ASME SA213 UNS S35045 Alloy 803 class Al–Ti 25–29Cr / 32–37Ni seamless boiler, superheater and heat-exchanger tube — C 0.06–0.10%, Ti 0.15–0.60%, Al 0.15–0.60%, Cu ≤0.75%, tensile 70/25 ksi, solution anneal 2000 °F [1100 °C] still air cool or faster. No TP letter. SHH STEEL supplies seamless cold- and hot-finished tube with EN 10204 3.1 MTC.
Grade
UNS S35045 (no TP letter — Alloy 803 class Al–Ti 25Cr–35Ni austenitic)
Standard
ASME SA213 / SA213M
Product form
Seamless boiler / superheater / heat-exchanger tube (cold-finished and hot-finished)
Size
Typical OD × min wall (or average wall) within ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD and ~0.015–0.500 in. [0.4–12.7 mm] wall; other diameters by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is ASME SA213 UNS S35045 Stainless Steel Tube

ASME SA-213 / SA-213M is the ASME Boiler and Pressure Vessel Code Book adoption covering seamless ferritic and austenitic alloy-steel boiler, superheater, and heat-exchanger tubes. When a Code-stamped high-temperature heater, reformer-adjacent exchanger, or oxidation-leaning process HX names that adoption, SA-213 is the governing product standard for this Alloy 803 class Al–Ti austenitic tube — written as its own Code Book line, not as a merged synonym of ASTM A213. Begin from SA213/SA213M when the enquiry is Code-led.

UNS S35045 sits in the stainless chemistry table without a TP grade letter. Melting carbon is a deliberate 0.06–0.10% range; chromium 25.0–29.0%; nickel 32.0–37.0%; titanium 0.15–0.60%; aluminum 0.15–0.60%; copper ≤0.75%; manganese ≤1.50%; silicon ≤1.00%; phosphorus ≤0.045%; and sulfur ≤0.015%. Molybdenum and nitrogen are no-requirement ellipses — this is not a PREN-first chloride grade. Table 4 asks for 70 ksi [485 MPa] tensile, 25 ksi [170 MPa] yield, 35% elongation, and hardness max 192 HBW / 200 HV / 90 HRB. Buyers who write “Alloy 803 HX tube” on a bill of materials still need ASME SA-213 UNS S35045 on the purchase order so the mill applies the tube product standard, minimum-wall rules, and the Al/Ti windows together. This is not a dual stamp of SA213 TP310S or of a generic Alloy 800 nickname without the SA-213 UNS.

SHH STEEL can supply ASME SA213 UNS S35045 as seamless cold-finished and hot-finished tube in the usual OD × wall / BWG band, with EN 10204 3.1 certificates that report aluminum and titanium together with the 70/25 ksi tensile set, 35% elongation, and hardness. Dual SA-213/A213 marking is added only when the purchase order asks; the live twin is A213 UNS S35045.

Shop names include “S35045” and “Alloy 803.” Helpful for routing; the commercial Alloy 803 nickname does not replace UNS S35045 on the MTC. The purchase order should still carry ASME SA-213 UNS S35045, wall basis, OD × wall or BWG, finish route, and any Supplementary Requirements. Sister SA213 pages include SA213 TP310S, SA213 TP310H, and SA213 UNS S30815.

Chemical Composition of SA213 UNS S35045

UNS S35045 chemistry under ASME SA-213 is built for high-temperature oxidation and carburization-leaning service inside a 25–29% Cr / 32–37% Ni window with deliberate aluminum and titanium additions (each 0.15–0.60%). Carbon is a range (0.06–0.10%), not a low-C max. Molybdenum and nitrogen are no-requirement ellipses — this is not a PREN-first chloride grade. Melting analysis is mandatory; product analysis applies when ordered through A480/A480M Table A1.1. Copper stays ≤0.75%.

Melting analysis — UNS S35045

Element UNS S35045 melting analysis
Carbon (C) 0.06 – 0.10
Manganese (Mn) ≤ 1.50
Phosphorus (P) ≤ 0.045
Sulfur (S) ≤ 0.015
Silicon (Si) ≤ 1.00
Chromium (Cr) 25.0 – 29.0
Nickel (Ni) 32.0 – 37.0
Molybdenum (Mo) … (no requirement)
Nitrogen (N) … (no requirement)
Niobium (Nb) … (no requirement)
Titanium (Ti) 0.15 – 0.60
Aluminum (Al) 0.15 – 0.60
Copper (Cu) ≤ 0.75

Source: public SA-213 / A213 stainless chemistry table for UNS S35045 (same grade-text family; excerpt in _ref_a213.txt). Aluminum 0.15–0.60% and titanium 0.15–0.60% must both appear on the certificate; an MTC that only shows “Alloy 803 nickname chemistry” without the SA-213 ranges is incomplete. UNCERTAIN: edition year / table number of the SA-213 Book the mill stamps; confirm the ordered Code edition on the PO.

Product analysis — A480/A480M Table A1.1 tolerances applied

Element Melting Tolerance (A480 A1.1) Product analysis limit
Carbon (C) 0.06 – 0.10 0.01 under / over 0.05 – 0.11
Manganese (Mn) ≤ 1.50 0.04 over ≤ 1.54
Phosphorus (P) ≤ 0.045 0.010 over ≤ 0.055
Sulfur (S) ≤ 0.015 0.005 over ≤ 0.020
Silicon (Si) ≤ 1.00 0.05 over ≤ 1.05
Chromium (Cr) 25.0 – 29.0 0.25 under / over 24.75 – 29.25
Nickel (Ni) 32.0 – 37.0 0.15 under / 0.20 over (UNCERTAIN for 32–37 band) 31.85 – 37.20
Titanium (Ti) 0.15 – 0.60 0.05 under / over (UNCERTAIN) 0.10 – 0.65
Aluminum (Al) 0.15 – 0.60 0.05 under / over (UNCERTAIN) 0.10 – 0.65
Copper (Cu) ≤ 0.75 0.03 over ≤ 0.78

UNCERTAIN: A480 Table A1.1 tolerance digits for nickel at the 32–37% band and for Ti/Al at these levels — confirm against the A480/A480M edition named on the purchase order before releasing product-analysis acceptance. Product analysis is not a free substitute for melting compliance.

Snapshot vs nearby high-temp SA213 sisters

Element TP310S (S31008) Alloy 800 (N08800)* UNS S35045
C ≤ 0.08 ≤ 0.10 0.06 – 0.10
Cr 24.0 – 26.0 19.0 – 23.0 25.0 – 29.0
Ni 19.0 – 22.0 30.0 – 35.0 32.0 – 37.0
Al … 0.15 – 0.60 0.15 – 0.60
Ti … 0.15 – 0.60 0.15 – 0.60
Cu … ≤ 0.75 ≤ 0.75

*Alloy 800 (N08800) appears in the same public A213/SA-213 stainless table family for chemistry comparison only — it is not a published SHH STEEL SA213 product page in this stainless queue. Reading the snapshot: SA213 TP310S shares a high-chromium heat-resistant theme but lacks the Al–Ti package and runs lower nickel; S35045 deliberately carries both Al and Ti at 0.15–0.60% inside a higher Cr/Ni window. Do not dual-stamp a TP310S heat as S35045 because both show ~25% Cr on a PMI gun.

Mechanical Properties of SA213 UNS S35045

Mechanical acceptance for ASME SA213 UNS S35045 follows the stainless tensile table for this UNS designation. S35045 carries a single tensile / yield floor across the usual wall band: 70 ksi [485 MPa] tensile minimum, 25 ksi [170 MPa] yield minimum, 35% elongation minimum, and hardness not exceeding 192 HBW / 200 HV or 90 HRB.

Property UNS S35045 requirement
Tensile strength, min 70 ksi [485 MPa]
Yield strength (0.2% offset), min 25 ksi [170 MPa]
Elongation in 2 in. or 50 mm, min 35%
Hardness, max 192 HBW / 200 HV or 90 HRB

The 70/25 ksi floor aligns with several high-nickel austenitic rows and sits below the high-N superaustenitic floors — intentional for this Al–Ti oxidation package, not a mill shortfall. Hardness above 192 HBW / 90 HRB after solution treatment is a reject condition even if tensile clears. Specimens and testing follow the general requirements invoked by SA-213 (commonly ASTM A1016/A1016M) for the ordered finish route.

Dimensions and Tolerances

Dimensional supply for ASME SA213 UNS S35045 is tube language — outside diameter × wall thickness (minimum wall or average wall) and, commercially, BWG / gauge — not ASME B36.19 pipe schedules as the primary size story. Usual SA-213 sizes run from about 1/8 in. [3.2 mm] inside diameter to 5 in. [127 mm] outside diameter, with minimum wall from about 0.015 to 0.500 in. [0.4 to 12.7 mm]; other diameters may be furnished when all other requirements are met.

High-temperature heater and oxidation-leaning heat-exchanger datasheets that pick Alloy 803 class S35045 usually assume minimum wall — state wall basis on the purchase order. Outside-diameter and wall variations follow the general requirements invoked by SA-213 (commonly ASTM A1016/A1016M). The Al/Ti package does not rewrite the dimensional tolerance tables; it changes which heat clears the grade stamp.

Item Typical SA213 UNS S35045 dimensional practice
Product form Seamless only (cold-finished or hot-finished)
Usual size band ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD; wall ~0.015–0.500 in. [0.4–12.7 mm]
Wall basis Minimum wall (common for heater / HX datasheets) or average wall if PO says so
OD / wall tolerance Per general requirements (commonly A1016/A1016M) for the ordered finish
Length Straight random / cut-to-length; U-bend by agreement

BWG / gauge callouts are accepted on enquiry; certificates should still show OD and wall in inch or millimetre units. U-bends and polished ID finishes are commercial options — they do not change the SA-213 Al/Ti chemistry or tensile floors.

Equivalent Grades

UNS S35045 under ASME SA-213 has no TP letter. The commercial Alloy 803 nickname is widely used in high-temperature HX routing, but it does not replace the UNS product mark. Nearby high-temp sisters such as SA213 TP310S and Alloy 800 (N08800 — chemistry comparison only in this series) share oxidation themes, not identical Cr–Ni–Al–Ti packages. Plate chemistry conversations often point at A240 / SA240 — that is not a tube product stamp.

Designation Notes
ASME SA-213 / SA-213M UNS S35045 Governing Code Book seamless boiler / HX tube product standard — no TP letter
UNS S35045 Unified number that uniquely identifies the alloy
Alloy 803 (commercial) Shop name for Al–Ti 25Cr–35Ni-class chemistry — do not replace SA-213 product marking
Near Alloy 800 / 310 sisters (not substitutes) N08800 / TP310S share high-temp themes but different Cr–Ni–Al–Ti packages
ASTM A213 UNS S35045 Independent ASTM twin — dual-mark only when the PO asks

When a non-Code purchase needs the ASTM twin, use A213 UNS S35045. Do not write “SA213/A213 S35045” as a single merged standard title on the H1 or Standard param.

Heat Treatment and Delivery Condition

UNS S35045 under ASME SA-213 is furnished solution treated at a minimum of 2000 °F [1100 °C], then cooled in still air or faster — a cooling path that differs from the water-or-rapid-cool language printed for most neighboring austenitic rows. Do not force a mandatory water quench stamp onto S35045 if the ordered edition still allows still-air cool or faster; likewise do not invent a slower furnace cool that the grade text does not permit. Public heat-treatment tables do not print a mandatory grain-size number for this grade (ellipsis / no requirement).

Cold-finished and hot-finished seamless routes are both in scope; the heat-treatment minimum applies to the finished tube before final testing. Delivery condition on the MTC should read solution treated (annealed) with the actual temperature and cool method recorded when the purchaser asks. UNCERTAIN: Footnote F OCR placement near the HT row in some public excerpts — confirm the ordered SA-213 edition for any Footnote F temperature qualifier; S35045’s published floor remains 2000 °F [1100 °C] still air cool or faster.

Corrosion Resistance

Corrosion / oxidation framing for ASME SA213 UNS S35045 is high-temperature oxidation and carburization-leaning: the 25–29% Cr / 32–37% Ni window with Al and Ti each at 0.15–0.60% supports scale resistance and high-temp heater service, not the chloride PREN story told by SA213 UNS S31254 or SA213 UNS S31277.

Do not specify S35045 as a silent substitute for seawater cooler 6Mo tube, and do not treat it as interchangeable with SA213 TP310S simply because both show high chromium. Aluminum and titanium must appear on the MTC; a “25Cr–35Ni” PMI snapshot without Al/Ti is incomplete for this grade. Match media, temperature, carburizing potential, and Code design before release.

Applications of SA213 UNS S35045 Tube

Typical applications for ASME SA213 UNS S35045 seamless tube include Code-stamped high-temperature heaters, oxidation-leaning process heat exchangers, and related boiler / superheater circuits where the purchaser has named this Alloy 803 class Al–Ti grade rather than commodity SA213 TP310S or a generic Alloy 800 nickname without the SA-213 UNS.

The grade fits projects that need C 0.06–0.10%, Cr 25–29%, Ni 32–37%, Al 0.15–0.60%, Ti 0.15–0.60%, the 70/25 ksi tensile floor, and a 2000 °F solution anneal with still-air-or-faster cool. It is not the default choice for aggressive seawater chloride coolers (prefer 6Mo class such as SA213 UNS S31254). Confirm media, design temperature, and wall basis on the enquiry.

Weldability

UNS S35045 welds with practices appropriate for high-nickel Al–Ti austenitic stainless tube: controlled heat input, matching or nickel-base filler selected by the welding procedure, and attention to aluminum and titanium retention themes in the weld metal discussion. Solution-treated base metal remains the delivery condition for SA-213 product; post-weld heat treatment is a fabrication decision, not a substitute for the mill 2000 °F anneal.

Procedure qualification should use the actual S35045 chemistry — do not qualify on a TP310S heat and assume identical Al–Ti behavior. Cleanliness before welding matters; residual oils and sulfur compounds undermine hot-ductility in Al–Ti austenitics. For Code work, follow the Section IX procedure rules named by the purchaser.

Surface Finishes

Surface finishes for ASME SA213 UNS S35045 seamless tube follow ordinary SA-213 tube practice: as-cold-finished, pickled / passivated, or bright annealed routes by agreement. High-temperature heater ID cleanliness is often specified; state roughness or pickling requirements on the purchase order rather than assuming a mill default.

Light OD polish for appearance does not change chemistry or tensile acceptance. Heavy grinding that removes wall below the ordered minimum is a reject condition. Marking and stencil location should leave a readable SA-213 UNS S35045 identity after any agreed polish.

Inspection and Testing

Inspection and testing for ASME SA213 UNS S35045 follow the SA-213 product clauses plus the general requirements commonly invoked through ASTM A1016/A1016M: heat analysis, tensile / hardness, flattening / flaring as applicable, nondestructive electric or hydrostatic testing per the ordered option, and dimensional checks against OD × wall tolerances.

SHH STEEL supplies EN 10204 3.1 mill test certificates that list C, Mn, Si, Cr, Ni, Ti, Al, and Cu in the S35045 windows together with tensile, yield, elongation, and hardness. Supplementary Requirements (when ordered) may add product analysis, stricter NDE, or purchaser witness. PMI for Cr/Ni alone is not enough — aluminum and titanium at 0.15–0.60% need certified reporting.

Packaging and Shipping

Packaging for ASME SA213 UNS S35045 tube is chosen to protect ends, OD, and stencil identity through export handling: capped or plugged ends as agreed, bundled or boxed by size, with waterproof wrapping for ocean freight when specified. Heat and lot identity travel with the bundle so receiving inspectors can match the 3.1 certificate.

Cut-to-length bundles for high-temperature heater and HX projects are marked by OD × wall and heat number. U-bend sets, when ordered, ship with bend identity retained. Shipping documents reference ASME SA-213 UNS S35045 — not a generic “Alloy 803 tube” line that loses the UNS grade.

Why Choose SHH STEEL

SHH STEEL treats ASME SA213 UNS S35045 as a Code Book Alloy 803 class Al–Ti product with enforceable C 0.06–0.10%, Cr 25.0–29.0%, Ni 32.0–37.0%, Ti 0.15–0.60%, Al 0.15–0.60%, Cu ≤0.75%, 70/25 ksi tensile, 35% elongation, hardness max 192 HBW / 90 HRB, 2000 °F anneal with still-air-or-faster cool, and marking rules — not as “TP310S with an Alloy 803 sticker” checked only by a chromium PMI peak. Enquiry review verifies the aluminum and titanium windows before release.

That stops silent substitution with TP310S heats on datasheets that actually require S35045. We keep SA-213 and A213 independent, dual-mark only on request, and put Al and Ti on the 3.1 certificate so inspectors can verify the grade. The commercial Alloy 803 nickname is allowed for routing — it never replaces S35045 on the MTC.

Cross-links: SA213 TP310S, SA213 TP310H, SA213 UNS S30815, hub SA213/SA213M.

Supply Capability

SHH STEEL can supply ASME SA213 UNS S35045 stainless steel tube against the edition and finish route named on your enquiry. The capability table below summarizes sizes, finishes, and documents we regularly quote, followed by the Stock / Available sizes map for Alloy 803 class high-temperature heater and heat-exchanger tube.

Item SHH STEEL capability for UNS S35045
Standard ASME SA213 / SA213M (dual A213 marking on request)
Grade UNS S35045 (no TP letter)
Product form Seamless only — cold-finished and hot-finished
Size Typical OD × min wall (or average wall) in the SA-213 usual band; other diameters by agreement
Wall / gauge Minimum wall or average wall; BWG / gauge callouts accepted on enquiry
Length Cut-to-length for heater / HX bundles; U-bend by agreement
Documentation EN 10204 3.1 MTC with Al / Ti windows; witness on request
Trade terms FOB / CFR / CIF / EXW and other agreed Incoterms

Stock / Available sizes

SHH STEEL quotes S35045 against a stock-and-mill enquiry range rather than a frozen SKU or tonnage list. Representative OD × wall / BWG combinations below are an enquiry map for Alloy 803 class high-temperature heater and heat-exchanger tube — confirm live availability and cut lengths on the RFQ.

OD (in.) Typical wall / BWG enquiry band Notes
1/2 – 1 BWG 18–14 / ~0.049–0.083 in. Small heater / HX sizes
1-1/4 – 2 BWG 16–12 / ~0.065–0.109 in. Common high-temp HX band
2-1/2 – 3 0.083 – 0.180 in. min wall Heavier heater wall
3-1/2 – 5 0.120 – 0.250 in. min wall Large OD by agreement; confirm mill route

Send OD × wall (or BWG), wall basis, length / U-bend needs, finish, and whether dual A213 UNS S35045 marking is required. We return chemistry window confirmation (Al/Ti), tensile / hardness, anneal temperature and cool method, and lead time against the named SA-213 edition.

FAQ

Is ASME SA-213 the same as ASTM A213 for UNS S35045?
No. ASME SA-213 / SA-213M is the Code Book adoption that governs when a boiler or heat-exchanger specification invokes ASME by name; ASTM A213 / A213M is an independent ASTM product standard with the same grade-text family. Dual marking is a purchase-order choice, not automatic. SHH STEEL keeps the titles separate on certificates and only adds the ASTM twin when you ask for it.
Does ASME SA213 UNS S35045 have a TP grade letter?
No. UNS S35045 is listed without a TP letter in the SA-213 stainless table. Purchase orders and MTCs should carry UNS S35045, not an invented TP35045 stamp. The commercial Alloy 803 nickname is a routing aid only and does not replace the UNS designation on the certificate.
Is Alloy 803 the same as ASME SA213 UNS S35045?
Alloy 803 is the common commercial nickname for this Al–Ti 25Cr–35Ni-class chemistry family. It is useful for shop routing, but the governing product mark under this series is ASME SA-213 UNS S35045. Always write the UNS (and SA-213) on the purchase order and expect it on the MTC — a nickname alone is not a Code product stamp.
How does S35045 differ from TP310S under SA-213?
Both grades serve high-temperature themes, but the packages diverge. TP310S runs Cr 24–26% / Ni 19–22% without required Al or Ti. S35045 holds Cr 25–29%, Ni 32–37%, and deliberate Al and Ti each at 0.15–0.60%, with carbon 0.06–0.10%. Tensile floors and heat-treatment cool paths also differ. Do not dual-stamp a TP310S heat as S35045 because a PMI gun sees ~25% chromium.
How does S35045 relate to Alloy 800 (N08800)?
Alloy 800 (N08800) shares an Al–Ti high-nickel austenitic theme and appears in the same public chemistry-table family for comparison, but the Cr/Ni windows and product markings differ. S35045 runs higher chromium (25–29% vs 19–23%) and a slightly different nickel band. They are near sisters, not interchangeable SA-213 tube stamps. N08800 is not a published product page in this stainless SA213 queue.
What is special about the S35045 heat-treatment cool?
S35045 is solution treated at a minimum of 2000 °F [1100 °C] and cooled in still air or faster — unlike most neighboring austenitic rows that print water quench or other rapid cool. Do not force a mandatory water-quench stamp if the ordered edition allows still-air cool or faster, and do not invent a slower furnace cool the grade text does not permit.
Should I order minimum wall or average wall for S35045?
Most high-temperature heater and heat-exchanger datasheets that name SA-213 expect minimum wall unless the purchaser explicitly allows average wall. State the wall basis on the purchase order together with OD × wall or BWG. Minimum-wall tube is designed so the thinnest permitted wall still meets the ordered thickness; average-wall practice uses a different tolerance story under the general requirements.
Does ASME SA213 UNS S35045 cover welded or HCW tube?
No. SA-213 product scope for this series is seamless boiler, superheater, and heat-exchanger tube — cold-finished and/or hot-finished. Welded (WLD) and hot-finished continuous-welded (HCW) manufacturing types are outside this product page. If your datasheet needs welded high-nickel austenitic tube, that is a different product standard conversation.
Must aluminum and titanium both appear on the MTC?
Yes. Melting aluminum 0.15–0.60% and titanium 0.15–0.60% are both part of the S35045 chemistry window. An MTC that reports only “25Cr–35Ni” or “Alloy 803 nickname” without the Al and Ti bands is incomplete for this grade. Rely on certified chemistry, not a hand-held PMI guess for aluminum at these levels.
Can SHH STEEL dual-certify SA-213 and A213 for S35045?
Yes, when the purchase order asks. Dual SA-213/A213 marking is available for heats that meet both product standards’ requirements for UNS S35045. The ASME title remains the lead standard on Code jobs; the ASTM twin is the live page A213 UNS S35045. We do not merge the two titles into one H1 or Standard param line.
Is S35045 suitable for seawater cooler chloride service?
No as a default. S35045 is an Al–Ti high-temperature oxidation / carburization-leaning grade without a molybdenum or nitrogen PREN package. Seawater cooler datasheets written for 6Mo chemistry should look at grades such as UNS S31254 or UNS S31277 instead. Match media and failure mode first, then pick the SA-213 grade that actually carries those windows.

Conclusion

ASME SA213 UNS S35045 is the Alloy 803 class Al–Ti 25–29Cr / 32–37Ni seamless stainless steel tube grade for Code high-temperature heater, oxidation-leaning heat-exchanger, and related boiler / HX service when C 0.06–0.10%, Ti 0.15–0.60%, Al 0.15–0.60%, Cu ≤0.75%, 70/25 ksi tensile with 35% elongation, hardness max 192 HBW / 90 HRB, and a 2000 °F [1100 °C] solution anneal with still-air cool or faster are required together. SHH STEEL supplies cold-finished and hot-finished seamless tube in the usual OD × wall / BWG band with EN 10204 3.1 MTCs that report the aluminum and titanium windows. The commercial Alloy 803 nickname does not replace UNS S35045 on the certificate. For quotations and technical review, contact admin@steelspecs.com.

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X