ASME SA213 TP310HCb Stainless Steel Tube | ASME SA213 Stainless Steel - SHH STEEL

ASME SA213 TP310HCb Stainless Steel Tube

ASME SA213 TP310HCb / UNS S31041 seamless boiler, superheater and heat-exchanger tube — the H-grade niobium-stabilized 24–26% Cr / 19–22% Ni austenitic with C 0.04–0.10%, Nb 10×C–1.10%, a 75/30 ksi tensile floor, hardness max 192 HBW / 90 HRB, a 1900 °F solution anneal, and ASTM grain size No. 7 or coarser. Chosen when creep-range carbon/grain-size and Nb stabilization sit together on the 25Cr-20Ni balance. SHH STEEL supplies cold-finished and hot-finished seamless tube with EN 10204 3.1 MTCs that report Nb and grain size.
Grade
TP310HCb / UNS S31041
Standard
ASME SA213 / SA213M
Product form
Seamless boiler / superheater / heat-exchanger tube (cold-finished and hot-finished)
Size
Typical OD × min wall (or average wall) within ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD and ~0.015–0.500 in. [0.4–12.7 mm] wall; other diameters by agreement
Share:
Overview
Chemical Composition
Mechanical Properties
Specification
Equivalent Grades
Heat Treatment
Corrosion Resistance
Applications
Weldability
Surface Finishes
Inspection and Testing
Packaging and Shipping
Why Choose SHH STEEL
Supply Capability
FAQ
Conclusion

What is ASME SA213 TP310HCb Stainless Steel Tube

ASME SA-213 / SA-213M is the ASME Boiler and Pressure Vessel Code Book adoption of the seamless ferritic and austenitic alloy-steel boiler, superheater, and heat-exchanger tube product standard. Grade TP310HCb under that Code Book text is the H-grade niobium-stabilized member of the 310 family, listed as UNS S31041, with melting carbon held in a 0.04–0.10% band, chromium 24.0–26.0%, nickel 19.0–22.0%, niobium (columbium) held to the formula band 10×C–1.10%, and a mandatory ASTM grain-size requirement of No. 7 or coarser after solution treatment. When a Code-stamped boiler, superheater, or furnace heat-exchanger datasheet calls for SA-213 TP310HCb, the purchase order and mill test certificate should carry the ASME HCb designation, the carbon band, the niobium result, and the grain-size result — not a synonym stamp on ordinary TP310H or TP310Cb.

SHH STEEL can supply ASME SA213 TP310HCb stainless steel tube as seamless cold-finished and hot-finished product in the usual boiler, furnace, and heat-exchanger OD × wall / BWG band, documented on EN 10204 3.1 mill test certificates that report the full ladle chemistry including niobium, the tensile plus hardness acceptance set, and the ASTM E112 grain-size result for the heat-treatment lot. Dual SA-213 / A213 marking on the same lengths is available only when the purchase order asks for both independent standards; ASME SA213 and ASTM A213 remain separate documents even when the grade text aligns closely for a referenced edition. Browse the grade family on the SA213/SA213M hub.

Commercially the same tube is still called 310HCb, S31041, H-grade Nb 25Cr-20Ni tube, or SA213 310HCb tube; none of those phrases replace the ASME grade on the stencil or MTC. Sister grades under the same ASME standard include SA213 TP310H, SA213 TP310Cb, SA213 TP310HCbN, SA213 TP309HCb, and SA213 TP310S. SA-213 covers seamless tube only — there is no welded or HCW manufacturing type under this product standard — so cold-finished versus hot-finished seamless route is the process choice, not a WLD/HCW stencil letter. For the sister ASTM product page on the same UNS, see A213 TP310HCb.

Chemical Composition of SA213 TP310HCb

Two chemistry layers matter for TP310HCb under ASME SA-213. The melting (heat or ladle) analysis is mandatory for every heat under the stainless chemistry table; product analysis on finished tube applies only when Supplementary Requirement wording or the purchase order invokes it through the general requirements path (commonly ASTM A1016/A1016M), with product-analysis tolerances typically taken from ASTM A480/A480M Table A1.1. Reviewers should check three lines together: the 0.04–0.10% carbon band, the Nb 10×C–1.10 formula, and the 24–26 / 19–22 Cr–Ni windows — missing any one of those means the heat is not TP310HCb. SHH STEEL reports the actual ladle values — including Nb — and the product values when ordered, and does not advertise unpublished tighter catalogue windows.

The tables below reproduce the melt limits for TP310HCb / UNS S31041 and the product-analysis limits that result from applying A480 Table A1.1 tolerances, plus an H vs Cb vs HCb snapshot. Values are maximum unless a range or formula is shown; an ellipsis (…) means the ordered edition sets no requirement for that element. UNCERTAIN: exact SA-213 / A213 edition year and whether austenitic grades sit in Table 1 or Table 2 of that edition; grain-size clause or heat-treatment table number; Footnote H full wording and S2 stabilizing temperature/time text across editions; A480 Cr/Ni/Nb tolerance digits — confirm the ordered edition on the purchase order.

Melting analysis (heat / ladle analysis)

Source: public SA-213 / A213 grade-table summaries for TP310HCb / UNS S31041. Confirm the ordered ASME edition on the purchase order.

Element TP310HCb (UNS S31041) melting analysis
Carbon (C) 0.04 – 0.10
Manganese (Mn) ≤ 2.00
Phosphorus (P) ≤ 0.045
Sulfur (S) ≤ 0.030
Silicon (Si) ≤ 1.00
Chromium (Cr) 24.0 – 26.0
Nickel (Ni) 19.0 – 22.0
Molybdenum (Mo) … (no requirement)
Nitrogen (N) … (no requirement)
Niobium (Nb / Cb) 10×C – 1.10

Product analysis — A480/A480M Table A1.1 tolerances applied

Element Melting Tolerance (A480 A1.1) Product analysis limit
Carbon (C) 0.04 – 0.10 0.01 under / over 0.03 – 0.11
Manganese (Mn) ≤ 2.00 0.04 over ≤ 2.04
Phosphorus (P) ≤ 0.045 0.010 over ≤ 0.055
Sulfur (S) ≤ 0.030 0.005 over ≤ 0.035
Silicon (Si) ≤ 1.00 0.05 over ≤ 1.05
Chromium (Cr) 24.0 – 26.0 0.25 under / over 23.75 – 26.25
Nickel (Ni) 19.0 – 22.0 0.15 under / 0.20 over 18.85 – 22.20
Niobium (Nb) 10×C – 1.10 0.05 under / over on max; min remains formula-tied max ≤ 1.15; heat-analysis 10×C floor not relaxed — confirm A480 path if contractual

H vs Cb vs HCb snapshot

Element TP310H (S31009) TP310Cb (S31040) TP310HCb (S31041)
C 0.04 – 0.10 ≤ 0.08 0.04 – 0.10
Nb (Cb) … 10×C – 1.10 10×C – 1.10
Grain size No. 7 or coarser no mandate No. 7 or coarser
Cr / Ni 24–26 / 19–22 24–26 / 19–22 24–26 / 19–22

TP310HCb is not “TP310H with optional Nb” and not “TP310Cb with optional H marking.” Both the carbon band and the niobium formula are mandatory on the melt, and grain size No. 7 or coarser is mandatory on the heat-treatment lot. When only stabilization without the H package is required, stay on SA213 TP310Cb; when only H-grade carbon/grain-size without Nb is required, stay on SA213 TP310H; when nitrogen-strengthened HCbN tensile floors are required, open SA213 TP310HCbN.

When product analysis is ordered, finished tube may read C 0.03–0.11%, Mn ≤2.04%, P ≤0.055%, S ≤0.035%, Si ≤1.05%, Cr 23.75–26.25%, and Ni 18.85–22.20%, with Nb max ≤1.15 under typical A480 over-tolerance on the 1.10 ceiling. Put any tighter project floors on the purchase order before heat selection.

Mechanical Properties of SA213 TP310HCb

ASME SA-213 sets the room-temperature tensile acceptance floor for TP310HCb at 75 ksi [515 MPa] tensile strength and 30 ksi [205 MPa] yield strength (0.2% offset), with elongation of 35% minimum in 2 in. or 50 mm — the same room-temperature pair as TP310H and TP310Cb. Hardness is capped at 192 HBW / 200 HV or 90 HRB. The HCb mechanical distinction in the product standard is the grain-size requirement: ASTM No. 7 or coarser per heat-treatment lot, alongside chemistry that already includes both the carbon band and niobium. Every lot sampled under the edition’s specimen rules must meet those numbers after the final solution treatment.

Source: public SA-213 / A213 mechanical-table summaries for TP310HCb / UNS S31041 (commonly Table 4) and H-grade grain-size language. Mechanical property requirements do not apply to tubing smaller than 1/8 in. [3.2 mm] inside diameter or thinner than 0.015 in. [0.4 mm] wall.

Property TP310HCb requirement
Tensile strength, min 75 ksi [515 MPa]
Yield strength (0.2% offset), min 30 ksi [205 MPa]
Elongation in 2 in. or 50 mm, min 35%
Hardness, max 192 HBW / 200 HV or 90 HRB
Grain size ASTM No. 7 or coarser (per heat-treatment lot)

A complete TP310HCb release package reports tensile, hardness, niobium, carbon band, and grain size together. Omitting grain size or Nb turns an HCb certificate into an incomplete surrogate for TP310H or TP310Cb. When the datasheet needs the higher nitrogen-strengthened 95/43 ksi tensile floor with a fixed Nb band, open SA213 TP310HCbN; when a step down in Cr–Ni on an H+Cb path is enough, open SA213 TP309HCb.

Dimensions and Tolerances

Dimensional supply for ASME SA213 TP310HCb is tube language — outside diameter × wall thickness (minimum wall or average wall) and, commercially, BWG / gauge — not ASME B36.19 pipe schedules as the primary size story. The sizes usually furnished under SA-213 run from about 1/8 in. [3.2 mm] inside diameter to 5 in. [127 mm] outside diameter, with minimum wall from about 0.015 to 0.500 in. [0.4 to 12.7 mm]; tubing with other diameters may be furnished when all other requirements of the specification are met. Boiler and superheater datasheets almost always assume a minimum-wall reading — state wall basis on the purchase order, because remaining wall after high-temperature oxidation and creep is often a design input on the circuits where HCb is chosen.

Outside-diameter and wall variations follow the general requirements invoked by SA-213 (commonly ASTM A1016/A1016M), with cold-finished and hot-finished routes carrying different practical bands. Cold-finished tubes commonly hold tighter OD control; hot-finished tubes allow wider OD and wall windows. Permissible variations from a specified average wall for cold-finished tube are often summarized as ±10% of the specified average wall, while minimum-wall product is accepted to the minimum-wall tables rather than a symmetric ± window. Confirm the exact general-requirements rows for the OD and finish route on the ordered edition.

Item Typical SA213 TP310HCb dimensional practice
Product form Seamless only (cold-finished or hot-finished)
Usual size band ~1/8 in. [3.2 mm] ID to 5 in. [127 mm] OD; wall ~0.015–0.500 in. [0.4–12.7 mm] min (or average wall if PO says so)
Wall basis Minimum wall (default for boiler / superheater) or average wall when specified
OD / wall tolerances Per general requirements for the finish route and size; cold-finished average wall often ±10%
Length Cut lengths for boiler / furnace / HX bundles, or mill random lengths by agreement
Secondary size note ASME B36.19 schedules may appear only when a buyer asks for a pipe-schedule cross-reference — not as the primary SA-213 size callout

Put the cut list, design metal temperature context, Nb and grain-size reporting expectation, U-bend or straight-tube preference, and end preparation on the enquiry so mill and stock lengths can be mixed efficiently. Minimum wall is a first-class SA-213 concept for HCb tube the same way it is for other H-grade tube.

Equivalent Grades

Equivalence language around TP310HCb tube often collapses plate, cast, and ordinary H or Cb nicknames into one stamp. ASME SA-213 Grade TP310HCb / UNS S31041 is the governing designation for this article; near-chemistry wrought names are not automatic substitutes on an SA-213 mill test certificate. When a datasheet says “equivalent to 310HCb,” confirm which product standard, carbon band, niobium formula, grain-size clause, and heat-treatment row the mill will actually certify.

Designation Notes
ASME SA-213 / SA-213M Grade TP310HCb Governing ASME Code Book seamless boiler / HX tube product standard for this article
UNS S31041 Unified number listed with the grade chemistry
ASTM A213 TP310HCb Separate ASTM International product specification — dual-mark only when the PO asks; see A213 TP310HCb
Related H-grade SA213 TP310H — H carbon/grain-size without Nb
Related Cb SA213 TP310Cb — Nb formula without H package
Related HCbN SA213 TP310HCbN — fixed Nb band + N + higher tensile floor
Related 309HCb SA213 TP309HCb — lower Cr–Ni H+Cb step
Related plate A240 / SA240 flat product in the 310 family — order plate and tube under their own product standards

ASTM A213 TP310HCb is the separate ASTM product specification sharing the same grade family; dual SA-213/A213 marking is a purchase-order option, not a claim that the two standards are one document. Compare TP310H, TP310Cb, and TP310HCbN on their own ASME SA213 pages before swapping 310-family grades inside a furnace or boiler tube list.

Heat Treatment and Delivery Condition

TP310HCb under ASME SA-213 is furnished solution treated at a minimum of 1900 °F [1040 °C], then quenched in water or cooled rapidly by other means. That heat-treatment row carries Footnote H and the ASTM grain-size requirement of No. 7 or coarser for the heat-treatment lot. Footnote H warns that a solution-treating temperature above 1950 °F [1065 °C] may impair resistance to intergranular corrosion after subsequent sensitizing exposure in the indicated grades; when the purchaser specifies it, a lower-temperature stabilization or resolution anneal shall follow the higher-temperature solution anneal prescribed in the table.

Cold-finished versus hot-finished is a process and dimensional route, not a substitute for the anneal, the grain-size check, or any ordered stabilizing hold. Delivery condition for SHH STEEL TP310HCb is solution annealed and pickled (or bright annealed by agreement), with anneal temperature, quench method, niobium result, and E112 grain-size result on the EN 10204 3.1 certificate. Straightening, cutting, and end finishing follow heat treatment.

Supplementary Requirement S2 (stabilizing heat treatment) explicitly lists TP310HCb among the grades that shall be given a stabilizing treatment after the solution anneal when the purchaser specifies S2. Write S2 onto the purchase order when the datasheet requires that post-solution stabilizing hold — do not assume base SA-213 includes it automatically for every HCb shipment. Full temperature/time wording is edition text — confirm on the ordered edition. When nitrogen-strengthened HCbN tensile floors are required instead, open SA213 TP310HCbN.

Corrosion Resistance

TP310HCb is selected for high-temperature oxidation resistance from 24–26% Cr / 19–22% Ni, plus niobium stabilization against intergranular corrosion, plus H-grade carbon and grain-size controls — not for molybdenum-driven chloride pitting resistance. In oxidizing furnace atmospheres, hot-process gas circuits, and creep-range steam services where 18-8 and even 309HCb scale too quickly, the higher Cr–Ni oxide scale is the commercial reason to pay for 310HCb. In chloride-bearing cooling waters and wet brine-leaning exchangers, buyers usually step to SA213 TP316 / SA213 TP316L or higher rather than treating 310HCb as a chloride upgrade.

ASME SA-213 itself does not publish a corrosion-rate or oxidation-life table for TP310HCb; selection remains engineering judgment against temperature, atmosphere, velocity, and inspection philosophy. Optional S2 and any ordered A262 Practice E exist because Nb-bearing H grades can lose IGC resistance if solution temperatures run too high without a subsequent stabilizing or resolution step. Put those Supplementary Requirements on the purchase order when the project requires demonstrated IGC performance rather than chemistry-and-grain-size assurance alone. Sulfidation and carburizing atmospheres still need process-specific review. SHH STEEL will not rank TP310HCb as equal to 316 in chlorides — higher chromium, nickel, and niobium are not a molybdenum substitute.

Applications of SA213 TP310HCb Tube

Because TP310HCb brings controlled carbon 0.04–0.10%, Nb 10×C–1.10%, ASTM No. 7 or coarser grain size, and a 24–26% Cr / 19–22% Ni oxidation balance under SA-213, it shows up in creep-range boiler and superheater circuits, furnace-related heat exchangers, and elevated-temperature HX duty where both H-grade carbon/grain-size and Nb stabilization are written into the datasheet. The table below pairs typical application areas with a selection note so the grade is chosen for metal temperature, atmosphere, and Code language — not only for the familiar “310HCb” name on the BOM.

Application area Typical use of TP310HCb tube Selection note
Creep-range boiler / superheater + IGC risk Seamless generating or superheater tubing ordered to SA-213 with Nb and grain-size reporting Confirm design metal temperature and S2 needs
Severe high-temperature oxidation Seamless tube where 25Cr-20Ni scale resistance outperforms 18-8 and 309HCb Prefer TP309HCb if a step down in Cr–Ni is enough
Furnace / hot-gas heat exchangers Straight and U-bend tubes in oxidizing hot-gas circuits with thermal cycling Open TP310H if Nb is not required; TP310Cb if H package is not required
Chemical process (oxidizing, low chloride) Tube-side circuits with hot oxidizing media Prefer TP316/TP316L if chlorides dominate
Chloride-rich cooling water Usually not the preferred selection Open molybdenum grades on the hub
General Code tube duty Seamless tube where SA-213 HCb documentation is preferred over pipe forms Do not substitute SA312 / A312 pipe paperwork for SA-213 tube acceptance

For H-grade without Nb open SA213 TP310H; for Nb without H package open SA213 TP310Cb; for nitrogen-strengthened HCbN open SA213 TP310HCbN; browse the same SA213/SA213M hub before locking the tube bill of materials.

Weldability

TP310HCb tube welds with matching or near-matching austenitic filler for tube-to-tubesheet joints, attachment welds, and fabrication joins. Common practice uses ER310 / Nb-bearing or controlled-carbon deposits under a qualified WPS; fabricators often prefer Nb-bearing fillers when the base tube relies on niobium for post-weld intergranular resistance on an H-grade carbon heat. Heat input control, interpass limits, and post-weld cleaning remain the fabricator’s responsibility under the applicable boiler or pressure-vessel Code — SA-213 governs the seamless tube product, not the field or shop weld procedure.

Because SA213 TP310HCb is seamless, there is no mill longitudinal weld to radiograph the way welded pipe standards describe. Focus inspection language on tube integrity (hydro or NDE of each length), niobium and grain-size documentation on the base metal, tube-to-tubesheet joint quality, and any contractual corrosion test. For tube that will enter service as-welded in a sensitizing environment, discuss whether S2 stabilizing, a post-weld solution treatment, or a move to TP310HCbN better protects the joint. Specify end preparation and surface finish on the tube PO when orbital or clean-service joins are planned.

Surface Finishes

Standard mill delivery for ASME SA213 TP310HCb is solution annealed and pickled, leaving a clean matte finish suitable for most boiler, furnace, and heat-exchanger tube duty. Bright annealing under protective atmosphere produces a smoother reflective surface used on some clean-process tube lines and must be called out because it changes the heat-treatment route while still needing to clear the H-grade grain-size requirement and any ordered S2 stabilizing hold. Light polish or specified Ra on the bore or OD is a commercial or service-center operation on top of SA-213 product, not automatic with the grade stamp.

When a fouling-sensitive or clean-process exchanger specification quotes an Ra maximum on the bore, put it on the tube purchase order with its own acceptance language and sampling plan. SHH STEEL stencils grade, heat treatment, and grain-size identity as standard requirements and reports niobium on the MTC; polish, special OD grind, and passivation after fabrication remain commercial extras unless the contract says otherwise. End preparation should be ordered together with finish so receiving inspection shares one acceptance language.

Inspection and Testing

Base ASME SA-213 testing for TP310HCb includes heat analysis (with niobium), tension tests to the 75/30 ksi floor, hardness tests to the 192 HBW / 90 HRB maximum, grain-size determination to ASTM No. 7 or coarser per heat-treatment lot, flattening and flaring tests on a lot basis, and either hydrostatic testing or nondestructive electric testing of each length. The manufacturer may choose hydro versus NDE unless the purchase order fixes the method; both are acceptance routes inside the product standard, not informal upgrades. Marking includes the ASME designation, grade, size, heat number, and other clause-required data so receiving inspection can tie each length back to the MTC.

Supplementary Requirements commonly added on TP310HCb tube orders are summarized below. Invoke them by number or clear purchase-order wording; mills will not assume product analysis, S2 stabilizing, or intergranular-corrosion testing from a verbal “full certs” note. Grain size and niobium are both part of the base HCb acceptance — confirm both results appear on the certificate before releasing the heat.

Option Purpose
Product analysis Confirms chemistry including Nb on finished tube (via general requirements / PO language)
S2 stabilizing heat treatment Post-solution stabilizing hold — explicitly listed for TP310HCb when purchaser specifies S2
Intergranular corrosion A262 Practice E (or agreed practice) as a contractual Supplementary Requirement; related to Footnote H
Minimum vs average wall States which wall basis the size callout uses
Fixed hydro or NDE method Removes manufacturer’s option when the end user mandates one route
Third-party inspection / EN 10204 3.2 Witnessed testing and certificate when the project requires it

Lot definitions for continuous heat treatment or direct quench after hot forming follow the size-based lot sizes in SA-213; ask the mill to state lot identity clearly on the certificate so hardness, tension, grain-size, and chemistry specimens map cleanly to the bundle you receive.

Packaging and Shipping

TP310HCb tube leaves SHH STEEL bundled, capped or end-protected, and tagged for export or domestic delivery according to the length mix and bend form on the order. Bundle tags repeat the ASME SA213 grade, OD × wall (or BWG), heat number, and PO reference so site receiving can check the shipment without opening every certificate packet first. U-bent tubes need extra cradle or case protection so bend radii and legs are not distorted in transit.

Export packing can be bare bundles, wrapped bundles, or wooden-cased lengths for bright-annealed, polished, or small-bore material. We ship under the Incoterms on the order acknowledgement — FOB, CFR, CIF, EXW, or other agreed terms. Inland trucking, bilingual destination marks, or project color coding for bundle tags should be stated on the enquiry beside the metallurgical notes — including the Nb and grain-size reporting expectations that distinguish HCb release packages.

Why Choose SHH STEEL

SHH STEEL treats ASME SA213 TP310HCb as a Code Book product standard with enforceable chemistry (including niobium), tensile, hardness, heat-treatment, grain-size, and marking rules — not as a catalogue nickname for “any 310HCb tube.” The MTC reports the full ladle chemistry with Nb, the tensile/hardness acceptance set, and the E112 grain-size result; the stencil carries seamless tube identity under SA-213; and dual SA-213/A213 marking is offered only when requested so Code and non-Code jobs stay cleanly documented.

We keep the 310-family conversation honest for creep-range boiler and furnace duty. If only H-grade carbon/grain-size without Nb is required, we open SA213 TP310H. If only Nb stabilization without the H package is required, we open SA213 TP310Cb. If nitrogen-strengthened HCbN tensile floors are required, we open SA213 TP310HCbN. If a step down in chromium–nickel on an H+Cb path is enough, we open SA213 TP309HCb. If chlorides dominate a wet exchanger, we open SA213 TP316 / SA213 TP316L rather than stretching 310HCb into the wrong service. The SA213/SA213M hub is organized the same way — grade by grade under ASME, seamless tube only.

Lead times combine near-term stock lengths with mill schedules; we say which is which on the quotation. Cut-to-length, U-bending, polish, and third-party inspection are defined extras. The tube that arrives should match the ASME HCb callout the engineer wrote, with paperwork a third-party inspector can read without translation.

Supply Capability

SHH STEEL can supply ASME SA213 TP310HCb stainless steel tube against the edition and finish route named on your enquiry. The capability table below summarizes the sizes, finishes, and documents we regularly quote for this HCb grade, followed by the Stock / Available sizes map buyers ask for when they need a quick sense of what to enquire against for creep-range boiler, superheater, and furnace tube with Nb stabilization.

Item SHH STEEL capability for TP310HCb
Standard ASME SA213 / SA213M (dual A213 marking on request)
Grade TP310HCb / UNS S31041
Product form Seamless only — cold-finished and hot-finished
Size Typical OD × min wall (or average wall) in the SA-213 usual band; other diameters by agreement
Wall / gauge Minimum wall or average wall; BWG / gauge callouts accepted on enquiry
Length Cut-to-length for boiler / superheater / furnace / HX bundles; mill random by agreement; U-bends on enquiry
Finish Annealed and pickled; bright annealed or light polish by agreement
Testing Tension (75/30 ksi), hardness (max 192 HBW / 90 HRB), grain size ASTM No. 7 or coarser, flattening, flaring, hydro or NDE per length; full ladle chemistry including Nb on MTC; product analysis / S2 / IGC on order
Documents EN 10204 3.1 with full ladle chemistry, Nb, and grain-size result; third-party inspection / 3.2 on request
Trade terms FOB / CFR / CIF / EXW and other agreed Incoterms

Stock / Available sizes

SHH STEEL quotes TP310HCb tube against a practical stock-and-mill enquiry range rather than a frozen warehouse SKU list. The sizes below are the OD × wall / BWG combinations buyers most often request for creep-range high-temperature oxidation-resistant boiler and furnace tube with niobium stabilization; availability of any single line on a given week depends on mill drawing and our inbound schedule, so treat the table as a supply map for enquiry — not a guarantee that every line sits on the floor with a published tonnage.

Item Typical stock / enquiry range for TP310HCb
Outside diameter 19.05, 25.4, 31.8, 38.1, 44.5, 50.8, 63.5, 76.2 mm (and other boiler/furnace/HX ODs on enquiry; up through the usual SA-213 ~5 in. [127 mm] band)
Wall / BWG BWG 10–18 class walls and metric min-wall equivalents; lighter and heavier walls by agreement
Common OD × wall examples 25.4 × 2.11 mm; 25.4 × 2.77 mm; 31.8 × 2.77 mm; 38.1 × 2.77 mm; 38.1 × 3.40 mm; 50.8 × 3.40 mm; 50.8 × 3.60 mm — illustrative H+Cb boiler/furnace sizes, confirm min vs average wall
Length Cut lengths for boiler, superheater, and high-temperature bundles; U-bends and straight random lengths on enquiry
Special Non-standard OD/wall, bright anneal, polished bore, Nb and grain-size reporting confirmation, S2 stabilizing, and dual SA-213/A213 marking — confirm on enquiry before the heat is reserved

When you send an enquiry, list OD × wall (or BWG), wall basis (minimum or average), cold-finished or hot-finished preference, quantity or cut list, required marking (SA-213 alone or dual SA-213/A213), Nb and grain-size reporting expectation, S2 needs, and any Supplementary Requirements. We reply with what we can ship from near-term stock versus what needs a mill run, without inventing fake warehouse codes or tonnage claims.

Send the size list, finish route, quantity or cut lengths, required marking (SA-213 or dual SA-213/A213), Supplementary Requirements, and destination on one enquiry. We will confirm chemistry including Nb, tensile, hardness, and grain size against the ordered edition, state what ships from near-term availability versus mill production, and keep the offer aligned with the ASME SA213 / SA213M product standard that governs this page. Related grades such as SA213 TP310H, SA213 TP310Cb, and SA213 TP310HCbN sit on the same hub when the datasheet steps beyond TP310HCb.

FAQ

Is ASME SA-213 the same as ASTM A213 for TP310HCb?
No. ASME SA-213 / SA-213M is the ASME Code Book adoption of the seamless boiler, superheater, and heat-exchanger tube grade text; ASTM A213 / A213M is the separate ASTM International product specification. Chemistry, tensile, hardness, niobium, and grain-size floors align closely for a given referenced edition, but they remain two independent standards. Dual-mark SA-213/A213 tube only when the purchase order asks for both names on the stencil and MTC.
Does ASME SA213 TP310HCb include welded or HCW tube?
No. ASME SA-213 covers seamless tube only. There is no WLD or HCW manufacturing type under this product standard the way ASME SA312 describes pipe. The process choice for TP310HCb under SA-213 is cold-finished versus hot-finished seamless tube, plus the heat-treatment, grain-size, and testing clauses of the ordered edition. If you need welded stainless pipe, that is a different product standard and a different steelspecs page family.
What is the chemistry of ASME SA213 TP310HCb?
TP310HCb is UNS S31041. Melting limits include carbon 0.04–0.10%, manganese ≤2.00%, phosphorus ≤0.045%, sulfur ≤0.030%, silicon ≤1.00%, chromium 24.0–26.0%, nickel 19.0–22.0%, and niobium 10×C–1.10%, with molybdenum and nitrogen as no-requirement ellipses. Product-analysis limits apply only when ordered, typically from A480 Table A1.1 tolerances via the general-requirements path. Confirm the ordered SA-213 edition before treating a secondary catalogue as acceptance text.
TP310HCb vs TP310H — when do I need niobium under SA213?
Order TP310HCb when the datasheet needs niobium stabilization (Nb 10×C–1.10%) together with H-grade carbon 0.04–0.10% and ASTM No. 7 or coarser grain size on the 24–26% Cr / 19–22% Ni balance. Order TP310H when Nb is not required. Both share a 75/30 ksi tensile floor and the same grain-size mandate, so tensile equality alone is not a reason to swap; confirm the Nb callout before substituting either grade for the other.
TP310HCb vs TP310Cb — which SA213 grade should I order?
Order TP310HCb when the boiler or superheater datasheet needs carbon 0.04–0.10% and ASTM No. 7 or coarser grain size together with the Nb 10×C–1.10% formula. Order TP310Cb when you need Nb stabilization without the H-grade carbon band and grain-size package. Do not treat "310HCb" as a synonym stamp for ordinary TP310Cb on the MTC.
Why does SA-213 require grain size for TP310HCb?
The H-grade heat-treatment row requires ASTM No. 7 or coarser grain size per heat-treatment lot because coarse grain is part of the elevated-temperature / creep-oriented acceptance package that distinguishes TP310HCb from ordinary TP310Cb. A tensile-only certificate that omits the E112 result — or that reports Nb without grain size — is incomplete for TP310HCb release. Ask for both Nb and grain size on the EN 10204 3.1 mill test certificate.
What is S2 stabilizing heat treatment for TP310HCb?
Supplementary Requirement S2 explicitly lists TP310HCb among grades that shall be given a stabilizing treatment after the solution anneal when the purchaser specifies S2. Write S2 onto the purchase order when the datasheet requires that post-solution stabilizing hold — do not assume base SA-213 includes it automatically for every HCb shipment. Full temperature/time wording is edition text; confirm on the ordered edition and relate it to Footnote H language about high solution temperatures.
Does SA-213 set a hardness limit for TP310HCb?
Yes. Public mechanical-table summaries for TP310HCb set a hardness maximum of 192 HBW / 200 HV or 90 HRB alongside the 75 ksi tensile and 30 ksi yield floors. Hardness testing sits on a lot basis with tension, flattening, flaring, and grain-size determination. If a project quotes a tighter hardness window, put it on the purchase order as a contractual extra — the product-standard ceiling remains the acceptance floor unless the mill accepts a tighter guarantee in writing.
What heat treatment does ASME SA-213 require for TP310HCb?
TP310HCb is solution treated at a minimum of 1900 °F [1040 °C] and quenched in water or cooled rapidly by other means. The same heat-treatment row carries Footnote H and the ASTM grain-size requirement of No. 7 or coarser for the heat-treatment lot. Cold-finished versus hot-finished is a dimensional route, not a substitute for the anneal, the grain-size check, or any ordered S2 stabilizing hold. Delivery condition is typically solution annealed and pickled, with anneal temperature, quench method, Nb, and E112 result on the MTC.
Minimum wall vs average wall — which should I order for SA213 TP310HCb?
Boiler and superheater datasheets almost always assume minimum wall because remaining wall after high-temperature oxidation and creep is a design input. Average wall is acceptable when the purchase order says so and the general-requirements tolerances for that finish route are understood. State the wall basis explicitly on the enquiry so mill and stock lengths are rolled and accepted to the correct table — do not leave wall basis implied by a BWG number alone.
Is TP310HCb a good choice for chloride-rich cooling water under SA213?
Usually no. TP310HCb is built for high-temperature oxidation resistance, niobium stabilization, and H-grade carbon/grain-size controls; molybdenum is a no-requirement ellipsis. For chloride-rich cooling water and wet brine-leaning exchangers, open molybdenum grades such as SA213 TP316 / TP316L or higher rather than treating 310HCb as a chloride upgrade. Higher chromium, nickel, and niobium are not a molybdenum substitute.
Can you dual-certify ASME SA-213 and ASTM A213 TP310HCb?
Yes, when the purchase order asks for both independent standards on the stencil and mill test certificate. ASME SA-213 and ASTM A213 remain separate documents even when chemistry and tensile floors align for a referenced edition. Dual-mark only when both names are required; do not assume an A213-only certificate substitutes for an SA-213 Code callout, or the reverse.

Conclusion

ASME SA213 TP310HCb / UNS S31041 is the H-grade niobium-stabilized 24–26% Cr / 19–22% Ni seamless stainless steel tube grade for Code boiler, superheater, and furnace heat-exchanger service when creep-range carbon control, ASTM No. 7 or coarser grain size, and Nb binding of carbon against intergranular attack matter together on the 25Cr-20Ni balance. SHH STEEL supplies cold-finished and hot-finished seamless tube in the usual OD × wall / BWG band, solution annealed at 1900 °F with Footnote H awareness, tested to the 75/30 ksi tensile and hardness acceptance floors with Nb and grain-size reporting, and documented on EN 10204 3.1 certificates — with dual A213 marking only when the order asks for that separate ASTM standard. For sister grades and stock-oriented size discussions, start from the SA213/SA213M hub, then send your OD × wall list, wall basis, Nb and grain-size reporting expectation, and marking requirements so we can align mill and near-term availability to the ASME callout.

Contact: admin@steelspecs.com

Contact Us

Quality Steel Needed? Inquire for Offers

Need quality steel for your project? Inquire now to get tailored offers. Our team ensures quick responses, matching your needs with reliable steel solutions. Start your inquiry today.

    *

    *

    *

    *


    Related Products

    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response
    SHH STEEL Get Your Steel Quote—Inquire Now for Quick Response

      *

      *

      *

      *


      X