ASME SA213 UNS S31002 Stainless Steel Tube | ASME SA213 Stainless Steel - SHH STEEL

ASME SA213 UNS S31002 Stainless Steel Tube

ASME SA213 UNS S31002 low-carbon low-silicon 25Cr–20Ni austenitic seamless boiler, superheater and heat-exchanger tube — C ≤0.02%, Si ≤0.15%, Cr 24.0–26.0%, Ni 19.0–22.0%, Mo ≤0.10%, N ≤0.10%, P ≤0.020%, S ≤0.015%, Table 4 73/30 ksi with elongation 35% min, hardness max 192 HBW / 90 HRB, 1900 °F solution anneal. No TP letter — order by UNS. SHH STEEL supplies cold-finished and hot-finished seamless tube with EN 10204 3.1 MTCs that report the low-C / low-Si windows together.
Grade
UNS S31002 (no TP letter — low-C low-Si 25Cr–20Ni austenitic)
Standard
ASME SA213 / SA213M
Product form
Seamless boiler / superheater / heat-exchanger tube (cold-finished and hot-finished)
Size
Typical OD × min wall (or average wall) within ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD and ~0.015–0.500 in. [0.4–12.7 mm] wall; other diameters by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is ASME SA213 UNS S31002 Stainless Steel Tube

ASME SA-213 / SA-213M is the ASME Boiler and Pressure Vessel Code Book adoption of the seamless ferritic and austenitic alloy-steel boiler, superheater, and heat-exchanger tube product text. When Code-stamped boilers, superheaters, or heat exchangers invoke that adoption by name, SA-213 is the governing product standard for this low-carbon, low-silicon 25Cr–20Ni austenitic tube — written as its own Code Book line, not as a merged synonym of ASTM A213. Begin from SA213/SA213M when the enquiry is Code-led.

UNS S31002 sits in the stainless chemistry table without a TP grade letter (Footnote C practice). Melting carbon is capped at ≤0.02%, silicon at ≤0.15%, chromium at 24.0–26.0%, and nickel at 19.0–22.0% — the same Cr–Ni oxidation window as TP310S, but with deliberately tighter carbon and silicon ceilings. Molybdenum is capped at ≤0.10%, nitrogen at ≤0.10%, phosphorus at ≤0.020%, and sulfur at ≤0.015%. Table 4 sets tensile at 73 ksi [500 MPa] / 30 ksi [205 MPa] with elongation 35% minimum and hardness max 192 HBW / 90 HRB. Buyers who write “low-C 310” or “310L-type HX tube” on a bill of materials still need to name SA-213 UNS S31002 on the purchase order so the mill applies the tube product standard, minimum-wall rules, and the low-C / low-Si windows together. This is not a dual stamp of SA213 TP310S or of SA213 TP310H.

SHH STEEL can supply ASME SA213 UNS S31002 as seamless cold-finished and hot-finished tube in the usual OD × wall / BWG band, with EN 10204 3.1 certificates that report the carbon and silicon ceilings together with the 73/30 ksi tensile set, 35% elongation, and hardness. Dual SA-213/A213 marking is added only when the purchase order asks; the live twin is A213 UNS S31002.

Shop names include “S31002,” “low-C 310,” and “25-20 low-Si.” Helpful for routing; the commercial nickname does not replace UNS S31002 on the MTC. The purchase order should still carry ASME SA-213 UNS S31002, wall basis, OD × wall or BWG, finish route, and any Supplementary Requirements when needed. Sister SA213 pages include SA213 TP310S, SA213 TP310H, SA213 TP310Cb, and SA213 TP310MoLN. Seamless only — no Manufacturing Types (SML / WLD / HCW) product-form split on this page.

Chemical Composition of SA213 UNS S31002

Two chemistry layers matter for UNS S31002 under ASME SA-213. Melting analysis is mandatory for every heat; product analysis on finished tube applies only when Supplementary Requirement wording or the purchase order invokes it through the general requirements (commonly ASTM A1016/A1016M), with tolerances typically from ASTM A480/A480M Table A1.1. The defining package for a reviewer is carbon ≤0.02% together with silicon ≤0.15%, chromium 24.0–26.0%, and nickel 19.0–22.0% — the same Cr–Ni window as TP310S, but with carbon and silicon far tighter than the ≤0.08% / ≤1.00% TP310S ceilings. Molybdenum ≤0.10% and nitrogen ≤0.10% are explicit caps on this row; phosphorus ≤0.020% and sulfur ≤0.015% are tighter than commodity 310S. There is no mandatory Nb or Ti band on the public row.

The tables below reproduce the melt limits for UNS S31002, the product-analysis limits from A480 Table A1.1 practice, and a short 310-family snapshot against TP310S and TP310H. Later SA-213 / A213 editions place austenitic stainless grades in Table 2 (older editions used Table 1); confirm the ordered edition on the purchase order. UNCERTAIN: exact edition year and stainless chem table number on the ordered Code Book text.

Melting analysis (heat / ladle analysis)

Element UNS S31002 melting analysis
Carbon (C) ≤ 0.02
Manganese (Mn) ≤ 2.00
Phosphorus (P) ≤ 0.020
Sulfur (S) ≤ 0.015
Silicon (Si) ≤ 0.15
Chromium (Cr) 24.0 – 26.0
Nickel (Ni) 19.0 – 22.0
Molybdenum (Mo) ≤ 0.10
Nitrogen (N) ≤ 0.10
Niobium (Nb) … (no requirement)
Titanium (Ti) … (no requirement)

Source: public SA-213 / A213 stainless chemistry table for UNS S31002 (same grade text family; public A213/A213M − 13 excerpt). Carbon and silicon ceilings must both appear on the certificate; an MTC that only shows “310S chemistry” is incomplete for S31002. Where ellipses appear, the ordered edition sets no requirement for that element. Nitrogen analysis method is by agreement when N is reported (Footnote B practice).

Product analysis — A480/A480M Table A1.1 tolerances applied

Element Melting Tolerance (A480 A1.1) Product analysis limit
Carbon (C) ≤ 0.02 0.005 over ≤ 0.025
Manganese (Mn) ≤ 2.00 0.04 over ≤ 2.04
Phosphorus (P) ≤ 0.020 0.005 over ≤ 0.025
Sulfur (S) ≤ 0.015 0.005 over ≤ 0.020
Silicon (Si) ≤ 0.15 0.05 over ≤ 0.20
Chromium (Cr) 24.0 – 26.0 0.25 under / over 23.75 – 26.25
Nickel (Ni) 19.0 – 22.0 0.15 under / 0.20 over 18.85 – 22.20
Molybdenum (Mo) ≤ 0.10 0.02 over ≤ 0.12
Nitrogen (N) ≤ 0.10 0.01 over ≤ 0.11

Product analysis is not automatic — order it when the project needs finished-tube chemistry, especially the low-carbon and low-silicon ceilings. UNCERTAIN: A480 product-tolerance digits should be confirmed against the ordered A480 edition if the PO makes product analysis contractual.

310-family snapshot — S31002 / TP310S / TP310H

Element S31002 TP310S (S31008) TP310H (S31009)
C ≤ 0.02 ≤ 0.08 0.04 – 0.10
Si ≤ 0.15 ≤ 1.00 ≤ 1.00
Cr 24.0 – 26.0 24.0 – 26.0 24.0 – 26.0
Ni 19.0 – 22.0 19.0 – 22.0 19.0 – 22.0
Mo ≤ 0.10 … …
N ≤ 0.10 … …

Reading tip: a heat that clears TP310S still fails S31002 if carbon sits above 0.02% or silicon sits near 1%. Do not accept a verbal “low-C 310” shop note as proof that the MTC prints S31002 with the C and Si ceilings satisfied.

Mechanical Properties of SA213 UNS S31002

Table 4 of the public SA-213 / A213 grade text family sets UNS S31002 tensile strength at 73 ksi [500 MPa] minimum and yield (0.2% offset) at 30 ksi [205 MPa] minimum — note the tensile floor is two ksi below TP310S / TP310H’s 75 ksi under the same product standard. Elongation in 2 in. or 50 mm is 35% minimum, and hardness is capped at 192 HBW / 200 HV or 90 HRB. A TP310S tensile-only certificate does not clear S31002, and an S31002 heat does not automatically dual-certify to TP310S on tensile alone even when chemistry overlaps are checked carefully.

Property UNS S31002 requirement (Table 4)
Tensile strength, min 73 ksi [500 MPa]
Yield strength (0.2% offset), min 30 ksi [205 MPa]
Elongation in 2 in. or 50 mm, min 35%
Hardness, max 192 HBW / 200 HV or 90 HRB
Grain size No mandatory ASTM grain-size number (unlike TP310H)

Room-temperature tensile is slightly below TP310S; the reason to order S31002 is the low-C / low-Si chemistry for IGC-leaning 25-20 duty, not a higher Table 4 floor. S31002 has no mandatory ASTM grain-size number in the heat-treatment column — unlike TP310H. If a project datasheet asks for an E112 grain-size report, put that supplementary requirement on the purchase order. Mechanical property requirements generally do not apply to tubing smaller than 1/8 in. [3.2 mm] ID or thinner than 0.015 in. [0.4 mm] wall. Flattening and flaring follow the general requirements for the ordered size.

Dimensions and Tolerances

Dimensional supply for ASME SA213 UNS S31002 is tube language — outside diameter × wall thickness (minimum wall or average wall) and, commercially, BWG / gauge — not ASME B36.19 pipe schedules as the primary size story. Usual SA-213 sizes run from about 1/8 in. [3.2 mm] inside diameter to 5 in. [127 mm] outside diameter, with minimum wall from about 0.015 to 0.500 in. [0.4 to 12.7 mm]; other diameters may be furnished when all other requirements are met.

Boiler and heat-exchanger datasheets that pick low-C / low-Si S31002 usually assume minimum wall — state wall basis on the purchase order. Outside-diameter and wall variations follow the general requirements invoked by SA-213 (commonly ASTM A1016/A1016M). The low-C / low-Si package does not change the dimensional tolerance tables; it changes which heat clears the grade stamp.

Item Typical SA213 UNS S31002 dimensional practice
Product form Seamless only (cold-finished or hot-finished)
Usual size band ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD; wall ~0.015–0.500 in. [0.4–12.7 mm]
Wall basis Minimum wall (common for boiler / HX datasheets) or average wall if PO says so
OD / wall tolerance Per general requirements (commonly A1016/A1016M) for the ordered finish
Length Straight random / cut-to-length; U-bend by agreement

BWG / gauge callouts are accepted on enquiry; certificates should still show OD and wall in inch or millimetre units. U-bends and polished ID finishes are commercial options — they do not replace the carbon and silicon ceiling checks.

Equivalent Grades

Equivalence talk for S31002 should start from the Code Book product standard and the UNS, not from a casual “low-C 310” nickname. ASME SA-213 UNS S31002 is the governing designation on this page. ASTM A213 UNS S31002 is the separate ASTM twin used when dual marking or a non-Code purchase is agreed — it is not a substitute lead standard for an SA-213 order. Related 310-family grades (TP310S, TP310H, TP310Cb, TP310MoLN) are sister options under the same hub family, not automatic dual stamps.

Designation Notes
ASME SA-213 / SA-213M UNS S31002 Governing Code Book seamless boiler / HX tube product standard for this article
UNS S31002 Unified number — no TP letter (Footnote C)
Low-C 310 / 25-20 low-Si (commercial) Shop names — do not replace S31002 on the MTC
ASTM A213 UNS S31002 Separate ASTM product specification — dual-mark only when the PO asks; twin page A213 UNS S31002
Related TP310S SA213 TP310S — same Cr–Ni window, looser C/Si ceilings, 75 ksi tensile
Related TP310H SA213 TP310H — H-grade carbon + grain-size controls
Related plate A240 / SA240 flat product in the 310 family — order plate and tube under their own standards

Hub entry point: SA213/SA213M. When a bill of materials only says “low-C 310,” ask whether C ≤0.02% and Si ≤0.15% are actually required before shipping S31002 or a TP310S alternative.

Heat Treatment and Delivery Condition

UNS S31002 under ASME SA-213 is furnished solution treated at a minimum of 1900 °F [1040 °C], then quenched in water or cooled rapidly by other means. Public Table 3 OCR places a Footnote F marker near the S31002 row; TP310S clearly carries Footnote F on the same 1900 °F minimum. UNCERTAIN: confirm ordered-edition footnote attachment for S31002 — if Footnote F applies, quench capability must be sufficient to prevent carbide re-precipitation as demonstrable by A262 Practice E capability, and the manufacturer need not run the test unless the purchase order specifies it (Supplementary Requirement S4).

Cold-finished versus hot-finished is a process and dimensional route, not a substitute for the anneal. Low-carbon 310-family tube still needs a thorough solution treatment and rapid cool so the ≤0.02% carbon advantage is not wasted by slow cooling through the sensitization range. Delivery condition for SHH STEEL S31002 is solution annealed and pickled (or bright annealed by agreement), with anneal temperature and quench method on the EN 10204 3.1 certificate. Straightening, cutting, and end finishing follow heat treatment.

Unlike SA213 TP310H, S31002 has no mandatory ASTM grain-size number in the heat-treatment column. If a project datasheet asks for an E112 grain-size report, put that supplementary requirement on the purchase order rather than assuming base SA-213 includes it.

Corrosion Resistance

S31002 under ASME SA-213 is selected primarily for the low-carbon / low-silicon path inside the 25Cr–20Ni oxidation window — IGC-leaning and clean 310-family duty where TP310S carbon or silicon ceilings are too loose — not as a general wet-chloride upgrade over TP316. The ≤0.02% carbon and ≤0.15% silicon ceilings support reduced sensitization risk relative to commodity 310S in many heat-exchanger and boiler services that still want the 24–26 Cr / 19–22 Ni oxidation band.

Where a datasheet mixes “low-C 310” with aggressive aqueous chlorides or seawater-side condensates, ask whether the service is actually looking for a molybdenum-bearing or duplex tube instead of a low-Si austenitic. SHH STEEL will not treat a chromium PMI peak alone as proof of aqueous corrosion suitability — chemistry, heat treatment, and the intended medium have to be read together. For H-grade carbon and grain-size controls open SA213 TP310H; for Nb stabilization open SA213 TP310Cb.

Applications of SA213 UNS S31002 Tube

Typical ASME SA213 UNS S31002 placements are Code-stamped boiler, superheater, and heat-exchanger tubes where the material list names S31002 or explicitly requires C ≤0.02% with Si ≤0.15% inside the 25-20 Cr–Ni window — not generic “310S” or “310H” replacements. IGC-sensitive HX bundles and clean 310-family furnace tubes that already distinguish low-C / low-Si chemistry from TP310S are the natural fit.

When the enquiry only says “low-C 310” without UNS language, confirm whether the buyer actually needs SA213 TP310S, SA213 TP310H, or a Mo-bearing 310-family grade before substituting. SHH STEEL quotes S31002 when the enquiry names the UNS or the low-C / low-Si package explicitly.

Weldability

S31002 welds as a low-carbon, low-silicon 25Cr–20Ni austenitic. Filler selection should respect the low-C / low-Si chemistry rather than copying a high-silicon ER310 procedure without review. Matching or near-matching low-carbon austenitic fillers with adequate chromium and nickel are the usual starting point; confirm chemistry against the WPS when the project treats C and Si ceilings as contractual on the weld metal as well as the tube.

Autogenous welds and thin-wall HX joints need heat-input control to protect the as-annealed low-carbon condition near the HAZ. Post-weld heat treatment is not a default SA-213 requirement for this grade — if the vessel code or the buyer wants a separate resolution anneal after welding, write that as a negotiated step. SHH STEEL can coordinate weld coupons when the PO asks.

Surface Finishes

Standard mill delivery for ASME SA213 UNS S31002 is solution annealed and pickled, leaving a clean matte finish suitable for boiler and heat-exchanger tube duty. Bright annealing is available by agreement when OD appearance or polish steps favor it.

ID/OD polish and U-bend conditioning are commercial additions — they do not replace the carbon and silicon ceiling checks. End caps and dry export packaging matter more than paint on pickled stainless. SHH STEEL notes the ordered surface route on the packing list and aligns it with the MTC finish description for receiving inspection.

Inspection and Testing

Base ASME SA-213 testing for UNS S31002 includes heat analysis (C ≤0.02%, Si ≤0.15%, Cr 24.0–26.0%, Ni 19.0–22.0%, Mo ≤0.10%, N ≤0.10%, P ≤0.020%, S ≤0.015%), tension tests to the 73/30 ksi floors with 35% elongation, hardness to 192 HBW / 90 HRB, and flattening / flaring tests for the ordered size. Hydrostatic testing or NDE follows the path selected on the purchase order.

Certificate reviewers should confirm the carbon and silicon ceilings rather than trusting a “low-C 310” shop nickname or a TP310S-family PMI without C ≤0.02% and Si ≤0.15%. Product analysis, when ordered, applies A480 tolerances with digits noted as UNCERTAIN above if the ordered A480 edition differs. A262 Practice E applies only when S4 is named and Footnote F applies on the ordered edition. EN 10204 3.1 is default; 3.2 when required. Dual SA-213/A213 names appear only when dual marking was ordered.

Packaging and Shipping

S31002 tube leaves SHH STEEL bundled, capped or end-protected, and tagged for export or domestic delivery according to length mix and bend form. Bundle tags repeat ASME SA-213 UNS S31002, heat number, size, and wall basis so receivers can match the 3.1 certificate — including C and Si — without opening every bundle.

Export packing uses seaworthy bundling appropriate for pickled stainless. Marking follows SA-213 and any dual-mark text the PO adds, referencing A213 UNS S31002 only when dual ASTM marking was ordered. The commercial “low-C 310” nickname may appear in packing notes for routing, but the stencil and MTC still carry UNS S31002.

Why Choose SHH STEEL

SHH STEEL treats ASME SA213 UNS S31002 as a Code Book low-carbon low-silicon 25Cr–20Ni product with enforceable C ≤0.02%, Si ≤0.15%, Cr 24–26%, Ni 19–22%, Mo ≤0.10%, N ≤0.10%, P ≤0.020%, S ≤0.015%, 73/30 ksi tensile, 35% elongation, hardness, and marking rules — not as “310S with a low-carbon sticker” checked only by a Cr PMI peak. Enquiry review verifies the carbon and silicon ceilings before release.

That stops silent substitution with TP310S or TP310H heats on datasheets that actually require S31002. We keep SA-213 and A213 independent, dual-mark only on request, and put C and Si on the 3.1 certificate so inspectors can verify the grade. The commercial “low-C 310” nickname is allowed for routing — it never replaces S31002 on the MTC.

Cross-links: SA213 TP310S, SA213 TP310H, SA213 TP310Cb, hub SA213/SA213M.

Supply Capability

SHH STEEL can supply ASME SA213 UNS S31002 stainless steel tube against the edition and finish route named on your enquiry. The capability table below summarizes sizes, finishes, and documents we regularly quote, followed by the Stock / Available sizes map for low-C / low-Si 310-family boiler and heat-exchanger tube.

Item SHH STEEL capability for UNS S31002
Standard ASME SA213 / SA213M (dual A213 marking on request)
Grade UNS S31002 (no TP letter)
Product form Seamless only — cold-finished and hot-finished
Size Typical OD × min wall (or average wall) in the SA-213 usual band; other diameters by agreement
Wall / gauge Minimum wall or average wall; BWG / gauge callouts accepted on enquiry
Length Cut-to-length for boiler / HX bundles; U-bend by agreement
Documentation EN 10204 3.1 MTC with C / Si ceilings; S4 A262 / witness on request
Trade terms FOB / CFR / CIF / EXW and other agreed Incoterms

Stock / Available sizes

SHH STEEL quotes S31002 against a stock-and-mill enquiry range rather than a frozen SKU or tonnage list. Representative OD × wall / BWG combinations below are an enquiry map for low-C / low-Si 310-family boiler and heat-exchanger tube — confirm live availability and cut lengths on the RFQ.

OD (in.) Typical wall / BWG enquiry band Notes
1/2 – 1 BWG 16–12 / ~0.065–0.109 in. Small HX / instrument sizes
1-1/4 – 2 BWG 14–10 / ~0.083–0.134 in. Common boiler / HX band
2-1/2 – 3 0.120 – 0.250 in. min wall Heavier HX / boiler wall
3-1/2 – 5 0.180 – 0.300 in. min wall Upper usual SA-213 OD by agreement

Send OD × wall (or BWG), wall basis, quantity, length mix, finish route, and any dual-mark or A262 needs with the RFQ so we can align mill capacity to the low-C / low-Si package on the first reply.

FAQ

Is ASME SA-213 the same as ASTM A213 for UNS S31002?
No. ASME SA-213 / SA-213M is the ASME Code Book adoption; ASTM A213 / A213M is the separate ASTM product specification. Chemistry — including C ≤0.02%, Si ≤0.15%, Cr 24.0–26.0%, Ni 19.0–22.0%, Mo ≤0.10%, and N ≤0.10% — tensile 73/30 ksi, elongation 35%, and hardness floors align in the shared grade text family, but the standards remain independent documents. Dual marking is a purchase-order option, not proof that the two titles are one standard.
Does ASME SA213 UNS S31002 have a TP grade letter?
No. S31002 appears in the stainless chemistry table without a TP letter (Footnote C practice). Order and mark by UNS S31002 under ASME SA-213 / SA-213M. Do not invent a “TP31002” stencil or assume the grade dual-stamps as TP310S or TP310H. The purchase order and MTC should carry the UNS designation explicitly so inspectors can match C, Si, and tensile to the correct row.
How does S31002 differ from TP310S under SA-213?
S31002 caps carbon at ≤0.02% and silicon at ≤0.15%, with Mo ≤0.10%, N ≤0.10%, tighter P/S, and a 73 ksi tensile floor. TP310S allows C ≤0.08% and Si ≤1.00% with a 75 ksi floor and no mandatory Mo/N caps on the public row. Same Cr–Ni oxidation window, different chemistry and tensile story. A heat that clears TP310S still fails S31002 if carbon or silicon sits above the S31002 ceilings.
How does S31002 differ from TP310H under SA-213?
TP310H requires carbon in a 0.04–0.10% band and carries mandatory ASTM grain-size controls for creep-oriented H-grade service. S31002 is the opposite carbon story — ≤0.02% — with no mandatory grain-size number and a 73 ksi tensile floor. They are not dual stamps. If the datasheet wants H-grade carbon and grain size, open TP310H; if it wants low-C / low-Si 25-20, open S31002.
What hardness limit applies to ASME SA213 UNS S31002 tube?
Table 4 caps S31002 hardness at 192 HBW / 200 HV or 90 HRB — the same ceiling as TP310S. Hardness is checked together with the 73/30 ksi tensile set and 35% elongation. A hardness result alone does not prove low-C / low-Si compliance; certificate reviewers should still read the carbon and silicon ceilings on the MTC.
What heat treatment applies to SA213 UNS S31002?
Solution treatment at a minimum of 1900 °F [1040 °C] followed by rapid cooling is the public path. Footnote F attachment on the ordered edition is UNCERTAIN for this row — if it applies, quench capability must be sufficient to prevent carbide re-precipitation as demonstrable by A262 Practice E when that test is ordered (S4). There is no mandatory ASTM grain-size number for this grade, unlike TP310H.
Should I order minimum wall or average wall for S31002?
Boiler and heat-exchanger datasheets that pick S31002 usually assume minimum wall. Average wall is acceptable when the purchase order says so and the general requirements for the ordered finish are applied. State wall basis, OD × wall or BWG, and length mix on the RFQ so the mill does not default to a basis your inspector will reject at receiving.
Is S31002 suitable for wet chloride heat-exchanger service?
Not as a default upgrade. S31002 is framed for the low-C / low-Si path inside the 25Cr–20Ni oxidation window. Aggressive aqueous chlorides usually need molybdenum-bearing, duplex, or other project-specified alloys instead of a low-Si austenitic. Ask for a corrosion review before substituting S31002 into a wet-chloride HX datasheet that never named the UNS.
Does ASME SA213 UNS S31002 cover welded or HCW tube?
No. ASME SA-213 for this stainless series is a seamless boiler, superheater, and heat-exchanger tube product standard. SHH STEEL supplies S31002 as seamless cold-finished or hot-finished tube only. Welded (WLD) or heavily cold-worked welded (HCW) manufacturing types are outside this page’s product form and are not offered as a Manufacturing Types split under the SA213 UNS S31002 listing.
Can SHH STEEL dual-certify SA-213 and A213 for S31002?
Yes, when the purchase order asks for dual marking and the heat meets both product standards’ grade text for UNS S31002. Dual marking is a documentation and stencil option — it does not merge the two standards into one title. For non-Code purchases that only want the ASTM twin, see A213 UNS S31002; for Code-led work, keep SA-213 as the lead standard on the PO.
Why is the tensile floor for S31002 lower than TP310S?
Table 4 sets S31002 at 73 ksi [500 MPa] tensile versus 75 ksi for TP310S / TP310H under the same product standard. That two-ksi difference is intentional grade text — do not invent a single “75 ksi for all 310-family” rule. The reason to order S31002 is the low-C / low-Si chemistry, not a higher tensile floor. A TP310S tensile-only certificate does not clear S31002.

Conclusion

ASME SA213 UNS S31002 is the low-carbon low-silicon 25Cr–20Ni seamless stainless steel tube grade for Code boiler, superheater, and heat-exchanger service when C ≤0.02%, Si ≤0.15%, Cr 24.0–26.0%, Ni 19.0–22.0%, Mo ≤0.10%, N ≤0.10%, P ≤0.020%, S ≤0.015%, a 73/30 ksi tensile floor with 35% elongation, hardness max 192 HBW / 90 HRB, and a 1900 °F solution anneal are required together. SHH STEEL supplies cold-finished and hot-finished seamless tube in the usual OD × wall / BWG band with EN 10204 3.1 MTCs that report the C and Si ceilings. The commercial “low-C 310” nickname does not replace UNS S31002 on the certificate. For quotations and technical review, contact admin@steelspecs.com.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X