ASME SA213 TP347 Stainless Steel Tube | ASME SA213 Stainless Steel - SHH STEEL

ASME SA213 TP347 Stainless Steel Tube

ASME SA213 TP347 / UNS S34700 niobium-stabilized seamless boiler, superheater and heat-exchanger tube — C ≤0.08%, Cr 17.0–20.0%, Ni 9.0–13.0%, Nb ≥10×C ≤1.10%, no Mo requirement, Table 4 75/30 ksi with elongation 35% min, hardness max 192 HBW / 90 HRB, 1900 °F solution anneal (Footnotes F, H). SHH STEEL supplies cold-finished and hot-finished seamless tube with EN 10204 3.1 MTCs that report the niobium formula result.
Grade
TP347 / UNS S34700
Standard
ASME SA213 / SA213M
Product form
Seamless boiler / superheater / heat-exchanger tube (cold-finished and hot-finished)
Size
Typical OD × min wall (or average wall) within ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD and ~0.015–0.500 in. [0.4–12.7 mm] wall; other diameters by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is ASME SA213 TP347 Stainless Steel Tube

ASME SA-213 / SA-213M is the ASME Boiler and Pressure Vessel Code Book adoption of the seamless ferritic and austenitic alloy-steel boiler, superheater, and heat-exchanger tube product text. When Code-stamped boilers, superheaters, or heat exchangers invoke that adoption by name, SA-213 is the governing product standard for this niobium-stabilized 18-8 tube — written as its own Code Book line, not as a merged synonym of ASTM A213. Begin from SA213/SA213M when the enquiry is Code-led.

Grade TP347 / UNS S34700 is the niobium-stabilized austenitic row inside that stainless family. Melting carbon is capped at 0.08%, chromium sits at 17.0–20.0%, nickel at 9.0–13.0%, and niobium must satisfy ≥10 × C with a 1.10% ceiling — molybdenum has no requirement on this row. Table 4 sets tensile at 75 ksi [515 MPa] / 30 ksi [205 MPa] with elongation 35% minimum and hardness max 192 HBW / 90 HRB. Buyers who write “347 HX tube” on a bill of materials still need to name SA-213 on the purchase order so the mill applies the tube product standard, minimum-wall rules, and the niobium formula together. This is not a dual stamp of TP304L, TP321, or TP347H.

SHH STEEL can supply ASME SA213 TP347 as seamless cold-finished and hot-finished tube in the usual OD × wall / BWG band, with EN 10204 3.1 certificates that report the niobium formula result together with the 75/30 ksi tensile set, 35% elongation, and hardness. Dual SA-213/A213 marking is added only when the purchase order asks; the live twin is A213 TP347.

Shop names include “347,” “S34700,” “Nb-stabilized 18-8 tube,” and older “columbium-stabilized” wording. Helpful for routing; the purchase order should still carry ASME SA-213 Grade TP347 / UNS S34700, wall basis, OD × wall or BWG, finish route, and any Supplementary Requirements (S1 / S2 when needed). Sister SA213 pages include SA213 TP347H, SA213 TP347HFG, SA213 TP347LN, and SA213 TP321. Seamless only — no Manufacturing Types (SML / WLD / HCW) H2 on this product page.

Chemical Composition of SA213 TP347

Two chemistry layers matter for TP347 under ASME SA-213. Melting analysis is mandatory for every heat; product analysis on finished tube applies only when Supplementary Requirement wording or the purchase order invokes it through the general requirements (commonly ASTM A1016/A1016M), with tolerances typically from ASTM A480/A480M Table A1.1. The defining line for a reviewer is niobium ≥10 × C with a 1.10% ceiling — not a low-carbon max alone, and not a titanium addition. A heat with 0.06% carbon needs at least 0.60% Nb, while a leaner-carbon heat can clear the formula with less niobium, still capped at 1.10%. Chromium 17.0–20.0% and nickel 9.0–13.0% sit near the 18-8 family but are wider than TP304’s classic windows and different from TP321’s 17–19 / 9–12 windows.

The tables below reproduce the melt limits for TP347 / UNS S34700, the product-analysis limits from A480 Table A1.1 practice, and a short stabilizer snapshot against TP304L, TP321, and TP347H. Later SA-213 / A213 editions place austenitic stainless grades in Table 2 (older editions used Table 1); confirm the ordered edition on the purchase order.

Melting analysis (heat / ladle analysis)

Element TP347 (UNS S34700) melting analysis
Carbon (C) ≤ 0.08
Manganese (Mn) ≤ 2.00
Phosphorus (P) ≤ 0.045
Sulfur (S) ≤ 0.030
Silicon (Si) ≤ 1.00
Chromium (Cr) 17.0 – 20.0
Nickel (Ni) 9.0 – 13.0
Molybdenum (Mo) … (no requirement)
Nitrogen (N) … (no requirement)
Niobium (Nb / Cb) ≥ 10 × C, ≤ 1.10
Titanium (Ti) … (no requirement)

Source: public SA-213 / A213 stainless chemistry table for Grade TP347 / UNS S34700 (same grade text family). Confirm the ordered edition. Where ellipses appear, the ordered edition sets no requirement for that element. Older shop language still says “columbium”; modern MTCs usually print Nb. UNCERTAIN: exact edition year and stainless chem table number on the ordered Code Book text.

Product analysis — A480/A480M Table A1.1 tolerances applied

Element Melting Tolerance (A480 A1.1) Product analysis limit
Carbon (C) ≤ 0.08 0.01 over ≤ 0.09
Manganese (Mn) ≤ 2.00 0.04 over ≤ 2.04
Phosphorus (P) ≤ 0.045 0.010 over ≤ 0.055
Sulfur (S) ≤ 0.030 0.005 over ≤ 0.035
Silicon (Si) ≤ 1.00 0.05 over ≤ 1.05
Chromium (Cr) 17.0 – 20.0 0.20 under / over 16.80 – 20.20
Nickel (Ni) 9.0 – 13.0 0.15 under / 0.20 over 8.85 – 13.20
Niobium (Nb) ≥ 10 × C, ≤ 1.10 0.05 over on max (Nb formula practice) max ≤ 1.15 product; min tied to heat C

UNCERTAIN: A480 Nb product-tolerance digits on the formula max and the Ni 9–13 band practice — confirm against the ordered A480 edition when product analysis is invoked. Footnotes F/H and S1/S2 full negotiated A262 / stabilization wording — confirm ordered edition.

Stabilizer snapshot — TP304L / TP321 / TP347 / TP347H

Element TP304L (S30403) TP321 (S32100) TP347 (S34700) TP347H (S34709)
C ≤ 0.035 ≤ 0.08 ≤ 0.08 0.04 – 0.10
Cr 18.0 – 20.0 17.0 – 19.0 17.0 – 20.0 17.0 – 19.0
Ni 8.0 – 12.0 9.0 – 12.0 9.0 – 13.0 9.0 – 13.0
Stabilizer / C path low C (no Ti/Nb) Ti ≥ 5 × (C+N), ≤ 0.70 Nb ≥ 10 × C, ≤ 1.10 Nb ≥ 8 × C, ≤ 1.10

Heats that also meet an H-grade carbon floor while clearing the TP347 carbon ceiling, the tighter H-grade Nb formula (8 × C), tensile, hardness, and grain-size paths can be dual-certified TP347/TP347H when the purchase order asks — do not assume it from a PMI gun. Dual TP347/TP321 is not a chemistry path: one grade requires niobium, the other titanium. Versus SA213 TP304L, TP347 accepts higher carbon because niobium, not an L-grade carbon ceiling, is the IGC strategy. Compare SA213 TP321 and SA213 TP347H before swapping on a familiar “347” PMI reading alone.

Mechanical Properties of SA213 TP347

ASME SA-213 Table 4 sets the tensile acceptance floor for TP347 / UNS S34700 at 75 ksi [515 MPa] tensile strength and 30 ksi [205 MPa] yield strength (0.2% offset), with elongation of 35% minimum in 2 in. or 50 mm and hardness max 192 HBW / 200 HV or 90 HRB. That is the same room-temperature pair as TP321 and TP304 — niobium stabilization does not raise the room-temperature tensile floor; it changes sensitization framing and the chemistry check on the MTC. The public heat-treatment table does not print a mandatory ASTM grain-size number for TP347 (unlike TP347H’s “7” and TP347HFG’s “7–10”), so a tensile-and-hardness MTC without grain size can still be complete for non-H TP347 unless the purchase order adds a grain-size Supplementary Requirement.

Property TP347 requirement (Table 4)
Tensile strength, min 75 ksi [515 MPa]
Yield strength (0.2% offset), min 30 ksi [205 MPa]
Elongation in 2 in. or 50 mm, min 35%
Hardness, max 192 HBW / 200 HV or 90 HRB
Grain size No mandatory ASTM number in the public Table 3 row (confirm ordered edition)

Source: public SA-213 / A213 Table 4 for UNS S34700 / TP347. Mechanical property requirements do not apply to tubing smaller than 1/8 in. [3.2 mm] inside diameter or thinner than 0.015 in. [0.4 mm] wall. Flattening and flaring tests are also required on a lot basis. A tensile-only MTC that omits the niobium formula result is incomplete for TP347. For H-grade carbon floor and grain-size control, open SA213 TP347H; for fine-grain creep framing open SA213 TP347HFG.

Dimensions and Tolerances

Dimensional supply for ASME SA213 TP347 is tube language — outside diameter × wall thickness (minimum wall or average wall) and, commercially, BWG / gauge — not ASME B36.19 pipe schedules as the primary size story. Usual SA-213 sizes run from about 1/8 in. [3.2 mm] inside diameter to 5 in. [127 mm] outside diameter, with minimum wall from about 0.015 to 0.500 in. [0.4 to 12.7 mm]; other diameters may be furnished when all other requirements are met.

Boiler and heat-exchanger datasheets that pick niobium-stabilized tube usually assume minimum wall — state wall basis on the purchase order. Outside-diameter and wall variations follow the general requirements invoked by SA-213 (commonly ASTM A1016/A1016M). Niobium chemistry does not change the dimensional tolerance tables; it changes which heat clears the grade stamp.

Item Typical SA213 TP347 dimensional practice
Product form Seamless only (cold-finished or hot-finished)
Usual size band ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD; wall ~0.015–0.500 in. [0.4–12.7 mm]
Wall basis Minimum wall (common for HX / boiler datasheets) or average wall if PO says so
OD / wall tolerance Per general requirements (commonly A1016/A1016M) for the ordered finish
Length Straight random / cut-to-length; U-bend by agreement

BWG / gauge callouts are accepted on enquiry; certificates should still show OD and wall in inch or millimetre units. U-bends and polished ID finishes are commercial options — they do not replace the niobium formula check.

Equivalent Grades

Equivalence language around 347 tube often treats it as “304 with niobium” or collapses it with 347H. ASME SA-213 Grade TP347 / UNS S34700 is the governing designation for this article; EN 1.4550 / X6CrNiNb18-10 and JIS SUS347 / SUS347TB are approximate wrought names that point to similar niobium-stabilized 18-8 families but are not automatic substitutes on an SA-213 mill test certificate.

Designation Notes
ASME SA-213 / SA-213M Grade TP347 Governing ASME Code Book seamless boiler / HX tube product standard for this article
UNS S34700 Unified number in the stainless chemistry table
ASTM A213 TP347 Separate ASTM product specification — twin page A213 TP347; dual-mark only when the PO asks
EN 1.4550 (X6CrNiNb18-10) Approximate wrought Nb-stabilized designation; order EN tube forms under the relevant EN tube specs
JIS SUS347 / SUS347TB Approximate Japanese grade / boiler-tube names; confirm the Japanese tube product standard
Related H / HFG / LN SA213 TP347H, SA213 TP347HFG, SA213 TP347LN
Related Ti-stabilized SA213 TP321 — titanium, not niobium
Related plate A240 / SA240 flat product in the same UNS family

Dual SA-213/A213 marking is a purchase-order option. Compare TP347H before swapping non-H 347 tube into a creep-range H-grade list.

Heat Treatment and Delivery Condition

TP347 under ASME SA-213 is furnished solution treated at a minimum of 1900 °F [1040 °C], then quenched in water or cooled rapidly by other means. Public heat-treatment language for this grade references Footnotes F and H on quench / subsequent exposure paths — confirm the full footnote text in the ordered edition. Footnote F ties quench capability to A262 Practice E demonstrability when that test is ordered (Supplementary Requirement S4); Footnote H warns that a solution treating temperature above 1950 °F [1065 °C] may impair intergranular-corrosion resistance after subsequent sensitizing exposure, and allows a purchaser-specified lower-temperature stabilization or resolution anneal after the higher solution anneal. The public table does not print a mandatory ASTM grain-size number for TP347.

Supplementary Requirement S2 lists TP347 among grades that shall be given a stabilization heat treatment at a temperature lower than the initial solution anneal when the purchaser specifies S2 — temperature as agreed between purchaser and vendor. Supplementary Requirement S1 allows stress-relieved annealed TP347 (1500–1650 °F [815–900 °C] after roll straightening) for certain chloride stress-corrosion services when ordered. Neither S1 nor S2 is automatic with the grade stamp.

Cold-finished versus hot-finished is a process and dimensional route, not a substitute for the anneal. Delivery condition for SHH STEEL TP347 is solution annealed and pickled (or bright annealed by agreement), with anneal temperature, quench method, and niobium result on the EN 10204 3.1 certificate. For H-grade carbon and grain-size controls open SA213 TP347H; for fine-grain creep framing open SA213 TP347HFG. UNCERTAIN: S2 stabilizing hold full temperature/time wording and Footnotes F/H full negotiated A262 wording when ordered.

Corrosion Resistance

ASME SA213 TP347 is selected when niobium stabilization is preferred over low-carbon chemistry for resistance to intergranular attack after welding or exposure in the sensitizing range, while keeping a standard 18-8 austenitic alloy without molybdenum. The Nb ≥10 × C rule ties up carbon as niobium carbides/carbonitrides so chromium stays available for the passive film — a different lever from titanium on TP321 or from L-carbon on TP304L.

It is not a molybdenum grade and is not automatically better than TP304L in every chloride service — in many wet cooling-water lists, L-carbon or Mo-bearing grades remain the better match. Niobium stabilization also does not replace H-grade carbon floor and grain-size control for creep-range boiler duty; that path is SA213 TP347H or, for fine-grain packaging, SA213 TP347HFG.

SHH STEEL reports the niobium formula result on the 3.1 certificate so inspectors can verify stabilization rather than accepting a plain 304 heat stamped as 347 on an Nb PMI trace alone.

Applications of SA213 TP347 Tube

Typical ASME SA213 TP347 uses include Code-stamped heat-exchanger and condenser tubes where niobium stabilization is specified, process heaters that see intermittent sensitizing temperatures, and selected boiler / superheater services that name TP347 rather than the H grade. It is also quoted for replacement tube when original 347 MTCs must be matched on the niobium formula.

  • Heat-exchanger / condenser tubes naming Nb-stabilized 347
  • Process heaters with intermittent sensitizing exposure
  • Boiler / superheater tube when the datasheet names SA-213 TP347 (not H)
  • Replacement bundles matching original S34700 certificates

For creep-range H-grade duty with grain-size control, compare SA213 TP347H. For fine-grain cold-finished HFG, compare SA213 TP347HFG. For titanium stabilization, compare SA213 TP321. For ultra-low-C + N + Nb, compare SA213 TP347LN.

Weldability

TP347 welds with matching niobium-stabilized austenitic filler practices — commonly ER347 / E347 family wires selected to the project WPS. Niobium in the base metal supports as-welded intergranular framing; still follow qualified procedures for heat input, interpass, and purge on thin HX tube, and watch cleanliness that can deplete stabilization in the weld zone.

Autogenous orbital welds on thin-wall exchanger tube need purge discipline; Nb stabilization does not remove those controls. When S2 stabilization heat treatment is required after welding or mill anneal, put it on the purchase order — it is not automatic with the grade stamp.

Do not dual-stamp a TP304L or TP321 weld procedure as TP347 without reopening the niobium formula and filler selection on the WPS / PQR. Titanium-stabilized ER321 filler is not a substitute for ER347 on a niobium grade.

Surface Finishes

Standard mill delivery for ASME SA213 TP347 is solution annealed and pickled, leaving a clean matte finish suitable for boiler and heat-exchanger tube duty. Bright annealing is available by agreement when OD appearance or polish steps favor it.

ID/OD polish and U-bend conditioning are commercial additions — they do not replace the niobium formula check. End caps and dry export packaging matter more than paint on pickled stainless.

SHH STEEL notes the ordered surface route on the packing list and aligns it with the MTC finish description for receiving inspection.

Inspection and Testing

Base ASME SA-213 testing for TP347 includes heat analysis (C ≤0.08%, Cr 17.0–20.0%, Ni 9.0–13.0%, Nb ≥10 × C ≤1.10%), tension tests to the 75/30 ksi floors with 35% elongation, hardness to 192 HBW / 90 HRB, and flattening / flaring tests for the ordered size. Hydrostatic testing or NDE follows the path selected on the purchase order.

Certificate reviewers should confirm the niobium formula result rather than trusting a “304 family” PMI without Nb. Product analysis, when ordered, applies A480 tolerances including the Nb max window noted as UNCERTAIN digit confirmation above. S1 / S2 and A262 practices apply only when named on the PO.

EN 10204 3.1 is default; 3.2 when required. Dual SA-213/A213 names appear only when dual marking was ordered.

Packaging and Shipping

TP347 tube leaves SHH STEEL bundled, capped or end-protected, and tagged for export or domestic delivery according to length mix and bend form. Bundle tags repeat ASME SA-213 Grade TP347, UNS S34700, heat number, size, and wall basis so receivers can match the 3.1 certificate — including the niobium formula — without opening every bundle.

Export packing uses seaworthy bundling appropriate for pickled stainless. Marking follows SA-213 and any dual-mark text the PO adds, referencing A213 TP347 only when dual ASTM marking was ordered.

Why Choose SHH STEEL

SHH STEEL treats ASME SA213 TP347 as a Code Book niobium-stabilized product with enforceable C ≤0.08%, Cr 17–20%, Ni 9–13%, Nb ≥10 × C ≤1.10%, 75/30 ksi tensile, 35% elongation, hardness, and marking rules — not as “304 with a niobium trace” checked only by an Nb PMI peak. Enquiry review verifies the niobium formula before release.

That stops silent substitution with TP304, TP304L, or TP321 heats on datasheets that actually require S34700. We keep SA-213 and A213 independent, dual-mark only on request, and put Nb on the 3.1 certificate so inspectors can verify stabilization.

Cross-links: SA213 TP347H, SA213 TP347HFG, SA213 TP347LN, SA213 TP321, hub SA213/SA213M.

Supply Capability

SHH STEEL can supply ASME SA213 TP347 stainless steel tube against the edition and finish route named on your enquiry. The capability table below summarizes sizes, finishes, and documents we regularly quote, followed by the Stock / Available sizes map for niobium-stabilized boiler and heat-exchanger tube.

Item SHH STEEL capability for TP347
Standard ASME SA213 / SA213M (dual A213 marking on request)
Grade TP347 / UNS S34700
Product form Seamless only — cold-finished and hot-finished
Size Typical OD × min wall (or average wall) in the SA-213 usual band; other diameters by agreement
Wall / gauge Minimum wall or average wall; BWG / gauge callouts accepted on enquiry
Length Cut-to-length for boiler / HX bundles; U-bend by agreement
Documentation EN 10204 3.1 MTC with Nb formula result; S1 / S2 / A262 / witness on request
Trade terms FOB / CFR / CIF / EXW and other agreed Incoterms

Stock / Available sizes

SHH STEEL quotes TP347 against a stock-and-mill enquiry range rather than a frozen SKU or tonnage list. Representative OD × wall / BWG combinations below are an enquiry map for niobium-stabilized boiler and heat-exchanger tube — confirm live availability and cut lengths on the RFQ.

OD (in.) Typical wall / BWG enquiry band Notes
1/2 – 1 BWG 16–12 / ~0.065–0.109 in. Small HX / instrument sizes
1-1/4 – 2 BWG 14–10 / ~0.083–0.134 in. Common boiler / HX band
2-1/2 – 3 0.120 – 0.250 in. min wall Heavier HX / boiler wall
3-1/2 – 5 0.180 – 0.300 in. min wall Upper usual SA-213 OD by agreement

Send OD × wall (or BWG), wall basis (min or average), quantity, finish route, and whether dual A213 marking, S1 / S2, or A262 is required. We reply with available mill / stock options for ASME SA213 TP347 and the matching document set.

FAQ

Is ASME SA-213 the same as ASTM A213 for TP347?
No. ASME SA-213 / SA-213M is the ASME Code Book adoption; ASTM A213 / A213M is the separate ASTM product specification. Chemistry — including C ≤0.08%, Cr 17.0–20.0%, Ni 9.0–13.0%, and Nb ≥10 × C ≤1.10% — tensile 75/30 ksi, elongation 35%, and hardness floors align in the shared grade text family, but the standards remain independent documents. Dual marking is a purchase-order option, not proof that the two titles are one standard.
Does ASME SA213 TP347 include welded or HCW tube?
No. This SA213 product page covers seamless boiler, superheater, and heat-exchanger tube only. SA-213 for the austenitic grades discussed here is a seamless tube product form; welded (WLD) and hot-finished continuous-welded (HCW) manufacturing types are out of scope on this page. Order welded stainless tube under a different product standard when the datasheet truly needs welded product.
What is the UNS number and chemistry focus of ASME SA213 TP347?
UNS S34700. Check C ≤0.08%, Cr 17.0–20.0%, Ni 9.0–13.0%, and niobium ≥10 × C with a 1.10% ceiling. Molybdenum has no requirement on this row. A heat without enough niobium for the formula is not TP347 even when Cr/Ni look like 18-8. Older certificates may print “Cb” for columbium — modern MTCs usually print Nb.
TP347 vs TP304L — when do I need niobium instead of low carbon under SA213?
Order TP347 when the datasheet wants niobium stabilization (Nb ≥10 × C) rather than L-carbon chemistry for sensitizing-range or as-welded intergranular framing. Order TP304L when C ≤0.035% without a stabilizer is the named path. They are different levers — not dual stamps — and Cr/Ni windows also differ. Compare SA213 TP304L before swapping on a familiar 18-8 PMI reading alone.
TP347 vs TP321 — why choose Nb over Ti under SA213?
Both are stabilized 18-8 grades, but TP347 requires niobium ≥10 × C ≤1.10% while TP321 requires titanium ≥5 × (C + N) ≤0.70%. Cr/Ni windows also differ (347: 17–20 / 9–13; 321: 17–19 / 9–12). Dual TP347/TP321 is not a chemistry path. Order the stabilizer the datasheet names, and compare SA213 TP321 before swapping on a familiar “stabilized 18-8” PMI reading alone.
TP347 vs TP347H — when do I need the H grade under SA213?
Order TP347H when the datasheet needs carbon 0.04–0.10%, Nb ≥8 × C ≤1.10% (not the non-H 10 × C rule), finish-route solution temperatures (CF 2000 °F / HR 1925 °F), and ASTM grain size No. 7 or coarser for creep-range boiler / superheater duty. Order non-H TP347 when those H-grade controls are not named. Dual 347/347H is possible only when the heat clears both rows and the PO asks.
What do Footnotes F and H mean for TP347 heat treatment under SA213?
Public SA-213 / A213 heat-treatment language for TP347 references Footnotes F and H on quench and subsequent-exposure paths. Footnote F ties quench capability to A262 Practice E demonstrability when ordered; Footnote H warns about solution temperatures above 1950 °F [1065 °C] and allows a purchaser-specified lower-temperature stabilization after a higher anneal. Full negotiated wording is UNCERTAIN without the ordered edition — confirm before writing contractual A262 language.
What is Supplementary Requirement S2 for TP347 under SA213?
S2 requires a stabilization heat treatment at a temperature lower than the initial solution anneal when the purchaser specifies S2 — temperature as agreed between purchaser and vendor. S1 allows stress-relieved annealed delivery (1500–1650 °F) for certain chloride SCC services when ordered. Neither is automatic with the grade stamp; write S1 or S2 explicitly on the purchase order.
Does SA-213 set a hardness limit for TP347?
Yes. Table 4 caps hardness at 192 HBW / 200 HV or 90 HRB, with 75 ksi tensile, 30 ksi yield, and 35% elongation. Grade distinction versus TP304L or TP321 is the niobium formula (and Cr/Ni windows), not a different room-temperature tensile floor. A tensile-only MTC that omits Nb is incomplete for TP347.
Minimum wall vs average wall — which should I order for SA213 TP347?
Most boiler and heat-exchanger datasheets assume minimum wall; average wall only when the PO says so. Usual SA-213 sizes run about 1/8 in. ID to 5 in. OD with min wall about 0.015–0.500 in. State wall basis, OD × wall or BWG, and finish route on the RFQ so the mill applies the correct dimensional table.
Can you dual-certify ASME SA-213 and ASTM A213 TP347?
Yes, when the purchase order asks for dual marking and the heat meets both named editions — including C ≤0.08%, Cr 17–20%, Ni 9–13%, Nb ≥10 × C ≤1.10%, 75/30 ksi, and 35% elongation. Dual marking does not merge the standards into one document; it stencils both names on tube that already clears both. See also the twin page A213 TP347.
Is TP347 a good choice for chloride-rich cooling water under SA213?
Not automatically. Niobium stabilization addresses sensitizing-range intergranular framing; it does not add molybdenum for chloride pitting/crevice performance. Many wet cooling-water lists prefer L-carbon or Mo-bearing grades. Compare SA213 TP304L or Mo grades when chloride is the driver, and keep TP347 where Nb stabilization is the named requirement.

Conclusion

ASME SA213 TP347 / UNS S34700 is the niobium-stabilized seamless stainless steel tube grade for Code boiler, superheater, and heat-exchanger service when C ≤0.08%, Cr 17.0–20.0%, Ni 9.0–13.0%, Nb ≥10 × C ≤1.10%, a 75/30 ksi tensile floor with 35% elongation, hardness max 192 HBW / 90 HRB, and a 1900 °F solution anneal are required together. SHH STEEL supplies cold-finished and hot-finished seamless tube in the usual OD × wall / BWG band with EN 10204 3.1 MTCs that report the niobium formula result. For quotations and technical review, contact admin@steelspecs.com.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X