ASME SA213 TP304LN / UNS S30453 seamless boiler, superheater and heat-exchanger tube — low-carbon nitrogen-strengthened 18-8 with C ≤0.035% (Footnote D to 0.040%), N 0.10–0.16%, Cr 18.0–20.0%, Ni 8.0–11.0%, and a 75/30 ksi tensile floor with hardness max 192 HBW / 90 HRB. Solution anneal 1900 °F. SHH STEEL supplies cold-finished and hot-finished seamless tube with EN 10204 3.1 MTCs reporting C and N.
Grade
TP304LN / UNS S30453
Standard
ASME SA213 / SA213M
Product form
Seamless boiler / superheater / heat-exchanger tube (cold-finished and hot-finished)
Size
Typical OD × min wall (or average wall) within ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD and ~0.015–0.500 in. [0.4–12.7 mm] wall; other diameters by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is ASME SA213 TP304LN Stainless Steel Tube

ASME SA-213 / SA-213M is the ASME Boiler and Pressure Vessel Code Book adoption of the seamless ferritic and austenitic alloy-steel boiler, superheater, and heat-exchanger tube product standard. Grade TP304LN under that Code Book text is the low-carbon, nitrogen-strengthened 18-8 austenitic listed as UNS S30453, with melting limits of carbon ≤0.035% (Footnote D allowing ≤0.040% on small-diameter or thin-wall tube that needs many drawing passes), chromium 18.0–20.0%, nickel 8.0–11.0%, and nitrogen 0.10–0.16%. When a Code-stamped boiler, superheater, or heat-exchanger datasheet calls for SA-213 TP304LN, the purchase order and mill test certificate should carry the ASME designation together with both the low-carbon ceiling and the nitrogen band — not a borrowed TP304L chemistry without nitrogen, and not a TP304N heat that still sits at 0.08% carbon.

SHH STEEL can supply ASME SA213 TP304LN stainless steel tube as seamless cold-finished and hot-finished product in the usual boiler and heat-exchanger OD × wall / BWG band, documented on EN 10204 3.1 mill test certificates that report the full ladle chemistry — including carbon against the 0.035% (or Footnote D 0.040%) path and nitrogen in the 0.10–0.16% band — plus the tensile and hardness acceptance set. Dual SA-213 / A213 marking on the same lengths is available only when the purchase order asks for both independent standards; ASME SA213 and ASTM A213 remain separate documents even when the grade text aligns closely for a referenced edition. Browse the grade family on the SA213/SA213M hub.

Commercially the same tube is still called 304LN, S30453 boiler tube, low-carbon nitrogen 304 HX tube, or SA213 304LN tube; none of those phrases replace the ASME grade on the stencil or MTC. Sister grades under the same ASME standard include SA213 TP304L, SA213 TP304N, SA213 TP304, SA213 TP304H, and SA213 TP316LN. SA-213 covers seamless tube only — there is no welded or HCW manufacturing type under this product standard — so cold-finished versus hot-finished seamless route is the process choice, not a WLD/HCW stencil letter. For the sister ASTM product page on the same UNS, see A213 TP304LN.

Chemical Composition of SA213 TP304LN

Two chemistry layers matter for TP304LN under ASME SA-213. The melting (heat or ladle) analysis is mandatory for every heat under the stainless chemistry table; product analysis on finished tube applies only when Supplementary Requirement wording or the purchase order invokes it through the general requirements path (commonly ASTM A1016/A1016M), with product-analysis tolerances typically taken from ASTM A480/A480M Table A1.1. Nitrogen analysis method is a matter of agreement between purchaser and producer (Footnote B language in the public grade text) — put the agreed method on the PO when N reporting must follow a named technique. Footnote D is contractual for this grade: for small diameter or thin walls requiring many drawing passes, a carbon maximum of 0.040% may apply instead of 0.035%. SHH STEEL reports the actual ladle values — and the product values when ordered — and does not advertise unpublished tighter catalogue windows.

The tables below reproduce the melt limits for TP304LN / UNS S30453 and the product-analysis limits that result from applying A480 Table A1.1 tolerances. Values are maximum unless a range is shown; an ellipsis (…) means the ordered edition sets no requirement for that element. UNCERTAIN: exact SA-213 / A213 edition year and whether austenitic grades sit in Table 1 or Table 2 of that edition; Footnote D OD/wall trigger wording for the 0.040% carbon path; A480 product-tolerance digits for the 0.10–0.16% nitrogen band if product analysis is contractual; nitrogen analysis method by agreement — confirm the ordered edition on the purchase order before treating secondary catalogues as acceptance text.

Melting analysis (heat / ladle analysis)

Source: public SA-213 / A213 grade-table summaries for TP304LN / UNS S30453. Confirm the ordered ASME edition on the purchase order.

Element TP304LN (UNS S30453) melting analysis
Carbon (C) ≤ 0.035 (Footnote D: ≤ 0.040 for small OD / thin wall with many drawing passes)
Manganese (Mn) ≤ 2.00
Phosphorus (P) ≤ 0.045
Sulfur (S) ≤ 0.030
Silicon (Si) ≤ 1.00
Chromium (Cr) 18.0 – 20.0
Nickel (Ni) 8.0 – 11.0
Molybdenum (Mo) … (no requirement)
Nitrogen (N) 0.10 – 0.16

Product analysis — A480/A480M Table A1.1 tolerances applied

Element Melting Tolerance (A480 A1.1) Product analysis limit
Carbon (C) ≤ 0.035 0.01 over ≤ 0.045
Manganese (Mn) ≤ 2.00 0.04 over ≤ 2.04
Phosphorus (P) ≤ 0.045 0.010 over ≤ 0.055
Sulfur (S) ≤ 0.030 0.005 over ≤ 0.035
Silicon (Si) ≤ 1.00 0.05 over ≤ 1.05
Chromium (Cr) 18.0 – 20.0 0.20 under / over 17.80 – 20.20
Nickel (Ni) 8.0 – 11.0 0.10 under / 0.15 over 7.90 – 11.15
Nitrogen (N) 0.10 – 0.16 0.01 under / 0.02 over 0.09 – 0.18

Read carbon and nitrogen together. Holding C ≤0.035% (or ≤0.040% under Footnote D) reduces chromium-carbide precipitation at grain boundaries during welding or slow cooling through the sensitizing range, which is why LN exists beside standard-carbon TP304N. The 0.10–0.16% nitrogen band then supports austenite stability and contributes to the tensile floor the mechanical table assigns this grade. Unlike SA213 TP304N, which keeps C ≤0.08% and lifts strength to 80/35 ksi, TP304LN keeps the low-carbon path and sits on the 75/30 ksi mechanical row — so buyers who need both as-welded IGC resistance and nitrogen should not assume the N-grade tensile pair applies.

When product analysis is ordered, finished tube may read up to C 0.045%, Mn 2.04%, P 0.055%, S 0.035%, and Si 1.05%, with Cr 17.80–20.20%, Ni 7.90–11.15%, and N 0.09–0.18%. Those are the only product limits we quote from the A480 A1.1 path for this grade. Put any tighter project carbon ceiling, Footnote D applicability note, or nitrogen floor on the purchase order before the heat is selected.

Mechanical Properties of SA213 TP304LN

ASME SA-213 sets the tensile acceptance floor for TP304LN at 75 ksi [515 MPa] tensile strength and 30 ksi [205 MPa] yield strength (0.2% offset), with elongation of 35% minimum in 2 in. or 50 mm. Hardness is capped at 192 HBW / 200 HV or 90 HRB — the same hardness ceiling carried by TP304 and TP304L. That combination matters commercially: nitrogen is present for austenite stability and modest strength support, but the Code Book mechanical row for LN stays on the 75/30 pair rather than the 80/35 pair reserved for standard-carbon TP304N. Every lot sampled under the edition’s specimen rules must meet those numbers after the final solution treatment.

Source: public SA-213 / A213 mechanical-table summaries for TP304LN / UNS S30453 (commonly Table 4). Mechanical property requirements do not apply to tubing smaller than 1/8 in. [3.2 mm] inside diameter or thinner than 0.015 in. [0.4 mm] wall.

Property TP304LN requirement
Tensile strength, min 75 ksi [515 MPa]
Yield strength (0.2% offset), min 30 ksi [205 MPa]
Elongation in 2 in. or 50 mm, min 35%
Hardness, max 192 HBW / 200 HV or 90 HRB

Flattening and flaring tests sit beside tension and hardness on a lot basis. Design calculations should use the 75/30 ksi pair unless the purchase order states higher guaranteed values the mill has accepted in writing. Do not assume a TP304L certificate automatically clears TP304LN — a heat without the nitrogen band is a different grade even when carbon is low. When the datasheet needs the higher 80/35 ksi nitrogen-strengthened floor and can accept C ≤0.08%, open SA213 TP304N; when creep-range H-grade carbon and grain-size controls are required, open SA213 TP304H.

Dimensions and Tolerances

Dimensional supply for ASME SA213 TP304LN is tube language — outside diameter × wall thickness (minimum wall or average wall) and, commercially, BWG / gauge — not ASME B36.19 pipe schedules as the primary size story. The sizes usually furnished under SA-213 run from about 1/8 in. [3.2 mm] inside diameter to 5 in. [127 mm] outside diameter, with minimum wall from about 0.015 to 0.500 in. [0.4 to 12.7 mm]; tubing with other diameters may be furnished when all other requirements of the specification are met. Footnote D’s carbon relief for small OD / thin wall with many drawing passes is a chemistry accommodation, not a free pass on dimensional tolerances — still name the wall basis on the purchase order.

Outside-diameter and wall variations follow the general requirements invoked by SA-213 (commonly ASTM A1016/A1016M), with cold-finished and hot-finished routes carrying different practical bands. Cold-finished tubes commonly hold tighter OD control; hot-finished tubes allow wider OD and wall windows. Permissible variations from a specified average wall for cold-finished tube are often summarized as ±10% of the specified average wall, while minimum-wall product is accepted to the minimum-wall tables rather than a symmetric ± window. Confirm the exact general-requirements rows for the OD and finish route on the ordered edition.

Item Typical SA213 TP304LN dimensional practice
Product form Seamless only (cold-finished or hot-finished)
Usual size band ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD; wall ~0.015–0.500 in. [0.4–12.7 mm] min (or average wall if PO says so)
Wall basis Minimum wall (default commercial practice) or average wall when specified
OD / wall tolerances Per general requirements for the finish route and size; cold-finished average wall often ±10%
Length Cut lengths for HX / boiler bundles, or mill random lengths by agreement
Footnote D note Small OD / thin wall with many draws may use C max 0.040% — chemistry, not a size exemption
Secondary size note ASME B36.19 schedules may appear only when a buyer asks for a pipe-schedule cross-reference — not as the primary SA-213 size callout

Put the cut list, U-bend or straight-tube preference, end preparation, and any Footnote D applicability note on the enquiry so mill and stock lengths can be mixed efficiently. Nitrogen-bearing low-carbon 18-8 still work-hardens during U-bending, so bend radius and any post-bend anneal should be discussed early. Minimum wall is a first-class SA-213 concept: if the datasheet assumes average wall, say so explicitly before the heat is rolled.

Equivalent Grades

Equivalence language around TP304LN tube is often looser than a Code or heat-exchanger purchase order can afford. ASME SA-213 Grade TP304LN / UNS S30453 is the governing designation for this article; EN and JIS wrought names that point to low-carbon nitrogen-bearing 18-8 families are not automatic substitutes on an SA-213 mill test certificate. When a datasheet says “equivalent to 304LN,” confirm which product standard, carbon path, nitrogen band, tensile floor, and heat-treatment clause the mill will actually certify.

Designation Notes
ASME SA-213 / SA-213M Grade TP304LN Governing ASME Code Book seamless boiler / HX tube product standard for this article
UNS S30453 Unified number listed with the low-carbon nitrogen-strengthened grade chemistry
ASTM A213 TP304LN Separate ASTM International product specification — dual-mark only when the PO asks; see A213 TP304LN
Related L sister SA213 TP304L for low carbon without the nitrogen band
Related N sister SA213 TP304N for C ≤0.08% + N 0.10–0.16% at the 80/35 ksi floor
Related plate A240 / SA240 flat product in the same UNS family — order plate and tube under their own product standards

ASTM A213 TP304LN is the separate ASTM product specification sharing the same grade family; dual SA-213/A213 marking is a purchase-order option, not a claim that the two standards are one document. Compare standard SA213 TP304, H-grade SA213 TP304H, and molybdenum LN sisters on their own ASME pages before swapping grades in a tube bundle.

Heat Treatment and Delivery Condition

TP304LN under ASME SA-213 is furnished solution treated at a minimum of 1900 °F [1040 °C], then quenched in water or cooled rapidly by other means at a rate sufficient to prevent carbide reprecipitation. That heat-treatment row applies to both cold-finished and hot-finished seamless tube. Low carbon reduces sensitization risk after welding, but it does not excuse a skipped or under-cooled solution treatment at the mill — nitrogen still needs to stay in solid solution for the austenite and tensile story to remain meaningful.

Cold-finished versus hot-finished is a process and dimensional route, not a substitute for the anneal. Delivery condition for SHH STEEL TP304LN is solution annealed and pickled (or bright annealed by agreement), with heat-treatment temperature and quench method stated on the EN 10204 3.1 certificate. Straightening, cutting, and end finishing follow heat treatment.

When Supplementary Requirement language for intergranular-corrosion capability (commonly tied to ASTM A262 Practice E) is ordered, the corrosion test report travels with the heat-treatment record. H-grade grain-size rules do not rewrite the TP304LN path — use SA213 TP304H when the datasheet calls for H-grade carbon and grain-size controls, or SA213 UNS S30432 when Cu–Nb–N USC boiler framing is required.

Corrosion Resistance

TP304LN’s chromium-rich passive film behaves broadly like other 18-8 grades in oxidizing process fluids, clean steam-side and water-side duties, and many organic media that do not lean heavily on chlorides. The low-carbon ceiling is the corrosion-related commercial point: it improves resistance to intergranular attack after tube-to-tubesheet welding or after sensitizing thermal cycles compared with standard-carbon TP304N. Nitrogen can improve localized corrosion resistance modestly in some chloride-leaning assessments, but ASME SA-213 does not publish a PREN or corrosion-rate table for the grade, and buyers facing seawater-leaning cooling water usually still step up to SA213 TP316L / SA213 TP316LN or higher.

Selection remains engineering judgment against fluid, temperature, velocity, and inspection philosophy inside the boiler or exchanger. When a specification calls for ASTM A262 Practice E, write that Supplementary Requirement onto the purchase order so the test is contractual rather than assumed from a verbal “full certs” note — even though the low-carbon chemistry already leans toward as-welded IGC resistance. SHH STEEL will not rank TP304LN as equal to 316 in chlorides — low carbon plus nitrogen is not a molybdenum substitute.

Applications of SA213 TP304LN Tube

Because TP304LN combines a low-carbon melt path with a mandatory nitrogen band under SA-213, it shows up where designers want as-welded intergranular resistance and nitrogen-supported austenite in utility heat exchangers, process HX duty, and moderate-temperature boiler circuits that do not need H-grade creep framing. The table below pairs typical application areas with a selection note so the grade is chosen for the fluid, temperature, and fabrication route — not only for the familiar “304LN” name on the BOM.

Application area Typical use of TP304LN tube Selection note
As-welded heat exchangers Seamless HX tubes where tube-to-tubesheet joints enter service without a full re-anneal Low-C base metal with nitrogen-supported austenite; confirm Footnote D if many draws on small OD/thin wall
Process / chemical exchangers Oxidizing or mild corrosive tube-side circuits needing better IGC resistance than TP304N Prefer TP316L/TP316LN if chlorides dominate
Utility condensers / coolers (low chloride) Straight and U-bend tubes in clean cooling circuits Clear chloride review before substituting for molybdenum grades
Boiler / moderate-temperature steam Seamless generating and process steam tubing ordered to SA-213 For creep-critical H-grade service open TP304H, not TP304LN
Programs needing LN + strength documentation When PO wants both C ≤0.035% and N 0.10–0.16% on one MTC Do not borrow the TP304N 80/35 ksi row — LN stays on 75/30
General corrosive tube duty Seamless tube where SA-213 documentation is preferred over pipe forms Do not substitute SA312 / A312 pipe paperwork for SA-213 tube acceptance

For standard-carbon nitrogen strength at 80/35 ksi open SA213 TP304N; for creep-range H-grade boiler tubing open SA213 TP304H; for chloride-rich cooling water move to the molybdenum grades on the same SA213/SA213M hub.

Weldability

TP304LN tube welds with matching or near-matching austenitic filler for tube-to-tubesheet joints, attachment welds, and fabrication joins. Common practice uses ER308L (or equivalent covered electrodes) under a qualified WPS so the weld metal carbon stays aligned with the low-carbon base metal story; some fabricators still use ER308 when the WPS already qualifies it, but ER308L is the usual preference for LN tube. Heat input control, interpass limits, and post-weld cleaning remain the fabricator’s responsibility under the applicable boiler or pressure-vessel Code — SA-213 governs the seamless tube product, not the field or shop weld procedure.

Because SA213 TP304LN is seamless, there is no mill longitudinal weld to radiograph the way welded pipe standards describe. Focus inspection language on tube integrity (hydro or NDE of each length), tube-to-tubesheet joint quality, and any contractual corrosion test on the base metal. The low-carbon chemistry is why many owners choose LN for as-welded sensitizing service instead of relying on a perfect weld procedure alone to protect standard-carbon TP304N. Specify end preparation and surface finish on the tube PO when orbital or clean-service joins are planned, and note Footnote D applicability when many cold draws on small OD / thin wall change the carbon path.

Surface Finishes

Standard mill delivery for ASME SA213 TP304LN is solution annealed and pickled, leaving a clean matte finish suitable for most boiler and heat-exchanger tube duty. Bright annealing under protective atmosphere produces a smoother reflective surface used on some clean-process and instrumentation tube lines and must be called out because it changes the heat-treatment route. Light polish or specified Ra on the bore or OD is a commercial or service-center operation on top of SA-213 product, not automatic with the grade stamp.

When a hygienic or fouling-sensitive exchanger specification quotes an Ra maximum on the bore, put it on the tube purchase order with its own acceptance language and sampling plan. SHH STEEL stencils grade and heat treatment as standard requirements; polish, special OD grind, and passivation after fabrication remain commercial extras unless the contract says otherwise. End preparation (plain, slightly beveled, or as needed for tube expanding) should be ordered together with finish so receiving inspection shares one acceptance language.

Inspection and Testing

Base ASME SA-213 testing for TP304LN includes heat analysis (with carbon against the 0.035% or Footnote D 0.040% path and nitrogen reported in the 0.10–0.16% band), tension tests to the 75/30 ksi floor, hardness tests to the 192 HBW / 90 HRB maximum, flattening and flaring tests on a lot basis, and either hydrostatic testing or nondestructive electric testing of each length. The manufacturer may choose hydro versus NDE unless the purchase order fixes the method; both are acceptance routes inside the product standard, not informal upgrades. Marking includes the ASME designation, grade, size, heat number, and other clause-required data so receiving inspection can tie each length back to the MTC.

Supplementary Requirements commonly added on TP304LN tube orders are summarized below. Invoke them by number or clear purchase-order wording; mills will not assume product analysis or intergranular-corrosion testing from a verbal “full certs” note.

Option Purpose
Product analysis Confirms chemistry on finished tube (via general requirements / PO language)
Intergranular corrosion A262 Practice E (or agreed practice) as a contractual Supplementary Requirement for as-welded IGC confidence
Footnote D carbon note Clarifies when C max 0.040% applies for small OD / thin wall
Minimum vs average wall States which wall basis the size callout uses
Fixed hydro or NDE method Removes manufacturer’s option when the end user mandates one route
Third-party inspection / EN 10204 3.2 Witnessed testing and certificate when the project requires it

Lot definitions for continuous heat treatment or direct quench after hot forming follow the size-based lot sizes in SA-213; ask the mill to state lot identity clearly on the certificate so hardness and tension specimens map cleanly to the bundle you receive. An MTC that omits nitrogen or that reports C above the applicable Footnote D path without PO coverage is incomplete for S30453 — reject it before the heat leaves the mill.

Packaging and Shipping

TP304LN tube leaves SHH STEEL bundled, capped or end-protected, and tagged for export or domestic delivery according to the length mix and bend form on the order. Bundle tags repeat the ASME SA213 grade, OD × wall (or BWG), heat number, and PO reference so site receiving can check the shipment without opening every certificate packet first. U-bent tubes need extra cradle or case protection so bend radii and legs are not distorted in transit.

Export packing can be bare bundles, wrapped bundles, or wooden-cased lengths for bright-annealed, polished, or small-bore material. We ship under the Incoterms on the order acknowledgement — FOB, CFR, CIF, EXW, or other agreed terms. Inland trucking, bilingual destination marks, or project color coding for bundle tags should be stated on the enquiry beside the metallurgical notes.

Why Choose SHH STEEL

SHH STEEL treats ASME SA213 TP304LN as a Code Book product standard with enforceable chemistry, tensile, hardness, heat-treatment, and marking rules — not as a catalogue nickname for “any low-carbon 304 tube with a little nitrogen.” The MTC reports the full ladle chemistry including carbon against the 0.035% (or Footnote D 0.040%) path and nitrogen in the 0.10–0.16% band, plus the 75/30 ksi tensile and hardness acceptance set; the stencil carries seamless tube identity under SA-213; and dual SA-213/A213 marking is offered only when requested so Code and non-Code jobs stay cleanly documented.

We keep the 304-family conversation honest for boiler and HX duty. If low carbon without a nitrogen band is enough, we open SA213 TP304L. If the datasheet needs the 80/35 ksi nitrogen-strengthened floor and can accept C ≤0.08%, we open SA213 TP304N. If creep-range H-grade carbon and grain-size controls are required, we open SA213 TP304H. If chlorides dominate, we open SA213 TP316L / SA213 TP316LN. The SA213/SA213M hub is organized the same way — grade by grade under ASME, seamless tube only.

Lead times combine near-term stock lengths with mill schedules; we say which is which on the quotation. Cut-to-length, U-bending, polish, and third-party inspection are defined extras. The tube that arrives should match the ASME callout the engineer wrote, with paperwork a third-party inspector can read without translation.

Supply Capability

SHH STEEL can supply ASME SA213 TP304LN stainless steel tube against the edition and finish route named on your enquiry. The capability table below summarizes the sizes, finishes, and documents we regularly quote for this grade, followed by the Stock / Available sizes map buyers ask for when they need a quick sense of what to enquire against for boiler and heat-exchanger duty.

Item SHH STEEL capability for TP304LN
Standard ASME SA213 / SA213M (dual A213 marking on request)
Grade TP304LN / UNS S30453
Product form Seamless only — cold-finished and hot-finished
Size Typical OD × min wall (or average wall) in the SA-213 usual band; other diameters by agreement
Wall / gauge Minimum wall or average wall; BWG / gauge callouts accepted on enquiry
Length Cut-to-length for HX / boiler bundles; mill random by agreement; U-bends on enquiry
Finish Annealed and pickled; bright annealed or light polish by agreement
Testing Tension (75/30 ksi), hardness (max 192 HBW / 90 HRB), flattening, flaring, hydro or NDE per length; full ladle chemistry including C and N on MTC; product analysis / IGC on order
Documents EN 10204 3.1 with full ladle chemistry; third-party inspection / 3.2 on request
Trade terms FOB / CFR / CIF / EXW and other agreed Incoterms

Stock / Available sizes

SHH STEEL quotes TP304LN tube against a practical stock-and-mill enquiry range rather than a frozen warehouse SKU list. The sizes below are the OD × wall / BWG combinations buyers most often request for low-carbon nitrogen-bearing boiler and heat-exchanger tube; availability of any single line on a given week depends on mill drawing and our inbound schedule, so treat the table as a supply map for enquiry — not a guarantee that every line sits on the floor with a published tonnage.

Item Typical stock / enquiry range for TP304LN
Outside diameter 12.7, 15.88, 19.05, 25.4, 31.8, 38.1, 50.8, 63.5, 76.2 mm (and other HX/boiler ODs on enquiry; up through the usual SA-213 ~5 in. [127 mm] band)
Wall / BWG BWG 12–20 class walls and metric min-wall equivalents; Footnote D sizes called out when many draws apply; lighter and heavier walls by agreement
Common OD × wall examples 15.88 × 1.65 mm; 19.05 × 1.65 mm; 19.05 × 2.11 mm; 25.4 × 2.11 mm; 25.4 × 2.77 mm; 31.8 × 2.77 mm; 38.1 × 2.77 mm — illustrative HX/boiler sizes, confirm min vs average wall
Length Cut lengths for exchanger bundles; U-bends and straight random lengths on enquiry
Special Non-standard OD/wall, bright anneal, polished bore, Footnote D carbon path, and dual SA-213/A213 marking — confirm on enquiry before the heat is reserved

When you send an enquiry, list OD × wall (or BWG), wall basis (minimum or average), cold-finished or hot-finished preference, quantity or cut list, required marking (SA-213 alone or dual SA-213/A213), Footnote D applicability, and any Supplementary Requirements. We reply with what we can ship from near-term stock versus what needs a mill run, without inventing fake warehouse codes or tonnage claims.

Send the size list, finish route, quantity or cut lengths, required marking (SA-213 or dual SA-213/A213), Supplementary Requirements, and destination on one enquiry. We will confirm chemistry (including carbon against the applicable Footnote D path and nitrogen), tensile, and hardness against the ordered edition, state what ships from near-term availability versus mill production, and keep the offer aligned with the ASME SA213 / SA213M product standard that governs this page. Related grades such as SA213 TP304L, SA213 TP304N, and SA213 TP316LN sit on the same hub when the datasheet steps beyond TP304LN.

FAQ

Is ASME SA-213 the same as ASTM A213 for TP304LN?
No. ASME SA-213 / SA-213M is the ASME Code Book adoption of the seamless boiler, superheater, and heat-exchanger tube grade text; ASTM A213 / A213M is the separate ASTM International product specification. Chemistry, tensile, and hardness floors align closely for a given referenced edition, but they remain two independent standards. Dual-mark SA-213/A213 tube only when the purchase order asks for both names on the stencil and MTC.
Does ASME SA213 TP304LN include welded or HCW tube?
No. ASME SA-213 covers seamless tube only. There is no WLD or HCW manufacturing type under this product standard the way ASME SA312 describes pipe. The process choice for TP304LN under SA-213 is cold-finished versus hot-finished seamless tube, plus the heat-treatment and testing clauses of the ordered edition. If you need welded stainless pipe, that is a different product standard and a different steelspecs page family.
What carbon and nitrogen limits apply to SA213 TP304LN?
Melt carbon is ≤0.035%, with Footnote D allowing ≤0.040% for small-diameter or thin-wall tube that needs many drawing passes. Nitrogen is a mandatory 0.10–0.16% band on the melt analysis. Nitrogen analysis method is by agreement under Footnote B language. Confirm Footnote D’s OD/wall trigger on the ordered edition before treating a secondary catalogue note as acceptance text, and require both C and N on the EN 10204 3.1 certificate.
TP304LN vs TP304L — why add nitrogen under SA213?
Both grades keep a low-carbon melt path for as-welded intergranular resistance, but TP304LN adds the 0.10–0.16% nitrogen band that TP304L does not require. Nitrogen supports austenite stability and is part of the grade identity for S30453. Order TP304L when the datasheet does not need nitrogen; order TP304LN when the PO calls for both low carbon and the nitrogen band on one MTC. Do not treat a TP304L heat as automatic LN without the nitrogen analysis.
TP304LN vs TP304N — which SA213 tube should I specify?
Order TP304LN when as-welded IGC resistance is the driver and you need C ≤0.035% (or Footnote D 0.040%) together with N 0.10–0.16% on the 75/30 ksi mechanical row. Order TP304N when the datasheet needs the higher 80/35 ksi nitrogen-strengthened floor and can accept C ≤0.08%. They are not interchangeable stamps — carbon path and tensile floor both differ. Spell the required grade on the enquiry so the heat is selected correctly.
Does SA-213 set a hardness limit for TP304LN?
Yes. The mechanical table for TP304LN lists tensile strength, yield strength, elongation, and a hardness maximum of 192 HBW / 200 HV or 90 HRB. Hardness tests are part of lot acceptance under SA-213, which differs from many SA312 / A312 pipe rows for related UNS numbers that omit a hardness cap. If a project needs a tighter hardness window than the table, write it into the purchase order as an additional requirement.
Minimum wall vs average wall — which should I order for SA213 TP304LN?
Order minimum wall when the design and datasheet are written around a guaranteed minimum thickness after tolerance. Order average wall only when the purchase order explicitly allows average-wall product and the designer has accepted that basis. The two readings produce different tube from the same OD × wall line. Footnote D’s carbon relief for small OD/thin wall does not change which wall basis you must name on the enquiry.
Hydrostatic test vs NDE — which do I get on SA213 TP304LN tube?
ASME SA-213 requires each tube to be hydrostatically tested or nondestructively electrically tested. The manufacturer may choose the method unless the purchase order fixes one. Neither route is an informal upgrade over the other inside the product standard. State the preferred method on the enquiry if your end user or inspector mandates hydro only or a named NDE technique.
What heat treatment does ASME SA-213 require for TP304LN?
TP304LN is solution treated at a minimum of 1900 °F [1040 °C] and then water quenched or rapidly cooled to prevent carbide reprecipitation. Both cold-finished and hot-finished seamless tube follow that heat-treatment requirement. Ask the mill to state anneal temperature and quench method on the EN 10204 3.1 certificate so receiving inspection can clear the heat without chasing verbal confirmations.
Should I order A262 Practice E with SA213 TP304LN tube?
Often yes when as-welded intergranular resistance is a project requirement. Low carbon already leans toward IGC resistance, but ASME SA-213 does not make A262 Practice E automatic for every LN heat. Write the Supplementary Requirement onto the purchase order with the practice and specimen condition you need so the test is contractual. Verbal "full certs" language is not a substitute for a numbered corrosion-test callout.
Can you dual-certify ASME SA-213 and ASTM A213 TP304LN, or TP304LN/TP304L?
Yes on both axes when the heat and testing support it. Dual SA-213/A213 marking is available when the purchase order requests both independent standards on the stencil and MTC. Dual TP304LN/TP304L is available only when ladle chemistry meets both carbon paths and the nitrogen band required for LN, and when tensile plus hardness clear both mechanical-table rows. Spell the required marking on the enquiry so the heat is selected correctly.

Conclusion

ASME SA213 TP304LN / UNS S30453 is the low-carbon, nitrogen-bearing 18-8 seamless stainless steel tube grade for Code boiler, superheater, and heat-exchanger service when as-welded intergranular resistance and a mandatory nitrogen band matter on the same MTC. SHH STEEL supplies cold-finished and hot-finished seamless tube in the usual OD × wall / BWG band, solution annealed, tested to the 75/30 ksi tensile and hardness acceptance floors, and documented on EN 10204 3.1 certificates that report both carbon and nitrogen — with dual A213 marking only when the order asks for that separate ASTM standard. For sister grades and stock-oriented size discussions, start from the SA213/SA213M hub, then send your OD × wall list, wall basis, Footnote D notes, and marking requirements so we can align mill and near-term availability to the ASME callout.

Contact: admin@steelspecs.com

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X