ASME SA213 TP304L Stainless Steel Tube

ASME SA213 TP304L / UNS S30403 seamless boiler, superheater and heat-exchanger tube with C ≤0.035% (Footnote D to 0.040% on small-OD / light-wall), Cr 18.0–20.0%, Ni 8.0–12.0%, a 70/25 ksi tensile floor, hardness max 192 HBW / 90 HRB, and a 1900 °F solution anneal. SHH STEEL supplies cold-finished and hot-finished seamless tube with EN 10204 3.1 MTCs.
Grade
TP304L / UNS S30403
Standard
ASME SA213 / SA213M
Product form
Seamless boiler / superheater / heat-exchanger tube (cold-finished and hot-finished)
Size
Typical OD × min wall (or average wall) within ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD and ~0.015–0.500 in. [0.4–12.7 mm] wall; other diameters by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is ASME SA213 TP304L Stainless Steel Tube

ASME SA-213 / SA-213M is the ASME Boiler and Pressure Vessel Code Book adoption of the seamless ferritic and austenitic alloy-steel boiler, superheater, and heat-exchanger tube product standard. Grade TP304L under that Code Book text is the low-carbon 18-8 chromium-nickel austenitic listed as UNS S30403, with melting limits of carbon ≤0.035% (or the Footnote D 0.040% ceiling on small-OD / light-wall paths), chromium 18.0–20.0%, and nickel 8.0–12.0%. When a Code-stamped boiler, superheater, or heat-exchanger datasheet calls for SA-213 TP304L — typically because tube-to-tubesheet joints will run as-welded in a sensitizing environment — the purchase order and mill test certificate should carry the ASME designation, not only a shop nickname such as “304L HX tube.”

SHH STEEL can supply ASME SA213 TP304L stainless steel tube as seamless cold-finished and hot-finished product in the usual boiler and heat-exchanger OD × wall / BWG band, documented on EN 10204 3.1 mill test certificates that report the full ladle chemistry and the tensile plus hardness acceptance set. Dual SA-213 / A213 marking on the same lengths is available only when the purchase order asks for both independent standards; ASME SA213 and ASTM A213 remain separate documents even when the grade text aligns closely for a referenced edition. Browse the grade family on the SA213/SA213M hub.

Commercially the same tube is still called 304L, low-carbon 18-8, S30403 boiler tube, or SA213 304L HX tube; none of those phrases replace the ASME grade on the stencil or MTC. Sister grades under the same ASME standard include SA213 TP304, SA213 TP304H, SA213 TP316L, SA213 TP321, and SA213 TP347. SA-213 covers seamless tube only — there is no welded or HCW manufacturing type under this product standard — so cold-finished versus hot-finished seamless route is the process choice, not a WLD/HCW stencil letter. For the sister ASTM product page on the same UNS, see A213 TP304L.

Chemical Composition of SA213 TP304L

Two chemistry layers matter for TP304L under ASME SA-213. The melting (heat or ladle) analysis is mandatory for every heat, while product analysis on finished tube applies only when Supplementary Requirement wording or the purchase order invokes product analysis through the general requirements path (commonly ASTM A1016/A1016M as referenced by the ordered SA-213 edition). Product-analysis tolerances are not reprinted as a standalone chemistry table inside SA-213 itself; when ordered, they typically flow from ASTM A480/A480M Table A1.1. SHH STEEL reports the actual ladle carbon at or below the 0.035% ceiling (or the Footnote D 0.040% ceiling when that thin-wall path applies) and does not advertise a tighter “0.030 shop grade” that the Code Book text does not publish.

The tables below reproduce the heat analysis for TP304L / UNS S30403 and the product-analysis limits that result from applying A480 Table A1.1 tolerances. Values are maximum unless a range is shown, and an ellipsis (…) means the ordered edition sets no requirement for that element, so it need not be determined or reported on the certificate. UNCERTAIN: exact SA-213 / A213 edition year and whether austenitic grades sit in Table 1 or Table 2 of that edition; Footnote D OD/wall trigger for the 0.040% carbon path is also edition text — confirm the ordered edition on the purchase order before treating secondary catalogues as acceptance text.

Melting analysis (heat / ladle analysis)

Source: public SA-213 / A213 grade-table summaries for TP304L / UNS S30403. Confirm the ordered ASME edition on the purchase order.

Element TP304L (UNS S30403) melting analysis
Carbon (C) ≤ 0.035 D
Manganese (Mn) ≤ 2.00
Phosphorus (P) ≤ 0.045
Sulfur (S) ≤ 0.030
Silicon (Si) ≤ 1.00
Chromium (Cr) 18.0 – 20.0
Nickel (Ni) 8.0 – 12.0
Molybdenum (Mo) … (no requirement)
Nitrogen (N) … (no requirement; analysis method by agreement when reported)

Footnote D: for small diameter or thin walls, or both, where many drawing passes are required, a carbon maximum of 0.040% is necessary in Grades TP304L, TP304LN, TP316L, and TP316LN. Confirm the ordered edition before treating any secondary catalogue as the acceptance text.

Product analysis — A480/A480M Table A1.1 tolerances applied

Element Melting Tolerance (A480 A1.1) Product analysis limit
Carbon (C) ≤ 0.035 0.01 over ≤ 0.045
Manganese (Mn) ≤ 2.00 0.04 over ≤ 2.04
Phosphorus (P) ≤ 0.045 0.010 over ≤ 0.055
Sulfur (S) ≤ 0.030 0.005 over ≤ 0.035
Silicon (Si) ≤ 1.00 0.05 over ≤ 1.05
Chromium (Cr) 18.0 – 20.0 0.20 under / over 17.80 – 20.20
Nickel (Ni) 8.0 – 12.0 0.10 under / 0.15 over 7.90 – 12.15

The low carbon ceiling (0.035%, or Footnote D 0.040%) reduces the carbon available to form chromium carbides at grain boundaries during welding or slow cooling through the sensitizing range, which is why exchanger fabricators specify L-grade tube for as-welded tube-to-tubesheet service. Nickel at 8.0–12.0% is wider than TP304’s 8.0–11.0% band, so dual TP304/TP304L heats must clear both nickel windows and both tensile floors. Chromium stays at 18–20% — the same passive-film builder as standard TP304 — while molybdenum remains a no-requirement ellipsis on this grade.

When product analysis is ordered, finished tube may read up to C 0.045%, Mn 2.04%, P 0.055%, S 0.035%, and Si 1.05%, with Cr 17.80–20.20% and Ni 7.90–12.15%. Those are the only product limits we quote from the A480 A1.1 path for this grade. Put any tighter project carbon ceiling on the purchase order before the heat is selected, and confirm whether Footnote D applies to the OD × wall you are buying.

Mechanical Properties of SA213 TP304L

ASME SA-213 sets the tensile acceptance floor for TP304L at 70 ksi [485 MPa] tensile strength and 25 ksi [170 MPa] yield strength (0.2% offset), with elongation of 35% minimum in 2 in. or 50 mm. That 70/25 ksi pair is deliberately lower than the 75/30 ksi floor on TP304 — the trade-off that comes with guaranteed low carbon. The same mechanical table also lists a hardness maximum for TP304L of 192 HBW / 200 HV or 90 HRB, and hardness tests are part of the lot acceptance scheme — a point that often surprises buyers who only know SA312 / A312 pipe rows for the same UNS number. Every lot sampled under the edition’s specimen rules must meet those numbers after the final solution treatment.

Source: public SA-213 / A213 mechanical-table summaries for TP304L / UNS S30403 (commonly Table 4). Mechanical property requirements do not apply to tubing smaller than 1/8 in. [3.2 mm] inside diameter or thinner than 0.015 in. [0.4 mm] wall.

Property TP304L requirement
Tensile strength, min 70 ksi [485 MPa]
Yield strength (0.2% offset), min 25 ksi [170 MPa]
Elongation in 2 in. or 50 mm, min 35%
Hardness, max 192 HBW / 200 HV or 90 HRB

Flattening and flaring tests are also required on a lot basis for finished tube; they sit beside tension and hardness rather than replacing them. Dual TP304/TP304L certification is common when a heat meets the tighter carbon rules and still clears the higher 75/30 ksi TP304 tensile floor plus both hardness maxima — ask for that dual marking on the purchase order rather than assuming it from a PMI gun. For creep-range boiler service that needs a controlled carbon floor and grain-size language, open SA213 TP304H rather than stretching low-carbon TP304L into H-grade framing.

Dimensions and Tolerances

Dimensional supply for ASME SA213 TP304L is tube language — outside diameter × wall thickness (minimum wall or average wall) and, commercially, BWG / gauge — not ASME B36.19 pipe schedules as the primary size story. The sizes usually furnished under SA-213 run from about 1/8 in. [3.2 mm] inside diameter to 5 in. [127 mm] outside diameter, with minimum wall from about 0.015 to 0.500 in. [0.4 to 12.7 mm]; tubing with other diameters may be furnished when all other requirements of the specification are met. State on the purchase order whether wall is minimum or average, because that choice changes how the mill interprets tolerance and how the designer reads remaining wall after fabrication.

Outside-diameter and wall variations follow the general requirements invoked by SA-213 (commonly ASTM A1016/A1016M), with cold-finished and hot-finished routes carrying different practical bands. Cold-finished tubes commonly hold tighter OD control; hot-finished tubes allow wider OD and wall windows. Permissible variations from a specified average wall for cold-finished tube are often summarized as ±10% of the specified average wall, while minimum-wall product is accepted to the minimum-wall tables rather than a symmetric ± window. Confirm the exact general-requirements rows for the OD and finish route on the ordered edition — do not treat a catalogue one-liner as a substitute for the table.

Item Typical SA213 TP304L dimensional practice
Product form Seamless only (cold-finished or hot-finished)
Usual size band ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD; wall ~0.015–0.500 in. [0.4–12.7 mm] min (or average wall if PO says so)
Wall basis Minimum wall (default commercial practice) or average wall when specified
OD / wall tolerances Per general requirements for the finish route and size; cold-finished average wall often ±10%
Length Cut lengths for HX / boiler bundles, or mill random lengths by agreement
Secondary size note ASME B36.19 schedules may appear only when a buyer asks for a pipe-schedule cross-reference — not as the primary SA-213 size callout

Put the cut list, U-bend or straight-tube preference, and end preparation on the enquiry so mill and stock lengths can be mixed efficiently. Minimum wall is a first-class SA-213 concept: if the datasheet assumes average wall, say so explicitly before the heat is rolled. When Footnote D carbon allowance is relevant, also state the OD × wall so the mill can apply the correct carbon ceiling.

Equivalent Grades

Equivalence language around TP304L tube is often looser than a Code or heat-exchanger purchase order can afford. ASME SA-213 Grade TP304L / UNS S30403 is the governing designation for this article; EN 1.4307 and JIS SUS304L are approximate wrought names that point to similar chemistry families but are not automatic substitutes on an SA-213 mill test certificate. When a datasheet says “equivalent to 304L,” confirm which product standard, tensile/hardness table, and heat-treatment clause the mill will actually certify.

Designation Notes
ASME SA-213 / SA-213M Grade TP304L Governing ASME Code Book seamless boiler / HX tube product standard for this article
UNS S30403 Unified number listed with the grade chemistry
ASTM A213 TP304L Separate ASTM International product specification — dual-mark only when the PO asks; see A213 TP304L
EN 1.4307 (X2CrNi18-9) Approximate wrought stainless designation; order EN tube forms under the relevant EN tube specs, not by EN number alone on an SA-213 MTC
JIS SUS304L Approximate Japanese grade name; confirm the Japanese tube product standard when ordering JIS product
Related plate A240 / SA240 flat product in the same UNS family — order plate and tube under their own product standards

ASTM A213 TP304L is the separate ASTM product specification sharing the same grade family; dual SA-213/A213 marking is a purchase-order option, not a claim that the two standards are one document. Compare standard-carbon, H-grade, and molybdenum sisters on their own ASME SA213 pages before swapping grades in a tube bundle that was written around low-carbon 304L.

Heat Treatment and Delivery Condition

TP304L under ASME SA-213 is furnished solution treated at a minimum of 1900 °F [1040 °C], then quenched in water or cooled rapidly by other means at a rate sufficient to prevent carbide reprecipitation. That heat-treatment row applies to both cold-finished and hot-finished seamless tube. Even with low carbon, skipping or under-cooling the solution treatment can leave a structure that sensitizes in service — L-grade chemistry is not a license to skip the anneal.

Cold-finished versus hot-finished is a process and dimensional route, not a substitute for the anneal: cold-finished tube is typically drawn after hot working and then solution treated; hot-finished tube may be quenched after hot forming when the edition allows and finishing temperature is not below the minimum anneal. Delivery condition for SHH STEEL TP304L is solution annealed and pickled (or bright annealed by agreement), with heat-treatment temperature and quench method stated on the EN 10204 3.1 certificate. Straightening, cutting, and end finishing follow heat treatment.

When Supplementary Requirement language for intergranular-corrosion capability (commonly tied to ASTM A262 Practice E on sensitized or as-shipped specimens, depending on grade type) is ordered, the corrosion test report travels with the heat-treatment record. H-grade grain-size rules do not rewrite the TP304L path — use SA213 TP304H when the datasheet calls for H-grade carbon and grain-size controls, and keep TP304L for as-welded IGC concern rather than for creep-range framing.

Corrosion Resistance

TP304L’s chromium-rich passive film handles a wide band of oxidizing process fluids, clean steam-side and water-side duties, and many organic media that do not lean heavily on chlorides — with the added benefit that low carbon improves resistance to intergranular attack after welding or slow cooling through the sensitizing range. In chloride-bearing waters, coastal cooling circuits, and many brine-leaning heat-exchanger services, pitting and crevice attack become limiting, and buyers usually step up to SA213 TP316L (or SA213 TP316 when standard carbon is acceptable). The L designation does not add molybdenum; it only caps carbon.

ASME SA-213 itself does not publish a corrosion-rate table for TP304L; selection remains engineering judgment against fluid, temperature, velocity, and inspection philosophy inside the boiler or exchanger. When a specification calls for ASTM A262 Practice E, write that Supplementary Requirement onto the purchase order so the test is contractual rather than assumed from a verbal “full certs” note. SHH STEEL will not rank TP304L as equal to 316L in chlorides — that claim is not supported by the product standard.

Applications of SA213 TP304L Tube

Because TP304L is the default low-carbon austenitic seamless tube grade when as-welded intergranular resistance matters and molybdenum is not required, it shows up across process heat exchangers, condensers, food and pharmaceutical utilities, and general corrosive tube duty where fabricators prefer not to rely on a perfect weld procedure alone. The table below pairs typical application areas with a selection note so the grade is chosen for the fluid, temperature, and fabrication route — not only for the familiar “304L” name on the BOM.

Application area Typical use of TP304L tube Selection note
Heat exchangers / condensers Straight and U-bend HX tubes where tube-to-tubesheet joints run as-welded State min vs average wall, BWG, and bend radius; consider dual TP304/TP304L when tensile floor must match 75/30
Chemical and process Tube-side or shell-side circuits with oxidizing or mild corrosive media and welding in the field Prefer TP316L if chlorides dominate
Food / pharmaceutical utilities Utility and process HX where low-carbon 304 stainless tube is accepted Follow hygiene finish and welding procedure requirements
Boiler and moderate-temperature steam Seamless tubing ordered to SA-213 where L-grade carbon is specified For creep-critical H-grade service open TP304H — not TP304L
Cryogenic / low-temperature HX Austenitic toughness in cold-box and LNG-related exchangers Confirm low-temperature Code acceptance for the grade
General corrosive tube duty Seamless tube where SA-213 documentation and low carbon are preferred Do not substitute SA312 / A312 pipe paperwork for SA-213 tube acceptance

For standard-carbon 75/30 ksi duty without as-welded IGC concern open SA213 TP304; for high-temperature creep-range boiler tubing open TP304H; for chloride-rich cooling water move to the molybdenum L-grade on the same SA213/SA213M hub.

Weldability

TP304L tube welds readily with matching or near-matching low-carbon austenitic filler for tube-to-tubesheet joints, attachment welds, and fabrication joins. Common practice uses ER308L (or equivalent covered electrodes) under a qualified WPS so weld-metal carbon stays in the L-grade band; fabricators who deposit ER308 on L-grade base metal should confirm that the finished joint still meets the project’s carbon and corrosion expectations. Heat input control, interpass limits, and post-weld cleaning remain the fabricator’s responsibility under the applicable boiler or pressure-vessel Code — SA-213 governs the seamless tube product, not the field or shop weld procedure.

Because SA213 TP304L is seamless, there is no mill longitudinal weld to radiograph the way welded pipe standards describe. Focus inspection language on tube integrity (hydro or NDE of each length), tube-to-tubesheet joint quality, and any contractual corrosion test on the base metal. The whole point of ordering TP304L is often to enter service as-welded without a full post-weld solution anneal of the bundle — still specify end preparation and surface finish on the tube PO when orbital or clean-service joins are planned.

Surface Finishes

Standard mill delivery for ASME SA213 TP304L is solution annealed and pickled, leaving a clean matte finish suitable for most boiler and heat-exchanger tube duty. Bright annealing under protective atmosphere produces a smoother reflective surface used on some clean-process and instrumentation tube lines and must be called out because it changes the heat-treatment route. Light polish or specified Ra on the bore or OD is a commercial or service-center operation on top of SA-213 product, not automatic with the grade stamp.

When a hygienic or fouling-sensitive exchanger specification quotes an Ra maximum on the bore, put it on the tube purchase order with its own acceptance language and sampling plan. SHH STEEL stencils grade and heat treatment as standard requirements; polish, special OD grind, and passivation after fabrication remain commercial extras unless the contract says otherwise. End preparation (plain, slightly beveled, or as needed for tube expanding) should be ordered together with finish so receiving inspection shares one acceptance language.

Inspection and Testing

Base ASME SA-213 testing for TP304L includes heat analysis, tension tests to the 70/25 ksi mechanical-table floors, hardness tests to the hardness maximum, flattening and flaring tests on a lot basis, and either hydrostatic testing or nondestructive electric testing of each length. The manufacturer may choose hydro versus NDE unless the purchase order fixes the method; both are acceptance routes inside the product standard, not informal upgrades. Marking includes the ASME designation, grade, size, heat number, and other clause-required data so receiving inspection can tie each length back to the MTC.

Supplementary Requirements commonly added on TP304L tube orders are summarized below. Invoke them by number or clear purchase-order wording; mills will not assume product analysis or intergranular-corrosion testing from a verbal “full certs” note.

Option Purpose
Product analysis Confirms chemistry on finished tube (via general requirements / PO language)
Intergranular corrosion A262 Practice E (or agreed practice) as a contractual Supplementary Requirement — often paired with L-grade selection
Minimum vs average wall States which wall basis the size callout uses
Fixed hydro or NDE method Removes manufacturer’s option when the end user mandates one route
Dual TP304/TP304L marking When the heat clears both carbon and tensile floors
Third-party inspection / EN 10204 3.2 Witnessed testing and certificate when the project requires it

Lot definitions for continuous heat treatment or direct quench after hot forming follow the size-based lot sizes in SA-213; ask the mill to state lot identity clearly on the certificate so hardness and tension specimens map cleanly to the bundle you receive.

Packaging and Shipping

TP304L tube leaves SHH STEEL bundled, capped or end-protected, and tagged for export or domestic delivery according to the length mix and bend form on the order. Bundle tags repeat the ASME SA213 grade, OD × wall (or BWG), heat number, and PO reference so site receiving can check the shipment without opening every certificate packet first. U-bent tubes need extra cradle or case protection so bend radii and legs are not distorted in transit.

Export packing can be bare bundles, wrapped bundles, or wooden-cased lengths for bright-annealed, polished, or small-bore material. We ship under the Incoterms on the order acknowledgement — FOB, CFR, CIF, EXW, or other agreed terms. Inland trucking, bilingual destination marks, or project color coding for bundle tags should be stated on the enquiry beside the metallurgical notes.

Why Choose SHH STEEL

SHH STEEL treats ASME SA213 TP304L as a Code Book product standard with enforceable chemistry, tensile, hardness, heat-treatment, and marking rules — not as a catalogue nickname for “any low-carbon 304 tube.” The MTC reports the actual ladle carbon against the 0.035% (or Footnote D 0.040%) ceiling and the tensile/hardness acceptance set; the stencil carries seamless tube identity under SA-213; and dual SA-213/A213 marking is offered only when requested so Code and non-Code jobs stay cleanly documented.

We keep the 304-family conversation honest for boiler and HX duty. If the datasheet needs the standard 75/30 ksi floor and carbon ≤0.08% is acceptable, we open SA213 TP304 or dual TP304/TP304L on a qualifying heat. If creep-range boiler service needs H-grade carbon and grain-size controls, we open SA213 TP304H. If chlorides dominate the cooling water or process fluid, we open SA213 TP316L. The SA213/SA213M hub is organized the same way — grade by grade under ASME, seamless tube only.

Lead times combine near-term stock lengths with mill schedules; we say which is which on the quotation. Cut-to-length, U-bending, polish, and third-party inspection are defined extras. The tube that arrives should match the ASME callout the engineer wrote, with paperwork a third-party inspector can read without translation.

Supply Capability

SHH STEEL can supply ASME SA213 TP304L stainless steel tube against the edition and finish route named on your enquiry. The capability table below summarizes the sizes, finishes, and documents we regularly quote for this grade, followed by the Stock / Available sizes map buyers ask for when they need a quick sense of what to enquire against for boiler and heat-exchanger duty.

Item SHH STEEL capability for TP304L
Standard ASME SA213 / SA213M (dual A213 marking on request)
Grade TP304L / UNS S30403
Product form Seamless only — cold-finished and hot-finished
Size Typical OD × min wall (or average wall) in the SA-213 usual band; other diameters by agreement
Wall / gauge Minimum wall or average wall; BWG / gauge callouts accepted on enquiry
Length Cut-to-length for HX / boiler bundles; mill random by agreement; U-bends on enquiry
Finish Annealed and pickled; bright annealed or light polish by agreement
Testing Tension (70/25 ksi), hardness (max 192 HBW / 90 HRB), flattening, flaring, hydro or NDE per length; full ladle chemistry on MTC; product analysis / IGC on order
Documents EN 10204 3.1 with full ladle chemistry; third-party inspection / 3.2 on request
Trade terms FOB / CFR / CIF / EXW and other agreed Incoterms

Stock / Available sizes

SHH STEEL quotes TP304L tube against a practical stock-and-mill enquiry range rather than a frozen warehouse SKU list. The sizes below are the OD × wall / BWG combinations buyers most often request for boiler and heat-exchanger tube; availability of any single line on a given week depends on mill drawing and our inbound schedule, so treat the table as a supply map for enquiry — not a guarantee that every line sits on the floor with a published tonnage.

Item Typical stock / enquiry range for TP304L
Outside diameter 12.7, 15.88, 19.05, 25.4, 31.8, 38.1, 50.8, 63.5, 76.2 mm (and other HX/boiler ODs on enquiry; up through the usual SA-213 ~5 in. [127 mm] band)
Wall / BWG BWG 10–20 class walls and metric min-wall equivalents; lighter and heavier walls by agreement
Common OD × wall examples 19.05 × 1.65 mm; 19.05 × 2.11 mm; 25.4 × 2.11 mm; 25.4 × 2.77 mm; 31.8 × 2.77 mm; 38.1 × 2.77 mm; 50.8 × 2.77 mm — illustrative HX/boiler sizes, confirm min vs average wall
Length Cut lengths for exchanger bundles; U-bends and straight random lengths on enquiry
Special Non-standard OD/wall, bright anneal, polished bore, dual SA-213/A213 marking, and dual TP304/TP304L — confirm on enquiry before the heat is reserved

When you send an enquiry, list OD × wall (or BWG), wall basis (minimum or average), cold-finished or hot-finished preference, quantity or cut list, required marking (SA-213 alone, dual SA-213/A213, and/or dual TP304/TP304L), and any Supplementary Requirements. We reply with what we can ship from near-term stock versus what needs a mill run, without inventing fake warehouse codes or tonnage claims.

Send the size list, finish route, quantity or cut lengths, required marking, Supplementary Requirements, and destination on one enquiry. We will confirm chemistry, tensile, and hardness against the ordered edition, state what ships from near-term availability versus mill production, and keep the offer aligned with the ASME SA213 / SA213M product standard that governs this page. Related grades such as SA213 TP304LN, SA213 TP321, and SA213 TP347 sit on the same hub when the datasheet steps beyond standard TP304L.

FAQ

Is ASME SA-213 the same as ASTM A213 for TP304L?
No. ASME SA-213 / SA-213M is the ASME Code Book adoption of the seamless boiler, superheater, and heat-exchanger tube grade text; ASTM A213 / A213M is the separate ASTM International product specification. Chemistry, tensile, and hardness floors align closely for a given referenced edition, but they remain two independent standards. Dual-mark SA-213/A213 tube only when the purchase order asks for both names on the stencil and MTC.
Does ASME SA213 TP304L include welded or HCW tube?
No. ASME SA-213 covers seamless tube only. There is no WLD or HCW manufacturing type under this product standard the way ASME SA312 describes pipe. The process choice for TP304L under SA-213 is cold-finished versus hot-finished seamless tube, plus the heat-treatment and testing clauses of the ordered edition. If you need welded stainless pipe, that is a different product standard and a different steelspecs page family.
Minimum wall vs average wall — which should I order for SA213 TP304L?
Order minimum wall when the design and datasheet are written around a guaranteed minimum thickness after tolerance. Order average wall only when the purchase order explicitly allows average-wall product and the designer has accepted that basis. The two readings produce different tube from the same OD × wall line, so put the wall basis on the enquiry before the mill selects tooling and tolerance tables from the general requirements.
Hydrostatic test vs NDE — which do I get on SA213 TP304L tube?
ASME SA-213 requires each tube to be hydrostatically tested or nondestructively electrically tested. The manufacturer may choose the method unless the purchase order fixes one. Neither route is an informal upgrade over the other inside the product standard. State the preferred method on the enquiry if your end user or inspector mandates hydro only or a named NDE technique.
Does SA-213 set a hardness limit for TP304L?
Yes. The mechanical table for TP304L lists tensile strength, yield strength, elongation, and a hardness maximum of 192 HBW / 200 HV or 90 HRB. Hardness tests are part of lot acceptance under SA-213, which differs from many SA312 / A312 pipe rows for the same UNS number that omit a hardness cap. If a project needs a tighter hardness window than the table, write it into the purchase order as an additional requirement.
What is the UNS number and chemistry of ASME SA213 TP304L?
TP304L is UNS S30403. Melting limits include carbon ≤0.035% (Footnote D may raise the ceiling to 0.040% on small-OD / light-wall paths), manganese ≤2.00%, phosphorus ≤0.045%, sulfur ≤0.030%, silicon ≤1.00%, chromium 18.0–20.0%, and nickel 8.0–12.0%, with molybdenum and nitrogen as no-requirement ellipses. Product-analysis limits apply only when ordered. Confirm the ordered SA-213 edition and whether Footnote D applies to your size.
TP304 vs TP304L — which SA213 tube should I order?
Order TP304 when the specification calls for the standard 75/30 ksi tensile floor, 192 HBW / 90 HRB hardness maximum, and carbon ≤0.08% is acceptable. Order TP304L when as-welded intergranular resistance is the driver and the lower 70/25 ksi floor is acceptable. Dual TP304/TP304L certification is possible on qualifying heats — ask for it on the PO rather than assuming it from a PMI gun reading.
TP304L vs TP316L — which SA213 grade for chlorides?
TP316L keeps the low-carbon ceiling and adds molybdenum at 2.00–3.00%, which generally improves chloride pitting and crevice resistance compared with TP304L. Choose TP304L when chlorides are low and low carbon is the main fabrication driver; open TP316L when cooling water or process fluid is chloride-leaning. ASME SA-213 does not publish a chloride ranking table — open both grade pages on the hub when the fluid analysis is borderline.
What heat treatment does ASME SA-213 require for TP304L?
TP304L is solution treated at a minimum of 1900 °F [1040 °C] and then water quenched or rapidly cooled to prevent carbide reprecipitation. Both cold-finished and hot-finished seamless tube follow that heat-treatment requirement. Low carbon does not replace the anneal. Ask the mill to state anneal temperature and quench method on the EN 10204 3.1 certificate so receiving inspection can clear the heat without chasing verbal confirmations.
What does Footnote D mean for SA213 TP304L carbon?
Footnote D states that for small diameter or thin walls, or both, where many drawing passes are required, a carbon maximum of 0.040% is necessary in TP304L (and related L / LN grades). The base melting limit remains ≤0.035% unless that path applies. Confirm the ordered edition wording and whether your OD × wall triggers the footnote before treating a catalogue "0.040 max" line as universal acceptance text.
Can you dual-certify ASME SA-213 and ASTM A213 TP304L, or TP304/TP304L?
Yes on both axes when the heat and testing support it. Dual SA-213/A213 marking is available when the purchase order requests both independent standards on the stencil and MTC. Dual TP304/TP304L is available when ladle chemistry meets the tighter carbon rules and tensile plus hardness results clear both mechanical-table rows. Spell the required marking on the enquiry so the heat is selected correctly.

Conclusion

ASME SA213 TP304L / UNS S30403 is the low-carbon 18-8 seamless stainless steel tube grade for Code boiler, superheater, and heat-exchanger service when as-welded intergranular resistance matters and molybdenum is not required. SHH STEEL supplies cold-finished and hot-finished seamless tube in the usual OD × wall / BWG band, solution annealed, tested to the 70/25 ksi tensile and 192 HBW / 90 HRB hardness floors, and documented on EN 10204 3.1 certificates — with dual A213 marking only when the order asks for that separate ASTM standard. For sister grades and stock-oriented size discussions, start from the SA213/SA213M hub, then send your OD × wall list, wall basis, and marking requirements so we can align mill and near-term availability to the ASME callout.

Contact: admin@steelspecs.com

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X