ASME SA213 TP XM-19 Stainless Steel Tube | ASME SA213 Stainless Steel - SHH STEEL

ASME SA213 TP XM-19 Stainless Steel Tube

ASME SA213 XM-19 / UNS S20910 (Nitronic 50) seamless boiler, superheater and heat-exchanger tube with Cr 20.5–23.5%, Ni 11.5–13.5%, Mo 1.50–3.00%, N 0.20–0.40%, Nb and V 0.10–0.30% each. Mechanical floor 100/55 ksi with hardness max 250 HBW / 25 HRC; solution anneal 1900 °F. SHH STEEL supplies cold-finished and hot-finished seamless tube with EN 10204 3.1 MTCs.
Grade
XM-19 / UNS S20910
Standard
ASME SA213 / SA213M
Product form
Seamless boiler / superheater / heat-exchanger tube (cold-finished and hot-finished)
Size
Typical OD × min wall (or average wall) within ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD and ~0.015–0.500 in. [0.4–12.7 mm] wall; other diameters by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is ASME SA213 TP XM-19 Stainless Steel Tube

ASME SA-213 / SA-213M is the ASME Boiler and Pressure Vessel Code Book adoption of the seamless ferritic and austenitic alloy-steel boiler, superheater, and heat-exchanger tube product standard. Grade XM-19 under that Code Book text is the nitrogen-strengthened austenitic listed as UNS S20910 — commercially known as Nitronic 50 — with melting limits of carbon ≤0.06%, chromium 20.5–23.5%, nickel 11.5–13.5%, molybdenum 1.50–3.00%, nitrogen 0.20–0.40%, and both niobium and vanadium at 0.10–0.30% each. When a Code-stamped boiler, superheater, or heat-exchanger datasheet calls for SA-213 XM-19, the purchase order and mill test certificate should carry the ASME designation and the 100/55 ksi tensile floor that belongs to this grade — not a borrowed 316 or 304 mechanical row.

SHH STEEL can supply ASME SA213 TP XM-19 stainless steel tube as seamless cold-finished and hot-finished product in the usual boiler and heat-exchanger OD × wall / BWG band, documented on EN 10204 3.1 mill test certificates that report the full ladle chemistry — including Mo, N, Nb, and V — and the tensile plus hardness acceptance set. Dual SA-213 / A213 marking on the same lengths is available only when the purchase order asks for both independent standards; ASME SA213 and ASTM A213 remain separate documents even when the grade text aligns closely for a referenced edition. Browse the grade family on the SA213/SA213M hub.

Commercially the same tube is still called XM-19, Nitronic 50, S20910 boiler tube, or SA213 XM19 HX tube; none of those phrases replace the ASME grade on the stencil or MTC. Sister grades under the same ASME standard include SA213 TP316 / SA213 TP316L, SA213 TP317 / SA213 TP317L, SA213 TP304N, and SA213 UNS S31254. SA-213 covers seamless tube only — there is no welded or HCW manufacturing type under this product standard — so cold-finished versus hot-finished seamless route is the process choice, not a WLD/HCW stencil letter. For the sister ASTM product page on the same UNS, see A213 TP XM-19.

Chemical Composition of SA213 XM-19

Two chemistry layers matter for XM-19 under ASME SA-213. The melting (heat or ladle) analysis is mandatory for every heat, while product analysis on finished tube applies only when Supplementary Requirement wording or the purchase order invokes product analysis through the general requirements path (commonly ASTM A1016/A1016M as referenced by the ordered SA-213 edition). Product-analysis tolerances typically flow from ASTM A480/A480M Table A1.1. SHH STEEL reports the actual ladle values — and the product values when ordered — and does not advertise unpublished tighter catalogue windows. Every controlled element on this grade (including Nb, V, Mo, and N) must appear on the certificate; an MTC that omits niobium or vanadium is incomplete for S20910.

The tables below reproduce the heat analysis for XM-19 / UNS S20910 and the product-analysis limits that result from applying A480 Table A1.1 tolerances. Values are maximum unless a range is shown. UNCERTAIN: exact SA-213 / A213 edition year and whether austenitic grades sit in Table 1 or Table 2 of that edition; A480 product-tolerance digits for Nb/V/Mo/N bands if product analysis is contractual; nitrogen analysis method by agreement — confirm the ordered edition on the purchase order before treating secondary catalogues as acceptance text.

Melting analysis (heat / ladle analysis)

Source: public SA-213 / A213 grade-table summaries for XM-19 / UNS S20910. Confirm the ordered ASME edition on the purchase order.

Element XM-19 (UNS S20910) melting analysis
Carbon (C) ≤ 0.06
Manganese (Mn) 4.0 – 6.0
Phosphorus (P) ≤ 0.045
Sulfur (S) ≤ 0.030
Silicon (Si) ≤ 1.00
Chromium (Cr) 20.5 – 23.5
Nickel (Ni) 11.5 – 13.5
Molybdenum (Mo) 1.50 – 3.00
Nitrogen (N) 0.20 – 0.40
Niobium (Nb) 0.10 – 0.30
Vanadium (V) 0.10 – 0.30

Product analysis — A480/A480M Table A1.1 tolerances applied

Element Melting Tolerance (A480 A1.1) Product analysis limit
Carbon (C) ≤ 0.06 0.01 over ≤ 0.07
Manganese (Mn) 4.0 – 6.0 0.05 under / over 3.95 – 6.05
Phosphorus (P) ≤ 0.045 0.010 over ≤ 0.055
Sulfur (S) ≤ 0.030 0.005 over ≤ 0.035
Silicon (Si) ≤ 1.00 0.05 over ≤ 1.05
Chromium (Cr) 20.5 – 23.5 0.25 under / over 20.25 – 23.75
Nickel (Ni) 11.5 – 13.5 0.15 under / over 11.35 – 13.65
Molybdenum (Mo) 1.50 – 3.00 0.05 under / 0.10 over 1.45 – 3.10
Niobium (Nb) 0.10 – 0.30 0.05 under / over 0.05 – 0.35
Nitrogen (N) 0.20 – 0.40 0.02 under / 0.04 over 0.18 – 0.44
Vanadium (V) 0.10 – 0.30 0.03 under / over 0.07 – 0.33

The combination of chromium above 20%, molybdenum in the 1.5–3% band, and nitrogen at 0.20–0.40% is why XM-19 sits well above standard 18-8 and even above many molybdenum grades on the SA-213 tensile table. Niobium and vanadium at 0.10–0.30% each are controlled additions that must be reported — they are not optional “trace” lines a mill can drop from the certificate. Carbon is held to ≤0.06%, tighter than TP304’s 0.08% ceiling, which helps keep the as-annealed structure clean for the high nitrogen load.

When product analysis is ordered, finished tube may read within the product-limit column above. Those are the only product limits we quote from the A480 A1.1 path for this grade. Put any tighter project nitrogen, molybdenum, or sulfur ceiling on the purchase order before the heat is selected, and agree the nitrogen analysis method in writing when N reporting must follow a named technique.

Mechanical Properties of SA213 XM-19

ASME SA-213 sets the tensile acceptance floor for XM-19 at 100 ksi [690 MPa] tensile strength and 55 ksi [380 MPa] yield strength (0.2% offset), with elongation of 35% minimum in 2 in. or 50 mm. That 100/55 ksi pair sits far above TP304’s 75/30 and TP316’s 75/30 rows and even above nitrogen-bearing TP304N’s 80/35 — a direct result of the Mo–N–Nb–V solid-solution and microalloy package the product standard captures in this row. The same mechanical table lists a hardness maximum of 250 HBW / 265 HV or 25 HRC, and hardness tests are part of the lot acceptance scheme. Every lot sampled under the edition’s specimen rules must meet those numbers after the final solution treatment.

Source: public SA-213 / A213 mechanical-table summaries for XM-19 / UNS S20910 (commonly Table 4). Mechanical property requirements do not apply to tubing smaller than 1/8 in. [3.2 mm] inside diameter or thinner than 0.015 in. [0.4 mm] wall.

Property XM-19 requirement
Tensile strength, min 100 ksi [690 MPa]
Yield strength (0.2% offset), min 55 ksi [380 MPa]
Elongation in 2 in. or 50 mm, min 35%
Hardness, max 250 HBW / 265 HV or 25 HRC

Flattening and flaring tests are also required on a lot basis for finished tube; they sit beside tension and hardness rather than replacing them. The high yield floor is why designers reach for XM-19 when wall thickness, design pressure, or vibration/fatigue margins are tight in a chloride-leaning exchanger — but only after fabrication and weld reviews clear the nitrogen-strengthened chemistry. Actual mill certificates often clear the 100/55 ksi floor with margin; design calculations should still use the Code Book floor unless the purchase order states higher guaranteed values that the mill has accepted in writing.

Dimensions and Tolerances

Dimensional supply for ASME SA213 XM-19 is tube language — outside diameter × wall thickness (minimum wall or average wall) and, commercially, BWG / gauge — not ASME B36.19 pipe schedules as the primary size story. The sizes usually furnished under SA-213 run from about 1/8 in. [3.2 mm] inside diameter to 5 in. [127 mm] outside diameter, with minimum wall from about 0.015 to 0.500 in. [0.4 to 12.7 mm]; tubing with other diameters may be furnished when all other requirements of the specification are met. State on the purchase order whether wall is minimum or average, because that choice changes how the mill interprets tolerance and how the designer reads remaining wall after fabrication.

Outside-diameter and wall variations follow the general requirements invoked by SA-213 (commonly ASTM A1016/A1016M), with cold-finished and hot-finished routes carrying different practical bands. Cold-finished tubes commonly hold tighter OD control; hot-finished tubes allow wider OD and wall windows. Permissible variations from a specified average wall for cold-finished tube are often summarized as ±10% of the specified average wall, while minimum-wall product is accepted to the minimum-wall tables rather than a symmetric ± window. Confirm the exact general-requirements rows for the OD and finish route on the ordered edition.

Item Typical SA213 XM-19 dimensional practice
Product form Seamless only (cold-finished or hot-finished)
Usual size band ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD; wall ~0.015–0.500 in. [0.4–12.7 mm] min (or average wall if PO says so)
Wall basis Minimum wall (default commercial practice) or average wall when specified
OD / wall tolerances Per general requirements for the finish route and size; cold-finished average wall often ±10%
Length Cut lengths for HX / boiler bundles, or mill random lengths by agreement
Secondary size note ASME B36.19 schedules may appear only when a buyer asks for a pipe-schedule cross-reference — not as the primary SA-213 size callout

Put the cut list, U-bend or straight-tube preference, and end preparation on the enquiry so mill and stock lengths can be mixed efficiently. Nitrogen-strengthened grades work-harden more than standard 18-8 during U-bending, so bend radius and any post-bend anneal should be discussed early. Minimum wall is a first-class SA-213 concept: if the datasheet assumes average wall, say so explicitly before the heat is rolled.

Equivalent Grades

Equivalence language around XM-19 tube is often looser than a Code or heat-exchanger purchase order can afford. ASME SA-213 Grade XM-19 / UNS S20910 is the governing designation for this article; Nitronic 50 is a commercial trademark name pointing to the same UNS family but is not itself a Code product standard. When a datasheet says “equivalent to Nitronic 50,” confirm which product standard, tensile/hardness table, and heat-treatment clause the mill will actually certify.

Designation Notes
ASME SA-213 / SA-213M Grade XM-19 Governing ASME Code Book seamless boiler / HX tube product standard for this article
UNS S20910 Unified number listed with the grade chemistry
ASTM A213 XM-19 Separate ASTM International product specification — dual-mark only when the PO asks; see A213 TP XM-19
Nitronic 50 Commercial trademark name for the S20910 family — not a substitute for the ASME grade on the MTC
EN / other wrought names Approximate wrought designations may exist; order EN tube forms under the relevant EN tube specs, not by EN number alone on an SA-213 MTC
Related plate A240 / SA240 flat product in the same UNS family — order plate and tube under their own product standards

ASTM A213 XM-19 is the separate ASTM product specification sharing the same grade family; dual SA-213/A213 marking is a purchase-order option, not a claim that the two standards are one document. Compare molybdenum sisters such as SA213 TP316 and high-Mo SA213 UNS S31254 on their own ASME pages before swapping grades in a tube bundle.

Heat Treatment and Delivery Condition

XM-19 under ASME SA-213 is furnished solution treated at a minimum of 1900 °F [1040 °C], then quenched in water or cooled rapidly by other means at a rate sufficient to prevent carbide reprecipitation. That heat-treatment row applies to both cold-finished and hot-finished seamless tube. Nitrogen must stay in solid solution after the anneal; under-cooling or skipping the quench can leave a structure that loses the strength benefit the grade was ordered for and can invite sensitization despite the ≤0.06% carbon ceiling.

Cold-finished versus hot-finished is a process and dimensional route, not a substitute for the anneal: cold-finished tube is typically drawn after hot working and then solution treated; hot-finished tube may be quenched after hot forming when the edition allows and finishing temperature is not below the minimum anneal. Delivery condition for SHH STEEL XM-19 is solution annealed and pickled (or bright annealed by agreement), with heat-treatment temperature and quench method stated on the EN 10204 3.1 certificate. Straightening, cutting, and end finishing follow heat treatment.

When Supplementary Requirement language for intergranular-corrosion capability is ordered, the corrosion test report travels with the heat-treatment record. After heavy U-bending, ask whether a re-solution anneal of the bend zone is part of the fabrication sequence — nitrogen-strengthened grades work-harden and can pick up residual stress that a fabricator needs to manage deliberately. H-grade grain-size rules do not rewrite the XM-19 path — use SA213 TP304H or the H-grade molybdenum sisters when the datasheet calls for H-grade carbon and grain-size controls.

Corrosion Resistance

XM-19’s higher chromium, molybdenum in the 1.5–3% band, and nitrogen at 0.20–0.40% give it a stronger starting position against chloride pitting and crevice attack than standard TP304 or lean Mn–N grades, and often a competitive position relative to TP316 in many cooling-water and process exchangers. That does not make it a universal substitute for superaustenitic grades such as SA213 UNS S31254 in severe seawater or high-halide service — PREN and project corrosion testing still govern. Intergranular corrosion risk after tube-to-tubesheet welding is moderated by the ≤0.06% carbon ceiling and by solution treating after fabrication when the sequence allows.

ASME SA-213 itself does not publish a corrosion-rate or PREN table for XM-19; selection remains engineering judgment against fluid, temperature, velocity, and inspection philosophy inside the boiler or exchanger. When a specification calls for ASTM A262 Practice E or a project-specific pitting test, write that Supplementary Requirement onto the purchase order so the test is contractual rather than assumed from a verbal “Nitronic 50 equivalent” note. SHH STEEL will not rank XM-19 as automatically equal to 6% Mo superaustenitics — that claim is not supported by the product standard alone.

Applications of SA213 XM-19 Tube

Because XM-19 pairs a 100/55 ksi floor with molybdenum and elevated nitrogen, it shows up where designers need high-strength austenitic seamless tube in chloride-leaning heat exchangers, process coolers, and demanding utility circuits that outgrow standard 316. The table below pairs typical application areas with a selection note so the grade is chosen for the fluid, temperature, and fabrication route — not only for the familiar “Nitronic 50” name on the BOM.

Application area Typical use of XM-19 tube Selection note
Chloride-leaning heat exchangers Seamless HX tubes where 100/55 ksi and Mo+N help wall and pitting margins Compare TP316/TP317 and S31254 before final grade lock
Process coolers / condensers Straight and U-bend tubes in aggressive cooling circuits State min vs average wall, BWG, and bend radius on the enquiry
High-pressure utility HX Tube where design pressure rewards the elevated yield floor Confirm Code allowables for S20910 in the design code edition
Marine / coastal cooling Seamless tube in coastal or brackish service short of full seawater superaustenitic Severe seawater may still need S31254 or duplex — do not assume
Chemical and process Tube-side circuits needing higher strength than TP316 Qualify weld procedure for nitrogen-strengthened base metal
General corrosive tube duty Seamless tube where SA-213 documentation is preferred over pipe forms Do not substitute SA312 / A312 pipe paperwork for SA-213 tube acceptance

For creep-critical H-grade boiler tubing open the H-grade sisters on the SA213/SA213M hub; for severe seawater PREN programs open SA213 UNS S31254 rather than stretching XM-19 beyond its intended framing.

Weldability

XM-19 tube welds with austenitic practice written for the nitrogen-strengthened, molybdenum-bearing chemistry — not with a blind copy of a 316L procedure. Matching or near-matching fillers used on S20910 / Nitronic 50 wrought product are the starting point for tube-to-tubesheet joints and fabrication joins; many shops qualify a dedicated WPS because the elevated nitrogen and niobium/vanadium change solidification behavior relative to standard 316. Heat input control, interpass limits, and post-weld cleaning remain the fabricator’s responsibility under the applicable boiler or pressure-vessel Code — SA-213 governs the seamless tube product, not the field or shop weld procedure.

Because SA213 XM-19 is seamless, there is no mill longitudinal weld to radiograph the way welded pipe standards describe. Focus inspection language on tube integrity (hydro or NDE of each length), tube-to-tubesheet joint quality, and any contractual corrosion test on the base metal. Nitrogen-strengthened work hardening after U-bending can leave residual stress in the bend; discuss whether a local re-anneal is part of the fabrication sequence before the bundle ships. Specify end preparation and surface finish on the tube PO when orbital or clean-service joins are planned.

Surface Finishes

Standard mill delivery for ASME SA213 XM-19 is solution annealed and pickled, leaving a clean matte finish suitable for most boiler and heat-exchanger tube duty. Bright annealing under protective atmosphere produces a smoother reflective surface used on some clean-process and instrumentation tube lines and must be called out because it changes the heat-treatment route. Light polish or specified Ra on the bore or OD is a commercial or service-center operation on top of SA-213 product, not automatic with the grade stamp.

When a fouling-sensitive or coastal exchanger specification quotes an Ra maximum on the bore, put it on the tube purchase order with its own acceptance language and sampling plan. SHH STEEL stencils grade and heat treatment as standard requirements; polish, special OD grind, and passivation after fabrication remain commercial extras unless the contract says otherwise. End preparation (plain, slightly beveled, or as needed for tube expanding) should be ordered together with finish so receiving inspection shares one acceptance language.

Inspection and Testing

Base ASME SA-213 testing for XM-19 includes heat analysis (with Mo, N, Nb, and V reported), tension tests to the 100/55 ksi floor, hardness tests to the 250 HBW / 25 HRC maximum, flattening and flaring tests on a lot basis, and either hydrostatic testing or nondestructive electric testing of each length. The manufacturer may choose hydro versus NDE unless the purchase order fixes the method; both are acceptance routes inside the product standard, not informal upgrades. Marking includes the ASME designation, grade, size, heat number, and other clause-required data so receiving inspection can tie each length back to the MTC.

Supplementary Requirements commonly added on XM-19 tube orders are summarized below. Invoke them by number or clear purchase-order wording; mills will not assume product analysis or intergranular-corrosion testing from a verbal “full certs” note.

Option Purpose
Product analysis Confirms chemistry on finished tube (via general requirements / PO language)
Intergranular corrosion A262 Practice E (or agreed practice) as a contractual Supplementary Requirement
Minimum vs average wall States which wall basis the size callout uses
Fixed hydro or NDE method Removes manufacturer’s option when the end user mandates one route
Third-party inspection / EN 10204 3.2 Witnessed testing and certificate when the project requires it

Lot definitions for continuous heat treatment or direct quench after hot forming follow the size-based lot sizes in SA-213; ask the mill to state lot identity clearly on the certificate so hardness and tension specimens map cleanly to the bundle you receive. An MTC that omits niobium, vanadium, molybdenum, or nitrogen is incomplete for S20910 — reject it before the heat leaves the mill.

Packaging and Shipping

XM-19 tube leaves SHH STEEL bundled, capped or end-protected, and tagged for export or domestic delivery according to the length mix and bend form on the order. Bundle tags repeat the ASME SA213 grade, OD × wall (or BWG), heat number, and PO reference so site receiving can check the shipment without opening every certificate packet first. U-bent tubes need extra cradle or case protection so bend radii and legs are not distorted in transit — especially important on nitrogen-strengthened grades that work-harden.

Export packing can be bare bundles, wrapped bundles, or wooden-cased lengths for bright-annealed, polished, or small-bore material. We ship under the Incoterms on the order acknowledgement — FOB, CFR, CIF, EXW, or other agreed terms. Inland trucking, bilingual destination marks, or project color coding for bundle tags should be stated on the enquiry beside the metallurgical notes.

Why Choose SHH STEEL

SHH STEEL treats ASME SA213 XM-19 as a Code Book product standard with enforceable chemistry, tensile, hardness, heat-treatment, and marking rules — not as a catalogue nickname for “any Nitronic 50 tube.” The MTC reports the full ladle chemistry including Mo, N, Nb, and V and the 100/55 ksi tensile plus hardness acceptance set; the stencil carries seamless tube identity under SA-213; and dual SA-213/A213 marking is offered only when requested so Code and non-Code jobs stay cleanly documented.

We keep the high-strength austenitic conversation honest for boiler and HX duty. If standard molybdenum chemistry and the 75/30 ksi floor are enough, we open SA213 TP316 / SA213 TP316L. If nitrogen-strengthened 18-8 without molybdenum is the callout, we open SA213 TP304N. If severe seawater PREN programs need 6% Mo superaustenitic, we open SA213 UNS S31254. The SA213/SA213M hub is organized the same way — grade by grade under ASME, seamless tube only.

Lead times combine near-term stock lengths with mill schedules; we say which is which on the quotation. Cut-to-length, U-bending, polish, and third-party inspection are defined extras. The tube that arrives should match the ASME callout the engineer wrote, with paperwork a third-party inspector can read without translation.

Supply Capability

SHH STEEL can supply ASME SA213 TP XM-19 stainless steel tube against the edition and finish route named on your enquiry. The capability table below summarizes the sizes, finishes, and documents we regularly quote for this grade, followed by the Stock / Available sizes map buyers ask for when they need a quick sense of what to enquire against for boiler and heat-exchanger duty.

Item SHH STEEL capability for XM-19
Standard ASME SA213 / SA213M (dual A213 marking on request)
Grade XM-19 / UNS S20910
Product form Seamless only — cold-finished and hot-finished
Size Typical OD × min wall (or average wall) in the SA-213 usual band; other diameters by agreement
Wall / gauge Minimum wall or average wall; BWG / gauge callouts accepted on enquiry
Length Cut-to-length for HX / boiler bundles; mill random by agreement; U-bends on enquiry
Finish Annealed and pickled; bright annealed or light polish by agreement
Testing Tension (100/55 ksi), hardness (max 250 HBW / 25 HRC), flattening, flaring, hydro or NDE per length; full ladle chemistry including Mo+N+Nb+V on MTC; product analysis / IGC on order
Documents EN 10204 3.1 with full ladle chemistry; third-party inspection / 3.2 on request
Trade terms FOB / CFR / CIF / EXW and other agreed Incoterms

Stock / Available sizes

SHH STEEL quotes XM-19 tube against a practical stock-and-mill enquiry range rather than a frozen warehouse SKU list. The sizes below are the OD × wall / BWG combinations buyers most often request for high-strength HX and boiler tube; availability of any single line on a given week depends on mill drawing and our inbound schedule, so treat the table as a supply map for enquiry — not a guarantee that every line sits on the floor with a published tonnage.

Item Typical stock / enquiry range for XM-19
Outside diameter 12.7, 15.88, 19.05, 25.4, 31.8, 38.1, 50.8, 63.5, 76.2 mm (and other HX/boiler ODs on enquiry; up through the usual SA-213 ~5 in. [127 mm] band)
Wall / BWG BWG 10–20 class walls and metric min-wall equivalents; lighter and heavier walls by agreement
Common OD × wall examples 19.05 × 1.65 mm; 19.05 × 2.11 mm; 25.4 × 2.11 mm; 25.4 × 2.77 mm; 31.8 × 2.77 mm; 38.1 × 2.77 mm; 50.8 × 2.77 mm — illustrative HX/boiler sizes, confirm min vs average wall
Length Cut lengths for exchanger bundles; U-bends and straight random lengths on enquiry
Special Non-standard OD/wall, bright anneal, polished bore, and dual SA-213/A213 marking — confirm on enquiry before the heat is reserved

When you send an enquiry, list OD × wall (or BWG), wall basis (minimum or average), cold-finished or hot-finished preference, quantity or cut list, required marking (SA-213 alone or dual SA-213/A213), and any Supplementary Requirements. We reply with what we can ship from near-term stock versus what needs a mill run, without inventing fake warehouse codes or tonnage claims.

Send the size list, finish route, quantity or cut lengths, required marking (SA-213 or dual SA-213/A213), Supplementary Requirements, and destination on one enquiry. We will confirm chemistry (including Mo, N, Nb, and V), tensile, and hardness against the ordered edition, state what ships from near-term availability versus mill production, and keep the offer aligned with the ASME SA213 / SA213M product standard that governs this page. Related grades such as SA213 TP316, SA213 TP304N, and SA213 UNS S31254 sit on the same hub when the datasheet steps beyond XM-19.

FAQ

Is ASME SA-213 the same as ASTM A213 for XM-19?
No. ASME SA-213 / SA-213M is the ASME Code Book adoption of the seamless boiler, superheater, and heat-exchanger tube grade text; ASTM A213 / A213M is the separate ASTM International product specification. Chemistry, tensile, and hardness floors align closely for a given referenced edition, but they remain two independent standards. Dual-mark SA-213/A213 tube only when the purchase order asks for both names on the stencil and MTC.
Does ASME SA213 XM-19 include welded or HCW tube?
No. ASME SA-213 covers seamless tube only. There is no WLD or HCW manufacturing type under this product standard the way ASME SA312 describes pipe. The process choice for XM-19 under SA-213 is cold-finished versus hot-finished seamless tube, plus the heat-treatment and testing clauses of the ordered edition. If you need welded stainless pipe, that is a different product standard and a different steelspecs page family.
Minimum wall vs average wall — which should I order for SA213 XM-19?
Order minimum wall when the design and datasheet are written around a guaranteed minimum thickness after tolerance. Order average wall only when the purchase order explicitly allows average-wall product and the designer has accepted that basis. The two readings produce different tube from the same OD × wall line, so put the wall basis on the enquiry before the mill selects tooling and tolerance tables from the general requirements.
Hydrostatic test vs NDE — which do I get on SA213 XM-19 tube?
ASME SA-213 requires each tube to be hydrostatically tested or nondestructively electrically tested. The manufacturer may choose the method unless the purchase order fixes one. Neither route is an informal upgrade over the other inside the product standard. State the preferred method on the enquiry if your end user or inspector mandates hydro only or a named NDE technique.
Does SA-213 set a hardness limit for XM-19?
Yes. The mechanical table for XM-19 lists tensile strength, yield strength, elongation, and a hardness maximum of 250 HBW / 265 HV or 25 HRC. Hardness tests are part of lot acceptance under SA-213. If a project needs a tighter hardness window than the table, write it into the purchase order as an additional requirement rather than assuming a catalogue claim will be enforced.
What is the UNS number and chemistry of ASME SA213 XM-19?
XM-19 is UNS S20910. Melting limits include carbon ≤0.06%, manganese 4.0–6.0%, phosphorus ≤0.045%, sulfur ≤0.030%, silicon ≤1.00%, chromium 20.5–23.5%, nickel 11.5–13.5%, molybdenum 1.50–3.00%, nitrogen 0.20–0.40%, niobium 0.10–0.30%, and vanadium 0.10–0.30%. Product-analysis limits apply only when ordered. Confirm the ordered SA-213 edition and nitrogen analysis method before treating a secondary catalogue as acceptance text.
Is Nitronic 50 the same as SA213 XM-19?
Nitronic 50 is a commercial trademark name for the S20910 chemistry family; ASME SA-213 Grade XM-19 is the Code Book product designation that must appear on the stencil and MTC for this tube article. Ordering "Nitronic 50 tube" without naming SA-213 XM-19 leaves the product standard, tensile floor, and heat-treatment clause ambiguous. Put the ASME grade on the purchase order and treat the trademark as a commercial alias only.
XM-19 vs TP316 — which SA213 grade should I order?
Order XM-19 when the datasheet needs the 100/55 ksi floor and the Mo–N–Nb–V package of S20910. Order TP316 / TP316L when standard molybdenum 18-8 chemistry and the 75/30 ksi floor are enough for the corrosion and design case. XM-19 is not a silent upgrade stamp for every 316 enquiry — clear Code allowables, weld procedure, and cost before swapping.
What heat treatment does ASME SA-213 require for XM-19?
XM-19 is solution treated at a minimum of 1900 °F [1040 °C] and then water quenched or rapidly cooled to prevent carbide reprecipitation and to keep nitrogen in solid solution. Both cold-finished and hot-finished seamless tube follow that heat-treatment requirement. Ask the mill to state anneal temperature and quench method on the EN 10204 3.1 certificate so receiving inspection can clear the heat without chasing verbal confirmations.
Why is XM-19 tensile strength so high under SA213?
Molybdenum, elevated nitrogen (0.20–0.40%), and the niobium plus vanadium microalloy additions raise the SA-213 tensile floor for XM-19 to 100 ksi tensile and 55 ksi yield. That strength advantage is a mechanical-table fact tied to the full chemistry package — not a claim that any "high-N 316" heat automatically clears XM-19. Use the 100/55 ksi floor only when the heat reports Mo, N, Nb, and V in band.
Can you dual-certify ASME SA-213 and ASTM A213 XM-19?
Yes when the heat and testing support it. Dual SA-213/A213 marking is available when the purchase order requests both independent standards on the stencil and MTC. Spell the required marking on the enquiry so the heat is selected correctly, and do not assume dual marking from a verbal "Nitronic 50 full certs" note.

Conclusion

ASME SA213 XM-19 / UNS S20910 (Nitronic 50) is the high-strength molybdenum-nitrogen austenitic seamless stainless steel tube grade under the Code Book text when a project needs the 100/55 ksi floor and the full Mo–N–Nb–V chemistry package. SHH STEEL supplies cold-finished and hot-finished seamless tube in the usual OD × wall / BWG band, solution annealed, tested to the tensile and hardness acceptance floors, and documented on EN 10204 3.1 certificates — with dual A213 marking only when the order asks for that separate ASTM standard. For sister grades and stock-oriented size discussions, start from the SA213/SA213M hub, then send your OD × wall list, wall basis, and marking requirements so we can align mill and near-term availability to the ASME callout.

Contact: admin@steelspecs.com

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X