Product Showcase
ASME SA213/SA213M Stainless Steel Products
ASME SA213 is the ASME code version of seamless ferritic and austenitic alloy-steel boiler, superheater and heat-exchanger tubes. It covers the same grade family as ASTM A213, including T11, T22, T91, TP304, TP316L, TP321 and TP347, and is intended for use under ASME Boiler and Pressure Vessel Code rules. SHH STEEL supplies ASME SA213 tubes with mill certification, competitive pricing and global delivery support.
-
ASME SA213 UNS S35045 Stainless Steel Tube
ASME SA213 UNS S35045 Alloy 803 class Al–Ti 25–29Cr / 32–37Ni seamless boiler, superheater and heat-exchanger tube — C 0.06–0.10%, Ti 0.15–0.60%, Al 0.15–0.60%, Cu ≤0.75%, tensile 70/25 ksi, solution anneal 2000 °F [1100 °C] still air cool or faster. No TP letter. SHH STEEL supplies seamless cold- and hot-finished tube with EN 10204 3.1 MTC.View More -
ASME SA213 UNS S31277 Stainless Steel Tube
ASME SA213 UNS S31277 27-7MO class high-Mo/N superaustenitic seamless boiler, superheater and heat-exchanger tube — C ≤0.020%, Cr 20.5–23.0%, Ni 26.0–28.0%, Mo 6.5–8.0%, N 0.30–0.40%, Cu 0.50–1.50%, tensile 112/52 ksi, solution anneal 2050 °F [1120 °C]. No TP letter. SHH STEEL supplies seamless cold- and hot-finished tube with EN 10204 3.1 MTC.View More -
ASME SA213 UNS S31272 Stainless Steel Tube
ASME SA213 UNS S31272 Ti–B microalloyed 14–16Cr / 14–16Ni seamless boiler, superheater and heat-exchanger tube — C 0.08–0.12%, Mn 1.50–2.00%, Si 0.30–0.70%, Mo 1.00–1.40%, Ti 0.30–0.60%, B 0.004–0.008%, tensile 65/29 ksi, solution anneal 1920 °F [1050 °C]. No TP letter. SHH STEEL supplies seamless cold- and hot-finished tube with EN 10204 3.1 MTC.View More -
ASME SA213 UNS S31254 Stainless Steel Tube
ASME SA213 UNS S31254 6Mo / 254 SMO class superaustenitic seamless boiler, superheater and heat-exchanger tube — C ≤0.020%, Cr 19.5–20.5%, Ni 17.5–18.5%, Mo 6.0–6.5%, N 0.18–0.22%, Cu 0.50–1.00%, wall-split Table 4 floors of 98/45 or 95/45 ksi with elongation 35% min, hardness max 220 HBW / 96 HRB, 2100 °F [1150 °C] solution anneal. No TP letter — order by UNS. SHH STEEL supplies cold-finished and hot-finished seamless tube with EN 10204 3.1 MTCs that report Mo, N, and Cu together.View More -
ASME SA213 UNS S31002 Stainless Steel Tube
ASME SA213 UNS S31002 low-carbon low-silicon 25Cr–20Ni austenitic seamless boiler, superheater and heat-exchanger tube — C ≤0.02%, Si ≤0.15%, Cr 24.0–26.0%, Ni 19.0–22.0%, Mo ≤0.10%, N ≤0.10%, P ≤0.020%, S ≤0.015%, Table 4 73/30 ksi with elongation 35% min, hardness max 192 HBW / 90 HRB, 1900 °F solution anneal. No TP letter — order by UNS. SHH STEEL supplies cold-finished and hot-finished seamless tube with EN 10204 3.1 MTCs that report the low-C / low-Si windows together.View More -
ASME SA213 UNS S30815 Stainless Steel Tube
ASME SA213 UNS S30815 Ce–N high-temperature austenitic seamless boiler, superheater and heat-exchanger tube — commercially 253 MA class — C 0.05–0.10%, Si 1.40–2.00%, Mn ≤0.80%, Cr 20.0–22.0%, Ni 10.0–12.0%, N 0.14–0.20%, Ce 0.03–0.08%, Table 4 87/45 ksi with elongation 40% min, hardness max 217 HBW / 95 HRB, 1920 °F solution anneal. No TP letter — order by UNS. SHH STEEL supplies cold-finished and hot-finished seamless tube with EN 10204 3.1 MTCs that report Ce and N together.View More -
ASME SA213 UNS S30615 Stainless Steel Tube
ASME SA213 UNS S30615 high-silicon aluminium-bearing austenitic seamless boiler, superheater and heat-exchanger tube — C 0.16–0.24%, Si 3.2–4.0%, Al 0.8–1.5%, Cr 17.0–19.5%, Ni 13.5–16.0%, Table 4 90/40 ksi with elongation 35% min, hardness max 192 HBW / 90 HRB, 1900 °F solution anneal with Footnote F. No TP letter — order by UNS. SHH STEEL supplies cold-finished and hot-finished seamless tube with EN 10204 3.1 MTCs that report Si and Al together.View More -
ASME SA213 TP XM-15 Stainless Steel Tube
ASME SA213 XM-15 / UNS S38100 high-silicon high-nickel seamless boiler, superheater and heat-exchanger tube — C ≤0.08%, Si 1.50–2.50%, Cr 17.0–19.0%, Ni 17.5–18.5%, P/S ≤0.030%, no Mo/Nb/Ti requirement, Table 4 75/30 ksi with elongation 35% min, hardness max 192 HBW / 90 HRB, 1900 °F solution anneal (Footnote F). SHH STEEL supplies cold-finished and hot-finished seamless tube with EN 10204 3.1 MTCs that report the Si and Ni windows together. Commercial shop name 18-18-2 does not replace XM-15 on the MTC.View More -
ASME SA213 TP348H Stainless Steel Tube
ASME SA213 TP348H / UNS S34809 H-grade cobalt- and tantalum-controlled niobium-stabilized seamless boiler, superheater and heat-exchanger tube — C 0.04–0.10%, Cr 17.0–19.0%, Ni 9.0–13.0%, Nb+Ta ≥8×C ≤1.10% (chemistry Footnote H), Co ≤0.20%, Ta ≤0.10%, Table 4 75/30 ksi with elongation 35% min, hardness max 192 HBW / 90 HRB, finish-route solution anneal (CF 2000 °F / HR 1925 °F) with Footnote H, grain size ASTM No. 7 or coarser. SHH STEEL supplies cold-finished and hot-finished seamless tube with EN 10204 3.1 MTCs that report Nb+Ta, Co, Ta, and grain size.View More -
ASME SA213 TP348 Stainless Steel Tube
ASME SA213 TP348 / UNS S34800 cobalt- and tantalum-controlled niobium-stabilized seamless boiler, superheater and heat-exchanger tube — C ≤0.08%, Cr 17.0–19.0%, Ni 9.0–13.0%, Nb+Ta ≥10×C ≤1.10% (Footnote G), Co ≤0.20%, Ta ≤0.10%, Table 4 75/30 ksi with elongation 35% min, hardness max 192 HBW / 90 HRB, 1900 °F solution anneal (Footnotes F, H). SHH STEEL supplies cold-finished and hot-finished seamless tube with EN 10204 3.1 MTCs that report Nb+Ta, Co, and Ta.View More -
ASME SA213 TP347W Stainless Steel Tube
ASME SA213 TP347W / UNS S34705 tungsten-bearing niobium-stabilized seamless boiler, superheater and heat-exchanger tube — C ≤0.05%, Cr 17.0–20.0%, Ni 8.00–11.0%, N 0.10–0.25%, Nb 0.25–0.50%, V 0.20–0.50%, W 1.50–2.60%, Table 4 90/38 ksi with elongation 30% min, hardness max 219 HBW / 95 HRB, 2000 °F solution anneal, grain size ASTM No. 7–10. SHH STEEL supplies cold-finished and hot-finished seamless tube with EN 10204 3.1 MTCs that report W, V, N, and Nb together.View More -
ASME SA213 TP347LN Stainless Steel Tube
ASME SA213 TP347LN / UNS S34751 ultra-low-carbon niobium-stabilized nitrogen-bearing seamless boiler, superheater and heat-exchanger tube — C 0.005–0.020%, N 0.06–0.10%, Cr 17.0–19.0%, Ni 9.0–13.0%, Nb 0.20–0.50% and ≥15×C, Table 4 75/30 ksi with elongation 35% min, hardness max 192 HBW / 90 HRB, 1900 °F solution anneal (Footnote F). SHH STEEL supplies cold-finished and hot-finished seamless tube with EN 10204 3.1 MTCs that report the C / N / Nb package.View More
ASME SA213/SA213M Stainless Steel Products
Stainless Steel Pipes and Tubes
SHH STEEL, a premier Stainless Steel Pipes and Tubes exporter, produces and exports stainless steel pipes and tubes for chemical, marine, and food processing industries. Our seamless and welded products, like 304 and 316L (ASTM A312), ensure corrosion resistance and strength. With a 5,000-ton inventory, we deliver in 3–5 days, backed by SGS/TUV inspections and mill certificates. Choose SHH STEEL for seamless stainless steel pipes and custom solutions.
Stainless Steel Pipes and Tubes
X