ASME SA213 TP309HCb Stainless Steel Tube | ASME SA213 Stainless Steel - SHH STEEL

ASME SA213 TP309HCb Stainless Steel Tube

ASME SA213 TP309HCb / UNS S30941 seamless boiler, superheater and heat-exchanger tube — the H-grade niobium-stabilized 22–24% Cr austenitic with C 0.04–0.10%, Ni 12.0–16.0%, Nb 10×C–1.10%, a 75/30 ksi tensile floor, hardness max 192 HBW / 90 HRB, 1900 °F solution anneal, and ASTM grain size No. 7 or coarser. SHH STEEL supplies cold-finished and hot-finished seamless tube with EN 10204 3.1 MTCs that report Nb and grain size.
Grade
TP309HCb / UNS S30941
Standard
ASME SA213 / SA213M
Product form
Seamless boiler / superheater / heat-exchanger tube (cold-finished and hot-finished)
Size
Typical OD × min wall (or average wall) within ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD and ~0.015–0.500 in. [0.4–12.7 mm] wall; other diameters by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is ASME SA213 TP309HCb Stainless Steel Tube

ASME SA-213 / SA-213M is the ASME Boiler and Pressure Vessel Code Book adoption of the seamless ferritic and austenitic alloy-steel boiler, superheater, and heat-exchanger tube product standard. Grade TP309HCb under that Code Book text is the combined H-grade and niobium-stabilized higher chromium–nickel austenitic listed as UNS S30941, with melting limits of carbon 0.04–0.10%, chromium 22.0–24.0%, nickel 12.0–16.0%, and niobium (columbium) held between ten times the carbon content and 1.10%, plus ASTM grain size No. 7 or coarser on the heat-treatment lot. When a Code-stamped boiler or superheater datasheet calls for SA-213 TP309HCb, the purchase order and mill test certificate should carry the ASME designation, the H-grade carbon window, the Nb line, and the grain-size result — not a shop nickname such as “309HCb tube,” and not an assumed upgrade stamp on ordinary TP309Cb or TP309H.

SHH STEEL can supply ASME SA213 TP309HCb stainless steel tube as seamless cold-finished and hot-finished product in the usual boiler and heat-exchanger OD × wall / BWG band, documented on EN 10204 3.1 mill test certificates that report the full ladle chemistry — including measured Nb — the tensile plus hardness acceptance set, and the grain-size result for the heat-treatment lot. Dual SA-213 / A213 marking on the same lengths is available only when the purchase order asks for both independent standards; ASME SA213 and ASTM A213 remain separate documents even when the grade text aligns closely for a referenced edition. Browse the grade family on the SA213/SA213M hub.

Commercially the same tube is still called 309HCb, 309HNb, S30941 H-grade boiler tube, or H+Cb stabilized 309 tube; none of those phrases replace the ASME grade on the stencil or MTC. Sister grades under the same ASME standard include SA213 TP309H, SA213 TP309Cb, SA213 TP309S, SA213 TP347H, and SA213 TP310H. SA-213 covers seamless tube only — there is no welded or HCW manufacturing type under this product standard — so cold-finished versus hot-finished seamless route is the process choice, not a WLD/HCW stencil letter. For the sister ASTM product page on the same UNS, see A213 TP309HCb.

Chemical Composition of SA213 TP309HCb

Two chemistry layers matter for TP309HCb under ASME SA-213. The melting (heat or ladle) analysis is mandatory for every heat under the stainless chemistry table; product analysis on finished tube applies only when Supplementary Requirement wording or the purchase order invokes it through the general requirements path (commonly ASTM A1016/A1016M), with product-analysis tolerances typically taken from ASTM A480/A480M Table A1.1. Two lines drive selection before anything else: carbon 0.04–0.10% (the H-grade floor and ceiling) and niobium 10×C–1.10%. SHH STEEL reports the actual ladle values — including Nb — and the product values when ordered, and does not advertise unpublished tighter catalogue windows.

The tables below reproduce the melt limits for TP309HCb / UNS S30941 and the product-analysis limits that result from applying A480 Table A1.1 tolerances, plus a snapshot versus TP309H and TP309Cb. Values are maximum unless a range is shown; an ellipsis (…) means the ordered edition sets no requirement for that element. UNCERTAIN: exact SA-213 / A213 edition year and whether austenitic grades sit in Table 1 or Table 2 of that edition; grain-size clause/table number across editions; A480 Cr/Ni/Nb tolerance digits for the 22–24% Cr / 12–16% Ni band and the formula-minimum Nb path; S2 stabilizing applicability wording for TP309HCb — confirm the ordered edition text on the purchase order.

Melting analysis (heat / ladle analysis)

Source: public SA-213 / A213 grade-table summaries for TP309HCb / UNS S30941. Confirm the ordered ASME edition on the purchase order.

Element TP309HCb (UNS S30941) melting analysis
Carbon (C) 0.04 – 0.10
Manganese (Mn) ≤ 2.00
Phosphorus (P) ≤ 0.045
Sulfur (S) ≤ 0.030
Silicon (Si) ≤ 1.00
Chromium (Cr) 22.0 – 24.0
Nickel (Ni) 12.0 – 16.0
Molybdenum (Mo) … (no requirement)
Nitrogen (N) … (no requirement)
Niobium (Nb / Cb) 10×C – 1.10

Product analysis — A480/A480M Table A1.1 tolerances applied

Element Melting Tolerance (A480 A1.1) Product analysis limit
Carbon (C) 0.04 – 0.10 0.01 under / over 0.03 – 0.11
Manganese (Mn) ≤ 2.00 0.04 over ≤ 2.04
Phosphorus (P) ≤ 0.045 0.010 over ≤ 0.055
Sulfur (S) ≤ 0.030 0.005 over ≤ 0.035
Silicon (Si) ≤ 1.00 0.05 over ≤ 1.05
Chromium (Cr) 22.0 – 24.0 0.25 under / over 21.75 – 24.25
Nickel (Ni) 12.0 – 16.0 0.15 under / over 11.85 – 16.15
Niobium (Nb) 10×C – 1.10 0.05 under / over on max; min remains formula-tied max ≤ 1.15; min still ≥10×C on melt basis — confirm A480 path if contractual

Snapshot — TP309H vs TP309Cb vs TP309HCb

Element / control TP309H (S30909) TP309Cb (S30940) TP309HCb (S30941)
C 0.04 – 0.10 ≤ 0.08 0.04 – 0.10
Ni 12.0 – 15.0 12.0 – 16.0 12.0 – 16.0
Nb (Cb) … 10×C – 1.10 10×C – 1.10
Grain size No. 7 or coarser no mandatory number No. 7 or coarser

TP309HCb is not “TP309H with Nb added as a verbal extra” and not “TP309Cb stamped H.” The H-grade carbon floor of 0.04% plus the ASTM No. 7 or coarser grain-size requirement sit on top of the same Nb 10×C–1.10% and Ni 12.0–16.0% window used on TP309Cb. When creep-range boiler service needs H-grade carbon and grain size without niobium, open SA213 TP309H; when Nb stabilization at C ≤0.08% without mandatory grain size is enough, open SA213 TP309Cb.

When product analysis is ordered, finished tube may read C 0.03–0.11%, Mn ≤2.04%, P ≤0.055%, S ≤0.035%, and Si ≤1.05%, with Cr 21.75–24.25% and Ni 11.85–16.15%. The Nb maximum may move to 1.15% under the usual A480 0.05 over path, while the formula minimum remains melt-tied — confirm the contractual A480 reading if product Nb is acceptance-critical. Put any tighter project carbon, sulfur, or niobium window on the purchase order before the heat is selected.

Mechanical Properties of SA213 TP309HCb

ASME SA-213 sets the room-temperature tensile acceptance floor for TP309HCb at 75 ksi [515 MPa] tensile strength and 30 ksi [205 MPa] yield strength (0.2% offset), with elongation of 35% minimum in 2 in. or 50 mm. Hardness is capped at 192 HBW / 200 HV or 90 HRB — the same room-temperature pair as TP309H and TP309Cb. What distinguishes the grade mechanically in the product standard is the grain-size requirement of ASTM No. 7 or coarser on the heat-treatment lot, not a higher tensile floor. Every lot sampled under the edition’s specimen rules must meet the tensile and hardness numbers after the final solution treatment, and the grain-size result must be reported.

Source: public SA-213 / A213 mechanical-table and heat-treatment summaries for TP309HCb / UNS S30941. Mechanical property requirements do not apply to tubing smaller than 1/8 in. [3.2 mm] inside diameter or thinner than 0.015 in. [0.4 mm] wall.

Property TP309HCb requirement
Tensile strength, min 75 ksi [515 MPa]
Yield strength (0.2% offset), min 30 ksi [205 MPa]
Elongation in 2 in. or 50 mm, min 35%
Hardness, max 192 HBW / 200 HV or 90 HRB
Grain size ASTM No. 7 or coarser (per heat-treatment lot)

Flattening and flaring tests sit beside tension and hardness on a lot basis. Design calculations should use the 75/30 ksi pair unless the purchase order states higher guaranteed values the mill has accepted in writing. When the datasheet needs Nb without H-grade carbon and grain size, open SA213 TP309Cb; when H-grade carbon and grain size without Nb are enough, open SA213 TP309H; when even higher Cr–Ni oxidation resistance with H framing is required, open SA213 TP310H.

Dimensions and Tolerances

Dimensional supply for ASME SA213 TP309HCb is tube language — outside diameter × wall thickness (minimum wall or average wall) and, commercially, BWG / gauge — not ASME B36.19 pipe schedules as the primary size story. The sizes usually furnished under SA-213 run from about 1/8 in. [3.2 mm] inside diameter to 5 in. [127 mm] outside diameter, with minimum wall from about 0.015 to 0.500 in. [0.4 to 12.7 mm]; tubing with other diameters may be furnished when all other requirements of the specification are met. State on the purchase order whether wall is minimum or average, because remaining wall after high-temperature oxidation and creep-range exposure is often a design input on the circuits where H+Cb 309 is chosen.

Outside-diameter and wall variations follow the general requirements invoked by SA-213 (commonly ASTM A1016/A1016M), with cold-finished and hot-finished routes carrying different practical bands. Cold-finished tubes commonly hold tighter OD control; hot-finished tubes allow wider OD and wall windows. Permissible variations from a specified average wall for cold-finished tube are often summarized as ±10% of the specified average wall, while minimum-wall product is accepted to the minimum-wall tables rather than a symmetric ± window. Confirm the exact general-requirements rows for the OD and finish route on the ordered edition.

Item Typical SA213 TP309HCb dimensional practice
Product form Seamless only (cold-finished or hot-finished)
Usual size band ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD; wall ~0.015–0.500 in. [0.4–12.7 mm] min (or average wall if PO says so)
Wall basis Minimum wall (default commercial practice) or average wall when specified
OD / wall tolerances Per general requirements for the finish route and size; cold-finished average wall often ±10%
Length Cut lengths for HX / boiler / superheater bundles, or mill random lengths by agreement
Secondary size note ASME B36.19 schedules may appear only when a buyer asks for a pipe-schedule cross-reference — not as the primary SA-213 size callout

Put the cut list, U-bend or straight-tube preference, and end preparation on the enquiry so mill and stock lengths can be mixed efficiently. Minimum wall is a first-class SA-213 concept: if the datasheet assumes average wall, say so explicitly before the heat is rolled.

Equivalent Grades

Equivalence language around TP309HCb tube often collapses plate, cast, and tube product forms into one nickname. ASME SA-213 Grade TP309HCb / UNS S30941 is the governing designation for this article; EN and JIS wrought names that point to similar H+Nb high-Cr–Ni chemistry families are not automatic substitutes on an SA-213 mill test certificate. When a datasheet says “equivalent to 309HCb,” confirm which product standard, tensile/hardness table, Nb line, grain-size clause, and heat-treatment temperature the mill will actually certify.

Designation Notes
ASME SA-213 / SA-213M Grade TP309HCb Governing ASME Code Book seamless boiler / HX tube product standard for this article
UNS S30941 Unified number listed with the grade chemistry
ASTM A213 TP309HCb Separate ASTM International product specification — dual-mark only when the PO asks; see A213 TP309HCb
Related H without Nb SA213 TP309H — H carbon/grain-size, Ni 12–15, no Nb
Related Cb without H SA213 TP309Cb — Nb stabilization, C ≤0.08, no mandatory grain size
Related 18-8 H+Nb SA213 TP347H — H+Nb at lower Cr–Ni
Related plate A240 / SA240 flat product in the same UNS family — order plate and tube under their own product standards

ASTM A213 TP309HCb is the separate ASTM product specification sharing the same grade family; dual SA-213/A213 marking is a purchase-order option, not a claim that the two standards are one document. Compare sister SA213 TP309H and SA213 TP309Cb on their own ASME pages before swapping grades in a tube bundle.

Heat Treatment and Delivery Condition

TP309HCb under ASME SA-213 is furnished solution treated at a minimum of 1900 °F [1040 °C], then quenched in water or cooled rapidly by other means at a rate sufficient to prevent carbide reprecipitation. That heat-treatment row also carries the ASTM grain-size requirement of No. 7 or coarser for the heat-treatment lot — the clause that separates HCb acceptance from ordinary TP309Cb solution treatment at the same temperature. Both cold-finished and hot-finished seamless tube follow that path.

Cold-finished versus hot-finished is a process and dimensional route, not a substitute for the anneal or the grain-size result. Delivery condition for SHH STEEL TP309HCb is solution annealed and pickled (or bright annealed by agreement), with heat-treatment temperature, quench method, measured Nb, and grain size stated on the EN 10204 3.1 certificate. Straightening, cutting, and end finishing follow heat treatment.

When Supplementary Requirement language for intergranular-corrosion capability or stabilizing heat treatment (commonly discussed as S2 for listed HCb grades) is ordered, confirm the exact wording on the ordered edition and put it on the purchase order; mills will not assume stabilizing treatment from a verbal “HCb full certs” note. Use SA213 TP309Cb when Nb without H-grade grain-size is enough, and SA213 TP309H when H-grade carbon and grain size without Nb are enough.

Corrosion Resistance

TP309HCb is selected primarily for high-temperature oxidation and creep-range boiler or superheater service where the 22–24% chromium / 12–16% nickel balance, controlled H-grade carbon, niobium stabilization, and coarse grain size are specified together. The higher Cr–Ni oxide scale outperforms ordinary 18-8 grades in oxidizing furnace atmospheres and elevated-temperature steam circuits, while Nb prefers niobium carbides over chromium carbides and the H-grade grain-size clause supports creep-oriented design language. In chloride-bearing cooling waters and wet brine-leaning exchangers, buyers usually step to SA213 TP316 / SA213 TP316L or higher rather than treating 309HCb as a chloride upgrade.

ASME SA-213 itself does not publish a corrosion-rate, oxidation-life, or creep-rupture table for TP309HCb; selection remains engineering judgment against temperature, atmosphere, stress, and inspection philosophy. Intergranular corrosion risk after welding is moderated by the mandatory Nb line, by solution treating after fabrication when the sequence allows, or by invoking a contractual A262 Practice E Supplementary Requirement on the tube PO. SHH STEEL will not rank TP309HCb as equal to 316 in chlorides — neither niobium nor H-grade carbon is a molybdenum substitute.

Applications of SA213 TP309HCb Tube

Because TP309HCb combines H-grade carbon and grain-size controls with niobium stabilization on the 22–24% Cr / 12–16% Ni balance under SA-213, it shows up in creep-range boiler and superheater circuits, furnace-related heat exchangers, and elevated-temperature HX duty where both H framing and Cb stabilization are written into the datasheet. The table below pairs typical application areas with a selection note so the grade is chosen for atmosphere, metal temperature, creep need, and stabilization — not only for the familiar “309HCb” name on the BOM.

Application area Typical use of TP309HCb tube Selection note
Creep-range boiler / superheater Seamless tube where H carbon, grain size No. 7 or coarser, and Nb are specified together Confirm design metal temperature, stress, and MTC grain-size reporting
High-temperature oxidation + stabilization Seamless generating or process tubing ordered to SA-213 with Nb and H controls Prefer TP309H if Nb is not required; TP309Cb if grain size is not required
Furnace / hot-gas heat exchangers Straight and U-bend tubes in oxidizing hot-gas circuits needing H+Cb Prefer TP310H / TP310HCb if even higher Cr–Ni is specified
Welded high-temp circuits with H framing Tube where Nb plus H-grade controls protect HAZ and creep language together Still qualify the WPS; Nb and grain size do not replace PWHT when Code requires it
Chloride-rich cooling water Usually not the preferred selection Open molybdenum grades on the hub
General corrosive tube duty Seamless tube where SA-213 documentation is preferred over pipe forms Do not substitute SA312 / A312 pipe paperwork for SA-213 tube acceptance

For H without Nb open SA213 TP309H; for Nb without H open SA213 TP309Cb; for plain S-grade open SA213 TP309S; browse the same SA213/SA213M hub before locking the tube bill of materials.

Weldability

TP309HCb tube welds with matching or near-matching austenitic filler for tube-to-tubesheet joints, attachment welds, and fabrication joins. Common practice uses ER309 / ER309L or niobium-bearing austenitic fillers under a qualified WPS; many fabricators prefer low-carbon deposits even when the base tube already carries both H-grade carbon and Nb stabilization. Heat input control, interpass limits, and post-weld cleaning remain the fabricator’s responsibility under the applicable boiler or pressure-vessel Code — SA-213 governs the seamless tube product, not the field or shop weld procedure.

Because SA213 TP309HCb is seamless, there is no mill longitudinal weld to radiograph the way welded pipe standards describe. Focus inspection language on tube integrity (hydro or NDE of each length), tube-to-tubesheet joint quality, grain-size reporting on the MTC, and any contractual corrosion test on the base metal. The mandatory Nb line plus H-grade controls reduce — but do not eliminate — sensitization and creep-related concerns in the heat-affected zone; discuss whether a post-weld solution treatment or stabilizing Supplementary Requirement better protects the joint when service temperatures sit in the sensitizing or creep range. Specify end preparation and surface finish on the tube PO when orbital or clean-service joins are planned.

Surface Finishes

Standard mill delivery for ASME SA213 TP309HCb is solution annealed and pickled, leaving a clean matte finish suitable for most boiler and superheater tube duty. Bright annealing under protective atmosphere produces a smoother reflective surface used on some clean-process tube lines and must be called out because it changes the heat-treatment route and must still clear the grain-size requirement. Light polish or specified Ra on the bore or OD is a commercial or service-center operation on top of SA-213 product, not automatic with the grade stamp.

When a fouling-sensitive or clean-process exchanger specification quotes an Ra maximum on the bore, put it on the tube purchase order with its own acceptance language and sampling plan. SHH STEEL stencils grade, heat treatment, Nb identity, and grain-size reporting as standard requirements; polish, special OD grind, and passivation after fabrication remain commercial extras unless the contract says otherwise. End preparation should be ordered together with finish so receiving inspection shares one acceptance language.

Inspection and Testing

Base ASME SA-213 testing for TP309HCb includes heat analysis (with Nb reported), tension tests to the 75/30 ksi floor, hardness tests to the 192 HBW / 90 HRB maximum, grain-size determination to ASTM No. 7 or coarser on the heat-treatment lot, flattening and flaring tests on a lot basis, and either hydrostatic testing or nondestructive electric testing of each length. The manufacturer may choose hydro versus NDE unless the purchase order fixes the method; both are acceptance routes inside the product standard, not informal upgrades. Marking includes the ASME designation, grade, size, heat number, and other clause-required data so receiving inspection can tie each length back to the MTC.

Supplementary Requirements commonly added on TP309HCb tube orders are summarized below. Invoke them by number or clear purchase-order wording; mills will not assume product analysis, stabilizing treatment, or intergranular-corrosion testing from a verbal “full certs” note.

Option Purpose
Product analysis Confirms chemistry — including Nb — on finished tube (via general requirements / PO language)
Intergranular corrosion A262 Practice E (or agreed practice) as a contractual Supplementary Requirement
Stabilizing heat treatment (S2-class) Confirm applicability and temperature/time wording on the ordered edition for HCb grades
Minimum vs average wall States which wall basis the size callout uses
Fixed hydro or NDE method Removes manufacturer’s option when the end user mandates one route
Third-party inspection / EN 10204 3.2 Witnessed testing and certificate when the project requires it

Lot definitions for continuous heat treatment or direct quench after hot forming follow the size-based lot sizes in SA-213; ask the mill to state lot identity and grain-size result clearly on the certificate so hardness, tension, and grain-size specimens map cleanly to the bundle you receive.

Packaging and Shipping

TP309HCb tube leaves SHH STEEL bundled, capped or end-protected, and tagged for export or domestic delivery according to the length mix and bend form on the order. Bundle tags repeat the ASME SA213 grade, OD × wall (or BWG), heat number, and PO reference so site receiving can check the shipment without opening every certificate packet first. U-bent tubes need extra cradle or case protection so bend radii and legs are not distorted in transit.

Export packing can be bare bundles, wrapped bundles, or wooden-cased lengths for bright-annealed, polished, or small-bore material. We ship under the Incoterms on the order acknowledgement — FOB, CFR, CIF, EXW, or other agreed terms. Inland trucking, bilingual destination marks, or project color coding for bundle tags should be stated on the enquiry beside the metallurgical notes that call out Nb and grain-size reporting.

Why Choose SHH STEEL

SHH STEEL treats ASME SA213 TP309HCb as a Code Book product standard with enforceable chemistry — including the H-grade carbon window and Nb 10×C–1.10% line — tensile, hardness, grain-size, heat-treatment, and marking rules, not as a catalogue nickname for “any H or stabilized 309 tube.” The MTC reports the full ladle chemistry with measured Nb, the tensile/hardness acceptance set, and the grain-size result; the stencil carries seamless tube identity under SA-213; and dual SA-213/A213 marking is offered only when requested so Code and non-Code jobs stay cleanly documented.

We keep the 309-family conversation honest for creep-range boiler and HX duty. If H-grade carbon and grain size are required without Nb, we open SA213 TP309H. If Nb stabilization at C ≤0.08% without mandatory grain size is enough, we open SA213 TP309Cb. If ordinary S-grade oxidation resistance without H or Nb is enough, we open SA213 TP309S. If chlorides dominate a wet exchanger, we open SA213 TP316 / SA213 TP316L rather than stretching 309HCb into the wrong service. The SA213/SA213M hub is organized the same way — grade by grade under ASME, seamless tube only.

Lead times combine near-term stock lengths with mill schedules; we say which is which on the quotation. Cut-to-length, U-bending, polish, and third-party inspection are defined extras. The tube that arrives should match the ASME callout the engineer wrote, with paperwork a third-party inspector can read without translation.

Supply Capability

SHH STEEL can supply ASME SA213 TP309HCb stainless steel tube against the edition and finish route named on your enquiry. The capability table below summarizes the sizes, finishes, and documents we regularly quote for this grade, followed by the Stock / Available sizes map buyers ask for when they need a quick sense of what to enquire against for H-grade niobium-stabilized high-temperature boiler and superheater duty.

Item SHH STEEL capability for TP309HCb
Standard ASME SA213 / SA213M (dual A213 marking on request)
Grade TP309HCb / UNS S30941
Product form Seamless only — cold-finished and hot-finished
Size Typical OD × min wall (or average wall) in the SA-213 usual band; other diameters by agreement
Wall / gauge Minimum wall or average wall; BWG / gauge callouts accepted on enquiry
Length Cut-to-length for HX / boiler / superheater bundles; mill random by agreement; U-bends on enquiry
Finish Annealed and pickled; bright annealed or light polish by agreement
Testing Tension (75/30 ksi), hardness (max 192 HBW / 90 HRB), grain size No. 7 or coarser, flattening, flaring, hydro or NDE per length; full ladle chemistry including Nb on MTC; product analysis / IGC / S2-class on order
Documents EN 10204 3.1 with full ladle chemistry, Nb, and grain size; third-party inspection / 3.2 on request
Trade terms FOB / CFR / CIF / EXW and other agreed Incoterms

Stock / Available sizes

SHH STEEL quotes TP309HCb tube against a practical stock-and-mill enquiry range rather than a frozen warehouse SKU list. The sizes below are the OD × wall / BWG combinations buyers most often request for H-grade niobium-stabilized boiler and superheater tube; availability of any single line on a given week depends on mill drawing and our inbound schedule, so treat the table as a supply map for enquiry — not a guarantee that every line sits on the floor with a published tonnage.

Item Typical stock / enquiry range for TP309HCb
Outside diameter 19.05, 25.4, 31.8, 38.1, 44.5, 50.8, 63.5, 76.2 mm (and other HX/boiler ODs on enquiry; up through the usual SA-213 ~5 in. [127 mm] band)
Wall / BWG BWG 10–18 class walls and metric min-wall equivalents; lighter and heavier walls by agreement
Common OD × wall examples 25.4 × 2.11 mm; 25.4 × 2.77 mm; 31.8 × 2.77 mm; 38.1 × 2.77 mm; 38.1 × 3.40 mm; 50.8 × 3.40 mm; 50.8 × 3.60 mm — illustrative H-grade boiler/superheater sizes, confirm min vs average wall
Length Cut lengths for exchanger and high-temperature bundles; U-bends and straight random lengths on enquiry
Special Non-standard OD/wall, bright anneal, polished bore, Nb and grain-size reporting callouts, and dual SA-213/A213 marking — confirm on enquiry before the heat is reserved

When you send an enquiry, list OD × wall (or BWG), wall basis (minimum or average), cold-finished or hot-finished preference, quantity or cut list, required marking (SA-213 alone or dual SA-213/A213), Nb and grain-size reporting expectation, and any Supplementary Requirements including stabilizing treatment if applicable. We reply with what we can ship from near-term stock versus what needs a mill run, without inventing fake warehouse codes or tonnage claims.

Send the size list, finish route, quantity or cut lengths, required marking (SA-213 or dual SA-213/A213), Supplementary Requirements, and destination on one enquiry. We will confirm chemistry including Nb, tensile, hardness, and grain size against the ordered edition, state what ships from near-term availability versus mill production, and keep the offer aligned with the ASME SA213 / SA213M product standard that governs this page. Related grades such as SA213 TP309H, SA213 TP309Cb, and SA213 TP347H sit on the same hub when the datasheet steps beyond TP309HCb.

FAQ

Is ASME SA-213 the same as ASTM A213 for TP309HCb?
No. ASME SA-213 / SA-213M is the ASME Code Book adoption of the seamless boiler, superheater, and heat-exchanger tube grade text; ASTM A213 / A213M is the separate ASTM International product specification. Chemistry, tensile, hardness, and grain-size floors align closely for a given referenced edition, but they remain two independent standards. Dual-mark SA-213/A213 tube only when the purchase order asks for both names on the stencil and MTC.
Does ASME SA213 TP309HCb include welded or HCW tube?
No. ASME SA-213 covers seamless tube only. There is no WLD or HCW manufacturing type under this product standard the way ASME SA312 describes pipe. The process choice for TP309HCb under SA-213 is cold-finished versus hot-finished seamless tube, plus the heat-treatment, grain-size, and testing clauses of the ordered edition. If you need welded stainless pipe, that is a different product standard and a different steelspecs page family.
What is the chemistry of ASME SA213 TP309HCb?
TP309HCb is UNS S30941. Melting limits include carbon 0.04–0.10%, manganese ≤2.00%, phosphorus ≤0.045%, sulfur ≤0.030%, silicon ≤1.00%, chromium 22.0–24.0%, nickel 12.0–16.0%, and niobium (Cb) 10×C–1.10%, with molybdenum and nitrogen as no-requirement ellipses. Product-analysis limits apply only when ordered, typically from A480 Table A1.1 tolerances. Confirm the ordered SA-213 edition before treating a secondary catalogue as acceptance text.
TP309HCb vs TP309H — when do I need niobium under SA213?
Order TP309HCb when the datasheet requires both H-grade carbon 0.04–0.10% with ASTM No. 7 or coarser grain size and Nb 10×C–1.10% on the 22–24% Cr balance with Ni 12.0–16.0%. Order TP309H when H-grade carbon and grain size without niobium are enough and the nickel window stays 12.0–15.0%. Both share a 75/30 ksi tensile floor, so tensile equality alone is not a reason to swap.
TP309HCb vs TP309Cb — which SA213 grade should I order?
Order TP309HCb when creep-range H-grade carbon and grain-size controls are required on top of niobium stabilization. Order TP309Cb when Nb 10×C–1.10% at C ≤0.08% is enough and no mandatory ASTM grain-size number is called out. Do not treat "HCb" as a synonym stamp for ordinary TP309Cb on the MTC — the carbon floor, grain-size result, and H designation are contractual.
Why does SA-213 require grain size for TP309HCb?
The H designation under SA-213 pairs controlled carbon 0.04–0.10% with ASTM grain size No. 7 or coarser on the heat-treatment lot to support creep-oriented boiler and superheater design language. Room-temperature tensile floors remain 75/30 ksi — the same as TP309Cb — so grain size is not a substitute for a higher tensile number. Ask the mill to report the grain-size result on the EN 10204 3.1 certificate for every heat-treatment lot.
What is S2 stabilizing heat treatment for TP309HCb?
Supplementary Requirement language commonly discussed as S2 covers a stabilizing heat treatment for listed stabilized HCb grades under the ordered edition. Exact temperature, time, and applicability wording vary by edition, so confirm the ordered SA-213 text and put the Supplementary Requirement number or clear PO wording on the enquiry. Mills will not assume stabilizing treatment from a verbal "HCb full certs" note alone.
Does SA-213 set a hardness limit for TP309HCb?
Yes. The mechanical table for TP309HCb lists tensile strength, yield strength, elongation, and a hardness maximum of 192 HBW / 200 HV or 90 HRB. Hardness tests are part of lot acceptance under SA-213, which differs from many SA312 / A312 pipe rows for related UNS numbers that omit a hardness cap. If a project needs a tighter hardness window than the table, write it into the purchase order as an additional requirement.
What heat treatment does ASME SA-213 require for TP309HCb?
TP309HCb is solution treated at a minimum of 1900 °F [1040 °C] and then water quenched or rapidly cooled to prevent carbide reprecipitation, with ASTM grain size No. 7 or coarser required on the heat-treatment lot. Both cold-finished and hot-finished seamless tube follow that path. Ask the mill to state anneal temperature, quench method, measured Nb, and grain size on the EN 10204 3.1 certificate.
Minimum wall vs average wall — which should I order for SA213 TP309HCb?
Order minimum wall when the design and datasheet are written around a guaranteed minimum thickness after tolerance — especially important when remaining wall after high-temperature oxidation and creep-range exposure is a design input. Order average wall only when the purchase order explicitly allows average-wall product and the designer has accepted that basis. Put the wall basis on the enquiry before the mill selects tooling.
Is TP309HCb a good choice for chloride-rich cooling water under SA213?
Usually no. TP309HCb is framed for high-temperature oxidation and creep-range service with Nb stabilization, not for molybdenum-driven chloride pitting resistance. In seawater-leaning cooling water and wet brine exchangers, open TP316 / TP316L or higher-Mo grades on the SA213 hub. ASME SA-213 does not publish a chloride ranking that supports treating 309HCb as a 316 substitute.
Can you dual-certify ASME SA-213 and ASTM A213 TP309HCb?
Yes when the heat and testing support both independent standards, including grain-size and Nb reporting. Dual SA-213/A213 marking is available when the purchase order requests both names on the stencil and MTC. Spell the required marking on the enquiry so the heat is selected and documented correctly — a "309HCb" nickname alone is not dual certification.

Conclusion

ASME SA213 TP309HCb / UNS S30941 is the H-grade niobium-stabilized 22–24% Cr / 12–16% Ni seamless stainless steel tube grade for Code boiler, superheater, and heat-exchanger service when controlled carbon 0.04–0.10%, Nb 10×C–1.10%, and ASTM grain size No. 7 or coarser are required together. SHH STEEL supplies cold-finished and hot-finished seamless tube in the usual OD × wall / BWG band, solution annealed, tested to the 75/30 ksi tensile and hardness acceptance floors, with Nb and grain size reported on EN 10204 3.1 certificates — and dual A213 marking only when the order asks for that separate ASTM standard. For sister grades and stock-oriented size discussions, start from the SA213/SA213M hub, then send your OD × wall list, wall basis, Nb and grain-size reporting expectation, and marking requirements so we can align mill and near-term availability to the ASME callout.

Contact: admin@steelspecs.com

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X