-Ni without Ce–N is enough, open A213 TP XM-15. When 25Cr–20Ni oxidation without Ce–N is enough, open A213 TP310S on the A213/A213M hub.

Weldability

S30815 tube welds with austenitic practices using matching or near-matching Ce–N–Si austenitic fillers selected for the joint design and service temperature — commonly 253 MA-matched or other S30815-aligned consumables under a qualified WPS. Do not default to ER308L simply because it is familiar; a soft deposit undercuts the 45 ksi design intent that often drove the base-metal selection. Heat input, interpass limits, and post-weld cleaning remain the fabricator’s responsibility under the applicable code — A213 governs the seamless tube product, not the shop weld procedure.

Because A213 S30815 is seamless, there is no mill longitudinal weld to radiograph the way welded pipe standards describe. Focus inspection on tube integrity (hydro or NDE of each length), joint quality including strength matching, and any contractual corrosion test on the base metal. When tubesheet cladding chemistry differs from S30815, write the joint design and filler explicitly on the fabrication package.

Surface Finishes

Standard delivery for ASTM A213 UNS S30815 from SHH STEEL is solution annealed and pickled, with a clean ID/OD suitable for furnace and exchanger fabrication. Bright annealed or polished finishes are available by agreement when the process side needs lower roughness.

State finish expectations on the enquiry together with OD × wall and end preparation. Do not assume a bright finish from a generic “stainless tube” line item — pickled anneal is the default boiler/HX path unless the purchase order says otherwise.

Inspection and Testing

Lot testing for ASTM A213 UNS S30815 follows the tension, hardness, flattening, and flaring requirements of A213 together with A1016/A1016M. Chemistry is verified on the heat (and on product when ordered) — cerium, nitrogen, and silicon must all report inside their bands. Non-destructive examination follows the ordered edition and any purchaser supplementary requirements.

EN 10204 3.1 mill test certificates from SHH STEEL report ladle chemistry including Ce and N, tensile and hardness results (87/45 ksi, 217 HBW / 95 HRB), heat-treatment condition at the 1920 °F [1050 °C] minimum, and dimensions. Ask for A262 Practice E on the PO when intergranular-corrosion capability must be demonstrated by actual test. Third-party witness and dual A213/SA-213 marking are available when written into the enquiry.

Packaging and Shipping

S30815 tubes ship in capped or plugged bundles with weather protection suited to the destination and transport mode. Cut lengths for furnace and exchanger bundles are labeled by heat and size; export packing uses wooden cases or steel-frame crates when the route requires them.

Marking includes ASTM A213, UNS S30815, size, heat number, and SHH STEEL identification. Dual SA-213 marking appears only when the purchase order requests it. Packing lists reference the same heat numbers shown on the EN 10204 3.1 certificates.

Why Choose SHH STEEL

SHH STEEL treats ASTM A213 UNS S30815 as a specification-led tube product, not a nickname swap for “any 253 MA tube” or TP309S. Every quotation ties OD × wall / BWG, wall basis, finish route, and marking language to the ordered edition — so furnace buyers receive Ce 0.03–0.08%, N 0.14–0.20%, Si 1.40–2.00%, the 1920 °F anneal, and Table 4 87/45 ksi results that match what the datasheet actually called.

We keep the high-temperature austenitic distinctions honest: S30815 Ce–N versus S30615 Si–Al versus XM-15 high-Si versus TP310S 25-20. Dual A213/SA-213 marking, A262 when ordered, and EN 10204 3.1 documentation are written options. Browse sister grades on the A213/A213M hub before locking a furnace tube list.

Supply Capability

SHH STEEL supplies ASTM A213 UNS S30815 seamless stainless steel tube in cold-finished and hot-finished routes across the usual boiler, furnace, and heat-exchanger OD × wall / BWG band. Capability below is an enquiry range — not a frozen warehouse SKU or tonnage claim.

Capability SHH STEEL practice for UNS S30815
Product form Seamless cold-finished and hot-finished tube
Standards ASTM A213 / A213M; dual SA-213 when PO asks
Size band Typical within ~1/8 in. ID to 5 in. OD; other diameters by agreement
Wall basis Minimum wall or average wall as specified
Documentation EN 10204 3.1 MTC with Ce, N, and Si reported; third-party witness on request
Trade terms FOB / CFR / CIF / EXW and other agreed Incoterms

Stock / Available sizes

SHH STEEL quotes S30815 against a stock-and-mill enquiry range rather than a frozen SKU/tonnage list. Representative OD × wall / BWG combinations for furnace, boiler, and heat-exchanger tube appear below.

Item Typical stock / enquiry range for UNS S30815
Outside diameter 19.05, 25.4, 31.8, 38.1, 42.4, 50.8, 60.3, 76.2 mm (and other furnace/HX ODs on enquiry; through the usual A213 ~5 in. [127 mm] band)
Wall / BWG BWG 10–18 class walls and metric min-wall equivalents; thinner walls exploiting 45 ksi yield by agreement after design review
Common OD × wall examples 25.4 × 1.65 mm; 25.4 × 2.11 mm; 31.8 × 2.11 mm; 38.1 × 2.77 mm; 50.8 × 2.77 mm; 60.3 × 3.05 mm — illustrative, confirm min vs average wall
Length Cut lengths for furnace / exchanger bundles; bends and random mill lengths on enquiry
Special Non-standard OD/wall, bright anneal, matched filler notes, dual A213/SA-213, A262 Practice E — confirm before heat reservation

Send OD × wall (or BWG), wall basis, finish route, quantity or cut list, marking (A213 or dual A213/SA-213), filler expectations, and Supplementary Requirements on one enquiry. We confirm Ce–N–Si chemistry, 1920 °F anneal, and Table 4 87/45 ksi without inventing fake warehouse codes. Sisters A213 UNS S30615, A213 TP XM-15, and A213 TP310S sit on the same hub.

FAQ

Is ASTM A213 the same as ASME SA-213 for UNS S30815?
No. ASTM A213 / A213M is the ASTM International product specification for seamless boiler, superheater, and heat-exchanger tubes; ASME SA-213 / SA-213M is the separate ASME Code Book adoption. Dual-mark only when the purchase order asks for both names on the stencil and MTC. Chemistry and tensile floors align closely for a given referenced edition, but the standards remain independent.
Why does S30815 have no TP letter under A213?
Footnote C to the stainless chemistry table states that for these alloys there is no common grade designation — the UNS number uniquely identifies the alloy. Order and mark by UNS S30815 on the purchase order, stencil, and MTC. Do not invent a TP letter or assume a TP309S stamp will clear an S30815 datasheet.
Is 253 MA the same as ASTM A213 UNS S30815?
253 MA is the common trade name for the Ce–N–Si chemistry family around UNS S30815. On an A213 mill test certificate and stencil, the governing designation is UNS S30815 under ASTM A213 / A213M. Write the UNS number on the purchase order; treat the trade name as a commercial alias, not a substitute product standard.
What is the chemistry of ASTM A213 UNS S30815?
Melting analysis includes C 0.05–0.10%, Mn ≤0.80%, P ≤0.040%, S ≤0.030%, Si 1.40–2.00%, Cr 20.0–22.0%, Ni 10.0–12.0%, N 0.14–0.20%, and Ce 0.03–0.08%, with Mo, Nb, and Ti as no-requirement ellipses. Nitrogen analysis method is by agreement (Footnote B). Product-analysis tolerances from A480 Table A1.1 apply only when product analysis is invoked; Ce product digits are UNCERTAIN until the ordered A480 edition is confirmed.
What tensile and hardness floors does Table 4 set for S30815?
Table 4 for UNS S30815 lists 87 ksi [600 MPa] tensile strength, 45 ksi [310 MPa] yield strength, 40% elongation, and a hardness maximum of 217 HBW or 95 HRB. Hardness tests are part of lot acceptance under A213. That yield floor sits above TP309S / TP310S 30 ksi under the same product standard — match filler and joint design to the strength level.
S30815 vs TP310S — which high-temperature A213 tube should I order?
TP310S uses 24–26% Cr / 19–22% Ni with Si ≤1.00% and Table 4 floors of 75/30 ksi. S30815 uses 20–22% Cr / 10–12% Ni with Si 1.40–2.00%, N 0.14–0.20%, Ce 0.03–0.08%, and Table 4 floors of 87/45 ksi. Order S30815 when the datasheet needs the Ce–N–Si package and higher yield; order TP310S when the higher Cr–Ni oxidation step without Ce–N is what the PO asks for.
What heat treatment does A213 require for UNS S30815?
Solution treatment at a minimum of 1920 °F [1050 °C], followed by water quench or other rapid cool. That minimum sits above the 1900 °F [1040 °C] used for many sister austenitics — do not paste a 1900 °F block onto an S30815 certificate. Ask the mill to state anneal temperature and quench method on the EN 10204 3.1 certificate.
Does ASTM A213 UNS S30815 include welded or HCW tube?
No. ASTM A213 covers seamless boiler, superheater, and heat-exchanger tubes only. There is no WLD or HCW manufacturing-type letter under A213. Cold-finished versus hot-finished describes the seamless process route and dimensional tolerances — not a welded product form.
Minimum wall vs average wall for A213 S30815 — which should I specify?
Furnace, boiler, and superheater datasheets almost always expect minimum wall — especially important when walls are thinned to exploit the 45 ksi yield. Average wall is allowed when the purchase order says so and tolerances follow A1016/A1016M for that basis. State the wall basis explicitly on the enquiry.
Is S30815 a good choice for chloride-rich cooling water?
Usually no as a primary chloride strategy. Molybdenum is a no-requirement ellipsis on S30815, so pitting resistance in wet chlorides is not the grade’s design story. Use molybdenum-bearing grades such as TP316L for chloride-rich cooling service, and reserve S30815 for high-temperature Ce–N–Si oxidation-led furnace and HX duty.
Can you dual-certify A213 and SA-213 UNS S30815?
Yes, when the purchase order asks for both independent standard names on the stencil and MTC, and the heat clears the chemistry and mechanical requirements of the referenced editions. Dual marking is a documentation and stamping option — it does not merge ASTM A213 and ASME SA-213 into one standard. Spell Ce, N, Si, and dual-mark requirements into the enquiry before heat reservation.

Conclusion

ASTM A213 UNS S30815 (commercially 253 MA) is the Ce–N–Si seamless stainless steel tube grade for boiler, furnace, and heat-exchanger service when cerium 0.03–0.08%, nitrogen 0.14–0.20%, silicon 1.40–2.00%, and an 87/45 ksi Table 4 floor share one datasheet. SHH STEEL supplies cold-finished and hot-finished seamless tube in the usual OD × wall / BWG band, solution annealed at 1920 °F [1050 °C], tested to Table 4 tensile and hardness limits, and documented on EN 10204 3.1 certificates with full Ce–N–Si chemistry — with dual SA-213 marking only when the purchase order asks.

Contact: admin@steelspecs.com

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X