ASTM A213 TP347LN Stainless Steel Tube | ASTM A213 Stainless Steel - SHH STEEL

ASTM A213 TP347LN Stainless Steel Tube

ASTM A213 TP347LN / UNS S34751 seamless boiler, superheater and heat-exchanger tube with ultra-low carbon 0.005–0.020%, nitrogen 0.06–0.10%, Cr 17.0–19.0%, Ni 9.0–13.0%, niobium 0.20–0.50% and ≥15×C, Table 4 floor 75/30 ksi, and hardness max 192 HBW / 90 HRB. SHH STEEL supplies cold-finished and hot-finished seamless tube solution treated at 1900 °F [1040 °C] with EN 10204 3.1 MTCs that report C, N, and Nb against the 15×C formula.
Grade
TP347LN / UNS S34751
Standard
ASTM A213 / A213M
Product form
Seamless boiler / superheater / heat-exchanger tube (cold-finished and hot-finished)
Size
Typical OD × min wall (or average wall) within ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD and ~0.015–0.500 in. [0.4–12.7 mm] wall; other diameters by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is ASTM A213 TP347LN Stainless Steel Tube

ASTM A213 / A213M is the ASTM International product specification for seamless ferritic and austenitic alloy-steel boiler, superheater, and heat-exchanger tubes. Grade TP347LN / UNS S34751 sits at the intersection of three ideas that buyers often keep separate: ultra-low melting carbon (0.005–0.020%), intentional nitrogen (0.06–0.10%), and a fixed-plus-formula niobium window (0.20–0.50% and not less than 15 × C). That combination is not a typing error for TP347 or for TP304LN — it is its own stainless-table row. Chromium 17.0–19.0% and nickel 9.0–13.0% place the grade in the Nb-stabilized 18-8 neighbourhood, while the 15 × C niobium multiplier is stricter than the 10 × C rule on non-H A213 TP347. Buyers who write “347LN tube” still need to name A213 (or the separate ASME SA-213 adoption) on the purchase order so the mill applies the C/N/Nb package, heat-treatment, test, and marking clauses rather than a loose shop nickname.

SHH STEEL can supply ASTM A213 TP347LN stainless steel tube as seamless cold-finished and hot-finished product in the usual boiler and heat-exchanger OD × wall / BWG band, shipped with EN 10204 3.1 mill test certificates that report the full ladle chemistry (including carbon inside 0.005–0.020%, nitrogen inside 0.06–0.10%, and niobium against both the 0.20–0.50% band and the 15 × C floor), the Table 4 tensile and hardness results, and the anneal temperature for the heat-treatment lot. When a project also needs ASME Code Book marking, we dual-mark A213 / SA-213 on the same lengths only if the purchase order says so. Browse the grade family on the A213/A213M hub.

Commercially, TP347LN tube is still called 347LN, S34751, or low-carbon nitrogen-bearing Nb-stabilized boiler tube; none of those shop names replace the ASTM grade on the MTC or stencil. Sister grades under the same ASTM standard include A213 TP347, A213 TP347H, A213 TP304LN, A213 TP321, and A213 TP348. A213 covers seamless tube only — no welded or HCW manufacturing type — so cold-finished versus hot-finished is the process choice, not a WLD/HCW stencil letter.

Chemical Composition of A213 TP347LN

Two chemistry layers matter for TP347LN under ASTM A213. Melting (heat or ladle) analysis is mandatory for every heat; product analysis on finished tube applies only when Supplementary Requirement wording or the purchase order invokes it through ASTM A1016/A1016M. Product-analysis tolerances typically flow from ASTM A480/A480M Table A1.1. SHH STEEL reports actual ladle values — and product values when ordered — and does not advertise unpublished tighter catalogue windows. Three lines define the grade for a reviewer: carbon locked inside 0.005–0.020% (tighter than any L-grade ceiling alone), nitrogen 0.06–0.10%, and niobium held both in a fixed 0.20–0.50% band and at ≥15 × C per Footnote F. A heat with 0.015% carbon needs at least 0.225% Nb from the formula and still must land inside 0.20–0.50%; a heat at the carbon ceiling of 0.020% needs at least 0.30% Nb. Chromium 17.0–19.0% is narrower than TP347’s 17.0–20.0% window.

The tables below reproduce the heat analysis for TP347LN / UNS S34751, the product-analysis limits from A480 Table A1.1 practice, and a short C/N/Nb snapshot against TP347, TP304LN, and TP347H. Later A213 editions place austenitic stainless grades in Table 2 (older editions used Table 1); confirm the ordered edition on the purchase order. Nitrogen analysis method is a matter of agreement (Footnote B) — write the method on the PO when N is contractual.

Melting analysis (heat / ladle analysis)

Element TP347LN (UNS S34751) melting analysis
Carbon (C) 0.005 – 0.020
Manganese (Mn) ≤ 2.00
Phosphorus (P) ≤ 0.045
Sulfur (S) ≤ 0.030
Silicon (Si) ≤ 1.00
Chromium (Cr) 17.0 – 19.0
Nickel (Ni) 9.0 – 13.0
Molybdenum (Mo) … (no requirement)
Nitrogen (N) 0.06 – 0.10
Niobium (Nb / Cb) 0.20 – 0.50 and ≥ 15 × C (Footnote F)
Titanium (Ti) … (no requirement)

Source: ASTM A213/A213M stainless chemistry table for Grade TP347LN / UNS S34751 (public mill / specification PDF excerpt — _ref_a213.txt / A213–13 table text). Confirm the ordered edition. Where ellipses appear, the ordered edition sets no requirement for that element. Older shop language still says “columbium”; modern MTCs usually print Nb.

Product analysis — A480/A480M Table A1.1 tolerances applied

Element Melting Tolerance (A480 A1.1) Product analysis limit
Carbon (C) 0.005 – 0.020 0.005 under / over (tight low-C band practice) 0.000 – 0.025 (confirm A480 edition)
Manganese (Mn) ≤ 2.00 0.04 over ≤ 2.04
Phosphorus (P) ≤ 0.045 0.010 over ≤ 0.055
Sulfur (S) ≤ 0.030 0.005 over ≤ 0.035
Silicon (Si) ≤ 1.00 0.05 over ≤ 1.05
Chromium (Cr) 17.0 – 19.0 0.20 under / over 16.80 – 19.20
Nickel (Ni) 9.0 – 13.0 0.15 under / 0.20 over 8.85 – 13.20
Nitrogen (N) 0.06 – 0.10 0.01 under / 0.02 over (sister LN practice) 0.05 – 0.12
Niobium (Nb) 0.20 – 0.50 and ≥ 15 × C 0.05 under / over on band (Nb range practice) 0.15 – 0.55 product band; formula min still tied to heat C

C / N / Nb snapshot — TP347 / TP347LN / TP304LN / TP347H

Element TP347 (S34700) TP347LN (S34751) TP304LN (S30453) TP347H (S34709)
C ≤ 0.08 0.005 – 0.020 ≤ 0.035 0.04 – 0.10
N … (no req.) 0.06 – 0.10 0.10 – 0.16 … (no req.)
Cr 17.0 – 20.0 17.0 – 19.0 18.0 – 20.0 17.0 – 19.0
Ni 9.0 – 13.0 9.0 – 13.0 8.0 – 11.0 9.0 – 13.0
Nb / stabilizer ≥ 10 × C, ≤ 1.10 0.20 – 0.50 and ≥ 15 × C none (N strengthens) ≥ 8 × C, ≤ 1.10

Do not treat TP347LN as a dual of TP347 just because both carry niobium: the carbon ceiling, nitrogen band, Nb multiplier, and chromium window all differ. Versus A213 TP304LN, TP347LN adds niobium stabilization and a much tighter carbon band, while its nitrogen window (0.06–0.10%) sits below TP304LN’s 0.10–0.16%. Dual TP347LN/TP347 is not a routine chemistry path — ask the mill before assuming it from a PMI gun.

When product analysis is ordered, finished tube may read C near 0.000–0.025%, Mn ≤2.04%, P ≤0.055%, S ≤0.035%, Si ≤1.05%, Cr 16.80–19.20%, Ni 8.85–13.20%, N 0.05–0.12%, and Nb inside a 0.15–0.55% product band with the 15 × C floor still tied to heat carbon. Put any tighter project carbon or niobium floor on the purchase order before the heat is selected. A480 digits for the ultra-low carbon band and for the Nb fixed band are applied from sister-pack practice and are labeled UNCERTAIN pending the ordered A480 edition.

Mechanical Properties of A213 TP347LN

ASTM A213 Table 4 sets the room-temperature tensile acceptance floor for TP347LN at 75 ksi [515 MPa] tensile strength and 30 ksi [205 MPa] yield strength (0.2% offset), with elongation of 35% minimum in 2 in. or 50 mm — the same room-temperature pair as TP347 and TP304 despite the ultra-low carbon, because intentional nitrogen recovers strength that a bare low-C melt would otherwise lose. Hardness maximum is 192 HBW / 200 HV or 90 HRB, and hardness tests are part of lot acceptance under A213. The public heat-treatment table does not print a mandatory ASTM grain-size number for TP347LN (unlike TP347H’s “7” and TP347W’s “7–10”), so a tensile-and-hardness MTC without grain size can still be complete unless the purchase order adds a grain-size Supplementary Requirement.

Property TP347LN requirement
Tensile strength, min (Table 4) 75 ksi [515 MPa]
Yield strength (0.2% offset), min (Table 4) 30 ksi [205 MPa]
Elongation in 2 in. or 50 mm, min (Table 4) 35%
Hardness, max (Table 4) 192 HBW / 200 HV or 90 HRB
Grain size No mandatory ASTM number in the public Table 3 row (confirm ordered edition)

Source: ASTM A213/A213M Table 4 for TP347LN / UNS S34751 (public specification PDF excerpt — _ref_a213.txt / A213–13). Mechanical property requirements do not apply to tubing smaller than 1/8 in. [3.2 mm] inside diameter or thinner than 0.015 in. [0.4 mm] wall. Flattening and flaring tests are also required on a lot basis.

Room-temperature tensile equality with sister 18-8 grades is why buyers sometimes look for dual marking with TP347; the ultra-low C + N + 15 × C Nb package is why TP347LN exists as its own row. A tensile-only MTC that omits carbon, nitrogen, or niobium is incomplete — ask for the C / N / Nb check on the certificate before releasing the heat to fabrication. For H-grade grain-size and carbon-floor framing open A213 TP347H; for tungsten-bearing strength open A213 TP347W.

Dimensions and Tolerances

Dimensional supply for ASTM A213 TP347LN is tube language — outside diameter × wall thickness (minimum wall or average wall) and, commercially, BWG / gauge — not ASME B36.19 pipe schedules as the primary size story. The sizes usually furnished under A213 run from about 1/8 in. [3.2 mm] inside diameter to 5 in. [127 mm] outside diameter, with minimum wall from about 0.015 to 0.500 in. [0.4 to 12.7 mm]; other diameters may be furnished when all other requirements are met. State on the purchase order whether wall is minimum or average — boiler and heat-exchanger datasheets almost always assume a minimum-wall reading.

Outside-diameter and wall variations follow ASTM A1016/A1016M as invoked by A213. Cold-finished tubes commonly hold tighter OD control; hot-finished tubes allow wider OD and wall windows. Permissible variations from a specified average wall for cold-finished tube are often summarized as ±10% of the specified average wall. Confirm the exact A1016 rows for the OD and finish route on the ordered edition.

Item Typical A213 TP347LN dimensional practice
Product form Seamless only (cold-finished or hot-finished)
Usual size band ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD; wall ~0.015–0.500 in. [0.4–12.7 mm] min (or average wall if PO says so)
Wall basis Minimum wall (default for boiler / HX) or average wall when specified
OD / wall tolerances Per ASTM A1016/A1016M for the finish route and size; cold-finished average wall often ±10%
Length Cut lengths for boiler / superheater / HX bundles, or mill random lengths by agreement
Secondary size note ASME B36.19 schedules may appear only when a buyer asks for a pipe-schedule cross-reference — not as the primary A213 size callout

Put the cut list and end preparation on the enquiry so mill and stock lengths can be mixed efficiently. Minimum wall is a first-class A213 concept: if the datasheet assumes average wall, say so explicitly before the heat is rolled.

Equivalent Grades

Equivalence language around TP347LN tube is often looser than a low-carbon Nb-stabilized purchase order can afford. ASTM A213 Grade TP347LN / UNS S34751 is the governing designation for this article; European or Japanese wrought names that mention “347LN” or low-carbon Nb-stabilized 18-8 point to related families but are not automatic substitutes on an A213 mill test certificate. When a datasheet says “equivalent to 347LN,” confirm which product standard, tensile/hardness table, C/N/Nb package, and heat-treatment path the mill will actually certify.

Designation Notes
ASTM A213 / A213M Grade TP347LN Governing ASTM seamless boiler / HX tube product standard for this article
UNS S34751 Unified number listed in the stainless chemistry table
ASME SA-213 TP347LN Separate ASME Code Book adoption — dual-mark only when the PO asks
Related Nb grades TP347 / S34700 and TP347H / S34709 — different C/Nb formulas; not synonym stamps
Related LN (no Nb) TP304LN / S30453 — nitrogen-strengthened without niobium
Related plate A240 / SA240 flat product in related UNS families — order plate and tube under their own product standards

Dual A213/SA-213 marking is a purchase-order option, not a claim that the two standards are one document. Compare TP347, TP304LN, and TP348 on their own ASTM A213 pages before swapping grades on a familiar “347” or “LN” PMI reading alone.

Heat Treatment and Delivery Condition

TP347LN under ASTM A213 is furnished solution treated at a minimum of 1900 °F [1040 °C], then quenched in water or cooled rapidly by other means. The public heat-treatment table marks this row with Footnote F. Footnote F ties quench capability to A262 Practice E demonstrability when that test is ordered (Supplementary Requirement S4). Unlike TP347 and TP348, the public Table 3 row for TP347LN does not carry Footnote H beside the solution temperature. The public table also does not print a mandatory ASTM grain-size number for TP347LN.

Supplementary Requirement S2 in the public A213–13 excerpt lists TP347, TP347H, TP348, and TP348H among grades that shall receive a stabilization heat treatment when specified — TP347LN is not on that printed list. Supplementary Requirement S1 lists TP304L, TP316L, TP321, TP347, and TP348 for stress-relieved annealed delivery — again without TP347LN. Do not assume S1 or S2 from a verbal “stabilize like 347” note; write negotiated stabilization language on the purchase order if the project needs it for this UNS.

Cold-finished versus hot-finished is a process and dimensional route, not a substitute for the anneal. Delivery condition for SHH STEEL TP347LN is solution annealed and pickled (or bright annealed by agreement), with anneal temperature, quench method, and the C / N / Nb results on the EN 10204 3.1 certificate. For standard Nb framing open A213 TP347; for H-grade carbon and grain-size controls open A213 TP347H.

Corrosion Resistance

TP347LN’s chromium-rich passive film, ultra-low carbon, and niobium stabilization handle many boiler, superheater, and heat-exchanger duties where sensitizing thermal cycles would otherwise deplete chromium at grain boundaries. Ultra-low carbon reduces the carbon available to form chromium carbides; niobium ties up what remains; nitrogen restores room-temperature strength without reopening an L-grade-only path. That package is an IGC strategy, not a molybdenum addition for chlorides. In chloride-bearing cooling waters and many process exchangers, pitting and crevice attack become limiting, and buyers usually step to A213 TP316 / A213 TP316L or a higher-PREN grade rather than stretching Nb-stabilized 18-8 into wet corrosive service.

ASTM A213 itself does not publish a corrosion-rate table for TP347LN; selection remains engineering judgment against fluid, temperature, velocity, and inspection philosophy. When a specification calls for ASTM A262 Practice E, write Supplementary Requirement S4 onto the purchase order. Because TP347LN is both low-carbon and Nb-bearing, Practice E testing on sensitized specimens is the usual A262 expectation for this family — confirm the ordered edition and any negotiated sensitization path. SHH STEEL will not market TP347LN as a wet-chloride upgrade over molybdenum grades; the LN + Nb designation is about carbon control and stabilization chemistry, not about higher PREN.

Applications of A213 TP347LN Tube

TP347LN seamless tube under A213 is chosen for boiler, superheater, and heat-exchanger service where ultra-low carbon, intentional nitrogen, and a strict 15 × C niobium floor must deliver intergranular-corrosion resistance without forcing a molybdenum addition or an H-grade grain-size mandate. It is a selection for as-welded or thermally cycled steam and process tubing when the datasheet names S34751 specifically. It is the wrong default for chloride-rich cooling water that really needs Mo, and it is not an H-grade creep row. The table below pairs typical application areas with a selection note.

Application area Typical use of TP347LN tube Selection note
Boiler / steam HX Seamless A213 tube where ultra-low C + Nb + N is specified Confirm C 0.005–0.020, N 0.06–0.10, Nb ≥15×C on the MTC
Sensitizing thermal cycles Stabilized steam / process tubing ordered to S34751 Do not substitute TP347 without checking C/N/Nb
Process heat exchangers Seamless tube needing IGC resistance with recovered strength Prefer TP316L when chlorides dominate
Vs TP304LN duty When niobium stabilization is required on top of LN thinking Open TP304LN only if Nb is not on the datasheet
Vs H-grade duty When H carbon floor and grain size are NOT required If H-grade framing is needed, open TP347H / TP348H

For standard Nb open A213 TP347; for LN without Nb open A213 TP304LN; for Co/Ta-controlled Nb open A213 TP348 on the A213/A213M hub.

Weldability

TP347LN tube welds with matching or near-matching niobium-bearing austenitic filler for tube-to-tubesheet joints, attachment welds, and fabrication joins. Common practice uses ER347 / E347 (or equivalent covered electrodes) under a qualified WPS so weld-metal niobium supports stabilized service; many fabricators avoid defaulting to ER308L when the base tube is Nb-stabilized and the design assumes stabilization chemistry in the joint. Heat input control, interpass limits, and post-weld cleaning remain the fabricator’s responsibility under the applicable boiler or pressure-vessel code — A213 governs the seamless tube product, not the field or shop weld procedure.

Because A213 TP347LN is seamless, there is no mill longitudinal weld to radiograph the way welded pipe standards describe. Focus inspection language on tube integrity (hydro or NDE of each length), tube-to-tubesheet joint quality, C / N / Nb documentation on the base metal, and any contractual corrosion test. For tube that will enter wet as-welded service where an L-grade carbon ceiling without Nb is preferred, many owners change the base metal to A213 TP304L or A213 TP304LN. Specify end preparation and surface finish on the tube PO when orbital or clean-service joins are planned.

Surface Finishes

Standard mill delivery for ASTM A213 TP347LN is solution annealed and pickled, leaving a clean matte finish suitable for most boiler and heat-exchanger tube duty. Bright annealing under protective atmosphere produces a smoother reflective surface used on some clean-process lines and must be called out because it changes the heat-treatment route. Light polish or specified Ra on the bore or OD is a commercial or service-center operation on top of A213 product, not automatic with the grade stamp.

When a fouling-sensitive exchanger specification quotes an Ra maximum on the bore, put it on the tube purchase order with its own acceptance language and sampling plan. SHH STEEL stencils grade and heat treatment as standard requirements; polish, special OD grind, and passivation after fabrication remain commercial extras unless the contract says otherwise. Order end preparation together with finish so receiving inspection shares one acceptance language.

Inspection and Testing

Base ASTM A213 testing for TP347LN includes heat analysis (carbon 0.005–0.020%, nitrogen 0.06–0.10%, niobium meeting 0.20–0.50% and ≥15 × C), tension tests to the Table 4 floors (75/30 ksi), hardness tests to the Table 4 maximum (192 HBW / 90 HRB), flattening and flaring tests on a lot basis, and either hydrostatic testing or nondestructive electric testing of each length. The manufacturer may choose hydro versus NDE unless the purchase order fixes the method. Marking includes the ASTM designation, grade, size, heat number, and other clause-required data. Grain-size reporting is not a mandatory Table 3 item for TP347LN in the public excerpt unless the PO adds it.

Supplementary Requirements commonly added on TP347LN tube orders are summarized below. Invoke them by number or clear purchase-order wording; mills will not assume product analysis or IGC testing from a verbal “full certs” note. Note that S1 and S2 are not printed for TP347LN in the public A213–13 excerpt — negotiate separately if needed.

Option Purpose
Product analysis Confirms chemistry on finished tube — useful when C, N, or Nb sits near a band edge
S4 intergranular corrosion A262 Practice E on sensitized specimens for this low-C / stabilized family
Negotiated stabilization S2 is not printed for TP347LN — write agreed temperature/time if the project needs it
Nitrogen method Footnote B — analysis method by purchaser/producer agreement
Minimum vs average wall States which wall basis the size callout uses
Fixed hydro or NDE method Removes manufacturer’s option when the end user mandates one route
Third-party inspection / EN 10204 3.2 Witnessed testing and certificate when the project requires it

Ask the mill to state lot identity clearly on the certificate so hardness, tension, and C / N / Nb specimens map cleanly to the bundle you receive.

Packaging and Shipping

TP347LN tube leaves SHH STEEL bundled, capped or end-protected, and tagged for export or domestic delivery according to the length mix and bend form on the order. Bundle tags repeat the ASTM A213 grade, OD × wall (or BWG), heat number, and PO reference so site receiving can check the shipment without opening every certificate packet first. U-bent tubes need extra cradle or case protection so bend radii and legs are not distorted in transit.

Export packing can be bare bundles, wrapped bundles, or wooden-cased lengths for bright-annealed, polished, or small-bore material. We ship under the Incoterms on the order acknowledgement — FOB, CFR, CIF, EXW, or other agreed terms. Inland trucking, bilingual destination marks, or project color coding for bundle tags should be stated on the enquiry beside the metallurgical notes.

Why Choose SHH STEEL

SHH STEEL treats ASTM A213 TP347LN as a product standard with enforceable chemistry (ultra-low C, N band, Nb band and 15 × C formula), tensile, hardness, heat-treatment, and marking rules — not as a catalogue nickname for “any 347LN tube.” The MTC reports the full ladle chemistry including carbon, nitrogen, and niobium against both the fixed band and 15 × C, the Table 4 tensile/hardness set (75/30 ksi, 192 HBW / 90 HRB), and the anneal temperature; the stencil carries seamless tube identity under A213; and dual A213/SA-213 marking is offered only when requested.

We keep the LN + Nb conversation honest for boiler and HX duty. If standard Nb without the ultra-low C band is enough, we open A213 TP347. If H-grade carbon and grain size are required, we open A213 TP347H. If LN without niobium is enough, we open A213 TP304LN. If Co/Ta control is specified, we open A213 TP348. The A213/A213M hub is organized grade by grade under ASTM, seamless tube only.

Lead times combine near-term stock lengths with mill schedules; we say which is which on the quotation. Cut-to-length, U-bending, polish, and third-party inspection are defined extras. The tube that arrives should match the ASTM callout the engineer wrote, with paperwork a third-party inspector can read without translation.

Supply Capability

SHH STEEL can supply ASTM A213 TP347LN stainless steel tube against the edition and finish route named on your enquiry. The capability table below summarizes the sizes, finishes, and documents we regularly quote for this grade, followed by the Stock / Available sizes map buyers ask for when they need a quick sense of what to enquire against for ultra-low-C Nb-stabilized boiler and heat-exchanger duty.

Item SHH STEEL capability for TP347LN
Standard ASTM A213 / A213M (dual SA-213 marking on request) Grade TP347LN / UNS S34751
Product form Seamless only — cold-finished and hot-finished
Size Typical OD × min wall (or average wall) in the A213 usual band; other diameters by agreement
Wall / gauge Minimum wall or average wall; BWG / gauge callouts accepted on enquiry
Length Cut-to-length for boiler / superheater / HX bundles; mill random by agreement; U-bends on enquiry
Finish Annealed and pickled; bright annealed or light polish by agreement
Testing Tension (75/30 ksi), hardness (max 192 HBW / 90 HRB), C/N/Nb vs 15×C, flattening, flaring, hydro or NDE per length; full ladle chemistry on MTC; product analysis / S4 on order
Documents EN 10204 3.1 with full ladle chemistry and C/N/Nb results; third-party inspection / 3.2 on request
Trade terms FOB / CFR / CIF / EXW and other agreed Incoterms

Stock / Available sizes

SHH STEEL quotes TP347LN tube against a practical stock-and-mill enquiry range rather than a frozen warehouse SKU list. The sizes below are OD × wall / BWG combinations buyers most often request for ultra-low-C Nb-stabilized boiler and heat-exchanger tube; availability of any single line on a given week depends on mill drawing and our inbound schedule, so treat the table as a supply map for enquiry — not a guarantee of floor tonnage.

Item Typical stock / enquiry range for TP347LN
Outside diameter 19.05, 25.4, 31.8, 38.1, 44.5, 50.8, 63.5 mm (and other boiler/HX ODs on enquiry; up through the usual A213 ~5 in. [127 mm] band)
Wall / BWG BWG 14–18 class walls and metric min-wall equivalents; heavier walls for high-pressure duty by agreement
Common OD × wall examples 19.05 × 1.65 mm; 25.4 × 2.11 mm; 31.8 × 2.11 mm; 38.1 × 2.41 mm; 50.8 × 2.77 mm — illustrative HX/boiler sizes, confirm min vs average wall
Length Cut lengths for boiler / exchanger bundles; U-bends and straight random lengths on enquiry
Special Non-standard OD/wall, bright anneal, negotiated stabilization, dual A213/SA-213 marking, S4 IGC — confirm on enquiry before the heat is reserved

When you send an enquiry, list OD × wall (or BWG), wall basis (minimum or average), cold-finished or hot-finished preference, quantity or cut list, required marking (A213 alone or dual A213/SA-213), and any Supplementary Requirements (S4, product analysis, nitrogen method). We reply with what we can ship from near-term stock versus what needs a mill run, without inventing fake warehouse codes or tonnage claims.

Send the size list, finish route, quantity or cut lengths, required marking, Supplementary Requirements, and destination on one enquiry. We will confirm chemistry (including the C/N/Nb package), tensile, and hardness against the stainless chemistry table and Table 4, state what ships from near-term availability versus mill production, and keep the offer aligned with ASTM A213 / A213M. Related grades such as A213 TP347, A213 TP304LN, and A213 TP348 sit on the same hub when the datasheet steps beyond TP347LN.

FAQ

Is ASTM A213 the same as ASME SA-213 for TP347LN?
No. ASTM A213 / A213M is the ASTM International product specification for seamless boiler, superheater, and heat-exchanger tubes; ASME SA-213 / SA-213M is the separate ASME Code Book adoption of that grade text. Chemistry, tensile, hardness, and C/N/Nb rules align closely for a given referenced edition, but they remain two independent standards. Dual-mark A213/SA-213 tube only when the purchase order asks for both names on the stencil and MTC.
Does ASTM A213 TP347LN include welded or HCW tube?
No. ASTM A213 covers seamless tube only. There is no WLD or HCW manufacturing type under this product standard the way ASTM A312 describes pipe. The process choice for TP347LN under A213 is cold-finished versus hot-finished seamless tube, plus the ultra-low-C, nitrogen, Nb-formula chemistry, heat-treatment, and testing clauses of the ordered edition.
What are the carbon, nitrogen, and niobium limits for A213 TP347LN?
Melting carbon is 0.005–0.020%, nitrogen is 0.06–0.10%, and niobium is 0.20–0.50% with Footnote F requiring Nb not less than 15 times the carbon content. Chromium is 17.0–19.0% and nickel is 9.0–13.0%. That package is stricter on carbon and on the Nb multiplier than TP347’s ≤0.08% C and ≥10 × C rule. Confirm the ordered A213 edition for the exact stainless-table number.
TP347LN vs TP347 — when do I need the LN grade?
Order TP347LN when the datasheet needs ultra-low carbon 0.005–0.020%, intentional nitrogen 0.06–0.10%, and niobium both in the 0.20–0.50% band and at ≥15 × C. Order TP347 when Nb ≥10 × C with C ≤0.08% and no mandatory nitrogen band are enough. They share a niobium family but are not synonym stamps on the MTC — chromium windows and Nb formulas differ as well.
TP347LN vs TP304LN — niobium or nitrogen-only strengthening?
Both carry intentional nitrogen and low carbon, but TP304LN has no niobium requirement and uses N 0.10–0.16% with C ≤0.035% (Footnote D to 0.040% on small/thin tube), while TP347LN uses N 0.06–0.10%, C 0.005–0.020%, and Nb 0.20–0.50% ≥15 × C. Choose TP347LN when the datasheet demands Nb stabilization on top of LN thinking; choose TP304LN when nitrogen-strengthened 18-8 without Nb is enough.
What does Footnote F mean for TP347LN heat treatment and chemistry?
Two different Footnote F markers appear in public A213 text. On the chemistry table, Footnote F for TP347LN requires Nb ≥15 × C in addition to the 0.20–0.50% band. On the heat-treatment table, Footnote F ties quench rate to A262 Practice E capability when that test is ordered under Supplementary Requirement S4. Neither footnote makes S4 automatic — write S4 on the PO when IGC testing is required.
Is Supplementary Requirement S2 listed for TP347LN?
Not in the public A213–13 excerpt. S2 lists TP309HCb, TP310HCb, TP310HCbN, TP321, TP321H, TP347, TP347H, TP348, and TP348H for a purchaser-specified stabilization heat treatment. TP347LN is absent from that printed list. If your project needs a lower-temperature stabilization after the 1900 °F solution anneal for S34751, negotiate the temperature and time on the purchase order rather than assuming S2 applies by grade nickname.
Does Table 4 set a hardness limit for TP347LN?
Yes. Table 4 for TP347LN lists tensile strength 75 ksi [515 MPa], yield strength 30 ksi [205 MPa], elongation 35%, and a hardness maximum of 192 HBW / 200 HV or 90 HRB. Hardness tests are part of lot acceptance under A213, which differs from many A312 pipe rows for related UNS numbers that omit a Table 4 hardness cap. Ask the mill to report hardness beside the tensile results on the EN 10204 3.1 certificate.
Minimum wall vs average wall for A213 TP347LN — which should I specify?
Order minimum wall when the boiler or heat-exchanger datasheet is written around a guaranteed minimum thickness after tolerance — the usual practice for A213 tube. Order average wall only when the purchase order explicitly allows average-wall product and the designer has accepted that basis. Put the wall basis on the enquiry before the mill selects A1016 tolerance tables.
Can I dual-certify TP347LN with TP347 on the same heat?
Usually not as a routine path. TP347LN’s carbon ceiling of 0.020% sits well below TP347’s ≤0.08%, but TP347 does not require nitrogen 0.06–0.10% or the 15 × C Nb floor, and TP347LN’s chromium window is 17–19% versus TP347’s 17–20%. A heat that clears both chemistries plus both tensile/hardness paths is uncommon. Spell any dual-marking request on the enquiry before the heat is selected rather than assuming it from a PMI gun.
Is TP347LN a good choice for chloride-rich cooling water?
Usually no as a first choice. Ultra-low carbon and niobium help intergranular corrosion resistance but do not raise PREN the way molybdenum does. Prefer TP316L or a higher-Mo grade when chlorides dominate aqueous service; reserve TP347LN for stabilized boiler and heat-exchanger framing where the C/N/Nb package earns its keep.
What heat treatment does A213 require for TP347LN?
Solution treatment at a minimum of 1900 °F [1040 °C] followed by water quench or other rapid cool, with Footnote F quench/A262 capability language when S4 is ordered. There is no mandatory ASTM grain-size number in the public Table 3 row for TP347LN, and Footnote H is not printed beside this grade’s solution temperature in the public excerpt. Confirm the ordered edition on the purchase order.

Conclusion

ASTM A213 TP347LN / UNS S34751 is the ultra-low-carbon, nitrogen-bearing, niobium-stabilized seamless stainless steel tube grade for boiler, superheater, and heat-exchanger service when C 0.005–0.020%, N 0.06–0.10%, and Nb 0.20–0.50% with ≥15 × C must deliver IGC resistance without a molybdenum addition or an H-grade grain-size mandate. SHH STEEL supplies cold-finished and hot-finished seamless tube in the usual OD × wall / BWG band, solution annealed at 1900 °F [1040 °C], tested to Table 4 tensile and hardness limits with C / N / Nb reported, and documented on EN 10204 3.1 certificates — with dual SA-213 marking only when the order asks for that separate ASME standard. For sister grades and stock-oriented size discussions, start from the A213/A213M hub, then send your OD × wall list, wall basis, dual-marking needs, and C/N/Nb requirements so we can align mill and near-term availability to the ASTM callout.

Contact: admin@steelspecs.com

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response