ASME SA213 TP310Cb Stainless Steel Tube

ASME SA213 TP310Cb / UNS S31040 seamless boiler, superheater and heat-exchanger tube — the niobium-stabilized 24–26% Cr / 19–22% Ni austenitic with C ≤0.08%, Nb 10×C–1.10%, a 75/30 ksi tensile floor, hardness max 192 HBW / 90 HRB, and a 1900 °F solution anneal. Chosen when 25Cr-20Ni oxidation resistance must sit with Nb binding of carbon against intergranular attack. SHH STEEL supplies cold-finished and hot-finished seamless tube with EN 10204 3.1 MTCs that report niobium.
Grade
TP310Cb / UNS S31040
Standard
ASME SA213 / SA213M
Product form
Seamless boiler / superheater / heat-exchanger tube (cold-finished and hot-finished)
Size
Typical OD × min wall (or average wall) within ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD and ~0.015–0.500 in. [0.4–12.7 mm] wall; other diameters by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is ASME SA213 TP310Cb Stainless Steel Tube

ASME SA-213 / SA-213M is the ASME Boiler and Pressure Vessel Code Book adoption of the seamless ferritic and austenitic alloy-steel boiler, superheater, and heat-exchanger tube product standard. Grade TP310Cb under that Code Book text is the niobium-stabilized member of the 310 family, listed as UNS S31040, with melting carbon ≤0.08%, chromium 24.0–26.0%, nickel 19.0–22.0%, and niobium (columbium) held to the formula band 10×C–1.10%. The “Cb” suffix is the stabilization story — not an H-grade carbon floor and not a molybdenum chloride grade. When a Code-stamped boiler, furnace, or heat-exchanger datasheet calls for SA-213 TP310Cb, the purchase order and mill test certificate should carry the ASME designation and the niobium result — not a tensile-only “310S” nickname stamped as if Nb were optional.

SHH STEEL can supply ASME SA213 TP310Cb stainless steel tube as seamless cold-finished and hot-finished product in the usual boiler, furnace, and heat-exchanger OD × wall / BWG band, documented on EN 10204 3.1 mill test certificates that report the full ladle chemistry including niobium and the tensile plus hardness acceptance set. Dual SA-213 / A213 marking on the same lengths is available only when the purchase order asks for both independent standards; ASME SA213 and ASTM A213 remain separate documents even when the grade text aligns closely for a referenced edition. Browse the grade family on the SA213/SA213M hub.

Commercially the same tube is still called 310Cb, 310Nb, S31040, stabilized 25Cr-20Ni tube, or SA213 310Cb tube; none of those phrases replace the ASME grade on the stencil or MTC. Sister grades under the same ASME standard include SA213 TP310S, SA213 TP310H, SA213 TP310HCb, SA213 TP309Cb, and SA213 TP304. SA-213 covers seamless tube only — there is no welded or HCW manufacturing type under this product standard — so cold-finished versus hot-finished seamless route is the process choice, not a WLD/HCW stencil letter. For the sister ASTM product page on the same UNS, see A213 TP310Cb.

Chemical Composition of SA213 TP310Cb

Two chemistry layers matter for TP310Cb under ASME SA-213. The melting (heat or ladle) analysis is mandatory for every heat under the stainless chemistry table; product analysis on finished tube applies only when Supplementary Requirement wording or the purchase order invokes it through the general requirements path (commonly ASTM A1016/A1016M), with product-analysis tolerances typically taken from ASTM A480/A480M Table A1.1. Niobium is the first line a stabilization reviewer should check: the melt must satisfy Nb ≥10×C and Nb ≤1.10% together with C ≤0.08% and the 24–26 / 19–22 Cr–Ni windows. SHH STEEL reports the actual ladle values — including Nb — and the product values when ordered, and does not advertise unpublished tighter catalogue windows.

The tables below reproduce the melt limits for TP310Cb / UNS S31040 and the product-analysis limits that result from applying A480 Table A1.1 tolerances, plus a stabilization snapshot versus TP310S and TP310HCb. Values are maximum unless a range or formula is shown; an ellipsis (…) means the ordered edition sets no requirement for that element. UNCERTAIN: exact SA-213 / A213 edition year and whether austenitic grades sit in Table 1 or Table 2 of that edition; A480 Cr/Ni/Nb tolerance digits for the 24–26% Cr / 19–22% Ni band and formula Nb minimum — applied from sister 310 / high-Cr practice; S2 stabilizing applicability wording for non-HCb 310Cb rows across editions — confirm the ordered edition on the purchase order.

Melting analysis (heat / ladle analysis)

Source: public SA-213 / A213 grade-table summaries for TP310Cb / UNS S31040. Confirm the ordered ASME edition on the purchase order. “Cb” and “Nb” are the same stabilizer element in this grade row.

Element TP310Cb (UNS S31040) melting analysis
Carbon (C) ≤ 0.08
Manganese (Mn) ≤ 2.00
Phosphorus (P) ≤ 0.045
Sulfur (S) ≤ 0.030
Silicon (Si) ≤ 1.00
Chromium (Cr) 24.0 – 26.0
Nickel (Ni) 19.0 – 22.0
Molybdenum (Mo) … (no requirement)
Nitrogen (N) … (no requirement)
Niobium (Nb / Cb) 10×C – 1.10

Product analysis — A480/A480M Table A1.1 tolerances applied

Element Melting Tolerance (A480 A1.1) Product analysis limit
Carbon (C) ≤ 0.08 0.01 over ≤ 0.09
Manganese (Mn) ≤ 2.00 0.04 over ≤ 2.04
Phosphorus (P) ≤ 0.045 0.010 over ≤ 0.055
Sulfur (S) ≤ 0.030 0.005 over ≤ 0.035
Silicon (Si) ≤ 1.00 0.05 over ≤ 1.05
Chromium (Cr) 24.0 – 26.0 0.25 under / over 23.75 – 26.25
Nickel (Ni) 19.0 – 22.0 0.15 under / 0.20 over 18.85 – 22.20
Niobium (Nb) 10×C – 1.10 0.05 under / over on max; min remains formula-tied max ≤ 1.15; min still ≥10×C on melt basis — confirm A480 path if contractual

Stabilization snapshot — TP310S / TP310Cb / TP310HCb

Element TP310S (S31008) TP310Cb (S31040) TP310HCb (S31041)
C ≤ 0.08 ≤ 0.08 0.04 – 0.10
Cr / Ni 24–26 / 19–22 24–26 / 19–22 24–26 / 19–22
Nb (Cb) … 10×C – 1.10 10×C – 1.10
Grain size no mandate no mandate No. 7 or coarser

Chromium 24–26% and nickel 19–22% are the oxidation-resistance story; niobium is the stabilization story. Carbon ≤0.08% is the same ceiling as TP310S — not an H-grade floor. Dual TP310S/TP310Cb is not automatic: niobium must be intentionally melted to the formula band. When combined H-grade carbon plus Nb is required, open SA213 TP310HCb; when only H-grade carbon/grain-size without Nb is required, open SA213 TP310H; when a step down in Cr–Ni with Nb is enough, open SA213 TP309Cb.

When product analysis is ordered, finished tube may read up to C 0.09%, Mn 2.04%, P 0.055%, S 0.035%, and Si 1.05%, with Cr 23.75–26.25% and Ni 18.85–22.20%. Niobium product-analysis practice for formula minima is edition-sensitive — confirm the A480 path if product Nb is contractual. Put any tighter project carbon or sulfur ceiling on the purchase order before the heat is selected.

Mechanical Properties of SA213 TP310Cb

ASME SA-213 sets the room-temperature tensile acceptance floor for TP310Cb at 75 ksi [515 MPa] tensile strength and 30 ksi [205 MPa] yield strength (0.2% offset), with elongation of 35% minimum in 2 in. or 50 mm — the same room-temperature pair as TP310S. Hardness is capped at 192 HBW / 200 HV or 90 HRB. Unlike TP310H / TP310HCb, TP310Cb does not carry a mandatory ASTM grain-size number in the heat-treatment table — acceptance is chemistry (including Nb), tensile, hardness, and heat treatment. Every lot sampled under the edition’s specimen rules must meet those numbers after the final solution treatment.

Source: public SA-213 / A213 mechanical-table summaries for TP310Cb / UNS S31040 (commonly Table 4). Mechanical property requirements do not apply to tubing smaller than 1/8 in. [3.2 mm] inside diameter or thinner than 0.015 in. [0.4 mm] wall.

Property TP310Cb requirement
Tensile strength, min 75 ksi [515 MPa]
Yield strength (0.2% offset), min 30 ksi [205 MPa]
Elongation in 2 in. or 50 mm, min 35%
Hardness, max 192 HBW / 200 HV or 90 HRB
Grain size No mandatory ASTM grain-size number (unlike TP310H / TP310HCb)

Flattening and flaring tests sit beside tension and hardness on a lot basis. Niobium stabilization is a chemistry acceptance story, not a higher tensile floor. Ask for the Nb result on the EN 10204 3.1 certificate together with tensile and hardness — a 310S-looking MTC without Nb does not prove TP310Cb. When the datasheet needs H-grade carbon 0.04–0.10% and ASTM No. 7 or coarser grain size together with Nb, open SA213 TP310HCb; when only H-grade carbon/grain-size without Nb is required, open SA213 TP310H.

Dimensions and Tolerances

Dimensional supply for ASME SA213 TP310Cb is tube language — outside diameter × wall thickness (minimum wall or average wall) and, commercially, BWG / gauge — not ASME B36.19 pipe schedules as the primary size story. The sizes usually furnished under SA-213 run from about 1/8 in. [3.2 mm] inside diameter to 5 in. [127 mm] outside diameter, with minimum wall from about 0.015 to 0.500 in. [0.4 to 12.7 mm]; tubing with other diameters may be furnished when all other requirements of the specification are met. State on the purchase order whether wall is minimum or average, because remaining wall after high-temperature oxidation is often a design input on the circuits where stabilized 310Cb is chosen.

Outside-diameter and wall variations follow the general requirements invoked by SA-213 (commonly ASTM A1016/A1016M), with cold-finished and hot-finished routes carrying different practical bands. Cold-finished tubes commonly hold tighter OD control; hot-finished tubes allow wider OD and wall windows. Permissible variations from a specified average wall for cold-finished tube are often summarized as ±10% of the specified average wall, while minimum-wall product is accepted to the minimum-wall tables rather than a symmetric ± window. Confirm the exact general-requirements rows for the OD and finish route on the ordered edition.

Item Typical SA213 TP310Cb dimensional practice
Product form Seamless only (cold-finished or hot-finished)
Usual size band ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD; wall ~0.015–0.500 in. [0.4–12.7 mm] min (or average wall if PO says so)
Wall basis Minimum wall (default commercial practice) or average wall when specified
OD / wall tolerances Per general requirements for the finish route and size; cold-finished average wall often ±10%
Length Cut lengths for HX / boiler / furnace bundles, or mill random lengths by agreement
Secondary size note ASME B36.19 schedules may appear only when a buyer asks for a pipe-schedule cross-reference — not as the primary SA-213 size callout

Put the cut list, U-bend or straight-tube preference, Nb reporting expectation, and end preparation on the enquiry so mill and stock lengths can be mixed efficiently. Minimum wall is a first-class SA-213 concept: if the datasheet assumes average wall, say so explicitly before the heat is rolled.

Equivalent Grades

Equivalence language around TP310Cb tube often collapses plate, cast, and tube product forms into one nickname. ASME SA-213 Grade TP310Cb / UNS S31040 is the governing designation for this article; EN and JIS wrought names that point to similar Nb-bearing high-Cr–Ni families are not automatic substitutes on an SA-213 mill test certificate. When a datasheet says “equivalent to 310Cb,” confirm which product standard, tensile/hardness table, niobium formula, and heat-treatment clause the mill will actually certify.

Designation Notes
ASME SA-213 / SA-213M Grade TP310Cb Governing ASME Code Book seamless boiler / HX tube product standard for this article
UNS S31040 Unified number listed with the grade chemistry
ASTM A213 TP310Cb Separate ASTM International product specification — dual-mark only when the PO asks; see A213 TP310Cb
Related S-grade SA213 TP310S — same Cr–Ni, C ≤0.08, no Nb mandate
Related H+Cb SA213 TP310HCb — H-grade carbon plus same Nb formula, grain size No. 7 or coarser
Related 309Cb SA213 TP309Cb — lower Cr–Ni oxidation step with Nb stabilization
Related plate A240 / SA240 flat product in the 310 family — order plate and tube under their own product standards

ASTM A213 TP310Cb is the separate ASTM product specification sharing the same grade family; dual SA-213/A213 marking is a purchase-order option, not a claim that the two standards are one document. Compare TP310S, TP310H, and TP310HCb on their own ASME SA213 pages before swapping 310-family grades inside a furnace or boiler tube list.

Heat Treatment and Delivery Condition

TP310Cb under ASME SA-213 is furnished solution treated at a minimum of 1900 °F [1040 °C], then quenched in water or cooled rapidly by other means. The heat-treatment table does not list a mandatory ASTM grain-size number for TP310Cb (unlike TP310H / TP310HCb). That heat-treatment row applies to both cold-finished and hot-finished seamless tube.

Cold-finished versus hot-finished is a process and dimensional route, not a substitute for the anneal. Delivery condition for SHH STEEL TP310Cb is solution annealed and pickled (or bright annealed by agreement), with heat-treatment temperature, quench method, and niobium result stated on the EN 10204 3.1 certificate. Straightening, cutting, and end finishing follow heat treatment.

Supplementary Requirement S2 (stabilizing heat treatment) in public SA-213 / A213 excerpts explicitly lists TP310HCb among grades that shall receive a post-solution stabilizing treatment when S2 is specified; TP310Cb is not assumed from that HCb listing alone. If a project needs a contractual stabilizing hold after solution treatment on a non-HCb 310Cb heat, write the requirement onto the purchase order in clear language rather than relying on an HCb-only S2 row. When H-grade carbon and grain-size controls are also required with Nb, open SA213 TP310HCb.

Corrosion Resistance

TP310Cb is selected primarily for high-temperature oxidation resistance from its 24–26% chromium / 19–22% nickel balance, plus niobium stabilization against intergranular corrosion after welding or thermal exposure — not for molybdenum-driven chloride pitting resistance. In oxidizing furnace atmospheres, hot-process gas circuits, and elevated-temperature steam services where 18-8 and even 309Cb scale too quickly, the higher Cr–Ni oxide scale is the commercial reason to pay for 310Cb. In chloride-bearing cooling waters and wet brine-leaning exchangers, buyers usually step to SA213 TP316 / SA213 TP316L or higher rather than treating 310Cb as a chloride upgrade.

ASME SA-213 itself does not publish a corrosion-rate or oxidation-life table for TP310Cb; selection remains engineering judgment against temperature, atmosphere, velocity, and inspection philosophy. Niobium binds carbon as NbC so chromium stays available for the passive film after thermal cycling; that is a chemistry story, not a higher tensile floor. When creep-range H-grade carbon and grain-size controls are also required alongside Nb, evaluate SA213 TP310HCb. Sulfidation and carburizing atmospheres still need process-specific review beyond catalogue oxidation claims. SHH STEEL will not rank TP310Cb as equal to 316 in chlorides — higher chromium, nickel, and niobium are not a molybdenum substitute.

Applications of SA213 TP310Cb Tube

Because TP310Cb brings Nb 10×C–1.10% stabilization on a 24–26% Cr / 19–22% Ni oxidation balance under SA-213 without adding an H-grade carbon floor, it shows up in high-temperature oxidation-prone boiler and process circuits, furnace-related heat exchangers, and elevated-temperature HX duty where welded or thermally cycled tube needs Nb binding of carbon. The table below pairs typical application areas with a selection note so the grade is chosen for atmosphere, metal temperature, and stabilization need — not only for the familiar “310Cb” name on the BOM.

Application area Typical use of TP310Cb tube Selection note
Severe high-temperature oxidation + IGC risk Seamless tube where 25Cr-20Ni scale resistance and Nb stabilization sit together Confirm design metal temperature and weld/thermal cycle exposure
Boiler / process steam (oxidation-limited) Seamless generating or process tubing ordered to SA-213 with Nb reporting For creep-critical H+Cb open TP310HCb
Furnace / hot-gas heat exchangers Straight and U-bend tubes in oxidizing hot-gas circuits Prefer TP309Cb if a step down in Cr–Ni is enough
Chemical process (oxidizing, low chloride) Tube-side circuits with hot oxidizing media and thermal cycling Prefer TP316/TP316L if chlorides dominate
Chloride-rich cooling water Usually not the preferred selection Open molybdenum grades on the hub
General corrosive tube duty Seamless tube where SA-213 documentation is preferred over pipe forms Do not substitute SA312 / A312 pipe paperwork for SA-213 tube acceptance

For H-grade carbon and grain-size without Nb open SA213 TP310H; for combined H+Cb open SA213 TP310HCb; for a step down in Cr–Ni with Nb open SA213 TP309Cb; browse the same SA213/SA213M hub before locking the tube bill of materials.

Weldability

TP310Cb tube welds with matching or near-matching austenitic filler for tube-to-tubesheet joints, attachment welds, and fabrication joins. Common practice uses ER310 / Nb-bearing or near-matching deposits under a qualified WPS; fabricators often prefer controlled-carbon or Nb-bearing fillers when the base tube relies on niobium for post-weld intergranular resistance. Heat input control, interpass limits, and post-weld cleaning remain the fabricator’s responsibility under the applicable boiler or pressure-vessel Code — SA-213 governs the seamless tube product, not the field or shop weld procedure.

Because SA213 TP310Cb is seamless, there is no mill longitudinal weld to radiograph the way welded pipe standards describe. Focus inspection language on tube integrity (hydro or NDE of each length), niobium documentation on the base metal, tube-to-tubesheet joint quality, and any contractual corrosion test. For tube that will enter service as-welded in a sensitizing environment, discuss whether the Nb chemistry alone is enough or whether a post-weld solution treatment or a move to TP310HCb better protects the joint. Specify end preparation and surface finish on the tube PO when orbital or clean-service joins are planned.

Surface Finishes

Standard mill delivery for ASME SA213 TP310Cb is solution annealed and pickled, leaving a clean matte finish suitable for most boiler, furnace, and heat-exchanger tube duty. Bright annealing under protective atmosphere produces a smoother reflective surface used on some clean-process tube lines and must be called out because it changes the heat-treatment route. Light polish or specified Ra on the bore or OD is a commercial or service-center operation on top of SA-213 product, not automatic with the grade stamp.

When a fouling-sensitive or clean-process exchanger specification quotes an Ra maximum on the bore, put it on the tube purchase order with its own acceptance language and sampling plan. SHH STEEL stencils grade and heat treatment as standard requirements and reports niobium on the MTC; polish, special OD grind, and passivation after fabrication remain commercial extras unless the contract says otherwise. End preparation should be ordered together with finish so receiving inspection shares one acceptance language.

Inspection and Testing

Base ASME SA-213 testing for TP310Cb includes heat analysis (with niobium), tension tests to the 75/30 ksi floor, hardness tests to the 192 HBW / 90 HRB maximum, flattening and flaring tests on a lot basis, and either hydrostatic testing or nondestructive electric testing of each length. The manufacturer may choose hydro versus NDE unless the purchase order fixes the method; both are acceptance routes inside the product standard, not informal upgrades. Marking includes the ASME designation, grade, size, heat number, and other clause-required data so receiving inspection can tie each length back to the MTC.

Supplementary Requirements commonly added on TP310Cb tube orders are summarized below. Invoke them by number or clear purchase-order wording; mills will not assume product analysis or intergranular-corrosion testing from a verbal “full certs” note. Niobium is part of the base chemistry acceptance — confirm the Nb result appears on the certificate before releasing the heat.

Option Purpose
Product analysis Confirms chemistry including Nb on finished tube (via general requirements / PO language)
Intergranular corrosion A262 Practice E (or agreed practice) as a contractual Supplementary Requirement
Stabilizing heat treatment Write clear PO language if a post-solution stabilizing hold is required (do not assume HCb-only S2 covers TP310Cb)
Minimum vs average wall States which wall basis the size callout uses
Fixed hydro or NDE method Removes manufacturer’s option when the end user mandates one route
Third-party inspection / EN 10204 3.2 Witnessed testing and certificate when the project requires it

Lot definitions for continuous heat treatment or direct quench after hot forming follow the size-based lot sizes in SA-213; ask the mill to state lot identity clearly on the certificate so hardness, tension, and chemistry specimens map cleanly to the bundle you receive.

Packaging and Shipping

TP310Cb tube leaves SHH STEEL bundled, capped or end-protected, and tagged for export or domestic delivery according to the length mix and bend form on the order. Bundle tags repeat the ASME SA213 grade, OD × wall (or BWG), heat number, and PO reference so site receiving can check the shipment without opening every certificate packet first. U-bent tubes need extra cradle or case protection so bend radii and legs are not distorted in transit.

Export packing can be bare bundles, wrapped bundles, or wooden-cased lengths for bright-annealed, polished, or small-bore material. We ship under the Incoterms on the order acknowledgement — FOB, CFR, CIF, EXW, or other agreed terms. Inland trucking, bilingual destination marks, or project color coding for bundle tags should be stated on the enquiry beside the metallurgical notes — including the niobium reporting expectation that distinguishes Cb-grade release packages.

Why Choose SHH STEEL

SHH STEEL treats ASME SA213 TP310Cb as a Code Book product standard with enforceable chemistry (including niobium), tensile, hardness, heat-treatment, and marking rules — not as a catalogue nickname for “any stabilized 310 tube.” The MTC reports the full ladle chemistry with Nb and the tensile/hardness acceptance set; the stencil carries seamless tube identity under SA-213; and dual SA-213/A213 marking is offered only when requested so Code and non-Code jobs stay cleanly documented.

We keep the 310-family conversation honest for high-temperature boiler and furnace duty. If the specification only needs C ≤0.08% without Nb, we open SA213 TP310S. If H-grade carbon and grain-size controls are required without Nb, we open SA213 TP310H. If both H-grade carbon/grain-size and Nb are required, we open SA213 TP310HCb. If a step down in chromium–nickel with Nb is enough, we open SA213 TP309Cb. If chlorides dominate a wet exchanger, we open SA213 TP316 / SA213 TP316L rather than stretching 310Cb into the wrong service. The SA213/SA213M hub is organized the same way — grade by grade under ASME, seamless tube only.

Lead times combine near-term stock lengths with mill schedules; we say which is which on the quotation. Cut-to-length, U-bending, polish, and third-party inspection are defined extras. The tube that arrives should match the ASME Cb-grade callout the engineer wrote, with paperwork a third-party inspector can read without translation.

Supply Capability

SHH STEEL can supply ASME SA213 TP310Cb stainless steel tube against the edition and finish route named on your enquiry. The capability table below summarizes the sizes, finishes, and documents we regularly quote for this stabilized grade, followed by the Stock / Available sizes map buyers ask for when they need a quick sense of what to enquire against for high-temperature oxidation-resistant boiler and furnace tube with Nb stabilization.

Item SHH STEEL capability for TP310Cb
Standard ASME SA213 / SA213M (dual A213 marking on request)
Grade TP310Cb / UNS S31040
Product form Seamless only — cold-finished and hot-finished
Size Typical OD × min wall (or average wall) in the SA-213 usual band; other diameters by agreement
Wall / gauge Minimum wall or average wall; BWG / gauge callouts accepted on enquiry
Length Cut-to-length for boiler / furnace / HX bundles; mill random by agreement; U-bends on enquiry
Finish Annealed and pickled; bright annealed or light polish by agreement
Testing Tension (75/30 ksi), hardness (max 192 HBW / 90 HRB), flattening, flaring, hydro or NDE per length; full ladle chemistry including Nb on MTC; product analysis / IGC on order
Documents EN 10204 3.1 with full ladle chemistry including niobium; third-party inspection / 3.2 on request
Trade terms FOB / CFR / CIF / EXW and other agreed Incoterms

Stock / Available sizes

SHH STEEL quotes TP310Cb tube against a practical stock-and-mill enquiry range rather than a frozen warehouse SKU list. The sizes below are the OD × wall / BWG combinations buyers most often request for high-temperature oxidation-resistant boiler and furnace tube with niobium stabilization; availability of any single line on a given week depends on mill drawing and our inbound schedule, so treat the table as a supply map for enquiry — not a guarantee that every line sits on the floor with a published tonnage.

Item Typical stock / enquiry range for TP310Cb
Outside diameter 19.05, 25.4, 31.8, 38.1, 44.5, 50.8, 63.5, 76.2 mm (and other boiler/furnace/HX ODs on enquiry; up through the usual SA-213 ~5 in. [127 mm] band)
Wall / BWG BWG 10–18 class walls and metric min-wall equivalents; lighter and heavier walls by agreement
Common OD × wall examples 25.4 × 2.11 mm; 25.4 × 2.77 mm; 31.8 × 2.77 mm; 38.1 × 2.77 mm; 38.1 × 3.40 mm; 50.8 × 3.40 mm; 50.8 × 3.60 mm — illustrative stabilized HX/boiler sizes, confirm min vs average wall
Length Cut lengths for exchanger and high-temperature bundles; U-bends and straight random lengths on enquiry
Special Non-standard OD/wall, bright anneal, polished bore, Nb reporting confirmation, and dual SA-213/A213 marking — confirm on enquiry before the heat is reserved

When you send an enquiry, list OD × wall (or BWG), wall basis (minimum or average), cold-finished or hot-finished preference, quantity or cut list, required marking (SA-213 alone or dual SA-213/A213), niobium reporting expectation, and any Supplementary Requirements. We reply with what we can ship from near-term stock versus what needs a mill run, without inventing fake warehouse codes or tonnage claims.

Send the size list, finish route, quantity or cut lengths, required marking (SA-213 or dual SA-213/A213), Supplementary Requirements, and destination on one enquiry. We will confirm chemistry including Nb, tensile, and hardness against the ordered edition, state what ships from near-term availability versus mill production, and keep the offer aligned with the ASME SA213 / SA213M product standard that governs this page. Related grades such as SA213 TP310S, SA213 TP310HCb, and SA213 TP309Cb sit on the same hub when the datasheet steps beyond TP310Cb.

FAQ

Is ASME SA-213 the same as ASTM A213 for TP310Cb?
No. ASME SA-213 / SA-213M is the ASME Code Book adoption of the seamless boiler, superheater, and heat-exchanger tube grade text; ASTM A213 / A213M is the separate ASTM International product specification. Chemistry, tensile, hardness, and niobium floors align closely for a given referenced edition, but they remain two independent standards. Dual-mark SA-213/A213 tube only when the purchase order asks for both names on the stencil and MTC.
Does ASME SA213 TP310Cb include welded or HCW tube?
No. ASME SA-213 covers seamless tube only. There is no WLD or HCW manufacturing type under this product standard the way ASME SA312 describes pipe. The process choice for TP310Cb under SA-213 is cold-finished versus hot-finished seamless tube, plus the heat-treatment and testing clauses of the ordered edition. If you need welded stainless pipe, that is a different product standard and a different steelspecs page family.
What is the chemistry of ASME SA213 TP310Cb?
TP310Cb is UNS S31040. Melting limits include carbon ≤0.08%, manganese ≤2.00%, phosphorus ≤0.045%, sulfur ≤0.030%, silicon ≤1.00%, chromium 24.0–26.0%, nickel 19.0–22.0%, and niobium 10×C–1.10%, with molybdenum and nitrogen as no-requirement ellipses. Product-analysis limits apply only when ordered, typically from A480 Table A1.1 tolerances via the general-requirements path. Confirm the ordered SA-213 edition before treating a secondary catalogue as acceptance text.
TP310Cb vs TP310S — which SA213 grade should I order?
Order TP310Cb when the datasheet needs niobium stabilization (Nb 10×C–1.10%) on the same 24–26% Cr / 19–22% Ni balance and C ≤0.08% ceiling as TP310S. Order TP310S when Nb is not required. Both share a 75/30 ksi tensile floor and lack a mandatory grain-size number, so tensile equality alone is not a reason to swap; confirm the Nb callout before substituting either grade for the other.
TP310Cb vs TP310HCb — which SA213 grade should I order?
Order TP310Cb when you need Nb stabilization without the H-grade carbon band and grain-size package. Order TP310HCb when the boiler or superheater datasheet needs carbon 0.04–0.10%, ASTM No. 7 or coarser grain size, and the same Nb 10×C–1.10% formula together. Do not treat "310HCb" as a synonym stamp for ordinary TP310Cb on the MTC.
Does SA-213 set a hardness limit for TP310Cb?
Yes. Public mechanical-table summaries for TP310Cb set a hardness maximum of 192 HBW / 200 HV or 90 HRB alongside the 75 ksi tensile and 30 ksi yield floors. Hardness testing sits on a lot basis with tension, flattening, and flaring. If a project quotes a tighter hardness window, put it on the purchase order as a contractual extra — the product-standard ceiling remains the acceptance floor unless the mill accepts a tighter guarantee in writing.
What heat treatment does ASME SA-213 require for TP310Cb?
TP310Cb is solution treated at a minimum of 1900 °F [1040 °C] and quenched in water or cooled rapidly by other means. Unlike TP310H / TP310HCb, there is no mandatory ASTM grain-size number on the TP310Cb heat-treatment row. Cold-finished versus hot-finished is a dimensional route, not a substitute for the anneal. Delivery condition is typically solution annealed and pickled, with anneal temperature, quench method, and niobium result on the MTC.
Is S2 stabilizing heat treatment automatic for SA213 TP310Cb?
No. Public SA-213 / A213 excerpts list TP310HCb among grades that shall receive a post-solution stabilizing treatment when Supplementary Requirement S2 is specified; TP310Cb is not assumed from that HCb listing alone. If your project needs a contractual stabilizing hold after solution treatment on a non-HCb 310Cb heat, write the requirement onto the purchase order in clear language rather than relying on an HCb-only S2 row.
Minimum wall vs average wall — which should I order for SA213 TP310Cb?
Most boiler and heat-exchanger datasheets assume minimum wall because remaining wall after high-temperature oxidation is a design input. Average wall is acceptable when the purchase order says so and the general-requirements tolerances for that finish route are understood. State the wall basis explicitly on the enquiry so mill and stock lengths are rolled and accepted to the correct table — do not leave wall basis implied by a BWG number alone.
Is TP310Cb a good choice for chloride-rich cooling water under SA213?
Usually no. TP310Cb is built for high-temperature oxidation resistance and niobium stabilization against intergranular attack; molybdenum is a no-requirement ellipsis. For chloride-rich cooling water and wet brine-leaning exchangers, open molybdenum grades such as SA213 TP316 / TP316L or higher rather than treating 310Cb as a chloride upgrade. Higher chromium, nickel, and niobium are not a molybdenum substitute.
Can you dual-certify ASME SA-213 and ASTM A213 TP310Cb?
Yes, when the purchase order asks for both independent standards on the stencil and mill test certificate. ASME SA-213 and ASTM A213 remain separate documents even when chemistry and tensile floors align for a referenced edition. Dual-mark only when both names are required; do not assume an A213-only certificate substitutes for an SA-213 Code callout, or the reverse.

Conclusion

ASME SA213 TP310Cb / UNS S31040 is the niobium-stabilized 24–26% Cr / 19–22% Ni seamless stainless steel tube grade for Code boiler, furnace, and heat-exchanger service when 25Cr-20Ni oxidation resistance must sit together with Nb binding of carbon against intergranular attack. SHH STEEL supplies cold-finished and hot-finished seamless tube in the usual OD × wall / BWG band, solution annealed at 1900 °F, tested to the 75/30 ksi tensile and hardness acceptance floors with niobium reported on the MTC, and documented on EN 10204 3.1 certificates — with dual A213 marking only when the order asks for that separate ASTM standard. For sister grades and stock-oriented size discussions, start from the SA213/SA213M hub, then send your OD × wall list, wall basis, Nb reporting expectation, and marking requirements so we can align mill and near-term availability to the ASME callout.

Contact: admin@steelspecs.com

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response