ASTM A213 UNS S31002 Stainless Steel Tube | ASTM A213 Stainless Steel - SHH STEEL

ASTM A213 UNS S31002 Stainless Steel Tube

ASTM A213 UNS S31002 (no TP letter — low-C low-Si 25Cr–20Ni austenitic) seamless boiler, superheater and heat-exchanger tube with C ≤0.02%, Si ≤0.15%, Cr 24.0–26.0%, Ni 19.0–22.0%, Mo ≤0.10%, N ≤0.10%, Table 4 floors of 73/30 ksi, hardness max 192 HBW / 90 HRB, and 1900 °F solution anneal. SHH STEEL supplies cold-finished and hot-finished seamless tube with EN 10204 3.1 MTCs.
Grade
UNS S31002 (no TP letter — low-C low-Si 25Cr–20Ni)
Standard
ASTM A213 / A213M
Product form
Seamless boiler / superheater / heat-exchanger tube (cold-finished and hot-finished)
Size
Typical OD × min wall (or average wall) within ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD and ~0.015–0.500 in. [0.4–12.7 mm] wall; other diameters by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is ASTM A213 UNS S31002 Stainless Steel Tube

ASTM A213 / A213M lists UNS S31002 among the austenitic stainless grades that carry no common TP letter — Footnote C states the UNS number uniquely identifies the alloy. Within the 310 family it is the low-carbon, low-silicon member: melting carbon ≤0.02%, silicon ≤0.15%, chromium 24.0–26.0%, nickel 19.0–22.0%, with molybdenum ≤0.10% and nitrogen ≤0.10% as controlled maxima rather than no-requirement ellipses. Commercially buyers sometimes call it 310L or low-carbon 310; those shop names still need A213 (or the separate ASME SA-213 adoption) on the purchase order so tube product-standard minimum-wall, test, and marking clauses apply.

SHH STEEL can supply ASTM A213 UNS S31002 stainless steel tube as seamless cold-finished and hot-finished product in the usual boiler, furnace, and heat-exchanger OD × wall / BWG band, shipped with EN 10204 3.1 mill test certificates that report the full low-C / low-Si chemistry set and the Table 4 tensile and hardness results (73 ksi [500 MPa] / 30 ksi [205 MPa], hardness max 192 HBW / 90 HRB). Dual A213 / SA-213 marking is available only when the purchase order asks for both independent standards. Browse 310-family grades on the A213/A213M hub.

Do not paste a TP310S chemistry block onto an S31002 certificate — carbon ≤0.02% and silicon ≤0.15% are much tighter than TP310S’s C ≤0.08% / Si ≤1.00%, and Table 4 tensile is 73 ksi rather than 75 ksi. Sister grades under the same ASTM standard include A213 TP310S, A213 TP310H, A213 TP310Cb, A213 TP310MoLN, and A213 TP309S. A213 covers seamless tube only — cold-finished versus hot-finished is the process choice, not a WLD/HCW manufacturing type.

Chemical Composition of A213 UNS S31002

UNS S31002 chemistry keeps the classic 24–26% Cr / 19–22% Ni oxidation window of the 310 family while tightening carbon to ≤0.02% and silicon to ≤0.15% — an IGC-leaning, low-residual path rather than an H-grade carbon floor or a high-Si furnace path. Melting analysis is mandatory; product analysis applies only when ordered through A1016 / A480 A1.1. Phosphorus ≤0.020% and sulfur ≤0.015% are also tighter than TP310S. Molybdenum and nitrogen appear as ≤0.10% maxima (not ellipses). There is no TP grade letter — order and mark by UNS S31002 (Footnote C). Nitrogen analysis method is by agreement (Footnote B).

The tables below reproduce the melt limits from the public A213 stainless chemistry table, product-analysis limits from A480 Table A1.1 practice, and a short snapshot against TP310S / TP310H. Confirm the ordered edition before treating secondary catalogues as acceptance text.

Melting analysis (heat / ladle analysis)

Element UNS S31002 melting analysis
Carbon (C) ≤ 0.02
Manganese (Mn) ≤ 2.00
Phosphorus (P) ≤ 0.020
Sulfur (S) ≤ 0.015
Silicon (Si) ≤ 0.15
Chromium (Cr) 24.0 – 26.0
Nickel (Ni) 19.0 – 22.0
Molybdenum (Mo) ≤ 0.10
Nitrogen (N) ≤ 0.10
Niobium (Nb) … (no requirement)
Titanium (Ti) … (no requirement)

Source: ASTM A213/A213M stainless chemistry table for UNS S31002 (public htpipe A213 PDF excerpt — _ref_a213.txt A213/A213M − 13). Silicon ≤0.15% and carbon ≤0.02% must both appear on the certificate; an MTC that only shows “310S chemistry” is incomplete for S31002.

Product analysis — A480/A480M Table A1.1 tolerances applied

Element Melting Tolerance (A480 A1.1) Product analysis limit
Carbon (C) ≤ 0.02 0.005 over ≤ 0.025
Manganese (Mn) ≤ 2.00 0.04 over ≤ 2.04
Phosphorus (P) ≤ 0.020 0.005 over ≤ 0.025
Sulfur (S) ≤ 0.015 0.005 over ≤ 0.020
Silicon (Si) ≤ 0.15 0.05 over ≤ 0.20
Chromium (Cr) 24.0 – 26.0 0.25 under / over 23.75 – 26.25
Nickel (Ni) 19.0 – 22.0 0.15 under / 0.20 over 18.85 – 22.20
Molybdenum (Mo) ≤ 0.10 0.02 over ≤ 0.12
Nitrogen (N) ≤ 0.10 0.01 over ≤ 0.11

310-family snapshot — S31002 / TP310S / TP310H

Element S31002 TP310S (S31008) TP310H (S31009)
C ≤ 0.02 ≤ 0.08 0.04 – 0.10
Si ≤ 0.15 ≤ 1.00 ≤ 1.00
Cr 24.0 – 26.0 24.0 – 26.0 24.0 – 26.0
Ni 19.0 – 22.0 19.0 – 22.0 19.0 – 22.0
Mo ≤ 0.10 … …
N ≤ 0.10 … …

Read carbon and silicon first: S31002 is the low-C / low-Si path inside the same Cr–Ni oxidation window as A213 TP310S. It is not an H-grade (no 0.04% carbon floor, no mandatory grain-size number) and not a niobium-stabilized grade like A213 TP310Cb. Dual S31002/TP310S certification is not automatic — TP310S allows higher carbon and silicon than S31002 can carry.

When product analysis is ordered, use the A480 path above and put any tighter carbon or silicon ceiling on the purchase order before the heat is selected. Ultra-low C and low-Si product tolerances are edition-sensitive — confirm the ordered A480 edition if product analysis is contractual.

Mechanical Properties of A213 UNS S31002

ASTM A213 Table 4 sets UNS S31002 tensile acceptance at 73 ksi [500 MPa] tensile strength and 30 ksi [205 MPa] yield strength (0.2% offset), with elongation 35% minimum in 2 in. or 50 mm and hardness max 192 HBW / 200 HV or 90 HRB. Note the tensile floor is 73 ksi — two ksi below TP310S / TP310H’s 75 ksi under the same product standard — so a TP310S tensile-only certificate does not clear S31002, and an S31002 heat does not automatically dual-certify to TP310S on tensile alone even when chemistry overlaps are checked carefully.

Property UNS S31002 requirement (Table 4)
Tensile strength, min 73 ksi [500 MPa]
Yield strength (0.2% offset), min 30 ksi [205 MPa]
Elongation in 2 in. or 50 mm, min 35%
Hardness, max 192 HBW / 200 HV or 90 HRB
Grain size No mandatory ASTM grain-size number (unlike TP310H)

Source: ASTM A213/A213M Table 4 for UNS S31002 (public htpipe A213 PDF excerpt). Mechanical property requirements do not apply to tubing smaller than 1/8 in. [3.2 mm] ID or thinner than 0.015 in. [0.4 mm] wall. Flattening and flaring tests apply on a lot basis beside tension and hardness.

Room-temperature tensile is slightly below TP310S; the reason to order S31002 is the low-C / low-Si chemistry for IGC-leaning 25-20 duty, not a higher Table 4 floor. A tensile-only MTC that omits hardness is incomplete for boiler-tube release. For H-grade carbon and grain-size controls open A213 TP310H; for Nb stabilization open A213 TP310Cb.

Dimensions and Tolerances

Dimensional supply for ASTM A213 UNS S31002 remains tube language — OD × min wall (or average wall) and BWG / gauge — covering boiler, furnace, and heat-exchanger sizes rather than leading with ASME B36.19 pipe schedules. Usual A213 sizes run from about 1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD with min wall about 0.015–0.500 in. [0.4–12.7 mm]; other diameters by agreement. Furnace and radiant-tube datasheets almost always assume a minimum-wall reading — state wall basis on the purchase order.

OD and wall variations follow ASTM A1016/A1016M as invoked by A213. Cold-finished tubes commonly hold tighter OD; hot-finished tubes allow wider windows. Cold-finished average wall is often summarized as ±10%; minimum-wall product follows A1016 minimum-wall tables. Confirm exact rows for the OD and finish on the ordered edition.

Item Typical A213 UNS S31002 dimensional practice
Product form Seamless only (cold-finished or hot-finished)
Usual size band ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD; wall ~0.015–0.500 in. [0.4–12.7 mm]
Wall basis Minimum wall (default for boiler / furnace / HX) or average wall when specified
OD / wall tolerances Per ASTM A1016/A1016M for finish route and size
Length Cut lengths for furnace / boiler / HX bundles; mill random by agreement
Secondary note B36.19 schedules only as a buyer cross-reference

Put cut list, design metal temperature context, and end preparation on the enquiry. Minimum wall remains a first-class A213 concept for S31002 the same way it does for other 310-family boiler tube.

Equivalent Grades

Equivalence language around S31002 tube often collapses “310L” nicknames across plate, cast, and tube product forms. ASTM A213 UNS S31002 is the governing designation for this article; commercial 310L aliases point to similar low-carbon 25Cr–20Ni chemistry families but are not automatic substitutes on an A213 MTC.

Designation Notes
ASTM A213 / A213M UNS S31002 Governing ASTM seamless boiler / HX tube product standard — no TP letter (Footnote C)
UNS S31002 Unified number that uniquely identifies the alloy
310L (commercial) Shop name for low-carbon 310-family chemistry — does not replace S31002 on the MTC
ASME SA-213 UNS S31002 Separate ASME Code Book adoption — dual-mark only when the PO asks
Related S-grade A213 TP310S — same Cr–Ni, C ≤0.08, Si ≤1.00, Table 4 75/30 ksi
Related H-grade A213 TP310H — C 0.04–0.10, grain size No. 7 or coarser
Related Nb grade A213 TP310Cb — C ≤0.08 plus niobium stabilization
Related plate A240 / SA240 flat product in the 310 family — order plate and tube under their own standards

Dual A213/SA-213 marking is a purchase-order option. Compare TP310S, TP310H, and TP310Cb on their own ASTM A213 pages before swapping 310-family grades inside a furnace or boiler tube list.

Heat Treatment and Delivery Condition

UNS S31002 under ASTM A213 is furnished solution treated at a minimum of 1900 °F [1040 °C], then quenched in water or cooled rapidly by other means. Public Table 3 OCR places a Footnote F marker near the S31002 row; TP310S clearly carries Footnote F on the same 1900 °F minimum. UNCERTAIN: confirm ordered-edition footnote attachment for S31002 — if Footnote F applies, quench capability must be sufficient to prevent carbide re-precipitation as demonstrable by A262 Practice E capability, and the manufacturer need not run the test unless the purchase order specifies it (Supplementary Requirement S4).

Cold-finished versus hot-finished is a process and dimensional route, not a substitute for the anneal. Low-carbon 310-family tube still needs a thorough solution treatment and rapid cool so the ≤0.02% carbon advantage is not wasted by slow cooling through the sensitization range. Delivery condition for SHH STEEL S31002 is solution annealed and pickled (or bright annealed by agreement), with anneal temperature and quench method on the EN 10204 3.1 certificate.

Unlike A213 TP310H, S31002 has no mandatory ASTM grain-size number in the heat-treatment column. If a project datasheet asks for an E112 grain-size report, put that supplementary requirement on the purchase order rather than assuming base A213 includes it.

Corrosion Resistance

S31002 keeps the high-temperature oxidation and scaling resistance of the 24–26% Cr / 19–22% Ni balance that defines the 310 family, while the ≤0.02% carbon ceiling and ≤0.15% silicon ceiling lean the grade toward as-welded intergranular-corrosion resistance relative to higher-carbon 310 compositions. Molybdenum is only ≤0.10% — not a 2–3% chloride-pitting addition — so wet chloride cooling-water framing still belongs with A213 TP316L or higher-PREN grades, not with S31002 as a primary chloride strategy.

S31002 is not an H-grade and not a niobium-stabilized grade. When IGC after welding is the primary concern and the datasheet allows Nb stabilization at C ≤0.08%, evaluate A213 TP310Cb. When contractual A262 Practice E testing is required, write it onto the purchase order. Sulfidation, carburizing, and molten-salt environments need process-specific review beyond a generic “310L” catalogue claim.

Applications of A213 UNS S31002 Tube

Buyers specify ASTM A213 UNS S31002 when furnace, radiant, reformer, or high-temperature heat-exchanger duty needs the 25Cr–20Ni oxidation step with a low-carbon / low-silicon path for IGC-leaning fabrication — without an H-grade carbon floor or niobium stabilization. Typical placements include furnace tubes and hangers, radiant coils, muffles, retorts, and heat-exchanger bundles where scaling resistance at elevated metal temperature drives grade selection and as-welded IGC risk must stay low.

Service theme Why S31002 is considered
Furnace / radiant tube (IGC-leaning) 24–26 Cr / 19–22 Ni oxidation plus C ≤0.02%
High-temperature HX Seamless A213 tube form + low-C / low-Si 310 chemistry
Not an H-grade substitute No carbon floor / grain-size mandate — open TP310H for creep framing
Not primary for wet chlorides Mo ≤0.10% only — use Mo grades for chloride PREN

When S-grade carbon ≤0.08% without the ultra-low C / low-Si path is enough, open A213 TP310S. When creep-range carbon and grain-size controls are mandatory, move to A213 TP310H. When Nb stabilization is mandatory, open A213 TP310Cb on the A213/A213M hub.

Weldability

S31002 tube welds with conventional austenitic practices using matching or near-matching 310 / 25-20 fillers selected for the joint design and service temperature. The ≤0.02% carbon ceiling reduces sensitization risk in the heat-affected zone relative to higher-carbon 310 compositions; heat input control and post-weld cleaning still matter for corrosive or cyclic thermal service. Do not assume a soft ER308L deposit will match 25-20 oxidation performance without a qualified WPS review.

For tube-to-tubesheet and coil welding, keep the filler chemistry aligned with the base-metal Cr–Ni windows and confirm any project restriction on ferrite or residual elements. When the datasheet demands niobium-stabilized base metal for IGC after welding, do not “solve” that with filler alone — specify A213 TP310Cb or A213 TP310HCb. Repair welding, when permitted, follows A1016/A1016M practice invoked by A213.

Surface Finishes

Standard delivery for ASTM A213 UNS S31002 from SHH STEEL is solution annealed and pickled, with a clean ID/OD suitable for furnace and exchanger fabrication. Bright annealed or polished finishes are available by agreement when the process side needs lower roughness or a brighter appearance.

State finish expectations on the enquiry together with OD × wall and end preparation. Do not assume a bright finish from a generic “stainless tube” line item — pickled anneal is the default boiler/HX path unless the purchase order says otherwise.

Inspection and Testing

Lot testing for ASTM A213 UNS S31002 follows the tension, hardness, flattening, and flaring requirements of A213 together with A1016/A1016M. Chemistry is verified on the heat (and on product when ordered) — carbon ≤0.02% and silicon ≤0.15% must both clear. Non-destructive examination follows the ordered edition and any purchaser supplementary requirements.

EN 10204 3.1 mill test certificates from SHH STEEL report ladle chemistry, tensile and hardness results (73/30 ksi, 192 HBW / 90 HRB), heat-treatment condition, and dimensions. Ask for A262 Practice E on the PO when IGC capability must be demonstrated by actual test. Third-party witness and dual A213/SA-213 marking are available when written into the enquiry.

Packaging and Shipping

S31002 tubes ship in capped or plugged bundles with weather protection suited to the destination and transport mode. Cut lengths for furnace and exchanger bundles are labeled by heat and size; export packing uses wooden cases or steel-frame crates when the route requires them.

Marking includes ASTM A213, UNS S31002, size, heat number, and SHH STEEL identification. Dual SA-213 marking appears only when the purchase order requests it. Packing lists reference the same heat numbers shown on the EN 10204 3.1 certificates.

Why Choose SHH STEEL

SHH STEEL treats ASTM A213 UNS S31002 as a specification-led tube product, not a nickname swap for TP310S or “any 310L tube.” Every quotation ties OD × wall / BWG, wall basis, finish route, and marking language to the ordered edition — so furnace and boiler buyers receive C ≤0.02%, Si ≤0.15%, and Table 4 73/30 ksi results that match what the datasheet actually called.

We keep the 310-family distinctions honest: S31002 low-C / low-Si versus TP310S carbon ceiling versus TP310H floor and grain size versus TP310Cb stabilization. Dual A213/SA-213 marking, A262 when ordered, and EN 10204 3.1 documentation are written options. Browse sister grades on the A213/A213M hub before locking a furnace tube list.

Supply Capability

SHH STEEL supplies ASTM A213 UNS S31002 seamless stainless steel tube in cold-finished and hot-finished routes across the usual boiler, furnace, and heat-exchanger OD × wall / BWG band. Capability below is an enquiry range — not a frozen warehouse SKU or tonnage claim.

Capability SHH STEEL practice for UNS S31002
Product form Seamless cold-finished and hot-finished tube
Standards ASTM A213 / A213M; dual SA-213 when PO asks
Size band Typical within ~1/8 in. ID to 5 in. OD; other diameters by agreement
Wall basis Minimum wall or average wall as specified
Documentation EN 10204 3.1 MTC with C ≤0.02% and Si ≤0.15% reported; third-party witness on request
Trade terms FOB / CFR / CIF / EXW and other agreed Incoterms

Stock / Available sizes

SHH STEEL quotes S31002 against a stock-and-mill enquiry range rather than a frozen SKU/tonnage list. Representative OD × wall / BWG combinations for furnace, boiler, and heat-exchanger tube appear below.

Item Typical stock / enquiry range for UNS S31002
Outside diameter 19.05, 25.4, 31.8, 38.1, 42.4, 50.8, 60.3, 76.2 mm (and other furnace/HX ODs on enquiry; through the usual A213 ~5 in. [127 mm] band)
Wall / BWG BWG 10–18 class walls and metric min-wall equivalents; heavier walls by agreement
Common OD × wall examples 25.4 × 2.11 mm; 31.8 × 2.77 mm; 38.1 × 2.77 mm; 42.4 × 3.56 mm; 50.8 × 3.05 mm; 60.3 × 3.91 mm — illustrative, confirm min vs average wall
Length Cut lengths for furnace / exchanger bundles; bends and random mill lengths on enquiry
Special Non-standard OD/wall, bright anneal, dual A213/SA-213, A262 Practice E, third-party witness — confirm before heat reservation

Send OD × wall (or BWG), wall basis, finish route, quantity or cut list, marking (A213 or dual A213/SA-213), and Supplementary Requirements on one enquiry. We confirm C ≤0.02% / Si ≤0.15% / Cr 24–26% / Ni 19–22% chemistry and Table 4 73/30 ksi without inventing fake warehouse codes. Sisters A213 TP310S, A213 TP310H, and A213 TP309S sit on the same hub.

FAQ

Is ASTM A213 the same as ASME SA-213 for UNS S31002?
No. ASTM A213 / A213M is the ASTM International product specification for seamless boiler, superheater, and heat-exchanger tubes; ASME SA-213 / SA-213M is the separate ASME Code Book adoption. Dual-mark only when the purchase order asks for both names on the stencil and MTC. Chemistry and tensile floors align closely for a given referenced edition, but the standards remain independent.
Why does S31002 have no TP letter under A213?
Footnote C to the stainless chemistry table states that for these alloys there is no common grade designation — the UNS number uniquely identifies the alloy. Order and mark by UNS S31002 on the purchase order, stencil, and MTC. Do not invent a TP letter or assume a TP310S stamp will clear an S31002 datasheet.
What is the chemistry of ASTM A213 UNS S31002?
Melting analysis includes C ≤0.02%, Mn ≤2.00%, P ≤0.020%, S ≤0.015%, Si ≤0.15%, Cr 24.0–26.0%, Ni 19.0–22.0%, Mo ≤0.10%, and N ≤0.10%, with Nb and Ti as no-requirement ellipses. Nitrogen analysis method is by agreement (Footnote B). Confirm the ordered A213 edition on the purchase order; stainless table number is edition-dependent.
S31002 vs TP310S — which 310-family A213 tube should I order?
TP310S uses C ≤0.08%, Si ≤1.00%, and Table 4 floors of 75/30 ksi, with Mo and N as no-requirement ellipses. S31002 tightens carbon to ≤0.02% and silicon to ≤0.15%, lists Mo ≤0.10% and N ≤0.10%, and clears a slightly lower 73/30 ksi tensile floor. Order S31002 when the datasheet needs the ultra-low C / low-Si path; stay with TP310S when the S-grade carbon ceiling without those tighter residuals is what the PO asks for.
S31002 vs TP310H — when do I need the H grade instead?
TP310H holds carbon in a 0.04–0.10% band and requires ASTM grain size No. 7 or coarser, with Table 4 floors of 75/30 ksi. S31002 uses C ≤0.02%, has no mandatory grain-size number, and clears 73/30 ksi. Order TP310H when creep-range carbon and coarse-grain controls drive the datasheet; order S31002 when the low-C / low-Si IGC-leaning path is what the PO asks for.
Is 310L the same as ASTM A213 UNS S31002?
310L is a common commercial alias for low-carbon 310-family chemistry. On an A213 mill test certificate and stencil, the governing designation is UNS S31002 under ASTM A213 / A213M. Write the UNS number on the purchase order; treat the shop name as a commercial alias, not a substitute product standard — and do not assume every "310L" catalogue matches S31002’s Si ≤0.15% and Mo/N maxima.
What tensile and hardness floors does Table 4 set for S31002?
Table 4 for UNS S31002 lists 73 ksi [500 MPa] tensile strength, 30 ksi [205 MPa] yield strength, 35% elongation, and a hardness maximum of 192 HBW / 200 HV or 90 HRB. Hardness tests are part of lot acceptance under A213. Note the tensile floor is two ksi below TP310S — do not treat the grades as interchangeable on tensile paperwork alone.
What heat treatment does A213 require for UNS S31002?
Solution treatment at a minimum of 1900 °F [1040 °C], followed by water quench or other rapid cool. Public Table 3 OCR places a Footnote F marker near the S31002 row — confirm ordered-edition footnote attachment; if Footnote F applies, A262 Practice E capability language sits on the quench requirement and the manufacturer need not run the test unless the purchase order specifies it (S4).
Does ASTM A213 UNS S31002 include welded or HCW tube?
No. ASTM A213 covers seamless boiler, superheater, and heat-exchanger tubes only. There is no WLD or HCW manufacturing-type letter under A213. Cold-finished versus hot-finished describes the seamless process route and dimensional tolerances — not a welded product form.
Minimum wall vs average wall for A213 S31002 — which should I specify?
Boiler, furnace, and superheater datasheets almost always expect minimum wall. Average wall is allowed when the purchase order says so and tolerances follow A1016/A1016M for that basis. State the wall basis explicitly on the enquiry — do not assume a schedule-number pipe reading replaces min-wall tube language under A213.
Can you dual-certify A213 and SA-213 UNS S31002?
Yes, when the purchase order asks for both independent standard names on the stencil and MTC, and the heat clears the chemistry and mechanical requirements of the referenced editions. Dual marking is a documentation and stamping option — it does not merge ASTM A213 and ASME SA-213 into one standard. Spell C ≤0.02%, Si ≤0.15%, and dual-mark requirements into the enquiry before heat reservation.

Conclusion

ASTM A213 UNS S31002 is the low-carbon, low-silicon 24–26% Cr / 19–22% Ni seamless stainless steel tube grade for boiler, furnace, and heat-exchanger service when C ≤0.02% / Si ≤0.15% IGC-leaning chemistry — not H-grade carbon/grain-size controls or molybdenum chloride framing — drives grade selection inside the 310 family. SHH STEEL supplies cold-finished and hot-finished seamless tube in the usual OD × wall / BWG band, solution annealed at 1900 °F [1040 °C], tested to Table 4 73/30 ksi and hardness limits, and documented on EN 10204 3.1 certificates — with dual SA-213 marking only when the purchase order asks.

Contact: admin@steelspecs.com

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X