ASTM A213 TP310H Stainless Steel Tube | ASTM A213 Stainless Steel - SHH STEEL

ASTM A213 TP310H Stainless Steel Tube

ASTM A213 TP310H / UNS S31009 seamless boiler, superheater and heat-exchanger tube — the H-grade 24–26% Cr / 19–22% Ni austenitic with controlled carbon 0.04–0.10%, Table 4 floors of 75/30 ksi, hardness max 192 HBW / 90 HRB, 1900 °F solution anneal, and ASTM grain size No. 7 or coarser. SHH STEEL supplies cold-finished and hot-finished seamless tube with EN 10204 3.1 MTCs that report grain size.
Grade
TP310H / UNS S31009
Standard
ASTM A213 / A213M
Product form
Seamless boiler / superheater / heat-exchanger tube (cold-finished and hot-finished)
Size
Typical OD × min wall (or average wall) within ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD and ~0.015–0.500 in. [0.4–12.7 mm] wall; other diameters by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is ASTM A213 TP310H Stainless Steel Tube

ASTM A213 / A213M covers seamless ferritic and austenitic alloy-steel boiler, superheater, and heat-exchanger tubes. Grade TP310H / UNS S31009 is the high-temperature carbon-controlled member of the 310 family: melting carbon is held in a 0.04–0.10% band (both floor and ceiling), chromium 24.0–26.0%, nickel 19.0–22.0%, and the heat-treatment path carries an ASTM grain-size requirement of No. 7 or coarser. That combination exists for creep-range boiler and furnace duty where the higher Cr–Ni oxidation resistance of 310 is needed together with H-grade carbon and coarse-grain controls — not as a synonym stamp for ordinary A213 TP310S.

SHH STEEL can supply ASTM A213 TP310H stainless steel tube as seamless cold-finished and hot-finished product in the usual boiler, furnace, and heat-exchanger OD × wall / BWG band, shipped with EN 10204 3.1 mill test certificates that report the full ladle chemistry, the Table 4 tensile and hardness results, and the grain-size result for the heat-treatment lot. Dual A213 / SA-213 marking is available only when the purchase order asks for both independent standards. Browse 310-family grades on the A213/A213M hub.

Shop names such as 310H, S31009, or “H-grade 25-20 boiler tube” do not replace the ASTM grade on the MTC. Sister grades under the same ASTM standard include A213 TP310S, A213 TP310Cb, A213 TP310HCb, A213 TP309H, and A213 TP304H. A213 covers seamless tube only — cold-finished versus hot-finished is the process choice, not a WLD/HCW manufacturing-type letter.

Chemical Composition of A213 TP310H

Two chemistry layers matter for TP310H under ASTM A213. Melting analysis is mandatory for every heat; product analysis on finished tube applies only when Supplementary Requirement wording or the purchase order invokes it through ASTM A1016/A1016M, with tolerances typically from ASTM A480/A480M Table A1.1. The carbon range is the first line a reviewer should check: TP310H is not “310S with a little more carbon” written as a max — it is a 0.04–0.10% band with both floor and ceiling, paired with the same 24–26 / 19–22 Cr–Ni windows as TP310S.

The tables below reproduce the melt limits for TP310H / UNS S31009, the product-analysis limits from A480 Table A1.1, and a short carbon snapshot against TP310S and TP310Cb. Values are maximum unless a range is shown; ellipsis (…) means no requirement.

Melting analysis (heat / ladle analysis)

Element TP310H (UNS S31009) melting analysis
Carbon (C) 0.04 – 0.10
Manganese (Mn) ≤ 2.00
Phosphorus (P) ≤ 0.045
Sulfur (S) ≤ 0.030
Silicon (Si) ≤ 1.00
Chromium (Cr) 24.0 – 26.0
Nickel (Ni) 19.0 – 22.0
Molybdenum (Mo) … (no requirement)
Nitrogen (N) … (no requirement)
Niobium (Nb / Cb) … (no requirement)

Source: ASTM A213/A213M stainless chemistry table for Grade TP310H / UNS S31009 (public mill / specification PDF excerpt — htpipe A213 table text / _ref_a213.txt). Confirm the ordered edition on the purchase order. Stainless table number is edition-dependent (Table 2 later / Table 1 older).

Product analysis — A480/A480M Table A1.1 tolerances applied

Element Melting Tolerance (A480 A1.1) Product analysis limit
Carbon (C) 0.04 – 0.10 0.01 under / over 0.03 – 0.11
Manganese (Mn) ≤ 2.00 0.04 over ≤ 2.04
Phosphorus (P) ≤ 0.045 0.010 over ≤ 0.055
Sulfur (S) ≤ 0.030 0.005 over ≤ 0.035
Silicon (Si) ≤ 1.00 0.05 over ≤ 1.05
Chromium (Cr) 24.0 – 26.0 0.25 under / over 23.75 – 26.25
Nickel (Ni) 19.0 – 22.0 0.15 under / 0.20 over 18.85 – 22.20

Carbon snapshot — TP310S / TP310H / TP310Cb

Element TP310S (S31008) TP310H (S31009) TP310Cb (S31040)
C ≤ 0.08 0.04 – 0.10 ≤ 0.08
Cr 24.0 – 26.0 24.0 – 26.0 24.0 – 26.0
Ni 19.0 – 22.0 19.0 – 22.0 19.0 – 22.0
Nb (Cb) … … 10×C – 1.10

Heats that also meet the TP310S carbon ceiling can be dual-certified TP310S/TP310H when tensile, hardness, and grain-size results clear both rows — ask for that dual marking on the PO rather than assuming it from a PMI reading. Dual TP310H/TP310Cb is not automatic: niobium is a no-requirement ellipsis on TP310H. When Nb stabilization plus H-grade carbon is required, open A213 TP310HCb.

When product analysis is ordered, finished tube may read C 0.03–0.11%, Mn ≤2.04%, P ≤0.055%, S ≤0.035%, Si ≤1.05%, Cr 23.75–26.25%, and Ni 18.85–22.20%. Put any tighter project carbon floor on the purchase order before the heat is selected — the H-grade carbon floor is intentional for elevated-temperature strength.

Mechanical Properties of A213 TP310H

ASTM A213 Table 4 sets the room-temperature tensile acceptance floor for TP310H at 75 ksi [515 MPa] tensile strength and 30 ksi [205 MPa] yield strength (0.2% offset), with elongation of 35% minimum in 2 in. or 50 mm — the same room-temperature pair as TP310S. Hardness maximum is 192 HBW / 200 HV or 90 HRB. What distinguishes the H grade mechanically in the product standard is the grain-size requirement: ASTM No. 7 or coarser, determined per heat-treatment lot under the ordered edition’s clause referencing ASTM E112.

Property TP310H requirement
Tensile strength, min (Table 4) 75 ksi [515 MPa]
Yield strength (0.2% offset), min (Table 4) 30 ksi [205 MPa]
Elongation in 2 in. or 50 mm, min (Table 4) 35%
Hardness, max (Table 4) 192 HBW / 200 HV or 90 HRB
Grain size ASTM No. 7 or coarser (per heat-treatment lot)

Source: ASTM A213/A213M Table 4 for TP310H / UNS S31009 and H-grade grain-size language (public specification PDF excerpt — htpipe A213 heat-treatment table showing grain-size column “7” for TP310H). Mechanical property requirements do not apply to tubing smaller than 1/8 in. [3.2 mm] ID or thinner than 0.015 in. [0.4 mm] wall. Flattening and flaring tests sit beside tension and hardness on a lot basis.

Room-temperature tensile equality with TP310S is why dual 310S/310H stock is attractive; elevated-temperature allowables, the carbon floor, and the coarse-grain requirement are why the H grade exists. A tensile-only MTC that omits grain size is incomplete for TP310H — ask for the E112 result on the certificate before releasing the heat to fabrication.

Dimensions and Tolerances

Dimensional supply for ASTM A213 TP310H is tube language — OD × wall (minimum or average) and BWG / gauge — covering boiler, furnace, and heat-exchanger sizes rather than leading with ASME B36.19 pipe schedules. Usual A213 sizes run from about 1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD with min wall about 0.015–0.500 in. [0.4–12.7 mm]; other diameters by agreement. Boiler and superheater datasheets almost always assume a minimum-wall reading — state wall basis on the purchase order.

OD and wall variations follow ASTM A1016/A1016M as invoked by A213. Cold-finished tubes commonly hold tighter OD; hot-finished tubes allow wider windows. Cold-finished average wall is often summarized as ±10% of specified average wall; minimum-wall product follows A1016 minimum-wall tables. Confirm exact rows for the OD and finish on the ordered edition.

Item Typical A213 TP310H dimensional practice
Product form Seamless only (cold-finished or hot-finished)
Usual size band ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD; wall ~0.015–0.500 in. [0.4–12.7 mm]
Wall basis Minimum wall (default for boiler / superheater) or average wall when specified
OD / wall tolerances Per ASTM A1016/A1016M for finish route and size
Length Cut lengths for boiler / furnace / HX bundles; mill random by agreement
Secondary note B36.19 schedules only as a buyer cross-reference

Put cut list, design metal temperature context, and end preparation on the enquiry. Minimum wall remains a first-class A213 concept for 310H the same way it does for other H-grade tube.

Equivalent Grades

Equivalence language around 310H tube often collapses plate, cast, and tube product forms into one nickname. ASTM A213 Grade TP310H / UNS S31009 is the governing designation for this article; EN and JIS wrought names that point to similar high-Cr–Ni chemistry families are not automatic substitutes on an A213 MTC.

Designation Notes
ASTM A213 / A213M Grade TP310H Governing ASTM seamless boiler / HX tube product standard for this article
UNS S31009 Unified number in the stainless chemistry table
ASME SA-213 TP310H Separate ASME Code Book adoption — dual-mark only when the PO asks
Related S-grade A213 TP310S — same Cr–Ni, C ≤0.08, no grain-size mandate
Related H+Cb A213 TP310HCb — H-grade carbon plus niobium stabilization
Related 309H A213 TP309H — lower Cr–Ni oxidation step with the same H-grade carbon/grain-size pattern
Related plate A240 / SA240 flat product in the 310 family — order plate and tube under their own standards

Dual A213/SA-213 marking is a purchase-order option. Compare TP310S, TP310Cb, and TP310HCb on their own ASTM A213 pages before swapping 310-family grades inside a furnace or boiler tube list.

Heat Treatment and Delivery Condition

TP310H under ASTM A213 is furnished solution treated at a minimum of 1900 °F [1040 °C], then quenched in water or cooled rapidly by other means. That Table 3 heat-treatment row also carries the ASTM grain-size requirement of No. 7 or coarser for the heat-treatment lot — the clause that separates H-grade acceptance from ordinary TP310S solution treatment at the same temperature.

Cold-finished versus hot-finished is a process and dimensional route, not a substitute for the anneal or the grain-size check. Delivery condition for SHH STEEL TP310H is solution annealed and pickled (or bright annealed by agreement), with anneal temperature, quench method, and E112 grain-size result on the EN 10204 3.1 certificate. Straightening, cutting, and end finishing follow heat treatment.

When Nb stabilization is also required on an H-grade carbon heat, do not assume TP310H covers it — specify A213 TP310HCb, which adds the 10×C–1.10 niobium band and carries Footnote H / S2 stabilizing language when the purchaser invokes those options.

Corrosion Resistance

TP310H is selected for high-temperature oxidation and creep-oriented service, not for wet chloride pitting resistance. Molybdenum remains a no-requirement ellipsis, so seawater or chloride-rich cooling-water exchanger framing belongs with A213 TP316L or higher-Mo grades.

The 0.04–0.10% carbon band intentionally raises carbon relative to an L-grade mindset; sensitization risk in the weld heat-affected zone is managed by procedure, not by pretending TP310H is a low-carbon grade. When intergranular corrosion after thermal cycling is a datasheet driver alongside H-grade carbon, evaluate niobium-stabilized A213 TP310HCb. Sulfidation and carburizing atmospheres still need process-specific review beyond catalogue oxidation claims.

Applications of A213 TP310H Tube

Buyers specify ASTM A213 TP310H when creep-range boiler, superheater, or furnace tube lists demand both the 25Cr–20Ni oxidation step and the H-grade carbon floor with coarse-grain control. Typical placements include high-temperature superheater and reheater sections, furnace radiant coils, and heat-exchanger bundles where design metal temperature and Code allowables point to an H grade rather than an S-grade ceiling alone.

Do not treat TP310H as a drop-in rename of A213 TP309H — the Cr–Ni windows differ. When the PO needs Nb stabilization with the same H-grade carbon band, open A213 TP310HCb. SHH STEEL quotes OD × wall / BWG against the datasheet temperature and wall basis rather than a shop nickname.

Service theme Why TP310H is considered
Creep-range boiler / superheater C 0.04–0.10 + grain size No. 7 or coarser
High-temperature furnace / radiant 24–26 Cr / 19–22 Ni oxidation resistance
Dual 310S/310H stock programs Same Table 4 floors when heat clears both rows
Not primary for wet chlorides No Mo requirement — use Mo grades instead

Weldability

TP310H welds with austenitic practices using matching or near-matching 310H / 25-20 fillers chosen for joint design and design metal temperature. The intentional carbon floor means HAZ sensitization control relies on heat-input discipline and cleaning — not on L-grade carbon math. Procedure qualification should reflect the actual carbon band on the MTC.

For tube-to-tubesheet joints in creep-range service, confirm any project limits on grain size after welding and on residual cold work. When the datasheet demands niobium-stabilized H-grade base metal, specify A213 TP310HCb rather than trying to “stabilize” TP310H with filler chemistry alone. Repair welding, when permitted, follows A1016/A1016M as invoked by A213.

Surface Finishes

Standard delivery for ASTM A213 TP310H from SHH STEEL is solution annealed and pickled, ready for boiler and furnace fabrication. Bright annealed finishes are available by agreement when the process side specifies lower roughness.

State finish, OD × wall, and end preparation together on the enquiry. Grain-size reporting on the MTC is part of H-grade acceptance — it is independent of whether the surface is pickled or bright.

Inspection and Testing

Lot testing for ASTM A213 TP310H follows tension, hardness, flattening, and flaring under A213 / A1016, plus the ASTM grain-size determination (E112) required for the heat-treatment lot. Chemistry is verified on the heat (and on product when ordered). NDE — eddy current, ultrasonic, or hydrostatic — follows the ordered edition and purchaser supplements.

EN 10204 3.1 certificates from SHH STEEL report ladle chemistry, Table 4 tensile and hardness, heat-treatment condition, and grain-size result. Dual A213/SA-213 marking and third-party witness are available when written into the enquiry. A certificate that omits grain size is not a complete TP310H release package.

Packaging and Shipping

TP310H tubes ship in capped or plugged bundles with weather protection matched to the transport route. Cut lengths for boiler and furnace bundles are labeled by heat and size; export packing uses cases or steel-frame crates when required.

Marking includes ASTM A213, grade TP310H / UNS S31009, size, heat number, and SHH STEEL identification. Dual SA-213 marking appears only when the purchase order requests it. Packing lists track the same heat numbers shown on the EN 10204 3.1 certificates, including grain-size lot identity where applicable.

Why Choose SHH STEEL

SHH STEEL treats ASTM A213 TP310H as an H-grade specification product: carbon floor and ceiling, Cr–Ni windows, Table 4 floors, and grain size No. 7 or coarser are checked together before a heat is offered against a creep-range tube list. Quotations state OD × wall / BWG, wall basis, finish route, and whether dual A213/SA-213 marking is required.

We keep S / H / Cb / HCb distinctions explicit so buyers do not receive 310S stamped as 310H by nickname. EN 10204 3.1 documentation includes the E112 grain-size result for H-grade lots. Compare sisters on the A213/A213M hub before freezing the boiler tube bill of materials.

Supply Capability

SHH STEEL supplies ASTM A213 TP310H seamless stainless steel tube in cold-finished and hot-finished routes across the usual boiler, furnace, and heat-exchanger OD × wall / BWG band. Capability below is an enquiry range — not a frozen warehouse SKU or tonnage claim.

Capability SHH STEEL practice for TP310H
Product form Seamless cold-finished and hot-finished tube
Standards ASTM A213 / A213M; dual SA-213 when PO asks
Size band Typical within ~1/8 in. ID to 5 in. OD; other diameters by agreement
Wall basis Minimum wall or average wall as specified
Documentation EN 10204 3.1 MTC with grain-size result; third-party witness on request
Trade terms FOB / CFR / CIF / EXW and other agreed Incoterms

Stock / Available sizes

SHH STEEL quotes TP310H against a stock-and-mill enquiry range rather than a frozen SKU/tonnage list. Representative OD × wall / BWG combinations for boiler, furnace, and heat-exchanger tube appear below.

Item Typical stock / enquiry range for TP310H
Outside diameter 19.05, 25.4, 31.8, 38.1, 42.4, 50.8, 60.3, 76.2 mm (and other boiler/HX ODs on enquiry; through the usual A213 ~5 in. [127 mm] band)
Wall / BWG BWG 10–18 class walls and metric min-wall equivalents; heavier walls by agreement
Common OD × wall examples 25.4 × 2.11 mm; 31.8 × 2.77 mm; 38.1 × 2.77 mm; 42.4 × 3.56 mm; 50.8 × 3.05 mm; 60.3 × 3.91 mm — illustrative, confirm min vs average wall
Length Cut lengths for boiler / furnace / exchanger bundles; bends and random mill lengths on enquiry
Special Non-standard OD/wall, bright anneal, dual A213/SA-213, dual 310S/310H, third-party witness — confirm before heat reservation

Send OD × wall (or BWG), wall basis, finish route, quantity or cut list, marking (A213 or dual A213/SA-213), and any grain-size or Supplementary Requirements on one enquiry. We confirm C 0.04–0.10%, Cr 24–26% / Ni 19–22%, Table 4 75/30 ksi, and ASTM grain size No. 7 or coarser without inventing fake warehouse codes. Sisters A213 TP310S, A213 TP309H, and A213 TP304H sit on the same hub.

FAQ

Is ASTM A213 the same as ASME SA-213 for TP310H?
No. ASTM A213 / A213M is the ASTM International product specification for seamless boiler, superheater, and heat-exchanger tubes; ASME SA-213 / SA-213M is the separate ASME Code Book adoption. Dual-mark only when the purchase order asks for both names on the stencil and MTC. Chemistry, tensile floors, and grain-size rules align closely for a given referenced edition, but the standards remain independent.
Does ASTM A213 TP310H include welded or HCW tube?
No. ASTM A213 covers seamless boiler, superheater, and heat-exchanger tubes only. There is no WLD or HCW manufacturing-type letter under A213. Cold-finished versus hot-finished describes the seamless process route — not a welded product form. Order welded product under a different standard when that form is required.
What is the chemistry of ASTM A213 TP310H?
Melting analysis for TP310H / UNS S31009 is C 0.04–0.10%, Mn ≤2.00%, P ≤0.045%, S ≤0.030%, Si ≤1.00%, Cr 24.0–26.0%, Ni 19.0–22.0%, with Mo, N, and Nb as no-requirement ellipses. Confirm the ordered A213 edition; stainless table number is edition-dependent. The carbon band has both a floor and a ceiling — it is not a ≤0.08% S-grade ceiling written differently.
TP310H vs TP310S — which A213 grade should I order?
Order TP310H when the datasheet requires the 0.04–0.10% carbon band and ASTM grain size No. 7 or coarser for creep-range service. Order TP310S when C ≤0.08% without a mandatory grain-size number is what the PO asks for. Both share 24–26% Cr / 19–22% Ni and Table 4 75/30 ksi floors. Dual 310S/310H marking is possible only when one heat clears both rows including grain size.
TP310H vs TP304H — when do I need the higher Cr–Ni?
Both are H grades with C 0.04–0.10% and grain size No. 7 or coarser, but TP304H sits near 18–20% Cr / 8–11% Ni while TP310H uses 24–26% Cr / 19–22% Ni. Choose TP310H when oxidation and scaling resistance at higher metal temperature need the 25-20 step; stay with TP304H when 18-8 H-grade chemistry matches the allowable and oxidation demand.
TP310H vs TP309H — which oxidation H-grade is higher?
TP310H raises chromium to 24–26% and nickel to 19–22%; TP309H uses 22–24% Cr / 12–15% Ni. Both carry C 0.04–0.10% and grain size No. 7 or coarser under A213. Order TP310H when the datasheet needs the higher Cr–Ni oxidation ladder; order TP309H when the 309H step is sufficient for the design metal temperature.
Why does A213 require grain size No. 7 or coarser for TP310H?
The coarse-grain requirement supports elevated-temperature / creep-oriented behavior expected from H-grade austenitic boiler tube. ASTM No. 7 or coarser is determined per heat-treatment lot (E112 practice as invoked by the ordered edition). A tensile-only MTC that omits grain size is incomplete for TP310H acceptance — ask for the result on the EN 10204 3.1 certificate.
Does Table 4 set a hardness limit for TP310H?
Yes. Table 4 lists hardness maximum 192 HBW / 200 HV or 90 HRB alongside 75 ksi tensile, 30 ksi yield, and 35% elongation. Hardness and grain size both belong on the release package for H-grade boiler tube — neither replaces the other.
What heat treatment does A213 require for TP310H?
Solution treatment at a minimum of 1900 °F [1040 °C], followed by water quench or other rapid cool, with ASTM grain size No. 7 or coarser for the heat-treatment lot. That grain-size column is what separates TP310H from TP310S at the same anneal temperature. Delivery is solution annealed and pickled unless bright anneal is agreed.
Minimum wall vs average wall for A213 TP310H — which should I specify?
Boiler and superheater datasheets almost always expect minimum wall. Average wall is allowed when the purchase order says so, with A1016/A1016M tolerances for that basis. State wall basis on the enquiry — schedule-number pipe language is only a secondary cross-reference under A213 tube supply.
Is TP310H a good choice for chloride-rich cooling water?
Not as a primary chloride strategy. Molybdenum is a no-requirement ellipsis on TP310H, so wet chloride pitting resistance is not the grade’s design story. Use Mo-bearing grades for chloride-rich cooling service; reserve TP310H for high-temperature oxidation and creep-oriented boiler/furnace duty.
Can you dual-certify A213 and SA-213 TP310H?
Yes, when the purchase order asks for both independent standard names on the stencil and MTC, and the heat clears chemistry, Table 4, and grain-size requirements of the referenced editions. Dual marking does not merge ASTM and ASME into one standard. Write the dual-mark request into the enquiry before heat reservation.

Conclusion

ASTM A213 TP310H / UNS S31009 is the H-grade 24–26% Cr / 19–22% Ni seamless stainless steel tube for boiler, furnace, and heat-exchanger service when high-temperature oxidation resistance and creep-oriented carbon/grain-size controls both drive grade selection. SHH STEEL supplies cold-finished and hot-finished seamless tube in the usual OD × wall / BWG band, solution annealed at 1900 °F [1040 °C], tested to Table 4 75/30 ksi and hardness limits, with ASTM grain size No. 7 or coarser reported on EN 10204 3.1 certificates — and dual SA-213 marking only when the purchase order asks.

Contact: admin@steelspecs.com

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X