ASTM A213 TP304 Stainless Steel Tube
What is ASTM A213 TP304 Stainless Steel Tube
ASTM A213 / A213M is the ASTM International product specification for seamless ferritic and austenitic alloy-steel boiler, superheater, and heat-exchanger tubes. Within that specification, Grade TP304 is the workhorse 18-8 chromium-nickel austenitic listed under UNS S30400, with Table 1 melting limits of carbon ≤0.08%, chromium 18.0–20.0%, and nickel 8.0–11.0%. Buyers who write “304 tube” or “304 HX tube” on a bill of materials still need to name A213 (or the separate ASME SA-213 adoption) on the purchase order so the mill knows which tube product standard, minimum-wall rules, tests, and marking clauses apply.
SHH STEEL can supply ASTM A213 TP304 stainless steel tube as seamless cold-finished and hot-finished product in the usual boiler and heat-exchanger OD × wall / BWG band, shipped with EN 10204 3.1 mill test certificates that report the full Table 1 ladle chemistry and the Table 4 tensile and hardness results. When a project also needs ASME Code Book marking, we dual-mark A213 / SA-213 on the same lengths only if the purchase order says so — ASTM A213 and ASME SA-213 remain two independent standards. Browse the grade family on the A213/A213M hub.
Commercially, TP304 tube is still called 304, 18-8, or S30400 boiler/HX tube; none of those shop names replace the ASTM grade on the MTC or stencil. Sister grades under the same ASTM standard include A213 TP304L, A213 TP304H, A213 TP316 / A213 TP316L, A213 TP321, and A213 TP347. A213 covers seamless tube only — there is no welded or HCW manufacturing type under this product standard — so cold-finished versus hot-finished seamless route is the finish/process choice, not a WLD/HCW stencil letter.
Chemical Composition of A213 TP304
Two chemistry layers matter for TP304 under ASTM A213. The melting (heat or ladle) analysis is mandatory for every heat under Table 1, while product analysis on finished tube applies only when Supplementary Requirement wording or the purchase order invokes product analysis through the general requirements in ASTM A1016/A1016M. Product-analysis tolerances are not reprinted as a standalone chemistry table inside A213 itself; when ordered, they typically flow from ASTM A480/A480M Table A1.1 via that general-requirements path. SHH STEEL reports the actual ladle values — and the product values when ordered — and does not advertise tighter catalogue chemistry windows that the ASTM standard does not publish.
The tables below reproduce the Table 1 heat analysis for TP304 / UNS S30400 and the product-analysis limits that result from applying A480 Table A1.1 tolerances. Values are maximum unless a range is shown, and an ellipsis (…) means the ordered edition sets no requirement for that element, so it need not be determined or reported on the certificate.
Melting analysis (heat / ladle analysis) — Table 1
| Element | TP304 (UNS S30400) melting analysis |
|---|---|
| Carbon (C) | ≤ 0.08 |
| Manganese (Mn) | ≤ 2.00 |
| Phosphorus (P) | ≤ 0.045 |
| Sulfur (S) | ≤ 0.030 |
| Silicon (Si) | ≤ 1.00 |
| Chromium (Cr) | 18.0 – 20.0 |
| Nickel (Ni) | 8.0 – 11.0 |
| Molybdenum (Mo) | … (no requirement) |
| Nitrogen (N) | … (no requirement) |
Source: ASTM A213/A213M Table 1 for Grade TP304 / UNS S30400 (public mill / specification summaries cross-checked). Confirm the ordered edition on the purchase order before treating any secondary catalogue as the acceptance text.
Product analysis — A480/A480M Table A1.1 tolerances applied to Table 1
| Element | Melting (Table 1) | Tolerance (A480 A1.1) | Product analysis limit |
|---|---|---|---|
| Carbon (C) | ≤ 0.08 | 0.01 over | ≤ 0.09 |
| Manganese (Mn) | ≤ 2.00 | 0.04 over | ≤ 2.04 |
| Phosphorus (P) | ≤ 0.045 | 0.010 over | ≤ 0.055 |
| Sulfur (S) | ≤ 0.030 | 0.005 over | ≤ 0.035 |
| Silicon (Si) | ≤ 1.00 | 0.05 over | ≤ 1.05 |
| Chromium (Cr) | 18.0 – 20.0 | 0.20 under / over | 17.80 – 20.20 |
| Nickel (Ni) | 8.0 – 11.0 | 0.10 under / 0.15 over | 7.90 – 11.15 |
The 18–20% chromium and 8–11% nickel balance makes TP304 the reference 18-8 austenitic tube grade: chromium builds the passive film and nickel keeps the structure fully austenitic after the 1900 °F [1040 °C] solution treatment. Carbon is capped at 0.08% on the melt; heats that also meet the TP304L carbon ceiling and overlapping nickel band can be dual-certified to A213 TP304L when both tensile floors and hardness limits are satisfied.
When product analysis is ordered, finished tube may read up to C 0.09%, Mn 2.04%, P 0.055%, S 0.035%, and Si 1.05%, with Cr 17.80–20.20% and Ni 7.90–11.15%. Those are the only product limits we quote from the A480 A1.1 path. Put any tighter project carbon or sulfur ceiling on the purchase order before the heat is selected.
Mechanical Properties of A213 TP304
ASTM A213 Table 4 sets the tensile acceptance floor for TP304 at 75 ksi [515 MPa] tensile strength and 30 ksi [205 MPa] yield strength (0.2% offset), with elongation of 35% minimum in 2 in. or 50 mm. Unlike many ASTM A312 pipe rows for the same UNS number, A213 Table 4 also lists a hardness maximum for TP304 of 192 HBW / 200 HV or 90 HRB, and hardness tests are part of the lot acceptance scheme in the product standard. Every lot sampled under the edition’s specimen rules must meet those numbers after the final solution treatment.
| Property | TP304 requirement (Table 4) |
|---|---|
| Tensile strength, min | 75 ksi [515 MPa] |
| Yield strength (0.2% offset), min | 30 ksi [205 MPa] |
| Elongation in 2 in. or 50 mm, min | 35% |
| Hardness, max | 192 HBW / 200 HV or 90 HRB |
Source: ASTM A213/A213M Table 4 for TP304 / UNS S30400 (public specification summaries). Mechanical property requirements do not apply to tubing smaller than 1/8 in. [3.2 mm] inside diameter or thinner than 0.015 in. [0.4 mm] wall. Flattening and flaring tests are also required on a lot basis for finished tube; they sit beside tension and hardness rather than replacing them.
Actual mill certificates often clear the 75/30 ksi floor with margin, but design calculations should still use Table 4 unless the purchase order states higher guaranteed values that the mill has accepted in writing. For creep-range boiler service that needs a controlled carbon floor and grain-size language, open A213 TP304H rather than stretching standard TP304 beyond its intended framing.
Dimensions and Tolerances
Dimensional supply for ASTM A213 TP304 is tube language — outside diameter × wall thickness (minimum wall or average wall) and, commercially, BWG / gauge — not ASME B36.19 pipe schedules as the primary size story. The sizes usually furnished under A213 run from about 1/8 in. [3.2 mm] inside diameter to 5 in. [127 mm] outside diameter, with minimum wall from about 0.015 to 0.500 in. [0.4 to 12.7 mm]; tubing with other diameters may be furnished when all other requirements of the specification are met. State on the purchase order whether wall is minimum or average, because that choice changes how the mill interprets tolerance and how the designer reads remaining wall after fabrication.
Outside-diameter and wall variations follow ASTM A1016/A1016M as invoked by A213, with cold-finished and hot-finished routes carrying different practical bands. Cold-finished tubes commonly hold tighter OD control; hot-finished tubes allow wider OD and wall windows. Permissible variations from a specified average wall for cold-finished tube are often summarized as ±10% of the specified average wall, while minimum-wall product is accepted to the A1016 minimum-wall tables rather than a symmetric ± window. Confirm the exact A1016 rows for the OD and finish route on the ordered edition — do not treat a catalogue one-liner as a substitute for the general-requirements table.
| Item | Typical A213 TP304 dimensional practice |
|---|---|
| Product form | Seamless only (cold-finished or hot-finished) |
| Usual size band | ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD; wall ~0.015–0.500 in. [0.4–12.7 mm] min (or average wall if PO says so) |
| Wall basis | Minimum wall (default commercial practice) or average wall when specified |
| OD / wall tolerances | Per ASTM A1016/A1016M for the finish route and size; cold-finished average wall often ±10% |
| Length | Cut lengths for HX / boiler bundles, or mill random lengths by agreement |
| Secondary size note | ASME B36.19 schedules may appear only when a buyer asks for a pipe-schedule cross-reference — not as the primary A213 size callout |
Put the cut list, U-bend or straight-tube preference, and end preparation on the enquiry so mill and stock lengths can be mixed efficiently. Minimum wall is a first-class A213 concept: if the datasheet assumes average wall, say so explicitly before the heat is rolled.
Equivalent Grades
Equivalence language around TP304 tube is often looser than a boiler or heat-exchanger purchase order can afford. ASTM A213 Grade TP304 / UNS S30400 is the governing designation for this article; EN 1.4301 and JIS SUS304 are approximate wrought names that point to similar chemistry families but are not automatic substitutes on an A213 mill test certificate. When a datasheet says “equivalent to 304,” confirm which product standard, tensile/hardness table, and heat-treatment clause the mill will actually certify.
| Designation | Notes |
|---|---|
| ASTM A213 / A213M Grade TP304 | Governing ASTM seamless boiler / HX tube product standard for this article |
| UNS S30400 | Unified number listed in Table 1 |
| ASME SA-213 TP304 | Separate ASME Code Book adoption of the A213 grade text — dual-mark only when the PO asks |
| EN 1.4301 (X5CrNi18-10) | Approximate wrought stainless designation; order EN tube forms under the relevant EN tube specs, not by EN number alone on an A213 MTC |
| JIS SUS304 | Approximate Japanese grade name; confirm the Japanese tube product standard when ordering JIS product |
| Related plate | A240 / SA240 flat product in the same UNS family — order plate and tube under their own product standards |
ASME SA-213 TP304 is the separate Code Book adoption of the same grade text; dual A213/SA-213 marking is a purchase-order option, not a claim that the two standards are one document. Compare low-carbon, H-grade, and molybdenum sisters on their own ASTM A213 pages before swapping grades in a tube bundle.
Heat Treatment and Delivery Condition
TP304 under ASTM A213 is furnished solution treated at a minimum of 1900 °F [1040 °C], then quenched in water or cooled rapidly by other means at a rate sufficient to prevent carbide reprecipitation. That heat-treatment row applies to both cold-finished and hot-finished seamless tube. Skipping or under-cooling the solution treatment can leave a structure that sensitizes in service even when ladle chemistry looked acceptable on paper.
Cold-finished versus hot-finished is a process and dimensional route, not a substitute for the anneal: cold-finished tube is typically drawn after hot working and then solution treated; hot-finished tube may be quenched after hot forming when the edition allows and finishing temperature is not below the minimum anneal. Delivery condition for SHH STEEL TP304 is solution annealed and pickled (or bright annealed by agreement), with heat-treatment temperature and quench method stated on the EN 10204 3.1 certificate. Straightening, cutting, and end finishing follow heat treatment.
When Supplementary Requirement language for intergranular-corrosion capability (commonly tied to ASTM A262 Practice E on sensitized or as-shipped specimens, depending on grade type) is ordered, the corrosion test report travels with the heat-treatment record. H-grade grain-size rules do not rewrite the TP304 path — use A213 TP304H when the datasheet calls for H-grade carbon and grain-size controls.
Corrosion Resistance
TP304’s chromium-rich passive film handles a wide band of oxidizing process fluids, clean steam-side and water-side duties, and many organic media that do not lean heavily on chlorides. In chloride-bearing waters, coastal cooling circuits, and many brine-leaning heat-exchanger services, pitting and crevice attack become limiting, and buyers usually step up to A213 TP316 or A213 TP316L. Intergranular corrosion risk after tube-to-tubesheet welding or after sensitizing thermal cycles is controlled by ordering A213 TP304L, by solution treating after fabrication when the sequence allows, or by invoking the contractual corrosion test on the tube PO.
ASTM A213 itself does not publish a corrosion-rate table for TP304; selection remains engineering judgment against fluid, temperature, velocity, and inspection philosophy inside the boiler or exchanger. When a specification calls for ASTM A262 Practice E, write that Supplementary Requirement onto the purchase order so the test is contractual rather than assumed from a verbal “full certs” note. SHH STEEL will not rank TP304 as equal to 316 in chlorides — that claim is not supported by the product standard.
Applications of A213 TP304 Tube
Because TP304 is the default austenitic seamless tube grade in so many boiler, superheater, and heat-exchanger specifications, it shows up across power-plant and industrial steam systems, process heat exchangers, condensers, and general corrosive tube duty where molybdenum is not required. The table below pairs typical application areas with a selection note so the grade is chosen for the fluid, temperature, and fabrication route — not only for the familiar “304” name on the BOM.
| Application area | Typical use of TP304 tube | Selection note |
|---|---|---|
| Boiler and superheater | Seamless generating-bank, screen, and moderate-temperature steam tubing ordered to A213 | For creep-critical H-grade service open TP304H; confirm design metal temperature |
| Heat exchangers / condensers | Straight and U-bend HX tubes in process and utility exchangers | State min vs average wall, BWG, and bend radius on the enquiry |
| Chemical and process | Tube-side or shell-side circuits with oxidizing or mild corrosive media | Prefer TP316/TP316L if chlorides dominate |
| Food / pharmaceutical utilities | Utility and process HX where 304 stainless tube is accepted | Follow hygiene finish and welding procedure requirements |
| Cryogenic / low-temperature HX | Austenitic toughness in cold-box and LNG-related exchangers | Confirm low-temperature code acceptance for the grade |
| General corrosive tube duty | Seamless tube where A213 documentation is preferred over pipe product forms | Do not substitute A312 pipe paperwork for A213 tube acceptance |
For as-welded tube-to-tubesheet joints in sensitizing service consider TP304L or dual TP304/TP304L; for high-temperature creep-range boiler tubing open TP304H; for chloride-rich cooling water move to the molybdenum grades on the same A213/A213M hub.
Weldability
TP304 tube welds readily with matching or near-matching austenitic filler for tube-to-tubesheet joints, attachment welds, and fabrication joins. Common practice uses ER308 / ER308L (or equivalent covered electrodes) under a qualified WPS; many exchanger fabricators prefer ER308L deposits for lower carbon in the weld metal even when the base tube is standard TP304. Heat input control, interpass limits, and post-weld cleaning remain the fabricator’s responsibility under the applicable boiler or pressure-vessel code — A213 governs the seamless tube product, not the field or shop weld procedure.
Because A213 TP304 is seamless, there is no mill longitudinal weld to radiograph the way welded pipe standards describe. Focus inspection language on tube integrity (hydro or NDE of each length), tube-to-tubesheet joint quality, and any contractual corrosion test on the base metal. For tube that will enter service as-welded in a sensitizing environment, many owners change the base metal to A213 TP304L rather than relying on a perfect weld procedure alone to protect standard-carbon TP304. Specify end preparation and surface finish on the tube PO when orbital or clean-service joins are planned.
Surface Finishes
Standard mill delivery for ASTM A213 TP304 is solution annealed and pickled, leaving a clean matte finish suitable for most boiler and heat-exchanger tube duty. Bright annealing under protective atmosphere produces a smoother reflective surface used on some clean-process and instrumentation tube lines and must be called out because it changes the heat-treatment route. Light polish or specified Ra on the bore or OD is a commercial or service-center operation on top of A213 product, not automatic with the grade stamp.
When a hygienic or fouling-sensitive exchanger specification quotes an Ra maximum on the bore, put it on the tube purchase order with its own acceptance language and sampling plan. SHH STEEL stencils grade and heat treatment as standard requirements; polish, special OD grind, and passivation after fabrication remain commercial extras unless the contract says otherwise. End preparation (plain, slightly beveled, or as needed for tube expanding) should be ordered together with finish so receiving inspection shares one acceptance language.
Inspection and Testing
Base ASTM A213 testing for TP304 includes heat analysis, tension tests to the Table 4 floors, hardness tests to the Table 4 maximum, flattening and flaring tests on a lot basis, and either hydrostatic testing or nondestructive electric testing of each length. The manufacturer may choose hydro versus NDE unless the purchase order fixes the method; both are acceptance routes inside the product standard, not informal upgrades. Marking includes the ASTM designation, grade, size, heat number, and other clause-required data so receiving inspection can tie each length back to the MTC.
Supplementary Requirements commonly added on TP304 tube orders are summarized below. Invoke them by number or clear purchase-order wording; mills will not assume product analysis or intergranular-corrosion testing from a verbal “full certs” note.
| Option | Purpose |
|---|---|
| Product analysis | Confirms chemistry on finished tube (via A1016 / PO language) |
| Intergranular corrosion | A262 Practice E (or agreed practice) as a contractual Supplementary Requirement |
| Minimum vs average wall | States which wall basis the size callout uses |
| Fixed hydro or NDE method | Removes manufacturer’s option when the end user mandates one route |
| Third-party inspection / EN 10204 3.2 | Witnessed testing and certificate when the project requires it |
Lot definitions for continuous heat treatment or direct quench after hot forming follow the size-based lot sizes in A213; ask the mill to state lot identity clearly on the certificate so hardness and tension specimens map cleanly to the bundle you receive.
Packaging and Shipping
TP304 tube leaves SHH STEEL bundled, capped or end-protected, and tagged for export or domestic delivery according to the length mix and bend form on the order. Bundle tags repeat the ASTM A213 grade, OD × wall (or BWG), heat number, and PO reference so site receiving can check the shipment without opening every certificate packet first. U-bent tubes need extra cradle or case protection so bend radii and legs are not distorted in transit.
Export packing can be bare bundles, wrapped bundles, or wooden-cased lengths for bright-annealed, polished, or small-bore material. We ship under the Incoterms on the order acknowledgement — FOB, CFR, CIF, EXW, or other agreed terms. Inland trucking, bilingual destination marks, or project color coding for bundle tags should be stated on the enquiry beside the metallurgical notes.
Why Choose SHH STEEL
SHH STEEL treats ASTM A213 TP304 as a product standard with enforceable chemistry, tensile, hardness, heat-treatment, and marking rules — not as a catalogue nickname for “any 304 tube.” The MTC reports the full Table 1 ladle chemistry and the Table 4 tensile/hardness set; the stencil carries seamless tube identity under A213; and dual A213/SA-213 marking is offered only when requested so Code and non-Code jobs stay cleanly documented.
We keep the 304-family conversation honest for boiler and HX duty. If tube-to-tubesheet joints will run as-welded in a sensitizing environment, we steer toward A213 TP304L or dual TP304/TP304L. If creep-range boiler service needs H-grade carbon and grain-size controls, we open A213 TP304H. If chlorides dominate the cooling water or process fluid, we open A213 TP316 / A213 TP316L. The A213/A213M hub is organized the same way — grade by grade under ASTM, seamless tube only.
Lead times combine near-term stock lengths with mill schedules; we say which is which on the quotation. Cut-to-length, U-bending, polish, and third-party inspection are defined extras. The tube that arrives should match the ASTM callout the engineer wrote, with paperwork a third-party inspector can read without translation.
Supply Capability
SHH STEEL can supply ASTM A213 TP304 stainless steel tube against the edition and finish route named on your enquiry. The capability table below summarizes the sizes, finishes, and documents we regularly quote for this grade, followed by the Stock / Available sizes map buyers ask for when they need a quick sense of what to enquire against for boiler and heat-exchanger duty.
| Item | SHH STEEL capability for TP304 |
|---|---|
| Standard | ASTM A213 / A213M (dual SA-213 marking on request) Grade TP304 / UNS S30400 |
| Product form | Seamless only — cold-finished and hot-finished |
| Size | Typical OD × min wall (or average wall) in the A213 usual band; other diameters by agreement |
| Wall / gauge | Minimum wall or average wall; BWG / gauge callouts accepted on enquiry |
| Length | Cut-to-length for HX / boiler bundles; mill random by agreement; U-bends on enquiry |
| Finish | Annealed and pickled; bright annealed or light polish by agreement |
| Testing | Tension (75/30 ksi), hardness (max 192 HBW / 90 HRB), flattening, flaring, hydro or NDE per length; full Table 1 chemistry on MTC; product analysis / IGC on order |
| Documents | EN 10204 3.1 with full Table 1 chemistry; third-party inspection / 3.2 on request |
| Trade terms | FOB / CFR / CIF / EXW and other agreed Incoterms |
Stock / Available sizes
SHH STEEL quotes TP304 tube against a practical stock-and-mill enquiry range rather than a frozen warehouse SKU list. The sizes below are the OD × wall / BWG combinations buyers most often request for boiler and heat-exchanger tube; availability of any single line on a given week depends on mill drawing and our inbound schedule, so treat the table as a supply map for enquiry — not a guarantee that every line sits on the floor with a published tonnage.
| Item | Typical stock / enquiry range for TP304 |
|---|---|
| Outside diameter | 12.7, 15.88, 19.05, 25.4, 31.8, 38.1, 50.8, 63.5, 76.2 mm (and other HX/boiler ODs on enquiry; up through the usual A213 ~5 in. [127 mm] band) |
| Wall / BWG | BWG 10–20 class walls and metric min-wall equivalents; lighter and heavier walls by agreement |
| Common OD × wall examples | 19.05 × 1.65 mm; 19.05 × 2.11 mm; 25.4 × 2.11 mm; 25.4 × 2.77 mm; 31.8 × 2.77 mm; 38.1 × 2.77 mm; 50.8 × 2.77 mm — illustrative HX/boiler sizes, confirm min vs average wall |
| Length | Cut lengths for exchanger bundles; U-bends and straight random lengths on enquiry |
| Special | Non-standard OD/wall, bright anneal, polished bore, and dual A213/SA-213 marking — confirm on enquiry before the heat is reserved |
When you send an enquiry, list OD × wall (or BWG), wall basis (minimum or average), cold-finished or hot-finished preference, quantity or cut list, required marking (A213 alone or dual A213/SA-213), and any Supplementary Requirements. We reply with what we can ship from near-term stock versus what needs a mill run, without inventing fake warehouse codes or tonnage claims.
Send the size list, finish route, quantity or cut lengths, required marking (A213 or dual A213/SA-213), Supplementary Requirements, and destination on one enquiry. We will confirm chemistry, tensile, and hardness against Table 1 and Table 4, state what ships from near-term availability versus mill production, and keep the offer aligned with the ASTM A213 / A213M product standard that governs this page. Related grades such as A213 TP321, A213 TP347H, and A213 UNS S30432 sit on the same hub when the datasheet steps beyond standard TP304.
FAQ
-
Is ASTM A213 the same as ASME SA-213 for TP304?
- No. ASTM A213 / A213M is the ASTM International product specification for seamless boiler, superheater, and heat-exchanger tubes; ASME SA-213 / SA-213M is the separate ASME Code Book adoption of that grade text. Chemistry, tensile, and hardness floors align closely for a given referenced edition, but they remain two independent standards. Dual-mark A213/SA-213 tube only when the purchase order asks for both names on the stencil and MTC.
-
Does ASTM A213 TP304 include welded or HCW tube?
- No. ASTM A213 covers seamless tube only. There is no WLD or HCW manufacturing type under this product standard the way ASTM A312 describes pipe. The process choice for TP304 under A213 is cold-finished versus hot-finished seamless tube, plus the heat-treatment and testing clauses of the ordered edition. If you need welded stainless pipe, that is a different product standard and a different steelspecs page family.
-
Minimum wall vs average wall — which should I order for A213 TP304?
- Order minimum wall when the design and datasheet are written around a guaranteed minimum thickness after tolerance. Order average wall only when the purchase order explicitly allows average-wall product and the designer has accepted that basis. The two readings produce different tube from the same OD × wall line, so put the wall basis on the enquiry before the mill selects tooling and tolerance tables from A1016.
-
Hydrostatic test vs NDE — which do I get on TP304 tube?
- ASTM A213 requires each tube to be hydrostatically tested or nondestructively electrically tested. The manufacturer may choose the method unless the purchase order fixes one. Neither route is an informal upgrade over the other inside the product standard. State the preferred method on the enquiry if your end user or inspector mandates hydro only or a named NDE technique.
-
Does A213 Table 4 set a hardness limit for TP304?
- Yes. Table 4 for TP304 lists tensile strength, yield strength, elongation, and a hardness maximum of 192 HBW / 200 HV or 90 HRB. Hardness tests are part of lot acceptance under A213, which differs from many A312 pipe rows for the same UNS number that omit a Table 4 hardness cap. If a project needs a tighter hardness window than Table 4, write it into the purchase order as an additional requirement.
-
What is the UNS number and chemistry of ASTM A213 TP304?
- TP304 is UNS S30400. Table 1 melting limits include carbon ≤0.08%, manganese ≤2.00%, phosphorus ≤0.045%, sulfur ≤0.030%, silicon ≤1.00%, chromium 18.0–20.0%, and nickel 8.0–11.0%, with molybdenum and nitrogen as no-requirement ellipses. Product-analysis limits apply only when ordered, typically from A480 Table A1.1 tolerances via the A1016 general-requirements path.
-
TP304 vs TP304L — which A213 tube should I order?
- Order TP304 when the specification calls for the standard 75/30 ksi tensile floor, 192 HBW / 90 HRB hardness maximum, and carbon ≤0.08% is acceptable. Order TP304L when as-welded intergranular resistance is the driver and the lower 70/25 ksi floor is acceptable. Dual TP304/TP304L certification is possible on qualifying heats — ask for it on the PO rather than assuming it from a PMI gun reading.
-
TP304 vs TP304H — when do I need the H grade under A213?
- Order TP304H when the boiler or superheater datasheet needs the H-grade carbon range, grain-size controls, and creep-rupture framing that the H designation carries under A213. Standard TP304 remains appropriate for many moderate-temperature HX and general corrosive tube duties. Do not treat "304H" as a synonym stamp for ordinary TP304 on the MTC.
-
TP304 vs TP316 — which A213 grade is better in chlorides?
- TP316 / TP316L adds molybdenum and generally resists chloride pitting and crevice corrosion better than TP304 in seawater-leaning cooling water, brines, and many process exchangers. TP304 remains appropriate for many oxidizing and low-chloride steam and process services. ASTM A213 does not publish a chloride ranking table; open the TP316 tube pages on the hub when chlorides dominate.
-
What heat treatment does ASTM A213 require for TP304?
- TP304 is solution treated at a minimum of 1900 °F [1040 °C] and then water quenched or rapidly cooled to prevent carbide reprecipitation. Both cold-finished and hot-finished seamless tube follow that heat-treatment requirement. Ask the mill to state anneal temperature and quench method on the EN 10204 3.1 certificate so receiving inspection can clear the heat without chasing verbal confirmations.
-
Can you dual-certify ASTM A213 and ASME SA-213 TP304, or TP304/TP304L?
- Yes on both axes when the heat and testing support it. Dual A213/SA-213 marking is available when the purchase order requests both independent standards on the stencil and MTC. Dual TP304/TP304L is available when ladle chemistry meets the tighter carbon rules and tensile plus hardness results clear both Table 4 rows. Spell the required marking on the enquiry so the heat is selected correctly.
Conclusion
ASTM A213 TP304 / UNS S30400 remains the reference 18-8 seamless stainless steel tube grade for boiler, superheater, and heat-exchanger service when molybdenum is not required and standard carbon is acceptable. SHH STEEL supplies cold-finished and hot-finished seamless tube in the usual OD × wall / BWG band, solution annealed, tested to Table 4 tensile and hardness limits, and documented on EN 10204 3.1 certificates — with dual SA-213 marking only when the order asks for that separate ASME standard. For sister grades and stock-oriented size discussions, start from the A213/A213M hub, then send your OD × wall list, wall basis, and marking requirements so we can align mill and near-term availability to the ASTM callout.
Contact: admin@steelspecs.com