ASME SA213 TP310S Stainless Steel Tube | ASME SA213 Stainless Steel - SHH STEEL

ASME SA213 TP310S Stainless Steel Tube

ASME SA213 TP310S / UNS S31008 seamless boiler, superheater and heat-exchanger tube — a 24–26% Cr / 19–22% Ni austenitic with C ≤0.08%, a 75/30 ksi tensile floor, hardness max 192 HBW / 90 HRB, and a 1900 °F solution anneal with Footnote F quench capability. Chosen for high-temperature oxidation resistance above the 309 family rather than molybdenum chloride service. SHH STEEL supplies cold-finished and hot-finished seamless tube with EN 10204 3.1 MTCs.
Grade
TP310S / UNS S31008
Standard
ASME SA213 / SA213M
Product form
Seamless boiler / superheater / heat-exchanger tube (cold-finished and hot-finished)
Size
Typical OD × min wall (or average wall) within ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD and ~0.015–0.500 in. [0.4–12.7 mm] wall; other diameters by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is ASME SA213 TP310S Stainless Steel Tube

ASME SA-213 / SA-213M is the ASME Boiler and Pressure Vessel Code Book adoption of the seamless ferritic and austenitic alloy-steel boiler, superheater, and heat-exchanger tube product standard. Grade TP310S under that Code Book text is the higher chromium–nickel austenitic listed as UNS S31008, with melting limits of carbon ≤0.08%, chromium 24.0–26.0%, and nickel 19.0–22.0%. When a Code-stamped boiler, superheater, or heat-exchanger datasheet calls for SA-213 TP310S, the purchase order and mill test certificate should carry the ASME designation — not a shop nickname such as “310 HX tube,” and not an assumed swap from TP309S simply because both clear a 75/30 ksi tensile floor and sit in the high-temperature oxidation conversation.

SHH STEEL can supply ASME SA213 TP310S stainless steel tube as seamless cold-finished and hot-finished product in the usual boiler and heat-exchanger OD × wall / BWG band, documented on EN 10204 3.1 mill test certificates that report the full ladle chemistry and the tensile plus hardness acceptance set. Dual SA-213 / A213 marking on the same lengths is available only when the purchase order asks for both independent standards; ASME SA213 and ASTM A213 remain separate documents even when the grade text aligns closely for a referenced edition. Browse the grade family on the SA213/SA213M hub.

Commercially the same tube is still called 310S, S31008 boiler tube, 25Cr-20Ni HX tube, or SA213 310S tube; none of those phrases replace the ASME grade on the stencil or MTC. Sister grades under the same ASME standard include SA213 TP310H, SA213 TP310Cb, SA213 TP309S, SA213 TP309H, and SA213 TP304. SA-213 covers seamless tube only — there is no welded or HCW manufacturing type under this product standard — so cold-finished versus hot-finished seamless route is the process choice, not a WLD/HCW stencil letter. For the sister ASTM product page on the same UNS, see A213 TP310S.

Chemical Composition of SA213 TP310S

Two chemistry layers matter for TP310S under ASME SA-213. The melting (heat or ladle) analysis is mandatory for every heat under the stainless chemistry table; product analysis on finished tube applies only when Supplementary Requirement wording or the purchase order invokes it through the general requirements path (commonly ASTM A1016/A1016M), with product-analysis tolerances typically taken from ASTM A480/A480M Table A1.1. The “S” in TP310S marks the ≤0.08% carbon ceiling relative to older high-carbon 310 compositions; chromium 24.0–26.0% and nickel 19.0–22.0% are the oxidation drivers. SHH STEEL reports the actual ladle values — and the product values when ordered — and does not advertise unpublished tighter catalogue windows.

The tables below reproduce the melt limits for TP310S / UNS S31008 and the product-analysis limits that result from applying A480 Table A1.1 tolerances, plus a snapshot versus TP310H and TP310Cb. Values are maximum unless a range is shown; an ellipsis (…) means the ordered edition sets no requirement for that element. UNCERTAIN: exact SA-213 / A213 edition year and whether austenitic grades sit in Table 1 or Table 2 of that edition; A480 Cr/Ni tolerance digits for the 24–26% Cr / 19–22% Ni band — applied from sister 310 / high-Cr practice; Footnote F full quench-capability wording across editions — confirm the ordered edition on the purchase order.

Melting analysis (heat / ladle analysis)

Source: public SA-213 / A213 grade-table summaries for TP310S / UNS S31008. Confirm the ordered ASME edition on the purchase order.

Element TP310S (UNS S31008) melting analysis
Carbon (C) ≤ 0.08
Manganese (Mn) ≤ 2.00
Phosphorus (P) ≤ 0.045
Sulfur (S) ≤ 0.030
Silicon (Si) ≤ 1.00
Chromium (Cr) 24.0 – 26.0
Nickel (Ni) 19.0 – 22.0
Molybdenum (Mo) … (no requirement)
Nitrogen (N) … (no requirement)
Niobium (Nb / Cb) … (no requirement)

Product analysis — A480/A480M Table A1.1 tolerances applied

Element Melting Tolerance (A480 A1.1) Product analysis limit
Carbon (C) ≤ 0.08 0.01 over ≤ 0.09
Manganese (Mn) ≤ 2.00 0.04 over ≤ 2.04
Phosphorus (P) ≤ 0.045 0.010 over ≤ 0.055
Sulfur (S) ≤ 0.030 0.005 over ≤ 0.035
Silicon (Si) ≤ 1.00 0.05 over ≤ 1.05
Chromium (Cr) 24.0 – 26.0 0.25 under / over 23.75 – 26.25
Nickel (Ni) 19.0 – 22.0 0.15 under / 0.20 over 18.85 – 22.20

Snapshot — TP310S vs TP310H vs TP310Cb

Element TP310S (S31008) TP310H (S31009) TP310Cb (S31040)
C ≤ 0.08 0.04 – 0.10 ≤ 0.08
Cr 24.0 – 26.0 24.0 – 26.0 24.0 – 26.0
Ni 19.0 – 22.0 19.0 – 22.0 19.0 – 22.0
Nb (Cb) … … 10×C – 1.10

The 24–26% chromium and 19–22% nickel balance is why TP310S sits above the 309 family for high-temperature oxidation resistance: more chromium builds a more durable oxide scale, and the higher nickel keeps the structure fully austenitic after the 1900 °F solution treatment. Carbon is capped at 0.08% — the same ceiling as TP304 and TP309S — so this is not an H-grade carbon story. When creep-range boiler service needs a controlled carbon floor and grain-size language on the same Cr–Ni balance, open SA213 TP310H; when Nb stabilization on the same 25Cr-20Ni balance is required, open SA213 TP310Cb; when a step down in Cr–Ni is enough, open SA213 TP309S.

When product analysis is ordered, finished tube may read up to C 0.09%, Mn 2.04%, P 0.055%, S 0.035%, and Si 1.05%, with Cr 23.75–26.25% and Ni 18.85–22.20%. Note the asymmetric A480 Ni product tolerance on this band (0.15 under / 0.20 over). Those are the only product limits we quote from the A480 A1.1 path for this grade. Put any tighter project carbon or sulfur ceiling on the purchase order before the heat is selected.

Mechanical Properties of SA213 TP310S

ASME SA-213 sets the room-temperature tensile acceptance floor for TP310S at 75 ksi [515 MPa] tensile strength and 30 ksi [205 MPa] yield strength (0.2% offset), with elongation of 35% minimum in 2 in. or 50 mm. Hardness is capped at 192 HBW / 200 HV or 90 HRB. That room-temperature pair matches many 18-8 and 309 grades; the commercial reason to pay for 310S is oxidation resistance from the higher Cr–Ni balance, not a higher tensile floor. Unlike the H grades, TP310S does not carry a mandatory ASTM grain-size number in the heat-treatment table — acceptance is chemistry plus tensile, hardness, and heat treatment. Every lot sampled under the edition’s specimen rules must meet those numbers after the final solution treatment.

Source: public SA-213 / A213 mechanical-table summaries for TP310S / UNS S31008 (commonly Table 4). Mechanical property requirements do not apply to tubing smaller than 1/8 in. [3.2 mm] inside diameter or thinner than 0.015 in. [0.4 mm] wall.

Property TP310S requirement
Tensile strength, min 75 ksi [515 MPa]
Yield strength (0.2% offset), min 30 ksi [205 MPa]
Elongation in 2 in. or 50 mm, min 35%
Hardness, max 192 HBW / 200 HV or 90 HRB
Grain size No mandatory ASTM grain-size number (unlike TP310H)

Flattening and flaring tests sit beside tension and hardness on a lot basis. Design calculations should use the 75/30 ksi pair unless the purchase order states higher guaranteed values the mill has accepted in writing. When the datasheet needs H-grade carbon 0.04–0.10% and ASTM No. 7 or coarser grain size on the same 24–26% Cr / 19–22% Ni balance, open SA213 TP310H; when a step down in Cr–Ni oxidation resistance is enough, open SA213 TP309S.

Dimensions and Tolerances

Dimensional supply for ASME SA213 TP310S is tube language — outside diameter × wall thickness (minimum wall or average wall) and, commercially, BWG / gauge — not ASME B36.19 pipe schedules as the primary size story. The sizes usually furnished under SA-213 run from about 1/8 in. [3.2 mm] inside diameter to 5 in. [127 mm] outside diameter, with minimum wall from about 0.015 to 0.500 in. [0.4 to 12.7 mm]; tubing with other diameters may be furnished when all other requirements of the specification are met. State on the purchase order whether wall is minimum or average, because remaining wall after high-temperature oxidation is often a design input on the circuits where 310S is chosen.

Outside-diameter and wall variations follow the general requirements invoked by SA-213 (commonly ASTM A1016/A1016M), with cold-finished and hot-finished routes carrying different practical bands. Cold-finished tubes commonly hold tighter OD control; hot-finished tubes allow wider OD and wall windows. Permissible variations from a specified average wall for cold-finished tube are often summarized as ±10% of the specified average wall, while minimum-wall product is accepted to the minimum-wall tables rather than a symmetric ± window. Confirm the exact general-requirements rows for the OD and finish route on the ordered edition.

Item Typical SA213 TP310S dimensional practice
Product form Seamless only (cold-finished or hot-finished)
Usual size band ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD; wall ~0.015–0.500 in. [0.4–12.7 mm] min (or average wall if PO says so)
Wall basis Minimum wall (default commercial practice) or average wall when specified
OD / wall tolerances Per general requirements for the finish route and size; cold-finished average wall often ±10%
Length Cut lengths for HX / boiler / high-temperature bundles, or mill random lengths by agreement
Secondary size note ASME B36.19 schedules may appear only when a buyer asks for a pipe-schedule cross-reference — not as the primary SA-213 size callout

Put the cut list, U-bend or straight-tube preference, and end preparation on the enquiry so mill and stock lengths can be mixed efficiently. Minimum wall is a first-class SA-213 concept: if the datasheet assumes average wall, say so explicitly before the heat is rolled.

Equivalent Grades

Equivalence language around TP310S tube often collapses plate, cast, and tube product forms into one nickname. ASME SA-213 Grade TP310S / UNS S31008 is the governing designation for this article; EN 1.4845 and JIS SUS310S are approximate wrought names that point to similar 25Cr-20Ni families but are not automatic substitutes on an SA-213 mill test certificate. When a datasheet says “equivalent to 310S,” confirm which product standard, tensile/hardness table, and heat-treatment clause the mill will actually certify.

Designation Notes
ASME SA-213 / SA-213M Grade TP310S Governing ASME Code Book seamless boiler / HX tube product standard for this article
UNS S31008 Unified number listed with the grade chemistry
ASTM A213 TP310S Separate ASTM International product specification — dual-mark only when the PO asks; see A213 TP310S
EN 1.4845 (X8CrNi25-21) Approximate wrought designation; order EN tube forms under the relevant EN tube specs
JIS SUS310S Approximate Japanese grade name; confirm the Japanese tube product standard when ordering JIS product
Related H-grade SA213 TP310H — same Cr–Ni, C 0.04–0.10, grain size No. 7 or coarser
Related Nb grade SA213 TP310Cb — C ≤0.08 plus niobium stabilization
Related 309 SA213 TP309S — lower Cr–Ni oxidation balance
Related plate A240 / SA240 flat product in the same UNS family — order plate and tube under their own product standards

ASTM A213 TP310S is the separate ASTM product specification sharing the same grade family; dual SA-213/A213 marking is a purchase-order option, not a claim that the two standards are one document. Compare H-grade SA213 TP310H and lower-alloy SA213 TP309S on their own ASME pages before swapping grades in a tube bundle.

Heat Treatment and Delivery Condition

TP310S under ASME SA-213 is furnished solution treated at a minimum of 1900 °F [1040 °C], then quenched in water or cooled rapidly by other means. The heat-treatment table carries Footnote F for this grade: quench rate must be sufficient to prevent carbide re-precipitation, as demonstrable by the capability of tubes — heat treated by separate solution annealing or by direct quenching — to pass Practice E of A262 (or the edition’s referenced intergranular-corrosion practice). That heat-treatment row applies to both cold-finished and hot-finished seamless tube.

Cold-finished versus hot-finished is a process and dimensional route, not a substitute for the anneal. Delivery condition for SHH STEEL TP310S is solution annealed and pickled (or bright annealed by agreement), with heat-treatment temperature and quench method stated on the EN 10204 3.1 certificate. Straightening, cutting, and end finishing follow heat treatment. Public heat-treatment language does not assign a mandatory ASTM grain-size number to TP310S — grain-size rules belong to the H grades.

When Supplementary Requirement language for intergranular-corrosion capability is ordered beyond Footnote F quench-capability language, the corrosion test report travels with the heat-treatment record. H-grade grain-size rules do not rewrite the TP310S path — use SA213 TP310H when the datasheet calls for H-grade carbon and grain-size controls on the same Cr–Ni balance.

Corrosion Resistance

TP310S is selected primarily for high-temperature oxidation and scaling resistance from its 24–26% chromium and 19–22% nickel balance, not for molybdenum-driven chloride pitting resistance. In oxidizing furnace atmospheres, hot-process gas circuits, and many elevated-temperature steam or air services, the higher Cr–Ni oxide scale outperforms both ordinary 18-8 grades and the 22–24% Cr / 12–15% Ni 309 family. In chloride-bearing cooling waters and wet brine-leaning exchangers, buyers usually step to SA213 TP316 / SA213 TP316L or higher rather than treating 310S as a chloride upgrade.

ASME SA-213 itself does not publish a corrosion-rate or oxidation-life table for TP310S; selection remains engineering judgment against temperature, atmosphere, velocity, and inspection philosophy. Intergranular corrosion risk after welding is controlled by solution treating after fabrication when the sequence allows, by the Footnote F quench-capability path on the mill heat treatment, by ordering an H-grade only when the datasheet truly needs it, or by invoking a contractual A262 Practice E Supplementary Requirement on the tube PO. SHH STEEL will not rank TP310S as equal to 316 in chlorides — higher chromium and nickel are not a molybdenum substitute.

Applications of SA213 TP310S Tube

Because TP310S brings a 24–26% Cr / 19–22% Ni balance under SA-213 without adding molybdenum, it shows up in severe high-temperature oxidation-prone boiler and process circuits, furnace-related heat exchangers, and elevated-temperature HX duty where 18-8 and even 309S scale too quickly. The table below pairs typical application areas with a selection note so the grade is chosen for atmosphere and metal temperature — not only for the familiar “310S” name on the BOM.

Application area Typical use of TP310S tube Selection note
Severe high-temperature oxidation Seamless tube where 25Cr-20Ni scale resistance outperforms 18-8 and 309 Confirm design metal temperature and atmosphere
Boiler / process steam (oxidation-limited) Seamless generating or process tubing ordered to SA-213 For creep-critical H-grade carbon/grain open TP310H
Furnace / hot-gas heat exchangers Straight and U-bend tubes in oxidizing hot-gas circuits Prefer TP309S if a step down in Cr–Ni is enough
Chemical process (oxidizing, low chloride) Tube-side circuits with hot oxidizing media Prefer TP316/TP316L if chlorides dominate
Chloride-rich cooling water Usually not the preferred selection Open molybdenum grades on the hub
General corrosive tube duty Seamless tube where SA-213 documentation is preferred over pipe forms Do not substitute SA312 / A312 pipe paperwork for SA-213 tube acceptance

For H-grade carbon and grain-size controls open SA213 TP310H; for Nb stabilization open SA213 TP310Cb; for a step down in Cr–Ni open SA213 TP309S; browse the same SA213/SA213M hub before locking the tube bill of materials.

Weldability

TP310S tube welds with matching or near-matching austenitic filler for tube-to-tubesheet joints, attachment welds, and fabrication joins. Common practice uses ER310 / ER310L (or equivalent covered electrodes) under a qualified WPS; many fabricators prefer low-carbon deposits for lower carbon in the weld metal even when the base tube is standard-carbon TP310S. Heat input control, interpass limits, and post-weld cleaning remain the fabricator’s responsibility under the applicable boiler or pressure-vessel Code — SA-213 governs the seamless tube product, not the field or shop weld procedure.

Because SA213 TP310S is seamless, there is no mill longitudinal weld to radiograph the way welded pipe standards describe. Focus inspection language on tube integrity (hydro or NDE of each length), tube-to-tubesheet joint quality, and any contractual corrosion test on the base metal. For tube that will enter service as-welded in a sensitizing environment, discuss whether a low-carbon filler path, a post-weld solution treatment, or a move to TP310Cb or TP310H better protects the joint. Specify end preparation and surface finish on the tube PO when orbital or clean-service joins are planned.

Surface Finishes

Standard mill delivery for ASME SA213 TP310S is solution annealed and pickled, leaving a clean matte finish suitable for most boiler and heat-exchanger tube duty. Bright annealing under protective atmosphere produces a smoother reflective surface used on some clean-process tube lines and must be called out because it changes the heat-treatment route while still needing to clear Footnote F quench-capability expectations. Light polish or specified Ra on the bore or OD is a commercial or service-center operation on top of SA-213 product, not automatic with the grade stamp.

When a fouling-sensitive or clean-process exchanger specification quotes an Ra maximum on the bore, put it on the tube purchase order with its own acceptance language and sampling plan. SHH STEEL stencils grade and heat treatment as standard requirements; polish, special OD grind, and passivation after fabrication remain commercial extras unless the contract says otherwise. End preparation should be ordered together with finish so receiving inspection shares one acceptance language.

Inspection and Testing

Base ASME SA-213 testing for TP310S includes heat analysis, tension tests to the 75/30 ksi floor, hardness tests to the 192 HBW / 90 HRB maximum, flattening and flaring tests on a lot basis, and either hydrostatic testing or nondestructive electric testing of each length. The manufacturer may choose hydro versus NDE unless the purchase order fixes the method; both are acceptance routes inside the product standard, not informal upgrades. Marking includes the ASME designation, grade, size, heat number, and other clause-required data so receiving inspection can tie each length back to the MTC.

Supplementary Requirements commonly added on TP310S tube orders are summarized below. Invoke them by number or clear purchase-order wording; mills will not assume product analysis or intergranular-corrosion testing from a verbal “full certs” note. Footnote F quench-capability language is part of the heat-treatment row for this grade — confirm whether a contractual A262 Practice E report is also required on the PO.

Option Purpose
Product analysis Confirms chemistry on finished tube (via general requirements / PO language)
Intergranular corrosion A262 Practice E (or agreed practice) as a contractual Supplementary Requirement; related to Footnote F quench capability
Minimum vs average wall States which wall basis the size callout uses
Fixed hydro or NDE method Removes manufacturer’s option when the end user mandates one route
Third-party inspection / EN 10204 3.2 Witnessed testing and certificate when the project requires it

Lot definitions for continuous heat treatment or direct quench after hot forming follow the size-based lot sizes in SA-213; ask the mill to state lot identity clearly on the certificate so hardness and tension specimens map cleanly to the bundle you receive.

Packaging and Shipping

TP310S tube leaves SHH STEEL bundled, capped or end-protected, and tagged for export or domestic delivery according to the length mix and bend form on the order. Bundle tags repeat the ASME SA213 grade, OD × wall (or BWG), heat number, and PO reference so site receiving can check the shipment without opening every certificate packet first. U-bent tubes need extra cradle or case protection so bend radii and legs are not distorted in transit.

Export packing can be bare bundles, wrapped bundles, or wooden-cased lengths for bright-annealed, polished, or small-bore material. We ship under the Incoterms on the order acknowledgement — FOB, CFR, CIF, EXW, or other agreed terms. Inland trucking, bilingual destination marks, or project color coding for bundle tags should be stated on the enquiry beside the metallurgical notes.

Why Choose SHH STEEL

SHH STEEL treats ASME SA213 TP310S as a Code Book product standard with enforceable chemistry, tensile, hardness, heat-treatment (including Footnote F quench capability), and marking rules — not as a catalogue nickname for “any 310 tube.” The MTC reports the full ladle chemistry and the tensile/hardness acceptance set; the stencil carries seamless tube identity under SA-213; and dual SA-213/A213 marking is offered only when requested so Code and non-Code jobs stay cleanly documented.

We keep the 310-family conversation honest for high-temperature boiler and HX duty. If creep-range H-grade carbon and grain-size controls are required on the same Cr–Ni balance, we open SA213 TP310H. If niobium stabilization on the same 25Cr-20Ni balance is specified, we open SA213 TP310Cb. If a step down in chromium–nickel is enough, we open SA213 TP309S / SA213 TP309H. If chlorides dominate a wet exchanger, we open SA213 TP316 / SA213 TP316L rather than stretching 310S into the wrong service. The SA213/SA213M hub is organized the same way — grade by grade under ASME, seamless tube only.

Lead times combine near-term stock lengths with mill schedules; we say which is which on the quotation. Cut-to-length, U-bending, polish, and third-party inspection are defined extras. The tube that arrives should match the ASME callout the engineer wrote, with paperwork a third-party inspector can read without translation.

Supply Capability

SHH STEEL can supply ASME SA213 TP310S stainless steel tube against the edition and finish route named on your enquiry. The capability table below summarizes the sizes, finishes, and documents we regularly quote for this grade, followed by the Stock / Available sizes map buyers ask for when they need a quick sense of what to enquire against for severe high-temperature boiler and heat-exchanger duty.

Item SHH STEEL capability for TP310S
Standard ASME SA213 / SA213M (dual A213 marking on request)
Grade TP310S / UNS S31008
Product form Seamless only — cold-finished and hot-finished
Size Typical OD × min wall (or average wall) in the SA-213 usual band; other diameters by agreement
Wall / gauge Minimum wall or average wall; BWG / gauge callouts accepted on enquiry
Length Cut-to-length for HX / boiler bundles; mill random by agreement; U-bends on enquiry
Finish Annealed and pickled; bright annealed or light polish by agreement
Testing Tension (75/30 ksi), hardness (max 192 HBW / 90 HRB), flattening, flaring, hydro or NDE per length; full ladle chemistry on MTC; product analysis / IGC on order; Footnote F quench capability on heat treatment
Documents EN 10204 3.1 with full ladle chemistry; third-party inspection / 3.2 on request
Trade terms FOB / CFR / CIF / EXW and other agreed Incoterms

Stock / Available sizes

SHH STEEL quotes TP310S tube against a practical stock-and-mill enquiry range rather than a frozen warehouse SKU list. The sizes below are the OD × wall / BWG combinations buyers most often request for severe high-temperature oxidation-resistant boiler and heat-exchanger tube; availability of any single line on a given week depends on mill drawing and our inbound schedule, so treat the table as a supply map for enquiry — not a guarantee that every line sits on the floor with a published tonnage.

Item Typical stock / enquiry range for TP310S
Outside diameter 19.05, 25.4, 31.8, 38.1, 44.5, 50.8, 63.5, 76.2 mm (and other HX/boiler ODs on enquiry; up through the usual SA-213 ~5 in. [127 mm] band)
Wall / BWG BWG 10–18 class walls and metric min-wall equivalents; lighter and heavier walls by agreement
Common OD × wall examples 25.4 × 2.11 mm; 25.4 × 2.77 mm; 31.8 × 2.77 mm; 38.1 × 2.77 mm; 38.1 × 3.40 mm; 50.8 × 3.40 mm; 50.8 × 3.60 mm — illustrative high-temp HX/boiler sizes, confirm min vs average wall
Length Cut lengths for exchanger and high-temperature bundles; U-bends and straight random lengths on enquiry
Special Non-standard OD/wall, bright anneal, polished bore, and dual SA-213/A213 marking — confirm on enquiry before the heat is reserved

When you send an enquiry, list OD × wall (or BWG), wall basis (minimum or average), cold-finished or hot-finished preference, quantity or cut list, required marking (SA-213 alone or dual SA-213/A213), and any Supplementary Requirements. We reply with what we can ship from near-term stock versus what needs a mill run, without inventing fake warehouse codes or tonnage claims.

Send the size list, finish route, quantity or cut lengths, required marking (SA-213 or dual SA-213/A213), Supplementary Requirements, and destination on one enquiry. We will confirm chemistry, tensile, and hardness against the ordered edition, state what ships from near-term availability versus mill production, and keep the offer aligned with the ASME SA213 / SA213M product standard that governs this page. Related grades such as SA213 TP310H, SA213 TP309S, and SA213 TP304 sit on the same hub when the datasheet steps beyond TP310S.

FAQ

Is ASME SA-213 the same as ASTM A213 for TP310S?
No. ASME SA-213 / SA-213M is the ASME Code Book adoption of the seamless boiler, superheater, and heat-exchanger tube grade text; ASTM A213 / A213M is the separate ASTM International product specification. Chemistry, tensile, and hardness floors align closely for a given referenced edition, but they remain two independent standards. Dual-mark SA-213/A213 tube only when the purchase order asks for both names on the stencil and MTC.
Does ASME SA213 TP310S include welded or HCW tube?
No. ASME SA-213 covers seamless tube only. There is no WLD or HCW manufacturing type under this product standard the way ASME SA312 describes pipe. The process choice for TP310S under SA-213 is cold-finished versus hot-finished seamless tube, plus the heat-treatment and testing clauses of the ordered edition. If you need welded stainless pipe, that is a different product standard and a different steelspecs page family.
What is the chemistry of ASME SA213 TP310S?
TP310S is UNS S31008. Melting limits include carbon ≤0.08%, manganese ≤2.00%, phosphorus ≤0.045%, sulfur ≤0.030%, silicon ≤1.00%, chromium 24.0–26.0%, and nickel 19.0–22.0%, with molybdenum, nitrogen, and niobium as no-requirement ellipses. Product-analysis limits apply only when ordered, typically from A480 Table A1.1 tolerances via the general-requirements path. Confirm the ordered SA-213 edition before treating a secondary catalogue as acceptance text.
TP310S vs TP309S — which oxidation grade should I order under SA213?
Order TP310S when the datasheet needs the higher 24–26% Cr / 19–22% Ni oxidation balance. Order TP309S when 22–24% Cr / 12–15% Ni is enough for the design metal temperature and atmosphere. Both share a 75/30 ksi tensile floor and a 192 HBW / 90 HRB hardness ceiling, so tensile equality alone is not a reason to swap; confirm the Cr–Ni callout before substituting either grade for the other.
TP310S vs TP310H — which SA213 grade should I order?
Order TP310S when the specification calls for the standard C ≤0.08% path without H-grade carbon and grain-size controls. Order TP310H when the boiler or superheater datasheet needs carbon 0.04–0.10% and ASTM No. 7 or coarser grain size on the same 24–26% Cr / 19–22% Ni balance. Do not treat "310H" as a synonym stamp for ordinary TP310S on the MTC.
TP310S vs TP304 — when do I need the higher Cr–Ni under SA213?
Order TP310S when high-temperature oxidation and scaling resistance from 24–26% Cr / 19–22% Ni matter more than the lower alloy cost of 18-8 TP304. Both grades share a 75/30 ksi room-temperature tensile floor and a 192 HBW / 90 HRB hardness ceiling, so tensile equality alone is not a reason to swap. Confirm design metal temperature and atmosphere before substituting either grade for the other.
Does SA-213 set a hardness limit for TP310S?
Yes. The mechanical table for TP310S lists tensile strength, yield strength, elongation, and a hardness maximum of 192 HBW / 200 HV or 90 HRB. Hardness tests are part of lot acceptance under SA-213, which differs from many SA312 / A312 pipe rows for related UNS numbers that omit a hardness cap. If a project needs a tighter hardness window than the table, write it into the purchase order as an additional requirement.
What heat treatment does ASME SA-213 require for TP310S?
TP310S is solution treated at a minimum of 1900 °F [1040 °C] and then water quenched or rapidly cooled. Footnote F on the heat-treatment row requires quench rate sufficient to prevent carbide re-precipitation, as demonstrable by A262 Practice E capability (or the edition’s referenced practice). Both cold-finished and hot-finished seamless tube follow that path. Ask the mill to state anneal temperature and quench method on the EN 10204 3.1 certificate.
Minimum wall vs average wall — which should I order for SA213 TP310S?
Order minimum wall when the design and datasheet are written around a guaranteed minimum thickness after tolerance — especially important when remaining wall after high-temperature oxidation is a design input. Order average wall only when the purchase order explicitly allows average-wall product and the designer has accepted that basis. Put the wall basis on the enquiry before the mill selects tooling.
Is TP310S a good choice for chloride-rich cooling water under SA213?
Usually no. TP310S is framed for high-temperature oxidation resistance from its Cr–Ni balance, not for molybdenum-driven chloride pitting resistance. In seawater-leaning cooling water and wet brine exchangers, open TP316 / TP316L or higher-Mo grades on the SA213 hub. ASME SA-213 does not publish a chloride ranking that supports treating 310S as a 316 substitute.
Can you dual-certify ASME SA-213 and ASTM A213 TP310S?
Yes when the heat and testing support both independent standards. Dual SA-213/A213 marking is available when the purchase order requests both names on the stencil and MTC. Spell the required marking on the enquiry so the heat is selected and documented correctly — a "310S" nickname alone is not dual certification.

Conclusion

ASME SA213 TP310S / UNS S31008 is the 24–26% Cr / 19–22% Ni seamless stainless steel tube grade for Code boiler, superheater, and heat-exchanger service when high-temperature oxidation resistance above the 309 family matters more than molybdenum chloride performance. SHH STEEL supplies cold-finished and hot-finished seamless tube in the usual OD × wall / BWG band, solution annealed at 1900 °F with Footnote F quench capability, tested to the 75/30 ksi tensile and hardness acceptance floors, and documented on EN 10204 3.1 certificates — with dual A213 marking only when the order asks for that separate ASTM standard. For sister grades and stock-oriented size discussions, start from the SA213/SA213M hub, then send your OD × wall list, wall basis, and marking requirements so we can align mill and near-term availability to the ASME callout.

Contact: admin@steelspecs.com

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X