JIS G3463

Product Showcase

JIS G3463 Stainless Steel Products

SHH STEEL offers JIS G3463-compliant 304/316 stainless steel tubes. JIS G3463 specifies stainless steel tubes for boilers and heat exchangers, suitable for high-temperature and high-pressure environments. Certified quality, competitive prices, customizable. Trust SHH STEEL!

JIS G3463 SUSXM27TB Stainless Steel Tube | JIS G3463 Stainless Steel Tube - SHH STEEL

JIS G3463 SUSXM27TB Stainless Steel Tube

JIS G3463 SUSXM27TB stainless steel tube (XM27 / UNS S44627 class (26Cr-Mo ferritic)), ferritic, Table 3 cast analysis, Rm min 412 N/mm² / proof min 245 N/mm², annealed. SHH STEEL can produce and supply seamless or welded routes with mill certificates.
View More

JIS G3463 SUSXM8TB Stainless Steel Tube

JIS G3463 SUSXM8TB stainless steel tube (XM8 / Ti-stabilised 18Cr ferritic), ferritic, Table 3 cast analysis, Rm min 412 N/mm² / proof min 206 N/mm², annealed. SHH STEEL can produce and supply seamless or welded routes with mill certificates.
View More
JIS G3463 SUSXM15J1TB Stainless Steel Tube | JIS G3463 Stainless Steel Tube - SHH STEEL

JIS G3463 SUSXM15J1TB Stainless Steel Tube

JIS G3463 SUSXM15J1TB stainless steel tube (XM15J1 / high-Si austenitic (≈XM-15 class)), austenitic, Table 3 cast analysis, Rm min 520 N/mm² / proof min 206 N/mm², solution annealed. SHH STEEL can produce and supply seamless or welded routes with mill certificates.
View More
JIS G3463 SUS890LTB Stainless Steel Tube | JIS G3463 Stainless Steel Tube - SHH STEEL

JIS G3463 SUS890LTB Stainless Steel Tube

JIS G3463 SUS890LTB stainless steel tube (~904L-class Cu-Mo austenitic (JIS SUS890L)), austenitic, Table 3 cast analysis, Rm min 481 N/mm² / proof min 177 N/mm², solution annealed. SHH STEEL can produce and supply seamless or welded routes with mill certificates.
View More
JIS G3463 SUS836LTB Stainless Steel Tube | JIS G3463 Stainless Steel Tube - SHH STEEL

JIS G3463 SUS836LTB Stainless Steel Tube

JIS G3463 SUS836LTB stainless steel tube (~6Mo / high-Mo Ni austenitic (JIS SUS836L)), austenitic, Table 3 cast analysis, Rm min 520 N/mm² / proof min 206 N/mm², solution annealed. SHH STEEL can produce and supply seamless or welded routes with mill certificates.
View More
JIS G3463 SUS444TB Stainless Steel Tube | JIS G3463 Stainless Steel Tube - SHH STEEL

JIS G3463 SUS444TB Stainless Steel Tube

JIS G3463 SUS444TB stainless steel tube (444 / UNS S44400), ferritic, Table 3 cast analysis, Rm min 412 N/mm² / proof min 245 N/mm², annealed. SHH STEEL can produce and supply seamless or welded routes with mill certificates.
View More
JIS G3463 SUS436LTB Stainless Steel Tube | JIS G3463 Stainless Steel Tube - SHH STEEL

JIS G3463 SUS436LTB Stainless Steel Tube

JIS G3463 SUS436LTB stainless steel tube (436L Mo ferritic), ferritic, Table 3 cast analysis, Rm min 410 N/mm² / proof min 245 N/mm², annealed. SHH STEEL can produce and supply seamless or welded routes with mill certificates.
View More

JIS G3463 SUS430J1LTB Stainless Steel Tube

JIS G3463 SUS430J1LTB stainless steel tube (Cu-Nb low-C ferritic (430J1L)), ferritic, Table 3 cast analysis, Rm min 390 N/mm² / proof min 205 N/mm², annealed. SHH STEEL can produce and supply seamless or welded routes with mill certificates.
View More

JIS G3463 SUS430LXTB Stainless Steel Tube

JIS G3463 SUS430LXTB stainless steel tube (430LX Ti/Nb-stabilised), ferritic, Table 3 cast analysis, Rm min 360 N/mm² / proof min 175 N/mm², annealed. SHH STEEL can produce and supply seamless or welded routes with mill certificates.
View More

JIS G3463 SUS430TB Stainless Steel Tube

JIS G3463 SUS430TB stainless steel tube (430 / UNS S43000), ferritic, Table 3 cast analysis, Rm min 412 N/mm² / proof min 245 N/mm², annealed. SHH STEEL can produce and supply seamless or welded routes with mill certificates.
View More
JIS G3463 SUS410TiTB Stainless Steel Tube | JIS G3463 Stainless Steel Tube - SHH STEEL

JIS G3463 SUS410TiTB Stainless Steel Tube

JIS G3463 SUS410TiTB stainless steel tube (410Ti / Ti-stabilised 12Cr), ferritic, Table 3 cast analysis, Rm min 412 N/mm² / proof min 206 N/mm², annealed. SHH STEEL can produce and supply seamless or welded routes with mill certificates.
View More
JIS G3463 SUS410TB Stainless Steel Tube | JIS G3463 Stainless Steel Tube - SHH STEEL

JIS G3463 SUS410TB Stainless Steel Tube

JIS G3463 SUS410TB stainless steel tube (410 / UNS S41000 class (tube as annealed ferritic practice)), ferritic, Table 3 cast analysis, Rm min 412 N/mm² / proof min 206 N/mm², annealed. SHH STEEL can produce and supply seamless or welded routes with mill certificates.
View More

JIS G3463 Stainless Steel Products

JIS G3463 SUSXM27TB Stainless Steel Tube JIS G3463 SUSXM8TB Stainless Steel Tube JIS G3463 SUSXM15J1TB Stainless Steel Tube JIS G3463 SUS890LTB Stainless Steel Tube
JIS G3463 SUS836LTB Stainless Steel Tube JIS G3463 SUS444TB Stainless Steel Tube JIS G3463 SUS436LTB Stainless Steel Tube JIS G3463 SUS430J1LTB Stainless Steel Tube
JIS G3463 SUS430LXTB Stainless Steel Tube JIS G3463 SUS430TB Stainless Steel Tube JIS G3463 SUS410TiTB Stainless Steel Tube JIS G3463 SUS410TB Stainless Steel Tube
JIS G3463 SUS409LTB Stainless Steel Tube JIS G3463 SUS409TB Stainless Steel Tube JIS G3463 SUS405TB Stainless Steel Tube JIS G3463 SUS329J4LTB Stainless Steel Tube
JIS G3463 SUS329J3LTB Stainless Steel Tube JIS G3463 SUS329J1TB Stainless Steel Tube JIS G3463 SUS347HTB Stainless Steel Tube JIS G3463 SUS347TB Stainless Steel Tube
JIS G3463 SUS321HTB Stainless Steel Tube JIS G3463 SUS321TB Stainless Steel Tube JIS G3463 SUS317LTB Stainless Steel Tube JIS G3463 SUS317TB Stainless Steel Tube
JIS G3463 SUS316TiTB Stainless Steel Tube JIS G3463 SUS316LTB Stainless Steel Tube JIS G3463 SUS316HTB Stainless Steel Tube JIS G3463 SUS316TB Stainless Steel Tube
JIS G3463 SUS315J2TB Stainless Steel Tube JIS G3463 SUS315J1TB Stainless Steel Tube JIS G3463 SUS312LTB Stainless Steel Tube JIS G3463 SUS310STB Stainless Steel Tube
JIS G3463 SUS310TB Stainless Steel Tube JIS G3463 SUS309STB Stainless Steel Tube JIS G3463 SUS309TB Stainless Steel Tube JIS G3463 SUS304LTB Stainless Steel Tube
JIS G3463 SUS304HTB Stainless Steel Tube JIS G3463 SUS304TB Stainless Steel Tube
Stainless Steel Pipes and Tubes supplier and exporter

Stainless Steel Pipes and Tubes

SHH STEEL, a premier Stainless Steel Pipes and Tubes exporter, produces and exports stainless steel pipes and tubes for chemical, marine, and food processing industries. Our seamless and welded products, like 304 and 316L (ASTM A312), ensure corrosion resistance and strength. With a 5,000-ton inventory, we deliver in 3–5 days, backed by SGS/TUV inspections and mill certificates. Choose SHH STEEL for seamless stainless steel pipes and custom solutions.

Stainless Steel Pipes and Tubes

SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

    *

    *

    *

    *


    X